Method for synthesizing fatty alcohol-polyoxyethylene ether sodium acetate through dehydrogenation of fatty alcohol-polyoxyethylene ether

By reacting fatty alcohol polyoxyethylene ether with tin oxide catalyst and sodium hydroxide, the problem of difficult separation of by-products and high cost of precious metal catalysts in traditional methods is solved, and efficient, safe and environmentally friendly AEC-Na synthesis is achieved, improving the improvement of the AEC-Na synthesis Product quality and conversion rate.

CN118894775APending Publication Date: 2024-11-05LIAONING HUAXING DAILY CHEM IND TECH RES INST CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202410948753.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-16
Publication Date
2024-11-05

AI Technical Summary

Technical Problem

In the prior art, carboxymethylation method and precious metal catalytic oxidation method have difficulty in separation of by-products in the production of fatty alcohol sodium polyoxyethylene ether acetate (AEC-Na), high cost, low activity, and explosive use of oxygen. Issues of risk.

Method used

The tin oxide catalyst is used to react with sodium hydroxide and sodium hydroxide under certain conditions and directly synthesize the fatty alcohol polyoxyethylene ether through dehydrogenation reaction, avoiding the risk of harmful substances in traditional methods and explosion. Reduces catalyst costs.

Benefits of technology

It has achieved an efficient, safe and environmentally friendly AEC-Na synthesis route, improved product quality and raw material conversion rate, ensured the safety and controllability of the production process, and avoided the high cost of precious metal catalysts.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118894775A_ABST
    Figure CN118894775A_ABST
Patent Text Reader

Abstract

The invention discloses a method for synthesizing fatty alcohol-polyoxyethylene ether sodium acetate by dehydrogenation of fatty alcohol-polyoxyethylene ether, which comprises the following steps: respectively putting fatty alcohol-polyoxyethylene ether, sodium hydroxide and a tin oxide catalyst into a reaction kettle, the mass ratio of the tin oxide catalyst to the fatty alcohol-polyoxyethylene ether is (2: 100)-(6: 100); after nitrogen is introduced to replace air in the reaction kettle, the temperature is increased to 200-260 DEG C, the constant-temperature stirring reaction is performed for 8-20 h, and sodium fatty alcohol polyoxyethylene ether acetate is obtained. The reaction process is safe, controllable and free of residues, the problem that a precious metal catalysis method is high in catalyst cost is solved through the used catalyst, and the raw material conversion rate and the product yield are greatly increased.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of daily chemical industry, and specifically relates to a method for synthesizing fatty alcohol polyoxyethylene ether sodium acetate by dehydrogenation of fatty alcohol polyoxyethylene ether. Background Art

[0002] Fatty alcohol polyoxyethylene ether carboxylate (AEC for short) is a green surfactant. From the perspective of its structure, it contains both polyoxyethylene (EO unit) and carboxyl groups in the molecule, which makes it have the properties of both anionic and non-ionic surfactants. On the one hand, the EO group in the molecule improves the hydrophilicity of the product; on the other hand, the carboxyl group at the end of the molecule improves the surface activity of the product in aqueous solutions with high hardness by complexing with metal ions. In addition, studies have found that AEC also has excellent emulsification, foaming, detergency and good compounding ability with other types of surfactants (anionic, cationic, non-ionic).

[0003] Fatty alcohol polyoxyethylene ether sodium acetate (AEC-Na for short) is a type of fatty alcohol polyoxyethylene ether carboxylate. AEC-Na is widely used in many industries due to its excellent performance. It is often used as a daily cleaning product such as shower gel due to its mild nature and rich foam. It is also used as a softener due to its good anti-greying and compounding ability. At the same time, AEC-Na can also be used as a heavy oil viscosity reducer in the petroleum industry and as a deinking agent in the papermaking industry. In addition, it is also often used as a degreasing agent, printing and dyeing agent, and disinfectant in the leather and textile industries.

