MEMS device and preparation method thereof, and MEMS micromirror

By forming a plurality of second grooves in the substrate of the MEMS micromirror and defining the reinforcing rib structure thickness using the second semiconductor material layer, the problems of rotation angle and mechanical strength of the movable structure in the prior art are solved, and the product is improved Stability and yield enhance impact resistance.

CN118908147APending Publication Date: 2024-11-08SEMICON MFG ELECTRONICS (SHAOXING) CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410969178.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-19
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

During the preparation of MEMS micromirror, it is difficult for the prior art to achieve the rotation angle of the movable structure required by higher performance, while reducing the weight of the movable structure while maintaining the mechanical strength of the device. The product reliability and yield still need to be improved.

Method used

By forming a first groove on the first surface side of the substrate and forming a plurality of second grooves in the second semiconductor material layer, the thickness of the reinforcement structure is defined by using the thickness of the second semiconductor material layer, and combining with the first medium The layer acts as an etch stop layer and mask to reduce process difficulty, improve thickness uniformity of the reinforcement rib structure, and enhance the mechanical support and stability of the device.

Benefits of technology

It improves the stability and yield of the product, reduces the impact of the etching process on the uniformity of the structural thickness of the reinforcement ribs, reduces the risk of device fragmentation, and improves impact resistance and production efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118908147A_ABST
    Figure CN118908147A_ABST
Patent Text Reader

Abstract

The embodiment of the invention relates to an MEMS device, a preparation method thereof and an MEMS micromirror, and the preparation method of the MEMS device comprises the steps: providing a substrate which comprises a first surface and a second surface which are opposite to each other, the substrate comprises a first semiconductor material layer, a first dielectric layer, a second semiconductor material layer, a second dielectric layer and a third semiconductor material layer which are sequentially stacked in the direction from the first surface to the second surface, the first dielectric layer comprises a mask part, and the mask part comprises a mask area and a non-mask area; forming a device structure layer on the second surface side, wherein at least part of the device structure layer is used for forming a movable structure; etching the first semiconductor material layer on the first surface side to form a first groove exposing the mask part of the first dielectric layer; the part, located in the mask area, of the first dielectric layer serves as a mask, etching is conducted through the first grooves, so that a plurality of second grooves exposing the second dielectric layer are formed in the second semiconductor material layer, and the part, located between every two adjacent second grooves, of the second semiconductor material layer is reserved to form a reinforcing rib structure, in the direction perpendicular to the first surface and the second surface, the reinforcing rib structure is located in the projection range of the movable structure. Therefore, the uniformity of the thickness of the reinforcing rib structure is better.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of semiconductor technology, and in particular to a MEMS device and a preparation method thereof, and a MEMS micromirror. Background Art

[0002] A MEMS micromirror is a MEMS device, a tiny drivable mirror made based on the Micro Electro Mechanical System (MEMS) technology. It can deflect, modulate, open and close, and control the phase of a light beam under driving. MEMS micromirrors are light in weight, small in size, easy to mass produce, low in production cost, and have excellent optical, mechanical properties, and power consumption. Therefore, they are widely used in projection, display, optical communication, LiDAR, and other scenarios.

[0003] As the requirements for the functions and performance of MEMS micromirrors continue to increase, higher requirements are also placed on the rotation angle of the device's movable structure. Currently, the main method in this field is to reduce the weight of the movable structure by performing an additional etching process on the back of the movable structure to achieve a larger rotation angle. After etching, a reinforcing rib structure will be formed on the back of the movable structure, which reduces the weight of the movable structure without sacrificing the rigidity of the device.

[0004] In order to achieve higher performance requirements, during the processing, the thickness of the rib structure is usually reduced by thinning the wafer to further reduce the weight of the movable structure. However, the extremely thin wafer is extremely difficult to handle during the processing, is easy to break, and is difficult to achieve mass production. At present, this field reduces the thickness of the rib structure by thinning only the thickness of the wafer located in the movable structure area, while the overall thickness of the wafer remains unchanged, thereby achieving better performance while ensuring the mechanical strength of the device. However, there are still many problems to be overcome in the process, and the reliability and yield of the product still need to be improved. Summary of the invention

[0005] In view of this, the embodiments of the present application provide a MEMS device and a method for manufacturing the same, and a MEMS micromirror to solve at least one problem existing in the background technology.

[0006] In a first aspect, an embodiment of the present application provides a method for preparing a MEMS device, comprising:

[0007] Providing a substrate, the substrate comprising a first surface and a second surface opposite to each other, the substrate comprising a first semiconductor material layer, a first dielectric layer, a second semiconductor material layer, a second dielectric layer, and a third semiconductor material layer sequentially stacked from the first surface to the second surface, the first dielectric layer comprising a mask portion, the mask portion comprising a mask area and a non-mask area;

[0008] forming a device structure layer on the second surface side, wherein at least a portion of the device structure layer is used to form a movable structure;

[0009] Etching the first semiconductor material layer on the first surface side to form a first groove exposing the mask portion of the first dielectric layer;

[0010] Using the portion of the first dielectric layer located in the mask area as a mask, etching is performed through the first groove to form a plurality of second grooves exposing the second dielectric layer in the second semiconductor material layer, and a portion of the second semiconductor material layer located between two adjacent second grooves is retained to form a reinforcing rib structure, and in a direction perpendicular to the first surface and the second surface, the reinforcing rib structure is located within the projection range of the movable structure.

[0011] In conjunction with the first aspect of the present application, in an optional implementation manner, providing a substrate includes:

[0012] Providing the first semiconductor material layer;

[0013] forming the first dielectric layer on the first semiconductor material layer;

[0014] Performing a patterning process on the mask portion of the first dielectric layer to remove the portion of the first dielectric layer located in the non-mask area and retaining the portion of the first dielectric layer located in the mask area;

[0015] The second semiconductor material layer is disposed on the first dielectric layer after the patterning process is performed.

[0016] In combination with the first aspect of the present application, in an optional implementation manner, forming the first groove and forming the second groove are implemented successively in the same etching process.

[0017] In combination with the first aspect of the present application, in an optional embodiment, the area of ​​the first end of the reinforcing rib structure is smaller than the area of ​​the second end of the reinforcing rib structure, the first end is the end of the reinforcing rib structure away from the second medium layer, and the second end is the end of the reinforcing rib structure close to the second medium layer.

[0018] In combination with the first aspect of the present application, in an optional embodiment, the angle between the side wall of the reinforcing rib structure and the second end is in the range of 50° to 60°, and the side wall connects the first end and the second end.

[0019] In combination with the first aspect of the present application, in an optional implementation, the process of forming the second groove includes a wet etching process.

[0020] In a second aspect, an embodiment of the present application provides a MEMS device, which is manufactured using the method for manufacturing a MEMS device as described in any one of the first aspects.

