High-temperature extrusion production process for bamboo-plastic composite board
The problem of low performance of bamboo and wood-plastic composite boards is solved through high-temperature extrusion technology, and the product performance improvement and production efficiency improvement are achieved, and the flame retardant characteristics and cost savings are achieved.
Patent Information
- Application Number
- CN202410981253.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-22
- Publication Date
- 2024-11-08
AI Technical Summary
During the production process of existing bamboo and wood-plastic composite boards, the product performance is reduced due to insufficient mixing and extrusion between bamboo and plastic.
Adopt high-temperature extrusion production process, including material preparation, high mixing, high-temperature heating, extrusion forming and cooling steps, and fully mixing and heating treatment is carried out through a single screw extruder and a small high-speed mixing and disperser to control the moisture content and temperature, and use the same Coupling agent improves material bonding.
It produces bamboo and wood-plastic composite boards with smooth surface, low density, light weight, easy to form, stretch and high tensile strength, and has flame retardant properties, which improves production efficiency and practicality and reduces costs.
Abstract
Description
Technical Field
[0001] The invention relates to the technical field related to the production of composite boards, in particular to a high-temperature extrusion production process for bamboo-wood-plastic composite boards. Background Art
[0002] Bamboo-wood-plastic composite board is a composite material composed of bamboo powder and resin matrix. It can realize the large-scale utilization of bamboo powder and effectively improve the performance of bamboo boards.
[0003] Most existing bamboo-wood-plastic composite boards have insufficient mixed extrusion of bamboo materials and plastics during the production process, resulting in greatly reduced performance of the bamboo-wood-plastic composite boards after production. In order to improve the production process, a high-temperature extrusion production process for bamboo-wood-plastic composite boards is proposed. Summary of the invention
[0004] The invention provides a high-temperature extrusion production process for a bamboo-wood-plastic composite board, which solves the problems in the above-mentioned background technology.
[0005] The present invention solves the technical problem by adopting the following technical solutions:
[0006] A high-temperature extrusion production process for bamboo-wood-plastic composite panels, comprising the following steps: material preparation, high-temperature mixing, high-temperature heating, extrusion molding, and cooling;
[0007] The material preparation comprises: passing 200 kg of bamboo chips through a sieve with an aperture of 110-124 μm successively, and drying the bamboo chips until the moisture content thereof is ≤3%; then adding 95-105 kg of polyvinyl chloride resin, 4.0-4.2 kg of calcium zinc composite stabilizer, 8-12 kg of chlorinated polyethylene, 20-40 kg of calcium carbonate, 2-3 kg of acrylic ester impact modifier ACR, 5-8 kg of titanium dioxide, 0.2-0.3 kg of stearic acid, 0.2-0.3 kg of polyethylene wax, 0.1-0.15 kg of coupling agent and 10-18 g of pigment, and performing mixing reaction and heating in order according to certain weight portions;
[0008] The high mixing: the two mixed materials are put into a small high-speed mixing and dispersing machine for high mixing;
[0009] The high temperature heating: adding the mixed mixture into the heating cylinder for preheating, and the preheating temperature is 170-200°C;
[0010] Extrusion molding: the mixture in a high temperature state is extruded by an extrusion mechanism through a die molding to finally form a bamboo-wood-plastic composite board;
[0011] The cooling: adopting the internal and external water cooling method to cool the bamboo-wood-plastic composite board to obtain the finished bamboo-wood-plastic composite board.
[0012] Preferably, the extrusion mechanism is a single screw extruder.
[0013] Preferably, the extrusion speed of the single-screw extruder is: 1.1 mm / s, the specific pressure is 145 MPa, the holding time is 16 s, and the number of extrusions is 2 times.
[0014] Preferably, the stirring time of the small high-speed mixing and dispersing machine is 10 minutes, followed by standing for 3 minutes. After the standing, stirring is continued for 3 minutes, and then the standing time is 22-28 minutes.
[0015] Preferably, the coupling agent is one or more of vinyl trichlorosilane, vinyl triacetoxysilane, propyl trimethoxysilane, and diisostearyl titanate.
[0016] Preferably, the high temperature state during the extrusion molding process is 130-150°C.
