Wet etching method for improving feature size consistency

By controlling the replacement interval and etching time of the etching liquid in the wet etching device, the problem of inconsistent feature sizes caused by the evaporation of water in the etching liquid during wet etching is solved, and the stability and performance improvement of product feature sizes are achieved.

CN118872031APending Publication Date: 2024-10-29BEIJING ADVANCED MEMORY TECH CO LTD +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202380023785.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-05-22
Publication Date
2024-10-29

AI Technical Summary

Technical Problem

The evaporation of water in the etching solution during wet etching causes the etching rate to increase, resulting in inconsistent feature sizes and affecting product yield and performance.

Method used

By setting up acid tanks, nozzles and conduits in the wet etching device, the replacement interval and etching time of the etching solution are controlled to ensure that the concentration of the etching solution is stable. A rotating platform is used for etching to keep the feature size consistent after etching.

Benefits of technology

It improves the feature size consistency of products etched at different times, and improves product yield and performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118872031A_ABST
    Figure CN118872031A_ABST
Patent Text Reader

Abstract

The invention provides a wet etching method for improving feature size consistency, and belongs to the field of integrated circuit manufacturing. The wet etching method comprises the following steps: a semiconductor component forming step: forming a semiconductor component on a semiconductor substrate of a wafer; an etching liquid replacement step: replacing the etching liquid in the acid tank; and an etching step: guiding the etching liquid in the acid tank to a spray head through a conduit, spraying the etching liquid to the surface of the wafer through the spray head, driving the wafer to rotate by the platform at the same time so as to etch the semiconductor assembly, and controlling the etching time t according to the interval time L between the etching liquid replacement step and the etching step. According to the wet etching method provided by the invention, the consistency of the characteristic size can be improved, so that the yield and the performance of a product are improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of integrated circuit manufacturing, and in particular to a wet etching method for improving feature size consistency. Background Art

[0002] Etching liquid is required in wet etching. Usually, etching liquid has a certain validity period. Etching liquid that exceeds the validity period cannot be used. Therefore, new etching liquid must be replaced every once in a while before etching. However, as time goes by, the water in the etching liquid will continue to evaporate, causing the concentration of the etching liquid to continue to increase, thereby causing the etching rate (Etch Rate) to continue to increase. In this way, when etching structures such as key holes, the CD (feature size) of the etched Key Hole will continue to increase. After a period of time, a new etching liquid is replaced, and the CD of the etched Key Hole will become smaller again. This results in products etched at different times, and the CD of the Key Hole after etching is inconsistent. This will reduce the yield of the product and affect the performance of the product. Summary of the invention

[0003] The present invention aims to provide a wet etching method capable of improving CD consistency.

[0004] The wet etching device used in the wet etching method for improving CD consistency provided by the present invention comprises: a chamber, a platform for placing a wafer arranged at the bottom of the chamber, a nozzle arranged at the top of the chamber for spraying etching liquid to the wafer, an acid tank arranged outside the chamber for storing the etching liquid, a conduit connecting the nozzle and the acid tank, and a waste liquid collecting component arranged around the platform. The wet etching method comprises: a semiconductor component forming step: forming a semiconductor component on a semiconductor substrate of the wafer; an etching liquid replacing step: replacing the etching liquid in the acid tank; and an etching step: guiding the etching liquid in the acid tank to the nozzle through the conduit, and spraying the etching liquid onto the surface of the wafer through the nozzle, while the platform drives the wafer to rotate, so as to etch the semiconductor component, and controlling the etching time t according to the interval time L between the etching liquid replacing step and the etching step.

[0005] The wet etching method of the present invention can improve the CD consistency of products etched at different times, thereby improving the yield and performance of the products. BRIEF DESCRIPTION OF THE DRAWINGS

[0006] Figure 1 is a schematic diagram of a wet etching device of the present invention;

[0007] Figure 2is a flow chart of the wet etching method of the present invention;

[0008] Figure 3 is a schematic diagram of a semiconductor component before wet etching of the present invention; and

[0009] Figure 4 Schematic diagram of a semiconductor component after wet etching according to the present invention.

