Refining method of sodium carbonate crude product in process of preparing tetrahydrofuran from LBDO

Through the steps of dissolution, ultrafiltration, dual-effect evaporation and drying, the crude sodium carbonate produced in the preparation of tetrahydrofuran of LBDO solved the problem of high cost of hazardous waste treatment, improved the purity and economic benefits of the product, and realized carbonic acid High-efficiency refining of crude sodium products.

CN118908244APending Publication Date: 2024-11-08INNER MONGOLIA MEIBANG ZHONGKE NEW MATERIAL CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202410954315.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-17
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

The crude sodium carbonate produced in the preparation of tetrahydrofuran of LBDO is a hazardous waste and has high treatment costs and needs to be refined to reduce environmental protection treatment costs and improve economic benefits.

Method used

The crude sodium carbonate product is refined by dissolution, ultrafiltration separation, dual-effect evaporation and drying steps, including adding pure water to the crude sodium carbonate product for dissolution, ultrafiltration using the surface-treated ceramic membrane, followed by dual-effect evaporation and Dry, and the purity of sodium carbonate and the total base amount are increased by this method.

Benefits of technology

It effectively reduces the cost of hazardous waste treatment of crude sodium carbonate products, improves the purity of the product, and makes it meet the standard of Class II qualified products in GB/T 210-2022, solves the problem of hazardous waste treatment and increases economic benefits.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure HDA0004948282300000011
    Figure HDA0004948282300000011
  • Figure HDA0004948282300000012
    Figure HDA0004948282300000012
Patent Text Reader

Abstract

The invention provides a method for refining a sodium carbonate crude product in a process of preparing tetrahydrofuran from LBDO, and belongs to the technical field of chemical product refinement, the method comprises the following steps: adding pure water into the sodium carbonate crude product for dissolving to obtain a sodium carbonate crude product solution; carrying out solid-liquid separation on the sodium carbonate crude product solution by adopting ultrafiltration to obtain sodium carbonate ultrafiltrate and concentrated solution; carrying out filter pressing treatment on the concentrated solution to obtain a clear solution and a solid substance; mixing the sodium carbonate ultrafiltrate obtained by ultrafiltration with the clear liquid obtained by filter pressing to obtain a sodium carbonate solution; the sodium carbonate solution is subjected to double-effect evaporation, water in the sodium carbonate solution is evaporated out, and meanwhile a kettle bottom solution is obtained; the kettle bottom solution is dried, free water is removed, and meanwhile the product sodium carbonate is obtained; by adopting the technology provided by the invention, the problem of hazardous waste treatment of the sodium carbonate crude product in the process of producing tetrahydrofuran from LBDO can be solved, and the environment-friendly treatment cost is greatly reduced. The sodium carbonate product can be prepared, the comprehensive utilization of LBDO waste liquid resources is further maximized, and remarkable economic benefits are brought to companies.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of chemical product refining, and more specifically, relates to a method for refining crude sodium carbonate in the process of preparing tetrahydrofuran from LBDO. Background Art

[0002] Tetrahydrofuran, THF for short, is an important organic synthetic raw material and a solvent with excellent performance, known as the "universal solvent". Tetrahydrofuran itself can be polycondensed into polytetrahydrofuran (PTMEG), which is an important raw material for the production of spandex, polyurethane (PU) and thermoplastic polyurethane (TPU) copolymers. Spandex fibers made of polytetrahydrofuran have good flexibility and resilience. When the elongation is 300%, the instantaneous rebound rate reaches 99.8%. The monofilament can be elongated 500% without breaking. It is known as the second skin of humans and is widely used in the field of textiles and clothing.

[0003] At present, tetrahydrofuran is mainly prepared by the 1,4-butanediol (BDO) cyclization dehydration method, which is widely used due to its simple production process, low reaction temperature, and high tetrahydrofuran yield.

