Preparation process of defoaming agent

Through the preparation of polyoxypropyl polyoxyethylglycerol ether, the problems of slow defoaming speed and poor storage stability of the defoaming agent are solved, the defoaming efficiency and scope of application are improved, and it is suitable for a variety of industrial production processes.

CN118892674APending Publication Date: 2024-11-05GUIZHOU ZHICHENG NEW MATERIAL TECHNOLOGY CO LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202410938978.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-12
Publication Date
2024-11-05

AI Technical Summary

Technical Problem

The existing defoaming agents are slow to defoam, difficult to dissolve in water, and cannot effectively drive away the foam inside the liquid. The oil is not resistant to storage and easily deteriorate, affecting the defoaming performance.

Method used

Polyoxypropyl polyoxyethylglycerol ether is used as the starting agent to initiate the polymerization of propylene oxide and ethylene oxide through a catalyst, and esterified with C10-18 fatty acids to prepare a longer hydrophilic and oleophilic The chain defoaming agent improves the dispersion and adsorption ability of the defoaming agent by adjusting the esterification degree and molecular weight.

Benefits of technology

It improves the defoaming efficiency and scope of application of the defoaming agent, enhances the dispersion in the water phase and the adsorption capacity of the liquid film, solves the problems of slow defoaming speed and storage stability, and is suitable for a variety of industrial production processes.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118892674A_ABST
    Figure CN118892674A_ABST
Patent Text Reader

Abstract

The invention discloses a preparation process of a defoaming agent, and relates to the technical field of defoaming agents. Comprising the four steps that polyglycerol serves as an initiator, polymerization of epoxypropane and ethylene oxide is initiated in the presence of a catalyst, polyoxypropyl polyoxyethyl glyceryl ether is obtained, then terminal hydroxyl of the polyoxypropyl polyoxyethyl glyceryl ether is esterified, the defoaming agent is obtained, the preparation method of the defoaming agent is simple, and residues do not need to be treated. According to the preparation process of the defoaming agent, the prepared polyoxypropyl polyoxyethyl glyceryl ether has longer hydrophilic chain links and longer oleophylic chain links in molecules, the viscosity is low, the dispersion of the defoaming agent in a water phase and the adsorption on a liquid film of foam are facilitated, the defoaming efficiency is improved, and by changing the amount and esterification degree of epoxypropane and ethylene oxide, the defoaming effect of the defoaming agent is improved. The hydrophilic-hydrophobic balance value (namely HLB value) and molecular weight of the defoaming agent can be conveniently adjusted, so that the application range of the defoaming agent is enlarged, and the defoaming agent is suitable for most production processes needing defoaming.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of defoamers, in particular to a preparation process of a defoamer. Background Art

[0002] With the rapid development of science and technology, all industries involving stirring in industry will be accompanied by the generation of foam, such as papermaking, ink, coating, fermentation, printing and dyeing industries. Foam is a coarse dispersion of gas in liquid. On the one hand, it will greatly limit industrial production capacity; on the other hand, it will cause waste of raw materials and products, affecting product quality and performance. In industry, defoamers are usually added to the reaction system to eliminate and inhibit the generation of foam. The functions of defoamers are divided into defoaming and foam suppression. After the foam is generated, when the defoamer contacts the foam, it immediately reacts with the hydrophobic segment molecules on the surface of the foam to form a double film layer. The surface tension of the defoamer is very low, and being pulled by the surrounding foaming film layer with high surface tension will cause an imbalance in the stress of the bubble, thereby causing the bubble to burst. If the foam has not yet been generated, the defoamer can penetrate into the system that is about to foam in the form of particles, destroying the elastic film of the bubble, thereby inhibiting its formation.

[0003] The invention with publication number CN108310813A discloses a method for preparing a defoamer, in which nano-silica is prepared using tetraethyl orthosilicate as a raw material. However, since it has abundant hydrophilic groups -OH, it is easy to agglomerate under the action of a large number of hydrogen bonds, thereby reducing the stability of the defoamer. Polydimethylsiloxane is loaded on the nano-silica, which can solve the problem of easy agglomeration of nano-silica, enhance its ability to disperse and increase the viscosity of the main components of the defoamer in the defoamer, and improve the emulsification effect.

