PCB laser drilling process

By laminating a light-absorbing film onto the PCB surface and removing it after laser drilling, the problems of long process flow, high cost, and unstable quality in existing PCB laser drilling processes are solved, achieving efficient and low-cost laser drilling results and reducing environmental pollution.

CN118900505AInactive Publication Date: 2024-11-05ZHONGSHAN XINCHENG SEMICON CO LTD
View PDF 8 Cites 0 Cited by

Patent Information

Application Number
CN202411115116.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-14
Publication Date
2024-11-05
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Existing PCB laser drilling processes suffer from problems such as long process flow, high cost, unstable quality, and potential damage to the board surface. In particular, issues such as missing holes and abnormal hole diameters exist in the pattern windowing and browning/blackening pretreatment methods.

Method used

A light-absorbing film is laminated onto the surface of the PCB blank. The adhesion between the light-absorbing film and the PCB is ensured by a vacuum laminating machine. The light-absorbing film is removed after laser drilling. The light-absorbing film is preferably a black polyester film with a thickness of 3 to 10 μm, covering the entire surface or a local area.

Benefits of technology

It improves the efficiency of laser drilling, reduces the difficulty, cost and time of pretreatment, avoids the negative impact of pretreatment on drilling quality, maintains the quality of finished products, and reduces environmental pollution.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention discloses a PCB laser drilling technology. The PCB laser drilling technology comprises the following steps that firstly, a PCB blank to be drilled is provided; 2, laminating a layer of light absorption film on the to-be-drilled surface of the PCB blank by using a vacuum film laminator; step 3, performing laser drilling on the PCB blank; and 4, removing the light absorption film on the surface of the PCB blank.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a PCB laser drilling process. Background Art

[0002] At present, laser drilling technology has been widely used in the PCB manufacturing process. In order to improve the drilling efficiency when laser drilling PCB, it is often necessary to pre-process the PCB. There are two common pre-processing methods, one is graphic windowing, and the other is brown-blackening. The process flow involved in graphic windowing generally includes "pre-treatment-film lamination-exposure-development-etching-AOI-laser drilling-cleaning". The process flow is long and the cost is high, and the quality of windowing will directly affect the quality of laser drilling. The process flow involved in brown-blackening generally includes "brown-blackening-laser drilling-de-brown-blackening". Although the process flow is relatively simple, it must be carried out in conjunction with a wet process horizontal line or gantry line. The initial investment is high, and the brown-blackening process may cause copper leakage on the board surface due to roller marks or panel scratches, which will eventually cause leakage holes, abnormal apertures and other problems during laser drilling.

[0003] Therefore, how to overcome the above-mentioned defects has become an important issue to be solved urgently by those skilled in the art. Summary of the invention

[0004] The present invention overcomes the deficiencies of the above-mentioned technologies and provides a PCB laser drilling process.

[0005] To achieve the above object, the present invention adopts the following technical solutions:

[0006] A PCB laser drilling process comprises the following steps:

[0007] Step 1: Provide a PCB blank to be drilled;

[0008] Step 2: Use a vacuum laminator to press a layer of light-absorbing film on the side of the PCB blank to be drilled;

[0009] Step 3: Laser drilling of PCB blanks;

[0010] Step 4: Remove the light-absorbing film on the surface of the PCB blank.

[0011] Preferably, the light-absorbing film is a black film.

[0012] Preferably, the black film is a black polyester film.

[0013] Preferably, the light absorbing film has a thickness of 3 to 10 μm.

[0014] Preferably, the PCB laser drilling process in this case also includes step five: cleaning the formed holes.

[0015] Preferably, in step 4, the light-absorbing film is removed by manually tearing off the film on the PCB blank, or in step 4, the light-absorbing film is removed by tearing off the film on the PCB blank by a film tearing machine.

[0016] Preferably, the light-absorbing film completely covers the surface of the PCB blank, or the light-absorbing film only covers a local area of ​​the surface of the PCB blank where holes need to be drilled.

[0017] Compared with the prior art, the present invention has the following beneficial effects:

[0018] In this case, the PCB laser drilling process will use a vacuum laminator to press a layer of light-absorbing film on the surface of the PCB blank before laser drilling. The light-absorbing film allows the surface of the PCB blank to absorb laser energy more efficiently, thereby achieving the purpose of improving the efficiency of laser drilling. Moreover, lamination by a vacuum laminator can effectively ensure the fit between the light-absorbing film and the PCB blank, while improving the lamination efficiency and consistency, and avoiding the quality of subsequent laser drilling affected by uneven lamination. Compared with traditional graphic window opening and brown-black pretreatment methods, this process can greatly reduce the difficulty, cost and time of pretreatment. Moreover, the process of this case can effectively avoid the negative impact of graphic window opening quality on laser drilling. At the same time, the pretreatment process of this process will not damage the PCB blank and affect the quality of the finished product. DETAILED DESCRIPTION

[0019] The features of the present invention and other related features are further described in detail below through embodiments to facilitate understanding by those skilled in the art:

[0020] A PCB laser drilling process comprises the following steps:

[0021] Step 1: Provide a PCB blank to be drilled;

[0022] Step 2: Use a vacuum laminator to press a layer of light-absorbing film on the side of the PCB blank to be drilled;

[0023] Step 3: Laser drilling of PCB blanks;

[0024] Step 4: Remove the light-absorbing film on the surface of the PCB blank.

