Physical failure analysis method for semiconductor tungsten wire contact window
By using a marker pen to apply C film on the cross-section of the PFA test piece of the tungsten wire contact window, the problem of component structural damage caused by electron beam evaporation was solved and accurate physical failure analysis of the tungsten wire contact window was achieved.
Patent Information
- Application Number
- CN202380024166.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-09-01
- Publication Date
- 2024-10-29
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The existing physical failure analysis method of tungsten wire contact windows may cause the component structure to deform during the carbon plating step, causing damage to originally defect-free locations and affecting the accuracy of subsequent observation steps.
Use a marker pen to coat the cross-section of the PFA test piece to form a C film instead of using the electron beam evaporation method to avoid damage to the component structure.
The marker coating method can ensure the integrity of the component structure, avoid defects in defect-free locations, and improve the accuracy of physical failure analysis.
Smart Images

Figure CN118872037A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of semiconductor integrated circuit manufacturing, and in particular to a physical failure analysis method for a semiconductor tungsten wire contact window. Background Art
[0002] In semiconductor integrated circuit manufacturing, after all manufacturing processes are completed, or after part of the manufacturing process is completed, the wafer needs to be tested by WAT (Wafer Acceptance Test). During the WAT test, if the tungsten wire contact window (WKH) in the wafer is found to be abnormal, it is necessary to perform PFA (Physical Failure Analysis) on the abnormal part of the tungsten wire contact window to find out the cause of the abnormality.
[0003] The existing PFA generally includes the following steps: a cutting step, cutting the part of the wafer that needs to be PFA into a PFA test piece. A coating step, coating a layer of C (carbon) on the cross section of the PFA test piece. An observation step, using a SEM (scanning electron microscope) to observe the cross section of the PFA test piece. Among them, the role of coating a layer of C on the cross section of the PFA test piece is to make the cross section of the PFA test piece conductive, so that in the subsequent steps, the cross section of the PFA test piece can be observed using a SEM (Scanning Electron Microscopy). In addition, for the tungsten wire contact window, by coating C on the cross section of the PFA test piece, the various interfaces of the component structure on the cross section can also be made clearer when observing with a SEM. In the prior art, the E-beam (electron beam evaporation) method is usually used for C coating. However, the use of the E-beam method to coat C may cause deformation of the component structure of the cross section of the tungsten wire contact window (WKH) PFA test piece, causing defects to appear in the position where there were no defects originally, which will interfere with the subsequent observation steps.
[0004] Therefore, a method for accurately performing PFA on the tungsten wire contact window (WKH) is urgently needed without causing damage to the device structure of the cross section of the PFA test piece. Summary of the invention
[0005] The present invention aims to provide a method for accurately performing PFA without damaging the component structure of the cross section of a tungsten wire contact window (WKH) PFA test piece.
[0006] The PFA method of the present invention comprises:
[0007] A cutting step, cutting the portion of the wafer that needs to be subjected to the physical failure analysis into physical failure analysis test pieces;
[0008] a coating step, coating with a marker pen on the cross section of the physical failure analysis specimen where the physical failure analysis is required; and
[0009] The observation step is to observe the cross section using a scanning electron microscope.
[0010] The PFA method provided by the present invention can avoid damage to the component structure of the cross section of the PFA test piece during preparation, thereby enabling accurate PFA. BRIEF DESCRIPTION OF THE DRAWINGS
[0011] Figure 1 is a flow chart of the PFA method of the present invention;
[0012] Figure 2 is a schematic top view of a wafer of the present invention; and
[0013] Figure 3 The PFA test piece of the present invention is Figure 2 Schematic cross-sectional view along the A-A' direction.
[0014] Explanation of symbols
[0015] 1 Wafer
[0016] 2PFA test piece
[0017] 3Tungsten wire contact window
[0018] 4 Cross-sections that require PFA DETAILED DESCRIPTION
[0019] Refer to the following Figures 1 to 3 The PFA method of the present invention is described. Figure 1 As shown, the PFA method of the present invention includes: a cutting step S001, a coating step S002, and an observation step S003. Each step will be described in detail below.
[0020] In the cutting step S001, the portion of the wafer 1 that needs to be subjected to PFA is cut into PFA test pieces 2. Figure 2 As shown, at the location where the abnormal tungsten wire contact window 3 is located, cutting is performed in a direction perpendicular to the wafer surface, and the abnormal tungsten wire contact window 3 and its surrounding parts are cut into PFA test pieces 2. Figure 3 The edge of PFA test piece 2 Figure 2 It should be noted that, for the sake of simplicity, Figure 3In the figure, only one layer is drawn above and below the tungsten wire contact window 3, but in fact, there may be many layers above and below the tungsten wire contact window 3. The PFA test piece 2 can be formed by a cutting method commonly used in the art, which will not be described in detail here.
[0021] In coating step S002, a marker pen is used to coat the cross section 4 of the PFA test piece 2 where PFA is required. Since the ink of the marker pen also contains C, a C film can be formed on the cross section 4 by coating the cross section 4 with the marker pen. This is the same as the effect of plating C on the cross section 4 by the E-beam method. In addition, coating with a marker pen will not cause damage to the component structure of the cross section 4, so defects will not appear in the position where there were no defects originally, so it will not cause interference when using SEM for subsequent observation.
[0022] In the observation step S003, the cross section 4 is observed using a SEM to find out the cause of the abnormality. The method of the observation step S003 is the same as that in the prior art, and thus will not be described in detail.
[0023] The PFA method provided by the present invention can avoid damage to the component structure of the cross section of the PFA test piece during preparation, thereby enabling accurate PFA.
[0024] Although the present invention has been disclosed in the above embodiments, it is not intended to limit the present invention. Any professional and technical personnel in the field may make various necessary changes and modifications without departing from the spirit and scope of the present invention. Therefore, the scope of protection of the present invention shall be based on the scope defined by the attached claims.
Claims
1. A physical failure analysis method for semiconductor tungsten wire contact window, include: Cutting step S001, cutting the portion of the wafer (1) that needs to be subjected to the physical failure analysis into physical failure analysis test pieces (2); A coating step S002, coating with a marker pen on the cross section (4) of the physical failure analysis specimen (2) where the physical failure analysis is to be performed; and Observation step S003: observing the cross section (4) using a scanning electron microscope.
Citation Information
Patent Citations
Method for manufacturing failure analysis sample in interconnection structure
CN102053169A
Preparation method of structure section sample of small-sized wafer sample for observation
CN102426119A
Detection method of high resistance of tungsten contact plug
CN103700603A
Method for preparing semiconductor failure analysis sample
CN103871917A
Analysis method of membrane-electrode assembly using scanning electron microscope
KR1020080103123A