Chip layer removing method

The wiring structure of the FEOL layer on the chip is removed through pretreatment and chemical reaction, revealing a flat front-section process layer, and compensating the surface undulation by coating organic film, solving the problem of surface unevenness in the prior art, and improving the microscope Image quality.

CN118899245APending Publication Date: 2024-11-05INTEGRA TED SERVICE TECHNOLOGY (SHANGHAI) CO LTD
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202410979166.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-22
Publication Date
2024-11-05

AI Technical Summary

Technical Problem

The prior art cannot effectively remove the wiring structure of the FEOL layer on the chip, resulting in uneven surfaces and making it difficult to obtain high-quality image information under a microscope.

Method used

The chip surface is thinned by pretreatment steps, and some wiring structures are removed by physical, chemical or machine etching. Then, chemical solution is used in an acid- and alkali-resistant beaker to remove the middle and rear-stage process layer and the latter. The layer is exposed to the front-stage process layer and the organic film is coated on the exposed surface to compensate for the ups and downs to obtain a flat surface.

Benefits of technology

It improves the flatness of the chip surface, reduces the scattering of the optical microscope, and improves the image clarity.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118899245A_ABST
    Figure CN118899245A_ABST
Patent Text Reader

Abstract

The invention provides a chip delamination method, which comprises the following steps of: firstly, thinning a chip through pretreatment, and removing a plurality of layers of wiring structures at the top; and putting the chip into a beaker, and completely removing the middle-section process layer and the rear-section process layer through chemical reaction so as to expose the front-section process layer. Compared with the mode that the chip is soaked in a chemical solution to remove the rear-section process layer and the middle-section process layer at a time, the pretreatment process is beneficial to improving the flatness of the surface of the chip. According to the method, a part of wiring structure layers on the upper layer are removed through short-time preprocessing, it is guaranteed that the difference between the number of the wiring structure layers reserved in the middle area of the chip and the number of the wiring structure layers reserved in the edge area of the chip does not exceed two, and then the wiring structure layers are finally removed through subsequent chemical reactions. Besides, the exposed surface of the front-section process layer is coated with an organic thin film, so that the fluctuation of the surface of the front-section process layer is compensated, a flat surface is obtained, and the image definition under a microscope is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of semiconductor detection, and in particular to a chip de-layering method. Background Art

[0002] In the integrated circuit (IC) industry, with the continuous development of domestic substitution, observation of the substrate has become an important part of the design stage. When designers are designing and verifying ICs, they need to carefully observe the characteristics of the substrate, especially the transistors on the FEOL layer on the substrate. The observation of the substrate provides key information that can be used to verify the feasibility of the design. It also helps to discover new design schemes or solutions, thereby promoting the process of technological innovation. Failure observation is also crucial in the production process of mass-produced products. By observing the damage of components, possible problems in production, such as manufacturing defects or material damage, can be discovered in a timely manner, so that timely measures can be taken to repair or adjust them. This helps to improve product quality and reliability and reduce costs and delays caused by component failures. Therefore, the observation of the substrate is not only of great significance in the IC design stage, but also plays a key role in the production process of mass-produced products, providing strong support for technological innovation and product quality improvement.

[0003] For observation of the FEOL layer on the substrate, the wiring structure on the chip needs to be removed. The existing method of removing the upper wiring structure cannot obtain a flat morphology, and it is difficult to obtain effective image information under a microscope. Summary of the invention

[0004] In view of the above-mentioned shortcomings of the prior art, the present invention provides a chip layer removal method, comprising the following steps:

[0005] Providing a chip, the chip comprising a substrate, a front-end process layer, a middle-end process layer and a back-end process layer stacked in sequence;

[0006] Pre-process the chip to remove several layers of wiring structures of the chip's back-end process layer away from the middle process layer;

[0007] The pre-treated chip is placed in an acid- and alkali-resistant beaker, and a chemical solution is used to perform a chemical reaction to remove the middle process layer and the back process layer, revealing the front process layer;

[0008] Flatness treatment is performed, and an organic film is coated to compensate for the ups and downs of the surface of the previous process layer to obtain a flat surface.

