Continuous casting slab solidification tail end forced cooling device and method based on crack control
By performing strong cooling in the solidification end area of the continuous casting blank and combining heat supplementation of the corners of the casting blank, the crack problem caused by strong cooling at the solidification end is solved, which significantly improves the internal quality of the casting blank, and solves the water volume and crack control. contradiction.
Patent Information
- Application Number
- CN202411030139.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-30
- Publication Date
- 2024-11-08
AI Technical Summary
Strong cooling at the solidified end is prone to cause corner cracks and temperature-return internal cracks when applied, and the water limiting results in limited improvement of the internal quality of the casting billet, especially under production conditions with low pull speed and high two-cold strength, the effect is extremely limited.
By installing nozzles at the solidification end area of the continuous casting blank for strong cooling, combining the heat replenishment device at the corners of the casting blank, adjust the strong cooling position and water volume, control the occurrence of internal cracks and corner cracks in the back temperature type, and ensure the internal quality of the casting blank. improve.
Effectively improve the amount of strong cold water at the solidification end, give full play to the improvement of the internal quality of the casting blank, control the internal and corner cracks caused by strong cold, and significantly improve the improvement of defects such as the center segregation, loosening, and shrinkage holes of the casting blank. Effect.
Smart Images

Figure CN118905171A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of metallurgy, and relates to a device and method for strong cooling at the solidification end of a continuous casting billet based on crack control. Background Art
[0002] With the advancement of technology and economic development, users have higher and higher requirements for the quality and performance of steel products. In the production process of steel products, internal quality defects such as central porosity, shrinkage, segregation, etc. of continuous casting billets are key factors affecting product quality and performance, and their control is particularly important. Electromagnetic stirring, light pressure reduction, and strong cooling at the end of solidification are the main measures to control the internal quality of the billet. Among them, strong cooling at the end of solidification is a method of improving the internal quality of the billet by spraying water at the end of solidification of the continuous casting billet. It has many advantages such as obvious improvement effect on the internal quality of the billet, simple equipment, and easy maintenance. However, when strong cooling at the end of solidification is applied, because its action position is close to the straightening area and it is achieved by spraying water, it is easy to cause corner cracks and regeneration type internal cracks. This problem is the main factor limiting the widespread application of strong cooling at the end of solidification.
[0003] At present, the main measures to solve the problem of cracks caused by strong cooling at the end of solidification are to control the position of strong cooling and the amount of water. The Chinese invention application with application number 202310826652.X proposes a method for controlling strong cooling at the end of solidification of continuous casting billets. The method is based on the mechanism of strong cooling at the end of solidification. The specific scheme is as follows: the starting position of strong cooling is the cooling rate of the center of the continuous casting billet at 0.2-0.6℃ / s, the solid phase ratio of the center of the continuous casting billet at the end of strong cooling is 0.85-0.90, the surface temperature recovery rate of the casting billet is within 100℃ / m, and the surface temperature of the continuous casting billet in the straightening zone is greater than the upper limit of the third brittle temperature zone of steel. The above scheme can effectively control the generation of corner cracks and regeneration type internal cracks, and improve the internal quality of the continuous casting billet to a certain extent, but there are the following problems: in order to control the surface regeneration rate within 100℃ / m and the surface temperature of the billet in the straightening zone to be greater than the upper limit of the third brittle temperature zone of steel, the amount of strong cooling water at the end of solidification cannot be too large, and the strong cooling effect is limited, resulting in limited improvement effect on the internal quality of the billet, especially under the production conditions of low pulling speed and high secondary cooling strength, the improvement effect is extremely limited.