[0021] In a third aspect, an embodiment of the present application provides a MEMS micromirror, comprising:

[0022] A substrate, comprising a first surface and a second surface opposite to each other, the substrate comprising a first semiconductor material layer, a first dielectric layer, a second semiconductor material layer, a second dielectric layer, and a third semiconductor material layer stacked in sequence from the first surface to the second surface;

[0023] A mirror and a coil, located on the first surface side;

[0024] A first groove is located in the first semiconductor material layer and penetrates the first semiconductor material layer;

[0025] A plurality of second grooves, located in the second semiconductor material layer and penetrating the second semiconductor material layer, wherein the second grooves are connected to the first grooves;

[0026] A portion of the second semiconductor material layer located between two adjacent second grooves is retained to form a reinforcing rib structure, and in a direction perpendicular to the first surface and the second surface, the reinforcing rib structure is located within the projection range of the mirror and the coil; wherein the first dielectric layer covers a first end of the reinforcing rib structure, and the first end is an end of the reinforcing rib structure away from the second dielectric layer.

[0027] In a fourth aspect, an embodiment of the present application provides a MEMS micromirror, comprising:

[0028] A substrate, comprising a first surface and a second surface opposite to each other, the substrate comprising a first semiconductor material layer, a first dielectric layer, a second semiconductor material layer, a second dielectric layer, and a third semiconductor material layer stacked in sequence from the first surface to the second surface;

[0029] A mirror and a coil, located on the first surface side;

[0030] A first groove is located in the first semiconductor material layer and penetrates the first semiconductor material layer;

[0031] A plurality of second grooves, located in the second semiconductor material layer and penetrating the second semiconductor material layer, wherein the second grooves are connected to the first grooves;

[0032] A portion of the second semiconductor material layer located between two adjacent second grooves is retained to form a reinforcing rib structure, and in a direction perpendicular to the first surface and the second surface, the reinforcing rib structure is located within the projection range of the mirror and the coil;

[0033] The area of ​​the first end of the reinforcing rib structure is smaller than the area of ​​the second end of the reinforcing rib structure, the first end is the end of the reinforcing rib structure away from the second medium layer, and the second end is the end of the reinforcing rib structure close to the second medium layer.

[0034] In conjunction with the fourth aspect of the present application, in an optional embodiment, the angle between the side wall of the reinforcing rib structure and the second end is in the range of 50° to 60°, and the side wall connects the first end and the second end.

[0035] The preparation method of the MEMS device provided in the embodiment of the present application and the MEMS device prepared by the method define the thickness of the reinforcing rib structure by the thickness of the second semiconductor material layer. Compared with forming a reinforcing rib structure with a certain thickness by an etching process, the influence of the precision and stability of the etching process on the uniformity of the thickness of the reinforcing rib structure is reduced, so that the thickness uniformity of the reinforcing rib structure is better, which is conducive to improving product stability and yield; the thickness of the reinforcing rib structure is defined by the thickness of the second semiconductor material layer, and the portion of the substrate where the first groove is not formed can be used as a supporting structure, so that the thickness of the portion where the movable structure of the device is located is smaller and the rigidity requirement of the device is guaranteed. The invention provides a novel method for forming a first semiconductor material layer and a second semiconductor material layer, and a first dielectric layer is used for forming a movable structure. The method can reduce the risk of fragmentation. When forming the first groove, the first dielectric layer can be used as an etching stop layer to reduce the difficulty of the process. When forming the second groove, the portion of the first dielectric layer located in the mask area is used as a mask, and there is no need to perform a step of patterning the mask layer after forming the first groove, thereby reducing the difficulty of the process and saving the process flow. Moreover, when forming the movable structure, the first semiconductor material layer, the first dielectric layer, the second semiconductor material layer, the second dielectric layer, and the third semiconductor material layer in the substrate can provide good mechanical support for the movable structure, thereby avoiding the risk of poor support strength and easy fragmentation of the device caused by first forming the reinforcing rib structure and then forming the device structure layer, and further improving the yield of the product.

[0036] In the MEMS micromirror provided in the embodiment of the present application, the rib structure is a portion of the second semiconductor material layer located between two adjacent second grooves. The thickness of the rib structure is defined by the thickness of the second semiconductor material layer, and the first dielectric layer covers the first end of the rib structure, thereby ensuring the uniformity of the thickness of the rib structure and facilitating improving product stability and yield.

[0037] In the MEMS micromirror provided in the embodiment of the present application, the rib structure is a portion of the second semiconductor material layer located between two adjacent second grooves. The thickness of the rib structure is defined by the thickness of the second semiconductor material layer, so that the thickness uniformity of the rib structure is better, which is beneficial to improving product stability and yield; the area of ​​the first end of the rib structure is smaller than the area of ​​the second end of the rib structure, which reduces the weight of the rib structure while ensuring the strength of the rib structure, thereby improving the impact resistance of the device.

[0038] Additional aspects and advantages of the present application will be given in part in the description below, and in part will become apparent from the description below, or will be learned through the practice of the present application. BRIEF DESCRIPTION OF THE DRAWINGS

[0039] The drawings described herein are used to provide a further understanding of the present application and constitute a part of the present application. The illustrative embodiments of the present application and their descriptions are used to explain the present application and do not constitute an improper limitation on the present application. In the drawings:

[0040] Figures 1 to 3 A schematic diagram of the cross-sectional structure of a MEMS device during the preparation process in the related art;

[0041] Figure 4 A schematic diagram of a process for preparing a MEMS device according to an embodiment of the present application;

[0042] Figures 5 to 15 A schematic diagram of the cross-sectional structure of a MEMS device during the preparation process provided in an embodiment of the present application;

[0043] Figures 16 to 19 A schematic diagram of a cross-sectional structure of a MEMS device during the preparation process provided in an optional specific embodiment of the present application;

[0044] Fig. 20 A schematic cross-sectional structure diagram of a MEMS micromirror provided as an optional specific implementation of the present application;

[0045] Figure 21 to Figure 23 A schematic cross-sectional structure diagram of a MEMS device during the preparation process provided in another optional specific embodiment of the present application;

[0046] Fig.24 A schematic cross-sectional structure diagram of a MEMS micromirror provided as another optional specific implementation of the present application.