[0004] For example, the patent document: A method for preparing tetrahydrofuran by liquid phase dehydration of 1,4-butanediol catalyzed by concentrated sulfuric acid (patent publication number: CN108148020B) comprises: contacting 1,4-butanediol with concentrated sulfuric acid and 13X molecular sieve to carry out liquid phase dehydration reaction of 1,4-butanediol to generate tetrahydrofuran, and distilling tetrahydrofuran during the liquid phase dehydration reaction, wherein the particle size of the 13X molecular sieve is less than or equal to 2 mm, and the surface sodium ion content does not exceed 20ppm. According to the method of the present invention, by adding specially treated 13X molecular sieve, the tar content is greatly reduced, the freezing point of the reaction liquid is greatly reduced, the operation flexibility is improved, and the operation is simplified, thereby significantly improving the application effect of the method for preparing tetrahydrofuran by liquid phase dehydration of 1,4-butanediol catalyzed by concentrated sulfuric acid.

[0005] In order to further reduce the production cost of tetrahydrofuran and solve the problem of treating BDO waste liquid (BDO content is about 10%-40%) in the BDO production process, BDO waste liquid (LBDO) is used to produce tetrahydrofuran. First, BDO in BDO waste liquid (LBDO) is extracted, and then BDO is converted into tetrahydrofuran. BDO tar is produced during the BDO extraction process. BDO tar mainly contains high-boiling substances with a boiling point above 230°C, sodium hydroxide, sodium formate and a small amount of 1,4-butanediol. BDO tar is usually incinerated at a high temperature of about 1000°C to obtain crude sodium carbonate and steam. The crude sodium carbonate mainly contains sodium carbonate, a small amount of castable solids dropped from the incinerator furnace, and a small amount of other inorganic salts. Since the crude sodium carbonate is produced in the tetrahydrofuran production process, it is a hazardous waste and needs to be sent to a hazardous waste treatment unit for treatment, and the treatment cost is relatively high. In order to convert crude sodium carbonate into non-hazardous chemicals, the crude sodium carbonate needs to be purified to solve the company's hazardous waste disposal problem and increase the company's economic benefits.

[0006] In order to solve the above problems, it is imperative to develop and study the purification method of crude sodium carbonate in the process of preparing tetrahydrofuran from LBDO. Summary of the invention

[0007] The object of the present invention is to provide a method for refining crude sodium carbonate in the process of preparing tetrahydrofuran from LBDO, aiming to solve the problem of solid waste treatment of crude sodium carbonate in the process of preparing tetrahydrofuran from LBDO, so as to further improve economic benefits.

[0008] To achieve the above object, the technical solution adopted by the present invention is:

[0009] A method for refining crude sodium carbonate in the process of preparing tetrahydrofuran from LBDO, the main steps comprising:

[0010] (1) Dissolution

[0011] First, pure water is added to the crude sodium carbonate and mixed to dissolve it to obtain a crude sodium carbonate solution.

[0012] The crude sodium carbonate is obtained by burning BDO tar, and mainly contains sodium carbonate and a small amount of solid powder of castable corroded during high-temperature burning. The sodium carbonate content (calculated as Na2CO3, on a dry basis) is 95-97w / %.

[0013] The concentration of solid powder in the crude sodium carbonate solution is 1% to 2.5%, the temperature is 20 to 60° C., and the pH value is alkaline.

[0014] Preferably, a flocculant may be added to the crude sodium carbonate solution to remove other inorganic salt ions.

[0015] Preferably, the flocculant can be selected from one or more of polyaluminium chloride (PAC), polyacrylamide (PAM), and polydimethyldiallylammonium chloride.

[0016] (2) Ultrafiltration separation

[0017] The crude sodium carbonate solution obtained in step (1) is subjected to solid-liquid separation by ultrafiltration, the crude sodium carbonate solution is first concentrated, and then dialyzed with pure water, the sodium carbonate in the concentrated solution is dialyzed into the ultrafiltrate, and when the sodium carbonate content in the concentrated solution is ≤1%, the addition of pure water is stopped to obtain a sodium carbonate ultrafiltrate and a concentrated solution; the concentrated solution is subjected to filter pressing to obtain a clear liquid and a solid substance; the sodium carbonate ultrafiltrate obtained by ultrafiltration and the clear liquid obtained by filter pressing are mixed to obtain a sodium carbonate solution.