[0004] In summary, the main contradiction in the application process of strong cooling at the end of solidification is to reduce the amount of water to control the generation of cracks and to increase the amount of water to ensure the improvement of the internal quality of the ingot. If this contradiction can be resolved, the application of strong cooling at the end of solidification will be greatly improved. Summary of the invention
[0005] In view of this, the purpose of the present invention is to provide a device and method for forced cooling at the end of solidification of continuous casting billets based on crack control, by adjusting the position of forced cooling at the end of solidification to control the generation of internal cracks of the temperature recovery type, by adopting a heating device for the corners of the billet to increase the corner temperature of the billet to control the generation of cracks at the corners of the billet, thereby solving the crack problem caused by the increase of the amount of forced cooling water at the end of solidification, and giving full play to the improvement effect of forced cooling at the end of solidification on the internal quality of the billet.
[0006] In order to achieve the above object, the present invention provides the following technical solutions:
[0007] A device for strong cooling at the end of solidification of a continuous casting billet based on crack control, comprising a nozzle and a device for supplementing heat at the edges and corners of the billet, wherein the nozzle is located in the end area of solidification of the continuous casting billet, and is used to spray water on the surface of the continuous casting billet for strong cooling in the end area of solidification of the continuous casting billet, and the device for supplementing heat at the edges and corners of the billet is located after the nozzle and before the straightening zone of the continuous casting machine, and is used to increase the temperature of the edges and corners of the continuous casting billet.
[0008] Furthermore, the nozzles are arranged in sequence along the billet drawing direction in the solidification terminal region of the continuous casting billet, and the overlap rate of the spraying water coverage ranges of two adjacent nozzles is 5% to 15%.
[0009] Furthermore, the nozzle is a conical water nozzle or a conical air-water nozzle, and the center line of the nozzle is perpendicular to the center of the surface of the continuous casting billet.
[0010] Furthermore, a plurality of nozzles are arranged in the circumferential direction of the cross section of the continuous casting billet so that the spraying water covers the outer surface of the continuous casting billet in the circumferential direction.
[0011] Furthermore, the device for heating the edges and corners of the ingot adopts flame heating or electromagnetic induction heating.
[0012] Furthermore, the nozzle is fixedly mounted on a spray frame, the spray frame is arranged along the billet drawing direction, and the length of the spray frame matches the length of the solidification terminal region of the continuous casting billet.
[0013] A method for strong cooling of the solidification end of a continuous casting billet based on crack control, using the strong cooling device for the solidification end of a continuous casting billet based on crack control, the method comprises the following steps:
[0014] S1: Calculate the temperature field of the continuous casting billet according to the process parameters of the continuous casting process;
[0015] S2: According to the temperature field of the continuous casting billet and the strong cooling mechanism at the end of the solidification of the continuous casting billet, the strong cooling parameters at the end of the solidification of the continuous casting billet are determined;
[0016] S3: According to the strong cooling parameters at the end of solidification of the continuous casting billet, the nozzle arrangement position and the amount of cooling water at the nozzle are adjusted to perform strong cooling at the end of solidification of the continuous casting billet;
[0017] S4: According to the corner temperature of the continuous casting billet after the strong cooling at the end of solidification, combined with the third brittle temperature zone of the corresponding production steel grade, determine the temperature compensation value of the billet corner heating device, and heat the continuous casting billet according to the temperature compensation value.
[0018] Furthermore, the process parameters of the continuous casting process include the type of steel produced, casting temperature, pulling speed, mold cooling water volume, mold cooling water temperature difference and secondary cooling water ratio; the strong cooling parameters at the end of the continuous casting billet solidification include the starting position and ending position of the end area of the continuous casting billet solidification and the nozzle cooling water volume.
[0019] Furthermore, the starting position of the continuous casting billet solidification terminal zone is a region where the solid phase ratio at the center of the billet is 0.30 to 0.50, and the ending position is a region where the billet is 0.2 to 1.0 m after the billet is completely solidified.
[0020] Furthermore, the amount of cooling water in the nozzle is controlled so that the cooling rate of the surface of the continuous casting billet in the terminal region of solidification of the continuous casting billet is 5 to 8 times the cooling rate of the center of the continuous casting billet.
