Cooling material for heating non-combustible cigarette as well as preparation method and application of cooling material
The cooling filter rod made of a combination of non-woven fabric matrix, polyethylene glycol and triacetin solves the problems of burning tips and burning sensation of smoke at the entrance of heat-not-burn cigarettes, achieving significant cooling effect and Convenient production process reduces production costs.
Patent Information
- Application Number
- CN202410834505.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-26
- Publication Date
- 2024-10-29
AI Technical Summary
The existing cooling method of heat-not-burn cigarettes has problems such as burning the mouth at the entrance, uncomfortable burning sensation of smoke, high production cost, and difficulty in mass production. In particular, the structure of the phase change material collapses and blocks the suction pipe, and the water absorption and cooling effect is not good. Obviously, the cooling effect is unsatisfactory.
Using a combination of non-woven fabric matrix, polyethylene glycol and triacetin, a cooling filter rod is made by spraying the mixed liquid on the non-woven fabric to reduce the flue gas inlet temperature and prevent mouth burning, and use conventional filter rod production equipment For mass production.
It effectively reduces the smoke inlet temperature of heat-not-burn cigarettes to below 52°C, preventing mouth burns. Raw materials are easily available, the production equipment is the same, no new equipment is needed, the cooling effect is significant, and the production cost is relatively low.
Smart Images

Figure CN118854681A_ABST
Abstract
Description
Technical Field
[0001] The present invention belongs to the technical field of heat-not-burn cigarette manufacturing, and specifically relates to a cooling material for heat-not-burn cigarettes and a preparation method and application thereof, and in particular to a cooling material for heat-not-burn cigarettes with good cooling effect and a preparation method and application thereof. Background Art
[0002] In recent years, various new tobacco products have developed rapidly. Among them, heat-not-burn cigarettes have attracted the attention and favor of consumers due to their low-tar and low-harm characteristics, and have quickly become a development hotspot and focus of the world tobacco industry.
[0003] Heat-not-burn tobacco products use heating devices to heat tobacco ingredients in a closed environment at 200℃ to 400℃ instead of burning to distill and crack tobacco components to release smoke, giving smokers the feeling of smoking tobacco and giving them a sense of satisfaction. However, due to the high water content of the aerosol produced and the short length of the cigarette, the mainstream smoke temperature is high, resulting in uncomfortable feelings such as burning mouth at the entrance and smoke burning.
[0004] At present, the commonly used cooling methods for heat-not-burn cigarettes mainly include material cooling, structural cooling and water absorption cooling. Material cooling is to incorporate phase change materials into the filter in different ways, and absorb heat through material phase change to achieve the cooling effect; structural cooling is to change the internal structure of the cigarette to extend the path and time of smoke circulation to achieve the cooling effect; water absorption cooling is to absorb water in the smoke aerosol through the water-absorbing material to achieve the cooling effect. The above cooling technologies have their own characteristics and shortcomings. For example, some phase change materials will produce structural collapse and block the suction pipe after absorbing heat; the water absorption cooling effect is not obvious and it is difficult to achieve satisfactory results; the process used for structural cooling has the problems of difficult mass production, high cost or low smoke volume. Therefore, how to take effective measures to reduce the mainstream smoke temperature of the product is an urgent problem to be solved. Summary of the invention
[0005] In view of the shortcomings of the prior art, the purpose of the present invention is to provide a cooling material for heat-not-burn cigarettes and a preparation method and application thereof, and in particular to provide a cooling material for heat-not-burn cigarettes with good cooling effect and a preparation method and application thereof. The cooling filter rod made of the cooling material provided by the present invention can reduce the smoke inlet temperature of heat-not-burn cigarettes to below 52°C to prevent the smoke from burning the mouth. At the same time, the raw materials are easy to obtain, and the equipment required for production is the same as the conventional filter rod production equipment, and no additional equipment is required.
[0006] In order to achieve the purpose of the invention, the present invention adopts the following technical solutions:
[0007] In a first aspect, the present invention provides a cooling material for heat-not-burn cigarettes, the cooling material comprising a non-woven fabric substrate and polyethylene glycol and triacetin dispersed on the non-woven fabric substrate.
[0008] The above method uses specific reagents and non-woven fabrics to produce a cooling material that can reduce the smoke inlet temperature of heat-not-burn cigarettes to below 52°C or even below 49°C to prevent the smoke from burning the mouth. At the same time, the raw materials are easy to obtain, and the equipment required for production is the same as the conventional filter rod production equipment, without the need for additional equipment.
