Rapid lossless non-contact measuring device and measuring method for surface strain of silicon material

Through femtosecond laser technology and data processing algorithms, fast lossless non-contact measurement of surface strain of silicon materials is achieved, solving the problems of speckle dependence and low frame rate in traditional methods, and achieving efficient and accurate strain detection.

CN118913122AActive Publication Date: 2024-11-08WUHAN UNIV

Patent Information

Application Number
CN202410898532.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-05
Publication Date
2024-11-08
Estimated Expiration
2044-07-05

AI Technical Summary

Technical Problem

Traditional strain measurement methods rely on speckle production quality and low frame rate, making it difficult to meet the demand for fast lossless non-contact measurement of surface strain on silicon materials.

Method used

Using femtosecond laser, time domain stretching component, optical signal amplification component, beam splitter, spatial dispersion component, microscope, high-speed photodetector and data processing device, the near-infrared/near-ultraviolet femtosecond laser imaging is achieved without loss Non-contact measurement, calculate strain distribution.

Benefits of technology

The surface strain of silicon material is rapidly, lossless, and speckle-free, and the frame rate reaches MHz level, reducing costs and improving measurement efficiency and accuracy.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118913122A_ABST
    Figure CN118913122A_ABST
Patent Text Reader

Abstract

The invention provides a silicon material surface strain rapid lossless non-contact measurement device and method, and the device comprises a femtosecond laser which is used for generating femtosecond laser pulses; the time domain stretching assembly is arranged on an emergent light path of the femtosecond laser; the optical signal amplification assembly is arranged on an emergent light path of the time domain stretching assembly; the beam splitter is positioned on an emergent light path of the optical signal amplification component and is used for splitting the femtosecond laser pulse into a test beam and a reference beam with a specific power ratio; the spatial dispersion assembly is arranged on an emergent light path of the test light beam of the beam splitter; the microscope objective is arranged on an emergent light path of the spatial dispersion assembly; the high-speed photoelectric detector is positioned on an emergent light path of the reference light beam of the beam splitter; the high-speed oscilloscope is electrically connected with the high-speed photoelectric detector; and the data processing device is electrically connected with the high-speed oscilloscope. The method is used for solving the problems of strong dependence on speckles and low detection frame number in the prior art.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of optical mechanics and deformation measurement, and in particular relates to a measurement method of a silicon material surface strain rapid non-destructive non-contact measurement device. Background Art

[0002] At present, the chip size has entered the nano era. Due to the reduction of chip packaging volume and the increase of chip overall power consumption, the heat generated by the chip is easy to accumulate, causing the chip temperature to rise. The chip substrate is often made of composite materials. Different components have different thermal expansion coefficients. Under temperature changes, thermal mismatch will occur inside, resulting in stress and strain, causing warping deformation, and even causing solder joint failure, chip cracking and delamination. Therefore, the detection of chip strain is receiving more and more attention.

[0003] Due to the small size of the chip and the microscopic measurement, the traditional contact strain measurement method based on strain gauges or extensometers is difficult to meet the needs of this field. At present, Digital Image Correlation (DIC) is a widely used non-contact measurement method in this field. This method first uses spraying, flooding, etching and other methods to make scattered spots on the surface of the sample, and then uses an optical microscope (OM) or a scanning electron microscope (SEM) to take the speckle image before and after deformation. By comparing the position changes of the scattered spots before and after deformation, the strain field distribution of the sample is analyzed and generated.

[0004] However, traditional strain measurement methods have two major limitations: First, traditional DIC technology is based on the production of speckles on the surface of the sample for analysis. The strain distribution and changes on the sample surface are calculated using an algorithm through the speckle patterns before and after deformation. The measurement quality depends largely on the quality of the speckle production. Second, traditional DIC technology requires expensive high-speed cameras to achieve high-frame-rate high-speed measurements. The frame rate is limited by the high-speed camera, with the maximum frame rate being in the order of 10,000 frames per second, and is constrained by the field of view size and resolution. Summary of the invention

[0005] One object of the present invention is to provide a device for fast, non-destructive and non-contact measurement of silicon surface strain in view of the shortcomings of the prior art, so as to solve the problems of the prior art's strong dependence on speckle and low detection frame number.

