Salt pan ore bed thickness identification method and system and storage medium

Through ultrasonic and pulsed electromagnetic wave technology, combining the relationship between electromagnetic wave diffusion depth and dielectric resistivity, the thickness of the salt field ore layer is accurately identified, which solves the problem of inaccurate identification of the thickness of the salt field ore layer in the existing technology, avoids clay layer damage, and improves measurement efficiency and Security.

CN118897337APending Publication Date: 2024-11-05ZHONGHUA GEOLOGY MINE ZONGJU GEOLOGY RES YUAN +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411114084.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-14
Publication Date
2024-11-05

AI Technical Summary

Technical Problem

The existing methods for identifying the thickness of the mineral layer in salt fields cannot accurately grasp the thickness of the mineral layer, which can easily damage the clay layer and lead to leakage at the bottom of the salt field.

Method used

Ultrasonic and pulsed electromagnetic wave technology is used to obtain the concentration and propagation time of the brine layer, calculate the thickness of the brine layer, and use the relationship between the electromagnetic wave diffusion depth and the dielectric resistivity to determine the ore layer thickness to avoid destroying the clay layer.

Benefits of technology

It improves the accuracy and measurement efficiency of identification of the thickness of the salt field ore layer, avoids damage to the clay layer, and reduces the risk of leakage at the bottom of the salt field.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118897337A_ABST
    Figure CN118897337A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of salt pan ore measurement, in particular to a salt pan ore bed thickness identification method and system and a storage medium, and aims to avoid damage to a clay layer. The salt pan ore bed thickness identification method comprises the steps that the concentration of salt pan brine and the propagation time of ultrasonic waves in the salt pan brine are acquired, and then the thickness of a brine layer is calculated; acquiring an attenuation voltage signal of the pulse electromagnetic wave detection salt pan, and further calculating a time-varying curve of the medium resistivity and a time-varying curve of the electromagnetic wave diffusion depth in the electromagnetic wave propagation process; according to the two curves, the corresponding relation between the electromagnetic wave diffusion depth and the resistivity is determined, and then the resistivity of the ore bed is determined; according to the resistivity of the ore bed, the preset resistivity of the clay layer and the corresponding relation between the electromagnetic wave diffusion depth and the resistivity, the depth of a boundary between the ore bed and the clay layer is determined, and then the thickness of the ore bed is calculated. According to the invention, the clay layer is prevented from being damaged, and the measurement efficiency is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of salt pan ore surveying, and in particular to a salt pan ore layer thickness identification method, system and storage medium. Background Art

[0002] The brine layer is located above the salt pan ore layer, and the clay layer is located below. The clay layer acts as a water barrier, making it difficult for brine in the salt pan to leak. Therefore, when using large salt mining ships to mine salt pans, salt mining companies need to understand the thickness of the salt mine to avoid damaging the clay layer and causing leakage at the bottom of the salt pan.

[0003] Currently, the commonly used method to identify the thickness of salt field ore layers is the manual rod measurement method. Since the thickness of the ore layer cannot be accurately grasped, the clay layer may be damaged, causing leakage in the salt mine. Summary of the invention

[0004] In order to solve the above problems in the prior art, the present invention proposes a salt pan ore layer thickness identification method, system and storage medium, which avoids the risk of damaging the clay layer.

[0005] In a first aspect of the present invention, a method for identifying the thickness of a salt pan ore layer is provided, the method comprising:

[0006] Obtaining the concentration of salt pan brine and the propagation time of ultrasonic waves in the salt pan brine, and then calculating the thickness of the brine layer;

[0007] Obtain the attenuated voltage signal of secondary induction when pulse electromagnetic wave is used to detect salt pan geology;

[0008] Calculating a curve of the change of the dielectric resistivity over time during the propagation of the pulse electromagnetic wave according to the attenuated voltage signal;

[0009] Calculating a curve of electromagnetic wave diffusion depth changing with time based on the curve of the medium resistivity changing with time;

[0010] Determining the corresponding relationship between the electromagnetic wave diffusion depth and the medium resistivity according to the curve of the medium resistivity changing with time and the curve of the electromagnetic wave diffusion depth changing with time;

[0011] Determining the resistivity of the ore layer according to the thickness of the brine layer and the corresponding relationship between the electromagnetic wave diffusion depth and the medium resistivity;

[0012] Determine the depth of the boundary between the mineral layer and the clay layer according to the resistivity of the mineral layer, the preset resistivity of the clay layer, and the corresponding relationship between the electromagnetic wave diffusion depth and the medium resistivity;

[0013] The thickness of the ore layer is calculated based on the thickness of the brine layer and the depth of the dividing line.