[0009] Optionally, several layers of wiring structures of the chip back-end process layer away from the middle process layer are removed, so that the number of layers of wiring structures retained in the back-end process layer does not exceed 5 layers.

[0010] Optionally, the thickness of the coated organic film is controlled to be 300-100 nm.

[0011] Optionally, the method of pre-processing the chip includes a physical method, a chemical method and a machine etching method.

[0012] Optionally, the physical method includes mechanical grinding, wherein the chip is first fixed on a workbench, and then the chip is ground and removed by a grinding disk.

[0013] Optionally, the chemical method includes immersing the chip in a reaction solution, which can react with the material of the back-end process layer to achieve de-layering.

[0014] Optionally, the machine etching method includes dry etching, and etching and removing layers are performed by plasma.

[0015] Optionally, the pretreated chip is placed in an acid- and alkali-resistant beaker for a chemical reaction time of 3 to 20 minutes.

[0016] Optionally, the pretreated chip is placed in an acid- and alkali-resistant beaker, and the chemical solution for chemical reaction includes an acidic solution and an alkaline solution. The alkaline solution includes an ammonia solution, a sodium hydroxide solution, and the acidic solution includes a hydrofluoric acid solution, a nitric acid solution, an acetic acid solution, and the like.

[0017] Optionally, the process of placing the pretreated chip in an acid- and alkali-resistant beaker for chemical reaction includes:

[0018] First, the pretreated chip is placed in the first chemical solution, and the metal layer in the wiring structure located on the outermost layer is removed by the first chemical solution. Then, the chip is placed in the second chemical solution, and the dielectric layer in the wiring structure located on the outermost layer is removed by the second chemical solution. The entire middle process layer and the back process layer are removed alternately in a cycle.

[0019] As described above, the present invention provides a chip de-layering method, which first thins the chip through pretreatment and removes several layers of wiring structure on the top; then the chip is placed in a beaker to completely remove the middle process layer and the back process layer through chemical reaction to reveal the front process layer. Compared with soaking the chip in a chemical solution to remove the back process layer and the middle process layer at one time, the pretreatment process of the present invention is conducive to improving the flatness of the chip surface. Because the reaction process will be carried out in the form of fast edge and slow middle, the chip will have irregular edge wear, fast edge wear, slow middle wear, and a longer reaction time will result in a larger height difference between the edge and the middle. Therefore, after a short period of pretreatment, part of the upper wiring structure layer is removed to ensure that the number of wiring structure layers retained in the middle area of ​​the chip is no more than 2 layers different from the number of wiring structure layers retained in the edge area of ​​the chip, and then it is finally removed through subsequent chemical reactions. In addition, the present invention also coats the surface of the exposed front process layer with an organic film, thereby compensating for the ups and downs of the surface of the front process layer, obtaining a flat surface, thereby reducing the scattering of the optical microscope, and thus improving the image clarity. BRIEF DESCRIPTION OF THE DRAWINGS

[0020] Figure 1 Shown is a schematic diagram of a complete chip structure in Embodiment 1 of the present invention.

[0021] Figure 2 Shown is a schematic diagram of the chip structure after preprocessing in Example 1 of the present invention.

[0022] Figure 3 It is a schematic diagram showing the step of placing the pre-treated chip into a beaker in the first embodiment of the present invention.

[0023] Figure 4 Shown is a schematic diagram of the chip structure showing the front-end process layer in the first embodiment of the present invention.

[0024] Figure 5 It shows a schematic diagram of the chip structure coated with an organic thin film in the first embodiment of the present invention.

[0025] Component number description

[0026] 10 Substrate

[0027] 11 Front-end process layer

[0028] 12. Middle process layer

[0029] 13 Back-end process layer

[0030] 21 Beaker

[0031] 111 Circuit Unit

[0032] 121 Metal plug

[0033] 122 dielectric layer

[0034] 131 Metal Layer

[0035] 141 Organic Film DETAILED DESCRIPTION

[0036] The following describes the embodiments of the present invention through specific examples, and those skilled in the art can easily understand other advantages and effects of the present invention from the contents disclosed in this specification. The present invention can also be implemented or applied through other different specific embodiments, and the details in this specification can also be modified or changed in various ways based on different viewpoints and applications without departing from the spirit of the present invention.