[0006] In order to solve the above technical problems, the present invention adopts the following technical solutions:

[0007] A device for fast, non-destructive and non-contact measurement of silicon surface strain, comprising:

[0008] A femtosecond laser, used to generate femtosecond laser pulses sufficient to reflect images on the surface of the sample to be tested without damaging the sample to be tested;

[0009] A time domain stretching component, which is connected to the near-infrared / near-ultraviolet femtosecond laser and is used to perform time domain stretching on the femtosecond laser pulse;

[0010] An optical signal amplifying component, which is connected to the time domain stretching component and is used to compensate the power of the femtosecond laser pulse stretched by the time domain stretching component;

[0011] A beam splitter is located on the outgoing optical path of the optical signal amplification component and is used to split the femtosecond laser pulse into a test beam and a reference beam with a specific power ratio, wherein the test beam returns to the beam splitter along the optical path after being reflected by the sample to be tested, and interferes with the reference beam to form an interference pulse with stable power;

[0012] A spatial dispersion component is arranged on the outgoing optical path of the test beam of the beam splitter, and is used to spatially disperse the outgoing pulse into a spatial pulse, and irradiate the spatial pulse along the opposite direction of the original optical path to the spatial dispersion component after being reflected by the sample to be tested, and the spatial dispersion component re-converges the spatial pulse to obtain a point light;

[0013] A microscope objective lens, which is arranged on the outgoing light path of the spatial dispersion component and is used to focus the spatial pulse onto the sample to be measured;

[0014] A high-speed photodetector, which is located on the outgoing optical path of the reference beam of the beam splitter and is used to convert the interference pulse optical signal into an analog electrical signal;

[0015] A high-speed oscilloscope, which is electrically connected to the high-speed photodetector and is used to collect and sample analog electrical signals;

[0016] The data processing device is electrically connected to the high-speed oscilloscope and is used to process and calculate the analog electrical signals collected and sampled to obtain the strain on the surface of the sample to be tested.

[0017] Furthermore, the femtosecond laser is a near-infrared femtosecond laser or a near-ultraviolet femtosecond laser.

[0018] Furthermore, it also includes an optical power meter. Before testing, the optical power meter is placed between the microscope objective lens and the sample to be tested. During testing, the optical power meter is moved out of the light path.

[0019] Furthermore, it also includes a lens assembly, which is arranged between the spatial dispersion assembly and the microscope objective lens, wherein the first lens assembly is used to adjust the size of the pulse spot and the angle of the pulse incident on the microscope objective lens.

[0020] Furthermore, it also includes a first collimator and a second collimator, wherein the first collimator is located between the optical signal amplifying component and the beam splitter, and is used to make the pulse amplified by the optical signal amplifying component incident on the beam splitter in the form of a specific angle and spatial light; the second collimator is located between the reference beam exit side of the beam splitter and the high-speed photodetector, and is used to couple the interference pulse into the optical path.

[0021] Furthermore, the spatial dispersion component includes an acousto-optic deflector and a diffraction grating which are sequentially arranged on the output light path of the optical signal amplification component, the acousto-optic deflector is used to change the incident position and direction of the pulse incident to the diffraction grating, and the diffraction grating is used to disperse the femtosecond laser pulse into a one-dimensional spatial pulse.

