Preparation method of cyclic alkyl sulfate

By using a composite photocatalyst of cadmium and ammonium tungstate compounds to oxidize cyclic alkyl sulfite esters under visible light, the problems of high raw material hazards and high costs in existing methods for preparing cyclic vinyl sulfate esters are solved, achieving efficient and environmentally friendly preparation of cyclic alkyl sulfate esters.

CN118894834AActive Publication Date: 2024-11-05JIANGSU HICOMER NEW MATERIAL CO LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202410829686.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-25
Publication Date
2024-11-05
Estimated Expiration
2044-06-25

AI Technical Summary

Technical Problem

Among the existing methods for preparing cyclic vinyl sulfate, the acylation method has hazardous raw materials and low yield, while the oxidation method uses precious metal catalysts, which is costly and pollutes the environment.

Method used

A composite material containing cadmium and ammonium tungstate compounds is used as a photocatalyst to carry out a photocatalytic oxidation reaction under visible light. The oxidant is used to generate cyclic alkyl sulfite esters in a highly oxidizing ionic state to produce cyclic alkyl sulfate esters.

Benefits of technology

It achieves a high-yield, low-cost, and environmentally friendly preparation process, simplifies process operation, reduces the generation of waste, and is suitable for industrial production.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0004911465590000011
    Figure BDA0004911465590000011
  • Figure BDA0004911465590000021
    Figure BDA0004911465590000021
  • Figure BDA0004911465590000081
    Figure BDA0004911465590000081
Patent Text Reader

Abstract

In order to solve the problems that in an existing cyclic ethylene sulfate preparation method, raw materials in an acylation method are large in harm and low in yield, and catalysts in an oxidation method are high in cost, the invention provides a preparation method of cyclic alkyl sulfate. The cyclic alkyl sulfite is subjected to a photocatalytic oxidation reaction under the action of a photocatalyst and an oxidizing agent, and cyclic alkyl sulfate is obtained; the photocatalyst comprises a composite material containing cadmium and an ammonium tungstate compound. The preparation method provided by the invention has the advantages of low cost, simple process operation, mild reaction conditions, small use amount of the photocatalyst, reutilization, less three wastes and the like on the basis of obtaining high yield.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of lithium ion battery additive synthesis methods, and in particular to a method for preparing cyclic alkyl sulfate. Background Art

[0002] Cyclic vinyl sulfate (1,3,2-Dioxathiolane 2,2-dioxide, referred to as DTD) is a white crystal or crystalline powder. Cyclic vinyl sulfate is a new type of lithium-ion battery additive. As a SEI film-forming additive for lithium-ion batteries, cyclic vinyl sulfate can reduce the decline in battery capacity, inhibit the expansion of the battery after being placed at high temperature, reduce capacity decay and battery internal resistance, improve the low-temperature charging and discharging performance of the battery, improve the stability of the graphite negative electrode, and enhance the battery cycle performance. In the pharmaceutical field, cyclic vinyl sulfate can be used as a pharmaceutical intermediate, as a raw material for a certain heterocyclic compound for synthetic gelatin hardening, antihypertensive drugs, and a new type of dual surfactant, and has broad market prospects. Its structural formula is:

[0003]

[0004] At present, the main preparation methods of cyclic vinyl sulfate include acylation method, substitution method, addition method, dioxane synthesis method and oxidation method. All of the above methods have advantages and disadvantages. Among them, the advantage of the acylation method is that its raw materials are cheap and easy to obtain, and the disadvantage is that the raw material sulfuryl chloride is harmful and the reaction yield is low. At present, the oxidation method is the most commonly used and relatively mature preparation method in industrial production. Ethylene glycol is used as the starting material, and it reacts with dichloroxythionyl to generate the intermediate vinyl sulfite, and then sodium hypochlorite is used as the oxidant to catalyze the vinyl sulfate in a ruthenium chloride aqueous solution to obtain the vinyl sulfate; the precious metal catalyst ruthenium chloride used in this method is expensive and difficult to recycle, and the sodium ions and chloride ions in the product vinyl sulfate are easy to exceed the standard. The use of sodium hypochlorite to produce a large amount of waste brine has a great impact on the environment, which is not conducive to environmental protection and does not meet the development requirements of green chemistry. Summary of the invention

[0005] In view of the problems that the acylation method for preparing cyclic vinyl sulfate has high hazards and low yield of raw materials, and the oxidation method for preparing catalyst has high cost, the present application provides a method for preparing cyclic alkyl sulfate.

[0006] In one aspect, the present invention provides a method for preparing a cyclic alkyl sulfate, the method comprising the following steps:

[0007] In a solvent, the cyclic alkyl sulfite undergoes a photocatalytic oxidation reaction under the action of a photocatalyst and an oxidant to obtain a cyclic alkyl sulfate;

[0008] The photocatalyst comprises a composite material containing cadmium and ammonium tungstate compounds.

[0009] Preferably, the composite material has a metal organic framework structure;

[0010] The ammonium tungstate compound includes tetrabutylammonium decatungstate.

[0011] Preferably, the molar ratio of the photocatalyst to the cyclic alkyl sulfite is (0.00015-0.003):1.

[0012] Preferably, the composite material is prepared by a hydrothermal solvent method, comprising the following steps: tetrabutylammonium decatungstate, trimesic acid and cadmium salt are prepared by a hydrothermal solvent method in an inorganic acid solution;

[0013] The cadmium salt includes cadmium chloride, and the inorganic acid solution includes hydrochloric acid solution.