[0010] Explanation of symbols

[0011] 100 wet etching equipment

[0012] 1 Chamber

[0013] 2 Wafer

[0014] 3 Platforms

[0015] 4 nozzles

[0016] 5 Acid Tanks

[0017] 6 Catheter

[0018] 7Waste liquid collection parts

[0019] 10Semiconductor substrate

[0020] 11First silicon nitride layer

[0021] 12Silicon oxide layer

[0022] 13 Second silicon nitride layer

[0023] 14The First Hole

[0024] 15 Second Hole

[0025] 16Third Hole

[0026] 20Semiconductor components DETAILED DESCRIPTION

[0027] Refer to the following Figures 1 to 4 The wet etching method of the present invention for improving CD uniformity is described.

[0028] like Figure 1 As shown, the wet etching device 100 used in the wet etching method of the present invention includes: a chamber 1, a platform 3 arranged at the bottom of the chamber 1 for placing a wafer 2, a nozzle 4 arranged at the top of the chamber 1 for spraying etching liquid to the wafer 2, an acid tank 5 arranged outside the chamber 1 for storing the etching liquid, a conduit 6 connecting the nozzle 4 and the acid tank 5, and a waste liquid collection component 7 arranged around the platform 3.

[0029] In this embodiment, the wet etching device 100 is DV-PRIME of LAM Company of the United States. However, the present invention is not limited thereto, and other machines may also be used. The components of the etching liquid are: HF (hydrofluoric acid), NH4F (ammonium fluoride) and water. The etching liquid is mainly used for etching silicon oxide. However, the present invention is not limited thereto, and etching liquids with other components may also be used.

[0030] like Figure 2 and Figure 3 As shown, the wet etching method of the present invention comprises:

[0031] Semiconductor component forming step S100 : forming a semiconductor component 20 on a semiconductor substrate 10 of a wafer 2 .

[0032] In this embodiment, the semiconductor component 20 includes: a first silicon nitride layer 11, a silicon oxide layer 12 and a second silicon nitride layer 13. However, the present invention is not limited thereto, and the semiconductor component 20 may also be other structures as long as it can be etched by a wet etching process. The semiconductor substrate 10 may be a silicon substrate, or a substrate of other materials, such as a ceramic material, an organic material, a glass material, etc. The semiconductor component 20 may be directly formed on the semiconductor substrate 10, or there may be other layers between the semiconductor component 20 and the semiconductor substrate 10.

[0033] Preferably, the semiconductor component forming step S100 includes: forming a first silicon nitride layer 11, a silicon oxide layer 12 and a second silicon nitride layer 13 on the semiconductor substrate 10 of the wafer 2, and forming a first hole 14 in the silicon oxide layer 12, and forming a second hole 15 in the second silicon nitride layer 13, and the diameter D1 of the first hole 14 is equal to the diameter D2 of the second hole 15.

[0034] The first silicon nitride layer 11, the silicon oxide layer 12, and the second silicon nitride layer 13 may be formed by methods commonly used in the art, such as PVD (physical vapor deposition), CVD (chemical vapor deposition) processes, etc. The first hole 14 may be formed in the silicon oxide layer 12, and the second hole 15 may be formed in the second silicon nitride layer 13 by methods commonly used in the art, such as photolithography and etching processes, etc.

[0035] like Figure 1 and Figure 2 As shown, the wet etching method of the present invention also includes:

[0036] Etching solution replacement step S200: Replace the etching solution in the acid tank 5. The life time of the etching solution in this embodiment is about three days, so the etching solution in the acid tank 5 is replaced every three days. However, the present invention is not limited to this, and other days may also be used.

[0037] like Figure 1-3As shown, the wet etching method of the present invention also includes:

[0038] Etching step S300: The etching liquid in the acid tank 5 is guided to the nozzle 4 through the conduit 6, and the etching liquid is sprayed onto the surface of the wafer 2 through the nozzle 4. At the same time, the platform 3 drives the wafer 2 to rotate, thereby etching the semiconductor component 20, and the etching time t is controlled according to the interval time L between the etching liquid replacement step S200 and the etching step S300.

