Mask device, manufacturing method of mask device and photoetching equipment
By designing the structure of phase shift and fully transparent areas in the mask device, using the interference effect of the light-shielding layer and the phase shift layer, the problem of engraving high-resolution patterns with proximity exposure machines is solved, and pattern resolution and uniformity are achieved Improved performance, suitable for equipment that lacks focus function.
Patent Information
- Application Number
- CN202310500530.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-05-06
- Publication Date
- 2024-11-08
AI Technical Summary
It is difficult for proximity exposure machines to engrave high resolution and refined graphics. The prior art methods to improve resolution are costly or inefficient, and are not suitable for equipment that lack focus function.
A mask device is designed, including a phase shift region and a fully transparent region on a transparent base plate. The phase shift region is provided with a light shielding layer and a phase shift layer. The distance between the light shielding layers is less than or equal to the width of the phase shift layer, and the phase shift layer is The light transmittance is 10% to 90%, so as to form a stable interference effect and improve the resolution and uniformity of the pattern.
It effectively improves the resolution and uniformity of the pattern, reduces the difficulty of manufacturing the mask device, and is suitable for proximity exposure machines, improving the refinement of the pattern line width and product yield.
Smart Images

Figure HDA0004213578180000011 
Figure HDA0004213578180000021 
Figure HDA0004213578180000031
Abstract
Description
Technical Field
[0001] The present application relates to the field of photolithography technology, and in particular to a mask device, a method for manufacturing a mask device, and a photolithography device. Background Art
[0002] In the field of flat panel displays, an exposure machine is usually used to transfer pattern information. The image information on the film or other transparent body is transferred to the surface coated with a photosensitive material through the irradiation of light. At present, the industry usually adopts a mask device to align the Mask Aligner to transfer the pattern. The industry generally uses proximity exposure machines and projection exposure machines. Due to the high price and low production efficiency of projection exposure machines, many manufacturers choose proximity exposure machines for production.
[0003] Due to the influence of the parallel half-angle and oblique angle of light in the proximity exposure machine, the actual width of the pattern after exposure will have a lower limit. For example, the current conventional equipment cannot produce a positive photoresist pattern with a line width of 5μm and a photoresist residual film rate of more than 80%. As the requirements for the refinement of product graphics become higher and higher, it is necessary to improve the graphic resolution of the proximity exposure machine. The conventional way to improve the resolution is to reduce the exposure GAP, reduce the parallel half-angle and oblique angle, reduce the exposure band or optimize the photoresist process. However, reducing the exposure GAP is likely to lead to a decrease in product yield. Theoretically, it is also difficult to continue to improve the parallel half-angle and oblique angle. The cost of reducing the exposure band is also very high. At the same time, the optimization of photoresist is also limited.
[0004] In order to solve the above problems, the industry currently mainly uses phase shift masks (PSM) to enhance resolution. The basic principle is to introduce phase differences in adjacent light-transmitting areas of the mask pattern or to supplement with changes in transmittance to change the interference state between the diffracted light beams of adjacent patterns, and at the same time use the intensity and phase of light to form an image. This is a resolution enhancement technology that reduces the light intensity of dark areas in the light field distribution and increases the light field of bright areas through destructive interference of light fields in adjacent light-transmitting areas, so as to improve contrast and resolution. In the mask device of the prior art, the focal length of the light source is adjusted by setting phase shift layers on both sides of the light-shielding layer, so that the weak light intensity area is narrowed to the focus. This method requires an exposure machine with a focusing function. For a proximity exposure machine, there is no focusing function, so it is not suitable for a proximity exposure machine.
[0005] It is difficult for proximity exposure machines to engrave high-resolution and fine graphics, which has become a problem that needs to be overcome in the industry. Summary of the invention
[0006] The present invention aims to solve the technical problem that a proximity exposure machine is difficult to engrave high-resolution and fine patterns. To this end, the present invention proposes a mask device, which has a high manufacturing precision structure, high resolution of the transferred pattern, good uniformity and consistency.
