Epitaxial wafer, epitaxial wafer defect evaluation method, epitaxial wafer defect evaluation device, epitaxial wafer defect evaluation equipment and medium

The grid haze map is obtained and divided by particle counters to objectively evaluate the metal aggregation defects of epitaxial wafers, solving the device reliability problems caused by metal diffusion in semiconductor manufacturing, and improving the accuracy and efficiency of evaluation.

CN118888465APending Publication Date: 2024-11-01XIAN ESWIN MATERIAL TECHNOLOGY CO LTD +1
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202410828620.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-25
Publication Date
2024-11-01

AI Technical Summary

Technical Problem

In semiconductor manufacturing processes, high-temperature treatment of epitaxial wafers causes metal elements to diffusion, forming metal aggregation defects, resulting in increased leakage current, reduced oxide breakdown voltage, device corrosion and short circuit, affecting device reliability and safety. The evaluation method relies on manual judgment, and there are problems of misjudgment and inefficiency.

Method used

The haze map is obtained through the particle counter, the haze map is divided into the grid, and the haze map is determined based on the haze maximum value of each grid, providing an objective, accurate and efficient evaluation method.

Benefits of technology

It reduces the misjudgment of manual judgment, improves the evaluation accuracy and efficiency of metal aggregation defects on the surface of epitaxial wafers, and avoids metal aggregation defects entering the back-end semiconductor device manufacturing process.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118888465A_ABST
    Figure CN118888465A_ABST
Patent Text Reader

Abstract

The invention provides an epitaxial wafer, an epitaxial wafer defect evaluation method, an epitaxial wafer defect evaluation device, epitaxial wafer defect evaluation equipment and a medium. The method comprises the following steps: acquiring a haze graph of a to-be-measured epitaxial wafer through a particle counter; dividing the haze map according to a set grid size to obtain a grid haze map of the epitaxial wafer to be measured; and according to the maximum haze value of each grid in the grid haze graph, determining whether the epitaxial wafer to be detected has a metal aggregation type defect caused by metal aggregation or not.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates to the field of semiconductor manufacturing technology, and in particular to an epitaxial wafer and defect evaluation method, device, equipment and medium. Background Art

[0002] In the epitaxial wafer manufacturing process, the high temperature environment of the heat treatment process will cause the metal elements (such as copper Cu and nickel Ni) in the wafer to diffuse to the wafer surface and enrich at the edge or surface of the epitaxial wafer to form circular or semicircular metal aggregation defects. The metal aggregation defects formed by these metal elements are likely to cause at least the following hazards in the back-end semiconductor device manufacturing process: 1. Increased leakage current in the PN structure, reduced oxide breakdown voltage and reduced carrier lifetime. 2. Harmful precipitation will form at the PN junction and Si / SiO2 interface, thereby enhancing the micro-roughness of the substrate surface and affecting the performance and reliability of the device. 3. Cause device corrosion, erosion, electron migration or short circuit, resulting in device failure, affecting the reliability and safety of the final product.

[0003] In order to avoid the above hazards in the back-end semiconductor device manufacturing process, on the one hand, it is necessary to optimize the epitaxial process conditions and reduce the introduction of metal elements. On the other hand, it is necessary to use effective defect assessment methods to prevent epitaxial wafers with metal aggregation defects from flowing into the back-end semiconductor device manufacturing process.

[0004] At present, the evaluation methods for this type of clustered defects mostly rely on the manual judgment of visual inspectors. However, manual judgment by visual inspectors usually leads to misjudgment due to their subjectivity, which reduces the accuracy of the above evaluation process; in addition, manual judgment by visual inspectors is slow and inefficient. Therefore, it is necessary to establish an objective, accurate and efficient abnormality evaluation scheme. Summary of the invention

[0005] The present disclosure provides an evaluation method, device, equipment and medium for an epitaxial wafer and its defects; the metal aggregation type defects caused by metal aggregation on the wafer surface can be objectively, efficiently and accurately evaluated based on a haze map.

[0006] The technical solution of the present disclosure is achieved as follows: In a first aspect, the present disclosure provides a method for evaluating epitaxial wafer defects, the method comprising: Obtaining a haze map of the epitaxial wafer to be tested by a particle counter; Dividing the haze map according to a set grid size to obtain a grid haze map of the epitaxial wafer to be tested; It is determined whether the epitaxial wafer to be tested has metal aggregation type defects caused by metal aggregation according to the maximum value of the haze of each grid in the grid haze map.