[0047] Description of reference numerals:

[0048] 100, substrate; 101, first surface; 102, second surface; 110, first semiconductor material layer; 111, first portion; 112, first support portion; 120, first dielectric layer; 121, mask portion; 1211a, mask area; 1212a, non-mask area; 1211, portion of the first dielectric layer located in the mask area; 122, second support portion; 130, second semiconductor material layer; 131, third support portion; 140, second dielectric layer; 150, third semiconductor material layer; 160, first groove; 170, second groove; 180, reinforcing rib structure; 18 1. First end; 182. Second end; 183. Side wall; 190. Support structure; 200. Device structure layer; 201. Movable structure; 201s. Projection range of movable structure; 2011. Movable mirror structure; 2012. Movable coil structure; 210. Varistor; 220. Third dielectric layer; 221. First connection hole; 230. Conductive connection structure; 240. Fourth dielectric layer; 241. Second connection hole; 242. Mirror opening; 250. Coil; 251. Coil conductive structure; 260. Mirror; 270. Third groove; 300. Patterned mask layer. DETAILED DESCRIPTION

[0049] The exemplary embodiments disclosed in the present application will be described in more detail below with reference to the accompanying drawings. Although the exemplary embodiments of the present application are shown in the accompanying drawings, it should be understood that the present application can be implemented in various forms and should not be limited by the specific embodiments described herein. On the contrary, these embodiments are provided to enable a more thorough understanding of the present application and to fully convey the scope disclosed in the present application to those skilled in the art.

[0050] In the following description, a large number of specific details are given to provide a more thorough understanding of the present application. However, it is obvious to those skilled in the art that the present application can be implemented without one or more of these details. In other examples, in order to avoid confusion with the present application, some technical features known in the art are not described; that is, all features of the actual embodiments are not described here, and well-known functions and structures are not described in detail.

[0051] In the drawings, the sizes of layers, regions, elements and their relative sizes may be exaggerated for clarity. Like reference numerals denote like elements throughout.

[0052] It should be understood that when an element or layer is referred to as "on ...", "adjacent to ...", "connected to" or "coupled to" other elements or layers, it can be directly on, adjacent to, connected to or coupled to other elements or layers, or there can be intervening elements or layers. On the contrary, when an element is referred to as "directly on ...", "directly adjacent to ...", "directly connected to" or "directly coupled to" other elements or layers, there is no intervening element or layer. It should be understood that although the terms first, second, third, etc. can be used to describe various elements, components, regions, layers and / or parts, these elements, components, regions, layers and / or parts should not be limited by these terms. These terms are only used to distinguish one element, component, region, layer or part from another element, component, region, layer or part. Therefore, without departing from the teachings of the present application, the first element, component, region, layer or part discussed below can be represented as the second element, component, region, layer or part. And when the second element, component, region, layer or part is discussed, it does not indicate that the present application necessarily has the first element, component, region, layer or part.

[0053] Spatially relative terms such as "under", "beneath", "below", "under", "above", "above", etc., may be used here for convenience of description to describe the relationship between an element or feature shown in the figure and other elements or features. It should be understood that in addition to the orientation shown in the figure, the spatial relationship terms are intended to also include different orientations of the device in use and operation. For example, if the device in the accompanying drawings is turned over, then the elements or features described as "under other elements" or "under it" or "under it" will be oriented as "on" other elements or features. Therefore, the exemplary terms "under" and "under" may include both upper and lower orientations. The device can be oriented otherwise (rotated 90 degrees or other orientations) and the spatial descriptors used herein are interpreted accordingly.

[0054] The purpose of the terms used herein is only to describe specific embodiments and is not intended to be limiting of the present application. When used herein, the singular forms "one", "an" and "said / the" are also intended to include plural forms, unless the context clearly indicates otherwise. It should also be understood that the terms "consisting of" and / or "comprising", when used in this specification, determine the presence of the features, integers, steps, operations, elements and / or parts, but do not exclude the presence or addition of one or more other features, integers, steps, operations, elements, parts and / or groups. When used herein, the term "and / or" includes any and all combinations of the relevant listed items.

[0055] In order to thoroughly understand the present application, detailed steps and detailed structures will be presented in the following description to illustrate the technical solution of the present application. The preferred embodiments of the present application are described in detail below, but in addition to these detailed descriptions, the present application may also have other implementation methods.

[0056] Figures 1 to 3 The cross-sectional structure schematic diagram of the MEMS device in the preparation process in the related art. As shown in the figure, in the related art, the preparation process of the reinforcing rib structure 180 includes: providing a substrate 100, the substrate 100 includes a first surface 101 and a second surface 102 opposite to each other, and the substrate 100 includes a first semiconductor material layer 110, a first dielectric layer 120 and a second semiconductor material layer 130 stacked in sequence from the first surface 101 to the second surface 102; forming a first groove 160 extending to the inside of the first semiconductor material layer 110 on the first surface 101 side of the substrate 100, and the portion of the first semiconductor material layer 110 located at the bottom of the first groove 160 is the first portion 111; forming a patterned mask layer 300 on the first surface 101; using the patterned mask layer 300 as a mask, etching the first portion 111 on the first surface 101 side to form a plurality of second grooves 170, and the portion of the first portion 111 located between two adjacent second grooves 170 is retained to form the reinforcing rib structure 180. It can be seen that in the related art, the thickness of the reinforcing rib structure 180 is determined by the thickness of the first portion 111, and the thickness of the first portion 111 is determined by the etching process for forming the first groove 160. Therefore, the accuracy and stability of the etching process will affect the thickness uniformity of the reinforcing rib structure 180, and the uneven thickness of the reinforcing rib structure 180 also means that the weight of the reinforcing rib structure 180 is uneven, which in turn affects the movement of the movable structure and affects the product stability and yield. It can be understood that the first surface 101 is, for example, the back side of the substrate 100, then Figure 1 and Figure 2 The cross-sectional structure when the backside process is performed on the substrate 100 is schematically shown. Figure 3 The cross-sectional structure of the MEMS device after flipping over after the backside process is performed is schematically shown.

[0057] In view of this, the present application embodiment provides a method for preparing a MEMS device, please refer to Figure 4 , the preparation method comprises:

[0058] Step S401: providing a substrate, the substrate comprising a first surface and a second surface opposite to each other, the substrate comprising a first semiconductor material layer, a first dielectric layer, a second semiconductor material layer, a second dielectric layer, and a third semiconductor material layer sequentially stacked from the first surface to the second surface, the first dielectric layer comprising a mask portion, the mask portion comprising a mask area and a non-mask area;

[0059] Step S402: forming a device structure layer on the second surface side, at least a portion of the device structure layer is used to form a movable structure;

[0060] Step S403: etching the first semiconductor material layer on the first surface side to form a first groove exposing a mask portion of the first dielectric layer;

[0061] Step S404: Using the portion of the first dielectric layer located in the mask area as a mask, etching is performed through the first groove to form a plurality of second grooves exposing the second dielectric layer in the second semiconductor material layer, and the portion of the second semiconductor material layer located between two adjacent second grooves is retained to form a reinforcing rib structure, and in a direction perpendicular to the first surface and the second surface, the reinforcing rib structure is located within the projection range of the movable structure.