[0004] As shown in the above invention, the purpose of the existing defoaming agent preparation method is generally to improve the dispersion, viscosity increasing and emulsification effects of oil-based defoaming agents, but it does not solve the problem of slow defoaming speed of existing defoaming agents. In addition, oil-based defoaming agents are difficult to dissolve in water and only have a defoaming effect on the foam on the surface of the liquid, and cannot drive away or eliminate the foam dispersed in the liquid. In addition, oils are not resistant to storage and are easily rancid and deteriorated, which affects the defoaming performance. Summary of the invention

[0005] In view of the deficiencies of the prior art, the present invention provides a preparation process of a defoaming agent to solve the existing problems.

[0006] To achieve the above object, the present invention is implemented by the following technical scheme: The preparation process of the defoaming agent comprises the following steps:

[0007] Step 1: Add sodium tripolyphosphate, tributyl phosphate and polystyrene into a reaction kettle, heat the reaction kettle, and stir while heating for 20-40 minutes at a stirring speed of 100-155 r / min;

[0008] Step 2: Add dimethyl silicone oil, linear oil, liquid paraffin and glycerol into the reactor in sequence, stir at a constant temperature of 80-100 degrees Celsius for 30 minutes, and the stirring speed is 250-300r / min;

[0009] Step 3: Put polyoxypropyl polyoxyethyl glycerol ether and C10-18 fatty acid into a reaction kettle, stir under normal pressure, control the temperature at 40-200° C., and control the time at 2-120 min to complete the esterification reaction;

[0010] Step 4: Cool the above reactants to about 30-70°C, add stabilizer, emulsifier and dispersant respectively, stir at 20-90°C for 20-80 minutes, and you can get a colorless to yellow liquid defoamer product with a pH value of 2-8 and a density of 0.2-1.

[0011] Preferably, the mass ratio of the sodium tripolyphosphate, tributyl phosphate, polystyrene, dimethyl silicone oil, linear grease, liquid paraffin, glycerol, polyoxypropyl polyoxyethyl glycerol ether, C10-18 fatty acid, stabilizer, emulsifier and dispersant is 3-4: 100-150: 50-60: 120-140: 20-30: 60-80: 5-8: 600-700: 200-300: 10-13: 3-5: 30-50.

[0012] Preferably, the preparation method of the polyoxypropyl glyceryl ether comprises the following steps:

[0013] S1, dissolving the catalyst in water, mixing with glycerol, reacting at 110-200° C. for 0.5-2 hours, and removing free water in the reaction system;

[0014] S2, reacting at 235-280° C. for 2.5-4.5 hours, removing the water generated by the reaction, and obtaining polyglycerol with a relatively uniform polymerization degree distribution and an average polymerization degree of 2-15;

[0015] S3, adding propylene oxide and ethylene oxide to the generated polyglycerol, and causing a ring-opening polymerization reaction at 80-140° C. under the catalysis of the same catalyst as step S1 to obtain polyoxypropyl polyoxyethyl glycerol ether.

[0016] Preferably, the mass ratio of the polyoxypropyl polyoxyethyl glyceryl ether to the C10-18 fatty acid is adjusted so that the degree of esterification of the polyoxypropyl glyceryl ether is 30% to 700%, where the degree of esterification refers to the ratio of the number of esterified hydroxyl groups to the total number of hydroxyl groups multiplied by 100%.

[0017] Preferably, the C10-18 fatty acid can be one or more of any straight-chain, branched-chain, saturated, or unsaturated fatty acids.

[0018] Preferably, the stabilizer is any one of sodium polyacrylate, methyl / hydroxypropyl cellulose, and sodium carboxymethyl cellulose.

[0019] Preferably, the dispersant is a polymer microsphere emulsion with a core-shell structure, the shell is polymerized with a hydroxyl acrylic monomer, the core is polystyrene, the polymer microsphere has a particle size of 150-350nm and a molecular weight of 20,000-300,000.