[0009] Preferably, the polyethylene glycol includes low molecular weight polyethylene glycol and / or medium-high molecular weight polyethylene glycol, the low molecular weight polyethylene glycol is polyethylene glycol with a molecular weight lower than 1000, and the medium-high molecular weight polyethylene glycol is polyethylene glycol with a molecular weight not lower than 1000.
[0010] Preferably, the polyethylene glycol includes low molecular weight polyethylene glycol and medium and high molecular weight polyethylene glycol.
[0011] Preferably, the low molecular weight polyethylene glycol includes any one of PEG200, PEG400, PEG600 or PEG800, or a combination of at least two of them.
[0012] Preferably, the medium-high molecular weight polyethylene glycol includes any one of PEG1000, PEG1500, PEG2000 or PEG4000, or a combination of at least two of them.
[0013] Preferably, the low molecular weight polyethylene glycol is PEG400 and PEG600.
[0014] Preferably, the medium-high molecular weight polyethylene glycol is PEG2000 and PEG4000.
[0015] The above-mentioned specific polyethylene glycol selection can further improve the cooling effect of the product.
[0016] Preferably, the mass ratio of the low molecular weight polyethylene glycol, medium and high molecular weight polyethylene glycol and triacetin is (1-4):(1-4):(1-4), wherein the number of low molecular weight polyethylene glycol can be 1, 1.5, 2, 2.5, 3, 3.5 or 4, the number of medium and high molecular weight polyethylene glycol can be 1, 1.5, 2, 2.5, 3, 3.5 or 4, and the number of triacetin can be 1, 1.5, 2, 2.5, 3, 3.5 or 4, but is not limited to the values listed above. Other values not listed within the above numerical range are also applicable, preferably (1-2):(2-4):2.
[0017] Preferably, the total amount of polyethylene glycol and triacetin loaded on the nonwoven fabric is 7.5-13.5 g / m2 , for example 7.5g / m 2 , 8g / m 2 , 8.5g / m 2 , 9g / m 2 , 9.5g / m 2 , 10g / m 2 , 10.5g / m 2 , 11g / m 2 , 11.5g / m 2 , 12g / m 2 , 12.5g / m 2 , 13g / m 2 or 13.5g / m 2 The above values are not limited to the above values. Other values not listed in the above value range are also applicable.
[0018] Preferably, the total amount of polyethylene glycol and triacetin loaded on the nonwoven fabric is 8.5-11 g / m 2 .
[0019] The above-mentioned specific parameter control can further reduce the flue gas inlet temperature.
[0020] In a second aspect, the present invention provides a method for preparing the cooling material as described above, the method comprising the following steps:
[0021] Polyethylene glycol and triacetin are mixed to obtain a mixed solution, and then the mixed solution is sprayed on a non-woven fabric to form the cooling material.
[0022] In a third aspect, the present invention provides a cooling filter rod, which comprises a shaping paper and the cooling material as described above wrapped in the shaping paper.
[0023] In a fourth aspect, the present invention provides a method for preparing the cooling filter rod as described above, the preparation method comprising the following steps:
[0024] The cooling material as described above is rolled and wrapped with a forming paper to obtain the cooling filter rod.
[0025] In a fifth aspect, the present invention further provides a heat-not-burn cigarette, which comprises a tobacco core segment, a hollow segment, a cooling segment and a acetate segment which are sequentially connected, and the cooling segment comprises the cooling filter rod as described above.
[0026] Preferably, the acetate segment comprises an acetate filter rod.
[0027] Preferably, the length of the cigarette core segment is 10-15 mm, such as 10 mm, 11 mm, 12 mm, 13 mm, 14 mm or 15 mm, but is not limited to the values listed above, and other values not listed within the above numerical range are also applicable.
[0028] Preferably, the length of the hollow segment is 5-10 mm, such as 5 mm, 6 mm, 7 mm, 8 mm, 9 mm or 10 mm, but is not limited to the above-listed values. Other values not listed within the above range are also applicable.
[0029] Preferably, the length of the cooling section is 12-18 mm, for example, 12 mm, 13 mm, 14 mm, 15 mm, 16 mm, 17 mm or 18 mm, but is not limited to the values listed above, and other values not listed within the above numerical range are also applicable.
