Zero-discharge treatment method for grey cloth bleaching wastewater
Through the segmented treatment schemes such as waste heat recovery, chemical recovery and wastewater reuse, combined with the selective removal technology of modified carbon spheres and ultrafiltration membranes, the problems of high energy consumption and high cost of wastewater treatment in the existing technology are solved, and the problem of high energy consumption and cost of wastewater treatment in the existing technology is realized. Resource reuse and zero-emission treatment of grey cloth deflooding wastewater.
Patent Information
- Application Number
- CN202411180649.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-27
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2044-08-27
AI Technical Summary
The existing grey cloth deflooding wastewater treatment process regards refining agents other than pollutants as waste, which fails to effectively reuse, resulting in high energy consumption, high cost and failure to effectively reduce the complexity of wastewater.
A zero-discharge treatment method for defrosting wastewater in grey cloth was designed. Through the segmented treatment schemes such as waste heat recovery, bleaching agent recycling, reboiling agent recycling and wastewater reuse, the modified carbon balls and ultrafiltration membranes are used to selectively remove pollution. The microbial degradation membrane separation and coupling process realizes the resource recycling of wastewater.
Resource recycling of grey cloth debleaching agents has been realized, which significantly reduces wastewater treatment costs, reduces energy losses, and reduces wastewater complexity through segmented treatment and improves treatment efficiency.
Smart Images

Figure CN118908476A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of wastewater treatment, and in particular to a method for zero-discharge treatment of grey cloth debleaching wastewater. Background Art
[0002] Grey cloth is a kind of natural cotton cloth for printing and dyeing. Grey cloth needs to undergo bleaching treatment after production, which mainly includes: pre-washing, boiling and bleaching, primary water washing, re-boiling, secondary water washing, neutralization and acid washing. During boiling, bleaching and re-boiling, a large amount of high-temperature wastewater will be generated. The water contains refining agents, chelating agents and other substances. Direct discharge will affect the external environment.
[0003] In order to meet the green needs of environmentally friendly processing, the grey cloth debleaching wastewater needs to be further treated before it can be discharged; in response to the above problems, the current wastewater treatment process and treatment equipment still treat the high COD caused by refining agents other than pollutants as waste instead of recycling it as resources and energy, which will lead to problems such as high energy consumption in the terminal treatment process, large demand for chemicals, and high costs.
[0004] In order to solve the above problems, the present invention designs a zero-discharge treatment method for grey cloth debleaching wastewater, aiming to provide a selective treatment plan, so that wastewater and pollutants in the water are no longer just regarded as pollutants, but as resources and energy carriers, and key pollutants in the wastewater are selectively removed and reused in the debleaching process. Summary of the invention
[0005] In order to achieve the above object, the present invention designs a method for zero-discharge treatment of grey cloth debleaching wastewater, and the scheme is as follows:
[0006] The traditional method for treating grey cloth debleaching wastewater is: degreasing and bleaching the grey cloth in sequence through pre-washing, boiling and bleaching, primary water washing, re-boiling, secondary water washing, pickling, and concentration processes; and the zero-discharge treatment method for grey cloth debleaching wastewater designed by the present invention adds the following process sections to the above process flow:
[0007] Process 1: Waste heat recovery: A heat exchange process is set up in the boiling, bleaching and re-boiling process section to recover the waste heat, and then transfer the waste heat to the concentration process section;
[0008] Process 2, recovery of boiling and bleaching agent: the wastewater generated by boiling and bleaching and the wastewater generated by the first washing are recorded as the first wastewater, and the first wastewater is treated based on the first adsorption process to obtain the first treated wastewater;
[0009] The first adsorption process is: firstly, the first wastewater is subjected to the first adsorption pretreatment by using tubular ceramic membrane adsorption, and then the first adsorption treatment is performed by using modified carbon ball adsorption and tubular ultrafiltration membrane adsorption;
[0010] Process 3, recovery of reboiling reagent: the wastewater generated by reboiling and the wastewater generated by secondary washing are recorded as the second wastewater, and the second wastewater is treated by the second adsorption process based on modified carbon balls to obtain the second treated wastewater;
[0011] Process 4, wastewater reuse: The wastewater generated in the pre-washing section is treated based on the microbial degradation membrane separation coupling process and returned to the pre-washing section; the first treated wastewater and the second treated wastewater are returned to the pre-washing section after being supplemented with water and chemicals.