[0007] Another object of the present invention is to provide a method for manufacturing a mask device.
[0008] Another object of the present invention is to provide a lithography device having the above-mentioned mask device.
[0009] According to a first aspect of the present invention, a mask device includes a transparent bottom plate, the transparent bottom plate includes a phase shift region and a fully transparent region, the phase shift region and the fully transparent region are arranged adjacent to each other, the phase shift region is provided with at least one group of phase shift units, a group of the phase shift units includes a light shielding layer and a phase shift layer, the light shielding layer is arranged on both sides of the phase shift layer, a distance G1 between the light shielding layers is less than or equal to a width D1 of the phase shift layer, and the width D1 of the phase shift layer is less than the sum of the total width D2 of the light shielding layers on both sides and the G1, and the light transmitted from both sides of the two light shielding layers is The interference effect of light on the light passing through the phase shift layer is the same. The width D1 of the phase shift layer is 1 to 5 μm, and the transmittance of the phase shift layer is 10% to 90%. The total width D2 of the shading layer is 1 to 8 μm. Therefore, the width of the phase shift zone can be limited by the distance of the shading layer, thereby reducing the manufacturing difficulty of the mask device and improving the fitting accuracy of the phase shift layer and the shading layer, so that the diffraction light below the phase shift layer and the diffraction light below the shading layer form a stable interference destructive phase, effectively improving the resolution of the interference pattern, and further reducing the line width of the interference pattern.
[0010] According to one embodiment of the present invention, the transmittance of the phase-shift layer is 50% to 70%, and the material of the phase-shift layer is a combination of one or more of metal oxides, metal nitrides, metal oxynitrides, metal carbides, metal alloy oxides, metal alloy nitrides, metal alloy oxynitrides or metal alloy carbides.
[0011] According to another embodiment of the present invention, the phase deflection angle Φ of the phase shift layer complies with the formula: n×160°≤Φ≤n×200°, n=1, 2 or 3.
[0012] According to another embodiment of the present invention, the light shielding layer is disposed on the lower side of the phase shift layer, or the phase shift layer is disposed on the lower side of the light shielding layer.
[0013] According to another embodiment of the present invention, the light shielding layer is a black film, and the black film is a combination of chromium and one or more of chromium oxide, carbide, nitride, carbon oxide or nitrogen oxide.
[0014] According to a method for manufacturing a mask device according to an embodiment of a second aspect of the present invention, the method for manufacturing a mask device comprises the following steps:
[0015] forming a first functional layer on the transparent substrate;
[0016] forming a second functional layer on the first functional layer;
[0017] The first functional layer is a light shielding layer, and the second functional layer is a phase shifting layer, or the first functional layer is a phase shifting layer, and the second functional layer is a light shielding layer.
[0018] According to the manufacturing method of the mask device of the embodiment of the present invention, the width of the phase shift layer is determined by the distance between the light shielding layers, which reduces the influence of the fitting accuracy of the phase shift layer and the light shielding layer. Therefore, the relative position between the light shielding layer and the phase shift layer can be freely selected, thereby making the manufacturing easier.
[0019] According to an embodiment of the third aspect of the present invention, the lithography equipment includes the mask device according to the embodiment of the first aspect of the present invention, and also includes a light source mechanism and a transfer mechanism. The wavelength of the light source used by the light source mechanism is 365nm~425nm. By setting the mask device according to the embodiment of the first aspect of the present invention, the resolution of the transfer pattern of the lithography equipment is improved and the line width of the transfer pattern is reduced.
[0020] According to one embodiment of the present invention, the light source is UV light with a wavelength of 365 nm.
[0021] According to another embodiment of the present invention, the pattern transferred by the transfer mechanism is a stripe pattern or a grid pattern formed by the intersection of the stripes, and the distance between adjacent lines in the stripe pattern or the distance between adjacent lines in the grid pattern is greater than 5 μm.