[0022] Another object of the present invention is to provide a method for measuring the surface strain of a silicon material according to the above-mentioned rapid non-destructive non-contact measuring device, comprising the following steps:

[0023] Step 1, clean the sample to be tested and fix it on the outgoing light path of the microscope objective lens;

[0024] Step 2, starting the femtosecond laser to generate a femtosecond laser pulse that is sufficient to penetrate the sample to be tested for imaging without damaging the sample to be tested;

[0025] Step 3, the time domain stretching component performs time domain stretching on the femtosecond pulse, and then amplifies it through the optical signal amplification component, and then generates a test beam and a reference beam after passing through a beam splitter, wherein the test beam is incident on the spatial dispersion component and then focused onto the sample to be tested through a microscope objective lens;

[0026] Step 4: The spatial pulse reflected by the sample to be tested interferes with the reference beam generated by the spatial dispersion component and the beam splitter to form an interference pulse. The high-speed photodetector detects the interference pulse and converts it into an analog signal. The high-speed oscilloscope collects the sampled analog signal and transmits it to the data processing device. The data processing device restores the test pulse signal distribution image sequence reflected by the sample to be tested based on the analog electrical signal sampled by the high-speed oscilloscope; and obtains the change in the contour boundary of the light intensity distribution image of the sample to be tested before and after the strain occurs based on the test pulse signal distribution image sequence, calculates the boundary strain, and obtains the strain on the sample surface through interpolation calculation.

[0027] Furthermore, the method for obtaining the test pulse signal distribution image sequence includes:

[0028] The interference pulse signal is analyzed and reconstructed by a data processing device to obtain the distribution of the test pulse reflected on the sample surface, and a two-dimensional light intensity distribution image sequence reflected on the sample surface is constructed, whose frame rate is equal to the repetition frequency of the near-infrared / near-ultraviolet femtosecond laser, from the sampled light pulse signal I(x) to the light intensity signal I s The conversion formula of (x) is as follows:

[0029]

[0030] Among them, I R (x) is the reference pulse intensity, T is the Hilbert transformed component of the filtered high-frequency component of the sampled optical pulse signal I(x), and re(T) and im(T) are the real part and imaginary part of T, respectively.

[0031] Furthermore, the method for the data processing device to calculate the surface strain of the sample to be tested according to the test pulse signal distribution image sequence includes:

[0032] The non-local mean algorithm is used to filter the test pulse signal distribution image sequence, and then the binary image is extracted from the filtered light intensity distribution map sequence. The eigenvalue and eigenvector method is used to track the distribution of each contour area of ​​the sample before and after strain. The position coordinate matrix A of each area at the boundary of the sample to be tested is expressed as: A = QΛQ, where Q is the matrix of eigenvectors and Λ is the matrix of eigenvalues;

[0033] The deformation of each region before and after strain is expressed as:

[0034]

[0035] Where: e i is a unit vector; and Represents the transformation matrix of each contour area before and after strain; E j is the characteristic value of the region;

[0036] The deformation tensor It is expressed as:

[0037]

[0038] Strain in each region Calculated by the following formula:

[0039]

[0040] Furthermore, the method of filtering the test pulse signal distribution image sequence using the non-local means algorithm includes:

[0041]

[0042] Where NL[v](i) is the filtered image of pixel i, v(j) is the unfiltered original image; I is the neighborhood of pixel i; w(i,j) represents the similarity between pixels i and j, and its value is determined by the square of the Euclidean distance between the search windows:

[0043]

[0044] in,

[0045] Where h is the smoothing parameter; is the attenuation function of the weighted Euclidean distance between pixel i and pixel j, a is the standard deviation of the Gaussian kernel; Z i is the normalization coefficient.

[0046] Compared with the prior art, the present invention has the following beneficial effects: the present invention uses near-infrared / near-ultraviolet light to perform ultrafast laser imaging on the sample to be tested, and the imaging frame rate is equivalent to the pulse repetition frequency of the laser, which can reach about MHz, so that the strain on the surface of the silicon material can be quickly measured; in addition, due to the high reflectivity of near-infrared / near-ultraviolet light to silicon materials, the image sequence formed by the method of the present invention contains the structural information of the surface of the chip or device to be tested, and after the image sequence is processed by a data processing device, the strain change on the surface of the chip or device to be tested can be accurately reflected, so that the obtained strain information on the surface of the silicon material is more accurate;