[0014] Preferably, the light source in the photocatalytic oxidation reaction uses visible light, and the wavelength of the visible light is 450 to 520 nm;

[0015] And / or, the reaction temperature of the photocatalytic oxidation reaction is 40-70° C., and the reaction time is 4h-12h.

[0016] Preferably, the structural formula of the cyclic alkyl sulfite is shown in Formula 1, and the structural formula of the cyclic alkyl sulfate is shown in Formula 2.

[0017]

[0018] Wherein, n is 0, 1, 2, 3; m is 0, 1, 2, 3; R1, R2, R3, R4, R5, R6 are each independently selected from a hydrogen atom, a halogen atom, and a hydrocarbon group having 1 to 10 carbon atoms.

[0019] Preferably, the solvent comprises a mixed solvent of an organic solvent and an ionic liquid.

[0020] The preparation of the mixed solvent comprises the following steps: uniformly mixing the organic solvent and the ionic liquid at a temperature T1; T1>40°C, and the mass ratio of the organic solvent to the ionic liquid is (100-1000):1.

[0021] Preferably, the organic solvent includes one or more of ketone solvents, nitrile solvents, ester solvents, alkane solvents, halogenated hydrocarbon solvents and aromatic hydrocarbon solvents;

[0022] The ionic liquid includes one or more of imidazole ionic liquids, pyridine ionic liquids, piperidine ionic liquids, quaternary ammonium ionic liquids, and guanidine ionic liquids.

[0023] Preferably, the mass ratio of the solvent to the cyclic alkyl sulfite is (2-10):1; the mass ratio of the solvent to the photocatalyst is (200-2000):1.

[0024] Preferably, in the solvent, the cyclic alkyl sulfite undergoes a photocatalytic oxidation reaction under the action of a photocatalyst and an oxidant to obtain the cyclic alkyl sulfate, further comprising obtaining the mixed solution after the photocatalytic oxidation reaction is completed, and post-treating the mixed solution to obtain the cyclic alkyl sulfate, wherein the post-treating comprises sequentially cooling and filtering the mixed solution;

[0025] The oxidant includes oxygen, and the gas flow rate of oxygen introduced is 0.4-2 mL / min for every 1 g of cyclic alkyl sulfite added.

[0026] The preparation method of the cyclic alkyl sulfate provided in the present application uses an oxidant in a solvent under light irradiation to convert the oxidant into some ionic states (oxygen ions (O 2- ), peroxide ion (O2 2- ) or superoxide ion (O2 - ) etc., these ions efficiently oxidize cyclic alkyl sulfite and generate cyclic alkyl sulfate under the action of photocatalyst. Compared with the prior art, the preparation method provided by the present application can achieve a high yield while having the advantages of low cost, simple process operation, mild reaction conditions, small amount of photocatalyst used and reusable, less waste, etc. DETAILED DESCRIPTION

[0027] In order to make the purpose, technical solution and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with the embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not used to limit the present invention.

[0028] In order to illustrate the technical solution of the present invention, specific embodiments are provided below for illustration.

[0029] In one embodiment of the present invention, a method for preparing a cyclic alkyl sulfate is provided, the method comprising the following steps:

[0030] In a solvent, the cyclic alkyl sulfite undergoes a photocatalytic oxidation reaction under the action of a photocatalyst and an oxidant to obtain a cyclic alkyl sulfate;

[0031] The photocatalyst comprises a composite material containing cadmium and ammonium tungstate compounds.

[0032] The preparation method of the cyclic alkyl sulfate provided in the present application uses an oxidant in a solvent under light irradiation to convert the oxidant into some ionic states (oxygen ions (O 2- ), peroxide ion (O2 2- ) or superoxide ion (O2 - ) etc., these ions efficiently oxidize cyclic alkyl sulfite and generate cyclic alkyl sulfate under the action of photocatalyst. Compared with the prior art, the preparation method provided by the present application can achieve a high yield while having the advantages of low cost, simple process operation, mild reaction conditions, small amount of photocatalyst used and reusable, less waste, etc.

[0033] In some embodiments, the composite material has a metal organic framework structure;

[0034] The ammonium tungstate compound includes tetrabutylammonium decatungstate.

[0035] Specifically, the photocatalyst uses a composite material of tetrabutylammonium decatungstate and cadmium, which has the following advantages over ordinary photocatalysts: first, visible light can be used for catalysis, with low energy consumption and low light source operation and maintenance costs; second, tetrabutylammonium tungstate itself has good optical activity, and the composite material uses a metal organic framework to combine it with cadmium, which also has optical activity, through a three-dimensional configuration, and has a larger specific surface area and higher catalytic efficiency than other photocatalysts; third, the combination of ionic liquid and composite material can better disperse the photocatalyst in the reaction system, so that it can be more fully contacted with alkyl sulfite and oxidant such as oxygen source, further improving the catalytic efficiency; fourth, the separation method uses a cooling method to condense the high melting point ionic liquid into a solid, and the composite material of the photocatalyst tetrabutylammonium decatungstate and cadmium has no solubility in the organic solvent system, and is directly filtered, which not only makes the preparation process relatively green and environmentally friendly, but also does not have three wastes that are difficult to treat or highly polluting, and does not require high equipment, the process operation is simple, the reaction conditions are relatively mild, the amount of photocatalyst used is also small and easy to separate and recover, so that the cost of the entire process is relatively low, which is convenient for large-scale industrial production.