[0007] In a second aspect, the present disclosure provides an epitaxial wafer defect evaluation device, the device comprising: an acquisition unit, a division unit and a determination unit; wherein: The acquisition unit is configured to acquire a haze map of the epitaxial wafer to be tested through a particle counter; The dividing unit is configured to divide the haze map according to a set grid size to obtain a grid haze map of the epitaxial wafer to be tested; The determination unit is configured to determine whether the epitaxial wafer to be tested has metal aggregation type defects caused by metal aggregation according to the maximum haze value of each grid in the grid haze map.

[0008] In a third aspect, the present disclosure provides a computing device, comprising: a processor and a memory; the processor is used to execute instructions stored in the memory to implement the epitaxial wafer defect evaluation method as described in the first aspect.

[0009] In a fourth aspect, the present disclosure provides a computer storage medium, wherein the storage medium stores at least one instruction, and the at least one instruction is used to be executed by a processor to implement the epitaxial wafer defect evaluation method as described in the first aspect.

[0010] In a fifth aspect, the present disclosure provides an epitaxial wafer. After the haze map obtained by the particle counter of the epitaxial wafer is divided into a grid haze map according to a set grid size, it is determined that the epitaxial wafer does not have metal aggregation type defects caused by metal aggregation based on the maximum haze value of each grid in the grid haze map.

[0011] The present disclosure provides an evaluation method, device, equipment and medium for epitaxial wafers and their defects; after the haze map of the epitaxial wafer to be tested is divided into grids, the maximum haze value of each grid is used to determine whether the epitaxial wafer to be tested has metal aggregation type defects, thereby proposing an objective metal aggregation type defect evaluation scheme, which reduces the occurrence of misjudgment compared to manual judgment and improves the accuracy and efficiency of the evaluation of metal aggregation type defects on the surface of the epitaxial wafer. BRIEF DESCRIPTION OF THE DRAWINGS

[0012] Figure 1 A schematic flow chart of a method for evaluating epitaxial wafer defects provided in the present invention.

[0013] Figure 2 A haze diagram of an epitaxial wafer with metal aggregation defects provided by the present invention.

[0014] FIG3 (A) is a haze diagram of another epitaxial wafer with metal cluster defects provided by the present disclosure.

[0015] FIG3(B) is a grid haze diagram provided by the present disclosure.

[0016] Figure 4 A schematic flow chart of another epitaxial wafer defect evaluation method provided in the present disclosure.

[0017] Figure 5 A haze diagram of another epitaxial wafer with metal cluster defects provided in the present disclosure.

[0018] Figure 6 Another grid haze map provided for the present disclosure.

[0019] Figure 7 A schematic diagram of the composition of an epitaxial wafer defect evaluation device provided in the present invention.

[0020] Figure 8 A schematic diagram of the structure of a computing device provided by the present disclosure. DETAILED DESCRIPTION

[0021] The technical solutions in the present disclosure will be described clearly and completely below in conjunction with the accompanying drawings in the present disclosure.

[0022] In order to avoid the misjudgment of metal aggregation defects by visual inspectors through manual judgment of metal aggregation defects and improve the objectivity, accuracy and efficiency of abnormality evaluation, the present disclosure provides an evaluation method for epitaxial wafer defects. Figure 1 , the method may include steps S110 to S130.

[0023] In step S110 , a haze map of the epitaxial wafer to be tested is obtained by using a particle counter.

[0024] In the present disclosure, for an epitaxial wafer having metal aggregation defects on the surface, a haze map obtained by particle counter detection is as follows: Figure 2 As shown. Figure 2 In the Haze map shown in , the white dots indicated by the arrows are the areas where metals are concentrated on the surface of the epitaxial wafer. Based on the existence of this area, it can be determined that the epitaxial wafer has metal concentration defects.

[0025] For a particle counter, the images collected may include bright field images and dark field images, and the dark field images can be obtained through three dark field channels. The three dark field channels are the dark-field narrow oblique (DNO) channel, the dark-field wide 1 oblique (DW1O) channel, and the dark-field wide 2 oblique (DW2O) channel. Each of the above channels includes a low-angle light source and a light receiver. The light emitted by the low-angle light source of each channel is incident on the surface of the epitaxial wafer to be tested, and after being reflected and / or scattered by the surface of the epitaxial wafer to be tested, the light receiver receives the reflected and / or scattered radiated light, and forms a haze map of the epitaxial wafer to be tested based on the radiated light.

