Plastic part processing technology
Through the specific plastic parts processing technology, including multi-step mixing and melting treatment, the component proportion and process parameters of the plastic parts are optimized, and the problem of insufficient structural strength and stability of traditional plastic parts is solved, achieving high strength and high stability plastic parts production.
Patent Information
- Application Number
- CN202411328971.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-24
- Publication Date
- 2024-11-08
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Traditional plastic parts have low structural strength and poor structural stability, making it difficult to meet the needs of complex applications.
A plastic parts processing technology is adopted, including mixing and stirring, drying, mixing and mixing of solid plastic raw materials, additives, melting and injection molding steps, and the structure of plastic parts is improved through the optimization of specific component ratios and process parameters. Strength and stability.
It realizes high structural strength and stability of plastic parts, can replace multiple traditional metal parts, simplify product structure and save manufacturing costs.
Smart Images

Figure CN118906277A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of plastic part manufacturing, and in particular to a plastic part processing technology. Background Art
[0002] Plastics are widely used and are indispensable components in home appliances, automobiles, mobile phones, medical equipment, and lighting appliances. With the rapid development of the plastics industry and the continuous improvement of plastic performance, plastic parts have been more widely used. Plastic parts are replacing traditional metal parts in different fields. A well-designed plastic part can often replace multiple traditional metal parts, thereby simplifying product structure and saving manufacturing costs.
[0003] However, conventional plastic materials, such as the technical solution disclosed in the patent application number CN201610059734.6, entitled A composite plastic material and a method for preparing the same, have low structural strength and poor structural stability. Summary of the invention
[0004] Based on this, it is necessary to provide a plastic parts processing technology to address the technical problems of low structural strength and poor structural stability of plastic parts made of traditional plastic materials.
[0005] A plastic parts processing process, the process comprising the following steps: Solid plastic raw material mixing and stirring step: the solid plastic raw material is mixed and stirred so that the components in the solid plastic raw material are evenly mixed together; Solid plastic raw material drying step: drying the mixed and stirred solid plastic raw materials; Liquid plastic raw material mixing and stirring step: mixing and stirring the liquid plastic raw material so that the components in the liquid plastic raw material are evenly mixed together; Plastic raw material mixing step: evenly mixing the solid plastic raw material and the liquid plastic raw material together to form a primary raw material; Additive adding step: adding the additive to the primary raw material and mixing and stirring evenly to form the secondary raw material; Plastic raw material melting step: using an extruder to heat, stir and pressurize the secondary raw material so that the secondary raw material becomes uniformly molten; Injection molding step: injecting the molten secondary raw material into the mold; Cooling and demoulding step: After the injection molding is completed, cooling and demoulding are performed to obtain the plastic part.
[0006] In one embodiment, in the solid plastic raw material mixing and stirring step, the solid plastic raw material includes the following components in parts by weight: 20 to 40 parts of powdered polymethyl methacrylate, 10 to 20 parts of chlorinated polyethylene, 8 to 14 parts of filler, 3 to 8 parts of ammonium polyphosphate powder, 5 to 15 parts of vinyl bisstearamide and 6 to 22 parts of polypropylene.
[0007] In one embodiment, the filler includes the following components in parts by weight: 8 to 25 parts of calcium carbonate powder, 14 to 28 parts of kaolin, 16 to 24 parts of talc, 20 to 40 parts of silica powder, and 10 to 20 parts of boron nitride.
[0008] In one of the embodiments, in the step of mixing and stirring the liquid plastic raw materials, the liquid plastic raw materials include the following components in parts by weight: 10 to 20 parts of polybutylene terephthalate, 12 to 22 parts of polyamide resin, 15 to 25 parts of butadiene rubber emulsion, 10 to 25 parts of polyurethane emulsion, 5 to 10 parts of ethylene propylene diene rubber, 2 to 5 parts of polydimethylsiloxane, 2 to 6 parts of liquid paraffin and 4 to 8 parts of liquid silicone rubber.
[0009] In one embodiment, in the plastic raw material mixing step, the mass ratio of the solid plastic raw material to the liquid plastic raw material is 1:2.
[0010] In one of the embodiments, in the auxiliary agent adding step, the mass ratio of the auxiliary agent to the primary raw material is 3:100.
[0011] In one embodiment, in the auxiliary agent adding step, the auxiliary agent includes the following components in parts by weight: 10 to 20 parts of lubricant, 15 to 25 parts of plasticizer, 15 to 30 parts of antioxidant, 5 to 15 parts of ultraviolet absorber, 12 to 22 parts of silane coupling agent and 10 to 18 parts of dispersant.
