Waterproof cloth surface dedusting coating process
By detecting cracks in the base fabric and applying adhesive to create wrinkles, the problem of production downtime caused by base fabric breakage was solved, and efficient production of waterproof fabric was achieved.
Patent Information
- Application Number
- CN202411330203.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-24
- Publication Date
- 2024-11-08
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
In existing technologies, when the base fabric breaks, the machine needs to be stopped for replacement, resulting in low production efficiency and increased costs.
The base fabric is inspected for cracks by taking photos. The base fabric is then evenly coated with adhesive using an adhesive coating mechanism. Cracks and wrinkles are formed on the drying mechanism. The base fabric is then bonded using a horizontal pressure plate and a drying roller. Finally, a wiping mechanism is used to clean up any remaining adhesive, thus enabling continuous production of the base fabric.
This effectively prevents the base fabric from breaking, ensuring production continuity and quality, reducing production costs, and improving production efficiency.
Smart Images

Figure CN118904683A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of waterproof cloth production, in particular to a dust removal coating process for the surface of waterproof cloth. Background Art
[0002] The waterproofing process of waterproof cloth mainly depends on coating a waterproof layer on the base cloth. The waterproof layer can form a dense rubber surface on the surface of the base cloth. The rubber surface can make the surface of the waterproof cloth smoother while being waterproof, ensuring its aesthetics.
[0003] When producing waterproof cloth, the base cloth needs to be processed. However, when the base cloth is damaged, it is very easy to break on a large scale under the action of tension, thus affecting the coating of the glue. If the broken part of the base cloth is directly cut off, the base cloth needs to be redirected, which affects the production efficiency of the base cloth and increases the production cost of the waterproof cloth. Summary of the invention
[0004] The purpose of the invention is to provide a dust removal coating process for the surface of a waterproof cloth.
[0005] The technical problem solved by the present invention is to solve the problem in the prior art that when the base cloth breaks, the machine needs to be stopped to replace the base cloth, which causes production stoppage and affects production efficiency.
[0006] The present invention can realize a dust removal coating process on the surface of waterproof cloth through the following technical scheme, including the following steps:
[0007] Diagnostic operation: detect the base fabric by taking photos to determine whether there are cracks on the base fabric and obtain the moving speed of the base fabric;
[0008] Gluing operation: moving the base fabric from the glue coating mechanism and evenly coating the base fabric with glue by using the glue coating mechanism;
[0009] The wrinkle processing operation forms wrinkles on the base fabric after the glue is applied by using the second drying mechanism according to the crack position of the base fabric and the moving speed of the base fabric.
[0010] A further technical improvement of the present invention is that a first drying operation is provided between the diagnosis operation and the gluing operation, the base fabric is moved from the first drying mechanism, and the base fabric is dried by the first drying mechanism.
[0011] A further technical improvement of the present invention is that a tension adjustment operation is provided after the pleating operation, and the tension adjustment mechanism is used to control the tightness of the base fabric.
[0012] A further technical improvement of the present invention is that in the process of forming cracks and wrinkles on the base cloth coated with glue, the second drying roller is used to press the crack position of the base cloth down to the position of the first horizontal pressing plate and the second horizontal pressing plate, and the first horizontal pressing plate and the second horizontal pressing plate are used to press the crack position of the base cloth horizontally.
[0013] A further technical improvement of the present invention is that when the first transverse pressure plate and the second transverse pressure plate are in operation, the first transverse pressure telescopic rod is used to start controlling the movement of the first transverse pressure plate, and the second transverse pressure telescopic rod is used to control the movement of the second transverse pressure plate until the transverse pressure protrusion enters the interior of the matching transverse pressure groove.
[0014] A further technical improvement of the present invention is that when the second drying roller is in use, the downward pressing protrusion is controlled to be in a vertical downward state by rotating the second drying roller, and the height of the second drying roller is controlled by starting the drying telescopic rod until the downward pressing protrusion acts on the base fabric.
[0015] A further technical improvement of the present invention is that it also includes a wiping operation, in which a wiping slider is driven by a power mechanism to act on the pressing protrusion to scrape off the glue on the pressing protrusion.