[0012] Furthermore, the following technical constraints are imposed on the pre-washing, scouring, bleaching, re-scouring and pickling process sections in the conventional process of the present invention:
[0013] Constraint 1. In the pre-wash process:
[0014] The additives include: LAS (sodium dodecylbenzene sulfonate) as a refining agent, added in an amount of 0.3% owf; EDTA (ethylenediaminetetraacetic acid) as a complexing agent, added in an amount of 0.3% owf; JFC (fatty alcohol polyoxyethylene ether) as a penetrant, added in an amount of 0.3% owf; sodium polyacrylate as a dispersant, added in an amount of 0.3% owf;
[0015] Note: The %owf addition unit used here refers to the ratio of the weight of the additive to the weight of the grey fabric;
[0016] The process parameters are: temperature 80-85°C, time 30-40 min;
[0017] Constraint 2: During the scouring and bleaching process:
[0018] The additives include: LAS as a refining agent, added in an amount of 1.2% owf; EDTA as a complexing agent, added in an amount of 1.2% owf; 98% NaOH by mass, added in an amount of 1-1.5% owf; 27.5% H2O2 by mass, added in an amount of 8% owf;
[0019] The process parameters are: temperature 98-100°C, time 60-70 min;
[0020] Constraint 3: In the re-cooking process:
[0021] The additives include: EDTA as a complexing agent, added in an amount of 1.2% owf; 98% NaOH by mass, added in an amount of 1-1.5% owf; 27.5% H2O2 by mass, added in an amount of 8% owf;
[0022] The process parameters are: temperature 98-100°C, time 60-70 min;
[0023] Constraint 4: During the pickling process:
[0024] The additive is: H2SO4, and the amount added is the amount added when the pH value of the water in the pickling process section is neutral.
[0025] Description: Refining agent LAS is used to remove natural impurities (such as grease, wax) in grey cloth and dirt introduced during processing; chelating agent EDTA is often used in high alkalinity and high temperature bleaching processes to chelate metal ions (such as calcium, magnesium, iron, etc.) in water to prevent them from reacting with other agents; penetrant JFC is used to improve the permeability of the agent so that the agent can act more evenly on the fiber; dispersant sodium polyacrylate can prevent dirt and impurities from re-depositing on the fiber and has excellent dispersing ability.
[0026] Furthermore, in the first adsorption process of process 2, the solid-liquid ratio of the modified carbon balls added to the first wastewater is 40-45 g / L, the adsorption temperature is 25-30° C., and the adsorption time is 10-12 h;
[0027] In the second adsorption process of process 3, the solid-liquid ratio of the modified carbon balls added to the second wastewater is 30-34 g / L, the adsorption temperature is 25-30° C., and the adsorption time is 5-6 h.
[0028] Furthermore, the surface of the modified carbon spheres in process 2 and process 3 is enriched with cationic groups and basic groups, and the iodine value ranges from 1300 to 1330 iodine, and the sub-lan value ranges from 20 to 25 sub-lan, and the preparation steps are:
[0029] SA-1, solid product 1 as carbon sphere precursor prepared based on template method;
[0030] SA-2, carbonization and etching: Under a protective atmosphere, the solid product 1 obtained in SA-1 was carbonized by gradient heating, and then the product was immersed in 20% HF for etching for 48 hours, and finally dried to obtain solid powder 2; the parameters of the gradient heating are: based on room temperature, the temperature is increased to 320°C at a rate of 3-5°C and kept warm for 1.3-1.5 hours, and then the temperature is increased to 850-870°C at a rate of 5-7°C and kept warm for 2-2.5 hours;
[0031] SA-3, pore-forming activation: The solid powder obtained in SA-2 was mixed with KOH and calcined at 800 °C for 2 h under a protective atmosphere to obtain a modified carbon sphere with a concave surface and a bowl shape; n is the rate coefficient and n∈R + , then the amount of solid powder 2 added is 1 g, and the amount of KOH added is n[5,7] mL.
[0032] Description: 3-aminophenol can be solubilized into the hydrophobic core of ditetradecyl dimethyl ammonium bromide micelles. When ammonia and formaldehyde are added, 3-aminophenol and formaldehyde can undergo a condensation reaction at the interface of ditetradecyl dimethyl ammonium bromide. Ammonia can cause the condensation reaction to produce a large amount of hydroxymethyl substitution in a mixed solution of water and ethanol. When the silicate anions hydrolyzed from TEOS meet the positively charged ditetradecyl dimethyl ammonium bromide, the strong electrostatic force causes the two to form a unique open bowl-shaped soft template structure, and finally the modified carbon spheres with an open bowl-shaped structure are prepared by carbonization.