[0037] For example, when describing the embodiments of the present invention in detail, for the sake of convenience, the cross-sectional view showing the device structure will not be partially enlarged according to the general scale, and the schematic view is only an example, which should not limit the scope of protection of the present invention. In addition, in actual production, the three-dimensional space dimensions of length, width and depth should be included.

[0038] For ease of description, spatial relational terms such as "under", "below", "below", "below", "above", "on", etc. may be used herein to describe the relationship of one element or feature shown in the drawings to other elements or features. It will be understood that these spatial relational terms are intended to include other directions of the device in use or operation in addition to the directions depicted in the drawings. In addition, when a layer is referred to as being "between" two layers, it can be the only layer between the two layers, or there can be one or more intervening layers. As used herein, "between..." means including the end point values.

[0039] In the context of the present application, a structure in which a first feature is described as being "above" a second feature may include embodiments in which the first and second features are formed in direct contact, and may also include embodiments in which additional features are formed between the first and second features, such that the first and second features may not be in direct contact.

[0040] It should be noted that the illustrations provided in this embodiment are only used to illustrate the basic concept of the present invention in a schematic manner, and therefore the illustrations only show components related to the present invention rather than being drawn according to the number, shape and size of components in actual implementation. In actual implementation, the type, quantity and proportion of each component may be changed arbitrarily, and the component layout may also be more complicated.

[0041] like Figure 1As shown in the figure, the complete silicon-based integrated circuit process flow can be classified into front-end process (FEOL), middle-end process (MOL) and back-end process (BEOL) according to the process module set. Front-end process (FEOL): The process of forming active MOS devices such as transistors at the bottom of the chip, mainly including shallow trench isolation, source and drain, gate, etc. Middle-end process (MOL): The main function of the middle-end process is to connect the front-end device with the first layer of metal in the back-end. The main process is the etching and deposition of tungsten plugs in the contact holes. Back-end process (BEOL): The formation of interconnects that can transmit electrical signals to various devices, mainly including intermetallic dielectric layer deposition, metal line formation, lead pads (Pad, also known as pads) and other processes.

[0042] like Figure 1 As shown, through the above chip manufacturing process, a front-end process layer 11 , a middle-end process layer 12 , and a back-end process layer 13 are sequentially formed on the substrate 10 .

[0043] Specifically, the substrate 10 may include one or more semiconductor materials, and the semiconductor material may be a Group IV semiconductor, a Group III-V compound semiconductor, or a Group II-VI compound semiconductor, for example, Si, SiGe, SiC, or the like; the substrate may also be an epitaxial layer, a silicon-on-insulator (SOI) layer, a semiconductor-on-insulator (SeOI) layer, or the like.

[0044] The front-end process layer 11 includes multiple circuit units 111, and the circuit units 111 include one of transistors, capacitors, and resistors; the transistor includes a source region, a drain region, a gate electrode, an active region and other structures, and the transistor can be a MOSFET, FinFET and other types, which are not overly limited here.

[0045] The middle process layer 12 includes a plug structure electrically connected to the front process layer 11, the plug structure includes a vertically arranged metal plug 121 and a dielectric layer 122 surrounding the metal plug 121, the metal plug 121 is made of Cu, W, Ta, Ti, Al or a combination thereof, and is used to be electrically connected to the circuit unit; the dielectric layer 122 can be composed of silicon oxide, silicon nitride, silicon oxynitride or a combination thereof.

[0046] The back-end process layer 13 includes a multi-layer wiring structure electrically connected to the middle process layer 12, the wiring structure includes a metal layer 131 and a dielectric layer 122 surrounding the metal layer 131, the metal layer 131 is made of Cu, W, Ta, Ti, Al or a combination thereof, and is electrically connected to the metal plug 121; the dielectric layer 122 can be made of silicon oxide, silicon nitride, silicon oxynitride or a combination thereof. A conductive channel is formed through the wiring structure to realize power supply to the circuit unit of the front-end process layer.

[0047] In the entire chip structure, the front-end process layer 11 located on the substrate 10 carries the design of the integrated circuit device. For the product development stage, this front-end process layer is the core area of ​​the circuit design. For failure observation, this layer is the most subtle part and is also the area most prone to abnormalities. Therefore, observing the substrate is a very important link in the integrated circuit.