[0018] The concentration of solid powder in the ultrafiltration concentrate is about 10% to 15%.

[0019] Among them, the amount of pure water used in ultrafiltration dialysis is 1.5 to 2.5 times the mass of the ultrafiltration concentrate.

[0020] Among them, ultrafiltration uses surface-treated ceramic membranes.

[0021] Among them, the filtration accuracy of the surface-treated ceramic membrane is 20 to 1000 nm.

[0022] Among them, the temperature during ultrafiltration is 30-50°C, the membrane inlet pressure is 0.35-0.45MPa, and the membrane outlet pressure is 0.15-0.2MPa.

[0023] Wherein, the surface treatment step is:

[0024] Step 1: Boil the ceramic membrane in a strong alkaline solution for 50-180 minutes, then wash and dry to obtain a fresh ceramic membrane;

[0025] Step 2: Immerse the ceramic membrane in the impregnation liquid, and then take it out and dry it;

[0026] Step 3: Subsequently, the dried ceramic film is placed in a plasma surface treatment apparatus, argon gas is passed through the plasma surface treatment apparatus to remove air, and then discharge treatment is performed at 10 to 15 kV for 10 to 15 minutes in a mixed atmosphere of ammonia, tungsten hexafluoride, and tetra(1-methylvinyl)stannane vapor; after the treatment, an organic tin modified ceramic film is obtained;

[0027] Wherein, the strong alkaline solution includes potassium hydroxide solution, sodium hydroxide solution and calcium hydroxide solution; the concentration of the potassium hydroxide solution or the sodium hydroxide solution is 5-10 mol / L; the calcium hydroxide solution is a saturated solution;

[0028] The impregnation liquid comprises mercaptosiloxane and solvent in a mass ratio of 1:20-30, mixed at room temperature for 10-30 hours, the mercaptosiloxane is selected from γ-mercaptopropyltriethoxysilane or γ-mercaptopropyltrimethoxysilane, and the solvent is selected from a combination of one or more of n-heptane, ethanol, acetone, acetonitrile and benzene;

[0029] Wherein, the argon gas flow rate is 10-30 ml / min;

[0030] The ammonia, tungsten hexafluoride and tetra(1-methylvinyl)stannane vapor are mixed in a volume ratio of 1-1.2:0.02-0.05:0.3-0.6.

[0031] Among them, the filtration can be performed by a plate and frame filter press or other equipment that can achieve the filtration function.

[0032] (3) Double-effect evaporation

[0033] The sodium carbonate solution obtained in step (2) is subjected to double-effect evaporation to evaporate water in the sodium carbonate solution and obtain kettle bottom liquid at the same time.

[0034] Among them, the temperature during double-effect evaporation is 70-85°C and the pressure is -0.08--0.09MPa.

[0035] (4) Drying

[0036] The bottom liquid obtained in step (3) is dried to remove free water and obtain the product sodium carbonate.

[0037] The drying temperature is 100 to 110°C.

[0038] The total mass of the pure water used for dissolving the crude sodium carbonate and the dialyzed water used for ultrafiltration in the present invention is greater than or equal to the total mass of the water evaporated by double-effect evaporation and drying.

[0039] The total alkali content of the obtained sodium carbonate product (calculated as Na2CO3, on a dry basis) w / %≥98%, and the product quality can meet the Class I qualified product standard of GB / T 210-2022.

[0040] Technical effects:

[0041] (1) The technology of the present invention can solve the problem of hazardous waste treatment of crude sodium carbonate in the process of producing tetrahydrofuran with LBDO, and significantly reduce the cost of environmental protection treatment.

[0042] (2) In the technology of the present invention, the pure water used in the dissolution and ultrafiltration steps can be applied to the free water removed by double-effect evaporation and drying, which basically meets the water balance and reduces the consumption of pure water.