[0033] Furthermore, the steps of preparing the solid product 1 based on the template method in SA-1 are:
[0034] SA-1-1, firstly, deionized water and anhydrous ethanol were added into the reactor, and the mixture was continuously stirred at 40°C and 300-350 r / min, and then 3-aminophenol, ditetradecyl dimethyl ammonium bromide, aqueous ammonia solution, formaldehyde solution and TEOS were added in sequence at time intervals of 15-25 min to obtain system 1;
[0035] Let n be the multiplication coefficient and n∈R + , then the amount of deionized water added is 40 mL, the amount of anhydrous ethanol added is n[40,50] mL, the amount of 3-aminophenol added is n[0.5,0.7] g, the amount of ditetradecyl dimethyl ammonium bromide added is n[0.5,1.2] g, the amount of 25wt.% ammonia solution added is n[0.5,0.8] mL, the amount of 40wt.% formaldehyde solution added is n[0.8,1.2] mL, and the amount of TEOS added is n[2,5] mL;
[0036] SA-1-2. The system 1 prepared in SA-1-1 is reacted at 30°C and 300-350 r / min with continuous stirring for 24 hours, and then subjected to a first drying, cooling, centrifugation, washing and a second drying to obtain a solid powder 1.
[0037] Furthermore, the modified carbon spheres prepared in SA-3 were magnetized, and the steps were as follows: the modified carbon spheres prepared in SA-3 were added to deionized water and continuously stirred, and then Fe3O4 powder was added and hydrothermally treated at 180-200°C for 10-12h, and finally magnetized modified carbon spheres were obtained after magnetic separation, washing and drying; the mass ratio of modified carbon spheres to Fe3O4 powder was 2-2.5:1.
[0038] Note: The main purpose of magnetization treatment is to make the modified carbon balls magnetic, so as to facilitate the subsequent removal and desorption from wastewater. It should be noted that although magnetic modification can greatly improve the recovery rate of modified carbon balls, the Fe3O4 particles occupy the concave bowl-shaped part of the modified carbon balls, which will cause the specific surface area of the modified carbon balls to decrease and weaken the adsorption performance. Therefore, in practical applications, modified carbon balls or magnetic modified carbon balls should be reasonably selected according to the actual situation.
[0039] Furthermore, the preparation steps of the ultrafiltration membrane in the tubular ultrafiltration membrane in process 2 are:
[0040] SB-1, preparing casting solution;
[0041] Polyethylene glycol 300 and graphene oxide are added to hexafluoroisopropanol and ultrasonically stirred for 2 to 3 hours; then PSf polymer particles are added under continuous stirring for 15 to 20 minutes; then the mixture is continuously stirred and heated at 60 to 65°C until the material is melted and evenly distributed, and finally bubbles are discharged at a negative pressure of 120 to 130 Pa and 30 to 33°C to obtain a casting solution;
[0042] Let n be the multiplication coefficient and n∈R + , then the amount of PSf polymer particles added is 20 g, the amount of polyethylene glycol 300 added is n[20,30] mL, the amount of graphene oxide added is n[0.5,0.8] g, and the amount of hexafluoroisopropanol added is n[100,110] mL;
[0043] SB-2. Prepare ultrafiltration membrane using scraping method: scraper speed is 4-5 m / s, scraper height is 100 μm, and the prepared ultrafiltration membrane is stored in 0.5% NaHSO3 solution after washing.
[0044] Description: The present invention uses graphene oxide as a filler to improve the pore structure of the membrane, adjust the pore size and membrane pore morphology of the membrane substrate, generate long strip-shaped pores that penetrate the membrane matrix, and improve the water flux of the membrane; not only that, because of the change in the membrane pore morphology, the mechanical strength of the membrane is also improved.
[0045] Furthermore, the concentration process specifically uses an evaporative crystallizer to remove sulfate from the wastewater by evaporative crystallization.
[0046] Furthermore, the specific steps of the microbial degradation membrane separation coupling process are: adjusting and balancing the pH value, temperature and turbidity of the wastewater generated in the pre-wash section, discharging it into the microbial treatment pool after adjustment to use microorganisms to degrade organic matter in the wastewater, using biofilm to deeply separate organic matter, heavy metal ions and trace pollutants after biological treatment, and finally performing ozone sterilization. The water after ozone sterilization is returned to the pre-wash section for reuse, thereby ensuring the quality of pre-washing while reducing water demand.
[0047] Compared with the existing grey cloth debleaching wastewater treatment method, the beneficial effects of the present invention are:
[0048] (1) The present invention realizes resource recovery of grey cloth debleaching agents and zero wastewater discharge through segmented treatment and resource recovery and reuse; compared with the traditional grey cloth debleaching wastewater treatment process in which wastewater from all process sections is mixed for treatment, the present invention realizes resource recovery of agents by selectively removing interference factors in selected process sections, while also effectively reducing the complexity of wastewater and significantly reducing wastewater treatment costs; in addition, the present invention can also effectively reduce energy loss through heat recovery.