[0048] For the prepared chip structure, the middle process layer 12 and the back process layer 13 need to be removed to observe the front process layer. The removal process requires the middle process layer and the back process layer to be corroded and removed by chemical methods to expose the substrate layer. However, the etching rate cannot be effectively controlled during the chemical reaction process, resulting in uneven surface during the processing. As a result, the surface of the front process layer will have obvious height differences or even over-etching after the chemical reaction, and high-quality substrate images cannot be obtained under a microscope.

[0049] Therefore, the present application proposes a chip de-layering method to remove the upper wiring layer to obtain a substrate layer with a flat surface, which is convenient for observation and analysis.

[0050] Embodiment 1

[0051] This embodiment provides a chip de-layering method, comprising the following steps:

[0052] S1: Provide chips, such as Figure 1 As shown, the chip includes a substrate 10, a front-end process layer 11, a middle-end process layer 12 and a back-end process layer 13 which are stacked in sequence.

[0053] Specifically, the substrate 10 may include one or more semiconductor materials, and the semiconductor material may be a group IV semiconductor, a group III-V compound semiconductor, or a group II-VI compound semiconductor, for example, Si, SiGe, SiC, etc. The substrate may also be an epitaxial layer, a silicon-on-insulator (SOI) layer, a semiconductor-on-insulator (SeOI) layer, etc. The front-end process layer.

[0054] The front-end process layer 11 includes multiple circuit units 111, and the circuit units 111 include one of transistors, capacitors, and resistors; the transistor includes a source region, a drain region, a gate electrode, an active region and other structures, and the transistor can be a MOSFET, FinFET and other types, which are not overly limited here.

[0055] The middle process layer 12 includes a plug structure electrically connected to the front process layer 11, the plug structure includes a vertically arranged metal plug 121 and a dielectric layer 122 surrounding the metal plug 121, the metal plug 121 is made of Cu, W, Al or a combination thereof, and is used to be electrically connected to the circuit unit; the dielectric layer 122 can be composed of silicon oxide, silicon nitride, silicon oxynitride or a combination thereof.

[0056] The back-end process layer 13 includes a multi-layer wiring structure electrically connected to the middle process layer 12, the wiring structure includes a metal layer 131 and a dielectric layer 122 surrounding the metal layer 131, the metal layer 131 is made of Cu, Ta, Ti, Al or a combination thereof, and is used to electrically connect to the metal plug; the dielectric layer 122 can be made of silicon oxide, silicon nitride, silicon oxynitride or a combination thereof. A conductive channel is formed through the wiring structure to realize power supply to the circuit unit of the front-end process layer.

[0057] Next, step S2 is performed: pre-processing the chip to achieve thinning, such as Figure 2 As shown, several layers of wiring structures of the chip back-end process layer 13 away from the middle process layer 12 are removed, so that the number of wiring structure layers retained in the back-end process layer 13 does not exceed 5 layers; the pretreatment includes physical method, chemical method and machine etching method.

[0058] Specifically, as an example, the chip is delayered by a physical method, which includes mechanical grinding. The chip is first fixed on a workbench and then ground by a grinding disc. During the grinding process, a grinding liquid including materials such as aluminum oxide and silicon oxide is added. The particles in the grinding liquid physically rub against the surface of the chip to remove compounds from the surface of the wafer. The fine residue is carried away with the water flow, and then the chip surface is blown dry and spun dry by high-purity nitrogen. During the grinding process, coarse grinding can be performed first and then fine grinding can be performed to obtain higher processing accuracy.

[0059] As another example, the chip is de-layered by chemical methods. The chip is immersed in a corresponding reaction solution. The reaction solution can react with the material of the back-end process layer to achieve de-layering. Since the structure of the back-end process layer includes a metal layer and a dielectric layer, de-layering can be achieved by introducing corresponding chemical reagents for reaction. Taking the dielectric layer as silicon dioxide and the metal layer as Cu as an example, nitric acid (HNO 3 ) solution can react with Cu, and hydrofluoric acid (HF) can react with silicon dioxide. Therefore, by immersing the chip in the corresponding reaction solution and controlling the reaction conditions, several layers of wiring structures on the upper layer can be removed. Depending on the materials of the metal layer and the dielectric layer, the corresponding reaction solution is selected, and the reaction solution is not excessively limited here.