[0014] Preferably, the step of "obtaining the concentration of salt pan brine and the propagation time of ultrasonic waves in the salt pan brine, and then calculating the thickness of the brine layer" includes:

[0015] The concentration of salt pan brine is obtained, and the K value corresponding to the salt pan brine is calculated according to a pre-fitted linear equation; the linear equation is used to express the relationship between the concentration of brine and the K value; the K value is the ratio of the propagation speed of ultrasonic wave in brine to the propagation speed in pure water;

[0016] Obtaining the propagation time of the ultrasonic wave in the salt pan brine, and then calculating the distance that the ultrasonic wave can propagate in pure water in the same time;

[0017] According to the propagation distance in the pure water and the K value corresponding to the salt pan brine, the thickness of the salt pan brine is calculated according to the following formula:

[0018] T 卤水 =K×T 纯水

[0019] Among them, T 纯水 is the propagation distance in the pure water; K is the ratio of the propagation speed of ultrasound in brine to that in pure water.

[0020] Preferably, the method further comprises:

[0021] The propagation time of ultrasonic waves in pure water of known thickness is obtained by using an ultrasonic sensor;

[0022] According to the propagation time of ultrasonic wave in the pure water of known thickness, the measured thickness is calculated according to the following formula:

[0023] T 测 =v 纯 t 纯

[0024] Among them, v 纯 is the propagation speed of ultrasound in pure water, preset value; t 纯 is the propagation time of ultrasound in pure water;

[0025] The ultrasonic sensor is calibrated according to the known thickness and the measured thickness.

[0026] Preferably, the step of fitting the linear equation comprises:

[0027] The propagation time of ultrasonic waves in various brines of known concentration and thickness is obtained respectively, and then the propagation speed of ultrasonic waves in each brine is calculated;

[0028] Calculate the ratio K of the propagation speed of ultrasound in each brine to that in pure water;

[0029] The linear equation is fitted according to the concentration of each brine and the corresponding K value.

[0030] Preferably, the step of "calculating a curve of the change of the dielectric resistivity over time during the propagation of the pulse electromagnetic wave according to the attenuated voltage signal" includes:

[0031] According to the preset time interval, the dielectric resistivity at multiple different time points is calculated according to the following formula, thereby obtaining a curve of the dielectric resistivity changing with time:

[0032] ρ τ =6.32×10 -3 L 4 / 3 q 2 / 3 [V(t)] -2 / 3 t -5 / 3

[0033] in,

[0034]

[0035] ρ τ is the dielectric resistivity; L is the side length of the transmitting coil; q is the equivalent area of ​​the receiving coil; V(t) is the attenuated voltage signal; t is the transient electromagnetic field diffusion time; I is the transmitting current; ρ is the resistivity of the uniform earth electromagnetic field, taking ρ=1; z is the transient field parameter, τ is the diffusion parameter, Φ(z) is the probability integral, is the first-order derivative of Φ(z), u(t) is the voltage response function of the step current, and u(t)=1.

[0036] Preferably, the step of "calculating a curve of electromagnetic wave diffusion depth varying with time based on the curve of medium resistivity varying with time" comprises:

[0037] According to the preset time interval, the electromagnetic wave diffusion depth at multiple different time points is calculated according to the following formula, so as to obtain a curve of the electromagnetic wave diffusion depth changing with time:

[0038]

[0039] in,

[0040] β=0.66,w=(100πρ τ t / μ0L 2 ) 1 / 4 ,μ0=4π×10-7 h / m.