[0016] A further technical improvement of the present invention is that when the power mechanism is started, the wiping motor is used to control the wiping screw, thereby controlling the movement of the wiping sliding base arranged at the output end of the wiping screw, driving the sliding of the wiping slider.
[0017] Compared with the prior art, the present invention has the following beneficial effects:
[0018] 1. The present application utilizes diagnostic operations to monitor the base fabric in real time by means of photographic detection to determine whether there are cracks in the base fabric. When there are cracks in the base fabric, based on the crack positions and the moving speed of the base fabric, the base fabric is coated with glue and then the pleating operation step is reached. That is, in this process, the crack positions and non-crack positions of the base fabric are bonded by gluing to avoid the influence of the cracks on the gluing operation of the base fabric, thereby ensuring the production quality of the base fabric and solving the problem of the base fabric being broken due to the gradual enlargement of the cracks in the base fabric.
[0019] 2. The present application uses the first transverse pressure telescopic rod to start and control the movement of the first transverse pressure plate, and uses the second transverse pressure telescopic rod to control the movement of the second transverse pressure plate, until the transverse pressure protrusion enters the interior of the matching transverse pressure groove, so that the crack position and non-crack position of the base fabric can be bonded, thereby achieving the processing of the crack position of the base fabric.
[0020] 3. The present application utilizes a wiping motor to control the wiping screw, thereby controlling the movement of a wiping sliding base disposed at the output end of the wiping screw, driving the sliding of the wiping slider, that is, utilizing the wiping slider to act on the pressing protrusion under the driving action of a power mechanism to scrape off the glue on the pressing protrusion, thereby ensuring the cleanliness of the pressing protrusion and facilitating the reuse of the pressing protrusion. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] In order to facilitate understanding by those skilled in the art, the present invention is further described below with reference to the accompanying drawings.
[0022] Figure 1 is a process flow chart of the present invention;
[0023] Figure 2 It is a schematic diagram of the position of the second drying mechanism of the present invention;
[0024] Figure 3 It is a schematic diagram of the position of the rotating glue coating roller of the present invention;
[0025] Figure 4 It is a structural schematic diagram of the second drying mechanism of the present invention;
[0026] Figure 5 It is a schematic diagram of the position of the wiping mechanism of the present invention;
[0027] Figure 6 For the present invention Figure 5 A partial enlarged view of the middle A;
[0028] Figure 7 The present invention is a schematic diagram of the relative positions of the transverse pressing protrusion and the matching transverse pressing groove.
[0029] In the figure: 1. first drying mechanism; 11. first telescopic rod; 12. drying rotating roller; 2. gluing mechanism; 21. rotating gluing roller; 22. second telescopic rod; 3. second drying mechanism; 31. drying telescopic rod; 32. first horizontal pressure plate; 33. first horizontal pressure telescopic rod; 34. downward pressure base; 35. downward pressure protrusion; 36. second drying roller; 37. second horizontal pressure telescopic rod; 38. matching horizontal pressure groove; 39. horizontal pressure protrusion; 310. wiping motor; 311. wiping screw base; 312. wiping sliding base; 313. matching wiping groove; 314. wiping slider; 315. wiping telescopic rod; 316. second horizontal pressure plate; 4. tension adjustment mechanism; 41. adjusting telescopic rod; 42. tension roller; 5. winding mechanism. DETAILED DESCRIPTION
[0030] In order to further explain the technical means and effects adopted by the present invention to achieve the predetermined invention purpose, the specific implementation mode, structure, characteristics and effects of the present invention are described in detail below in combination with the accompanying drawings and preferred embodiments.