[0049] (2) The present invention also designs modified carbon balls and ultrafiltration membranes for adsorption treatment in view of the pollutant characteristics of grey cloth debleaching wastewater; the modified carbon balls designed by the present invention have an open bowl-shaped structure, thus significantly increasing their surface area and mesoporosity while providing attachment sites and structural support for subsequent magnetic modification; moreover, the ultrafiltration membrane designed by the present invention improves the shape and permeability of the membrane pores, thereby increasing the water flux and mechanical strength of the ultrafiltration membrane. BRIEF DESCRIPTION OF THE DRAWINGS
[0050] Figure 1 It is a process flow chart of the present invention. DETAILED DESCRIPTION
[0051] In order to further illustrate the method adopted by the present invention and the effect achieved, the technical solution of the present invention will be clearly and completely described in combination with experiments below.
[0052] Example 1: This example describes a method for treating grey cloth debleaching wastewater with zero discharge, and aims to illustrate the improvement of the traditional process:
[0053] 1. In the traditional process, the following technical constraints are imposed in the pre-washing, scouring, re-scouring and pickling process sections:
[0054] Constraint 1. In the pre-wash process:
[0055] The additives include: LAS as a refining agent, added in an amount of 0.3% owf; EDTA as a complexing agent, added in an amount of 0.3% owf; JFC as a penetrant, added in an amount of 0.3% owf; sodium polyacrylate as a dispersant, added in an amount of 0.3% owf;
[0056] The process parameters are: temperature 80°C, time 30 min;
[0057] Constraint 2: During the scouring and bleaching process:
[0058] The additives include: LAS as a refining agent, added in an amount of 1.2% owf; EDTA as a complexing agent, added in an amount of 1.2% owf; 98% NaOH by mass, added in an amount of 1% owf; 27.5% H2O2 by mass, added in an amount of 8% owf;
[0059] The process parameters are: temperature 98°C, time 60 min;
[0060] Constraint 3: In the re-cooking process:
[0061] The additives include: EDTA as a complexing agent, added in an amount of 1.2% owf; 98% by mass NaOH, added in an amount of 1% owf; 27.5% by mass H2O2, added in an amount of 8% owf;
[0062] The process parameters are: temperature 98°C, time 60 min;
[0063] Constraint 4: During the pickling process:
[0064] The additive is: H2SO4, and the amount added is the amount added when the pH value of the water in the pickling process section is neutral.
[0065] Constraint 5: Use an evaporative crystallizer to remove sulfate from the wastewater during the concentration process.
[0066] 2. The technical improvements made to each process section are:
[0067] Process 1: Waste heat recovery: A heat exchange process is set up in the boiling, bleaching and re-boiling process section to recover the waste heat, and then transfer the waste heat to the concentration process section;
[0068] Process 2, recovery of boiling and bleaching agent: the wastewater generated by boiling and bleaching and the wastewater generated by the first washing are recorded as the first wastewater, and the first wastewater is treated based on the first adsorption process to obtain the first treated wastewater;
[0069] The first adsorption process is: firstly, the first wastewater is subjected to the first adsorption pretreatment by using tubular ceramic membrane adsorption, and then the first adsorption treatment is performed by using modified carbon ball adsorption and tubular ultrafiltration membrane adsorption;
[0070] Process 3, recovery of reboiling reagent: the wastewater generated by reboiling and the wastewater generated by secondary washing are recorded as the second wastewater, and the second wastewater is treated by the second adsorption process based on modified carbon balls to obtain the second treated wastewater;
[0071] Process 4, wastewater reuse: The wastewater generated in the pre-washing section is treated based on the microbial degradation membrane separation coupling process and returned to the pre-washing section; the first treated wastewater and the second treated wastewater are returned to the pre-washing section after being supplemented with water and chemicals.
[0072] The first adsorption process is: firstly, the first wastewater is subjected to the first adsorption pretreatment by using tubular ceramic membrane adsorption, and then the first adsorption treatment is performed by using modified carbon ball adsorption and tubular ultrafiltration membrane adsorption;
[0073] In the first adsorption process, the solid-liquid ratio of the modified carbon spheres added to the first wastewater was 40 g / L, the adsorption temperature was 25 °C, and the adsorption time was 10 h;
[0074] In the second adsorption process, the solid-liquid ratio of the modified carbon spheres added to the second wastewater was 30 g / L, the adsorption temperature was 25 °C, and the adsorption time was 5 h;
[0075] In the microbial degradation membrane separation coupling process, the specific steps of the microbial degradation membrane separation coupling process are:
[0076] The pH value, temperature and turbidity of the wastewater generated in the pre-wash section are adjusted and balanced, and then discharged into the microbial treatment pool to use microorganisms to degrade organic matter in the wastewater. After biological treatment, biofilm is used to deeply separate organic matter, heavy metal ions and trace pollutants, and finally ozone sterilization is carried out. The water after ozone sterilization is returned to the pre-wash section for reuse, ensuring the quality of pre-washing while reducing water demand.
