Ultrathin blue glass infrared current-carrying optical filter

By adjusting the glass raw materials and processes, a 0.2mm thick blue glass filter was prepared, which solved the problem of image quality degradation in the camera of traditional infrared filters, achieved efficient infrared light absorption and transmittance improvement, and improved the product's Service life and scope of application.

CN118894645APending Publication Date: 2024-11-05CHANGCHUN UNIV OF SCI & TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202310486574.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-05-04
Publication Date
2024-11-05

AI Technical Summary

Technical Problem

Traditional infrared filters are difficult to effectively remove infrared light in cameras, resulting in a decline in image quality. The stability and customization requirements of IR Coating coatings limit the service life and scope of application of the product.

Method used

By adjusting the glass raw materials and composition, a 0.2mm thick blue glass filter was prepared, using melting and annealing technology, combined with cutting, grinding and polishing, the infrared absorption performance and transmittance were improved, and the wavelength interval of 200 was tested using a spectrophotometer. —1100nm transmittance.

Benefits of technology

It achieves high transmittance in the 400-600nm band and low transmittance in the 700nm band, effectively absorbs infrared light, improves image quality and service life, and has a wider range of applications.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure FT_1
    Figure FT_1
Patent Text Reader

Abstract

The invention relates to ultra-thin blue glass capable of being used for an infrared current-carrying optical filter. The ultra-thin blue glass is prepared by adopting a melting quenching method. The glass comprises the following components in percentage by mole: 45% of P2O, 5%-10% of B2O3, 3%-20% of BaO-10% of Na2O, 10% of CuO-5% of ZnO. The thickness of the prepared blue glass infrared current-carrying optical filter is 0.2 mm, the average transmittance of the blue glass infrared current-carrying optical filter in the wave band of 400-600 nm is larger than 83%, the transmittance of the blue glass infrared current-carrying optical filter in the wave band of 700 nm or above is lower than 1%, and absorption of infrared light is effectively achieved. Compared with the existing blue glass optical filter, the infrared light filtering effect is obviously improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to an ultra-thin blue glass infrared current-carrying filter. Background Art

[0002] With the development and progress of the optical industry, the competition of electronic products is becoming increasingly fierce. In order to improve the image quality of electronic camera products, attempts have been made to introduce "blue glass filters" into cameras. Since then, all high-end devices equipped with 8 million pixels or more, such as mobile phones, digital cameras and rangefinders, have begun to popularize cameras with built-in blue glass filters. Among them, mobile phone cameras generally use CCD or CMOS sensors, which can easily capture visible light and some infrared light. When different light enters the camera at the same time, both visible light and infrared light will form images on the target surface after refraction through the lens. Among them, visible light will present a color image, while infrared light will present a black and white image. When visible light is focused into a clear image, infrared light will form a virtual image on the target surface, affecting the image quality.

[0003] In order to prevent infrared light from forming a virtual image on the target surface, the traditional method is to filter out infrared light through IR Coating or adding filters to obtain a clearer image. IR Coating filters out infrared light by reflection, but its disadvantage is that the stability of the film quality has a huge impact on product quality and product life, and IR Coating needs to be customized "one-to-one" for sensors of different specifications to obtain better imaging effects.

[0004] Blue glass filters are not restricted by the above conditions. They have high transmittance in the visible light band and can effectively absorb infrared light above 630nm. They also have good mechanical properties and chemical stability. Therefore, as an infrared current filter, blue glass performs better in service life and application range. Summary of the invention

[0005] The present invention aims at the application of blue filters in cameras. By adjusting the glass raw materials and composition, a 0.2mm thick blue glass filter is obtained, which effectively improves the infrared absorption performance of traditional filters and improves the transmittance performance of the filter in the 400-600nm band.

[0006] Technical solution: The present invention relates to an ultra-thin blue glass infrared current-carrying filter, and the preparation method thereof comprises the following steps: 1) Weigh the required raw materials in grams according to the molar composition percentage and grind and mix them thoroughly; 2) Add the mixed raw materials into the preheated crucible and return it to the furnace for melting; 3) After melting, the product is cast into shape and annealed in a muffle furnace; 4) Cutting, grinding and polishing the annealed glass to obtain a blue glass sheet with a thickness of 0.2 mm; 5) Use a spectrophotometer to test the transmittance of the blue glass.