[0036] In some embodiments, the molar ratio of the photocatalyst to the cyclic alkyl sulfite is (0.00015-0.003):1.

[0037] Specifically, the molar ratio of the photocatalyst to the cyclic alkyl sulfite is in the range of (0.00015-0.003):1. Under the action of the photocatalyst, the oxidant efficiently oxidizes the cyclic alkyl sulfite to form a cyclic alkyl sulfate. If the content of the photocatalyst is too low, the reaction rate is too slow. If the content of the photocatalyst is too high, although the reaction rate increases, the amount of organic solvent and deionized liquid required to be added also increases, and the preparation cost increases. Specifically, the molar ratio of the photocatalyst to the cyclic alkyl sulfite can be in the following ranges: (0.00015-0.0003):1, (0.0003-0.0005):1, (0.0005-0.001):1, (0.001-0.002):1 or (0.002-0.003):1.

[0038] In some preferred embodiments, the molar ratio of the photocatalyst to the cyclic alkyl sulfite is (0.0005-0.002):1.

[0039] Specifically, when the molar ratio of the photocatalyst to the cyclic alkyl sulfite is within the above preferred range, the photocatalytic oxidation reaction rate is fast, the production efficiency is high, and the preparation cost is low.

[0040] In some embodiments, the composite material is prepared by a hydrothermal solvent method, comprising the following steps: tetrabutylammonium decatungstate, trimesic acid and cadmium salt are prepared by a hydrothermal solvent method in an inorganic acid solution;

[0041] The cadmium salt includes cadmium chloride, and the inorganic acid solution includes hydrochloric acid solution.

[0042] Specifically, trimesic acid is a planar structure. After coordinating with cadmium ions, it is connected with tetrabutylammonium decatungstate through molecular bond forces to form a stable three-dimensional structure. This structure is basically stable below 180°C and has a photocatalytic oxidation effect.

[0043] The impurities are mainly hydrochloric acid and unreacted raw materials, which can be removed by rinsing with cold water, filtering and drying.

[0044] The cadmium salt provides cadmium ions to the composite material.

[0045] The inorganic acid provides the acidic environment required for the reaction and can dissolve the reaction raw materials at high temperatures.

[0046] The composite material is obtained by reacting tetrabutylammonium decatungstate, trimesic acid and cadmium salt in an inorganic acid solution by a hydrothermal solvent method. After the reaction is completed, the remaining inorganic acid and the raw materials that have not been completely reacted can be washed with cold water, filtered and dried out. The preparation method is simple, and the separation of the product and the reactant can be achieved directly by filtering after the reaction is completed, and the purification method is simple.

[0047] In some embodiments, the molar ratio of tetrabutylammonium decatungstate, trimesic acid and cadmium salt is (1-3):(9-27):(3-9).

[0048] Specifically, the molar ratio of tetrabutylammonium decatungstate, trimesic acid and cadmium salt is within the above range, which helps trimesic acid to coordinate with cadmium metal and form a stable three-dimensional structure with tetrabutylammonium decatungstate. The structure can stably exist below 180°C and play a good photocatalytic oxidation role. Specifically, the molar ratio of tetrabutylammonium decatungstate, trimesic acid and cadmium salt can be the following ratios: 1:9:3, 1:12:4, 1.5:15:5, 1.6:20:6, 1.8:23:7 or 2.0:27:9, as long as the molar ratio of tetrabutylammonium decatungstate, trimesic acid and cadmium salt is within the range of (1-3): (9-27): (3-9).

[0049] In some embodiments, tetrabutylammonium decatungstate, trimesic acid and cadmium salt are prepared in an inorganic acid solution by a hydrothermal solvent method, and the heating steps in the hydrothermal solvent method are as follows: first keep warm at 40-80°C for 2 hours, then heat to 150-200°C for reaction for 2-4 hours, then keep warm at a constant temperature of 100-140°C for 6 hours, and finally cool to room temperature. In the heating step, keep warm at a constant temperature of 100-140°C for 6 hours, and the function of the heat preservation is to shape the generated composite material. . The use of a gradient heating and cooling heating method helps trimesic acid to coordinate with cadmium ions, and then connect with tetrabutylammonium decatungstate through molecular bond forces to form a stable three-dimensional structure. In the heating step of the hydrothermal solvent method, if the reaction temperature is lower than the range of 150-200°C, or the reaction time is too short, the formation of the metal organic framework structure will be affected; if the constant temperature during the constant temperature stage after the reaction is completed is lower than the temperature range of 100-140°C, or the constant temperature insulation time is too short, it will also affect the molding of the composite material.

[0050] In some embodiments, the light source in the photocatalytic oxidation reaction uses visible light, and the wavelength of the visible light is 450-520 nm.

[0051] Specifically, the light source in the photocatalytic oxidation reaction uses visible light, the wavelength of which is in the range of 450 to 520 nm, which can effectively make the oxidant into some ionic states (oxygen ions (O 2- ), peroxide ion (O2 2- ) or superoxide ion (O2 - ) etc., which ions efficiently oxidize cyclic alkyl sulfites and generate cyclic alkyl sulfates under the action of photocatalysts.

