Manufacturing method of polycrystalline silicon gate
By using the photolithography and etching steps of the flash memory region to perform multiple lithography and etching in semiconductor manufacturing, the top deformation problem caused by the small photolithography process window of the logic region is solved, which improves device uniformity and reduces manufacturing cost.
Patent Information
- Application Number
- CN202411004850.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-24
- Publication Date
- 2024-11-08
AI Technical Summary
In semiconductor manufacturing, especially for embedded flash memory process platforms, the polysilicon gate in the logic region is deformed due to the small photolithography process window, affecting device uniformity, and existing improvement methods increase manufacturing costs.
By performing two photolithography and etching processes on the polysilicon material layer, the gate layout of the logic region is transferred using the existing photolithography and etching steps of the flash memory region to achieve multiple photolithography and etching, avoiding the additional preparation of the logic region light The need for cover reduces costs.
The morphological uniformity of the logic region polysilicon gate is improved, manufacturing costs are reduced, and device uniformity is improved through exposure plus etching steps in flash memory device processes.
Smart Images

Figure CN118919405A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of semiconductor manufacturing technology, and in particular to a method for manufacturing a polysilicon gate. Background Art
[0002] As semiconductor line width decreases, the gate pattern process window is challenged, especially in the embedded flash memory process platform. Considering the difference in flatness between the flash memory area and the logic area, the process window is further reduced.
[0003] In some special layout areas, such as the logic area of SRAM (Static Random-Access Memory), the polysilicon gate (poly) pattern in the logic area often violates the minimum layout rule, the lithography process window is small, and the top of the gate polysilicon is deformed due to the optical proximity effect, which leads to poor device uniformity.
[0004] Currently, multiple exposures and multiple etchings can be considered to improve the gate pattern. Although multiple photolithography and etching of the gate polysilicon in the logic area can improve the morphology, the current manufacturing process requires at least one more photolithography and etching process, which increases the manufacturing cost. Summary of the invention
[0005] The present application provides a method for manufacturing a polysilicon gate, which can solve at least one of the following problems: deformation of the top of the gate polysilicon in the logic area of a flash memory device due to a poor photolithography process, and high cost for improving the morphology of the gate polysilicon.
[0006] The present application provides a method for manufacturing a polysilicon gate, comprising:
[0007] A substrate is provided, the substrate comprising a flash memory area and a logic area, a shallow trench isolation structure is formed in the substrate of the logic area, at least a polysilicon material layer is formed on the substrate of the logic area; at least a bit line polysilicon layer is formed on the substrate of the flash memory area;
[0008] coating a first photoresist layer on the polysilicon material layer;
[0009] Transferring the first portion of the logic region gate pattern on the first photomask to the first photoresist layer by exposure and development to obtain a patterned first photoresist layer;
[0010] Using the patterned first photoresist layer as a mask, performing a first etching on the polysilicon material layer of the logic area;
[0011] coating a second photoresist layer on the polysilicon material layer;
[0012] By exposing and developing, the flash memory area layout and the second part of the logic area gate layout on the second mask are transferred to the second photoresist layer to obtain a patterned second photoresist layer; and
[0013] Using the patterned second photoresist layer as a mask, the bit line polysilicon layer of the flash memory area is etched, and the polysilicon material layer of the logic area is etched a second time, wherein a polysilicon gate is obtained in the logic area by etching the polysilicon material layer of the logic area for the first time and the second time.
[0014] Optionally, in the manufacturing method of the polysilicon gate, the logic area includes a plurality of logic device units arranged in an array, the active areas of the logic device units are arranged in the substrate along a first direction and different active areas are parallel to a second direction, the first direction and the second direction are perpendicular to each other, and the different active areas are isolated by the shallow trench isolation structure.