[0041] Preferably, the step of “determining the corresponding relationship between the electromagnetic wave diffusion depth and the medium resistivity according to the curve of the medium resistivity changing with time and the curve of the electromagnetic wave diffusion depth changing with time” comprises:

[0042] According to the preset time interval, a corresponding relationship is established between the electromagnetic wave diffusion depth and the medium resistivity at each same time point.

[0043] Preferably, after “establishing a corresponding relationship between the electromagnetic wave diffusion depth and the medium resistivity at each same time point according to the preset time interval”, the method further comprises:

[0044] Draw a resistivity profile of the salt pan according to the corresponding relationship between the electromagnetic wave diffusion depth and the medium resistivity;

[0045] The step of “determining the resistivity of the ore layer according to the thickness of the brine layer and the corresponding relationship between the electromagnetic wave diffusion depth and the medium resistivity” includes:

[0046] According to the thickness of the brine layer, a boundary line between the brine layer and the mineral layer is drawn in the resistivity profile diagram, thereby determining the resistivity of the mineral layer;

[0047] The step of “determining the depth of the boundary between the mineral layer and the clay layer according to the resistivity of the mineral layer, the preset resistivity of the clay layer, and the corresponding relationship between the electromagnetic wave diffusion depth and the medium resistivity” includes:

[0048] A boundary line between the ore layer and the clay layer is drawn in the resistivity profile according to the resistivity of the ore layer and the preset resistivity of the clay layer, and then the depth of the boundary line between the ore layer and the clay layer is determined.

[0049] A second aspect of the present invention provides a salt pan ore layer thickness identification system, the system comprising:

[0050] An ultrasonic sensor for measuring the propagation time of ultrasonic waves in the salt pan brine;

[0051] A pulse electromagnetic wave transceiver, used for transmitting pulse electromagnetic waves vertically downward from the liquid surface of the salt pan brine and receiving a returned attenuated voltage signal;

[0052] A signal analysis device is used to identify the thickness of the salt pan ore layer according to the method described above.

[0053] According to a third aspect of the present invention, a computer-readable storage medium is provided, storing a computer program that can be loaded by a processor and execute the method described above.

[0054] The present invention has the following beneficial effects:

[0055] This method is based on the principle of electromagnetic induction and ultrasonic technology. First, the thickness of the brine layer is identified based on the propagation time of ultrasonic waves in the salt field brine layer and the concentration of the salt field brine. Secondly, the thickness of the mineral layer is identified by utilizing the correspondence between the diffusion depth of electromagnetic waves and the resistivity of different media. Compared with the rod insertion method in the prior art, the present invention can avoid damage to the clay layer and improve the measurement efficiency.

[0056] The present invention calculates the K value corresponding to the salt pan brine by means of a linear equation between the pre-fitted brine concentration and the K value (the ratio of the propagation speed of ultrasonic waves in brine to that in pure water), and then calculates the thickness of the salt pan brine in seconds according to the K value. Compared with the prior art rod insertion method, the measurement efficiency is also improved. BRIEF DESCRIPTION OF THE DRAWINGS

[0057] Figure 1 It is a schematic diagram of the main steps of the first embodiment of the salt field ore layer thickness identification method of the present invention;

[0058] Figure 2 This is a schematic diagram of the main steps of Example 2 of the salt field ore layer thickness identification method of the present invention;

[0059] Figure 3 It is a schematic diagram of the main steps of the third embodiment of the salt field ore layer thickness identification method of the present invention;

[0060] Figure 4 is a schematic diagram of a resistivity cross section in an embodiment of the present invention;

[0061] Figure 5 It is a schematic diagram of the main components of an embodiment of a salt field ore layer thickness identification system in the present invention. DETAILED DESCRIPTION

[0062] The preferred embodiments of the present invention are described below with reference to the accompanying drawings. It should be understood by those skilled in the art that these embodiments are only used to explain the technical principles of the present invention and are not intended to limit the protection scope of the present invention.