[0031] See also Figure 1-7 As shown, a dust removal coating process for the surface of a waterproof cloth comprises the following steps:
[0032] Step 1: Diagnostic operation: take a photo of the base fabric to determine whether there are cracks on the base fabric, and monitor the position of the cracks in real time according to the transmission speed of the base fabric;
[0033] Step 2: a first drying operation, moving the primary base fabric from the first drying mechanism 1, and drying the primary base fabric by using the first drying mechanism 1;
[0034] Step 3: Gluing operation, moving the base fabric from the glue coating mechanism 2, and using the glue coating mechanism 2 to evenly coat the base fabric with glue, the glue coating operation includes coating the position of the crack;
[0035] Step 4, a second drying operation, using the second drying mechanism 3 to process the primary base fabric, so that the rest of the primary base fabric is dried, and the cracked position of the primary base fabric is folded and dried after folding, so as to ensure the tightness of the connection of the primary base fabric and avoid the possibility of the primary base fabric being broken;
[0036] Step 5, the tension adjustment operation, using the tension adjustment mechanism 4 to control the tightness of the base fabric, and at the same time using the tension adjustment mechanism 4 to re-coat the processed surface of the base fabric, so that the base fabric is dried in turn from the second drying mechanism 3, and the base fabric is coated for the second time using the glue coating mechanism 2, and then the first drying mechanism 1 is used to fully dry the base fabric.
[0037] When used in the tightness adjustment operation, when cracks appear on the base fabric, the crack parts of the base fabric are attached to control the tightness of the base fabric. After the attachment treatment of the base fabric is completed, the tightness of the base fabric is controlled to ensure the normal use of the base fabric.
[0038] When the second drying operation is used, the rotation of the second drying roller 36 makes the pressing protrusion 35 rotate to the lowest end, and the pressing protrusion 35 is used to squeeze the base fabric coated with glue between the adjacent first cross pressing plate 32 and the second cross pressing plate 316, and the relative movement of the first cross pressing plate 32 and the second cross pressing plate 316 is used to achieve preliminary squeezing of the base fabric. At this time, there is a pressing protrusion 35 between the first cross pressing plate 32 and the second cross pressing plate 316, and then the drying telescopic rod 31 is started to control the longitudinal movement of the second drying roller 36, that is, the pressing protrusion 35 is controlled to move out from between the first cross pressing plate 32 and the second cross pressing plate 316. At this time, the first cross pressing plate 32 and the second cross pressing plate 316 directly squeeze the base fabric with cracks, so as to achieve adhesion and overlap of the positions with cracks, and then the second drying roller 36 is rotated back to its original position, and the heating and hot air flow of the second drying roller 36 are used to dry the glue to achieve drying of the glue, so that the base fabric with cracks can be adhered to the position without cracks.
[0039] When the first transverse pressing plate 32 and the second transverse pressing plate 316 move toward each other, the transverse pressing protrusion 39 on the first transverse pressing plate 32 enters into the interior of the matching transverse pressing groove 38 of the second transverse pressing plate 316 to form a wrinkle on the base fabric, which is convenient for later cutting but does not affect the normal processing of the base fabric, thereby ensuring the normal processing of the waterproof fabric, maintaining the production efficiency of the waterproof fabric, and ensuring the production quality of the waterproof fabric.
[0040] When the pressing protrusion 35 is used, the wiping slider 314 is controlled by the wiping telescopic rod 315 to be inserted into the interior of the pressing protrusion 35, and then the wiping slider 314 is driven to slide by the wiping motor 310, so that the wiping slider 314 acts on the pressing protrusion 35 to scrape off the residual glue on the pressing protrusion 35, thereby ensuring the next use of the pressing protrusion 35.
[0041] The present application includes a first drying mechanism 1 for performing preliminary drying treatment on the base fabric, a gluing mechanism 2 for gluing the base fabric is arranged on the side of the first drying mechanism 1, wherein a second drying mechanism 3 for re-drying the base fabric is arranged on the side of the gluing mechanism 2, and a tension adjusting mechanism 4 for adjusting the tightness of the base fabric is arranged on the side of the second drying mechanism 3, wherein a winding mechanism 5 for winding the base fabric is arranged directly above the first drying mechanism 1. In the present application, the first drying mechanism 1 is first used to dry the base fabric to ensure that there is no moisture residue on the base fabric when gluing is performed, so as to facilitate the adhesion of the glue liquid to the base fabric and ensure the production stability of the base fabric, and then the dried base fabric is coated for the first time using the gluing mechanism 2, and then it is transferred to the second drying mechanism 3 for further drying. In the process, the glue liquid is dried, and the base fabric is adjusted by the tension adjusting mechanism 4, and then the winding function is realized by the winding mechanism 5.