[0022] According to another embodiment of the present invention, the transfer mechanism includes a transfer substrate, on which a positive photosensitive resin is coated.
[0023] The photolithography equipment of the mask device according to the embodiment of the present invention can improve the uniformity and consistency of the transferred pattern and improve the resolution of the transferred pattern.
[0024] Additional aspects and advantages of the present invention will be given in part in the following description and in part will be obvious from the following description, or will be learned through practice of the present invention. BRIEF DESCRIPTION OF THE DRAWINGS
[0025] The accompanying drawings are only used to illustrate the embodiments and are not to be considered as limiting the present invention. In addition, the same reference symbols are used to represent the same components throughout the accompanying drawings. In the accompanying drawings:
[0026] Figure 1 is a first cross-sectional schematic diagram of a mask device in the prior art;
[0027] Figure 2 A schematic diagram of light intensity of a mask device in the prior art;
[0028] Figure 3 is a first cross-sectional schematic diagram of another prior art mask device;
[0029] Figure 4 A schematic diagram of light intensity of another conventional mask device;
[0030] Figure 5 is a first cross-sectional schematic diagram of the mask device of the present application;
[0031] Figure 6 A schematic diagram of light intensity of the mask device of the present application;
[0032] Figure 7 A schematic diagram of an experimental data table of the mask device of the present application;
[0033] Figure 8 A schematic diagram of a method for manufacturing a mask device of the present application;
[0034] Fig. 9 Schematic diagram of the lithography equipment of the present application.
[0035] The meanings of the marks in the figure are:
[0036] 11. Light-shielding area; 12. Phase-shifting area; 13. Light-transmitting area;
[0037] 101. Transparent substrate; 102. Light-shielding film; 103. Phase shift film;
[0038] 21. Phase shift area; 22. Full transparency area;
[0039] 201, transparent bottom plate; 202, light shielding layer; 203, phase shifting part;
[0040] 300, photolithography equipment; 310, light source mechanism; 320, transfer mechanism; 321, transfer substrate;
[0041] 322. Positive photosensitive resin layer DETAILED DESCRIPTION
[0042] Embodiments of the present invention are described in detail below, examples of which are shown in the accompanying drawings, wherein the same or similar reference numerals throughout represent the same or similar elements or elements having the same or similar functions. The embodiments described below with reference to the accompanying drawings are exemplary and are only used to explain the present invention, and cannot be understood as limiting the present invention.
[0043] In the description of the present invention, it is to be understood that a feature defined as "first" or "second" may explicitly or implicitly include one or more of the features. In the description of the present invention, unless otherwise specified, "plurality" means two or more.
[0044] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0045] In order to illustrate the mask device and its manufacturing method, and the lithography equipment provided by the present application, they are described in detail below in conjunction with the drawings in the specification and the text description of the embodiments.
[0046] Figure 1-Figure 4 An embodiment of a prior art mask device is shown in FIG. Figure 1 As shown, in a specific embodiment of the prior art, a light shielding film 102 and a phase shift film 103 are provided on a transparent substrate 101, and phase shift films 103 are provided on both side edges of the light shielding film 102. The area covered by the light shielding film 102 is a light shielding area 11, and the area covered by the phase shift film 103 is a phase shift area 12. The area outside the light shielding area 11 and the phase shift area 12 is a light transmission area 13. Specifically, in one embodiment, on a proximity exposure machine, such as Figure 2 As shown, the arrangement of the light shielding film 102 and the phase shift film 103 causes mutual interference of light passing through adjacent phase shift regions 12, or the light of adjacent phase shift regions 12 cannot reach a completely consistent direction of eliminating noise, thereby forming new noise, which makes it very difficult to produce fine graphics, and the thickness uniformity of the produced graphics is very poor, thereby reducing the yield rate. The actual line width of the transferred graphics reaches 10μm, and the light in the center area of the line is enhanced, so the photoresist residual line produced is a wavy shape with thick sides and thin in the middle. In addition, this mask device usually needs to adjust the focal length of the light source to narrow the weak light intensity area to the focus, so it is not suitable for a proximity exposure machine; Figure 3-Figure 4As shown, in another specific embodiment of the prior art, a shading film 102 and a phase shift film 103 are arranged on a transparent substrate 101, and the phase shift film 103 is arranged on one side edge of the shading film 102. In the arrangement of the shading film 102 and the phase shift film 103, since the phase shift film 103 and the shading film 102 need to undergo two photolithography and etching processes during the manufacturing process, there is a problem of fitting accuracy between the phase shift film 103 and the shading film 102 during the manufacturing process. For example, when the shading film 102 is first manufactured, since the width of the phase shift film 103 is fixed, the line widths of the superimposed lines of the two are inconsistent, resulting in differences in the effective line widths of the phase shift film 103, and the uniformity of the produced mask device is poor. In the arrangement of the shading film 102 and the phase shift film 103, the light passing through the adjacent phase shift regions 12 will cause mutual interference. Although the line width of the transfer pattern is small, the uniformity and consistency of the transfer pattern are poor.