[0015] Optionally, in the method for manufacturing the polysilicon gate, the pattern on the patterned first photoresist layer includes at least: a plurality of strip-shaped dark field patterns, the dark field patterns are arranged on the polysilicon material layer on the surface of the active area along the second direction, and the plurality of the dark field patterns are parallel to the first direction;
[0016] The patterned first photoresist layer having the dark field pattern is used as a mask to perform a first etching on the polysilicon material layer in the logic area to obtain a gate transition layer.
[0017] Optionally, in the method for manufacturing the polysilicon gate, the pattern on the patterned second photoresist layer includes at least: a plurality of strip-shaped bright field patterns, the bright field patterns are arranged between different active regions along a first direction, and a plurality of the bright field patterns are parallel to a second direction;
[0018] The patterned second photoresist layer having the bright field pattern is used as a mask to perform a second etching on the polysilicon material layer in the logic area to cut off the gate transition layer and obtain the polysilicon gates corresponding to all logic device units.
[0019] Optionally, in the method for manufacturing the polysilicon gate, the line width of the bright field pattern is greater than the minimum spacing between adjacent polysilicon gates.
[0020] Optionally, in the method for manufacturing the polysilicon gate, a distance between the active area and the adjacent bright field pattern is smaller than a size of the active area corresponding to the bottom of the polysilicon gate extending out.
[0021] Optionally, in the method for manufacturing the polysilicon gate, a distance between the active area and the adjacent bright field pattern is greater than an overlay error between a first etching and a second etching.
[0022] The technical solution of this application has at least the following advantages:
[0023] The present application transfers the first part of the logic area gate layout on the first mask to the first photoresist layer through the first photolithography; uses the patterned first photoresist layer as a mask to perform the first etching on the polysilicon material layer of the logic area; then transfers the flash memory area layout and the second part of the logic area gate layout on the second mask to the second photoresist layer through the second photolithography; uses the patterned second photoresist layer as a mask to etch the bit line polysilicon layer of the flash memory area while performing the second etching on the polysilicon material layer of the logic area, wherein the polysilicon gate is obtained in the logic area through the first etching and the second etching. The present application utilizes the existing polysilicon photolithography and etching process steps of the flash memory area to realize multiple photolithography and etching of the polysilicon of the logic area gate. Without the need to add a mask specifically for preparing the logic area gate, the polysilicon morphology of the logic area gate is improved through the existing exposure and etching steps in the flash memory device preparation process, which in disguise reduces the manufacturing cost and improves the device uniformity. BRIEF DESCRIPTION OF THE DRAWINGS
[0024] In order to more clearly illustrate the specific implementation methods of the present application or the technical solutions in the prior art, the drawings required for use in the specific implementation methods or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some implementation methods of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative work.
[0025] Figure 1 is a flow chart of a method for manufacturing a polysilicon gate according to an embodiment of the present invention;
[0026] Figure 2 is a schematic top view of a logic area before the polysilicon material layer is first etched according to an embodiment of the present invention;
[0027] Figure 3 is a schematic top view of a logic area after the polysilicon material layer is etched for the first time according to an embodiment of the present invention;
[0028] Figure 4 is a schematic top view of a logic area before a polysilicon material layer is etched for the second time according to an embodiment of the present invention;
[0029] Figure 5 is a schematic top view of the logic area after the polysilicon material layer is etched for the second time according to an embodiment of the present invention;
[0030] Figure 6 yes Figure 5 A schematic cross-sectional view of the logic area along the AA' tangent line;
[0031] The reference numerals are as follows:
[0032] 10-substrate, 11-active area, 12-shallow trench isolation structure, 13-polysilicon material layer, 14-gate transition layer, 15-polysilicon gate, 16-gate dielectric layer, 20-dark field pattern, 30-bright field pattern, DETAILED DESCRIPTION
[0033] The following will be combined with the accompanying drawings to clearly and completely describe the technical solutions in this application. Obviously, the described embodiments are part of the embodiments of this application, not all of them. Based on the embodiments in this application, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of this application.