[0039] Specifically, the etching time t refers to the time for the nozzle 4 to spray the etching liquid and the time for the platform 3 to drive the wafer 2 to rotate. In addition, in this embodiment, the waste liquid collecting component 7 is cylindrical and is arranged around the platform 3. As the wafer 2 rotates at a high speed, the etching liquid will be thrown onto the waste liquid collecting component 7, and then discharged out of the chamber 1 through the drainage device (not shown) on the waste liquid collecting component 7.

[0040] Preferably, if Figure 1 and Figure 4 As shown, the etching step S300 includes: the etching liquid performs side etching (Pull Back) on the silicon oxide layer 12, thereby forming a third hole 16 in the silicon oxide layer 12, and the diameter D3 of the third hole 16 is greater than the diameter D2 of the second hole 15. In this embodiment, the etching liquid performs side etching (Pull Back) on the silicon oxide layer 12, but the present invention is not limited thereto, and other etching methods may also be used.

[0041] Preferably, the larger the interval time L is, the shorter the etching time t is. Because the larger the interval time L is, the more water in the etching solution evaporates, so the greater the concentration of the etching solution is, the greater the etching rate (Etch Rate) is. Therefore, in order to keep the diameter D3 (i.e., CD) of the third hole 16 after etching consistent, it is necessary to appropriately reduce the etching time t. In this embodiment, on the day when the etching solution is replaced, that is, when the interval time L is 0 days, the etching time is t0. When the interval time L is 1 day, the etching time is t1. When the interval time L is 2 days, the etching time is t2. Among them, t0>t1>t2. In this way, the CD of the Key Hole etched on different dates can be kept consistent, thereby improving the yield and performance of the product.

[0042] Although the present invention has been disclosed in the above embodiments, it is not intended to limit the present invention. Any professional and technical personnel in the field may make various necessary changes and modifications without departing from the spirit and scope of the present invention. Therefore, the scope of protection of the present invention shall be based on the scope defined by the attached claims.

[0043] Industrial Applicability

[0044] The wet etching method of the present invention can improve the CD consistency of products etched at different times, thereby improving the yield and performance of the products.

Claims

1. A wet etching method for improving feature size consistency, It is characterized in that The wet etching device (100) used in the wet etching method comprises: a chamber (1), a platform (3) arranged at the bottom of the chamber (1) for placing a wafer (2), a nozzle (4) arranged at the top of the chamber (1) for spraying etching liquid onto the wafer (2), an acid tank (5) arranged outside the chamber (1) for storing the etching liquid, a conduit (6) connecting the nozzle (4) and the acid tank (5), and a waste liquid collection component (7) arranged around the platform (3). The wet etching method comprises: Semiconductor component forming step: forming a semiconductor component (20) on the semiconductor substrate (10) of the wafer (2); Etching liquid replacement step: replacing the etching liquid in the acid tank (5); and Etching step: the etching liquid in the acid tank (5) is guided to the nozzle (4) through the conduit (6), and the etching liquid is sprayed onto the surface of the wafer (2) through the nozzle (4), and at the same time, the platform (3) drives the wafer (2) to rotate, thereby etching the semiconductor component (20), and the etching time t is controlled according to the interval time L between the etching liquid replacement step and the etching step.

2. The wet etching method for improving feature size consistency according to claim 1, It is characterized in that The semiconductor component forming step comprises: forming a first silicon nitride layer (11), a silicon oxide layer (12) and a second silicon nitride layer (13) on the semiconductor substrate (10), and forming a first hole (14) in the silicon oxide layer (12), and forming a second hole (15) in the second silicon nitride layer (13), wherein a diameter D1 of the first hole (14) is equal to a diameter D2 of the second hole (15).

3. The wet etching method for improving feature size consistency as claimed in claim 2, It is characterized in that The etching step comprises: the etching liquid performs side etching on the silicon oxide layer (12), thereby forming a third hole (16) in the silicon oxide layer (12), and the diameter D3 of the third hole (16) is greater than the diameter D2 of the second hole (15).

4. The wet etching method for improving feature size consistency according to claim 1, It is characterized in that The larger the interval time L is, the shorter the etching time t is.