[0043] (3) The ceramic membrane introduces thiol groups. Under the influence of plasma, the thiol groups (-SH) on the surface of the ceramic membrane react with the carbon-carbon double bond (C=C) in tetra(1-methylvinyl)stannane by click chemistry. The thiol group of the thiol opens the π bond with the olefin to form a new carbon-sulfur bond, thereby obtaining a functionalized ceramic membrane grafted with organic tin. The ceramic membrane grafted with organic tin and tungsten complexes has enhanced chemical adsorption capacity due to the introduction of surface functional groups, and can effectively adsorb impurities in the solution, such as metal ions and organic pollutants. This characteristic can be used to improve the purity of sodium carbonate products. The sodium carbonate product prepared by the technology of the present invention has a total alkali content (calculated as Na2CO3, on a dry basis) w / % ≥ 98.0%, and the product quality can meet the Class II qualified product standard in GB / T 210-2022. BRIEF DESCRIPTION OF THE DRAWINGS

[0044] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0045] Figure 1 A process flow chart of a method for refining crude sodium carbonate in the process of preparing tetrahydrofuran from LBDO provided in an embodiment of the present invention.

[0046] Figure 2 It is the industrial sodium carbonate standard GB / T 210-2022. DETAILED DESCRIPTION

[0047] In view of the deficiencies in the prior art, the inventor of this case, after long-term research and extensive practice, was able to propose the technical solution of the present invention. The technical solution, its implementation process and principle, etc. will be further explained as follows.

[0048] Example 1

[0049] The method for refining crude sodium carbonate in the process of preparing tetrahydrofuran from LBDO provided by the present invention comprises the following steps:

[0050] (1) Dissolution

[0051] First, add 540 kg of pure water to 200 kg of crude sodium carbonate with a sodium carbonate mass content of 95 w / % and mix well, then add a small amount of flocculant polyaluminium chloride (PAC) dropwise to obtain 740 kg of crude sodium carbonate solution with a sodium carbonate mass concentration of 25.7 w / % and a solid mass content of 2.5%, the temperature is 30°C, and the pH value is 10.5.

[0052] The crude sodium carbonate is obtained by incinerating BDO tar at a high temperature of about 1000°C, and mainly contains sodium carbonate and solid powder of castables corroded during the high-temperature incineration.

[0053] (2) Ultrafiltration separation

[0054] The crude sodium carbonate solution obtained in step (1) is separated by a surface-treated ceramic membrane separator with a filtration accuracy of 30 nm, and the membrane inlet pressure is controlled to be 0.35 MPa and the membrane outlet pressure is controlled to be 0.15 MPa; the filtration temperature is controlled at 30° C. When the concentration multiple reaches 14 times, pure water is continuously added to the concentrated solution side. When the sodium carbonate content on the concentrated solution side is less than 1%, no more pure water is added. The total mass of the dialyzed pure water added is 75 kg, and 765 kg of sodium carbonate ultrafiltrate and 50 kg of concentrated solution are obtained.

[0055] 50 kg of the concentrated solution was filtered using a plate and frame filter press to obtain a clear liquid and a solid substance, and the sodium carbonate ultrafiltrate obtained by filtration with a ceramic membrane and the clear liquid obtained by filtration with the plate and frame filter press were mixed to obtain a sodium carbonate solution.

[0056] The surface treatment method of the ceramic membrane after the surface treatment is as follows:

[0057] Step 1: Boil the ceramic membrane in a strong alkaline solution for 50 minutes, then wash and dry to obtain a fresh ceramic membrane;

[0058] Step 2: Immerse the ceramic membrane in the impregnation liquid, and then take it out and dry it;

[0059] Step 3: Then, the dried ceramic film is placed in a plasma surface treatment instrument, argon gas is passed through the plasma surface treatment instrument to remove air, and then discharge treatment is carried out at 10 kV for 10 minutes in a mixed atmosphere of ammonia, tungsten hexafluoride, and tetra(1-methylvinyl)stannane vapor; after the treatment, an organic tin modified ceramic film is obtained;

[0060] The strong alkaline solution is a potassium hydroxide solution; the concentration of the potassium hydroxide solution is 5 mol / L;

[0061] The impregnation liquid comprises mercaptosiloxane and a solvent in a mass ratio of 1:20, mixed at room temperature for 10 hours, the mercaptosiloxane is selected from γ-mercaptopropyltriethoxysilane, and the solvent is selected from acetonitrile;

[0062] The argon gas flow rate is 10 ml / min;

[0063] The ammonia, tungsten hexafluoride and tetra(1-methylvinyl)stannane vapor are mixed in a volume ratio of 1:0.02:0.3.