[0004] It has been more than 80 years since the first synthesis of fatty alcohol polyoxyethylene ether carboxylates abroad, during which many researchers have studied new synthetic routes. At present, the common methods for producing AEC-Na from fatty alcohol polyoxyethylene ether (abbreviated as AEO) are carboxymethylation and precious metal catalytic oxidation. The carboxymethylation method refers to the use of chloroacetic acid as a carboxymethylating agent to perform carboxymethylation reaction on fatty alcohol polyoxyethylene ether under alkaline conditions. This method has the problem of many by-products in the product that are difficult to separate and residual unreacted toxic sodium chloroacetate raw materials. The precious metal catalytic oxidation method is to use precious metals to catalytically oxidize the hydroxyethyl group at the end of fatty alcohol polyoxyethylene ether to carboxyl group under alkaline conditions. Chinese patent CN101357333B discloses a Pd / C catalyst, preparation method and application for preparing alcohol ether carboxylates. Alkaline earth metals Sr, Ba and transition metals Ni, Co, Cu, La are added to the traditional Pd / C catalyst as auxiliary components to improve the catalyst activity, oxygen is introduced, and the reactor pressure is maintained at 0.03-0.20MPa to increase the yield of alcohol ether carboxylates. However, the noble metal catalytic oxidation method has the disadvantages of high cost of noble metals and easy detachment from the carrier, making it difficult to industrialize the method. In addition, the use of oxygen as an oxidant makes the reaction system have the safety risk of explosion.

[0005] At present, since the domestic research on AEC-Na is still in its early stages, there are problems such as few product types and low output. Summary of the invention

[0006] In order to solve the problems of difficulty in separating chloroacetate from the product, residual harmful substances, high cost and low activity of precious metal catalysts in the process of producing AEC-Na by carboxymethylation, and explosion risk when using oxygen, the present invention discloses a method for synthesizing fatty alcohol polyoxyethylene ether sodium acetate by direct reaction of fatty alcohol polyoxyethylene ether with sodium hydroxide under tin oxide catalysis. The present invention is a new green, economical and environmentally friendly synthesis route, which solves the technical problems existing in the current production of AEC-Na by carboxymethylation and precious metal catalytic oxidation. The specific technical scheme is as follows:

[0007] A method for synthesizing fatty alcohol polyoxyethylene ether sodium acetate by dehydrogenation of fatty alcohol polyoxyethylene ether, the method is as follows: fatty alcohol polyoxyethylene ether, sodium hydroxide and a tin oxide catalyst are respectively put into a reaction kettle, wherein the molar ratio of sodium hydroxide to fatty alcohol polyoxyethylene ether is 1:1-2.2:1, and the mass ratio of the tin oxide catalyst to fatty alcohol polyoxyethylene ether is 2:100-6:100; nitrogen is introduced to replace the air in the reaction kettle, the temperature is raised to 200°C-260°C, and the reaction is stirred at a constant temperature for 8-20 hours to obtain fatty alcohol polyoxyethylene ether sodium acetate.

[0008] Preferably, the particle size distribution of the tin oxide catalyst is 3-15 nm, and the particle morphology of the tin oxide catalyst is spherical.

[0009] Preferably, the fatty alcohol polyoxyethylene ether is RO(CH2CH2O)2CH2CH2OH, R=C12-14.

[0010] Preferably, the tin oxide catalyst is prepared according to the following method: adding an aqueous ammonia solution dropwise into a SnCl4·5H2O solution at 50°C with stirring until the pH value reaches 8; continuing stirring for 1 hour, standing for 12 hours to obtain a white liquid, filtering and washing the white liquid to obtain a filter cake, drying the obtained filter cake, taking the filter cake to dry, grinding it, passing it through a 100-mesh sieve, and calcining it at 500°C for 2 hours to obtain a tin oxide catalyst.

[0011] In the present invention, the white liquid is filtered and washed to obtain a filter cake. The specific operation is to filter while washing, and after washing until the filtrate is neutral, filter to obtain the filter cake.

[0012] The flow rate of dropwise infusion was 1 mL / min.

[0013] Preferably, the concentration of the SnCl4·5H2O solution is 0.5 mol·L -1 .

[0014] Preferably, the stirring speed is 400 rpm.

[0015] Preferably, the drying is drying the filter cake at a temperature of 90° C. for 5 hours.