[0047] Compared with the non-contact traditional DIC technology, the present invention overcomes the difficulty of DIC technology requiring the preparation of speckles, and uses images derived from the structural characteristics of the sample chip itself for calculation and analysis, without the need to additionally produce speckles on the sample, thereby avoiding damage to the sample surface; by controlling the laser power, the generated laser of a specific wavelength can have a specific power after amplification, so that the laser does not damage the sample while passing through the sample and forming the image required for the test, thereby realizing non-contact non-destructive testing;

[0048] In addition, the present invention does not require expensive high-speed cameras and is not constrained by frame rate, field of view size and resolution. It only requires commonly used near-infrared / near-ultraviolet femtosecond lasers to quickly measure the strain changes inside the chip or device to be tested, which greatly reduces costs and improves measurement efficiency. BRIEF DESCRIPTION OF THE DRAWINGS

[0049] Figure 1 This is a schematic structural diagram of a device for rapid, non-destructive, and non-contact measurement of silicon material surface strain provided in Example 1 of the present invention. DETAILED DESCRIPTION

[0050] The technical solutions in the embodiments of the present invention will be described clearly and completely below in combination with the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0051] It should be noted that, in the absence of conflict, the embodiments of the present invention and the features in the embodiments may be combined with each other.

[0052] The present invention will be further described below in conjunction with specific embodiments, but the present invention is not limited thereto.

[0053] Embodiment 1:

[0054] Embodiment 1 provides a device for ultrafast non-destructive and non-contact measurement of silicon surface strain, such as Figure 1 As shown, it includes: a femtosecond laser 101, a time domain stretching component, an optical signal amplifying component, a beam splitter, a spatial dispersion component, a microscopic object, a high-speed photodetector, a high-speed oscilloscope and a data processing device. In this embodiment, the femtosecond laser 101 is one of a near-infrared femtosecond laser or a near-ultraviolet femtosecond laser, and both the near-infrared femtosecond laser and the near-ultraviolet femtosecond laser can be reflected on the surface of the silicon material. The time domain stretching component is a single-mode optical fiber 102, which is arranged on the output optical path of the near-infrared / near-ultraviolet femtosecond laser 101; the optical signal amplifying component is an erbium-doped fiber amplifier 103, which is arranged on the output optical path of the single-mode optical fiber 102. The beam splitter 105 is located on the output optical path of the optical signal amplifying component, and is used to divide the femtosecond laser pulse into a test beam (first direction) and a reference beam (second direction) with a specific power ratio; after being reflected by the sample to be tested, the test beam returns to the beam splitter 105 along the optical path, interferes with the reference beam, and forms an interference pulse with stable power. In order to allow the pulses amplified by the erbium-doped fiber amplifier 103 to be incident on the beam splitter 105 at a specific angle in the form of spatial light, a first collimator 104 is provided on the optical path between the erbium-doped fiber amplifier 103 and the beam splitter.

[0055] The spatial dispersion component includes an acousto-optic deflector 106 and a diffraction grating 107 which are sequentially arranged on the outgoing light path of the beam splitter 105, wherein the acousto-optic deflector 106 is used to change the incident position and direction of the near-infrared / near-ultraviolet femtosecond laser pulse incident on the diffraction grating 107, and the diffraction grating 107 is used to disperse the near-infrared / near-ultraviolet femtosecond laser pulse into a one-dimensional spatial pulse. In this embodiment, a microscope objective 110 is arranged on the outgoing light path of the acousto-optic deflector 106, which is used to focus the spatial pulse on the chip or device to be tested. In order to ensure that the pulse generated by the near-infrared / near-ultraviolet femtosecond laser 101 has a first power and a first wavelength after being amplified by the erbium-doped fiber amplifier 103, the first power is sufficient to reflect the image on the surface of the sample to be tested without damaging the object to be tested, and the first wavelength is sufficient to form an image with sufficient quality after penetrating the silicon and other polymer components of the sample to be tested, before the test, an optical power meter 111 is set between the microscope objective 110 and the sample to be tested, and the optical power meter 111 is moved out of the light path after the test starts.