[0052] For the wavelength of visible light, the power of the light source can be adjusted to make the wavelength of visible light within the set wavelength range. The greater the power of the light source, the smaller the wavelength, and the smaller the power, the larger the wavelength. In actual operation, you can choose a white light LED lamp with adjustable power to control the wavelength by adjusting its power, or choose LED lamps with different wavelengths to act separately.

[0053] It should be noted that not all wavelengths of visible light can work, nor can all wavelengths of visible light achieve the desired effect; if the wavelength is too large (greater than 520nm) or too small (less than 450nm), it may affect the generation of strong oxidizing ions and may even have a reverse effect on the oxidation of alkyl sulfate, and ultimately fail to achieve the desired yield. The inventors have found through a large number of experimental studies that when the wavelength of visible light is within the range of 450 to 520nm, a better yield can be obtained, indicating that controlling the wavelength within the range of 450 to 520nm can effectively make the oxidant into some ionic states (oxygen ions (O 2- ), peroxide ion (O2 2- ) or superoxide ion (O2 - ) etc., to increase the yield of the product.

[0054] Specifically, the wavelength of visible light may be in the following ranges: 450nm to 460nm, 460nm to 470nm, 470nm to 480nm, 480nm to 490nm, 490nm to 500nm, 500nm to 510nm, 510nm to 520nm.

[0055] In some embodiments, the reaction temperature of the photocatalytic oxidation reaction is 40 to 70° C., and the reaction time is 4 to 12 hours.

[0056] Specifically, since photocatalysts cannot be used directly in organic solvents, they will aggregate into clumps in organic solvents. Therefore, they must be used in a mixed solvent of ionic liquids and organic solvents. The mixed solvent of ionic liquids and organic solvents needs to be evenly mixed at a temperature above 40°C. Temperature is also an important factor affecting the effect of photocatalysts. Too high a temperature will destroy the structure of the photocatalyst molecules, and too low a temperature will reduce the catalyst's response to light. The reaction temperature of the photocatalytic oxidation reaction is within the range of 40 to 70°C, which will not destroy the structure of the photocatalyst molecules. At the same time, it can also ensure that the photocatalyst has a high response effect to light, has an efficient catalytic effect, and improves the yield of the product.

[0057] Specifically, the reaction temperature of the photocatalytic oxidation reaction can be, for example, 40°C, 42°C, 45°C, 47°C, 50°C, 53°C, 55°C, 60°C, 61°C, 65°C, 70°C, etc.

[0058] Specifically, the reaction time of the oxidation reaction is controlled to be 4 to 12 hours. Compared with the existing preparation process, the preparation time is greatly shortened and the production efficiency can be significantly improved.

[0059] In some preferred embodiments, the reaction temperature of the photocatalytic oxidation reaction is 40-60°C.

[0060] In some preferred embodiments, the reaction temperature of the photocatalytic oxidation reaction is 50-70°C.

[0061] In some more preferred embodiments, the reaction temperature of the photocatalytic oxidation reaction is 50-60°C.

[0062] In some embodiments, the structural formula of the cyclic alkyl sulfite is shown in Formula 1, and the structural formula of the cyclic alkyl sulfate is shown in Formula 2.

[0063]

[0064] Wherein, n is 0, 1, 2, 3; m is 0, 1, 2, 3; R1, R2, R3, R4, R5, R6 are each independently selected from a hydrogen atom, a halogen atom, and a hydrocarbon group having 1 to 10 carbon atoms.

[0065] The hydrocarbon group having 1 to 10 carbon atoms includes C1 to C10 straight-chain alkyl groups and C1 to C10 branched alkyl groups.

[0066] In some preferred embodiments, the cyclic alkyl sulfite comprises cyclic vinyl sulfite; and the cyclic alkyl sulfate comprises cyclic vinyl sulfate.

[0067] In some embodiments, the solvent comprises a mixed solvent of an organic solvent and an ionic liquid.

[0068] The preparation of the mixed solvent comprises the following steps: uniformly mixing the organic solvent and the ionic liquid at a temperature T1; T1>40°C, and the mass ratio of the organic solvent to the ionic liquid is (100-1000):1.

[0069] Specifically, the photocatalyst cannot be used directly in an organic solvent, as it will aggregate into clumps in the organic solvent. Therefore, it must be used in a mixed solvent of an ionic liquid and an organic solvent. The organic solvent and the ionic liquid need to be above 40°C to be evenly mixed.

[0070] The mass ratio of the organic solvent to the ionic liquid is in the range of (100-1000):1. The addition of more organic solvent can dissolve the reactants in the solvent. At the same time, the addition of the ionic liquid prevents the photocatalyst from agglomerating in the organic solvent and affecting the reaction rate. Specifically, the mass ratio of the organic solvent to the ionic liquid can be 100:1, 200:1, 300:1, 400:1, 500:1, 600:1, 700:1, 800:1, 900:1 or 1000:1, etc., as long as the mass ratio of the organic solvent to the ionic liquid is in the range of (100-1000):1.

[0071] In some preferred embodiments, the mass ratio of the organic solvent to the ionic liquid is (200-500):1. Specifically, the mass ratio of the organic solvent to the ionic liquid is within the above range. While effectively dissolving the reactants and catalysts, it can also effectively prevent the photocatalyst from agglomerating in the organic solvent, thereby increasing the reaction rate.