[0077] 3. The preparation steps of modified carbon spheres are:
[0078] SA-1, preparation of carbon sphere precursor based on template method;
[0079] SA-1-1, firstly, deionized water and anhydrous ethanol were added into the reactor, and the mixture was continuously stirred at 40°C and 300 r / min, and then 3-aminophenol, ditetradecyl dimethyl ammonium bromide, aqueous ammonia solution, formaldehyde solution and TEOS were added in sequence at time intervals of 15 min to obtain system 1;
[0080] The amount of deionized water added was 40 mL, the amount of anhydrous ethanol added was 40 mL, the amount of 3-aminophenol added was 0.5 g, the amount of ditetradecyl dimethyl ammonium bromide added was 0.5 g, the amount of 25 wt.% ammonia solution added was 0.5 mL, the amount of 40 wt.% formaldehyde solution added was 0.8 mL, and the amount of TEOS added was 2 mL;
[0081] SA-1-2, the system 1 prepared in SA-1-1 was reacted at 30°C and 300 r / min under continuous stirring for 24 hours, and then subjected to a first drying, cooling, centrifugation, washing, and a second drying to obtain a solid powder 1;
[0082] SA-2, carbonization and etching;
[0083] Under a protective atmosphere, the solid product 1 prepared in SA-1 was carbonized by gradient heating, and then the product was immersed in 20% HF for etching for 48 hours, and finally dried to obtain solid powder 2;
[0084] The parameters of gradient heating were as follows: based on room temperature, the temperature was increased to 320 °C at a rate of 3 °C and kept at that temperature for 1.3 h, and then the temperature was increased to 850 °C at a rate of 5 °C and kept at that temperature for 2 h;
[0085] SA-3, pore-forming activation;
[0086] The solid powder II prepared in SA-2 was mixed with KOH and calcined at 800°C for 2h under a protective atmosphere to obtain modified carbon spheres with surface depressions and a bowl shape; the amount of solid powder II added was 1g, and the amount of KOH added was 5mL.
[0087] 4. The preparation steps of the ultrafiltration membrane in the tubular ultrafiltration membrane are:
[0088] SB-1, preparing casting solution;
[0089] Polyethylene glycol 300 and graphene oxide were added to hexafluoroisopropanol and ultrasonically stirred for 2 hours; then PSf polymer particles were added under continuous stirring for 15 minutes; then the mixture was continuously stirred and heated at 60°C until the material was melted and evenly distributed, and finally the bubbles were discharged at a negative pressure of 120Pa and 30°C to obtain a casting solution;
[0090] The amount of PSf polymer particles added was 20 g, the amount of polyethylene glycol 300 added was 20 mL, the amount of graphene oxide added was 0.5 g, and the amount of hexafluoroisopropanol added was 100 mL;
[0091] SB-2, the ultrafiltration membrane was prepared by scraping method: the scraper speed was 4 m / s, the scraper height was 100 μm, and the prepared ultrafiltration membrane was stored in 0.5% NaHSO3 solution after washing.
[0092] Example 2: This example is designed based on the scheme in Example 1 and aims to illustrate the scheme under another parameter.
[0093] 1. In the traditional process, the following technical constraints are imposed in the pre-washing, scouring, re-scouring and pickling process sections:
[0094] Constraint 1. In the pre-wash process:
[0095] The additives include: LAS as a refining agent, added in an amount of 0.3% owf; EDTA as a complexing agent, added in an amount of 0.3% owf; JFC as a penetrant, added in an amount of 0.3% owf; sodium polyacrylate as a dispersant, added in an amount of 0.3% owf;
[0096] The process parameters are: temperature 85°C, time 40 min;
[0097] Constraint 2: During the scouring and bleaching process:
[0098] The additives include: LAS as a refining agent, added in an amount of 1.2% owf; EDTA as a complexing agent, added in an amount of 1.2% owf; 98% NaOH by mass, added in an amount of 1.5% owf; 27.5% H2O2 by mass, added in an amount of 8% owf;
[0099] The process parameters are: temperature 100°C, time 70 min;
[0100] Constraint 3: In the re-cooking process:
[0101] The additives include: EDTA as a complexing agent, added in an amount of 1.2% owf; 98% by mass NaOH, added in an amount of 1.5% owf; 27.5% by mass H2O2, added in an amount of 8% owf;
[0102] The process parameters are: temperature 100°C, time 70 min;
[0103] Constraint 4: During the pickling process:
[0104] The additive is: H2SO4, and the amount added is the amount added when the pH value of the water in the pickling process section is neutral.
[0105] Constraint 5: Use an evaporative crystallizer to remove sulfate from the wastewater during the concentration process.