[0056] In addition, a lens assembly is provided, which is sequentially provided with a first plano-convex lens 108 and a second plano-convex lens 109 on the optical path between the first diffraction grating 107 and the microscope objective 110, wherein the first lens assembly is used to adjust the size of the pulse spot and the angle of the pulse incident on the microscope objective.

[0057] The high-speed photodetector 113 is arranged on the outgoing optical path of the reference beam (second direction side) split by the beam splitter, and is used to convert the interference pulse signal into an analog signal. In this embodiment, the high-speed photodetector 113 selects the MHz-level and above high-speed free-space photodetector 113. In order to facilitate coupling the interference pulse into the optical path for detection by the high-speed photodetector 113, a second collimator 112 is arranged between the beam splitter 105 and the high-speed photodetector 113. A high-speed oscilloscope 114 for collecting sampled analog electrical signals is electrically connected downstream of the high-speed photodetector 113. In this embodiment, the high-speed oscilloscope 114 selects a MHz-level and above high-speed oscilloscope. The data processing device 115 is electrically connected to the high-speed oscilloscope 114, and is used to restore the test pulse signal distribution image sequence reflected by the sample to be tested according to the sampled analog electrical signal; and obtain the change of the contour boundary of the light intensity distribution image before and after the strain of the sample to be tested according to the test pulse signal distribution image sequence, calculate the boundary strain, and obtain the strain of the sample surface by interpolation calculation. In this embodiment, the data processing device 115 is a computer or other equipment capable of performing data processing and calculation.

[0058] Embodiment 2:

[0059] Embodiment 2 provides an ultrafast, non-destructive, and non-contact method for measuring the surface strain of a silicon material, which is implemented using the device provided in Embodiment 1 and mainly includes the following steps:

[0060] Step 1: Use chemical detergent and deionized water to clean and dry the sample to be tested, and fix it on the optical path of the microscope objective lens 110;

[0061] Step 2: Before the test, the optical power meter 111 is set on the optical path between the microscope objective 110 and the sample to be tested, and the near-infrared / near-ultraviolet femtosecond laser 101 and the erbium-doped fiber amplifier 103 are adjusted so that the femtosecond laser pulse generated by the near-infrared / near-ultraviolet femtosecond laser 101 has a first power and a first wavelength after being amplified by the erbium-doped fiber amplifier 103, and the first power is sufficient to penetrate the sample to be tested without damaging the sample to be tested, and the first wavelength is sufficient to form an image with sufficient quality after penetrating the silicon and other polymer components of the sample to be tested; after the test starts, the optical power meter 111 is moved out of the optical path, and the pulse power and wavelength emitted and amplified by the near-infrared / near-ultraviolet femtosecond laser 101 and the erbium-doped fiber amplifier 103 are kept unchanged;

[0062] Step 3, time-domain stretching is performed on the near-infrared / near-ultraviolet femtosecond laser pulse through the single-mode optical fiber 102, and the pulse after time-domain stretching is incident on the beam splitter 105 at a specific angle and in the form of spatial light through the first collimator 104, and the beam splitter 105 splits the femtosecond laser pulse into a test beam (first direction) and a reference beam (second direction) with a specific power ratio;

[0063] Step 4, the test beam is incident on the first acousto-optic deflector 106, and the crystal refractive properties inside the acousto-optic deflector are changed by controlling the acoustic wave driving frequency, so as to change the incident position and angle of the femtosecond laser on the first diffraction grating 107. The spatial light incident on the first diffraction grating 107 at different positions and angles is dispersed into one-dimensional spatial pulses, and then focused on different positions on the sample to be tested through the first plano-convex lens 108, the second plano-convex lens 109, and the microscope objective 110, so as to realize a large-scale two-dimensional scanning of the one-dimensional femtosecond laser on the object to be tested;