[0062] Therefore, the thickness of the rib structure is defined by the thickness of the second semiconductor material layer. Compared with forming a rib structure with a certain thickness through an etching process, the influence of the accuracy and stability of the etching process on the uniformity of the thickness of the rib structure is reduced, so that the thickness of the rib structure is more uniform, which is beneficial to improving product stability and yield; the thickness of the rib structure is defined by the thickness of the second semiconductor material layer, and the portion of the substrate where the first groove is not formed can be used as a supporting structure, so that the thickness of the portion where the movable structure of the device is located is smaller, and the rigidity requirement of the device is guaranteed, thereby reducing the risk of fragmentation; when forming the first groove The first dielectric layer can be used as an etching stop layer to reduce the difficulty of the process; when forming the second groove, the portion of the first dielectric layer located in the mask area is used as a mask, and there is no need to perform a step of patterning the mask layer after forming the first groove, which reduces the difficulty of the process and saves the process flow; and when forming the movable structure, the first semiconductor material layer, the first dielectric layer, the second semiconductor material layer, the second dielectric layer, and the third semiconductor material layer in the substrate can provide good mechanical support for the movable structure, avoiding the risk of poor support strength and easy breakage of the device caused by first forming the reinforcing rib structure and then forming the device structure layer, further improving the yield of the product.

[0063] It can be understood that the MEMS device can be any suitable device known to those skilled in the art.

[0064] Optionally, the MEMS device is a MEMS micromirror. This embodiment specifically takes the MEMS micromirror as an example to explain and illustrate the technical solution of the embodiment of the present application.

[0065] Please refer to Figures 5 to 8, perform step S401: provide a substrate 100, the substrate 100 includes a first surface 101 and a second surface 102 opposite to each other, the substrate 100 includes a first semiconductor material layer 110, a first dielectric layer 120, a second semiconductor material layer 130, a second dielectric layer 140, and a third semiconductor material layer 150 stacked in sequence from the first surface 101 to the second surface 102, the first dielectric layer 120 includes a mask portion 121, the mask portion 121 includes a mask area 1211a and a non-mask area 1212a.

[0066] It can be understood that the materials of the first semiconductor material layer 110, the second semiconductor material layer 130 and the third semiconductor material layer 150 can be any suitable semiconductor material well known to those skilled in the art, and the materials of the first dielectric layer 120 and the second dielectric layer 140 can be any suitable dielectric material well known to those skilled in the art. In this embodiment, the substrate 100 is specifically, for example, a double buried oxide layer SOI (Silicon-On-Insulator) substrate. The first semiconductor material layer 110 can be regarded as the bottom silicon layer of the double buried oxide layer SOI substrate, the first dielectric layer 120 can be regarded as the first oxide layer of the double buried oxide layer SOI substrate, and the second semiconductor material layer 130 can be regarded as the middle silicon layer of the double buried oxide layer SOI substrate; the second dielectric layer 140 can be regarded as the second oxide layer of the double buried oxide layer SOI substrate, and the third semiconductor material layer 150 can be regarded as the top silicon layer of the double buried oxide layer SOI substrate. Obviously, the embodiment of the present application does not exclude the situation that the substrate 100 is a double buried oxide layer GeOI (Germanium-On-Insulator) substrate.

[0067] Please refer to Figure 8 The first dielectric layer 120 further includes a second supporting portion 122 located at the periphery of the mask portion 121 , and the second supporting portion 122 is used to form a supporting structure.

[0068] Please refer to Figures 5 to 7In order to form a mask portion 121 including a mask area 1211a and a non-mask area 1212a, the step of providing a substrate 100 may specifically include: providing a first semiconductor material layer 110; forming a first dielectric layer 120 on the first semiconductor material layer 110; performing a patterning process on the first dielectric layer 120 to remove a portion of the first dielectric layer 120 located in the non-mask area 1212a, and retaining a portion 1211 of the first dielectric layer located in the mask area, thereby forming a mask portion 121 including the mask area 1211a and the non-mask area 1212a, and a portion of the outer periphery of the mask portion 121 is formed as a second supporting portion 122; and disposing a second semiconductor material layer 130 on the first dielectric layer 120 after the patterning process is performed. It can be understood that in the subsequent process of forming the second groove, the portion 1211 of the first dielectric layer located in the mask area is used as a mask. If a patterning process is performed on the first dielectric layer 120 after the first groove is formed, the first surface 101 of the substrate 100 is uneven at this time, and the patterning process is more difficult and requires higher alignment accuracy. Therefore, before setting the second dielectric layer 140, the patterning process is performed on the first dielectric layer 120 in advance, and the process difficulty is relatively low; and, generally, the thickness of the oxide layer in the SOI substrate is relatively small (the thickness of the first dielectric layer 120 in this embodiment is relatively small), and after removing the portion of the first dielectric layer 120 located in the non-mask area 1212a, the height of the gap formed at this position is relatively small, which does not affect the mechanical strength of the substrate 100.

[0069] In this embodiment, the thickness of the first dielectric layer 120 may range from 1 μm to 2 μm.

[0070] In addition, the mask portion 121 including the mask area 1211a and the non-mask area 1212a may also be formed in some other ways. For example, instead of directly removing the portion of the first dielectric layer 120 located in the non-mask area 1212a, the material of the portion is processed to convert it into a material that is easier to remove than the portion 1211 of the first dielectric layer located in the mask area. In this way, after the mask portion 121 of the first dielectric layer 120 is exposed through the first groove in a subsequent process, the portion of the first dielectric layer 120 located in the non-mask area 1212a can be easily removed, and can even be directly removed in the process of forming the second groove, thereby eliminating the need for additional patterning, reducing process difficulty, and saving process flow.

[0071] Please refer to Figures 7 and 8 The step of providing the substrate 100 may further include:

[0072] forming a second dielectric layer 140 on the second semiconductor material layer 130;

[0073] A third semiconductor material layer 150 is disposed on the second dielectric layer 140 .

[0074] In the present embodiment, the process of providing the second semiconductor material layer 130 and the process of providing the third semiconductor material layer 150 may include a bonding process.

[0075] Please refer to Figure 8 In this embodiment, the area of ​​the second semiconductor material layer 130 is smaller than the area of ​​the first semiconductor material layer 110. It can be understood that when performing the bonding process in actual preparation, it is difficult to align the rounded corners of the edges of different wafers for bonding, and there will be a certain amount of offset. Therefore, the area of ​​the second semiconductor material layer 130 is smaller than the area of ​​the first semiconductor material layer 110, which can avoid wafer cracking in subsequent processes.

[0076] In this embodiment, the process of forming the first dielectric layer 120 and the process of forming the second dielectric layer 140 may include a deposition process.

[0077] Please refer to Figures 9 to 16 , executing step S402: forming a device structure layer 200 on the second surface 102 side, at least a portion of the device structure layer 200 is used to form a movable structure.

[0078] Please continue to refer to Fig. 9 Forming the device structure layer 200 may include: forming a varistor 210 on the second surface 102 side of the substrate 100 .