[0017] The advantages and positive effects of the present invention are as follows: through the production sequence in the production process, a bamboo-wood-plastic composite board with a smooth and flat product surface can be obtained; the bamboo-wood-plastic composite board has a low density, a light weight, is easy to form, and has high tensile and tensile strengths; the bamboo-wood-plastic composite board has a flame retardant property that pure bamboo-wood boards do not have; and through a high-temperature extrusion process, the production efficiency of the entire bamboo-wood-plastic composite board can be further improved, and the practicality of the bamboo-wood-plastic composite board can also be greatly improved; and compared with the preparation process of the existing bamboo-plastic board, the granulation step is missing, and the obtained bamboo-plastic board is still full, strong, and has a delicate structure; and such a processing technology can also greatly save costs. DETAILED DESCRIPTION
[0018] The present invention will now be described in further detail.
[0019] The embodiments of the present invention are further described below:
[0020] The bamboo-wood-plastic composite board is a composite material composed of bamboo powder and a resin matrix, which can realize the large-scale utilization of bamboo powder and can effectively improve the performance of bamboo boards. Most existing bamboo-wood-plastic composite boards are not fully mixed and extruded during the production and processing of bamboo materials and plastics, resulting in greatly reduced performance of the bamboo-wood-plastic composite boards after production. In order to improve the production process, a high-temperature extrusion production process for bamboo-wood-plastic composite boards is proposed, which includes the following steps: material preparation, high-temperature mixing, high-temperature heating, extrusion molding, and cooling;
[0021] The material preparation comprises: passing 200 kg of bamboo chips through a sieve with an aperture of 110-124 μm successively, and drying the bamboo chips until the moisture content thereof is ≤3%; then adding 95-105 kg of polyvinyl chloride resin, 4.0-4.2 kg of calcium zinc composite stabilizer, 8-12 kg of chlorinated polyethylene, 20-40 kg of calcium carbonate, 2-3 kg of acrylic ester impact modifier ACR, 5-8 kg of titanium dioxide, 0.2-0.3 kg of stearic acid, 0.2-0.3 kg of polyethylene wax, 0.1-0.15 kg of coupling agent and 10-18 g of pigment, and performing mixing reaction and heating in order according to certain weight portions;
[0022] The high mixing: the two mixed materials are put into a small high-speed mixing and dispersing machine for high mixing;
[0023] The high temperature heating: adding the mixed mixture into the heating cylinder for preheating, and the preheating temperature is 170-200°C;
[0024] Extrusion molding: the mixture in a high temperature state is extruded by an extrusion mechanism through a die molding to finally form a bamboo-wood-plastic composite board;
[0025] The cooling method is to cool the bamboo-wood-plastic composite board by an internal and external water cooling method to obtain the finished bamboo-wood-plastic composite board. Through the production sequence in the production process, the product surface can be processed to be smooth and flat; the bamboo-wood-plastic composite board has low density, light weight, easy molding, high tensile and tensile strength, and the bamboo-wood-plastic composite board has flame retardant properties that pure bamboo-wood boards do not have. The high-temperature extrusion process can further improve the production efficiency of the entire bamboo-wood-plastic composite board, and can also greatly improve the practicality of the bamboo-wood-plastic composite board.
[0026] It should be noted that in order to ensure that the entire extrusion molding process is more stable, in this embodiment, the extrusion mechanism is a single-screw extruder; the single-screw extruder can ensure the purpose of orderly extrusion molding of the mixed raw materials under high temperature, and the temperature of the entire formed bamboo-wood-plastic composite board is always maintained at 130-150°C during the extrusion process. When the temperature cannot meet this requirement, the performance of the extruded composite board may be reduced.
[0027] Furthermore, the internal moisture content of the bamboo material proposed in the material preparation stage needs to be ≤3%. The purpose of this is to ensure that the moisture is controlled. When the moisture is controlled, the bamboo-wood-plastic hybrid material can be better mixed and molded, and its performance can also be guaranteed after subsequent extrusion molding.
[0028] In addition, the extrusion state data of the above-mentioned single-screw extruder are as follows: extrusion speed is: 1.1mm / s, specific pressure is 145MPa, holding time is 16s, and extrusion times are 2 times; the above-mentioned extrusion times of 2 times means that two extrusions are required within the same stage time.
