Power device
By designing a recessed front metal layer end face in SiC power devices, the contact metal layer acts as a moisture barrier, solving the problem of passivation layer damage and improving device reliability in high temperature and high humidity environments.
Patent Information
- Application Number
- CN202411266029.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-10
- Publication Date
- 2024-11-08
AI Technical Summary
Existing SiC power devices are prone to passivation layer damage in high temperature and high humidity environments, allowing moisture to penetrate to the semiconductor substrate surface, leading to device failure. The reliability of H3TRB is insufficient.
The front metal layer is designed to be recessed relative to the contact metal layer. The contact metal layer also serves as a moisture barrier layer, preventing moisture from penetrating to the semiconductor substrate surface and enhancing the protection of the passivation layer.
H3TRB improves the reliability of SiC power devices in high temperature and high humidity environments, prevents moisture penetration, protects the terminal electric field structure, and extends device life.
Smart Images

Figure CN118919574A_ABST
Abstract
Description
Technical Field
[0001] The embodiments of the present invention relate to the technical field of semiconductor devices, and in particular to a power device. Background Art
[0002] Power devices such as silicon carbide (SiC) Schottky diode devices are increasingly used in high temperature and high humidity environments, so tests such as high humidity reverse bias test (H3TRB) are usually used to characterize their reliability in these extreme environments. Compared with silicon (Si) materials, SiC materials themselves have excellent properties and can better withstand extreme working conditions. Therefore, the focus of the reliability of SiC power devices has gradually shifted from the semiconductor material itself to the passivation, metal contact, and packaging materials of the device. At present, SiC power devices will choose a passivation layer structure of silicon oxide and silicon nitride stacks to prevent moisture erosion, but this passivation layer is sometimes damaged. For example, under extreme working conditions, due to thermal expansion or water vapor intrusion, the passivation layer is prone to cracks and corrosion. Water vapor will accelerate the entry from the cracks under the action of high electric fields and penetrate into the semiconductor substrate of the device, such as the surface of the silicon carbide substrate, and the terminal electric field will be destroyed, eventually leading to device failure.
[0003] Therefore, how to effectively prevent water vapor from penetrating into the surface of the semiconductor substrate to improve the H3TRB reliability capability of the device is a technical problem that needs to be solved urgently. Summary of the invention
[0004] In view of this, an embodiment of the present invention provides a power device to improve the H3TRB reliability capability of the device.
[0005] Specifically, an embodiment of the present invention provides a power device, for example, including:
[0006] A semiconductor substrate having an active region and a peripheral region surrounding the active region;
[0007] a contact metal layer, disposed on the active area to form an electrical contact with the semiconductor substrate and extending from the active area toward the peripheral area;
[0008] a front metal layer, arranged on a side of the contact metal layer away from the semiconductor substrate and extending from the active area toward the peripheral area, wherein an end surface of the front metal layer is indented relative to an end surface of the contact metal layer;
[0009] a passivation layer, disposed on the semiconductor substrate, wherein the passivation layer covers the contact metal layer and the front metal layer and exposes at least a portion of the surface of the front metal layer, and the material of the passivation layer is an inorganic material; and
[0010] A protection layer is disposed on the semiconductor substrate, wherein the protection layer covers the passivation layer and exposes at least a portion of the surface of the front metal layer.
[0011] The above-mentioned embodiments of the present invention can have the following beneficial effects: through structural design, the end face of the front metal layer is retracted relative to the end face of the contact metal layer. The contact metal layer here plays the function of a water vapor barrier layer, which can prevent water vapor from penetrating into the surface of the semiconductor substrate even if the passivation layer is broken at the corner due to excessive stress. Therefore, the moisture resistance reliability capabilities of the power device such as H3TRB can be improved. BRIEF DESCRIPTION OF THE DRAWINGS
[0012] The specific implementation modes of the present invention will be described in detail below with reference to the accompanying drawings.
[0013] Figure 1 A schematic diagram of the structure of a power device provided by an embodiment of the present invention.
[0014] Figure 2 A schematic diagram of the structure of another power device provided by an embodiment of the present invention.
[0015] Figure 3 for Figure 1 An enlarged schematic diagram of part C of the power device shown.
[0016] Figure 4 A schematic diagram of the structure of another power device provided by an embodiment of the present invention.
[0017] Figure 5 A schematic structural diagram of a semiconductor substrate obtaining step in a method for manufacturing a power device provided by an embodiment of the present invention.
[0018] Figure 6 A schematic structural diagram of steps for forming a first implantation region, a second implantation region and a third implantation region in a method for manufacturing a power device provided by an embodiment of the present invention.
[0019] Figure 7 A schematic structural diagram of a field oxide layer forming step in a method for manufacturing a power device provided by an embodiment of the present invention.
[0020] FIG. 8A to FIG. 8C A schematic structural diagram of a step of forming a contact metal layer in a method for manufacturing a power device provided by an embodiment of the present invention.
[0021] 9A to 9C A schematic structural diagram of a front metal layer forming step in a method for manufacturing a power device provided by an embodiment of the present invention.