[0079] It can be understood that the MEMS micromirror generates electromagnetic force under the action of current by configuring permanent magnets and coils, and the movable structure of the MEMS micromirror rotates under the drive of the electromagnetic force. During this period, the varistor 210 will be subjected to a certain pressure and the resistance value will change. The change in resistance value is converted into a voltage output, and then combined with the preset output voltage and the reference standard of the movable structure rotation angle, the rotation angle of the movable structure can be measured to better understand the working state of the device.

[0080] In actual production, a patterned mask layer (not shown in the figure) can be formed on the second surface 102 of the substrate 100 through a photolithography process to form a preset opening for the varistor (not shown in the figure), and then the mask layer is used as a mask to prepare the varistor 210 through an ion implantation process and an annealing process, and the mask layer is removed after completion.

[0081] Please refer to Fig.10 Forming the device structure layer 200 may include: forming a third dielectric layer 220 covering the second surface 102 to achieve an insulation function.

[0082] Optionally, the material of the third dielectric layer 220 includes any one of several dielectric materials, such as oxides, nitrides and oxynitrides, especially silicon oxides, nitrides and oxynitrides. In this embodiment, the material of the third dielectric layer 220 may be silicon oxide.

[0083] In this embodiment, the process of forming the third dielectric layer 220 may include a deposition process.

[0084] Please continue to refer to Fig.10 Forming the device structure layer 200 may include: forming a first connection hole 221, the first connection hole 221 penetrates the third dielectric layer 220 and exposes a portion of the varistor 210, so that the varistor 210 can be led out through the conductive connection structure in subsequent process steps, and the rest of the varistor 210 is covered and protected by the third dielectric layer 220 to achieve surface insulation isolation.

[0085] In this embodiment, the process of forming the first connection hole 221 may include a photolithography process and an etching process.

[0086] Please refer to Fig.11 Forming the device structure layer 200 may include: forming a conductive connection structure 230 , wherein the conductive connection structure 230 is conductively connected to the varistor 210 .

[0087] Specifically, the step of forming the conductive connection structure 230 may include:

[0088] A conductive material layer (not shown in the figure) is formed on the third dielectric layer 220 by an evaporation process or a physical vapor sputtering deposition process, and the conductive material layer fills the first connection hole 221;

[0089] The conductive material layer is patterned by photolithography and dry etching or wet etching process to form a conductive connection structure 230 .

[0090] Optionally, the material of the conductive connection structure 230 includes metal, specifically one or more of aluminum, copper, gold, titanium, sodium, platinum, etc. In this embodiment, the material of the conductive connection structure 230 is aluminum.

[0091] Please refer to Fig.12 Forming the device structure layer 200 may include: forming a fourth dielectric layer 240 covering the third dielectric layer 220 and the conductive connection structure 230 to achieve surface insulation.

[0092] In this embodiment, the material of the fourth dielectric layer 240 can be the same as that of the third dielectric layer 220 , which will not be described in detail herein. Of course, the present application does not exclude the case where the fourth dielectric layer 240 is made of a material different from that of the third dielectric layer 220 .

[0093] In this embodiment, the process of forming the fourth dielectric layer 240 may be the same as that of the third dielectric layer 220, which will not be described in detail. Of course, this application does not exclude the situation that the process of forming the fourth dielectric layer 240 is different from the process of forming the third dielectric layer 220.

[0094] Please continue to refer to Fig.12 Forming the device structure layer 200 may include: forming a second connection hole 241 , the second connection hole 241 penetrates the fourth dielectric layer 240 and exposes a portion of the conductive connection structure 230 , so as to facilitate conductive connection between the subsequently formed coil 250 and the conductive connection structure 230 .

[0095] In this embodiment, the process of forming the second connection hole 241 may be the same as the process of forming the first connection hole 221, which will not be described in detail. Of course, this application does not exclude the situation that the process of forming the second connection hole 241 may be different from the process of forming the first connection hole 221.

[0096] Please refer to Fig.13 , forming the device structure layer 200 may include: forming a coil 250 and a coil conductive structure 251 on the fourth dielectric layer 240, wherein the coil 250 is distributed around the center of the device, and the coil conductive structure 251 is located in the second connection hole 241 and is conductively connected to the conductive connection structure 230. It can be understood that the coil conductive structure 251 can be formed in the same process step as the coil 250, and the coil conductive structure 251 is located at the end of the coil 250; in some embodiments, the coil conductive structure 251 can be identified as a part of the coil 250, specifically, a part that is used for conductive connection with the conductive connection structure 230 and no longer continues to surround the mirror 260.

[0097] Optionally, the material of the coil 250 includes gold, copper or other metal materials with good electrical conductivity. This embodiment of the present application is not limited to this. In addition, the material of the coil conductive structure 251 can be the same as the material of the coil 250.

[0098] In this embodiment, the process of forming the coil 250 may include an electroplating process.

[0099] Please refer to Fig.14 Forming the device structure layer 200 may include: etching the third dielectric layer 220 and the fourth dielectric layer 240 to form a mirror opening 242, wherein the coil 250 surrounds the outer periphery of the mirror opening 242, and the mirror opening 242 exposes a portion of the second surface 102 to facilitate the formation of a mirror in subsequent processes.

[0100] In this embodiment, the process of forming the mirror opening 242 includes a photolithography process and an etching process.

[0101] Please refer to Fig.15Forming the device structure layer 200 includes: forming a mirror 260 on the second surface 102 exposed by the mirror opening 242 .

[0102] In this embodiment, the process of forming the mirror surface 260 includes a photolithography process and an evaporation process.

[0103] Optionally, the mirror surface 260 is a high reflectivity mirror surface.

[0104] Optionally, the material of the mirror 260 includes gold, aluminum or other optical reflective film materials with high reflectivity.

[0105] At this point, the preparation of the device structure layer 200 is completed.

[0106] As an optional specific implementation, please refer to Fig.16 After forming the device structure layer 200 on the second surface 102 side, the preparation method also includes: forming a third groove 270 in the device structure layer 200, the third groove 270 penetrates the third semiconductor material layer 150, exposes a portion of the second dielectric layer 140, and the third groove 270 defines the area of ​​the movable structure 201.

[0107] The movable structure 201 of the MEMS micromirror may include a movable mirror structure 2011 and a movable coil structure 2012 .

[0108] Please refer to Fig.17 Before etching the first semiconductor material layer 110 on the first surface 101 side, the preparation method may further include: thinning the first semiconductor material layer 110 on the first surface 101 side to facilitate the subsequent etching process for forming the first groove.

[0109] Please refer to Fig.18 , performing step S403 : etching the first semiconductor material layer 110 on the first surface 101 side to form a first groove 160 exposing the mask portion 121 of the first dielectric layer 120 .

[0110] In this embodiment, the process of forming the first groove 160 may include a photolithography process and an etching process.