[0072] In some embodiments, the organic solvent includes one or more of a ketone solvent, a nitrile solvent, an ester solvent, an alkane solvent, a halogenated hydrocarbon solvent, and an aromatic hydrocarbon solvent;

[0073] The ionic liquid includes one or more of imidazole ionic liquids, pyridine ionic liquids, piperidine ionic liquids, quaternary ammonium ionic liquids, and guanidine ionic liquids.

[0074] Specifically, the type of organic solvent selected can better dissolve the reactant cyclic alkyl sulfate, and the type of ionic liquid selected can effectively prevent the photocatalyst from agglomerating in the organic solvent and affecting the catalytic reaction of the photocatalyst.

[0075] In some preferred embodiments, the ketone solvent includes one or more of acetone, butanone, methyl isobutyl ketone, and cyclohexanone;

[0076] The nitrile solvent includes one or more of acetonitrile and propionitrile;

[0077] The ester solvent includes one or more of methyl acetate, ethyl acetate, propyl acetate, isopropyl acetate, butyl acetate, isoamyl acetate, methyl propionate, ethyl propionate, propyl propionate, dimethyl carbonate, diethyl carbonate, and ethyl methyl carbonate;

[0078] The alkane solvent includes one or more of n-pentane, n-heptane, n-hexane, cyclohexane, and petroleum ether;

[0079] The halogenated hydrocarbon solvent includes one or more of dichloromethane and dichloroethane;

[0080] The aromatic hydrocarbon solvent includes one or more of benzene, toluene, xylene, chlorobenzene, o-dichlorobenzene, m-dichlorobenzene, and p-dichlorobenzene.

[0081] In some preferred embodiments, the imidazolium ionic liquid includes one or more of 1-ethyl-3-methylimidazolium chloride, 1-ethyl-3-methylimidazolium tetrafluoroborate, 1-ethyl-3-methylimidazolium hexafluorophosphate, and 1-hexyl-3-methylimidazolium chloride;

[0082] The pyridine ionic liquid includes 1-butylpyridinium chloride;

[0083] The piperidine ionic liquid includes N-methyl-N-propylpiperidinium bistrifluoromethanesulfonimide salt;

[0084] The quaternary ammonium ionic liquid includes tetraethylammonium chloride and tributylmethylammonium chloride, and the guanidine ionic liquid includes one or more of tetramethylguanidine hydrogen sulfate and guanidine hydrochloride.

[0085] In some embodiments, the mass ratio of the solvent to the cyclic alkyl sulfite is (2-10):1; the mass ratio of the solvent to the photocatalyst is (200-2000):1.

[0086] Specifically, the mass of the solvent here refers to the total mass of the organic solvent and the ionic liquid; the mass ratio of the solvent to the cyclic alkyl sulfite is in the range of (2 to 10):1, and the mass of the added solvent is 2 to 10 times the mass of the cyclic alkyl sulfite, so that the solvent can better and completely dissolve the added cyclic alkyl sulfite; the mass of the solvent is 200 to 2000 times the mass of the photocatalyst, which not only dissolves the photocatalyst but also prevents the photocatalyst from agglomerating in the solvent and improves the yield of the product. Specifically, the mass ratio of the solvent to the cyclic alkyl sulfite can be 2:1, 2.5:1, 3.0:1, 4:1, 5:1, 6:1, 7:1, 8:1, 9:1, or 10:1, etc., as long as the mass ratio of the solvent to the cyclic alkyl sulfite is in the range of (2 to 10):1. The mass ratio of the solvent to the photocatalyst is (200-2000):1, which can be 200:1, 250:1, 300:1, 400:1, 500:1, 600:1, 700:1, 800:1, 900:1, 1000:1, 1200:1, 1500:1, 1700:1, 1900:1 or 2000:1, etc., as long as the mass ratio of the solvent to the photocatalyst is within the range of (200-2000):1.

[0087] In some embodiments, in a solvent, a cyclic alkyl sulfite undergoes a photocatalytic oxidation reaction under the action of a photocatalyst and an oxidant to obtain a cyclic alkyl sulfate. The step also includes obtaining a mixed solution after the photocatalytic oxidation reaction is completed, and post-treating the mixed solution to obtain the cyclic alkyl sulfate, wherein the post-treatment includes sequentially cooling and filtering the mixed solution.

[0088] Specifically, the high-melting-point ionic liquid is first condensed into a solid by a cooling method. The composite material of the photocatalyst tetrabutylammonium decatungstate and cadmium has no solubility in the organic solvent system, and is directly filtered. This not only makes the preparation process relatively green and environmentally friendly, but also eliminates the three wastes that are difficult to treat or highly polluting. The equipment requirements are not high, the process operation is simple, the reaction conditions are relatively mild, the amount of photocatalyst used is small and it is easy to separate and recover, so that the cost of the entire process is relatively low, and it is convenient for large-scale industrial production.

[0089] In some embodiments, the oxidant includes oxygen, and the gas flow rate of oxygen introduced is 0.4-2 mL / min per 1 g of cyclic alkyl sulfite added.

[0090] Specifically, the oxidant includes oxygen, which may be pure oxygen gas (with a purity greater than 99%) or a mixed gas consisting of an inert gas and oxygen, or dry air. The inert gas may be nitrogen, argon, or the like.

[0091] The flow rate of oxygen gas relative to the added amount of the cyclic alkyl sulfite is 0.4 to 2 mL / min for every 1 g of cyclic alkyl sulfite added. More preferably, the flow rate of oxygen gas relative to the added amount of the cyclic alkyl sulfite is 0.6 to 1.2 mL / min for every 1 g of cyclic alkyl sulfite added.