[0063] In order to make the purpose, technical solution and advantages of the embodiments of the present invention clearer, the technical solution in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0064] It should be noted that, in the description of the present invention, the terms "first" and "second" are only for the convenience of description, and do not indicate or imply the relative importance of the devices, elements or parameters, and therefore cannot be understood as limiting the present invention. In addition, the term "and / or" in the present invention is only a description of the association relationship of associated objects, indicating that three relationships may exist. For example, A and / or B can represent: A exists alone, A and B exist at the same time, and B exists alone. In addition, the character " / " in this article, unless otherwise specified, generally indicates that the associated objects before and after are in an "or" relationship.

[0065] Figure 1 Schematic diagram of the main steps of the first embodiment of the salt field ore layer thickness identification method of the present invention. Figure 1 As shown, the identification method of this embodiment includes steps A10-A80:

[0066] Step A10, obtaining the concentration of salt pan brine and the propagation time of ultrasonic waves in the salt pan brine, and then calculating the thickness of the brine layer.

[0067] The propagation time here refers to the one-way time it takes for ultrasound to pass through the brine layer.

[0068] Specifically, step A10 may include steps A11-A13:

[0069] Step A11, obtaining the concentration of salt pan brine, and calculating the K value corresponding to the salt pan brine according to a pre-fitted linear equation.

[0070] The linear equation is used to express the relationship between the concentration of brine and the K value; the K value is the ratio of the propagation speed of ultrasound in brine to that in pure water. The concentration of salt field brine can be measured with the help of a liquid concentration meter.

[0071] Step A12, obtaining the propagation time of the ultrasonic wave in the salt pan brine, and then calculating the distance that the ultrasonic wave can propagate in pure water in the same time.

[0072] For example, when measuring salt pan brine with an ultrasonic sensor, if the propagation time of the acquired ultrasonic wave in the salt pan brine is t1, then the thickness of the salt pan brine is T 卤水 The propagation speed of ultrasound in salt field brine v卤水 The relationship between and time t1 is shown in formula (1):

[0073] T 卤水 = v 卤水 t1 (1)

[0074] According to formula (2), the distance T that the ultrasonic wave propagates in pure water in the same time can be calculated: 纯水 :

[0075] T 纯水 = v 纯水 t1 (2)

[0076] Among them, v 纯水 is the propagation speed of ultrasound in pure water, 1500m / s.

[0077] Furthermore, according to formulas (1) and (2), formula (3) can be obtained:

[0078]

[0079] If v 卤水 / v 纯水 Denoted as K, we get formula (4):

[0080] T 卤水 =K×T 纯水 (4)

[0081] Among them, T 卤水 and T 纯水 They are respectively the propagation distance of ultrasound in salt pan brine (i.e. the thickness of salt pan brine) and the propagation distance in pure water in the same time; K is the ratio of the propagation speed of ultrasound in brine to that in pure water.

[0082] Step A13, according to the propagation distance in pure water and the K value corresponding to the salt pan brine, the thickness of the salt pan brine is calculated according to the method shown in the above formula (4).

[0083] Step A20, obtaining the attenuated voltage signal of secondary induction when pulse electromagnetic waves are used to detect salt pan geology.

[0084] Step A30, calculating a curve of the change of the dielectric resistivity with time during the propagation of the pulse electromagnetic wave according to the attenuated voltage signal.

[0085] Specifically, according to the preset time intervals, the dielectric resistivity at multiple different time points is calculated according to formulas (5)-(6), thereby obtaining a curve of dielectric resistivity changing with time:

[0086] ρ τ =6.32×10 -3 L 4 / 3 q2 / 3 [V(t)] -2 / 3 t -5 / 3 (5)

[0087]

[0088] Among them, ρ τ is the dielectric resistivity; L is the side length of the transmitting coil; q is the equivalent area of ​​the receiving coil; V(t) is the attenuated voltage signal; t is the transient electromagnetic field diffusion time; I is the transmitting current; ρ is the resistivity of the uniform earth electromagnetic field, taking ρ=1; z is the transient field parameter, τ is the diffusion parameter, Φ(z) is the probability integral, is the first-order derivative of Φ(z), u(t) is the voltage response function of the step current, and u(t)=1.