[0106] 2. The technical improvements made to each process section are:
[0107] Process 1: Waste heat recovery: A heat exchange process is set up in the boiling, bleaching and re-boiling process section to recover the waste heat, and then transfer the waste heat to the concentration process section;
[0108] Process 2, recovery of boiling and bleaching agent: the wastewater generated by boiling and bleaching and the wastewater generated by the first washing are recorded as the first wastewater, and the first wastewater is treated based on the first adsorption process to obtain the first treated wastewater;
[0109] The first adsorption process is: firstly, the first wastewater is subjected to the first adsorption pretreatment by using tubular ceramic membrane adsorption, and then the first adsorption treatment is performed by using modified carbon ball adsorption and tubular ultrafiltration membrane adsorption;
[0110] Process 3, recovery of reboiling reagent: the wastewater generated by reboiling and the wastewater generated by secondary washing are recorded as the second wastewater, and the second wastewater is treated by the second adsorption process based on modified carbon balls to obtain the second treated wastewater;
[0111] Process 4, wastewater reuse: The wastewater generated in the pre-washing section is treated based on the microbial degradation membrane separation coupling process and returned to the pre-washing section; the first treated wastewater and the second treated wastewater are returned to the pre-washing section after being supplemented with water and chemicals.
[0112] The first adsorption process is: firstly, the first wastewater is subjected to the first adsorption pretreatment by using tubular ceramic membrane adsorption, and then the first adsorption treatment is performed by using modified carbon ball adsorption and tubular ultrafiltration membrane adsorption;
[0113] In the first adsorption process, the solid-liquid ratio of the modified carbon spheres added to the first wastewater was 40 g / L, the adsorption temperature was 25 °C, and the adsorption time was 10 h;
[0114] In the second adsorption process, the solid-liquid ratio of the modified carbon spheres added to the second wastewater was 30 g / L, the adsorption temperature was 25 °C, and the adsorption time was 5 h;
[0115] In the microbial degradation membrane separation coupling process, the specific steps of the microbial degradation membrane separation coupling process are:
[0116] The pH value, temperature and turbidity of the wastewater generated in the pre-wash section are adjusted and balanced, and then discharged into the microbial treatment pool to use microorganisms to degrade organic matter in the wastewater. After biological treatment, biofilm is used to deeply separate organic matter, heavy metal ions and trace pollutants, and finally ozone sterilization is carried out. The water after ozone sterilization is returned to the pre-wash section for reuse, ensuring the quality of pre-washing while reducing water demand.
[0117] 3. The preparation steps of modified carbon spheres are:
[0118] SA-1, preparation of carbon sphere precursor based on template method;
[0119] SA-1-1, firstly, deionized water and anhydrous ethanol were added into the reactor, and the mixture was continuously stirred at 40°C and 350 r / min, and then 3-aminophenol, ditetradecyl dimethyl ammonium bromide, aqueous ammonia solution, formaldehyde solution and TEOS were added in sequence at a time interval of 25 min to obtain system 1;
[0120] The amount of deionized water added is 40 mL, the amount of anhydrous ethanol added is 50 mL, the amount of 3-aminophenol added is 0.5 g, the amount of ditetradecyl dimethyl ammonium bromide added is 1.2 g, the amount of 25 wt.% ammonia solution added is 0.8 mL, the amount of 40 wt.% formaldehyde solution added is 1.2 mL, and the amount of TEOS added is 5 mL;
[0121] SA-1-2, the system 1 prepared in S2-1-1 was reacted at 30°C and 350 r / min with continuous stirring for 24 hours, and then subjected to first drying, cooling, centrifugation, washing and second drying to obtain a solid powder 1;
[0122] SA-2, carbonization and etching;
[0123] Under a protective atmosphere, the solid product 1 prepared in SA-1 was carbonized by gradient heating, and then the product was immersed in 20% HF for etching for 48 hours, and finally dried to obtain solid powder 2;
[0124] The parameters of gradient heating were as follows: based on room temperature, the temperature was increased to 320°C at a rate of 5°C and kept at that temperature for 1.5 h, and then the temperature was increased to 870°C at a rate of 7°C and kept at that temperature for 2.5 h;
[0125] SA-3, pore-forming activation;
[0126] The solid powder II prepared in SA-2 was mixed with KOH and calcined at 800°C for 2 h under a protective atmosphere to obtain a modified carbon sphere with a concave surface and a bowl shape; the amount of solid powder II added was 1 g, and the amount of KOH added was 7 mL;
[0127] 4. The preparation steps of the ultrafiltration membrane in the tubular ultrafiltration membrane are:
[0128] SB-1, preparing casting solution;
[0129] Polyethylene glycol 300 and graphene oxide were added to hexafluoroisopropanol and ultrasonically stirred for 3 hours; then PSf polymer particles were added under continuous stirring for 20 minutes; then the mixture was continuously stirred and heated at 65°C until the material was melted and evenly distributed, and finally the bubbles were discharged at a negative pressure of 130Pa and 33°C to obtain a casting solution;
[0130] The amount of PSf polymer particles added was 20 g, the amount of polyethylene glycol 300 added was 30 mL, the amount of graphene oxide added was 0.8 g, and the amount of hexafluoroisopropanol added was 110 mL;
[0131] SB-2, ultrafiltration membrane was prepared by scraping method: the scraper speed was 5 m / s, the scraper height was 100 μm, and the prepared ultrafiltration membrane was stored in 0.5% NaHSO3 solution after washing.