[0034] In the description of the present application, it should be noted that the terms "center", "upper", "lower", "left", "right", "vertical", "horizontal", "inner", "outer", etc., indicating the orientation or positional relationship, are based on the orientation or positional relationship shown in the drawings, and are only for the convenience of describing the present application and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present application. In addition, the terms "first", "second", and "third" are used for descriptive purposes only, and cannot be understood as indicating or implying relative importance.
[0035] In the description of this application, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, it can also be the internal connection of two components, it can be a wireless connection, or it can be a wired connection. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to specific circumstances.
[0036] In addition, the technical features involved in the different embodiments of the present application described below can be combined with each other as long as they do not conflict with each other.
[0037] The present application provides a method for manufacturing a polysilicon gate. Figure 1 , Figure 1 1 is a flow chart of a method for manufacturing a polysilicon gate according to an embodiment of the present invention. The method for manufacturing a polysilicon gate in a logic region includes:
[0038] Step S1: providing a substrate, wherein the substrate comprises a flash memory area and a logic area, a shallow trench isolation structure is formed in the substrate of the logic area, and at least a polysilicon material layer is formed on the substrate of the logic area; and at least a bit line polysilicon layer is formed on the substrate of the flash memory area;
[0039] Step S2: coating a first photoresist layer on the polysilicon material layer;
[0040] Step S3: transferring the first portion of the logic region gate pattern on the first mask to the first photoresist layer by exposure and development to obtain a patterned first photoresist layer;
[0041] Step S4: using the patterned first photoresist layer as a mask, performing a first etching on the polysilicon material layer of the logic area;
[0042] Step S5: coating a second photoresist layer on the polysilicon material layer;
[0043] Step S6: transferring the flash memory area layout and the second portion of the logic area gate layout on the second mask to the second photoresist layer by exposure and development to obtain a patterned second photoresist layer; and
[0044] Step S7: Using the patterned second photoresist layer as a mask, etching the bit line polysilicon layer of the flash memory area, and etching the polysilicon material layer of the logic area for a second time, wherein a polysilicon gate is obtained in the logic area by etching the polysilicon material layer of the logic area for the first time and the second time.
[0045] Specifically, refer to Figure 2-Figure 6 Next, the method for manufacturing the logic area polysilicon gate provided by the present application is described in detail.
[0046] First, a substrate 10 is provided, which includes a flash memory area and a logic area. A shallow trench isolation structure 12 is formed in the substrate of the logic area, and at least a polysilicon material layer 13 is formed on the substrate of the logic area; at least a bit line polysilicon layer (not shown) is formed on the substrate of the flash memory area.
[0047] In this embodiment, if Figure 6 As shown, a gate dielectric layer 16 may be formed between the substrate of the logic region and the polysilicon material layer 13 .
[0048] Specifically, the logic area includes a plurality of logic device units arranged in an array, the active areas 11 of the logic device units are arranged in a substrate 10 along a first direction and different active areas 11 are parallel to a second direction, the first direction and the second direction are perpendicular to each other, and different active areas 11 are isolated by the shallow trench isolation structure 12.
[0049] In this embodiment, the first direction is the X direction (lateral direction), and the second direction is the Y direction (vertical direction). In this embodiment, the logic area includes a plurality of logic device units arranged in an array, and the active areas 11 of the logic device units are arranged in the substrate 10 along the X direction and different active areas 11 are parallel to the Y direction, and different active areas 11 are isolated by the shallow trench isolation structure 12.
[0050] Then, a first photoresist layer is coated on the polysilicon material layer.
[0051] Next, the first portion of the logic region gate pattern on the first photomask is transferred to the first photoresist layer through exposure and development to obtain a patterned first photoresist layer.
[0052] Among them, the patterns on the patterned first photoresist layer at least include: a plurality of strip-shaped dark field patterns 20, which are arranged along the second direction on the polysilicon material layer 13 on the surface of the active area 11, and a plurality of the dark field patterns 20 are parallel to the first direction.