[0030] Preferably, the length of the acetate segment is 8-12 mm, such as 8 mm, 9 mm, 10 mm, 11 mm or 12 mm, but is not limited to the values listed above. Other values not listed within the above numerical range are also applicable.
[0031] Compared with the prior art, the present invention has the following beneficial effects:
[0032] The present invention provides a cooling material. By adopting specific reagents and non-woven fabrics, the prepared cooling filter rod can reduce the smoke inlet temperature of heat-not-burn cigarettes to below 52°C to prevent the smoke from scalding the mouth. At the same time, the raw materials are easy to obtain, and the equipment required for production is the same as the conventional filter rod production equipment, without the need for additional equipment. BRIEF DESCRIPTION OF THE DRAWINGS
[0033] Figure 1 It is a schematic diagram of the structure of the heat-not-burn cigarette provided in Application Example 1. DETAILED DESCRIPTION
[0034] The technical solution of the present invention is further described below by specific implementation methods. It should be understood by those skilled in the art that the embodiments are only to help understand the present invention and should not be regarded as specific limitations of the present invention.
[0035] In the following examples, the polyethylene glycol is food grade polyethylene glycol purchased from Guangzhou Suiyue Chemical Co., Ltd.; the width of the non-woven fabric is 117mm, and the basis weight is 107g / m 2 , purchased from Nantong Acetate Cellulose Co., Ltd.
[0036] Example 1
[0037] This embodiment provides a cooling filter rod, and the specific preparation steps are as follows:
[0038] PEG400, PEG600, PEG2000, PEG4000 and triacetin (mass ratio 0.7:0.8:1.5:1.5:2) were mixed to obtain a mixed solution, which was then evenly sprayed on the embossed nonwoven fabric through a spraying device (spraying amount was 9.5 g / m 2 ), and then gathered together and rolled into shape with forming paper to obtain the cooling filter rod (with a non-woven fabric filling amount of 1.5 g per 120 mm length).
[0039] Example 2
[0040] This embodiment provides a cooling filter rod, and the specific preparation steps are as follows:
[0041] PEG400, PEG600, PEG2000, PEG4000 and triacetin (mass ratio 0.5:0.5:2:2:2) were mixed to obtain a mixed solution, which was then evenly sprayed on the embossed nonwoven fabric through a spraying device (spraying amount was 8.5 g / m 2 ), and then gathered together and rolled into shape with forming paper to obtain the cooling filter rod (with a non-woven fabric filling amount of 1.5 g per 120 mm length).
[0042] Example 3
[0043] This embodiment provides a cooling filter rod, and the specific preparation steps are as follows:
[0044] PEG400, PEG600, PEG2000, PEG4000 and triacetin (mass ratio 1:1:1:1:2) were mixed to obtain a mixed solution, which was then evenly sprayed on the embossed nonwoven fabric through a spraying device (spraying amount was 11 g / m 2 ), and then gathered together and rolled into shape with forming paper to obtain the cooling filter rod (with a non-woven fabric filling amount of 1.5 g per 120 mm length).
[0045] Example 4
[0046] This embodiment provides a cooling filter rod, and the specific preparation steps are as follows:
[0047] PEG400, PEG600, PEG2000, PEG4000 and triacetin (mass ratio 0.5:0.5:2:2:1) were mixed to obtain a mixed solution, which was then evenly sprayed on the embossed nonwoven fabric through a spraying device (spraying amount was 7.5 g / m 2 ), and then gathered together and rolled into shape with forming paper to obtain the cooling filter rod (with a non-woven fabric filling amount of 1.5 g per 120 mm length).
[0048] Example 5
[0049] This embodiment provides a cooling filter rod, and the specific preparation steps are as follows:
[0050] PEG400, PEG600, PEG2000, PEG4000 and triacetin (mass ratio 2:2:0.5:0.5:4) were mixed to obtain a mixed solution, which was then evenly sprayed on the embossed nonwoven fabric through a spraying device (spraying amount was 13.5 g / m 2 ), and then gathered together and rolled into shape with forming paper to obtain the cooling filter rod (with a non-woven fabric filling amount of 1.5 g per 120 mm length).
[0051] Example 6
[0052] This embodiment provides a cooling filter rod. The specific preparation steps are the same as those of Embodiment 1 except that PEG400 is replaced by an equal amount of PEG600.