[0026] In the above three dark field channels, the angle (light receiving angle) at which the light receiver of each dark field channel receives the radiated light is different, wherein the light receiving angle of the light receiver of the DNO channel is higher than that of the light receivers of the DW1O channel and the DW2O channel, and the light receiving angle of the light receiver of the DW1O channel is higher than that of the light receiver of the DW2O channel. It should be noted that in the present disclosure, the light receiving angle is defined based on the surface of the epitaxial wafer to be measured.

[0027] Based on this, in some examples, obtaining a haze map of the epitaxial wafer to be tested by using a particle counter includes: The haze map of the epitaxial wafer to be tested is obtained through the dark field channel in the particle counter.

[0028] For the above example, in detail, obtaining the haze map of the epitaxial wafer to be tested through the dark field channel in the particle counter includes: irradiating incident light from a low-angle light source in a particle counter onto the surface of the epitaxial wafer to be measured; Using any light receiver in the particle counter to receive the incident light and the radiated light from the surface of the epitaxial wafer to be measured; A haze map of the epitaxial wafer to be tested is generated based on the emitted light.

[0029] For the above example and its detailed description, more specifically, among all channels, since the Haze value of the wafer collected by the DW2O channel is the largest, it can more clearly distinguish different Haze values, so that the haze of the wafer surface reflected is more accurate. Therefore, in the present disclosure, the haze map of the wafer to be tested can be obtained through the dark field width 2 tilt channel in the particle counter.

[0030] In step S120 , the haze map is divided according to a set grid size to obtain a grid haze map of the epitaxial wafer to be tested.

[0031] In the present disclosure, in order to determine the area where the Haze value is abnormal from the haze map of the epitaxial wafer to be tested, the haze map of the epitaxial wafer to be tested can be divided into multiple grids of the same size, so that the Haze value of each grid can be used to determine whether the position of the wafer at the grid is the location of the metal aggregation type defect. For example, after the haze map shown in Figure 3 (A) is divided into grids by step S120, a grid haze map as shown in Figure 3 (B) can be obtained. In the present disclosure, the grid size used to divide the grid may include: 2mm×2mm, 3mm×3mm, 5mm×5mm or 10mm×10mm.

[0032] In step S130 , it is determined whether the epitaxial wafer to be tested has metal aggregation type defects caused by metal aggregation according to the maximum haze value of each grid in the grid haze map.

[0033] Regarding step S130 , in some examples, after the haze map is divided into grids according to the grid size in step S120 to obtain the exemplary grid haze map as shown in FIG. 3 (B ), the maximum haze value (Hazemax) in each grid can be obtained.

[0034] Combination Figure 2 As shown in the figure, the haze value of the area with metal aggregation indicated by the black arrow is significantly different from that of other areas. In order to evaluate this difference, the maximum haze value of each grid can be compared with the upper threshold set for characterizing metal aggregation defects. If the maximum haze value of each grid of some grids is greater than the upper threshold, it can be determined that metal aggregation exists in these grids on the wafer surface, and the epitaxial wafer is a wafer with metal aggregation defects.

[0035] pass Figure 1 The technical scheme shown, after dividing the haze map of the epitaxial wafer to be tested into grids, uses the maximum haze value of each grid to determine whether the epitaxial wafer to be tested has metal aggregation type defects, thereby proposing an objective metal aggregation type defect evaluation scheme, which reduces the occurrence of misjudgment compared to manual judgment and improves the accuracy and efficiency of the evaluation of metal aggregation type defects on the surface of the epitaxial wafer.

[0036] based on Figure 2 The technical solution shown in Figure 4 , which shows another method flow for wafer abnormality assessment, the method comprising steps S401 to S406.

[0037] In step S401, a haze map of the epitaxial wafer to be tested is obtained through a dark field channel in a particle counter.

[0038] In step S402, the haze map is divided according to a set grid size to obtain a grid haze map of the epitaxial wafer to be tested.

[0039] It is understandable that the specific implementation details of the above steps S401 and S402 can be referred to the aforementioned Figure 1 The present disclosure does not elaborate on step S110 and step S120 in the technical solution shown.

[0040] In step S403, the maximum haze value of each grid in the grid haze map is obtained.