[0089] Step A40, calculating a curve of electromagnetic wave diffusion depth varying with time based on a curve of dielectric resistivity varying with time.

[0090] Specifically, according to the preset time interval, the electromagnetic wave diffusion depth at multiple different time points is calculated according to formula (7), so as to obtain a curve of the electromagnetic wave diffusion depth changing with time:

[0091]

[0092] Among them, β = 0.66, w = (100πρ τ t / μ0L 2 ) 1 / 4 ,μ0=4π×10 -7 h / m.

[0093] Step A50, determining the corresponding relationship between the electromagnetic wave diffusion depth and the medium resistivity according to the curve of the medium resistivity changing with time and the curve of the electromagnetic wave diffusion depth changing with time.

[0094] Specifically, because step A40 and step A50 use the same time interval to calculate the medium resistivity and the electromagnetic wave diffusion depth, a corresponding relationship between the electromagnetic wave diffusion depth and the medium resistivity at each same time point can be established according to the preset time interval.

[0095] Step A60, determining the resistivity of the ore layer according to the thickness of the brine layer and the corresponding relationship between the electromagnetic wave diffusion depth and the dielectric resistivity.

[0096] Knowing the thickness of the brine layer, the depth of the boundary between the brine layer and the mineral layer can be determined. Then, based on the correspondence between the electromagnetic wave diffusion depth and the dielectric resistivity, the resistivity of the brine layer and the resistivity of the mineral layer above and below the boundary can be obtained.

[0097] Step A70, determining the depth of the boundary between the ore layer and the clay layer according to the resistivity of the ore layer, the preset resistivity of the clay layer, and the correspondence between the electromagnetic wave diffusion depth and the dielectric resistivity. In this embodiment, the resistivity of the clay layer is 1-1.3Ω.m.

[0098] Step A80, calculating the thickness of the ore layer according to the thickness of the brine layer and the depth of the boundary line.

[0099] Figure 2 It is a schematic diagram of the main steps of Example 2 of the salt field ore layer thickness identification method in the present invention.

[0100] like Figure 2 As shown, the identification method of this embodiment includes steps B10-B90:

[0101] Step B10, calibrating the ultrasonic sensor. This step may specifically include steps B11-B13:

[0102] Step B11, obtaining the propagation time of ultrasonic waves in pure water of known thickness through an ultrasonic sensor.

[0103] Step B12, based on the propagation time of ultrasonic waves in pure water of known thickness, the measured thickness is calculated according to formula (8):

[0104] T 测 = v 纯 t 纯 (8)

[0105] Among them, v 纯 is the propagation speed of ultrasound in pure water, the preset value is (1500m / s); t 纯 It is the propagation time of ultrasound in pure water of known thickness (the time from emitting ultrasound to receiving the returned ultrasound divided by 2).

[0106] Step B13, calibrating the ultrasonic sensor according to the known thickness and the measured thickness.

[0107] Steps B20-B90 correspond to steps A10-A80 in the first embodiment and are the same as each other, and will not be described again here.

[0108] Preferably, the step of fitting a linear equation for representing the relationship between the concentration of brine and the K value may include the following (1)-(3):

[0109] (1) The propagation time of ultrasound in various brines of known concentration and thickness is obtained respectively, and then the propagation speed of ultrasound in each brine is calculated.

[0110] (2) Calculate the ratio K of the propagation speed of ultrasound in each brine to the propagation speed in pure water. As shown in Table 1 below, the concentration C of each brine is listed. 卤水 , the propagation speed of ultrasound in each brine v 卤水 , and the K value corresponding to each brine:

[0111] Table 1 Correspondence between brine concentration, propagation velocity and K value

[0112]

[0113] (3) Fit a linear equation based on the concentration of each brine and the corresponding K value.

[0114] The linear equation fitted according to Table 1 in the original embodiment is shown in formula (9):

[0115] y=0.0111x+1.0813 (9)

[0116] Where x is the brine concentration, corresponding to C in Table 1 卤水 ; y corresponds to the K value in Table 1.

[0117] Steps B20-B90 correspond to steps A10-A80 in the first embodiment and are the same as each other, and will not be described again here.