[0016] The mechanism of the present invention is that AEO-3 can dehydrogenate the terminal C-OH into an aldehyde group under the catalytic action of sodium hydroxide and tin oxide catalysts. In the absence of a tin oxide catalyst, the conversion rate of the aldehyde group to the carboxylate is relatively low. The tin oxide catalyst with a particle size of 3-15nm has a smaller grain size and a larger specific surface area, which significantly improves the catalytic performance of the catalyst and can effectively activate the sodium hydroxide molecules. The activated sodium hydroxide molecules promote the conversion of the aldehyde group into a carboxylate. Therefore, the tin oxide catalyst plays an important role in the conversion of the reaction intermediate into the carboxylate.

[0017] Beneficial effects of the present invention:

[0018] 1. The present invention uses tin oxide as a catalyst, which, on the one hand, avoids the high cost of the catalyst in the noble metal catalysis method; on the other hand, through the dehydrogenation reaction, avoids the problem of residual sodium chloroacetate, a harmful substance, in the traditional carboxymethylation product, and also avoids the problem of explosion risk when using oxygen and hydrogen peroxide as oxidants in the traditional method, thereby ensuring the safety and controllability of the production process.

[0019] 2. The present invention develops a new green and environmentally friendly AEC-Na synthesis route and improves the quality of the product.

[0020] 3. The present invention is a one-step method for directly synthesizing the target product AEC-Na, which greatly improves the raw material conversion rate and the product yield. Under the optimal conditions, the conversion rate of fatty alcohol polyoxyethylene ether reaches 100%, and the selectivity of fatty alcohol polyoxyethylene ether sodium carboxylate reaches 100%. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] Figure 1 This is a TEM image of the tin oxide catalyst in the present invention.

[0022] Figure 2 It is a bar graph showing the particle size distribution of the tin oxide catalyst in the present invention. DETAILED DESCRIPTION

[0023] In order to make the technical problems, technical solutions and beneficial effects solved by the present invention more clearly understood, the present invention is further described in detail below in conjunction with specific implementation methods. It should be understood that the specific implementation methods described herein are only used to explain the present invention and are not used to limit the present invention.

[0024] Example 1

[0025] (1) Preparation of tin oxide catalyst

[0026] Prepare 0.5 mol·L -1 SnCl4·5H2O solution was stirred in a 50°C water bath for 1 hour (stirring speed was 400 rpm), and then a 25% ammonia solution was dripped dropwise at a flow rate of 1 mL / min until the pH value of the solution reached 8, and the stirring was continued for 1 hour. The solution was allowed to stand for 12 hours to maintain stability, and a white liquid was obtained. The white liquid obtained after standing was filtered and washed to neutrality to obtain a filter cake, which was dried at 90°C for 5 hours, ground through a 100-mesh sieve, and then calcined in a muffle furnace at 500°C for 2 hours to obtain a tin oxide catalyst, and the morphology of the tin oxide catalyst particles was spherical.

[0027] (2) Catalytic reaction

[0028] Fatty alcohol polyoxyethylene ether (RO(CH2CH2O)2CH2CH2OH, R=C12-14) and sodium hydroxide are placed in a reaction kettle, and then the tin oxide catalyst prepared in the above step (1) is added, wherein the molar ratio of sodium hydroxide to fatty alcohol polyoxyethylene ether is 1:1, and the mass ratio of tin oxide catalyst to fatty alcohol polyoxyethylene ether is 2:100. After nitrogen is introduced to replace the air, the temperature is raised to 200°C, the reaction is carried out at a constant temperature for 8 hours, and the stirring speed is set to 400rpm to obtain fatty alcohol polyoxyethylene ether sodium acetate.

[0029] (3) Determination of conversion rate and selectivity

[0030] Take fatty alcohol polyoxyethylene ether sodium acetate in a beaker, add 37% concentrated hydrochloric acid to acidify to pH = 1, add chloroform to the above liquid and stir it thoroughly, then transfer the solution to a pear-shaped separatory funnel, let it stand for 10 minutes, take the lower organic phase, evaporate the chloroform and residual water with a rotary evaporator, and use gas chromatography to determine the content of fatty alcohol polyoxyethylene ether remaining in the acidified sample, and calculate its conversion rate. Use sodium hydroxide aqueous solution and alkali titration to determine the content of fatty alcohol polyoxyethylene ether sodium acetate in the acidified sample, and calculate the selectivity of fatty alcohol polyoxyethylene ether sodium acetate.