[0092] The present invention is further described below by way of examples.

[0093] Example 1

[0094] 1) Preparation of photocatalyst

[0095] Preparation by hydrothermal solvent method: tetrabutylammonium decatungstate, trimesic acid and cadmium chloride are prepared by hydrothermal solvent method in hydrochloric acid solution to obtain a photocatalyst, the photocatalyst contains a composite material of cadmium and ammonium tungstate compounds, and the prepared composite material is a metal organic framework material. Among them, the molar ratio of tetrabutylammonium decatungstate, trimesic acid and cadmium chloride is 1:9:3, and the heating procedure is to first heat to 60℃ for 2h, then heat to 160-180℃ for 2h, then keep constant temperature at 110-130℃ for 6h, and finally cool to room temperature.

[0096] 2) Preparation of cyclic vinyl sulfate

[0097] Cyclic vinyl sulfite is used as a raw material, a mixed solvent with an organic solvent and an ionic liquid in a mass ratio of 200:1 is used as a solvent, and under the irradiation of visible light with a wavelength of 500nm, in the presence of the photocatalyst prepared in the above step 1), oxygen is used as an oxygen source, and a photocatalytic oxidation reaction occurs to generate vinyl sulfate. The reaction temperature of the photocatalytic oxidation reaction is 50°C, and the reaction time is 10h; for each 1g of cyclic vinyl sulfite added, the gas flow rate of the oxygen introduced is in the range of 0.4 to 2mL / min.

[0098] The organic solvent is ethylene dichloride, and the ionic liquid is tetraethylammonium chloride. The organic solvent and the ionic liquid are uniformly mixed at a temperature above 40°C. The mass ratio of the solvent to cyclic vinyl sulfite is 2.5:1, and the mass ratio of the solvent to the photocatalyst is 833.33:1. The molar ratio of the photocatalyst to the cyclic vinyl sulfite is 0.003:1.

[0099] Example 2

[0100] Most of the steps of this embodiment are the same as those of Embodiment 1, except that the wavelength of the visible light is 520 nm, and the rest are the same as those of Embodiment 1.

[0101] Example 3

[0102] Most of the steps of this embodiment are the same as those of Embodiment 1, except that the wavelength of the visible light is 450 nm, and the rest is the same as Embodiment 1.

[0103] Example 4

[0104] Most of the steps of this embodiment are the same as those of Embodiment 1, except that the wavelength of the visible light is 400 nm, and the rest are the same as those of Embodiment 1.

[0105] Example 5

[0106] Most of the steps of this embodiment are the same as those of Embodiment 1, except that the wavelength of the visible light is 540 nm, and the rest are the same as those of Embodiment 1.

[0107] Example 6

[0108] Most of the steps of this embodiment are the same as those of embodiment 1, except that the reaction temperature of the photocatalytic oxidation reaction is 40° C. and the reaction time is 12 h. The rest is the same as embodiment 1.

[0109] Example 7

[0110] Most of the steps of this embodiment are the same as those of embodiment 1, except that the reaction temperature of the photocatalytic oxidation reaction is 70° C. and the reaction time is 4 h. The rest is the same as embodiment 1.

[0111] Example 8

[0112] Most of the steps of this embodiment are the same as those of embodiment 1, except that the reaction temperature of the photocatalytic oxidation reaction is 60° C. and the reaction time is 8 h. The rest is the same as embodiment 1.

[0113] Example 9

[0114] Most of the steps of this embodiment are the same as those of embodiment 1, except that the reaction temperature of the photocatalytic oxidation reaction is 35° C. and the reaction time is 10 h. The rest is the same as embodiment 1.

[0115] Example 10

[0116] Most of the steps of this embodiment are the same as those of embodiment 1, except that the reaction temperature of the photocatalytic oxidation reaction is 75° C. and the reaction time is 10 h. The rest is the same as embodiment 1.

[0117] Embodiment 11

[0118] Most of the steps of this embodiment are the same as those of embodiment 1, except that the solvent contains no ionic liquid but only an organic solvent.

[0119] Example 12

[0120] Most of the steps in this embodiment are the same as those in embodiment 1, except that the mass ratio of the organic solvent to the ionic liquid in the solvent is 900:1.

[0121] Embodiment 13

[0122] Most of the steps in this embodiment are the same as those in embodiment 1, except that the mass ratio of the organic solvent to the ionic liquid in the solvent is 1200:1.

[0123] Embodiment 14

[0124] Most of the steps in this embodiment are the same as those in Embodiment 1, except that the mass ratio of the organic solvent to the ionic liquid in the solvent is 50:1.

[0125] Embodiment 15

[0126] Most of the steps of this embodiment are the same as those of Embodiment 1, except that the molar ratio of the photocatalyst to cyclic vinyl sulfite is 0.001:1, and the mass ratio of the solvent to cyclic vinyl sulfate is 8:1, corresponding to a mass ratio of the solvent to the photocatalyst of 319.73:1.

[0127] Example 16

[0128] Most of the steps of this embodiment are the same as those of Embodiment 1, except that the molar ratio of the photocatalyst to cyclic vinyl sulfite is 0.0001:1, and the mass ratio of the solvent to cyclic vinyl sulfate is 3:1, corresponding to a mass ratio of the solvent to the photocatalyst of 1198.98:1.