[0007] in: In the step 2), the glass melting temperature is 1100° C. and the holding time is 1 hour; The annealing temperature in step 3) is 450°C; The test wavelength range of the spectrophotometer in step 5) is 200-1100 nm.

[0008] The technical effect of the present invention is mainly reflected in that the transmittance of a 0.2 mm thick blue glass sheet in the band below 400 nm is less than 1%, the transmittance in the band of 400-600 nm is higher than 83%, and the transmittance in the band above 700 nm is less than 1%, with no obvious growth trend, thereby effectively realizing the absorption of infrared light. BRIEF DESCRIPTION OF THE DRAWINGS

[0009] Figure 1 Example 3 # Transmittance test chart of the sample. DETAILED DESCRIPTION

[0010] The three specific embodiments of the blue glass of the present invention are as follows: Experimental case 1# Experimental formula: 45%P2O5-10%B2O3-20%BaO-10%Na2O-10%CuO-5%ZnO Na+ introduction method: NaNO3 Processing thickness: 0.2mm Experimental case 2# Experimental formula: 45%P2O5-10%B2O3-20%BaO-10%Na2O-10%CuO-5%ZnO Na+ introduction method: NaH2PO4 Processing thickness: 0.2mm Experimental case 3# Experimental formula: 45%P2O5-10%B2O3-20%BaO-10%Na2O-10%CuO-5%ZnO Na+ introduction method: NaF Processing thickness: 0.2mm Implementation Case 1# 1) Weigh 10 g of the required raw materials according to the stoichiometric ratio and grind and mix them thoroughly in a mortar; 2) Add the mixed raw materials into the preheated crucible and put them back into the furnace for melting at 1100°C for 1 hour; 3) After melting, the product is cast and annealed in a muffle furnace at 450°C and then cooled naturally to room temperature; 4) Cutting, grinding and polishing the annealed glass to obtain a blue glass sheet of 10 mm × 10 mm × 0.2 mm; 5) The transmittance of blue glass was tested using a spectrophotometer. The transmittance was 2.5% at a wavelength of 720nm, and the transmittance increased with the increase of wavelength.

[0011] Implementation Case 2# 1) Weigh 10 g of the required raw materials according to the stoichiometric ratio and grind and mix them thoroughly in a mortar; 2) Add the mixed raw materials into the preheated crucible and put them back into the furnace for melting at 1100°C for 1 hour; 3) After melting, the product is cast and annealed in a muffle furnace at 450°C and then cooled naturally to room temperature; 4) Cutting, grinding and polishing the annealed glass to obtain a blue glass sheet of 10 mm × 10 mm × 0.2 mm; 5) The transmittance of blue glass was obtained by spectrophotometer test. The transmittance was 2% at a wavelength of 735nm, and the transmittance increased with the increase of wavelength.

[0012] Implementation Case 3# 1) Weigh 10 g of the required raw materials according to the stoichiometric ratio and grind and mix them thoroughly in a mortar; 2) Add the mixed raw materials into the preheated crucible and put them back into the furnace for melting at 1100°C for 1 hour; 3) After melting, the product is cast and annealed in a muffle furnace at 450°C and then cooled naturally to room temperature; 4) Cut, grind and polish the annealed glass to obtain 10mm×10mm×0.2mm blue glass sheets; 5) The transmittance of blue glass was tested by spectrophotometer. The transmittance was less than 1% at a wavelength of 700nm. With the increase of wavelength, the transmittance showed no obvious growth trend and tended to be stable.

Claims

1. An ultra-thin blue glass infrared current-carrying filter, characterized in that: The transmittance of 0.2mm thick blue glass infrared current filter in the band above 700nm is less than 1%.

2. The blue glass infrared current-carrying filter according to claim 1, characterized in that: The transmittance of 0.2mm thick blue glass infrared current filter is less than 1% in the band below 400nm.

3. The blue glass infrared current-carrying filter according to claim 1, characterized in that: The transmittance of 0.2mm thick blue glass infrared current filter in the 400-600nm band is higher than 83%.

4. The blue glass infrared current-carrying filter according to claim 1, characterized in that: No weight loss after immersion in high temperature and high humidity environment for 48 hours.

5. The blue glass infrared current-carrying filter according to claim 1, characterized in that: After immersion in 1 mol / L nitric acid solution for 32 h, the weight loss rate was less than 9.2%.