[0021] Furthermore, the distance between the device for supplementing heating at the edges and corners of the ingot and the nozzle closest to the device for supplementing heating at the edges and corners of the ingot is greater than 1.0 m.
[0022] Furthermore, the temperature compensation value of the heating device at the corner of the ingot is calculated by the following formula:
[0023] T b =T u -T c +(20~50);
[0024] Among them, T b Indicates the temperature compensation value of the heating device at the corner of the casting, ℃; T u Indicates the upper limit of the third brittle temperature zone of the corresponding steel grade, °C; T c It indicates the corner temperature of the continuous casting billet after strong cooling at the end of solidification, ℃.
[0025] The beneficial effects of the present invention are:
[0026] The present invention provides a device and method for strong cooling of the solidification end of a continuous casting billet based on crack control. The device and method are used to strong cool the continuous casting billet in the solidification end region of the continuous casting billet through a nozzle, and the starting position of the solidification end region of the continuous casting billet is limited to be located in the region of 0.3 to 0.5 of the solid phase ratio in the center of the billet, and the ending position is located in the region of 0.2 to 1.0 m after the billet is completely solidified, so as to control the generation of internal cracks; by controlling the cooling water volume of the nozzle, the cooling rate of the billet surface in the strong cooling region is made to reach 5 to 8 times the cooling rate of the center, so as to give full play to the improvement effect of the strong cooling at the solidification end on the internal quality; after the strong cooling is completed, the temperature compensation value is performed through the billet corner heating device, so as to increase the temperature of the corner of the continuous casting billet to avoid the upper limit of the third brittle temperature zone of steel, so as to control the generation of corner cracks;
[0027] In summary, the present invention can greatly increase the amount of strong cooling water at the end of solidification, ensure the improvement effect of strong cooling at the end of solidification on internal quality defects such as central segregation, looseness, shrinkage holes, etc. of the ingot, and effectively control corner cracks and rewarming type internal cracks caused by strong cooling at the end of solidification.
[0028] Other advantages, objectives and features of the present invention will be described in the following description to some extent, and to some extent, will be obvious to those skilled in the art based on the following examination and study, or can be taught from the practice of the present invention. The objectives and other advantages of the present invention can be realized and obtained through the following description. BRIEF DESCRIPTION OF THE DRAWINGS
[0029] In order to make the purpose, technical solutions and advantages of the present invention more clear, the present invention will be described in detail below in conjunction with the accompanying drawings, wherein:
[0030] Figure 1 This is a schematic structural diagram of a solidification end strong cooling device based on crack control in an embodiment;
[0031] Figure 2 for Figure 1 AA section view;
[0032] Figure 3 for Figure 1 BB cross-sectional view;
[0033] Figure 4 This is a graph showing the change of the solid phase ratio at the center of the billet along the billet drawing direction in the embodiment;
[0034] Figure 5 It is a diagram of the cooling rate of the center of the ingot and the cooling rate of the surface of the ingot under different amounts of strong cooling water at the end of solidification in the embodiment.
[0035] Figure numerals: 1- ingot, 2- spray rack, 3- nozzle, 4- spray water, 5- heating device for ingot corners. DETAILED DESCRIPTION
[0036] The following describes the embodiments of the present invention by specific examples, and those skilled in the art can easily understand other advantages and effects of the present invention from the contents disclosed in this specification. The present invention can also be implemented or applied through other different specific embodiments, and the details in this specification can also be modified or changed in various ways based on different viewpoints and applications without departing from the spirit of the present invention. It should be noted that the illustrations provided in the following embodiments only illustrate the basic concept of the present invention in a schematic manner, and the following embodiments and features in the embodiments can be combined with each other without conflict.
[0037] Among them, the drawings are only used for illustrative explanations, and they only represent schematic diagrams rather than actual pictures, and should not be understood as limitations on the present invention. In order to better illustrate the embodiments of the present invention, some parts of the drawings may be omitted, enlarged or reduced, and do not represent the size of actual products. For those skilled in the art, it is understandable that some well-known structures and their descriptions in the drawings may be omitted.