[0031] The calculation formulas for AEO conversion and AEC selectivity in the present invention are as follows:

[0032]

[0033]

[0034] Example 2-Example 4

[0035] The other steps were the same as in Example 1, except that the reaction temperature in step (2) was changed, where the reaction temperatures in Example 2, Example 3 and Example 4 were 220° C., 240° C. and 260° C., respectively. The selectivity of the obtained products and the conversion rate of the raw materials are shown in Table 1.

[0036] Table 1 Experimental results of Example 1, Example 2, Example 3, and Example 4

[0037]

[0038] It can be seen from the experimental data in Table 1 that the reaction temperature in the present invention has an important influence on the reaction of fatty alcohol polyoxyethylene ether and sodium hydroxide catalyzed by tin oxide catalyst.

[0039] When the reaction temperature increases from 200°C to 260°C, the conversion rate of fatty alcohol polyoxyethylene ether increases from 60.9% to 93.1%, while the selectivity of fatty alcohol polyoxyethylene ether sodium carboxylate decreases from 100% to 94%. It can be seen that increasing the reaction temperature is beneficial to the reaction in the direction of generating fatty alcohol polyoxyethylene ether sodium acetate, but exceeding the maximum reaction limit may cause the fatty alcohol polyoxyethylene ether sodium carboxylate to decompose and produce by-products, which is not conducive to the generation of highly selective fatty alcohol polyoxyethylene ether sodium carboxylate.

[0040] Example 5-Example 7

[0041] The same as Example 1, only the reaction time in step (2) was changed, and the reaction time in Example 5, Example 6, and Example 7 was 12 h, 16 h, and 20 h, respectively. The experimental results are shown in Table 2.

[0042] Table 2 Experimental results of Example 1, Example 5, Example 6, and Example 7

[0043]

[0044] Table 2 shows that the reaction time in the present invention has an important influence on the reaction of fatty alcohol polyoxyethylene ether and sodium hydroxide catalyzed by tin oxide catalyst. After the reaction time is extended from 8h to 20h, the conversion rate of fatty alcohol polyoxyethylene ether and the selectivity of fatty alcohol polyoxyethylene ether sodium carboxylate both reach 100%, indicating that extending the reaction time is beneficial to the formation of fatty alcohol polyoxyethylene ether sodium carboxylate.

[0045] Example 8-Example 10

[0046] The same as Example 1, only the molar ratio of sodium hydroxide to fatty alcohol polyoxyethylene ether in step (2) was changed, and the molar ratios of Example 8, Example 9 and Example 10 were 1.4:1, 1.8:1 and 2.2:1 respectively. The experimental results are shown in Table 3.

[0047] Table 3 Experimental results of Example 1, Example 8, Example 9, and Example 10

[0048]

[0049] Table 3 shows that the amount of alkali has an important influence on the catalytic activity of tin oxide catalyzing the reaction of fatty alcohol polyoxyethylene ether and sodium hydroxide to generate fatty alcohol polyoxyethylene ether sodium carboxylate. The increase in the amount of alkali is conducive to the synthesis of high-purity fatty alcohol polyoxyethylene ether sodium carboxylate. When the molar ratio of sodium hydroxide to fatty alcohol polyoxyethylene ether is increased to 2.2:1 and the reaction time is 8h, the conversion rate of fatty alcohol polyoxyethylene ether and the selectivity of fatty alcohol polyoxyethylene ether sodium carboxylate both reach 100%.

[0050] Example 11-Example 12

[0051] The same as Example 1, only the mass ratio of the tin oxide catalyst to the fatty alcohol polyoxyethylene ether in step (2) was changed, and the mass ratios of Example 11 and Example 12 were 4:100 and 6:100 respectively. The experimental results are shown in Table 4.

[0052] Table 4 Experimental results of Example 1, Example 11, and Example 12

[0053]

[0054] The results in Table 4 show that the amount of catalyst has an important influence on the catalytic activity of the tin oxide catalyst in catalyzing the reaction of fatty alcohol polyoxyethylene ether with sodium hydroxide to generate fatty alcohol polyoxyethylene ether sodium carboxylate. As the amount of catalyst increases, it helps to improve the conversion rate of fatty alcohol polyoxyethylene ether.

[0055] Comparative Example 1, Comparative Example 2

[0056] The difference between Comparative Example 1 and Example 1 is that the added amount of tin oxide catalyst is 0.