[0020] Preferably, the emulsifier is one of alkyl sulfates, alkyl ether sulfates, alkyl phosphates, alkyl amide sulfonates, octadecanoates, dodecanoates, polyoxyethylene alkyl ethers, polyoxyethylene polyol ethers, and polyoxyethylene polyoxypropylene block copolymers.

[0021] Preferably, the catalyst used in the preparation process of the polyoxypropyl glyceryl ether is one of NaOH, KOH, a double metal cyanide complex catalyst, and a phosphine cyanide catalyst.

[0022] Beneficial Effects

[0023] The present invention provides a preparation process of a defoaming agent. Compared with the prior art, the present invention has the following beneficial effects:

[0024] 1. The preparation process of the defoamer is to use polyglycerol as an initiator to initiate the polymerization of propylene oxide and ethylene oxide in the presence of a catalyst to obtain polyoxypropyl polyoxyethyl glyceryl ether, and then esterify the terminal hydroxyl groups of the polyoxypropyl polyoxyethyl glyceryl ether to obtain the defoamer. The preparation method of the defoamer is simple and does not require the treatment of residues.

[0025] 2. The polyoxypropyl polyoxyethyl glycerol ether prepared by the preparation process of the defoamer has longer hydrophilic chain segments and longer lipophilic chain segments in its molecules and low viscosity, which is conducive to the dispersion of the defoamer in the aqueous phase and adsorption on the liquid film of the foam, thereby improving the defoaming efficiency; at the same time, by changing the amount of propylene oxide and ethylene oxide and the degree of esterification, the hydrophilic-hydrophobic balance value (i.e., HLB value) and molecular weight of the defoamer can be conveniently adjusted, thereby expanding the application scope of the defoamer and being suitable for most production processes requiring defoaming. BRIEF DESCRIPTION OF THE DRAWINGS

[0026] Figure 1 It is a schematic diagram of the method flow of the present invention;

[0027] Figure 2 The present invention is a schematic diagram of the preparation process of polyoxypropyl glyceryl ether. DETAILED DESCRIPTION

[0028] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0029] The present invention provides Figure 1-2 The technical solution shown:

[0030] The first implementation method:

[0031] A preparation process of a defoamer comprises the following steps:

[0032] Step 1: Add 3 parts of sodium tripolyphosphate, 100 parts of tributyl phosphate, and 50 parts of polystyrene into a reactor, heat the reactor, and stir while heating for 20-40 minutes at a stirring speed of 100-155 r / min;

[0033] Step 2: Add 120 parts of dimethyl silicone oil, 20 parts of straight-chain oil, 60 parts of liquid paraffin and 5 parts of glycerol into the reactor in sequence, and stir at a constant temperature of 80 degrees Celsius for 30 minutes at a stirring speed of 250 r / min;

[0034] Step 3: Put 600 parts of polyoxypropyl polyoxyethyl glycerol ether and 200 parts of C10-18 fatty acid into a reaction kettle, stir under normal pressure, control the temperature at 40°C, and control the time at 2 minutes to complete the esterification reaction;

[0035] Step 4: Cool the above reactants to about 30°C, add 10 parts of stabilizer, 3 parts of emulsifier and 30 parts of dispersant respectively, stir at 20°C for 20 minutes, and you can get a colorless to yellow liquid defoamer product with a pH value of 2 and a density of 0.2.

[0036] The preparation method of the above-mentioned polyoxypropyl glyceryl ether comprises the following steps:

[0037] S1, dissolving the catalyst in water, mixing with glycerol, reacting at 110° C. for 0.5 hours to remove free water in the reaction system;

[0038] S2, reacting at 235° C. for 2.5 hours, removing the water generated by the reaction, and obtaining polyglycerol with a relatively uniform degree of polymerization and an average degree of polymerization of 2;

[0039] S3, adding propylene oxide and ethylene oxide to the generated polyglycerol, and causing a ring-opening polymerization reaction at 80° C. under the catalysis of the same catalyst as step S1 to obtain polyoxypropyl polyoxyethyl glycerol ether.