[0038] The same or similar numbers in the drawings of the embodiments of the present invention correspond to the same or similar parts; in the description of the present invention, it should be understood that if the terms "upper", "lower", "left", "right", "front", "rear", etc. indicate the orientation or position relationship, they are based on the orientation or position relationship shown in the drawings, which is only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operate in a specific orientation. Therefore, the terms describing the position relationship in the drawings are only used for illustrative purposes and cannot be understood as limiting the present invention. For ordinary technicians in this field, the specific meanings of the above terms can be understood according to specific circumstances.
[0039] See also Figure 1 to Figure 5 , the following is a specific implementation case, targeting a square billet continuous casting machine in a steel plant, to further illustrate the device and method for strong cooling at the end of solidification of continuous casting billets based on crack control proposed in this application.
[0040] This embodiment is for a square billet continuous casting machine, the arc radius of the continuous casting machine is 10m, the cross-sectional size of the produced billet is 160mm×160mm, the produced steel grade is LX82B steel, the casting temperature is 1493℃, the casting speed is 1.6m / min, and the cooling water volume of the crystallizer is 122m 3 / h, the temperature difference between the inlet and outlet water of the crystallizer is 7.0°C, and the secondary cooling water volume is 0.80L / kg; the device and method for strong cooling at the solidification end of the continuous casting billet based on crack control proposed by the present invention are used to improve the internal quality of the casting billet.
[0041] Key References Figure 1 to Figure 3, which is a strong cooling device for the solidification end of a continuous casting billet based on crack control, and comprises a spray rack 2, a nozzle 3 and a heat supplement device 5 for the edges and corners of the billet, wherein: the nozzle 3 is fixedly mounted on the spray rack 2 and is located in the solidification end area of the continuous casting billet 1, and is used to spray spray water 4 to perform water spray strong cooling on the surface of the continuous casting billet; the heat supplement device 5 for the edges and corners of the billet is located after the nozzle 3 and before the straightening area of the continuous casting machine, and is used to increase the temperature of the edges and corners of the continuous casting billet.
[0042] Preferably, the nozzle 3 on the spray rack 2 is a conical air-water nozzle, the spray center line of the nozzle is perpendicular to the center of the continuous casting billet surface, and the overlapping rate of the spray water 4 coverage of two adjacent nozzles 3 along the billet drawing direction is 10%; the heating device 5 for the corners of the billet adopts flame heating.
[0043] Preferably, nozzles 3 are arranged on four sides of the casting billet 1 to spray the casting billet 1 in a full coverage manner in the circumferential direction.
[0044] According to the casting temperature, casting speed, mold cooling water volume, mold cooling water temperature difference, secondary cooling water ratio and other process parameters of LX82B steel, the temperature field of the continuous casting billet is calculated to obtain the center cooling rate, center solid phase ratio, surface cooling rate, etc. of the billet, and the center solid phase ratio of the billet is analyzed, such as Figure 4 As shown in the figure, the starting position of the strong cooling at the end of solidification, that is, the starting position of the spray rack, takes the solid phase ratio of the center of the billet as 0.40, and the distance from the meniscus to this position is 8.02m; the ending position of the strong cooling at the end of solidification, that is, the ending position of the spray rack, takes the position 0.8m after the billet is completely solidified, and the distance from the meniscus to the billet when it is completely solidified is 10.98m, so the ending position of the strong cooling at the end of solidification is 11.78m away from the meniscus.