[0012] In one embodiment, during the step of melting the plastic raw material, the stirring and pressurizing parameters are 0.8 kg / cm 2 :.
[0013] In one embodiment, in the step of melting the plastic raw material, the heating temperature is 250 degrees Celsius to 280 degrees Celsius.
[0014] In one of the embodiments, in the injection molding step, the injection pressure is 80 MPa to 250 MPa.
[0015] The above-mentioned plastic parts processing process steps are concise, exquisite, easy to control, and each step is carefully and meticulously. The solid plastic raw material is mixed and stirred evenly through the solid plastic raw material mixing and stirring step. The solid plastic raw material is dried through the solid plastic raw material drying step. The liquid plastic raw material is mixed and stirred evenly through the liquid plastic raw material mixing and stirring step. The solid plastic raw material and the liquid plastic raw material are mixed and stirred evenly to form a primary raw material through the plastic raw material mixing step. The auxiliary agent is added to the primary raw material through the auxiliary agent adding step and mixed and stirred evenly to form a secondary raw material. The secondary raw material is heated into a molten state through the plastic raw material melting step. The plastic parts are obtained through the injection molding step and the cooling and demolding step. The plastic parts obtained by the above-mentioned plastic parts processing technology have high structural strength and strong structural stability. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] Figure 1 FIG. 1 is a schematic diagram of a plastic parts processing process in an embodiment. DETAILED DESCRIPTION
[0017] In order to make the above-mentioned purpose, features and advantages of the present invention more obvious and easy to understand, the specific embodiments of the present invention are described in detail below in conjunction with the accompanying drawings. In the following description, many specific details are set forth so as to fully understand the present invention. However, the present invention can be implemented in many other ways different from those described herein, and those skilled in the art can make similar improvements without violating the connotation of the present invention, so the present invention is not limited by the specific embodiments disclosed below. In the description of the present invention, it should be understood that the orientation or position relationship indicated by the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise", "axial", "radial", "circumferential" and the like is based on the orientation or position relationship shown in the accompanying drawings, only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation of the present invention.
[0018] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" and "second" may explicitly or implicitly include at least one of the features. In the description of the present invention, the meaning of "plurality" is at least two, such as two, three, etc., unless otherwise clearly and specifically defined.
[0019] In the present invention, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements, unless otherwise clearly defined. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0020] In the present invention, unless otherwise clearly specified and limited, a first feature being "above" or "below" a second feature may mean that the first and second features are in direct contact, or the first and second features are in indirect contact through an intermediate medium. Moreover, a first feature being "above", "above" or "above" a second feature may mean that the first feature is directly above or obliquely above the second feature, or simply means that the first feature is higher in level than the second feature. A first feature being "below", "below" or "below" a second feature may mean that the first feature is directly below or obliquely below the second feature, or simply means that the first feature is lower in level than the second feature.
[0021] It should be noted that when an element is referred to as being "fixed to" or "disposed on" another element, it may be directly on the other element or there may be a central element. When an element is considered to be "connected to" another element, it may be directly connected to the other element or there may be a central element at the same time. The terms "vertical", "horizontal", "upper", "lower", "left", "right" and similar expressions used herein are for illustrative purposes only and do not represent the only implementation method.
[0022] See also Figure 1 The present invention provides a plastic parts processing technology, the process comprising the following steps: Step 101: Solid plastic raw material mixing and stirring step: The solid plastic raw material is mixed and stirred so that the components in the solid plastic raw material are evenly mixed together.
[0023] Specifically, the solid plastic raw material is mixed and stirred by a high-speed mixer, so that the components in the solid plastic raw material are evenly mixed together.
[0024] Step 102: Solid plastic raw material drying step: Drying the mixed solid plastic raw materials.
[0025] Specifically, the mixed solid plastic raw materials are dried at a drying temperature of 40 degrees Celsius to 50 degrees Celsius.
[0026] Step 103: Liquid plastic raw material mixing and stirring step: The liquid plastic raw material is mixed and stirred so that the components in the liquid plastic raw material are evenly mixed together.
[0027] Specifically, a high-speed stirrer is used to mix and stir the liquid plastic raw material so that the components in the liquid plastic raw material are evenly mixed together.