[0041] It should be noted that since the area occupied by metal aggregation is small, and metal aggregation defects appear as circular or semicircular dots, for each grid, if there is a metal aggregation defect, the area occupied by the defect is likely to occupy only a part of the grid area, or even only 1 to 2 pixels. Based on this, in order to significantly reflect the haze difference between the area where the metal aggregation defect is located and other areas on the surface of the epitaxial wafer, the present disclosure uses the maximum haze value in the grid to determine the metal aggregation defect.

[0042] In step S404, the maximum haze value of each grid is compared with an upper threshold value set for characterizing metal aggregation defects, and the number of grids in the grid haze map whose maximum haze value is greater than or equal to the upper threshold value is obtained.

[0043] In step S405 , when the number of grids is greater than zero, it is determined that metal aggregation defects exist on the surface of the epitaxial wafer to be tested.

[0044] In step S406 , when the number of grids is equal to zero, it is determined that there are no metal aggregation defects on the surface of the epitaxial wafer to be tested.

[0045] It can be understood that for the above steps S405 and S406, when metal aggregation defects exist on the surface of the epitaxial wafer to be tested, the epitaxial wafer should be intercepted in time to avoid flowing into the back-end semiconductor device manufacturing process.

[0046] It should be noted that during the manufacturing process of epitaxial wafers, silicon atoms on the surface will undergo atomic-level rearrangement to form a surface structure that matches the epitaxial layer lattice. Such rearrangement will cause changes in surface morphology, such as the appearance of specific shapes such as " / / "-shaped grooves. These specific morphological changes will produce an interference effect with the light emitted by the light source during the detection process of the particle counter, causing certain wavelengths of light to be enhanced or weakened, ultimately resulting in the formation of a regular pattern of white or other light colors with a more obvious contrast in the Haze map, such as a "four-leaf clover" pattern. However, generally speaking, metal aggregation defects have a higher scattered light intensity due to their higher atomic number (compared to silicon). Based on this, the present disclosure can avoid the situation where the "four-leaf clover" pattern is mistaken for a metal aggregation defect by setting an appropriate upper limit threshold.

[0047] based on Figure 4 The technical solution shown is Figure 5 Taking the Hazemap of an epitaxial wafer with metal cluster defects as an example, the white dotted areas in the Haze map are where the metal cluster defects are located. Figure 5 Divide the grid into 3mm×3mm to obtain Figure 6 After the grid haze map is shown, the maximum haze value of each grid is compared with the upper threshold. Figure 6 In the grid haze diagram shown in the figure, the maximum haze value of the grid pointed out by the arrow is greater than the upper threshold, and the grid is Figure 5 The white dotted area in the middle corresponds to the above-mentioned area. It can be seen that the method for evaluating epitaxial wafer defects proposed in the present invention improves the objectivity, accuracy and efficiency of evaluating metal aggregation defects on the surface of epitaxial wafers compared to manual judgment.

[0048] Based on the same inventive concept as the above technical solution, see Figure 7 , which shows an epitaxial wafer defect evaluation device 70 provided by the present disclosure, the device 70 comprises: an acquisition unit 701, a division unit 702 and a comparison unit 703; wherein, The acquisition unit 701 is configured to acquire a haze map of the epitaxial wafer to be tested through a particle counter; The dividing unit 702 is configured to divide the haze map according to a set grid size to obtain a grid haze map of the epitaxial wafer to be tested; The determination unit 703 is configured to determine whether the epitaxial wafer to be tested has metal aggregation type defects caused by metal aggregation according to the maximum haze value of each grid in the grid haze map.

[0049] In some examples, the acquisition unit 701 is configured to: The haze map of the epitaxial wafer to be tested is obtained through the dark field channel in the particle counter.

[0050] In some examples, the acquisition unit 701 is configured to: irradiating incident light from a low-angle light source in a particle counter onto the surface of the epitaxial wafer to be measured; Using any light receiver in the particle counter to receive the incident light and the radiated light from the surface of the epitaxial wafer to be measured; A haze map of the epitaxial wafer to be tested is generated based on the emitted light.

[0051] In some examples, the determining unit 703 is configured to: Get the maximum value of the haze of each grid in the grid haze map; The maximum haze value of each grid is compared with the upper threshold value set for characterizing metal aggregation defects, and the number of grids whose maximum haze value in the grid haze map is greater than or equal to the upper threshold value is obtained; When the number of grids is greater than zero, it is determined that there are metal aggregation defects on the surface of the epitaxial wafer to be tested; When the number of grids is equal to zero, it is determined that there are no metal aggregation defects on the surface of the epitaxial wafer to be tested.