[0064] Step 5, after the pulse reflected from the surface of the object to be measured is reflected and irradiated onto the microscope objective 110, the second plano-convex lens 109, and the first plano-convex lens 108 in the opposite direction of the original optical path, it passes through the first diffraction grating 107 and the first acousto-optic deflector 106 at an angle opposite to that of the incident pulse, is re-shaped into a one-dimensional pulse, and interferes with the reference pulse separated from it through the beam splitter, and is coupled to the MHz-level and above high-speed photodetector 113 through the second collimator 112;

[0065] Step 6: The interference pulse is converted into an analog electrical signal after passing through the high-speed photodetector 113, and then sampled to the computer 115 through the high-speed oscilloscope 114. The computer 115 analyzes and reconstructs the analog signal sampled by the high-speed oscilloscope 114 to obtain a distribution image sequence of the test pulse signal reflected by the sample to be tested, and its frame rate is equal to the repetition frequency of the near-infrared / near-ultraviolet femtosecond laser, from the sampled optical pulse signal I(x) to the light intensity signal I s The conversion formula of (x) is as follows:

[0066]

[0067] Among them, I R (x) is the reference pulse intensity, T is the Hilbert transformed component of the filtered high-frequency component of the sampled optical pulse signal I(x), and re(T) and im(T) are the real part and imaginary part of T, respectively.

[0068] For the test pulse signal distribution image sequence obtained by the above formula, in order to reduce the influence of test noise such as photodetector noise and oscilloscope measurement noise on the measurement results, the non-local mean algorithm is used for filtering to clarify the boundaries of each contour area in the image. The calculation formula of the algorithm is:

[0069] NL[v](i)=∑ j∈I v(j)w(i,j) (2)

[0070] Where NL[v](i) is the filtered image of pixel i, v(j) is the original image without filtering; I is the neighborhood of pixel i; w(i,j) represents the similarity between pixels i and j, and its value is determined by the square of the Euclidean distance between the search windows:

[0071]

[0072] in,

[0073]

[0074] In the formula, h is a smoothing parameter that controls the attenuation degree of the Gaussian function, and its specific value is based on the image noise level; is the attenuation function of the weighted Euclidean distance between pixel i and pixel j, a is the standard deviation of the Gaussian kernel; Z i is the normalization coefficient.

[0075] After the above filtering, the binary image is extracted, and the eigenvalue and eigenvector method is used to track the contour area distribution of the object to be measured before and after strain. The position coordinate matrix A of each area to the sample boundary can be expressed as A=QΛQ, where Q is the matrix of eigenvectors and Λ is the matrix of eigenvalues. The deformation of each area before and after strain can be expressed as:

[0076]

[0077] Where: e i is a unit vector; and Represent the transformation matrix of the region before and after strain respectively; E j is the eigenvalue of the region. Then the deformation tensor It can be expressed as:

[0078]

[0079] Strain in each region It can be calculated by the following formula:

[0080]

[0081] Get the strain of each area Afterwards, the node matrix is ​​constructed with the strains in each area and imported into MATLAB to call the two-dimensional spline interpolation toolbox. The strain distribution at various locations on the surface of the measured sample can be obtained through interpolation calculation.

[0082] Example 2 utilizes the characteristics of near-infrared / near-ultraviolet femtosecond laser pulse waves at the femtosecond level and high reflectivity on the surface of silicon materials, and uses diffraction gratings and acousto-optic deflectors to disperse spatial pulses to form spatial pulses that scan the surface of the object to be measured in two dimensions, thereby ultra-fast acquisition of the light intensity distribution of the pulse after reflection from the surface of the object to be measured, and the strain distribution on the surface of the object to be measured can be calculated by combining the algorithm. The entire measurement process is contactless, and can achieve ultra-fast, non-destructive, non-contact strain measurement of the observed object, with a sampling frequency of up to 10 6 Hz and above, it can effectively observe the transient strain distribution on the surface of electronic chips or devices.

[0083] The above are only preferred embodiments of the present invention, and are not intended to limit the implementation methods and protection scope of the present invention. Those skilled in the art should be aware that all solutions obtained by equivalent substitutions and obvious changes made using the contents of the specification of the present invention should be included in the protection scope of the present invention.