[0028] Step 104: Plastic raw material mixing step: the solid plastic raw material and the liquid plastic raw material are uniformly mixed and stirred together to form a primary raw material.
[0029] Specifically, a high-speed mixer is used to uniformly mix the solid plastic raw material and the liquid plastic raw material to form the primary raw material. In this embodiment, the mass ratio of the solid plastic raw material to the liquid plastic raw material is 1:2.
[0030] Step 105: Additive adding step: Add the additive to the primary raw material and mix and stir evenly to form the secondary raw material.
[0031] Specifically, a high-speed mixer is used to add the auxiliary agent to the primary raw material and mix and stir evenly to form the secondary raw material. In this embodiment, the mass ratio of the auxiliary agent to the primary raw material is 3:100.
[0032] Step 106: Plastic raw material melting step: Use an extruder to heat, stir, and pressurize the secondary raw material so that the secondary raw material becomes uniformly molten.
[0033] Specifically, the secondary raw material is heated, stirred and pressurized by an extruder so that the secondary raw material becomes uniformly molten. In this embodiment, the stirring and pressurizing parameters are 0.8 kg / cm 2 : The heating temperature is 250 degrees Celsius to 280 degrees Celsius.
[0034] Step 107: Injection molding step: injecting the molten secondary raw material into the mold.
[0035] Specifically, an injection molding device is used to inject the molten secondary raw material into a mold. In this embodiment, the injection molding pressure is 80 MPa to 250 MPa.
[0036] Step 108: Cooling and demoulding step: After the injection molding is completed, cooling and demoulding are performed to obtain a plastic part.
[0037] Specifically, after the injection molding is completed, the plastic is naturally cooled, and when it is cooled to room temperature, it is demoulded to obtain a plastic part.
[0038] In order to improve the structural strength of the plastic part, in one embodiment, in the step of mixing and stirring the solid plastic raw material, the solid plastic raw material includes the following components in parts by mass: 20 to 40 parts of powdered polymethyl methacrylate, 10 to 20 parts of chlorinated polyethylene, 8 to 14 parts of filler, 3 to 8 parts of ammonium polyphosphate powder, 5 to 15 parts of vinyl bisstearamide, and 6 to 22 parts of polypropylene. In this way, the solid plastic raw material composed of the above components can increase the structural strength of the plastic part.
[0039] In order to increase the structural stability and impact resistance of the plastic part, in one embodiment, the filler includes the following components in parts by weight: 8 to 25 parts of calcium carbonate powder, 14 to 28 parts of kaolin, 16 to 24 parts of talc, 20 to 40 parts of silicon dioxide powder, and 10 to 20 parts of boron nitride. In this way, the filler composed of the above components can increase the structural stability and impact resistance of the plastic part.
[0040] In order to increase the flexibility and tensile strength of plastic parts. In one embodiment, in the step of mixing and stirring the liquid plastic raw materials, the liquid plastic raw materials include the following components in parts by mass: 10 to 20 parts of polybutylene terephthalate, 12 to 22 parts of polyamide resin, 15 to 25 parts of butadiene rubber latex, 10 to 25 parts of polyurethane latex, 5 to 10 parts of ethylene propylene rubber, 2 to 5 parts of polydimethylsiloxane, 2 to 6 parts of liquid paraffin and 4 to 8 parts of liquid silicone rubber. In this way, the liquid plastic raw materials composed of the above components can increase the flexibility and tensile strength of plastic parts.
[0041] In order to increase the weather resistance and toughness of the plastic parts, in one embodiment, in the auxiliary agent adding step, the auxiliary agent includes the following components in parts by mass: 10 to 20 parts of lubricant, 15 to 25 parts of plasticizer, 15 to 30 parts of antioxidant, 5 to 15 parts of ultraviolet absorber, 12 to 22 parts of silane coupling agent and 10 to 18 parts of dispersant. Specifically, the lubricant is vinyl bis stearamide. The ultraviolet absorber is a benzotriazole ultraviolet absorber. The plasticizer is chlorinated paraffin. The dispersant is a modified polysiloxane solution. The antioxidant is a phosphite antioxidant. In this way, the auxiliary agent increases the weather resistance and toughness of the plastic parts.