[0053] Example 7
[0054] This embodiment provides a cooling filter rod. The specific preparation steps are the same as those of Embodiment 1 except that PEG600 is replaced by an equal amount of PEG400.
[0055] Example 8
[0056] This embodiment provides a cooling filter rod. The specific preparation steps are the same as those of Embodiment 1 except that PEG600 is replaced by an equal amount of PEG200.
[0057] Example 9
[0058] This embodiment provides a cooling filter rod. The specific preparation steps are the same as those of Embodiment 1 except that PEG2000 is replaced by an equal amount of PEG4000.
[0059] Example 10
[0060] This embodiment provides a cooling filter rod. The specific preparation steps are the same as those of Embodiment 1 except that PEG4000 is replaced by an equal amount of PEG2000.
[0061] Embodiment 11
[0062] This embodiment provides a cooling filter rod. The specific preparation steps are the same as those of Embodiment 1 except that PEG4000 is replaced by an equal amount of PEG1500.
[0063] Example 12
[0064] This embodiment provides a cooling filter rod. The specific preparation steps are the same as those of Embodiment 1, except that PEG400 and PEG600 are not added and the reduced portion is proportionally distributed to PEG2000 and PEG4000.
[0065] Embodiment 13
[0066] This embodiment provides a cooling filter rod. The specific preparation steps are the same as those of Embodiment 1 except that PEG2000 and PEG4000 are not added and the reduced part is proportionally distributed to PEG400 and PEG600.
[0067] Comparative Example 1
[0068] This comparative example provides a cooling filter rod, and the specific preparation steps are the same as those in Example 1 except that the non-woven fabric is replaced with an equal amount of acetate fiber.
[0069] Application Example 1
[0070] This application example provides a heat-not-burn cigarette, the structure of which is as follows: Figure 1 As shown, from left to right are the cigarette core section (12 mm), the hollow core section (hollow structure 8 mm, outer diameter = 7.15 mm, inner diameter = 6.15 mm), the cooling section (cooling filter rod provided in Example 1, 15 mm) and the acetate section (ordinary cellulose diacetate filter rod, 10 mm, purchased from Nantong Cigarette Filter Co., Ltd.).
[0071] Application Example 2-13
[0072] Application Examples 2-13 respectively provide a heat-not-burn cigarette, which is consistent with Application Example 1 except that the cooling filter rod provided in Example 1 is replaced by the cooling filter rods provided in Examples 2-13 respectively.
[0073] Comparative application example 1
[0074] This comparative application example provides a heat-not-burn cigarette, which is consistent with Application Example 1 except that the cooling section is replaced by a hollow section of equal length.
[0075] Comparative Application Example 2
[0076] This comparative application example provides a heat-not-burn cigarette, which is consistent with Application Example 1 except that the cooling section is replaced by a acetate section of equal length.
[0077] Comparative Application Example 3
[0078] This comparative application example provides a heat-not-burn cigarette, which is consistent with Application Example 1 except that the cooling filter rod provided in Example 1 is replaced by the cooling filter rod provided in Comparative Example 1.
[0079] Effect test:
[0080] The heat-not-burn cigarettes provided in Example 1-13 and Comparative Example 1-3 were tested for smoke inlet temperature using an electronic smoking machine using the Canadian deep puff test method, with the instrument parameters set as follows: preheating for 10 seconds, puffing for 2 seconds, interval for 30 seconds, and puff count of 10 puffs. The results are as follows:
[0081]
[0082]
[0083] The trend of flue gas inlet temperature is generally that the first three inlets gradually rise to the highest temperature at the third inlet, and then the temperature gradually decreases and tends to be flat. When discussing the flue gas inlet temperature, the first three inlets are generally the main focus.
[0084] Therefore, from the above data, it can be found that the cooling filter rod provided by the present invention can reduce the smoke inlet temperature to below 52°C, effectively reducing the smoke inlet temperature; by comparing application examples 1 and 6-13, it can be found that the present invention can further reduce the smoke inlet temperature by selecting specific raw materials, and can reduce the smoke inlet temperature to below 50°C; by comparing application example 1 and comparative application examples 1-2, it can be found that the cooling filter rod made of the cooling material provided by the present invention can effectively reduce the smoke inlet temperature; by comparing application example 1 and comparative application example 3, it can be found that the temperature of each port in application example 1 (using a cooling section with non-woven fabric as the matrix material) is about 5°C lower than that in comparative application example 3 (using a cooling section with cellulose acetate as the matrix material), and the cooling effect is more obvious, because the non-woven fabric matrix has better water absorption and can better absorb moisture in the smoke aerosol, and the non-woven fabric itself is a composite material, in which components such as PLA also have a certain cooling effect.