[0064] (3) Double-effect evaporation

[0065] The sodium carbonate solution obtained in step (2) is subjected to double-effect evaporation at a temperature of 70° C. and a pressure of −0.08 MPa to evaporate water in the sodium carbonate solution and obtain a kettle bottom liquid.

[0066] (4) Drying

[0067] The bottom liquid obtained in step (3) is dried at a temperature of 105° C. to remove free water, and 193 kg of product sodium carbonate is obtained. The total alkali content of the product sodium carbonate (calculated as Na2CO3, on a dry basis) is 98.12 w / %, meeting the Class II qualified product standard in GB / T 210-2022.

[0068] The total mass of the pure water used for dissolving the crude sodium carbonate and the dialyzed water used for ultrafiltration in the present invention is greater than or equal to the total mass of the water evaporated by double-effect evaporation and drying.

[0069] Example 2

[0070] The method for refining crude sodium carbonate in the process of preparing tetrahydrofuran from LBDO provided by the present invention comprises the following steps:

[0071] (1) Dissolution

[0072] First, add 450 kg of pure water to 200 kg of crude sodium carbonate with a sodium carbonate mass content of 96 w / % and mix well, then add a small amount of flocculant polyacrylamide (PAM) dropwise to obtain 650 kg of crude sodium carbonate solution with a sodium carbonate mass concentration of 29.5 w / % and a solid mass content of 1%, the temperature is 40° C., and the pH value is 10.6.

[0073] The crude sodium carbonate is obtained by incinerating BDO tar at a high temperature of about 1000°C, and mainly contains sodium carbonate and solid powder of castables corroded during the high-temperature incineration.

[0074] (2) Ultrafiltration separation

[0075] The crude sodium carbonate solution obtained in step (1) is separated by using a surface-treated ceramic membrane separator with a filtration accuracy of 50 nm, and the membrane inlet pressure is controlled to be 0.4 MPa and the membrane outlet pressure is controlled to be 0.18 MPa; the filtration temperature is controlled at 40° C., and when the concentration multiple reaches 47 times, pure water is continuously added to the concentrated solution side. When the sodium carbonate content on the concentrated solution side is less than 1%, no more pure water is added. The total mass of the dialyzed pure water added is 20 kg, and 656 kg of sodium carbonate ultrafiltrate and 13 kg of concentrated solution are obtained.

[0076] 13 kg of the concentrated solution was filtered using a plate and frame filter press to obtain a clear liquid and a solid substance, and the sodium carbonate ultrafiltrate obtained by filtration with a ceramic membrane and the clear liquid obtained by filtration with the plate and frame filter press were mixed to obtain a sodium carbonate solution.

[0077] The surface treatment method of the ceramic membrane after the surface treatment is as follows:

[0078] Step 1: Boil the ceramic membrane in a strong alkaline solution for 120 minutes, then wash and dry to obtain a fresh ceramic membrane;

[0079] Step 2: Immerse the ceramic membrane in the impregnation liquid, and then take it out and dry it;

[0080] Step 3: Then, the dried ceramic film is placed in a plasma surface treatment apparatus, argon gas is passed through the plasma surface treatment apparatus to remove air, and then discharge treatment is performed at 12 kV for 12 minutes in a mixed atmosphere of ammonia, tungsten hexafluoride, and tetra(1-methylvinyl)stannane vapor; after the treatment, an organotin-modified ceramic film is obtained;

[0081] The strong alkaline solution is a sodium hydroxide solution; the concentration of the sodium hydroxide solution is 8 mol / L;

[0082] The impregnation liquid comprises mercaptosiloxane and a solvent in a mass ratio of 1:25, mixed at room temperature for 20 hours, the mercaptosiloxane is selected from γ-mercaptopropyltrimethoxysilane, and the solvent is selected from acetone;

[0083] The argon gas flow rate is 20 ml / min;

[0084] The ammonia, tungsten hexafluoride and tetra(1-methylvinyl)stannane vapor are mixed in a volume ratio of 1.1:0.03:0.45.