[0047] Reference below Figure 5-Figure 6 The mask device according to the first embodiment of the present invention is described. The mask device can be used in a photolithography device 300. During the photolithography process, the mask device can be arranged below a light source, and the light source is aligned with the mask device of the substrate to transfer the target pattern. Figure 5As shown, a mask device according to an embodiment of the present invention includes a transparent bottom plate 201, and the transparent bottom plate 201 includes a phase shift area 21 and a fully transparent area 22. The phase shift area 21 and the fully transparent area 22 are arranged adjacent to each other. It can be understood that the light in the fully transparent area 22 can be fully transmitted, and the path of the light in the phase shift area 21 will be offset due to diffraction and interference phenomena. Specifically, the phase shift area 21 is provided with at least one group of phase shift units, and one group of phase shift units includes a shading layer 202 and a phase shift layer 203. The shading layer 202 is arranged on both sides of the phase shift layer 203, and the distance G1 between the shading layers 202 on both sides is less than or equal to the width D1 of the phase shift layer 203, thereby ensuring that no light in the phase shift area 21 will directly pass through, and the width D1 of the phase shift layer 203 is less than the sum of the total width D2 of the shading layers 202 on both sides and the distance G1 between the shading layers 202 on both sides, thereby ensuring that the phase shift layer 203 only exists in the shading layer 20 2, the interference effect of the light transmitted from both sides of the two shading layers 202 on the light transmitted through the phase shift layer 203 is the same, so that the interference effect of the light transmitted from both sides of the shading layer 202 on the light transmitted through the middle phase shift layer 203 is consistent. Specifically, the width D1 of the phase shift layer 203 is 1-5 μm, and the transmittance of the phase shift layer 203 when the wavelength of the light source is 330nm-430nm is 10%-90%, and the sum of the widths D2 of the two shading layers 202 is 1-8 μm. Therefore, the present solution can limit the width of the phase shift region 21 by the distance between the shading layers 202, thereby reducing the manufacturing difficulty of the mask device and improving the fitting accuracy of the phase shift layer 203 and the shading layer 202, so that the diffracted light below the phase shift layer 203 and the diffracted light below the shading layer 202 form a stable interference destructive phase, effectively improving the resolution of the interference pattern and improving the uniformity and consistency of the interference pattern.
[0048] It should be noted that, in order to achieve the same interference effect of the light shielding layers 202 on both sides on the light source of the phase shift layer 203, that is, the light transmitted from both sides of the two light shielding layers 202 has the same interference effect on the light transmitted through the phase shift layer 203, the light shielding layers 202 on both sides of the phase shift layer 203 can be light shielding layers 202 with the same material and shape. For example, the two light shielding layers 202 can be cubes or rectangular parallelepipeds with the same length, width and height. In another embodiment, the light shielding layers 202 on both sides of the phase shift layer 203 can be light shielding layers 202 with different materials. For example, the two light shielding layers 20 2 can be a cube or a cuboid with the same length, width and height. The light shielding layer 202 on one side is made of multiple materials or a multi-layer structure, and the light shielding layer 202 on the other side is made of one material or only a single-layer structure. However, the interference effect of the light shielding layers 202 on the phase shift layer 203 on both sides is consistent. In some other embodiments, the light shielding layer 202 can be an irregularly shaped pattern. Therefore, as long as the interference effect of the light passing through the two sides of the light shielding layers 202 on the light passing through the phase shift layer 203 is consistent, the shape and composition of the light shielding layer 202 are not specifically limited.