[0029] It should also be noted that the stirring time of the small high-speed mixing and dispersing machine is 10 minutes, followed by standing for 3 minutes. After the standing, stirring is continued for 3 minutes, and then the standing time is 22-28 minutes. The stirring frequency and time of the above-mentioned small high-speed mixing and dispersing machine are strictly limited to ensure that the mixture is fully mixed and stirred.
[0030] Furthermore, the coupling agent is one or more of vinyl trichlorosilane, vinyl triacetoxysilane, propyl trimethoxysilane, and diisostearyl titanate. The addition of the coupling agent can better combine the bamboo and plastic materials in the entire bamboo-wood-plastic composite board, and the performance after subsequent molding is guaranteed.
[0031] It should be emphasized that the embodiments described in the present invention are illustrative rather than restrictive, and therefore the present invention is not limited to the embodiments described in the specific implementation manners. Any other implementation manners derived by those skilled in the art based on the technical solutions of the present invention also fall within the scope of protection of the present invention.
Claims
1. A high temperature extrusion production process for bamboo-wood-plastic composite panels, characterized in that: The process comprises the following steps: material preparation, high mixing, high temperature heating, extrusion molding, and cooling; The material preparation comprises: passing 200 kg of bamboo chips through a sieve with an aperture of 110-124 μm successively, and drying the bamboo chips until the moisture content thereof is ≤3%; then adding 95-105 kg of polyvinyl chloride resin, 4.0-4.2 kg of calcium zinc composite stabilizer, 8-12 kg of chlorinated polyethylene, 20-40 kg of calcium carbonate, 2-3 kg of acrylic ester impact modifier ACR, 5-8 kg of titanium dioxide, 0.2-0.3 kg of stearic acid, 0.2-0.3 kg of polyethylene wax, 0.1-0.15 kg of coupling agent and 10-18 g of pigment, and performing mixing reaction and heating in order according to certain weight portions; The high mixing: the two mixed materials are put into a small high-speed mixing and dispersing machine for high mixing; The high temperature heating: adding the mixed mixture into the heating cylinder for preheating, and the preheating temperature is 170-200°C; Extrusion molding: the mixture in a high temperature state is extruded by an extrusion mechanism through a die molding to finally form a bamboo-wood-plastic composite board; The cooling: adopting the internal and external water cooling method to cool the bamboo-wood-plastic composite board to obtain the finished bamboo-wood-plastic composite board.
2. The high temperature extrusion production process of bamboo-wood-plastic composite board according to claim 1, characterized in that: The extrusion mechanism is a single screw extruder.
3. A high temperature extrusion production process for bamboo-wood-plastic composite panels according to claim 2, characterized in that: The extrusion speed of the single-screw extruder is 1.1 mm / s, the specific pressure is 145 MPa, the holding time is 16 s, and the number of extrusions is 2 times.
4. The high temperature extrusion production process of bamboo-wood-plastic composite board according to claim 1, characterized in that: The stirring time of the small high-speed mixing and dispersing machine is 10 minutes, followed by standing for 3 minutes. After standing, stirring is continued for 3 minutes, and then the standing time is 22-28 minutes.
5. The high temperature extrusion production process of bamboo-wood-plastic composite board according to claim 1, characterized in that: The coupling agent is one or more of vinyl trichlorosilane, vinyl triacetoxysilane, propyl trimethoxysilane, and diisostearyl titanate.
6. The high temperature extrusion production process of bamboo-wood-plastic composite board according to claim 1, characterized in that: The high temperature state during the extrusion molding process is 130-150°C.
Citation Information
Patent Citations
High-hardness polyvinyl chloride free foaming plate material and preparation method of same
CN102942754A
Polyethylene and polyvinyl chloride modified environment-friendly plastic check well and preparation method thereof
CN104356484A
Imitated wood stair railing material and preparation method thereof
CN106046616A
Hard environment-friendly flame-retardant polyvinyl chloride foaming board and manufacturing method thereof
CN106142790A
Integrally-formed high-weather-resistance toughened mineral bamboo-wood composite co-extrusion plate and preparation method thereof