Claims

1. A device for fast, non-destructive and non-contact measurement of silicon surface strain, characterized in that: include: A femtosecond laser, used to generate femtosecond laser pulses sufficient to reflect images on the surface of the sample to be tested without damaging the sample to be tested; A time domain stretching component is arranged on the output optical path of the near-infrared / near-ultraviolet femtosecond laser and is used for time domain stretching of the femtosecond laser pulse; An optical signal amplifying component, which is arranged in connection with the outgoing optical path of the time domain stretching component and is used for power compensation of the femtosecond laser pulse stretched by the time domain stretching component; A beam splitter is located on the outgoing optical path of the optical signal amplification component and is used to split the femtosecond laser pulse into a test beam and a reference beam with a specific power ratio, wherein the test beam returns to the beam splitter along the optical path after being reflected by the sample to be tested, and interferes with the reference beam to form an interference pulse with stable power; A spatial dispersion component is arranged on the outgoing optical path of the test beam of the beam splitter, and is used to spatially disperse the outgoing pulse into a spatial pulse, and irradiate the spatial pulse along the opposite direction of the original optical path to the spatial dispersion component after being reflected by the sample to be tested, and the spatial dispersion component re-converges the spatial pulse to obtain a point light; A microscope objective lens, which is arranged on the outgoing light path of the spatial dispersion component and is used to focus the spatial pulse onto the sample to be measured; A high-speed photodetector, which is located on the outgoing optical path of the reference beam of the beam splitter and is used to convert the interference pulse optical signal into an analog electrical signal; A high-speed oscilloscope, which is electrically connected to the high-speed photodetector and is used to collect and sample analog electrical signals; The data processing device is electrically connected to the high-speed oscilloscope and is used to process and calculate the analog electrical signals collected and sampled to obtain the strain on the surface of the sample to be tested.

2. The device for rapid, non-destructive and non-contact measurement of silicon material surface strain according to claim 1, characterized in that: The femtosecond laser is a near-infrared femtosecond laser or a near-ultraviolet femtosecond laser.

3. The device for rapid, non-destructive and non-contact measurement of silicon material surface strain according to claim 1, characterized in that: It also includes an optical power meter. Before testing, the optical power meter is placed between the microscope objective lens and the sample to be tested. During testing, the optical power meter is moved out of the light path.

4. The device for rapid, non-destructive, and non-contact measurement of silicon material surface strain according to claim 1, characterized in that: It also includes a lens assembly, which is arranged between the spatial dispersion assembly and the microscope objective lens, wherein the first lens assembly is used to adjust the size of the pulse spot and the angle at which the pulse is incident on the microscope objective lens.

5. The device for rapid, non-destructive, and non-contact measurement of silicon material surface strain according to claim 1, characterized in that: It also includes a first collimator and a second collimator, wherein the first collimator is located between the optical signal amplifying component and the beam splitter, and is used to make the pulse amplified by the optical signal amplifying component incident on the beam splitter in the form of a specific angle and spatial light; the second collimator is located between the reference beam exit side of the beam splitter and the high-speed photodetector, and is used to couple the interference pulse into the optical path.

6. The device for rapid, non-destructive, and non-contact measurement of silicon material surface strain according to claim 1, characterized in that: The spatial dispersion component includes an acousto-optic deflector and a diffraction grating which are sequentially arranged on the output light path of the optical signal amplification component. The acousto-optic deflector is used to change the incident position and direction of the pulse incident on the diffraction grating, and the diffraction grating is used to disperse the femtosecond laser pulse into a one-dimensional spatial pulse.