[0040] The mass ratio of the polyoxypropyl polyoxyethyl glyceryl ether to the C10-18 fatty acid is adjusted according to the esterification degree of the polyoxypropyl glyceryl ether being 30%, the esterification degree referring to the ratio of the number of esterified hydroxyl groups to the total number of hydroxyl groups multiplied by 100%, and the catalyst is one of NaOH, KOH, a double metal cyanide complex catalyst, and a phosphine cyanide catalyst.

[0041] The above-mentioned C10-18 fatty acid can be one or more of any straight chain, branched chain, saturated and unsaturated fatty acids. The dispersant is a polymer microsphere emulsion with a core-shell structure. The shell is polymerized with a hydroxyl acrylic monomer, and the core is polystyrene. The polymer microsphere has a particle size of 150nm and a molecular weight of 15. The emulsifier is one of alkyl sulfate, alkyl ether sulfate, alkyl phosphate, alkyl amide sulfonate, octadecanoate, dodecanoate, polyoxyethylene alkyl ether, polyoxyethylene polyol ether, and polyoxyethylene polyoxypropylene block copolymer.

[0042] The second implementation method:

[0043] A preparation process of a defoamer comprises the following steps:

[0044] Step 1: Add 4 parts of sodium tripolyphosphate, 130 parts of tributyl phosphate, and 55 parts of polystyrene into a reactor, heat the reactor, and stir while heating for 30 minutes at a stirring speed of 130 minutes;

[0045] Step 2: 130 parts of dimethyl silicone oil, 25 parts of straight-chain oil, 70 parts of liquid paraffin and 6 parts of glycerol were added to the reaction kettle in sequence, and stirred at a constant temperature of 90 degrees Celsius for 30 minutes at a stirring speed of 270 r / min;

[0046] Step 3: 650 parts of polyoxypropyl polyoxyethyl glyceryl ether and 250 parts of C10-18 fatty acid are placed in a reaction kettle, stirred under normal pressure, the temperature is controlled at 100° C., and the time is controlled at 60 minutes to complete the esterification reaction;

[0047] Step 4: Cool the above reactants to about 50°C, add 12 parts of stabilizer, 4 parts of emulsifier and 40 parts of dispersant respectively, stir at 60°C for 50 minutes, and you can get a colorless to yellow liquid defoamer product with a pH value of 5 and a density of 0.6.

[0048] The preparation method of the above-mentioned polyoxypropyl glyceryl ether comprises the following steps:

[0049] S1, dissolving the catalyst in water, mixing with glycerol, reacting at 160° C. for 1.2 hours to remove free water in the reaction system;

[0050] S2, reacting at 250° C. for 3.5 hours, removing the water generated by the reaction, and obtaining polyglycerol with a relatively uniform polymerization degree distribution and an average polymerization degree of 9;

[0051] S3, adding propylene oxide and ethylene oxide to the generated polyglycerol, and causing a ring-opening polymerization reaction at 110° C. under the catalysis of the same catalyst as step S1 to obtain polyoxypropyl polyoxyethyl glycerol ether.

[0052] The mass ratio of the polyoxypropyl polyoxyethyl glyceryl ether to the C10-18 fatty acid is adjusted according to the esterification degree of the polyoxypropyl glyceryl ether being 70%, the esterification degree referring to the ratio of the number of esterified hydroxyl groups to the total number of hydroxyl groups multiplied by 100%, and the catalyst is one of NaOH, KOH, a double metal cyanide complex catalyst, and a phosphine cyanide catalyst.

[0053] The above-mentioned C10-18 fatty acid can be one or more of any straight chain, branched chain, saturated and unsaturated fatty acids. The dispersant is a polymer microsphere emulsion with a core-shell structure. The shell is polymerized with a hydroxyl acrylic acid monomer, and the core is polystyrene. The polymer microsphere has a particle size of 200nm and a molecular weight of 150,000. The emulsifier is one of alkyl sulfates, alkyl ether sulfates, alkyl phosphates, alkyl amide sulfonates, octadecanoates, dodecanoates, polyoxyethylene alkyl ethers, polyoxyethylene polyol ethers, and polyoxyethylene polyoxypropylene block copolymers.