[0045] Taking into account comprehensively, the distance between the strong cooling area at the end of solidification and the meniscus is 8.02 to 11.78 m. The cooling rate of the center of the ingot and the cooling rate of the surface of the ingot under different strong cooling water volumes (nozzle cooling water volumes) at the end of solidification are calculated. Figure 5 As shown. Figure 5 It can be seen that under different amounts of strong cooling water at the end of solidification, the cooling rate at the center of the billet does not change much, but the cooling rate on the surface of the billet increases rapidly. The cooling rate on the surface of the billet in the strong cooling area at the end of solidification is 6 times the cooling rate at the center of the billet. Figure 5 It can be seen that the corresponding water volume is 5.78m 3 / h, at this time, the cooling rate of the center of the billet is 1.03℃ / s, and the cooling rate of the surface of the billet is 6.18℃ / s. 1.5m after the end of the strong cooling at the solidification end, install the heating device for the corners of the billet. The calculated amount of strong cooling water at the end of solidification is 5.78m 3 / h, the temperature of the corner of the ingot after strong cooling at the end of solidification is 714℃, the upper limit of the third brittle temperature zone of LX82B steel is 750℃, and the temperature compensation value of the heating device at the corner of the ingot is calculated according to the following formula, and the temperature compensation value is 56~86℃, and the temperature compensation value is 60℃.
[0046] T b =T u -T c +(20~50)
[0047] Among them, T b Indicates the temperature compensation value of the heating device at the corner of the casting, ℃; T u Indicates the upper limit of the third brittle temperature zone of the produced steel grade, ℃; T c Indicates the temperature of the corner of the ingot after strong cooling at the end of solidification, ℃.
[0048] The above-mentioned device and method are used to perform strong cooling at the end of solidification of the ingot. The solid phase ratio of the ingot center at the start of strong cooling is 0.40, at which time the temperature of the ingot center begins to drop rapidly. Strong cooling at the end of solidification of the ingot can improve the internal quality; the end of strong cooling at the end of solidification is 11.78m away from the meniscus, which is 0.8m after the ingot is completely solidified. At this time, the crack-sensitive area inside the ingot disappears, and no internal cracks of the temperature-recovering type will occur; the amount of strong cooling water at the end of solidification (nozzle cooling water) is 5.78m 3 / h, under this water volume, the cooling rate of the billet surface in the strong cooling zone at the end of solidification is 6 times the cooling rate of the billet center, which can ensure that the strong cooling at the end of solidification can fully play the role of improving the internal quality; after the strong cooling, the billet corner temperature is increased by 60℃ through the billet corner heating device. At this time, the billet corner temperature is 774℃, which is higher than the upper limit of the third brittle temperature zone of LX82B steel 750℃, thereby effectively avoiding the occurrence of corner cracks.
[0049] In summary, the device and method for strong cooling at the end of solidification of continuous casting billet based on crack control proposed in the present invention can greatly increase the amount of strong cooling water at the end of solidification, ensure the improvement effect of strong cooling at the end of solidification on internal quality defects such as central segregation, looseness, shrinkage holes, etc. of the billet, and effectively control corner cracks and rewarming type internal cracks caused by strong cooling at the end of solidification.
[0050] Finally, it should be noted that the above embodiments are only used to illustrate the technical solution of the present invention rather than to limit it. Although the present invention has been described in detail with reference to the preferred embodiments, those skilled in the art should understand that the technical solution of the present invention can be modified or replaced by equivalents without departing from the purpose and scope of the technical solution, which should be included in the scope of the claims of the present invention.
Claims
1. A strong cooling device for the solidification end of continuous casting based on crack control, characterized in that: It includes a nozzle and a heating device for the edges and corners of the continuous casting. The nozzle is located in the terminal area of solidification of the continuous casting, and is used to spray water on the surface of the continuous casting in the terminal area of solidification of the continuous casting. The heating device for the edges and corners of the continuous casting is located after the nozzle and before the straightening area of the continuous casting machine, and is used to increase the temperature of the edges and corners of the continuous casting.
2. The strong cooling device for the solidification end of continuous casting based on crack control according to claim 1 is characterized in that: The nozzles are arranged in sequence along the billet drawing direction in the solidification terminal area of the continuous casting billet, and the overlapping rate of the spraying water coverage ranges of two adjacent nozzles is 5% to 15%.