[0049] It should be noted that the width D1 of the phase shift layer 203 and the width of a single light shielding layer 202 are both greater than 0.5 μm and less than 5 μm, and the total width D2 of the two light shielding layers 202 is greater than 1 μm and less than 8 μm. Within this range, the interference effect can be optimized. If the width D1 of the phase shift layer 203 and the total width D2 of the light shielding layer 202 are too large or too small, the interference effect will be affected, thereby affecting the final graphic imaging effect. In some specific embodiments, the width D2 of each light shielding layer 202 is smaller than the width D1 of the phase shift layer 203, so that the interference effect is better.
[0050] It should be noted that the distance G1 between the light-shielding layers 202 on both sides is less than or equal to the width D1 of the phase-shift layer 203, and the width D1 of the phase-shift layer 203 is less than the sum of the total width D2 of the light-shielding layers 202 on both sides and the distance G1 between the light-shielding layers 202 on both sides. That is to say, both ends of the phase-shift layer 203 are in contact with the light-shielding layer 202, that is, both ends of the phase-shift layer 203 will not extend to the full-transmission area 22, so as to ensure that no light will directly bypass the phase-shift layer 203 and directly pass through the phase-shift area 21, and at the same time ensure that the phase-shift layer 203 will not interfere with the light in the full-transmission area 22, so that the light passing through the two sides of the light-shielding layer 202 can interfere with the light passing through the middle phase-shift layer 203.
[0051] According to an embodiment of the present invention, the light transmittance of the phase shift layer 203 is 50% to 70%. Figure 7As described above, different transmittances of the phase shift layer 203 have different effects on the line width and the residual film rate. When the transmittance is lower than 10%, the interference effect becomes worse, so that the transferred line width will be higher than 8μm, resulting in low resolution of the transferred pattern and excessive line width. At the same time, when the transmittance is higher than 90%, although the interference effect is better, it will lead to a decrease in the residual film rate, thereby reducing the yield rate of the product. It should be noted that when the transmittance of the phase shift layer 203 is 50% to 70%, the interference effect of light is better, and the residual film rate is maintained at a relatively high level, the comprehensive performance is the best, and a pattern with a smaller line width can be manufactured and the yield rate of the product can be guaranteed. Furthermore, the material of the phase shift layer 203 is a combination of one or more materials selected from metal oxides, metal nitrides, metal oxynitrides, metal carbides, metal alloy oxides, metal alloy nitrides, metal alloy oxynitrides, metal alloy carbides, etc., and is not specifically limited here.
[0052] According to another embodiment of the present invention, the phase deflection angle Φ of the phase shift layer 203 meets the formula: n×160°≤Φ≤n×200° (n=1, 2 or 3). For example, when n is 1, the phase deflection angle Φ is 160°-200°, when n is 2, the phase deflection angle Φ is 320°-400°, and when n is 3, the phase deflection angle Φ is 480°-600°. It should be noted that when the phase deflection angle Φ is greater than 180°, the imaging effect is better. However, since the manufacturing of the phase shift layer 203 often has errors, the phase deflection angle Φ may have an error of plus or minus 20°, and the imaging effect can still be ensured to be maintained in a better range. The phase deflection angle Φ in this range is beneficial for forming a compact fine pattern, and the resolution of the transferred line pattern is higher.