[0132] Example 3: This example is designed based on the scheme in Example 1, and aims to illustrate a method for treating grey cloth debleaching wastewater with low energy consumption and carbon emission reduction under another design. Except for the following contents, the rest are the same as Example 1:
[0133] The modified carbon spheres prepared in SA-3 were magnetized, and the steps were as follows: 20 g of the modified carbon spheres prepared in SA-3 were added to 50 mL of deionized water and stirred continuously, and then 10 g of Fe3O4 powder was added and hydrothermally treated at 200°C for 12 h, and finally the magnetized modified carbon spheres were obtained after magnetic separation, washing and drying.
[0134] Experimental Example 1: The purpose of this experimental example is to compare the performance differences between the modified carbon ball camera designed by the present invention and different types of activated carbon.
[0135] The wastewater sample used in this experimental example has a water content of 100 mL, a COD concentration of 13000 mg / L, a phenol concentration of 610 mg / L, and a chromaticity of 13 times.
[0136] Because iodine value and sub-lan value are important indicators affecting the adsorption performance of activated carbon, and a higher sub-lan value is conducive to the adsorption and removal of COD and phenol by activated carbon, the following control experiment is designed:
[0137] Table 1 Comparison of iodine values of different types of activated carbon
[0138]
[0139] Table 2 Comparison of the Alan values of different types of activated carbon
[0140]
[0141] It can be seen from the data in Table 1 and Table 2 that compared with traditional activated carbon, the modified carbon spheres designed by the present invention have a large number of cationic groups and alkaline groups on the surface, remove anionic groups and acidic groups, and have a developed mesoporous structure (their iodine value and Alan value are both higher than the average standard). Therefore, the modified carbon spheres designed by the present invention have excellent adsorption and removal effects on COD and phenol (there is a certain positive correlation between wastewater chromaticity and phenol concentration;).
[0142] Experimental Example 2: This experimental example designed a re-bleaching experiment based on the scheme in Example 1, the content is as follows:
[0143] Table 3 Rebleaching experiment
[0144]
[0145] From the data in Table 3, we can see that compared with the high energy consumption and high difficulty of traditional sewage treatment, which is to discharge the wastewater from each process section in a centralized manner, the advantages of sewage treatment and resource utilization under the entropy principle in the form of segmented treatment and recycling to the process section proposed in this method are as follows:
[0146] Traditional centralized treatment methods often require a lot of energy to treat highly mixed wastewater, which not only consumes a lot of energy, but also has high difficulty in treatment due to the complexity of different components in the wastewater, and the system entropy increases. The present invention reduces the complexity of wastewater mixing by treating and reusing wastewater in sections, combining waste heat recovery and selective removal of key pollutants, and realizes a more efficient and environmentally friendly sewage treatment and resource utilization method (such as treating high-pectin and high-COD wastewater separately, which can more effectively remove specific pollutants, reduce unnecessary energy consumption, and reduce system entropy increase); by treating wastewater separately in each process section, the direction of pollutants can be better controlled to avoid pollutants from spreading throughout the system (such as recycling low-pectin and low-chroma wastewater to the pre-wash section, which not only reduces the use of fresh water and some reagents, but also effectively controls the recycling of pollutants, which helps to reduce system entropy increase); in traditional centralized treatment methods, wastewater will cause a lot of energy loss during long-term and long-distance transmission, but the present invention does not have this problem.