[0053] Preferably, the patterned first photoresist layer completely covers the flash memory area, that is, the pattern on the patterned first photoresist layer in the flash memory area is completely a dark field pattern.
[0054] In this embodiment, if Figure 2 As shown, the dark field pattern 20 is arranged on the polysilicon material layer 13 on the surface of the active area 11 along the Y direction, and a plurality of the dark field patterns 20 are parallel to the X direction. In the logic area, except for the area covered by the dark field pattern on the patterned first photoresist layer, the other logic area areas are bright field patterns, which opens an etching window for the subsequent first etching of the polysilicon material layer 13.
[0055] Furthermore, the polysilicon material layer 13 in the logic area is first etched using the patterned first photoresist layer as a mask.
[0056] Specifically, Figure 3 As shown, the patterned first photoresist layer having the dark field pattern 20 is used as a mask to perform a first etching on the polysilicon material layer 13 of the logic area to obtain a gate transition layer 14 .
[0057] Next, a second photoresist layer is coated on the polysilicon material layer 13 , that is, a second photoresist layer is coated on the gate transition layer 14 .
[0058] Furthermore, the flash memory area layout and the second part of the logic area gate layout on the second mask are transferred to the second photoresist layer through exposure and development to obtain a patterned second photoresist layer.
[0059] The patterns on the patterned second photoresist layer at least include: a plurality of strip-shaped bright field patterns 30, the bright field patterns 30 are arranged between different active regions along a first direction, and a plurality of the bright field patterns are parallel to a second direction.
[0060] In this embodiment, if Figure 4 As shown, the bright field patterns 30 are arranged between different active regions along the X direction, and a number of the bright field patterns are parallel to the Y direction.
[0061] Finally, using the patterned second photoresist layer as a mask, the bit line polysilicon layer of the flash memory area is etched, and the polysilicon material layer of the logic area is etched a second time, wherein a polysilicon gate is obtained in the logic area by etching the polysilicon material layer of the logic area for the first time and the second time.
[0062] In this embodiment, if Figure 5 and Figure 6 As shown, using the patterned second photoresist layer having the bright field pattern 30 as a mask, the polysilicon material layer of the logic area (the polysilicon material layer here can also be understood as the gate transition layer 14) is etched for the second time and stopped at the surface of the shallow trench isolation structure 12 to cut off the gate transition layer 14 and obtain the polysilicon gate 15 corresponding to all logic device units.
[0063] Among them, the process of performing a second etching on the gate transition layer 14 of the logic area using the patterned second photoresist layer having the bright field pattern 30 as a mask needs to ensure a sufficient process window, while also etching away the polysilicon material corresponding to the bright field patterns of the flash memory area and the logic area.
[0064] from Figure 5 Hehe Figure 6 It can be seen that through the first photolithography and etching and the second photolithography and etching, the top of the polysilicon gate 15 extending out of the active area can maintain a rectangular shape, and the line width L of the polysilicon gate 15 has good uniformity.
[0065] It is worth noting that the present application does not necessarily require that the polysilicon material layer of the logic area is etched for the second time while the bit line polysilicon layer of the flash memory area is etched. It can also be that multiple photolithography and etching of the gate polysilicon of the logic area are achieved at the same time as other existing flash memory area polysilicon photolithography and etching process steps. The present embodiment is only an example of etching the polysilicon material layer of the logic area for the second time while etching the bit line polysilicon layer of the flash memory area. Therefore, the present application does not impose any limitation on the bright field pattern or dark field pattern of the flash memory area on the patterned second photoresist layer in the flash memory area photolithography process.
[0066] Preferably, the line width d of the bright field pattern 30 is greater than the minimum spacing b between adjacent polysilicon gates 15 .
[0067] Preferably, a spacing c between the active region and the adjacent bright field pattern is smaller than a size a of each active region corresponding to each polysilicon gate extending out of the bottom.