[0060] As another example, the chip is removed by machine etching, and dry etching is preferred in this embodiment. Compared with wet etching, dry etching uses plasma to etch thin films, which has less pollution and can be anisotropic. It is widely used in metal etching, dielectric etching and silicon etching processes in integrated circuit manufacturing. Currently commonly used etching technologies include, for example, reactive ion etching (RIE) and high-density plasma (HDP) etching, among which RIE has become the most widely used mainstream etching technology in integrated circuit manufacturing processes, and is also the etching technology commonly used for metal etching.

[0061] It should be noted that the above three methods (physical method, chemical method, machine etching method) can be selected at any one during the de-layering process, or any combination thereof can be used. The specific method can be flexibly selected according to the actual chip structure, and no excessive limitation is made here. As a preferred solution, during the thinning process, the three process methods of physical method, chemical method, and machine etching method are carried out in sequence, that is, gradually transitioning from coarse grinding to fine etching, gradually improving the process accuracy, and taking into account flatness and process efficiency.

[0062] The treatment process of this step is conducive to improving the flatness of the surface. If the chip is directly immersed in a chemical solution to remove the back-stage process layer and the middle stage process layer at one time, a long reaction time is required, and the whole process cannot be controlled. Because the reaction process will proceed in the form of fast edges and slow middle, the chip is removed as a whole layer at the beginning, but as more layers are removed, the chip will have irregular edge wear, the edge will be worn faster and the middle will be worn slower. The longer reaction time will cause a larger height difference between the edge and the middle. Therefore, first undergo a short pretreatment in this step to remove part of the upper wiring structure layer to ensure that the number of wiring structure layers retained in the middle area of ​​the chip differs from the number of wiring structure layers retained in the edge area of ​​the chip by no more than 2 layers, and then gradually remove them through the subsequent S3.

[0063] Next, step S3 is performed: placing the pretreated chip in an acid- and alkali-resistant beaker 21, such as Figure 3 to Figure 4 As shown, a chemical solution is used to perform a chemical reaction to remove the middle process layer and the back process layer, thereby exposing the front process layer. The entire reaction process is controlled within 3 to 20 minutes.

[0064] Specifically, the chemical solution includes one of an acidic solution and an alkaline solution. Similar to the chemical method in step S2, the alkaline solution includes one of ammonia water, sodium hydroxide and other solutions, and the acidic solution includes one of hydrofluoric acid, nitric acid, acetic acid and other solutions. The specific solution type needs to be selected according to the material. For example, when the material of the metal plug of the middle metal layer is tungsten, a mixed solution of hydrofluoric acid, nitric acid and acetic acid or a mixed solution of EDTA, hydrogen peroxide and ammonia water can be used; for titanium metal, a mixed solution of hydrogen peroxide and ammonia water can be used for removal. For aluminum metal, sodium hydroxide or hydrochloric acid can be used for removal; for copper metal, a nitric acid solution can be used for removal.

[0065] Furthermore, as an implementation method, since the materials of the metal layer and the dielectric layer in the wiring structure are different, the middle process layer and the back process layer can be removed in a cyclic alternating manner. First, the pretreated chip is placed in a first chemical solution, and the metal layer in the wiring structure located on the outermost layer is removed by the first chemical solution. Then, it is placed in a second chemical solution, and the dielectric layer in the wiring structure located on the outermost layer is removed by the second chemical solution. This cycle is repeated and the entire middle process layer and the back process layer are removed.

[0066] Next, step S4 is performed: flatness treatment is performed, including coating an organic film 141, and coating the exposed surface of the front-stage process layer with an organic film 141, thereby compensating for the ups and downs of the surface of the front-stage process layer and obtaining a flat surface. The thickness of the organic film is controlled to be 300-100nm, and the ups and downs of the structure are filled with organic materials to reduce the scattering of the optical microscope, thereby improving the image clarity.