[0129] Embodiment 17

[0130] Most of the steps of this embodiment are the same as those of Embodiment 1, except that the molar ratio of the photocatalyst to cyclic vinyl sulfite is 0.004:1, and the mass ratio of the solvent to cyclic vinyl sulfate is 10:1, corresponding to a mass ratio of the solvent to the photocatalyst of 99.91:1.

[0131] Embodiment 18

[0132] Most of the steps of this embodiment are the same as those of embodiment 1, except that the types of organic solvents and ionic liquids are different. The organic solvents are acetonitrile, acetone and chlorobenzene; and the ionic liquids are N-methyl-N-propylpiperidinium bistrifluoromethanesulfonyl imide salt, tributylmethylammonium chloride and tetramethylguanidine hydrogen sulfate.

[0133] Embodiment 19

[0134] Most of the steps of this embodiment are the same as those of embodiment 1, except that in the preparation of the photocatalyst, the heating temperature and time are different. The heating procedure is to first raise the temperature to 50°C and keep it for 2 hours, then raise the temperature to 140°C for reaction for 1 hour, then keep the temperature at 90°C for 2 hours, and finally cool it to room temperature.

[0135] Embodiment 20

[0136] Most of the steps of this embodiment are the same as those of embodiment 1, except that trimesic acid is not added in the preparation of the photocatalyst.

[0137] Comparative Example 1

[0138] Most of the steps of this comparative example are the same as those of Example 1, except that the existing photocatalyst used in this comparative example is nano-titanium dioxide.

[0139] Comparative Example 2

[0140] Most of the steps of this comparative example are the same as those of Example 1, except that the existing photocatalyst used in this comparative example is tetrabutylammonium decatungstate.

[0141] Comparative Example 3

[0142] Most of the steps of this comparative example are the same as those of Example 1, except that this comparative example uses existing photocatalysts of tetrabutylammonium decatungstate and molybdenum.

[0143] Comparative Example 4

[0144] Most of the steps of this comparative example are the same as those of Example 1, except that the existing photocatalysts used in this comparative example are tetrabutylammonium decatungstate and manganese.

[0145] Comparative Example 5

[0146] Most of the steps of this comparative example are the same as those of Example 1, except that this comparative example uses existing photocatalysts of tetrabutylammonium decatungstate and gold.

[0147] The yield results of cyclic vinyl sulfate prepared in the above examples and comparative examples are recorded in Table 1.

[0148] Table 1

[0149]

[0150]

[0151] It can be seen from Table 1 that, by comparing Example 1 with Comparative Examples 1-5, the photocatalyst of Comparative Example 1 uses nano-titanium dioxide, and the yield of the product cyclic vinyl sulfate is lower; Comparative Examples 2-5 use tetrabutylammonium decatungstate as a photocatalyst, or use it together with photocatalyst metal molybdenum, metal manganese, and metal gold as a photocatalyst, but the yield of the prepared cyclic vinyl sulfate is lower; it is speculated that this is because the photocatalyst provided in the present application is a composite material containing cadmium and ammonium tungstate compounds, and the composite material has a metal organic framework structure, trimesic acid is coordinated with cadmium metal, and forms a stable three-dimensional structure with tetrabutylammonium decatungstate, and the structure can stably exist below 180°C, has a larger specific surface area and a higher catalytic efficiency than other photocatalysts, and improves the yield of the product cyclic vinyl sulfate.

[0152] Comparing Examples 1-3 and 4-5, the wavelength of visible light in the photocatalytic oxidation reaction is in the range of 450-520nm, and the yield of the product cyclic vinyl sulfate is high. Comparing Examples 1, 6-8 and 9-10, the reaction temperature of the photocatalytic oxidation reaction is 40-70°C, the reaction time is in the range of 4h-12h, and the yield of the product cyclic vinyl sulfate is high; it is speculated that this is because the reaction temperature is lower than 40°C, which reduces the response effect of the catalyst to light, and too high a temperature will destroy the structure of the photocatalyst molecule, which affects the photocatalytic reaction. Comparing Example 1 and Example 11, there is no ionic liquid in the solvent, indicating that the photocatalyst without ionic liquid is easy to aggregate in the organic solvent, affecting the photocatalytic reaction and reducing the product yield. Comparing Examples 1, 12 and 13-14, the mass ratio of organic solvent to ionic liquid is in the range of (100-1000): 1. More organic solvent is added, which can dissolve the reactants in the solvent. At the same time, the addition of ionic liquid prevents the photocatalyst from aggregating in the organic solvent and improves the product yield. Comparing Examples 1 and 15 with Examples 16 and 17, the molar ratio of the photocatalyst to the cyclic vinyl sulfite is too low or too high, and the mass ratio of the solvent to the photocatalyst is too low or too high, and the yield of the product is low. This indicates that the molar ratio of the photocatalyst to the cyclic vinyl sulfite is in the range of (0.00015 to 0.003): 1, the mass ratio of the solvent to the photocatalyst is in the range of (200 to 2000): 1, and the mass ratio of the solvent to the cyclic alkyl sulfite is in the range of (2 to 10): 1, which helps to improve the yield of the product.