[0068] Furthermore, the spacing c between the active area and the adjacent bright field pattern is greater than the overlay error between the first etching and the second etching, and the overlay error can be obtained by measuring the overlay error between the alignment mark of the previous layer (first etching) and the alignment mark of the current layer (second etching).
[0069] In the present application, the existing polysilicon lithography and etching process steps in the flash memory area are utilized to implement multiple lithography and etching of the polysilicon of the logic area gate. Without the need for additional masks specifically for preparing the logic area gate, the existing exposure and etching steps in the flash memory device preparation process are used to improve the polysilicon morphology of the logic area gate, thereby reducing the manufacturing cost in disguise and improving the device uniformity.
[0070] Obviously, the above embodiments are merely examples for the purpose of clear explanation, and are not intended to limit the implementation methods. For those skilled in the art, other different forms of changes or modifications can be made based on the above description. It is not necessary and impossible to list all the implementation methods here. The obvious changes or modifications derived therefrom are still within the scope of protection created by this application.
Claims
1. A method for manufacturing a polysilicon gate, characterized in that: include: A substrate is provided, the substrate comprising a flash memory area and a logic area, a shallow trench isolation structure is formed in the substrate of the logic area, at least a polysilicon material layer is formed on the substrate of the logic area; at least a bit line polysilicon layer is formed on the substrate of the flash memory area; coating a first photoresist layer on the polysilicon material layer; Transferring the first portion of the logic region gate pattern on the first photomask to the first photoresist layer by exposure and development to obtain a patterned first photoresist layer; Using the patterned first photoresist layer as a mask, performing a first etching on the polysilicon material layer of the logic area; coating a second photoresist layer on the polysilicon material layer; Transferring the flash memory area layout and the second part of the logic area gate layout on the second mask to the second photoresist layer by exposure and development to obtain a patterned second photoresist layer; as well as Using the patterned second photoresist layer as a mask, the bit line polysilicon layer of the flash memory area is etched, and the polysilicon material layer of the logic area is etched a second time, wherein a polysilicon gate is obtained in the logic area by etching the polysilicon material layer of the logic area for the first time and the second time.
2. The method for manufacturing a polysilicon gate according to claim 1, characterized in that: The logic area includes a plurality of logic device units arranged in an array, the active areas of the logic device units are arranged in a substrate along a first direction and different active areas are parallel to a second direction, the first direction and the second direction are perpendicular to each other, and different active areas are isolated by the shallow trench isolation structure.
3. The method for manufacturing a polysilicon gate according to claim 2, characterized in that: The patterns on the patterned first photoresist layer at least include: a plurality of strip-shaped dark field patterns, the dark field patterns are arranged on the polysilicon material layer on the surface of the active area along the second direction, and the plurality of the dark field patterns are parallel to the first direction; The patterned first photoresist layer having the dark field pattern is used as a mask to perform a first etching on the polysilicon material layer in the logic area to obtain a gate transition layer.
4. The method for manufacturing a polysilicon gate according to claim 3, characterized in that: The patterns on the patterned second photoresist layer at least include: a plurality of strip-shaped bright field patterns, the bright field patterns are arranged between different active regions along a first direction, and a plurality of the bright field patterns are parallel to a second direction; The patterned second photoresist layer having the bright field pattern is used as a mask to perform a second etching on the polysilicon material layer in the logic area to cut off the gate transition layer and obtain the polysilicon gates corresponding to all logic device units.
5. The method for manufacturing a polysilicon gate according to claim 4, characterized in that: The line width of the bright field pattern is greater than the minimum spacing between adjacent polysilicon gates.
6. The method for manufacturing a polysilicon gate according to claim 4, characterized in that: The spacing between the active area and the adjacent bright field pattern is smaller than the size of the active area corresponding to the bottom of the polysilicon gate extending out.
7. The method for manufacturing a polysilicon gate according to claim 4, characterized in that: The spacing between the active area and the adjacent bright field pattern is greater than the overlay error between the first etching and the second etching.