[0111] Please continue to refer to Fig.18 , the portion of the first semiconductor material layer 110 located at the periphery of the first groove 160 is the first support portion 112, and the first support portion 112 is used to form a support structure. Therefore, by forming the first groove 160, the thickness of the portion of the substrate 100 located at the movable structure 201 is reduced, which is beneficial to improving the performance of the device, and the portion where the first groove 160 is not formed is the first support portion 112, which is used to form a support structure, so that it can be achieved that the thickness of the portion where the movable structure 201 of the device is located is small, and the rigidity requirements of the device are guaranteed, and the risk of fragmentation is reduced.

[0112] Please refer to Fig.18 and Fig.19 , step S404 is performed: using the portion 1211 of the first dielectric layer located in the mask area as a mask, etching is performed through the first groove 160 to form a plurality of second grooves 170 exposing the second dielectric layer 140 in the second semiconductor material layer 130, and the portion of the second semiconductor material layer 130 located between two adjacent second grooves 170 is retained to form a reinforcing rib structure 180, and in the direction perpendicular to the first surface 101 and the second surface 102, the reinforcing rib structure 180 is located within the projection range 201s of the movable structure. Thus, the reinforcing rib structure 180 is formed at the movable structure 201 through the second semiconductor material layer 130, and the thickness of the reinforcing rib structure 180 is defined by the thickness of the second semiconductor material layer 130, so that the thickness uniformity of the reinforcing rib structure 180 is better.

[0113] Please combine Fig.16 and Fig.19 The movable structure 201 includes a movable mirror structure 2011 and a movable coil structure 2012. The movable mirror structure 2011 is provided with a mirror 260, and the movable coil structure 2012 is provided with a coil 250. In this embodiment, the reinforcing rib structure 180 is located within the projection range 201s of the movable structure, which can be understood as the reinforcing rib structure 180 is located within the projection range of the movable mirror structure 2011 and the movable coil structure 2012; further, the reinforcing rib structure 180 is located within the projection range 201s of the movable structure, which can be understood as the reinforcing rib structure 180 is located within the projection range of the coil 250 and the mirror 260.

[0114] In some of the aforementioned optional embodiments, further, the formation of the first groove 160 and the formation of the second groove 170 are successively implemented in the same etching process. It can be understood that when the substrate 100 is provided, the patterning process has been performed on the first dielectric layer 120 in advance to complete the preparation of the mask. Therefore, after the first groove 160 is formed, the etching process can be continued to etch the second semiconductor material layer 130 to improve production efficiency.

[0115] Please continue to refer to Fig.19 , the portion of the second semiconductor material layer 130 corresponding to the second support portion 122 is the third support portion 131; the first support portion 112, the second support portion 122 and the third support portion 131 form a support structure 190; the thickness of the reinforcing rib structure 180 (such as Fig.19 h1) is smaller than the thickness of the support structure 190 (as shown in Fig.19As shown in h2 in the figure). As a result, the thickness of the reinforcing rib structure 180 is reduced, so that the thickness of the movable structure 201 of the device is reduced, which improves the product performance. At the same time, the supporting structure 190 can continue to maintain a relatively large thickness, ensuring the rigidity requirements of the device, reducing the risk of device breakage, and making it easier to mass produce.

[0116] Optionally, the thickness of the reinforcing rib structure 180 is in the range of 100 μm to 200 μm, and the thickness of the supporting structure 190 is in the range of 300 μm to 400 μm.

[0117] Please continue to refer to Fig. 20 Optionally, the area of ​​the first end 181 of the reinforcing rib structure 180 is smaller than the area of ​​the second end 182 of the reinforcing rib structure 180 , the first end 181 is the end of the reinforcing rib structure 180 away from the second dielectric layer 140 , and the second end 182 is the end of the reinforcing rib structure 180 close to the second dielectric layer 140 . It can be understood that the area of ​​the second end 182 of the reinforcing rib structure 180 is larger, that is, the contact area between the reinforcing rib structure 180 and the second dielectric layer 140 is larger, so that the reinforcing rib structure 180 has greater strength; under the condition that the thickness of the reinforcing rib structure 180 is certain, compared with the case where the area of ​​the first end 181 is equal to the area of ​​the second end 182, the area of ​​the first end 181 of the reinforcing rib structure 180 is smaller, so that the volume of the reinforcing rib structure 180 is reduced, that is, the weight of the reinforcing rib structure 180 is reduced; thus, the area of ​​the first end 181 of the reinforcing rib structure 180 is smaller than the area of ​​the second end 182 of the reinforcing rib structure 180, so that the reinforcing rib structure 180 has better mechanical properties and weight advantages, which is beneficial to improving the impact resistance of the device.

[0118] Optionally, in a direction perpendicular to the first surface 101 and the second surface 102 , the cross-section of the reinforcing rib structure 180 includes a trapezoid, the upper base of the trapezoid is located at the second end 182 , and the lower base of the trapezoid is located at the first end 181 .

[0119] Optionally, the angle between the side wall 183 of the reinforcing rib structure 180 and the second end 182 is in the range of 50° to 60°, and the side wall 183 connects the first end 181 and the second end 182. Thus, while the reinforcing rib structure 180 has better mechanical properties and weight advantages, the precision and difficulty of the process are taken into account. In this embodiment, the angle between the side wall 183 of the reinforcing rib structure 180 and the second end 182 is specifically 55°, for example.

[0120] Optionally, the process of forming the second groove 170 includes a wet etching process. It can be understood that the wet etching process is isotropic, which is more conducive to providing a uniform etching effect and ensuring the accuracy of the shape of the formed reinforcing rib structure 180. In addition, the wet etching process has low cost, simple operation, and is more conducive to production and preparation.

[0121] It can be understood that in this specific embodiment, the third groove 270 does not penetrate the second dielectric layer 140 , so when etching the second semiconductor material layer 130 , the second dielectric layer 140 can be used as an etching stop layer to reduce the difficulty of the process.

[0122] Please refer to Figure 19 to Figure 20 After executing step S404, the preparation method further includes: etching the second dielectric layer 140 from the first surface 101 side to connect the second groove 170 with the third groove 270. Thus, the movable structure 201 of the device is released.

[0123] Optionally, the process of etching the second dielectric layer 140 includes a dry etching process. It can be understood that in this embodiment, the material of the first dielectric layer 120 is the same as the material of the second dielectric layer 140. When the dry etching process is performed, the first dielectric layer 120 covering the first end 181 of the reinforcing rib structure 180 may be removed together. In this embodiment, the dry etching process is specifically taken as an example.

[0124] In a specific example in which the process of etching the second dielectric layer 140 is a dry etching process, before etching the second dielectric layer 140 from the first surface 101 side, the preparation method further includes: forming a protective tape (not shown in the figure) on the second surface 102 side. Thus, when performing the dry etching process, gas overflow is prevented from affecting the etching effect.