[0153] Comparison between Example 1 and Example 18 shows that changing the types of organic solvents and ionic liquids, as long as they are within the type range specified in this application, has the same effect, and improves the yield of the product cyclic vinyl sulfate. Comparison between Example 1 and Example 19 shows that in the preparation of the photocatalyst, the reaction temperature is lower than 150-200°C, the reaction time is too short, the constant temperature is lower than the range of 100-140°C, the reaction temperature is too low, and the insulation temperature and time are short, which is not conducive to the molding of the composite material, affects the photocatalytic oxidation reaction, and reduces the product yield; it is speculated that the heating process is to first keep the temperature at 40-80°C for 2h, then heat to 150-200°C for 2-4h, then keep the temperature at a constant temperature of 100-140°C for 6h, and finally cool to room temperature to generate a photocatalyst with a metal organic framework structure, high photocatalytic oxidation efficiency, and improved product yield.

[0154] Comparing Example 1 with Example 20, no trimesic acid was added during the preparation of the photocatalyst, and the metal organic framework structure could not be formed. The prepared material had a photocatalytic effect similar to that of tetrabutylammonium decatungstate, which reduced the product yield.

[0155] The above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit them. Although the present invention has been described in detail with reference to the above embodiments, it should be understood by those skilled in the art that the technical solutions described in the above embodiments can still be modified, or some of the technical features can be replaced by equivalents. However, these modifications or replacements do not deviate the essence of the corresponding technical solutions from the spirit and scope of the technical solutions of the embodiments of the present invention, and should be included in the protection scope of the present invention.

Claims

1. A method for preparing a cyclic alkyl sulfate, characterized in that: The method comprises the following steps: In a solvent, the cyclic alkyl sulfite undergoes a photocatalytic oxidation reaction under the action of a photocatalyst and an oxidant to obtain a cyclic alkyl sulfate; The photocatalyst comprises a composite material containing cadmium and ammonium tungstate compounds.

2. The method for preparing a cyclic alkyl sulfate according to claim 1, characterized in that: The composite material has a metal organic framework structure; The ammonium tungstate compound includes tetrabutylammonium decatungstate.

3. The method for preparing a cyclic alkyl sulfate according to claim 1, characterized in that: The molar ratio of the photocatalyst to the cyclic alkyl sulfite is (0.00015-0.003):

1.

4. The method for preparing a cyclic alkyl sulfate according to claim 2, characterized in that: The composite material is prepared by a hydrothermal solvent method, comprising the following steps: tetrabutylammonium decatungstate, trimesic acid and cadmium salt are prepared by a hydrothermal solvent method in an inorganic acid solution; The cadmium salt includes cadmium chloride, and the inorganic acid solution includes hydrochloric acid solution.

5. The method for preparing cyclic alkyl sulfate according to claim 1, characterized in that: The light source in the photocatalytic oxidation reaction uses visible light, and the wavelength of the visible light is 450-520nm; And / or, the reaction temperature of the photocatalytic oxidation reaction is 40-70° C., and the reaction time is 4h-12h.

6. The method for preparing cyclic alkyl sulfate according to claim 1, characterized in that: The structural formula of the cyclic alkyl sulfite is shown in Formula 1, and the structural formula of the cyclic alkyl sulfate is shown in Formula 2. Wherein, n is 0, 1, 2, 3; m is 0, 1, 2, 3; R1, R2, R3, R4, R5, R6 are each independently selected from a hydrogen atom, a halogen atom, and a hydrocarbon group having 1 to 10 carbon atoms.

7. The method for preparing cyclic alkyl sulfate according to claim 1, characterized in that: The solvent includes a mixed solvent of an organic solvent and an ionic liquid, The preparation of the mixed solvent comprises the following steps: The organic solvent and the ionic liquid are mixed uniformly at a temperature T1; T1>40°C, and the mass ratio of the organic solvent to the ionic liquid is (100-1000):

1.

8. The method for preparing cyclic alkyl sulfate according to claim 7, characterized in that: The organic solvent includes one or more of ketone solvents, nitrile solvents, ester solvents, alkane solvents, halogenated hydrocarbon solvents and aromatic hydrocarbon solvents; The ionic liquid includes one or more of imidazole ionic liquids, pyridine ionic liquids, piperidine ionic liquids, quaternary ammonium ionic liquids, and guanidine ionic liquids.

9. The method for preparing cyclic alkyl sulfate according to claim 1, characterized in that: The mass ratio of the solvent to the cyclic alkyl sulfite is (2-10):1; the mass ratio of the solvent to the photocatalyst is (200-2000):

1.

10. The method for preparing cyclic alkyl sulfate according to claim 1, characterized in that: In a solvent, the cyclic alkyl sulfite undergoes a photocatalytic oxidation reaction under the action of a photocatalyst and an oxidant to obtain a cyclic alkyl sulfate, further comprising obtaining a mixed solution after the photocatalytic oxidation reaction is completed, and post-treating the mixed solution to obtain the cyclic alkyl sulfate, wherein the post-treating comprises sequentially cooling and filtering the mixed solution; The oxidant includes oxygen, and the gas flow rate of oxygen introduced is 0.4-2 mL / min for every 1 g of cyclic alkyl sulfite added.

Citation Information

Patent Citations

  • Method for preparing cyclic sulphate

    CN104744427A

  • High-selectivity phenol synthesis method by benzoyl oxide

    CN107008253A

  • Method for preparing cyclic sulfate

    CN115141175A

  • Method for preparing ethylene sulfate through catalysis

    CN117362267A