[0052] In some examples, the grid size includes: 2mm×2mm, 3mm×3mm, 5mm×5mm, or 10mm×10mm.

[0053] Please refer to Figure 8 , which shows a structural block diagram of a computing device provided by an exemplary embodiment of the present disclosure. In some examples, the computing device 80 can be at least one of a smart phone, a smart watch, a desktop computer, a laptop, a virtual reality terminal, an augmented reality terminal, a wireless terminal, and a laptop portable computer. The computing device 80 has a communication function and can access a wired network or a wireless network. The computing device 80 can generally refer to one of a plurality of terminals, and those skilled in the art can know that the number of the above terminals can be more or less. In some examples, the computing device 80 can receive haze map data of the epitaxial wafer to be tested obtained by a particle counter based on the wired network or wireless network to which it is connected. It can be understood that the computing device 80 undertakes the calculation and processing work of the technical solution of the present disclosure, and the present disclosure does not limit this.

[0054] like Figure 8 As shown, the computing device in the present disclosure may include one or more of the following components: a processor 810 and a memory 820 .

[0055] Optionally, the processor 810 uses various interfaces and lines to connect various parts of the entire computing device, and executes various functions of the computing device and processes data by running or executing instructions, programs, code sets or instruction sets stored in the memory 820, and calling data stored in the memory 820. Optionally, the processor 810 can be implemented in at least one hardware form of digital signal processing (DSP), field-programmable gate array (FPGA), and programmable logic array (PLA). The processor 810 can integrate one or a combination of a central processing unit (CPU), a graphics processing unit (GPU), a neural network processor (NPU), and a baseband chip. Among them, the CPU mainly processes the operating system, user interface, and application programs; the GPU is responsible for rendering and drawing the content that needs to be displayed on the touch display; the NPU is used to implement artificial intelligence (AI) functions; and the baseband chip is used to process wireless communications. It is understandable that the above baseband chip may not be integrated into the processor 810, but may be implemented by a separate chip.

[0056] The memory 820 may include a random access memory (RAM) or a read-only memory (ROM). Optionally, the memory 820 includes a non-transitory computer-readable storage medium. The memory 820 may be used to store instructions, programs, codes, code sets, or instruction sets. The memory 820 may include a program storage area and a data storage area, wherein the program storage area may store instructions for implementing an operating system, instructions for at least one function (such as a touch function, a sound playback function, an image playback function, etc.), instructions for implementing the above various method embodiments, etc.; the data storage area may store data created according to the use of the computing device, etc.

[0057] In addition, those skilled in the art can understand that the structure of the computing device shown in the above drawings does not constitute a limitation on the computing device, and the computing device may include more or fewer components than shown in the figure, or combine certain components, or arrange the components differently. For example, the computing device also includes a display screen, a camera assembly, a microphone, a speaker, a radio frequency circuit, an input unit, a sensor (such as an acceleration sensor, an angular velocity sensor, a light sensor, etc.), an audio circuit, a WiFi module, a power supply, a Bluetooth module and other components, which will not be described in detail here.

[0058] The present disclosure also provides a computer-readable storage medium storing at least one instruction, wherein the at least one instruction is used to be executed by a processor to implement the epitaxial wafer defect evaluation method described in the above embodiments.

[0059] The present disclosure also provides a computer program product, which includes computer instructions stored in a computer-readable storage medium; a processor of a computing device reads the computer instructions from the computer-readable storage medium, and the processor executes the computer instructions, so that the computing device executes to implement the epitaxial wafer defect evaluation method described in the above-mentioned embodiments.

[0060] The present disclosure also provides a wafer, which is evaluated by the epitaxial wafer defect evaluation method described in the above embodiments to determine that there are no metal aggregation defects.

[0061] Specifically, for the above-mentioned wafer, after the haze map obtained by the particle counter of the wafer is divided into a grid haze map according to a set grid size, it is determined based on the maximum haze value of each grid in the grid haze map that the epitaxial wafer does not have metal aggregation type defects caused by metal aggregation.

[0062] In some examples, in the grid haze map, the maximum haze values ​​of all grids are less than a set upper threshold for characterizing metal aggregation defects.