[0085] (3) Double-effect evaporation

[0086] The sodium carbonate solution obtained in step (2) is subjected to double-effect evaporation at a temperature of 80° C. and a pressure of −0.08 MPa to evaporate water in the sodium carbonate solution and obtain a kettle bottom liquid.

[0087] (4) Drying

[0088] The bottom liquid obtained in step (3) is dried at a temperature of 110° C. to remove free water, and 195 kg of product sodium carbonate is obtained. The total alkali content of the product sodium carbonate (calculated as Na2CO3, on a dry basis) is 98.21%, which meets the Class II qualified product standard in GB / T210-2022.

[0089] The total mass of the pure water used for dissolving the crude sodium carbonate and the dialyzed water used for ultrafiltration in the present invention is greater than or equal to the total mass of the water evaporated by double-effect evaporation and drying.

[0090] Example 3

[0091] The method for refining crude sodium carbonate in the process of preparing tetrahydrofuran from LBDO provided by the present invention comprises the following steps:

[0092] (1) Dissolution

[0093] First, add 540 kg of pure water to 200 kg of crude sodium carbonate with a sodium carbonate mass content of 96.5 w / % and mix well, then add a small amount of flocculant polydimethyldiacrylammonium chloride dropwise to obtain 740 kg of crude sodium carbonate solution with a sodium carbonate mass concentration of 26 w / % and a solid mass content of 1.5%, the temperature is 30°C, and the pH value is 10.7.

[0094] The crude sodium carbonate is obtained by incinerating BDO tar at a high temperature of about 1000°C, and mainly contains sodium carbonate and solid powder of castables corroded during the high-temperature incineration.

[0095] (2) Ultrafiltration separation

[0096] The crude sodium carbonate solution obtained in step (1) is separated by a surface-treated ceramic membrane separator with a filtration accuracy of 1000 nm, and the membrane inlet pressure is controlled to be 0.40 MPa and the membrane outlet pressure is controlled to be 0.15 MPa; the filtration temperature is controlled at 50° C., and when the concentration multiple reaches 24 times, pure water is continuously added to the concentrated solution side. When the sodium carbonate content on the concentrated solution side is less than 1%, no more pure water is added. The total mass of the dialyzed pure water added is 45 kg, and 754 kg of sodium carbonate ultrafiltrate and 30 kg of concentrated solution are obtained.

[0097] 30 kg of the concentrated solution was filtered using a plate and frame filter press to obtain a clear liquid and a solid substance, and the sodium carbonate ultrafiltrate obtained by metal membrane filtration and the clear liquid obtained by the plate and frame filter press were mixed to obtain a sodium carbonate solution.

[0098] Wherein, the surface treatment method of the ceramic membrane after the surface treatment is:

[0099] Step 1: Boil the ceramic membrane in a strong alkaline solution for 180 minutes, then wash and dry to obtain a fresh ceramic membrane;

[0100] Step 2: Immerse the ceramic membrane in the impregnation liquid, and then take it out and dry it;

[0101] Step 3: Then, the dried ceramic film is placed in a plasma surface treatment instrument, argon gas is passed through the plasma surface treatment instrument to remove air, and then discharge treatment is carried out at 15 kV for 15 minutes in a mixed atmosphere of ammonia, tungsten hexafluoride, and tetra(1-methylvinyl)stannane vapor; after the treatment, an organic tin modified ceramic film is obtained;

[0102] The strong alkaline solution is a calcium hydroxide solution; the calcium hydroxide solution is a saturated solution;

[0103] The impregnation liquid comprises mercaptosiloxane and a solvent in a mass ratio of 1:30, mixed at room temperature for 30 hours, the mercaptosiloxane is selected from γ-mercaptopropyltriethoxysilane, and the solvent is selected from n-heptane;

[0104] The argon gas flow rate is 30 ml / min;

[0105] The ammonia, tungsten hexafluoride and tetra(1-methylvinyl)stannane vapor are mixed in a volume ratio of 1.2:0.05:0.6.