[0125] As another optional specific implementation, please refer to Fig.21 After forming the device structure layer 200 on the second surface 102 side, the preparation method further includes: forming a third groove 270 in the device structure layer 200, the third groove 270 penetrates the third semiconductor material layer 150 and the second dielectric layer 140, exposing a portion of the second semiconductor material layer 130, and the third groove 270 defines the region of the movable structure 201. Therefore, please refer to Fig.23 and Fig.24 After the second semiconductor material layer 130 is subsequently etched to form the second groove 170 , the second groove 170 is directly connected to the third groove 270 , thus saving process.

[0126] The difference between this embodiment and the aforementioned optional embodiment is that the third groove 270 penetrates different material layers, but the process methods in the two optional embodiments are consistent. Other processes include: thinning the substrate 100 (such as Fig. 22 As shown); forming a first groove 160 (as Fig.23 forming a second groove 170 and a reinforcing rib structure 180 (as shown); Fig.24 ) are also consistent, so they are not elaborated here. For details, please refer to the content of an optional specific implementation method mentioned above.

[0127] Accordingly, an embodiment of the present application provides a MEMS device, which is manufactured using the method for manufacturing a MEMS device as described in the above embodiment.

[0128] The present application also provides a MEMS micromirror, please refer to Fig.24 , which includes:

[0129] The substrate 100 includes a first surface 101 and a second surface 102 opposite to each other, and the substrate 100 includes a first semiconductor material layer 110, a first dielectric layer 120, a second semiconductor material layer 130, a second dielectric layer 140, and a third semiconductor material layer 150 stacked in sequence from the first surface 101 to the second surface 102;

[0130] The mirror 260 and the coil 250 are located on the first surface 101 side;

[0131] A first groove 160 is located in the first semiconductor material layer 110 and penetrates the first semiconductor material layer 110;

[0132] A plurality of second grooves 170 , located in the second semiconductor material layer 130 and penetrating the second semiconductor material layer 130 , the second grooves 170 being connected to the first grooves 160 ;

[0133] The portion of the second semiconductor material layer 130 located between two adjacent second grooves 170 is retained to form a reinforcing rib structure 180. In the direction perpendicular to the first surface 101 and the second surface 102, the reinforcing rib structure 180 is located within the projection range of the mirror 260 and the coil 250; wherein the first dielectric layer 120 covers the first end 181 of the reinforcing rib structure 180, and the first end 181 is the end of the reinforcing rib structure 180 away from the second dielectric layer 140.

[0134] Therefore, the thickness of the rib structure 180 is defined by the thickness of the second semiconductor material layer 130, which reduces the influence of the accuracy and stability of the etching process on the uniformity of the thickness of the rib structure. In addition, the first dielectric layer 120 covers the first end 181 of the rib structure 180, thereby ensuring better uniformity of the thickness of the rib structure 180, which is beneficial to improving product stability and yield.

[0135] Please continue to refer to Fig.24Optionally, the area of ​​the first end 181 of the reinforcing rib structure 180 is smaller than the area of ​​the second end 182 of the reinforcing rib structure 180, and the second end 182 is the end of the reinforcing rib structure 180 close to the second dielectric layer 140. It can be understood that the area of ​​the second end 182 of the reinforcing rib structure 180 is larger, that is, the contact area between the reinforcing rib structure 180 and the second dielectric layer 140 is larger, so that the reinforcing rib structure 180 has a greater strength; under the condition that the thickness of the reinforcing rib structure 180 is constant, compared with the case where the area of ​​the first end 181 is equal to the area of ​​the second end 182, the area of ​​the first end 181 of the reinforcing rib structure 180 away from the second dielectric layer 140 is smaller, so that the volume of the reinforcing rib structure 180 is reduced, that is, the weight of the reinforcing rib structure 180 is reduced; therefore, the area of ​​the first end 181 of the reinforcing rib structure 180 is smaller than the area of ​​the second end 182 of the reinforcing rib structure 180, so that the reinforcing rib structure 180 has better mechanical properties and weight advantages, which is conducive to improving the impact resistance of the device.

[0136] Optionally, in a direction perpendicular to the first surface 101 and the second surface 102 , the cross-section of the reinforcing rib structure 180 includes a trapezoid, the upper base of the trapezoid is located at the second end 182 , and the lower base of the trapezoid is located at the first end 181 .

[0137] Optionally, the angle between the side wall 183 of the reinforcing rib structure 180 and the second end 182 is in the range of 50° to 60°, and the side wall 183 connects the first end 181 and the second end 182. Thus, while the reinforcing rib structure 180 has better mechanical properties and weight advantages, the precision and difficulty of the process are taken into account. In this embodiment, the angle between the side wall 183 of the reinforcing rib structure 180 and the second end 182 is specifically 55°, for example.

[0138] The present application also provides a MEMS micromirror, please refer to Fig. 20 , which includes:

[0139] The substrate 100 includes a first surface 101 and a second surface 102 opposite to each other, and the substrate 100 includes a first semiconductor material layer 110, a first dielectric layer 120, a second semiconductor material layer 130, a second dielectric layer 140, and a third semiconductor material layer 150 stacked in sequence from the first surface 101 to the second surface 102;

[0140] The mirror 260 and the coil 250 are located on the first surface 101 side;

[0141] A first groove 160 is located in the first semiconductor material layer 110 and penetrates the first semiconductor material layer 110;

[0142] A plurality of second grooves 170 , located in the second semiconductor material layer 130 and penetrating the second semiconductor material layer 130 , the second grooves 170 being connected to the first grooves 160 ;

[0143] The portion of the second semiconductor material layer 130 located between two adjacent second grooves 170 is retained to form a reinforcing rib structure 180. In a direction perpendicular to the first surface 101 and the second surface 102, the reinforcing rib structure 180 is located within the projection range of the mirror 260 and the coil 250.

[0144] The area of ​​the first end 181 of the reinforcing rib structure 180 is smaller than the area of ​​the second end 182 of the reinforcing rib structure 180 . The first end 181 is the end of the reinforcing rib structure 180 away from the second dielectric layer 140 , and the second end 182 is the end of the reinforcing rib structure 180 close to the second dielectric layer 140 .

[0145] Therefore, the thickness of the rib structure 180 is defined by the thickness of the second semiconductor material layer 130, which reduces the influence of the accuracy and stability of the etching process on the uniformity of the thickness of the rib structure, making the thickness uniformity of the rib structure 180 better, which is beneficial to improving product stability and yield; the area of ​​the first end 181 of the rib structure 180 is smaller than the area of ​​the second end 182 of the rib structure 180, which reduces the weight of the rib structure 180 while ensuring the strength of the rib structure 180, thereby improving the impact resistance of the device.