[0042] The above-mentioned plastic parts processing process steps are concise, exquisite, easy to control, and each step is carefully and meticulously. The solid plastic raw material is mixed and stirred evenly through the solid plastic raw material mixing and stirring step. The solid plastic raw material is dried through the solid plastic raw material drying step. The liquid plastic raw material is mixed and stirred evenly through the liquid plastic raw material mixing and stirring step. The solid plastic raw material and the liquid plastic raw material are mixed and stirred evenly to form a primary raw material through the plastic raw material mixing step. The additive is added to the primary raw material through the additive adding step and mixed and stirred evenly to form a secondary raw material. The secondary raw material is heated into a molten state through the plastic raw material melting step. The plastic parts are obtained through the injection molding step and the cooling and demolding step. The plastic parts obtained by the above-mentioned plastic parts processing technology have high structural strength and strong structural stability. The technical features of the above embodiments may be combined arbitrarily. To make the description concise, not all possible combinations of the technical features in the above embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.
[0043] The above-mentioned embodiments only express several implementation methods of the present invention, and the descriptions thereof are relatively specific and detailed, but they cannot be understood as limiting the scope of the invention patent. It should be pointed out that, for ordinary technicians in this field, several variations and improvements can be made without departing from the concept of the present invention, and these all belong to the protection scope of the present invention. Therefore, the protection scope of the patent of the present invention shall be subject to the attached claims.
Claims
1. A plastic parts processing technology, characterized in that: The process comprises the following steps: Solid plastic raw material mixing and stirring step: the solid plastic raw material is mixed and stirred so that the components in the solid plastic raw material are evenly mixed together; Solid plastic raw material drying step: drying the mixed and stirred solid plastic raw materials; Liquid plastic raw material mixing and stirring step: mixing and stirring the liquid plastic raw material so that the components in the liquid plastic raw material are evenly mixed together; Plastic raw material mixing step: evenly mixing the solid plastic raw material and the liquid plastic raw material together to form a primary raw material; Additive adding step: adding the additive to the primary raw material and mixing and stirring evenly to form the secondary raw material; Plastic raw material melting step: using an extruder to heat, stir and pressurize the secondary raw material so that the secondary raw material becomes uniformly molten; Injection molding step: injecting the molten secondary raw material into the mold; Cooling and demoulding step: After the injection molding is completed, cooling and demoulding are performed to obtain the plastic part.
2. The process according to claim 1, characterized in that In the solid plastic raw material mixing and stirring step, the solid plastic raw material includes the following components in parts by mass: 20 to 40 parts of powdered polymethyl methacrylate, 10 to 20 parts of chlorinated polyethylene, 8 to 14 parts of filler, 3 to 8 parts of ammonium polyphosphate powder, 5 to 15 parts of vinyl bisstearamide and 6 to 22 parts of polypropylene.
3. The process according to claim 2, characterized in that The filler includes the following components in parts by mass: 8 to 25 parts of calcium carbonate powder, 14 to 28 parts of kaolin, 16 to 24 parts of talc, 20 to 40 parts of silicon dioxide powder and 10 to 20 parts of boron nitride.
4. The process according to claim 1, characterized in that In the liquid plastic raw material mixing and stirring step, the liquid plastic raw material includes the following components in parts by mass: 10 to 20 parts of polybutylene terephthalate, 12 to 22 parts of polyamide resin, 15 to 25 parts of butadiene rubber emulsion, 10 to 25 parts of polyurethane emulsion, 5 to 10 parts of ethylene propylene rubber, 2 to 5 parts of polydimethylsiloxane, 2 to 6 parts of liquid paraffin and 4 to 8 parts of liquid silicone rubber.
5. The process according to claim 1, characterized in that In the plastic raw material mixing step, the mass ratio of the solid plastic raw material to the liquid plastic raw material is 1:
2.
6. The process according to claim 1, characterized in that In the auxiliary agent adding step, the mass ratio of the auxiliary agent to the primary raw material is 3:
100.
7. The process according to claim 6, characterized in that In the auxiliary agent adding step, the auxiliary agent includes the following components in parts by mass: 10 to 20 parts of lubricant, 15 to 25 parts of plasticizer, 15 to 30 parts of antioxidant, 5 to 15 parts of ultraviolet absorber, 12 to 22 parts of silane coupling agent and 10 to 18 parts of dispersant.
8. The process according to claim 7, characterized in that In the step of melting the plastic raw material, the stirring and pressurizing parameters are 0.8 kg / cm 2 :.
9. The process according to claim 1, characterized in that In the step of melting the plastic raw material, the heating temperature is 250 degrees Celsius to 280 degrees Celsius.
10. The process according to claim 1, characterized in that In the injection molding step, the injection pressure is 80 MPa to 250 MPa.