[0057] The difference between Comparative Example 2 and Example 1 is that the average particle size of the tin oxide catalyst particles is 60-70 nm.

[0058] The experimental results are shown in Table 5. From the comparison of the results of Example 1 and Comparative Example 1, it can be seen that the effective amount of catalyst added can promote the conversion of fatty alcohol polyoxyethylene ether into the target product as much as possible, and the tin oxide catalyst can effectively activate the sodium hydroxide molecules. The synergistic effect of the two promotes the conversion of the reaction intermediate fatty alcohol polyoxyethylene ether acetaldehyde into fatty alcohol polyoxyethylene ether sodium carboxylate.

[0059] From the comparison between Example 1 and Comparative Example 2, it can be seen that the particle size of the catalyst has an important influence on its catalytic activity. The catalyst with a small particle size has a larger specific surface area, which improves the conversion rate of sodium fatty alcohol polyoxyethylene ether carboxylate by providing more catalytic active sites.

[0060] Table 5 Experimental results of Example 1, Comparative Example 1 and Comparative Example 2

[0061]

[0062] It can be understood that the above specific description of the present invention is only used to illustrate the present invention and is not limited to the technical solutions described in the embodiments of the present invention. Those skilled in the art should understand that the present invention can still be modified or replaced by equivalents to achieve the same technical effects; as long as the use requirements are met, they are within the protection scope of the present invention.

Claims

1. A method for synthesizing fatty alcohol polyoxyethylene ether sodium acetate by dehydrogenation of fatty alcohol polyoxyethylene ether, characterized in that: The method is as follows: fatty alcohol polyoxyethylene ether, sodium hydroxide, and a tin oxide catalyst are respectively placed in a reaction kettle, wherein the molar ratio of sodium hydroxide to fatty alcohol polyoxyethylene ether is 1:1-2.2:1, and the mass ratio of the tin oxide catalyst to fatty alcohol polyoxyethylene ether is 2:100-6:100; nitrogen is introduced to replace the air in the reaction kettle, the temperature is raised to 200°C-260°C, and the reaction is stirred at a constant temperature for 8-20 hours to obtain fatty alcohol polyoxyethylene ether sodium acetate.

2. The method for synthesizing fatty alcohol polyoxyethylene ether sodium acetate by dehydrogenation of fatty alcohol polyoxyethylene ether according to claim 1, characterized in that: The particle size distribution of the tin oxide catalyst is 3-15 nm, and the particle morphology of the tin oxide catalyst is spherical.

3. The method for synthesizing fatty alcohol polyoxyethylene ether sodium acetate by dehydrogenation of fatty alcohol polyoxyethylene ether according to claim 1, characterized in that: The fatty alcohol polyoxyethylene ether is RO(CH2CH2O)2CH2CH2OH, R=C12-14.

4. The method for synthesizing fatty alcohol polyoxyethylene ether sodium acetate by dehydrogenation of fatty alcohol polyoxyethylene ether according to claim 1, characterized in that: The tin oxide catalyst is prepared according to the following method: an ammonia solution is added dropwise into a SnCl4·5H2O solution at 50° C. and under stirring until the pH value is 8; stirring is continued for 1 hour, and the solution is allowed to stand for 12 hours to obtain a white liquid, the white liquid is filtered and washed to obtain a filter cake, the filter cake is dried, the filter cake is dried, ground, passed through a 100-mesh sieve, and calcined at 500° C. for 2 hours to obtain the tin oxide catalyst.

5. The method for synthesizing fatty alcohol polyoxyethylene ether sodium acetate by dehydrogenation of fatty alcohol polyoxyethylene ether according to claim 4, characterized in that: The concentration of the SnCl4·5H2O solution is 0.5 mol·L -1 .

6. The method for synthesizing fatty alcohol polyoxyethylene ether sodium acetate by dehydrogenation of fatty alcohol polyoxyethylene ether according to claim 4, characterized in that: The stirring speed is 400 rpm.

7. The method for synthesizing fatty alcohol polyoxyethylene ether sodium acetate by dehydrogenation of fatty alcohol polyoxyethylene ether according to claim 4, characterized in that: The drying step is to dry the filter cake at 90° C. for 5 hours.

Citation Information

Patent Citations

  • Pd / C catalyst for preparing alcohol ether carboxylate and production method and use thereof

    CN101357333B