[0085] The applicant declares that the present invention uses the above-mentioned embodiments to illustrate the cooling material for heat-not-burn cigarettes and its preparation method and application, but the present invention is not limited to the above-mentioned embodiments, that is, it does not mean that the present invention must rely on the above-mentioned embodiments to be implemented. Those skilled in the art should understand that any improvement of the present invention, equivalent replacement of various raw materials of the product of the present invention, addition of auxiliary components, selection of specific methods, etc., all fall within the protection scope and disclosure scope of the present invention.
[0086] The preferred embodiments of the present invention are described in detail above. However, the present invention is not limited to the specific details in the above embodiments. Within the technical concept of the present invention, a variety of simple modifications can be made to the technical solution of the present invention, and these simple modifications all belong to the protection scope of the present invention.
[0087] It should also be noted that the various specific technical features described in the above specific embodiments can be combined in any suitable manner without contradiction. In order to avoid unnecessary repetition, the present invention will not further describe various possible combinations.
Claims
1. A cooling material for heat-not-burn cigarettes, characterized in that: The cooling material comprises a non-woven fabric matrix and polyethylene glycol and triacetin dispersed on the non-woven fabric matrix.
2. The cooling material according to claim 1, characterized in that: The polyethylene glycol includes low molecular weight polyethylene glycol and / or medium-high molecular weight polyethylene glycol, wherein the low molecular weight polyethylene glycol is polyethylene glycol with a molecular weight lower than 1000, and the medium-high molecular weight polyethylene glycol is polyethylene glycol with a molecular weight not lower than 1000; Preferably, the polyethylene glycol includes low molecular weight polyethylene glycol and medium and high molecular weight polyethylene glycol; Preferably, the low molecular weight polyethylene glycol includes any one of PEG200, PEG400, PEG600 or PEG800, or a combination of at least two thereof; Preferably, the medium- and high-molecular-weight polyethylene glycol includes any one of PEG1000, PEG1500, PEG2000, or PEG4000, or a combination of at least two thereof.
3. The cooling material according to claim 2, characterized in that: The low molecular weight polyethylene glycol is PEG400 and PEG600; Preferably, the medium- and high-molecular-weight polyethylene glycols are PEG2000 and PEG4000; Preferably, the mass ratio of the low molecular weight polyethylene glycol, medium and high molecular weight polyethylene glycol and triacetin is (1-4):(1-4):(1-4), preferably (1-2):(2-4):
2.
4. The preparation method according to any one of claims 1 to 3, characterized in that The total amount of polyethylene glycol and triacetin loaded on the non-woven fabric is 7.5-13.5 g / m 2 .
5. The preparation method according to claim 4, characterized in that The total amount of polyethylene glycol and triacetin loaded on the non-woven fabric is 8.5-11 g / m 2 .
6. A method for preparing a cooling material according to any one of claims 1 to 5, characterized in that: The preparation method comprises the following steps: Polyethylene glycol and triacetin are mixed to obtain a mixed solution, and then the mixed solution is sprayed on a non-woven fabric to form the cooling material.
7. A cooling filter rod, characterized in that: The cooling filter rod comprises a wrapping paper and the cooling material according to any one of claims 1 to 5 wrapped in the wrapping paper.
8. A method for preparing a cooling filter rod according to claim 7, characterized in that: The preparation method comprises the following steps: The cooling filter rod is obtained by rolling and wrapping the cooling material according to any one of claims 1 to 5 with a forming paper.
9. A heat-not-burn cigarette, characterized in that: The heat-not-burn cigarette comprises a tobacco core segment, a hollow segment, a cooling segment and a acetate segment which are sequentially connected, and the cooling segment comprises the cooling filter rod according to claim 7.
10. The heat-not-burn cigarette according to claim 9, characterized in that: The acetate segment includes an acetate filter rod; Preferably, the length of the cigarette core segment is 10-15 mm; Preferably, the length of the hollow segment is 5-10 mm; Preferably, the length of the cooling section is 12-18 mm; Preferably, the length of the acetate segment is 8-12 mm.