[0106] (3) Double-effect evaporation

[0107] The sodium carbonate solution obtained in step (2) is subjected to double-effect evaporation at a temperature of 85° C. and a pressure of −0.09 MPa to evaporate water in the sodium carbonate solution and obtain a kettle bottom liquid.

[0108] (4) Drying

[0109] The bottom liquid obtained in step (3) is dried at a temperature of 108° C. to remove free water, and 196 kg of product sodium carbonate is obtained. The total alkali content of the product sodium carbonate (calculated as Na2CO3, on a dry basis) is 98.18%, meeting the Class II qualified product standard in GB / T210-2022.

[0110] The total mass of the pure water used for dissolving the crude sodium carbonate and the dialyzed water used for ultrafiltration in the present invention is greater than or equal to the total mass of the water evaporated by double-effect evaporation and drying.

[0111] Comparative Example 1

[0112] In this example, a ceramic membrane is used to replace the surface-treated ceramic membrane, and the remaining steps are the same as those in Example 1.

[0113] The bottom liquid obtained in step (3) is dried at a temperature of 105° C. to remove free water, and 193 kg of product sodium carbonate is obtained. The total alkali content of the product sodium carbonate (calculated as Na2CO3, on a dry basis) is 97.74 w / %, which does not meet the Class II qualified product standard in GB / T 210-2022.

[0114] Comparative Example 2

[0115] In this example, tetra(1-methylvinyl)stannane was not added during the surface treatment of the ceramic membrane, and the remaining steps were consistent with those in Example 1.

[0116] The bottom liquid obtained in step (3) is dried at a temperature of 105° C. to remove free water, and 193 kg of product sodium carbonate is obtained. The total alkali content of the product sodium carbonate (calculated as Na2CO3, on a dry basis) is 97.92 w / %, which does not meet the Class II qualified product standard in GB / T 210-2022.

[0117] Embodiment The sodium carbonate product prepared by the technology of the present invention has a total alkali content (calculated as Na2CO3, on a dry basis) w / % ≥ 98.0%, and the product quality can meet the Class II qualified product standard in GB / T 210-2022.

[0118] The above is only a preferred embodiment of the present invention. It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made without departing from the principle of the present invention. These improvements and modifications should also be regarded as the scope of protection of the present invention.

Claims

1. A method for refining crude sodium carbonate in the process of preparing tetrahydrofuran from LBDO, characterized in that: include: (1) Dissolution First, pure water is added to the crude sodium carbonate and mixed to dissolve it, so as to obtain a crude sodium carbonate solution; (2) Ultrafiltration separation The crude sodium carbonate solution obtained in step (1) is subjected to solid-liquid separation by ultrafiltration, the crude sodium carbonate solution is first concentrated, and then dialyzed with pure water, the sodium carbonate in the concentrate is dialyzed into the ultrafiltrate, and when the sodium carbonate content in the concentrate is ≤1%, the addition of pure water is stopped to obtain a sodium carbonate ultrafiltrate and a concentrated solution; the concentrated solution is subjected to filter pressing to obtain a clear liquid and a solid substance; the sodium carbonate ultrafiltrate obtained by ultrafiltration and the clear liquid obtained by filter pressing are mixed to obtain a sodium carbonate solution; (3) Double-effect evaporation The sodium carbonate solution obtained in step (2) is subjected to double-effect evaporation to evaporate water in the sodium carbonate solution and obtain a bottom liquid; Among them, the temperature during double-effect evaporation is 70-85°C and the pressure is -0.08--0.09MPa; (4) Drying The bottom liquid obtained in step (3) is dried to remove free water and obtain the product sodium carbonate.

2. The method for refining crude sodium carbonate in the process of preparing tetrahydrofuran from LBDO according to claim 1, characterized in that: The crude sodium carbonate in step (1) is obtained by incineration of BDO tar, and mainly contains sodium carbonate and a small amount of solid powder of castable corroded during high-temperature incineration, the sodium carbonate content is 95-97w / %, the concentration of solid powder in the crude sodium carbonate solution is 0%-2.5%, the temperature is 20-60°C, and the pH value is alkaline.