7. A method for measuring silicon material surface strain fast, non-destructive and non-contact according to any one of claims 1 to 6, characterized in that: The steps include: Step 1, clean the sample to be tested and fix it on the outgoing light path of the microscope objective lens; Step 2, starting the femtosecond laser to generate a femtosecond laser pulse sufficient to reflect an image on the surface of the sample to be tested without damaging the sample to be tested; Step 3, the time domain stretching component performs time domain stretching on the femtosecond pulse, and then amplifies it through the optical signal amplification component, and then generates a test beam and a reference beam after passing through a beam splitter, wherein the test beam is incident on the spatial dispersion component and then focused onto the sample to be tested through a microscope objective lens; Step 4: The spatial pulse reflected by the sample to be tested interferes with the reference beam generated by the beam splitter through the spatial dispersion component to form an interference pulse. The high-speed photodetector detects the interference pulse and converts it into an analog signal. The high-speed oscilloscope collects the sampled analog signal and transmits it to the data processing device. The data processing device restores the test pulse signal distribution image sequence reflected by the sample to be tested based on the analog electrical signal sampled by the high-speed oscilloscope. The change of the contour boundary of the light intensity distribution image before and after the strain of the sample to be tested is obtained according to the test pulse signal distribution image sequence, the boundary strain is calculated, and the strain of the sample surface is obtained by interpolation calculation.

8. The method for measuring silicon material surface strain fast, non-destructive and non-contact measuring device according to claim 7, characterized in that: The method for obtaining a test pulse signal distribution image sequence includes: The interference pulse signal is analyzed and reconstructed by a data processing device to obtain the distribution of the test pulse reflected on the sample surface, and a two-dimensional light intensity distribution image sequence reflected on the sample surface is constructed, whose frame rate is equal to the repetition frequency of the near-infrared / near-ultraviolet femtosecond laser, from the sampled light pulse signal I(x) to the light intensity signal I s The conversion formula of (x) is as follows: Among them, I R (x) is the reference pulse intensity, T is the Hilbert transformed component of the filtered high-frequency component of the sampled optical pulse signal I(x), and re(T) and im(T) are the real part and imaginary part of T, respectively.

9. The method for measuring the silicon material surface strain fast, non-destructive and non-contact measuring device according to claim 7, characterized in that: The method for calculating the surface strain of the sample to be tested by the data processing device according to the test pulse signal distribution image sequence includes: The non-local mean algorithm is used to filter the test pulse signal distribution image sequence, and then the binary image is extracted from the filtered light intensity distribution map sequence. The eigenvalue and eigenvector method is used to track the distribution of each contour area of ​​the sample before and after strain. The position coordinate matrix A of each area at the boundary of the sample to be tested is expressed as: A = QΛQ, where Q is the matrix of eigenvectors and Λ is the matrix of eigenvalues; The deformation of each region before and after strain is expressed as: Where: e i is a unit vector; and Represents the transformation matrix of each contour area before and after strain; E j is the characteristic value of the region; The deformation tensor It is expressed as: Strain in each region Calculated by the following formula:

10. The method for measuring silicon material surface strain fast, non-destructive and non-contact measuring device according to claim 9, characterized in that: The method of filtering the test pulse signal distribution image sequence using the non-local mean algorithm includes: Where NL[v](i) is the filtered image of pixel i, v(j) is the original image without filtering; I is the neighborhood of pixel i; w(i, j) represents the similarity between pixels i and j, and its value is determined by the square of the Euclidean distance between the search windows: in, Where h is the smoothing parameter; is the attenuation function of the weighted Euclidean distance between pixel i and pixel j, a is the standard deviation of the Gaussian kernel; Z i is the normalization coefficient.

Citation Information

Patent Citations

  • Method for measuring strain by aid of fiber F-P (Fabry-Perot) sensors

    CN108195300A

  • High-speed and high-flux particle speed measuring system based on optical time stretching

    CN109884657A

  • Transverse strain testing device and testing method of time stretching femtosecond laser pulse

    CN117168341A

  • Laser speckle measurement device for simultaneously measuring in-plane displacement and off-plane displacement

    CN202281596U

  • Silicon wafer surface strain distribution measuring device

    JP2007173526A

Cited By

  • Rapid lossless non-contact measuring device and measuring method for internal strain of silicon material

    CN118913123A

  • Device and method for rapid non-destructive contactless measurement of internal strain in silicon materials

    CN118913123B