[0053] According to another embodiment of the present invention, in the direction perpendicular to the transparent bottom plate 201, the shading layer 202 is arranged on the lower side of the phase-shift layer 203, or the phase-shift layer 203 is arranged on the lower side of the shading layer 202. Since the phase-shift layer 203 is located in the middle of the shading layer 202, the width of the phase-shift layer 203 is actually determined by the distance between the shading layers 202. Therefore, in the mask device, the relative position of the shading layer 202 and the phase-shift layer 203 will not affect the effective width of the phase-shift region 21. Therefore, the relative position of the shading layer 202 and the phase-shift layer 203 in the direction perpendicular to the transparent bottom plate 201 may not be restricted. For example, the phase-shift layer 203 and the shading layer 202 may both be in contact with the transparent bottom plate 201, and at the same time, the height of the phase-shift layer 203 in the direction perpendicular to the transparent bottom plate 201 is greater than that of the shading layer 202.
[0054] According to another embodiment of the present invention, the material of the light-shielding layer 202 is one or more of black films composed of chromium and chromium oxide, carbide, nitride, carbon oxide, nitrogen oxide, etc. It should be noted that in other embodiments, the light-shielding layer 202 can be any material that meets the transmittance requirements and is not specifically limited here.
[0055] According to a method for manufacturing a mask device according to a second aspect of the present invention, Figure 8 As shown, the method for manufacturing the mask device comprises the following steps:
[0056] S1: forming a first functional layer on the transparent substrate 201;
[0057] S2: forming a second functional layer on the first functional layer;
[0058] The first functional layer is the light shielding layer 202 , and the second functional layer is the phase shift layer 203 , or the first functional layer is the phase shift layer 203 , and the second functional layer is the light shielding layer 202 .
[0059] Specifically, in the direction perpendicular to the transparent bottom plate 201, the shading layer 202 is arranged on the lower side of the phase-shift layer 203, or the phase-shift layer 203 is arranged on the lower side of the shading layer 202. Since the phase-shift layer 203 is located in the middle of the shading layer 202, the width of the phase-shift layer 203 is actually determined by the distance between the shading layers 202. Therefore, in the mask device, the relative position of the shading layer 202 and the phase-shift layer 203 will not affect the effective width of the phase-shift region 21. Therefore, the relative position of the shading layer 202 and the phase-shift layer 203 in the direction perpendicular to the transparent bottom plate 201 may not be restricted. Therefore, when manufacturing the mask device, the shading layer 202 may be manufactured on the substrate first, and then the phase-shift layer 203 may be manufactured, or the phase-shift layer 203 may be manufactured first, and then the shading layer 202 may be manufactured. Since the manufacturing order of the shading layer 202 and the phase-shift layer 203 may be interchanged, the process may be adjusted according to production needs, making the manufacturing of the mask device easier.
[0060] According to the lithography apparatus 300 of the third aspect of the present invention, Fig. 9As shown, the lithography device 300 includes the above-mentioned mask device, and also includes a light source mechanism 310 and a transfer mechanism 320. The lithography device 300 is a proximity lithography device 300. The distance between the transparent base plate 201 of the mask device and the transfer mechanism 320 can be 50 to 200um. When the distance between the mask device and the transfer mechanism 320 is 50 to 200um, it is beneficial to transfer a transfer pattern with a finer width. Furthermore, the wavelength of the light source used by the light source mechanism 310 is 365nm to 425nm. The light source of the light source mechanism 310 can be a mercury lamp. Since the mercury lamp has strong peaks in the i-line, h-line, and g-line, the positive photosensitive resin with a good sensitivity range for the peak of 365nm or 425nm has a better effect, which is beneficial to better transfer the pattern.
[0061] According to an embodiment of the present invention, the light source used by the light source mechanism 310 is UV ultraviolet light with a wavelength of 365 nm. The light source with this wavelength has stable performance and better transfer imaging effect.