[0054] The third implementation method:

[0055] A preparation process of a defoamer comprises the following steps:

[0056] Step 1: Add 4 parts of sodium tripolyphosphate, 150 parts of tributyl phosphate and 60 parts of polystyrene into a reactor, heat the reactor, and stir while heating for 40 minutes at a stirring speed of 155 r / min;

[0057] Step 2: 140 parts of dimethyl silicone oil, 30 parts of straight-chain oil, 80 parts of liquid paraffin and 8 parts of glycerol were added to the reactor in sequence, and stirred at a constant temperature of 100 degrees Celsius for 30 minutes at a stirring speed of 300 r / min;

[0058] Step 3: 700 parts of polyoxypropyl polyoxyethyl glycerol ether and 300 parts of C10-18 fatty acid are placed in a reaction kettle, stirred under normal pressure, the temperature is controlled at 200° C., and the time is controlled at 120 min to complete the esterification reaction;

[0059] Step 4: Cool the above reactants to about 70°C, add 13 parts of stabilizer, 5 parts of emulsifier and 50 parts of dispersant respectively, stir at 90°C for 80 minutes, and you can get a colorless to yellow liquid defoamer product with a pH value of 8 and a density of 1.

[0060] The preparation method of the above-mentioned polyoxypropyl glyceryl ether comprises the following steps:

[0061] S1, dissolving the catalyst in water, mixing with glycerol, reacting at 200° C. for 2 hours to remove free water in the reaction system;

[0062] S2, reacting at 280° C. for 4.5 hours, removing the water generated by the reaction, and obtaining polyglycerol with a relatively uniform polymerization degree distribution and an average polymerization degree of 15;

[0063] S3, adding propylene oxide and ethylene oxide to the generated polyglycerol, and causing a ring-opening polymerization reaction at 140° C. under the catalysis of the same catalyst as step S1 to obtain polyoxypropyl polyoxyethyl glycerol ether.

[0064] The mass ratio of the polyoxypropyl polyoxyethyl glyceryl ether to the C10-18 fatty acid is adjusted based on the esterification degree of the polyoxypropyl glyceryl ether being 100%, the esterification degree referring to the ratio of the number of esterified hydroxyl groups to the total number of hydroxyl groups multiplied by 100%, and the catalyst is one of NaOH, KOH, a double metal cyanide complex catalyst, and a phosphine cyanide catalyst.

[0065] The above-mentioned C10-18 fatty acid can be one or more of any straight chain, branched chain, saturated and unsaturated fatty acids. The dispersant is a polymer microsphere emulsion with a core-shell structure. The shell is polymerized with a hydroxyl acrylic acid monomer, and the core is polystyrene. The polymer microsphere has a particle size of 200nm and a molecular weight of 150,000. The emulsifier is one of alkyl sulfates, alkyl ether sulfates, alkyl phosphates, alkyl amide sulfonates, octadecanoates, dodecanoates, polyoxyethylene alkyl ethers, polyoxyethylene polyol ethers, and polyoxyethylene polyoxypropylene block copolymers.

[0066] The defoaming effect test was carried out on the defoaming agents prepared in the above three embodiments:

[0067] Test method: Add 1000ml of foaming medium and a certain amount of defoamer into a 2500ml measuring cylinder equipped with a high-speed stirrer, start stirring and start timing, and record the time when the foam height reaches 500ml, 1000ml, and 1500ml. Under the same conditions, the longer the time, the better the defoaming effect.

[0068] The test results are shown in the following table (the percentages in the table are by mass):

[0069]

[0070] In summary, the above three embodiments can all prepare defoaming agents. Combined with the data in the above table, it can be seen that the defoaming agent prepared by the second implementation method has the best effect.

[0071] Meanwhile, the contents not described in detail in this specification belong to the prior art known to those skilled in the art, and the model parameters of each electrical appliance are not specifically limited, and conventional equipment can be used.

[0072] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device.