[0146] It can be understood that the area of ​​the second end 182 of the reinforcing rib structure 180 is larger, that is, the contact area between the reinforcing rib structure 180 and the second dielectric layer 140 is larger, so that the reinforcing rib structure 180 has greater strength; under the condition that the thickness of the reinforcing rib structure 180 is certain, compared with the case where the area of ​​the first end 181 is equal to the area of ​​the second end 182, the area of ​​the first end 181 of the reinforcing rib structure 180 away from the second dielectric layer 140 is smaller, so that the volume of the reinforcing rib structure 180 is reduced, that is, the weight of the reinforcing rib structure 180 is reduced; thus, the area of ​​the first end 181 of the reinforcing rib structure 180 is smaller than the area of ​​the second end 182 of the reinforcing rib structure 180, so that the reinforcing rib structure 180 has better mechanical properties and weight advantages, which is beneficial to improving the impact resistance of the device.

[0147] Optionally, in a direction perpendicular to the first surface 101 and the second surface 102 , the cross-section of the reinforcing rib structure 180 includes a trapezoid, the upper base of the trapezoid is located at the second end 182 , and the lower base of the trapezoid is located at the first end 181 .

[0148] Optionally, the angle between the side wall 183 of the reinforcing rib structure 180 and the second end 182 is in the range of 50° to 60°, and the side wall 183 connects the first end 181 and the second end 182. Thus, while the reinforcing rib structure 180 has better mechanical properties and weight advantages, the precision and difficulty of the process are taken into account. In this embodiment, the angle between the side wall 183 of the reinforcing rib structure 180 and the second end 182 is specifically 55°, for example.

[0149] It should be noted that the MEMS device manufacturing method embodiment, MEMS device embodiment and MEMS micromirror embodiment provided in the present application belong to the same concept; the technical features in the technical solutions recorded in the embodiments can be arbitrarily combined without conflict. However, it should be further noted that the MEMS micromirror provided in the embodiment of the present application, the combination of its various technical features can already solve the technical problem to be solved by the present application; therefore, the MEMS micromirror provided in the embodiment of the present application may not be limited by the MEMS device manufacturing method provided in the embodiment of the present application, and any MEMS micromirror manufactured by the manufacturing method that can form the MEMS micromirror structure provided in the embodiment of the present application is within the scope of protection of the present application.

[0150] It should be understood that the above embodiments are exemplary and are not intended to include all possible implementations included in the claims. Various modifications and changes may be made on the basis of the above embodiments without departing from the scope of the present disclosure. Similarly, the various technical features of the above embodiments may be arbitrarily combined to form other embodiments of the present application that may not be explicitly described. Therefore, the above embodiments only express several implementations of the present application and do not limit the scope of protection of the patent of this application.

Claims

1. A method for preparing a MEMS device, characterized in that: include: Providing a substrate, the substrate comprising a first surface and a second surface opposite to each other, the substrate comprising a first semiconductor material layer, a first dielectric layer, a second semiconductor material layer, a second dielectric layer, and a third semiconductor material layer sequentially stacked from the first surface to the second surface, the first dielectric layer comprising a mask portion, the mask portion comprising a mask area and a non-mask area; forming a device structure layer on the second surface side, wherein at least a portion of the device structure layer is used to form a movable structure; Etching the first semiconductor material layer on the first surface side to form a first groove exposing the mask portion of the first dielectric layer; Using the portion of the first dielectric layer located in the mask area as a mask, etching is performed through the first groove to form a plurality of second grooves exposing the second dielectric layer in the second semiconductor material layer, and a portion of the second semiconductor material layer located between two adjacent second grooves is retained to form a reinforcing rib structure, and in a direction perpendicular to the first surface and the second surface, the reinforcing rib structure is located within the projection range of the movable structure.

2. The method for preparing a MEMS device according to claim 1, characterized in that: The providing of the substrate comprises: Providing the first semiconductor material layer; forming the first dielectric layer on the first semiconductor material layer; Performing a patterning process on the mask portion of the first dielectric layer to remove the portion of the first dielectric layer located in the non-mask area and retaining the portion of the first dielectric layer located in the mask area; The second semiconductor material layer is disposed on the first dielectric layer after the patterning process is performed.

3. The method for preparing a MEMS device according to claim 2, characterized in that: The forming of the first groove and the forming of the second groove are successively implemented in the same etching process.

4. The method for preparing a MEMS device according to claim 1, characterized in that: The area of ​​the first end of the reinforcing rib structure is smaller than the area of ​​the second end of the reinforcing rib structure. The first end is the end of the reinforcing rib structure away from the second medium layer, and the second end is the end of the reinforcing rib structure close to the second medium layer.

5. The method for preparing a MEMS device according to claim 4, characterized in that: The included angle between the side wall of the reinforcing rib structure and the second end is in a range of 50° to 60°, and the side wall connects the first end and the second end.

6. The method for preparing a MEMS device according to claim 4 or 5, characterized in that: The process of forming the second groove includes a wet etching process.

7. A MEMS device, characterized in that: The MEMS device is prepared by the method for preparing the MEMS device according to any one of claims 1 to 6.

8. A MEMS micromirror, characterized in that: include: A substrate, comprising a first surface and a second surface opposite to each other, the substrate comprising a first semiconductor material layer, a first dielectric layer, a second semiconductor material layer, a second dielectric layer, and a third semiconductor material layer stacked in sequence from the first surface to the second surface; A mirror and a coil, located on the first surface side; A first groove is located in the first semiconductor material layer and penetrates the first semiconductor material layer; A plurality of second grooves, located in the second semiconductor material layer and penetrating the second semiconductor material layer, wherein the second grooves are connected to the first grooves; A portion of the second semiconductor material layer located between two adjacent second grooves is retained to form a reinforcing rib structure, and in a direction perpendicular to the first surface and the second surface, the reinforcing rib structure is located within the projection range of the mirror and the coil; wherein the first dielectric layer covers a first end of the reinforcing rib structure, and the first end is an end of the reinforcing rib structure away from the second dielectric layer.

9. A MEMS micromirror, characterized in that: include: A substrate, comprising a first surface and a second surface opposite to each other, the substrate comprising a first semiconductor material layer, a first dielectric layer, a second semiconductor material layer, a second dielectric layer, and a third semiconductor material layer stacked in sequence from the first surface to the second surface; A mirror and a coil, located on the first surface side; A first groove is located in the first semiconductor material layer and penetrates the first semiconductor material layer; A plurality of second grooves, located in the second semiconductor material layer and penetrating the second semiconductor material layer, wherein the second grooves are connected to the first grooves; A portion of the second semiconductor material layer located between two adjacent second grooves is retained to form a reinforcing rib structure, and in a direction perpendicular to the first surface and the second surface, the reinforcing rib structure is located within the projection range of the mirror and the coil; The area of ​​the first end of the reinforcing rib structure is smaller than the area of ​​the second end of the reinforcing rib structure, the first end is the end of the reinforcing rib structure away from the second medium layer, and the second end is the end of the reinforcing rib structure close to the second medium layer.

10. The MEMS micromirror according to claim 9, characterized in that: The included angle between the side wall of the reinforcing rib structure and the second end is in a range of 50° to 60°, and the side wall connects the first end and the second end.