3. The strong cooling device for the solidification end of continuous casting based on crack control according to claim 1 is characterized in that: The nozzle is a conical water nozzle or a conical air-water nozzle, and the center line of the nozzle is perpendicular to the center of the continuous casting billet surface.
4. The strong cooling device for the solidification end of continuous casting based on crack control according to claim 1 is characterized in that: A plurality of nozzles are arranged in the circumferential direction of the cross section of the continuous casting billet so that the spraying water covers the outer surface of the continuous casting billet in the circumferential direction.
5. The strong cooling device for the solidification end of continuous casting based on crack control according to claim 1 is characterized in that: The device for supplementing heat at the edges and corners of the ingot adopts flame heating or electromagnetic induction heating.
6. The strong cooling device for the solidification end of continuous casting based on crack control according to claim 1 is characterized in that: The nozzle is fixedly mounted on a spray frame, the spray frame is arranged along the billet drawing direction, and the length of the spray frame matches the length of the solidification terminal area of the continuous casting billet.
7. A method for strong cooling of continuous casting billet at the end of solidification based on crack control, characterized in that: The method adopts the crack-controlled continuous casting billet solidification terminal strong cooling device as described in any one of claims 1 to 6, and comprises the following steps: S1: Calculate the temperature field of the continuous casting billet according to the process parameters of the continuous casting process; S2: According to the temperature field of the continuous casting billet and the strong cooling mechanism at the end of the solidification of the continuous casting billet, the strong cooling parameters at the end of the solidification of the continuous casting billet are determined; S3: According to the strong cooling parameters at the end of solidification of the continuous casting billet, the nozzle arrangement position and the amount of cooling water at the nozzle are adjusted to perform strong cooling at the end of solidification of the continuous casting billet; S4: According to the corner temperature of the continuous casting billet after the strong cooling at the end of solidification, combined with the third brittle temperature zone of the corresponding production steel grade, determine the temperature compensation value of the billet corner heating device, and heat the continuous casting billet according to the temperature compensation value.
8. The method for strong cooling of continuous casting slab at the end of solidification based on crack control according to claim 7, characterized in that: The process parameters of the continuous casting process include the type of steel produced, casting temperature, drawing speed, mold cooling water volume, mold cooling water temperature difference and secondary cooling water ratio; the strong cooling parameters at the end of the continuous casting billet solidification include the starting position and ending position of the end area of the continuous casting billet solidification and the nozzle cooling water volume.
9. The method for strong cooling of continuous casting billet at the end of solidification based on crack control according to claim 8, characterized in that: The starting position of the continuous casting billet solidification terminal area is the area within the range of 0.30 to 0.50 of the solid phase ratio in the center of the billet, and the ending position is the area within the range of 0.2 to 1.0 m after the billet is completely solidified.
10. The method for strong cooling of continuous casting slab at the end of solidification based on crack control according to claim 8, characterized in that: The cooling water volume of the nozzle is controlled so that the cooling rate of the surface of the continuous casting billet in the terminal region of the continuous casting billet solidification is 5 to 8 times the cooling rate of the center of the continuous casting billet.
11. The method for strong cooling of continuous casting billet at the end of solidification based on crack control according to claim 8, characterized in that: The distance between the device for supplementing heating at the edges and corners of the ingot and the nozzle closest to the device for supplementing heating at the edges and corners of the ingot is greater than 1.0 m.
12. The method for strong cooling of continuous casting billet at the end of solidification based on crack control according to claim 7, characterized in that: The temperature compensation value of the heating device at the corners of the ingot is calculated by the following formula: T b =T u -T c +(20~50); Among them, T b Indicates the temperature compensation value of the heating device at the corner of the casting, ℃; T u Indicates the upper limit of the third brittle temperature zone of the corresponding steel grade, °C; T c It indicates the corner temperature of the continuous casting billet after strong cooling at the end of solidification, ℃.
Citation Information
Cited By
Continuous casting billet corner thermal compensation type slow cooling device and slow cooling method