3. The method for refining crude sodium carbonate in the process of preparing tetrahydrofuran from LBDO according to claim 1, characterized in that: A flocculant may also be added to the crude sodium carbonate solution in step (1) to remove other inorganic salt ions.

4. The method for refining crude sodium carbonate in the process of preparing tetrahydrofuran from LBDO according to claim 1, characterized in that: In step (2), the concentration of solid powder in the ultrafiltration concentrate is 10% to 15%, and the amount of pure water used for ultrafiltration dialysis is 1.5 to 2.5 times the mass of the ultrafiltration concentrate.

5. The method for refining crude sodium carbonate in the process of preparing tetrahydrofuran from LBDO according to claim 1, characterized in that: In step (2), the ultrafiltration uses a surface-treated ceramic membrane with a filtration accuracy of 20 to 1000 nm, the temperature during ultrafiltration is 30 to 50° C., the membrane inlet pressure is 0.35 to 0.45 MPa, and the membrane outlet pressure is 0.15 to 0.2 MPa; The surface treatment steps are: Step 1: Boil the ceramic membrane in a strong alkaline solution for 50-180 minutes, then wash and dry to obtain a fresh ceramic membrane; Step 2: Immerse the ceramic membrane in the impregnation liquid, and then take it out and dry it; Step 3: Subsequently, the dried ceramic film is placed in a plasma surface treatment apparatus, argon gas is passed through the plasma surface treatment apparatus to remove air, and then discharge treatment is performed at 10 to 15 kV for 10 to 15 minutes in a mixed atmosphere of ammonia, tungsten hexafluoride, and tetra(1-methylvinyl)stannane vapor; after the treatment, an organic tin modified ceramic film is obtained; The strong alkali solution includes potassium hydroxide solution, sodium hydroxide solution and calcium hydroxide solution; the concentration of the potassium hydroxide solution or the sodium hydroxide solution is 5-10 mol / L; the calcium hydroxide solution is a saturated solution; The impregnation liquid comprises mercaptosiloxane and solvent in a mass ratio of 1:20-30, mixed at room temperature for 10-30 hours, the mercaptosiloxane is selected from γ-mercaptopropyltriethoxysilane or γ-mercaptopropyltrimethoxysilane, and the solvent is selected from a combination of one or more of n-heptane, ethanol, acetone, acetonitrile and benzene; The argon gas flow rate is 10-30 ml / min; The ammonia, tungsten hexafluoride and tetra(1-methylvinyl)stannane vapor are mixed in a volume ratio of 1-1.2:0.02-0.05:0.3-0.

6.

6. The method for refining crude sodium carbonate in the process of preparing tetrahydrofuran from LBDO according to claim 1, characterized in that: In step (2), the filtration can be performed using a plate and frame filter press or other equipment that can achieve the filtration function.

7. The method for refining crude sodium carbonate in the process of preparing tetrahydrofuran from LBDO according to claim 1, characterized in that: In step (3), the temperature during double-effect evaporation is 70 to 85° C., and the pressure is -0.08 to -0.09 MPa.

8. The method for refining crude sodium carbonate in the process of preparing tetrahydrofuran from LBDO according to claim 1, characterized in that: In step (4), the drying temperature is 100-110°C.

9. The method for refining crude sodium carbonate in the process of preparing tetrahydrofuran from LBDO according to claim 1, characterized in that: The total mass of pure water used for dissolving the crude sodium carbonate and dialyzed water used for ultrafiltration is greater than or equal to the total mass of water evaporated by double-effect evaporation and drying.

10. The method for refining crude sodium carbonate in the process of preparing tetrahydrofuran from LBDO according to claim 1, characterized in that: The total alkali content of the obtained sodium carbonate product w / % is ≥98%.

Citation Information

Patent Citations

  • A method for preparing tetrahydrofuran by concentrated sulfuric acid-catalyzed liquid-phase dehydration of 1,4-butanediol.

    CN108148020B