[0118] Figure 3 Schematic diagram of the main steps of the third embodiment of the salt field ore layer thickness identification method of the present invention. Figure 3 As shown, the identification method of this embodiment may include steps C10-C90:

[0119] Among them, steps C10-C50 correspond to steps A10-A50 in embodiment 1 respectively and are the same, and are not repeated here.

[0120] Step C60, drawing a resistivity profile of the salt pan according to the corresponding relationship between the electromagnetic wave diffusion depth and the medium resistivity. Figure 4 Schematic diagram of resistivity profile in an embodiment of the present invention. Figure 4 As shown, the ordinate represents depth, the abscissa represents horizontal distance, and the different shades of color in the profile represent different resistivities.

[0121] Step C70, drawing a boundary line between the brine layer and the mineral layer in the resistivity profile diagram according to the thickness of the brine layer, and then determining the resistivity of the mineral layer.

[0122] According to the thickness of the brine layer, the boundary between the brine layer and the mineral layer can be found in the cross-section, such as Figure 4 The first dotted line in the figure shows that the dielectric resistivity on both sides of the dotted line is the brine layer resistivity and the mineral layer resistivity respectively.

[0123] Step C80, drawing a boundary line between the ore layer and the clay layer in the resistivity profile according to the resistivity of the ore layer and the preset resistivity of the clay layer, and then determining the depth of the boundary line between the ore layer and the clay layer.

[0124] Once the resistivity of the ore layer and the resistivity of the clay layer are known, the intersection of the two resistivities on the cross-section diagram is the boundary between the ore layer and the clay layer, such as Figure 4 The distance between this dividing line and the brine surface of the salt pan is its depth.

[0125] Step C90, calculating the thickness of the ore layer according to the thickness of the brine layer and the depth of the boundary between the ore layer and the clay layer.

[0126] In this step, the thickness of the ore layer is obtained by subtracting the thickness of the brine layer from the depth of the boundary between the ore layer and the clay layer.

[0127] Although the various steps in all the above method embodiments are described in a chronological order, those skilled in the art can understand that in order to achieve the effect of the present embodiment, different steps do not have to be executed in such an order, and they can be executed simultaneously (in parallel) or in a reverse order. These simple changes are within the scope of protection of the present invention.

[0128] Figure 5 FIG. 1 is a schematic diagram of the main components of an embodiment of a salt field ore layer thickness identification system in the present invention. Figure 5 As shown, the identification system of this embodiment mainly includes: an ultrasonic sensor 1, a pulse electromagnetic wave transceiver 2 (including a transceiver induction coil 2-1, a current transmission line 2-2 and a current generation and signal acquisition unit 2-3, a transceiver coil fixing device 2-4), a signal analysis device 3 and a measuring vessel 4.

[0129] Among them, the ultrasonic sensor 1 is fixed in the middle of the transceiver induction coil so as to be close to the brine surface, and is used to measure the propagation time of the ultrasonic wave in the salt pan brine; the pulse electromagnetic wave transceiver 2 is used to transmit the pulse electromagnetic wave vertically downward from the surface of the salt pan brine, and receive the returned attenuated voltage signal; the transceiver induction coil 2-1 is fixed on the outside of the measuring ship through the transceiver coil fixing device 2-4, and is close to the salt pan brine surface; the current transmission line 2-2 is connected between the current generating and signal collecting unit 2-3 and the transceiver induction coil 2-1, and is used to transmit the pulse electromagnetic wave generated by the current generating and signal collecting unit 2-3 to the transceiver induction coil 2-1, and transmit the attenuated voltage signal of the secondary induction of the transceiver induction coil 2-1 to the current generating and signal collecting unit 2-3; the signal analysis device 3 is used to identify the thickness of the salt pan ore layer according to the method described above; the measuring ship 4 is used to install and fix the above-mentioned ultrasonic sensor 1, the pulse electromagnetic wave transceiver 2 and the signal analysis device 3.