[0042] The first drying mechanism 1 includes a first telescopic rod 11, wherein a drying rotating roller 12 is rotatably provided at the output end of the first telescopic rod 11, that is, an air outlet is provided on the drying rotating roller 12 for discharging drying gas and directly drying the base fabric on the drying rotating roller 12.
[0043] The gluing mechanism 2 comprises a second telescopic rod 22, at the output end of which a rotating gluing roller 21 is rotatably provided, and the rotating gluing roller 21 is provided with a plurality of glue outlets for discharging glue, so as to evenly coat the base fabric with glue.
[0044] The tension adjustment mechanism 4 comprises an adjusting telescopic rod 41 , wherein an elastic roller 42 is rotatably provided at the output end of the adjusting telescopic rod 41 , wherein the elastic roller 42 is used to adjust the tightness of the base fabric.
[0045] The second drying mechanism 3 includes a drying telescopic rod 31, a downward pressing base 34 is fixedly installed at the output end of the drying telescopic rod 31, wherein a second drying roller 36 is arranged on the downward pressing base 34 through a rotating motor, and discharge holes for exhausting drying gas are evenly opened on the second drying roller 36, and two groups of downward pressing protrusions 35 are symmetrically arranged on the second drying roller 36, and a first horizontal pressing telescopic rod 33 and a second horizontal pressing telescopic rod 37 are also fixedly installed on the frame, wherein the output end of the first horizontal pressing telescopic rod 33 is fixedly installed with a first horizontal pressing plate 32, and the output end of the second horizontal pressing telescopic rod 37 is fixedly installed with a first horizontal pressing plate 32. A second transverse pressure plate 316 is fixedly installed at the output end of the telescopic rod 37, wherein the toward-toward movement of the first transverse pressure plate 32 and the second transverse pressure plate 316 is used to squeeze the base fabric into wrinkles, and a transverse pressure protrusion 39 is fixed on the first transverse pressure plate 32, and a matching transverse pressure groove 38 for matching with the transverse pressure protrusion 39 is provided on the second transverse pressure plate 316. When in use, the wrinkled part of the base fabric can be squeezed inside the matching transverse pressure groove 38, so that under the action of the glue, the formation of wrinkles in the base fabric is achieved, thereby reducing the influence of the gaps in the base fabric on the firmness of the base fabric.
[0046] In order to clean the residual glue on the pressing protrusion 35, a wiping screw base 311 is fixedly installed on the frame, wherein a wiping motor 310 is fixed on the wiping screw base 311, wherein the wiping motor 310 drives the wiping screw, and a wiping sliding base 312 is provided at the output end of the wiping screw, wherein the wiping sliding base 312 is slidably connected to the wiping screw base 311, and a wiping telescopic rod 315 is fixed to the side of the wiping sliding base 312, which A wiping slider 314 is fixedly installed at the output end of 315, and a cooperating wiping groove 313 for cooperating with the pressing protrusion 35 is opened on the wiping slider 314. When in use, the wiping motor 310 is started to drive the wiping screw, so that the wiping sliding base 312 slides on the wiping screw base 311, so that the residual glue on the pressing protrusion 35 is wiped off by the action of the wiping slider 314, thereby reducing the influence of the residual glue on the pressing protrusion 35 on the adhesion of the base cloth.
[0047] In the present application, the first drying mechanism 1 is used to dry the base fabric to ensure that there is no water residue on the base fabric when the glue is applied, so that the glue liquid adheres to the base fabric and ensures the production stability of the base fabric. Then, the dried base fabric is coated for the first time by the glue application mechanism 2, and then it is transferred to the second drying mechanism 3 for further drying. In this process, the glue liquid is dried, and the base fabric is adjusted by the tension adjustment mechanism 4, and then the winding mechanism 5 is used to realize the winding function.