Claims
1. A method for treating grey cloth de-bleaching wastewater with zero discharge, comprising the steps of: degreasing and bleaching the grey cloth by pre-washing, boiling and bleaching, primary washing, repeated boiling, secondary washing, pickling and concentration, characterized in that: At The following process sections are added to the above process flow: Process 1, waste heat recovery: a heat exchange process is set in the boiling, bleaching and re-boiling process section to recover the waste heat, and then the waste heat is transferred to the concentration process section; Process 2, recovery of bleaching agent: the wastewater generated by the bleaching and the wastewater generated by the first washing is recorded as the first wastewater, and the first wastewater is treated based on the first adsorption process to obtain the first treated wastewater; The first adsorption process is: firstly, using tubular ceramic membrane adsorption to perform first adsorption pretreatment on the first wastewater, and then using modified carbon ball adsorption and tubular ultrafiltration membrane adsorption to perform first adsorption treatment; Process 3, recovery of reboiling reagent: the wastewater generated by the reboiling and the wastewater generated by the secondary washing is recorded as the second wastewater, and the second wastewater is treated by the second adsorption process based on modified carbon balls to obtain the second treated wastewater; Process 4: Wastewater reuse: The wastewater generated in the pre-washing section is treated based on the microbial degradation membrane separation coupling process and returned to the pre-washing section; The first treated wastewater and the second treated wastewater are returned to the pre-washing section after being supplemented with water and chemicals.
2. A zero-discharge treatment method for grey cloth debleaching wastewater according to claim 1, characterized in that: The following technical constraints are imposed on the pre-washing, scouring, bleaching, re-scouring and pickling process sections: Constraint 1. In the pre-wash process: The additives include: LAS as a refining agent, added in an amount of 0.3% owf; EDTA as a complexing agent, added in an amount of 0.3% owf; JFC as a penetrant, added in an amount of 0.3% owf; sodium polyacrylate as a dispersant, added in an amount of 0.3% owf; The process parameters are: temperature 80-85°C, time 30-40 min; Constraint 2: During the scouring and bleaching process: The additives include: LAS as a refining agent, added in an amount of 1.2% owf; EDTA as a complexing agent, added in an amount of 1.2% owf; 98% NaOH by mass, added in an amount of 1-1.5% owf; 27.5% H2O2 by mass, added in an amount of 8% owf; The process parameters are: temperature 98-100°C, time 60-70 min; Constraint 3: In the re-cooking process: The additives include: EDTA as a complexing agent, added in an amount of 1.2% owf; 98% NaOH by mass, added in an amount of 1-1.5% owf; 27.5% H2O2 by mass, added in an amount of 8% owf; The process parameters are: temperature 98-100°C, time 60-70 min; Constraint 4: During the pickling process: The additive is: H2SO4, and the amount added is the amount added when the pH value of the water in the pickling process section is neutral.
3. A method for zero-discharge treatment of grey cloth debleaching wastewater according to claim 1, characterized in that: In the first adsorption process of process 2, the solid-liquid ratio of the modified carbon balls added to the first wastewater is 40-45 g / L, the adsorption temperature is 25-30° C., and the adsorption time is 10-12 h; In the second adsorption process of process 3, the solid-liquid ratio of the modified carbon balls added to the second wastewater is 30-34 g / L, the adsorption temperature is 25-30° C., and the adsorption time is 5-6 h.
4. A zero-discharge treatment method for grey cloth debleaching wastewater according to claim 1, characterized in that: The surfaces of the modified carbon spheres in process 2 and process 3 are enriched with cationic groups and basic groups, and the iodine value ranges from 1300 to 1330 iodine, and the sub-lane value ranges from 20 to 25 sub-lane.
5. A method for zero-discharge treatment of grey cloth debleaching wastewater according to claim 1, characterized in that: The preparation steps of the ultrafiltration membrane in the tubular ultrafiltration membrane in process 2 are: SB-1, preparation of casting solution: polyethylene glycol 300 and graphene oxide are added to hexafluoroisopropanol, and ultrasonic stirring is performed for 2 to 3 hours; then PSf polymer particles are added under continuous stirring for 15 to 20 minutes; then stirring and heating are continued at 60 to 65° C. until the materials are melted and evenly distributed, and finally bubbles are discharged at a negative pressure of 120 to 130 Pa and 30 to 33° C. to obtain a casting solution; Let n be the multiplication coefficient and n∈R + , the amount of PSf polymer particles added is 20 g, the amount of polyethylene glycol 300 added is n[20,30] mL, the amount of graphene oxide added is n[0.5,0.8] g, and the amount of hexafluoroisopropanol added is n[100,110] mL; SB-2. Prepare ultrafiltration membrane using scraping method: scraper speed is 4-5 m / s, scraper height is 100 μm, and the prepared ultrafiltration membrane is stored in 0.5% NaHSO3 solution after washing.
Citation Information
Patent Citations
Method for recycling textile, printing and dyeing wastewater
CN101514057A
Processing technique of roving for linen knitting by scouring and bleaching with sodium chlorite and hydrogen peroxide
CN106521924A
Fabric dyeing wastewater treatment method
CN108558140A
Hydrogen peroxide kiering process for linen roving
CN1087959A
Preparation method and application of nitrogen-doped carbon-loaded heteropolyacid nano composite material
CN113731453A