[0067] In summary, the present invention provides a chip de-layering method, which first thins the chip through pretreatment and removes several layers of wiring structure on the top; then the chip is placed in a beaker to completely remove the middle process layer and the back process layer through chemical reaction to reveal the front process layer. Compared with soaking the chip in a chemical solution to remove the back process layer and the middle process layer at one time, the pretreatment process of the present invention is conducive to improving the flatness of the chip surface. Because the reaction process will be carried out in the form of fast edge and slow middle, the chip will have irregular edge wear, fast edge wear, slow middle wear, and a long reaction time will result in a large height difference between the edge and the middle. Therefore, after a short period of pretreatment, part of the upper wiring structure layer is removed to ensure that the number of wiring structure layers retained in the middle area of ​​the chip is no more than 2 layers different from the number of wiring structure layers retained in the edge area of ​​the chip, and then it is finally removed through subsequent chemical reactions. In addition, the present invention also coats the surface of the exposed front process layer with an organic film, thereby compensating for the ups and downs of the surface of the front process layer, obtaining a flat surface, thereby reducing the scattering of the optical microscope, and thus improving the image clarity.

[0068] The above embodiments are merely illustrative of the principles and effects of the present invention, and are not intended to limit the present invention. Anyone familiar with the art may modify or alter the above embodiments without departing from the spirit and scope of the present invention. Therefore, all equivalent modifications or alterations made by a person of ordinary skill in the art without departing from the spirit and technical concept disclosed by the present invention shall still be covered by the claims of the present invention.

Claims

1. A chip de-layering method, characterized in that: The steps include: Providing a chip, the chip comprising a substrate, a front-end process layer, a middle-end process layer and a back-end process layer stacked in sequence; Pre-process the chip to remove several layers of wiring structures of the chip's back-end process layer away from the middle process layer; The pre-treated chip is placed in an acid- and alkali-resistant beaker, and a chemical solution is used to perform a chemical reaction to remove the middle process layer and the back process layer, revealing the front process layer; Flatness treatment is performed, and an organic film is coated to compensate for the ups and downs of the surface of the previous process layer to obtain a flat surface.

2. The chip de-layering method according to claim 1, characterized in that: Several layers of wiring structures in the back-end process layer of the chip away from the middle process layer are removed, so that the number of wiring structure layers retained in the back-end process layer does not exceed 5 layers, and the number of wiring structure layers retained in the middle area of ​​the chip differs from the number of wiring structure layers retained in the edge area of ​​the chip by no more than 2 layers.

3. The chip de-layering method according to claim 1, characterized in that: The thickness of the coated organic film is controlled at 300-100 nm.

4. The chip de-layering method according to claim 1, characterized in that: Methods for preprocessing chips include physical methods, chemical methods, and machine etching methods.

5. The chip de-layering method according to claim 4, characterized in that: The physical method includes mechanical grinding, which involves first fixing the chip on a workbench and then grinding the chip with a grinding disk to remove the layers.

6. The chip de-layering method according to claim 4, characterized in that: The chemical method involves immersing the chip in a reaction solution that reacts with the material of the subsequent process layer to achieve delamination.

7. The chip de-layering method according to claim 4, characterized in that: The machine etching method includes dry etching, which uses plasma to etch and remove layers.

8. The chip de-layering method according to claim 1, characterized in that: The pretreated chip is placed in an acid- and alkali-resistant beaker for a chemical reaction time of 3 to 20 minutes.

9. The chip de-layering method according to claim 1, characterized in that: The pretreated chip is placed in an acid- and alkali-resistant beaker, and the chemical solution for chemical reaction includes one of an acidic solution and an alkaline solution. The alkaline solution includes one of ammonia water and sodium hydroxide, and the acidic solution includes one of hydrofluoric acid, nitric acid, and acetic acid.

10. The chip de-layering method according to claim 1, characterized in that: The process of placing the pre-treated chip in an acid- and alkali-resistant beaker for chemical reaction includes: First, the pretreated chip is placed in the first chemical solution, and the metal layer in the wiring structure located on the outermost layer is removed by the first chemical solution. Then, the chip is placed in the second chemical solution, and the dielectric layer in the wiring structure located on the outermost layer is removed by the second chemical solution. The entire middle process layer and the back process layer are removed alternately in a cycle.

Citation Information

Cited By

  • Chip processing method

    CN120527230A