[0048] When a visual inspection mechanism for non-destructive inspection of the base fabric is also provided before the first drying mechanism 1, that is, a camera is used to detect whether there are cracks in the base fabric. If there are cracks, the time when the base fabric reaches the second drying mechanism 3 is determined according to the moving speed of the base fabric and the position of the cracks.
[0049] The second drying roller 36 is then started to dry the glue at this position quickly, thereby ensuring the continuity of the base fabric.
[0050] Then, the wiping motor 310 is started to drive the wiping screw, so that the wiping sliding base 312 slides on the wiping screw base 311, so that the residual glue on the pressing protrusion 35 is wiped off by the wiping slider 314, thereby reducing the influence of the residual glue on the pressing protrusion 35 on the adhesion of the base cloth.
[0051] The above description is only a preferred embodiment of the present invention and does not limit the present invention in any form. Although the present invention has been disclosed as a preferred embodiment as above, it is not used to limit the present invention. Any technical personnel in this field can make some changes or modify the technical contents disclosed above into equivalent embodiments without departing from the scope of the technical solution of the present invention. However, any simple modification, equivalent change and modification made to the above embodiments according to the technical essence of the present invention without departing from the content of the technical solution of the present invention still fall within the scope of the technical solution of the present invention.
Claims
1. A dust removal coating process for the surface of a waterproof cloth, characterized in that: The following steps are involved: Diagnostic operation: detect the base fabric by taking photos to determine whether there are cracks on the base fabric and obtain the moving speed of the base fabric; Gluing operation, the base fabric is continued to be moved from the glue coating mechanism (2), and the glue coating mechanism (2) is used to evenly coat the base fabric with glue; The wrinkle processing operation forms wrinkles on the base fabric after the glue is applied by using a second drying mechanism (3) according to the crack position of the base fabric and the moving speed of the base fabric.
2. A dust removal coating process for the surface of waterproof cloth according to claim 1, characterized in that: A first drying operation is provided between the diagnosis operation and the gluing operation, wherein the base fabric is moved from the first drying mechanism (1) and the first drying mechanism (1) is used to dry the base fabric.
3. A dust removal coating process for the surface of waterproof cloth according to claim 1, characterized in that: After the pleating operation, a tension adjustment operation is also provided, and the tension of the base fabric is controlled by using a tension adjustment mechanism (4).
4. A dust removal coating process for the surface of waterproof cloth according to claim 1, characterized in that: In the process of forming cracks and wrinkles on the base fabric after coating with glue, the second drying roller (36) is used to press the crack position of the base fabric down to the position of the first horizontal pressing plate (32) and the second horizontal pressing plate (316), and the first horizontal pressing plate (32) and the second horizontal pressing plate (316) are used to press the crack position of the base fabric horizontally.
5. A dust removal coating process for the surface of waterproof cloth according to claim 4, characterized in that: When the first transverse pressure plate (32) and the second transverse pressure plate (316) are operated, the first transverse pressure telescopic rod (33) is used to start and control the movement of the first transverse pressure plate (32), and the second transverse pressure telescopic rod (37) is used to control the movement of the second transverse pressure plate (316) until the transverse pressure protrusion (39) enters into the interior of the matching transverse pressure groove (38).
6. A dust removal coating process for the surface of waterproof cloth according to claim 4, characterized in that: When the second drying roller (36) is in use, the pressing protrusion (35) is controlled to be in a vertical downward state by the rotation of the second drying roller (36), and the height of the second drying roller (36) is controlled by starting the drying telescopic rod (31) until the pressing protrusion (35) acts on the base fabric.
7. A dust removal coating process for the surface of waterproof cloth according to claim 6, characterized in that: The method also includes a wiping operation, in which a wiping slider (314) is driven by a power mechanism to act on the pressing protrusion (35) to scrape off the glue on the pressing protrusion (35).
8. A dust removal coating process for the surface of waterproof cloth according to claim 7, characterized in that: When the power mechanism is started, the wiping motor (310) is used to control the wiping screw, thereby controlling the movement of the wiping sliding base (312) arranged at the output end of the wiping screw, thereby driving the sliding of the wiping slider (314).