[0025] As mentioned above, before laser drilling, the PCB laser drilling process in this case will use a vacuum laminator to press a layer of light-absorbing film on the surface of the PCB blank. The light-absorbing film allows the surface of the PCB blank to absorb laser energy more efficiently, thereby achieving the purpose of improving the efficiency of laser drilling. Moreover, lamination by a vacuum laminator can effectively ensure the fit between the light-absorbing film and the PCB blank, while improving the lamination efficiency and consistency, and avoiding the quality of subsequent laser drilling affected by uneven lamination. Compared with the traditional pretreatment methods of graphic window opening and brown-blackening, the process of this case can greatly reduce the difficulty, cost and time of pretreatment. Moreover, the process of this case can effectively avoid the negative impact of the quality of graphic window opening on laser drilling, and the pretreatment process of this case will not damage the PCB blank and affect the quality of the finished product.

[0026] Preferably, the light-absorbing film is a black film. Thus, the use of the black film as the light-absorbing film can achieve the purpose of improving the laser energy absorption efficiency.

[0027] Preferably, the black film is a black polyester film. In this way, the good thermal stability of the polyester film can ensure that the light-absorbing film will not be ablated at a low temperature, thereby ensuring that the absorption efficiency of laser energy can be maintained at a high level for a long time. In this way, the light-absorbing film can not only improve the efficiency of laser energy absorption but also ensure that such high-efficiency absorption can be sustained. In addition, the polyester film has good recyclability and biodegradability, so that the light-absorbing film waste generated after laser drilling can be prevented from polluting the environment.

[0028] Preferably, the light absorbing film has a thickness of 3 to 10 μm.

[0029] As described above, using a light-absorbing film with a thickness of 3 to 10 μm can ensure the light-absorbing effect of the light-absorbing film while allowing the light-absorbing film to have better thermal conductivity, thereby avoiding uneven temperature distribution in the drilling area due to excessive thickness of the light-absorbing film, which affects processing efficiency.

[0030] Preferably, the PCB laser drilling process in this case also includes step five: cleaning the formed holes, so as to avoid the light-absorbing film remaining at the holes and affecting the subsequent process flow of the PCB blank and the quality of the PCB finished product.

[0031] Preferably, in step four, the light-absorbing film is removed by manually tearing off the film on the PCB blank, or in step four, the light-absorbing film is removed by tearing off the film on the PCB blank by a film tearing machine. In this way, after the light-absorbing film on the surface of the PCB blank is torn off, the PCB blank can quickly enter the next process flow.

[0032] Preferably, the light-absorbing film completely covers the surface of the PCB blank, or the light-absorbing film only covers the local area of ​​the PCB blank surface where holes need to be drilled. In this way, different covering schemes can be selected according to the efficiency and cost requirements of different products, so that the comprehensive benefits of laser drilling are higher.

[0033] As mentioned above, this case protects a PCB laser drilling process, and all technical solutions that are the same or similar to this case should be deemed to fall within the scope of protection of this case.

Claims

1. A PCB laser drilling process, characterized in that The following steps are involved: Step 1: Provide a PCB blank to be drilled; Step 2: Use a vacuum laminator to press a layer of light-absorbing film on the side of the PCB blank to be drilled; Step 3: Laser drilling of PCB blanks; Step 4: Remove the light-absorbing film on the surface of the PCB blank.

2. A PCB laser drilling process according to claim 1, characterized in that The light absorbing film is a black film.

3. A PCB laser drilling process according to claim 2, characterized in that The black film is a black polyester film.

4. A PCB laser drilling process according to any one of claims 1 to 3, characterized in that The light absorption film has a thickness of 3 to 10 μm.

5. A PCB laser drilling process according to claim 1, characterized in that The method also includes step five: cleaning the formed holes.

6. A PCB laser drilling process according to claim 1, characterized in that In the step 4, the light-absorbing film is removed by manually tearing off the film of the PCB blank, or in the step 4, the light-absorbing film is removed by tearing off the film of the PCB blank by a film tearing machine.

7. A PCB laser drilling process according to claim 1, characterized in that The light-absorbing film completely covers the surface of the PCB blank, or the light-absorbing film only covers a local area of ​​the PCB blank surface where holes need to be drilled.

Citation Information

Patent Citations

  • Photosensitive resin composition, photosensitive film, method for forming pattern by using the photosensitive film, and printed board

    CN101652716A

  • Direct laser drilling method for processing blind hole of circuit board

    CN103313532A

  • Manufacturing method of solder mask layer of circuit board

    CN115226318A

  • Manufacturing method of odd-number-layer laminated circuit board with CORE structure

    CN116507047A

  • Wiring board, method of multilayer the same and surface protective film

    JP2002344144A