[0063] Those skilled in the art should be aware that in one or more of the above examples, the functions described in the present disclosure can be implemented using hardware, software, firmware, or any combination thereof. When implemented using software, these functions can be stored in a computer-readable medium or transmitted as one or more instructions or codes on a computer-readable medium. Computer-readable media include computer storage media and communication media, wherein communication media include any media that facilitates the transmission of computer programs from one place to another. Storage media can be any available media that can be accessed by a general or special-purpose computer.

[0064] It should be noted that the technical solutions described in the present disclosure can be combined arbitrarily without conflict.

[0065] The above is only a specific embodiment of the present invention, but the protection scope of the present invention is not limited thereto. Any person skilled in the art can easily think of changes or substitutions within the technical scope disclosed by the present invention, which should be included in the protection scope of the present invention. Therefore, the protection scope of the present invention should be based on the protection scope of the claims.

Claims

1. A method for evaluating epitaxial wafer defects, It is characterized in that The evaluation methods include: Obtaining a haze map of the epitaxial wafer to be tested by a particle counter; Dividing the haze map according to a set grid size to obtain a grid haze map of the epitaxial wafer to be tested; It is determined whether the epitaxial wafer to be tested has metal aggregation type defects caused by metal aggregation according to the maximum value of the haze of each grid in the grid haze map.

2. The method according to claim 1, It is characterized in that The method of obtaining a haze map of the epitaxial wafer to be tested by using a particle counter comprises: A haze map of the epitaxial wafer to be tested is obtained through a dark field channel in the particle counter.

3. The method according to claim 2, It is characterized in that The step of obtaining a haze map of the epitaxial wafer to be tested through a dark field channel in the particle counter comprises: irradiating incident light from a low-angle light source in the particle counter onto the surface of the epitaxial wafer to be tested; Using any light receiver in the particle counter to receive the incident light emitted from the surface of the epitaxial wafer to be measured; A haze map of the epitaxial wafer to be tested is generated according to the radiated light.

4. The method according to any one of claims 1 to 3, It is characterized in that The step of determining whether the epitaxial wafer to be tested has a metal aggregation defect caused by metal aggregation according to the maximum value of the haze of each grid in the grid haze map comprises: Obtaining the maximum value of the haze of each grid in the grid haze map; Compare the maximum haze value of each grid with the set upper limit threshold for characterizing metal aggregation defects, and obtain the number of grids in the grid haze map whose maximum haze value is greater than or equal to the upper limit threshold; When the number of grids is greater than zero, it is determined that the metal aggregation type defect exists on the surface of the epitaxial wafer to be tested; When the number of grids is equal to zero, it is determined that the metal aggregation type defects do not exist on the surface of the epitaxial wafer to be tested.

5. The method according to claim 1, It is characterized in that The grid sizes include: 2mm×2mm, 3mm×3mm, 5mm×5mm or 10mm×10mm.

6. An evaluation device for epitaxial wafer defects, It is characterized in that The device comprises: an acquisition unit, a division unit and a determination unit; wherein, The acquisition unit is configured to acquire a haze map of the epitaxial wafer to be tested through a particle counter; The dividing unit is configured to divide the haze map according to a set grid size to obtain a grid haze map of the epitaxial wafer to be tested; The determination unit is configured to determine whether the epitaxial wafer to be tested has metal aggregation type defects caused by metal aggregation according to the maximum haze value of each grid in the grid haze map.

7. A computing device, It is characterized in that The computing device comprises: a processor and a memory; the processor is used to execute instructions stored in the memory to implement the epitaxial wafer defect evaluation method as described in any one of claims 1 to 6.

8. A computer storage medium, It is characterized in that The storage medium stores at least one instruction, and the at least one instruction is used to be executed by a processor to implement the epitaxial wafer defect evaluation method according to any one of claims 1 to 6.

9. An epitaxial wafer, It is characterized in that After dividing the haze map obtained by the particle counter of the epitaxial wafer into a grid haze map according to a set grid size, it is determined that the epitaxial wafer does not have metal aggregation type defects caused by metal aggregation based on the maximum haze value of each grid in the grid haze map.

10. The epitaxial wafer according to claim 10, It is characterized in that In the grid haze map, the maximum haze values ​​of all grids are less than the set upper limit threshold for characterizing metal aggregation defects.

Citation Information

Cited By

  • Visual detection method for heavy metal nickel pollution of silicon wafer

    CN121499432A