[0062] According to another embodiment of the present invention, the pattern transferred by the transfer mechanism 320 is a stripe pattern or a grid pattern composed of crossed stripes, and the line spacing in the stripe pattern or the grid pattern is greater than 5μm. It can be understood that the stripe pattern can be a rectangular pattern or a diamond pattern, and the stripe pattern can be a regular pattern evenly distributed, or a locally regular pattern, which is not limited here.
[0063] According to another embodiment of the present invention, the transfer mechanism 320 also includes a transfer substrate 321, which is arranged on the transfer mechanism 320 and is opposite to the mask device. The transfer substrate 321 is coated with a positive photosensitive resin layer 322. The positive photosensitive resin layer 322 is more conducive to the formation process of the photolithography pattern and is conducive to forming a compact fine pattern, so that the resolution of the transferred fine width line pattern is higher.
[0064] The mask device and its manufacturing method, and the lithography equipment provided by the present application are preferred embodiments and should not be understood as limiting the scope of protection of the present application. Those skilled in the art should know that various improvements or replacements can be made without departing from the concept of the present application, and all improvements or replacements should be within the scope of protection of the present application, that is, the scope of protection of the present application should be based on the claims.
[0065] In the absence of conflict, the above embodiments and features in the embodiments may be combined with each other.
Claims
1. A mask device, It is characterized in that A transparent bottom plate is included, wherein the transparent bottom plate includes a phase shift area and a fully transparent area, the phase shift area and the fully transparent area are adjacently arranged, the phase shift area is provided with at least one group of phase shift units, one group of phase shift units includes a shading layer and a phase shift layer, the shading layer is arranged on both sides of the phase shift layer, the distance G1 between the shading layers is less than or equal to the width D1 of the phase shift layer, and the width D1 of the phase shift layer is less than the sum of the total width D2 of the shading layers on both sides and the distance G1 between the shading layers, the light passing through the two sides of the two shading layers has the same interference effect on the light passing through the phase shift layer, the width D1 of the phase shift layer is 1 to 5 μm, and the transmittance of the phase shift layer is 10% to 90%, and the total width D2 of the shading layer is 1 to 8 μm.
2. The mask device according to claim 1, It is characterized in that The light transmittance of the phase shift layer is 50% to 70%, and the phase shift layer is a combination of one or more of metal oxides, metal nitrides, metal oxynitrides, metal carbides, metal alloy oxides, metal alloy nitrides, metal alloy oxynitrides or metal alloy carbides.
3. The mask device according to claim 1, It is characterized in that The phase deflection angle Φ of the phase shift layer complies with the formula: n×160°≤Φ≤n×200°, where n=1, 2 or 3.
4. The mask device according to claim 1, It is characterized in that The light shielding layer is arranged on the lower side of the phase shift layer, or the phase shift layer is arranged on the lower side of the light shielding layer.
5. The mask device according to claim 1, It is characterized in that The light shielding layer is a black film, and the black film is a combination of chromium and one or more of chromium oxide, carbide, nitride, carbon oxide or nitrogen oxide.
6. A method for manufacturing a mask device, It is characterized in that forming a first functional layer on the transparent substrate; forming a second functional layer on the first functional layer, The first functional layer is a light shielding layer, and the second functional layer is a phase shifting layer, or the first functional layer is a phase shifting layer, and the second functional layer is a light shielding layer.
7. A lithography apparatus, comprising the mask device according to any one of claims 1 to 5, It is characterized in that It also includes a light source mechanism and a transfer mechanism. The light source wavelength used by the light source mechanism is 365nm-425nm.
8. The lithographic apparatus according to claim 7, It is characterized in that The light source is UV light with a wavelength of 365 nm.
9. The lithographic apparatus according to claim 7, It is characterized in that The pattern transferred by the transfer mechanism is a stripe pattern or a grid pattern formed by the intersection of the stripes, and the distance between adjacent lines in the stripe pattern or the distance between adjacent lines in the grid pattern is greater than 5 μm.
10. The lithographic apparatus according to claim 7, It is characterized in that The transfer mechanism comprises a transfer substrate on which a positive photosensitive resin is coated.