[0073] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A process for preparing a defoaming agent, characterized in that: The following steps are involved: Step 1: Add sodium tripolyphosphate, tributyl phosphate and polystyrene into a reaction kettle, heat the reaction kettle, and stir while heating for 20-40 minutes at a stirring speed of 100-155 r / min; Step 2: Add dimethyl silicone oil, linear oil, liquid paraffin and glycerol into the reactor in sequence, stir at a constant temperature of 80-100 degrees Celsius for 30 minutes, and the stirring speed is 250-300r / min; Step 3: Put polyoxypropyl polyoxyethyl glycerol ether and C10-18 fatty acid into a reaction kettle, stir under normal pressure, control the temperature at 40-200° C., and control the time at 2-120 min to complete the esterification reaction; Step 4: Cool the above reactants to about 30-70°C, add stabilizer, emulsifier and dispersant respectively, stir at 20-90°C for 20-80 minutes, and you can get a colorless to yellow liquid defoamer product with a pH value of 2-8 and a density of 0.2-1.

2. The preparation process of a defoamer according to claim 1, characterized in that: The mass ratio of the sodium tripolyphosphate, tributyl phosphate, polystyrene, dimethyl silicone oil, straight-chain oil, liquid paraffin, glycerol, polyoxypropyl polyoxyethyl glycerol ether, C10-18 fatty acid, stabilizer, emulsifier and dispersant is 3-4: 100-150: 50-60: 120-140: 20-30: 60-80: 5-8: 600-700: 200-300: 10-13: 3-5: 30-50.

3. The preparation process of a defoamer according to claim 1, characterized in that: The preparation method of the polyoxypropyl glyceryl ether comprises the following steps: S1, dissolving the catalyst in water, mixing with glycerol, reacting at 110-200° C. for 0.5-2 hours, and removing free water in the reaction system; S2, reacting at 235-280° C. for 2.5-4.5 hours, removing the water generated by the reaction, and obtaining polyglycerol with a relatively uniform polymerization degree distribution and an average polymerization degree of 2-15; S3, adding propylene oxide and ethylene oxide to the generated polyglycerol, and causing a ring-opening polymerization reaction at 80-140° C. under the catalysis of the same catalyst as step S1 to obtain polyoxypropyl polyoxyethyl glycerol ether.

4. The preparation process of a defoamer according to claim 1, characterized in that: The mass ratio of the polyoxypropyl polyoxyethyl glyceryl ether to the C10-18 fatty acid is adjusted according to the esterification degree of the polyoxypropyl glyceryl ether being 30% to 100%, wherein the esterification degree refers to the ratio of the number of esterified hydroxyl groups to the total number of hydroxyl groups multiplied by 100%.

5. The preparation process of a defoamer according to claim 1, characterized in that: The C10-18 fatty acid is any one or more of straight chain, branched chain, saturated and unsaturated fatty acids.

6. The preparation process of a defoamer according to claim 1, characterized in that: The stabilizer is any one of sodium polyacrylate, methyl / hydroxypropyl cellulose, and sodium carboxymethyl cellulose.

7. The preparation process of a defoamer according to claim 1, characterized in that: The dispersant is a polymer microsphere emulsion with a core-shell structure, the shell is polymerized with a hydroxyl acrylic acid monomer, the core is polystyrene, the particle size of the polymer microsphere is 150-350nm, and the molecular weight is 20,000-300,000.

8. The preparation process of a defoamer according to claim 1, characterized in that: The emulsifier is one of alkyl sulfate, alkyl ether sulfate, alkyl phosphate, alkyl amide sulfonate, octadecanoate, dodecanoate, polyoxyethylene alkyl ether, polyoxyethylene polyol ether, and polyoxyethylene polyoxypropylene block copolymer.

9. The preparation process of a defoamer according to claim 3, characterized in that: The catalyst used in the preparation process of the polyoxypropyl glyceryl ether is one of NaOH, KOH, a double metal cyanide complex catalyst and a phosphine cyanide catalyst.

Citation Information

Patent Citations

  • Preparation method of defoaming agent

    CN108310813A

  • Method for preparing foam killer

    CN101376089A

  • High-carbon fatty acid terminated polyether ester defoaming agent for papermaking

    CN104480787A

  • Polyether silicone oil triglyceride antifoaming agent and preparation method thereof

    CN105498302A

  • Defoaming agent with fast defoaming speed and preparation method thereof

    CN110559696A