[0130] Based on the above method embodiment, the present invention further proposes an embodiment of a computer-readable storage medium. The storage medium of this embodiment stores a computer program that can be loaded by a processor and execute the method as described above.

[0131] The computer-readable storage medium may include: a USB flash drive, a mobile hard disk, a read-only memory (ROM), a random access memory (RAM), a magnetic disk or an optical disk, and other media that can store program codes.

[0132] Those skilled in the art should be able to appreciate that the method steps of each example described in conjunction with the embodiments disclosed herein can be implemented in electronic hardware, computer software, or a combination of the two. In order to clearly illustrate the interchangeability of electronic hardware and software, the composition and steps of each example have been generally described in the above description according to function. Whether these functions are performed in electronic hardware or software depends on the specific application and design constraints of the technical solution. Those skilled in the art may use different methods to implement the described functions for each specific application, but such implementation should not be considered to be beyond the scope of the present invention.

[0133] So far, the technical solutions of the present invention have been described in conjunction with the preferred embodiments shown in the accompanying drawings. However, it is easy for those skilled in the art to understand that the protection scope of the present invention is obviously not limited to these specific embodiments. Without departing from the principle of the present invention, those skilled in the art can make equivalent changes or substitutions to the relevant technical features, and the technical solutions after these changes or substitutions will fall within the protection scope of the present invention.

Claims

1. A method for identifying the thickness of salt pan ore layers. It is characterized in that The method comprises: Obtaining the concentration of salt pan brine and the propagation time of ultrasonic waves in the salt pan brine, and then calculating the thickness of the brine layer; Obtain the attenuated voltage signal of secondary induction when pulse electromagnetic wave is used to detect salt pan geology; Calculating a curve of the change of the dielectric resistivity over time during the propagation of the pulse electromagnetic wave according to the attenuated voltage signal; Calculating a curve of electromagnetic wave diffusion depth changing with time based on the curve of the medium resistivity changing with time; Determining the corresponding relationship between the electromagnetic wave diffusion depth and the medium resistivity according to the curve of the medium resistivity changing with time and the curve of the electromagnetic wave diffusion depth changing with time; Determining the resistivity of the ore layer according to the thickness of the brine layer and the corresponding relationship between the electromagnetic wave diffusion depth and the medium resistivity; Determine the depth of the boundary between the mineral layer and the clay layer according to the resistivity of the mineral layer, the preset resistivity of the clay layer, and the corresponding relationship between the electromagnetic wave diffusion depth and the medium resistivity; The thickness of the ore layer is calculated based on the thickness of the brine layer and the depth of the dividing line.

2. The salt pan ore layer thickness identification method according to claim 1, It is characterized in that The step of "obtaining the concentration of salt pan brine and the propagation time of ultrasonic waves in the salt pan brine, and then calculating the thickness of the brine layer" includes: The concentration of salt pan brine is obtained, and the K value corresponding to the salt pan brine is calculated according to a pre-fitted linear equation; the linear equation is used to express the relationship between the concentration of brine and the K value; the K value is the ratio of the propagation speed of ultrasonic wave in brine to the propagation speed in pure water; Obtaining the propagation time of the ultrasonic wave in the salt pan brine, and then calculating the distance that the ultrasonic wave can propagate in pure water in the same time; According to the propagation distance in the pure water and the K value corresponding to the salt pan brine, the thickness of the salt pan brine is calculated according to the following formula: T 卤水 =K×T 纯水 Among them, T 纯水 is the propagation distance in the pure water; K is the ratio of the propagation speed of ultrasound in brine to that in pure water.

3. The salt pan ore layer thickness identification method according to claim 2, It is characterized in that The method further comprises: The propagation time of ultrasonic waves in pure water of known thickness is obtained by using an ultrasonic sensor; According to the propagation time of ultrasonic wave in the pure water of known thickness, the measured thickness is calculated according to the following formula: T 测 =v 纯 t 纯 Among them, v 纯 is the propagation speed of ultrasound in pure water, preset value; t 纯 is the propagation time of ultrasonic wave in the pure water of known thickness; The ultrasonic sensor is calibrated according to the known thickness and the measured thickness.

4. The salt pan ore layer thickness identification method according to claim 2, It is characterized in that The steps of fitting the linear equation include: The propagation time of ultrasonic waves in various brines of known concentration and thickness is obtained respectively, and then the propagation speed of ultrasonic waves in each brine is calculated; Calculate the ratio K of the propagation speed of ultrasound in each brine to that in pure water; The linear equation is fitted according to the concentration of each brine and the corresponding K value.

5. The salt pan ore layer thickness identification method according to claim 1, It is characterized in that The step of "calculating a curve of the change of the dielectric resistivity over time during the propagation of the pulse electromagnetic wave according to the attenuated voltage signal" includes: According to the preset time interval, the dielectric resistivity at multiple different time points is calculated according to the following formula, thereby obtaining a curve of the dielectric resistivity changing with time: ρ τ =6.32×10 -3 L 4 / 3 q 2 / 3 [V(t)] -2 / 3 t -5 / 3 in, ρ τ is the dielectric resistivity; L is the side length of the transmitting coil; q is the equivalent area of ​​the receiving coil; V(t) is the attenuated voltage signal; t is the transient electromagnetic field diffusion time; I is the transmitting current; ρ is the resistivity of the uniform earth electromagnetic field, taking ρ=1; z is the transient field parameter, τ is the diffusion parameter, Φ(z) is the probability integral, is the first-order derivative of Φ(z), u(t) is the voltage response function of the step current, and u(t)=1.

6. The salt pan ore layer thickness identification method according to claim 5, It is characterized in that The step of "calculating a curve of electromagnetic wave diffusion depth varying with time based on the curve of the medium resistivity varying with time" comprises: According to the preset time interval, the electromagnetic wave diffusion depth at multiple different time points is calculated according to the following formula, so as to obtain a curve of the electromagnetic wave diffusion depth changing with time: in, β=0.66,w=(100pr) τ t / m 0 L 2 ) 1 / 4 ,m 0 =4π×10 -7 h / m.

7. The salt pan ore layer thickness identification method according to claim 6, It is characterized in that The step of "determining the corresponding relationship between the electromagnetic wave diffusion depth and the medium resistivity according to the curve of the medium resistivity changing with time and the curve of the electromagnetic wave diffusion depth changing with time" includes: According to the preset time interval, a corresponding relationship is established between the electromagnetic wave diffusion depth and the medium resistivity at each same time point.

8. The salt pan ore layer thickness identification method according to claim 7, It is characterized in that After "establishing a corresponding relationship between the electromagnetic wave diffusion depth and the medium resistivity at each same time point according to the preset time interval", the method further includes: Draw a resistivity profile of the salt pan according to the corresponding relationship between the electromagnetic wave diffusion depth and the medium resistivity; The step of "determining the resistivity of the ore layer according to the thickness of the brine layer and the corresponding relationship between the electromagnetic wave diffusion depth and the medium resistivity" includes: According to the thickness of the brine layer, a boundary line between the brine layer and the mineral layer is drawn in the resistivity profile diagram, thereby determining the resistivity of the mineral layer; The step of "determining the depth of the boundary between the mineral layer and the clay layer according to the resistivity of the mineral layer, the preset resistivity of the clay layer, and the corresponding relationship between the electromagnetic wave diffusion depth and the medium resistivity" includes: A boundary line between the ore layer and the clay layer is drawn in the resistivity profile according to the resistivity of the ore layer and the preset resistivity of the clay layer, and then the depth of the boundary line between the ore layer and the clay layer is determined.

9. A salt field ore layer thickness identification system, It is characterized in that The system comprises: An ultrasonic sensor for measuring the propagation time of ultrasonic waves in the salt pan brine; A pulse electromagnetic wave transceiver, used for transmitting pulse electromagnetic waves vertically downward from the liquid surface of the salt pan brine and receiving a returned attenuated voltage signal; A signal analysis device for identifying the thickness of a salt pan ore layer according to the method described in any one of claims 1-8.

10. A computer-readable storage medium, It is characterized in that A computer program is stored which can be loaded by a processor and execute the method according to any one of claims 1 to 8.