[0022] Fig.10 A schematic structural diagram of a passivation layer forming step in a method for manufacturing a power device provided by an embodiment of the present invention.
[0023] [Description of Reference Numerals]
[0024] 10. Power device; 11. Semiconductor substrate; 110. Silicon carbide substrate; 112. Silicon carbide epitaxial layer; 11a. First injection region; 11b. Second injection region; 11c. Third injection region; 11e. Outer side of first injection region; 11f. Inner side of first injection region; 13. Field oxide layer; 13T. Upper surface of field oxide layer; 15. Contact metal layer; 15e. End surface of contact metal layer; 150. Metal material layer; 152. Bottom metal layer; 154. Top metal Layer; 15T, surface of contact metal layer; 17, front metal layer; 17e, end face of front metal layer; 17T, surface of front metal layer; 170, metal material layer; 18, passivation layer; 181, first stacked lateral segment; 182, first stacked longitudinal segment; 183, second stacked lateral segment; 184, second stacked longitudinal segment; 185, third stacked lateral segment; 19, protective layer; D1, D2, distance; CH, contact hole; PR1, photoresist layer; PR2, photoresist layer. DETAILED DESCRIPTION
[0025] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and easy to understand, the specific embodiments of the present invention are described in detail below with reference to the accompanying drawings.
[0026] In order to enable those skilled in the art to better understand the technical solution of the present invention, the technical solution in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative work should fall within the scope of protection of the present invention.
[0027] It should be noted that the terms "first", "second", etc. in the specification and claims of the present invention and the above-mentioned drawings are used to distinguish similar objects, and are not necessarily used to describe a specific order or sequence. It should be understood that the terms used in this way can be interchangeable where appropriate, so that the embodiments of the present invention described herein can be implemented in an order other than those illustrated or described herein. In addition, the terms "including" and "having" and any variations thereof are intended to cover non-exclusive inclusions, for example, a process, method, system, product or device that includes a series of steps or units is not necessarily limited to those steps or units that are clearly listed, but may include other steps or units that are not clearly listed or inherent to these processes, methods, products or devices.
[0028] It should also be noted that the division of multiple embodiments in the present invention is only for the convenience of description and should not constitute a special limitation. The features in various embodiments can be combined and referenced to each other without contradiction.
[0029] During the H3TRB reliability test, water vapor diffuses uniformly and passes through the plastic packaging material and protective layer (such as polyimide glue) of power devices such as SiC Schottky diode devices. The plastic packaging material and polyimide (PI) glue absorb water vapor and reach saturation.
[0030] On the one hand, the water vapor will be affected by the electric field between the terminal cutting path (where there is a positive voltage) and the front metal layer (where there is a negative voltage) and hydrolyze. Water molecules undergo oxidation reaction at the positive voltage to form a large number of hydrogen ions H + , the chemical equation occurring at positive voltage is (1):
[0031] 2H2O→O 2(g) +4H + +4e - … (1)
[0032] Water molecules are electrolyzed at negative voltage to generate a large amount of hydroxide ions OH - The chemical equation occurring at negative voltage is (2), thus forming an alkaline environment in the negative voltage region.
[0033]
[0034] On the other hand, the passivation layer of the device has high stress at the corners and is easy to break. When the passivation layer breaks, the alkaline water vapor continues to penetrate downward. In the presence of a field oxide layer, the composition of the field oxide layer is generally silicon dioxide, and the reaction of silicon dioxide and alkali will generate silicate ions. As a result, the passivation layer breaks and the field oxide layer also reacts. Eventually, the alkaline water vapor can invade the surface of the semiconductor substrate, such as the SiC substrate. The terminal structure here will be destroyed, the electric field will be distorted, and the device will experience increased reverse leakage or short circuit, and the H3TRB reliability of the device will fail. It is understandable that in the absence of a field oxide layer, when the passivation layer breaks, the alkaline water vapor will directly penetrate downward to the surface of the semiconductor substrate, such as the SiC substrate, causing the terminal structure here to be destroyed and the electric field to be distorted.
[0035] In view of this, the following embodiments of the present invention optimize the metal stacking method in the front electrode, and extend the lower metal layer that forms an electrical contact with the semiconductor substrate, such as a SiC substrate, such as a Schottky contact, outward by a certain distance compared to the upper metal layer. Even if the passivation layer is cracked and moisture penetrates, the lower metal layer also serves as a water vapor barrier layer to prevent water vapor from penetrating into the surface of the semiconductor substrate, such as a SiC substrate, that is, it can prevent water vapor from reacting with silicon carbide in the injection area, and the terminal electric field is protected, which can greatly improve the H3TRB reliability capability of the device.
[0036] An embodiment of the present invention provides a power device 10, which is, for example, a Schottky diode device, but the present invention is not limited thereto. Figure 1 and Figure 3 The power device 10 of this embodiment includes, for example, a semiconductor substrate 11 , a field oxide layer 13 , a contact metal layer 15 , a front metal layer 17 , a passivation layer 18 , and a protection layer 19 .
[0037] The semiconductor substrate 11 has an active region and a peripheral region surrounding the active region. As an example, the peripheral region includes a terminal region and a transition region between the terminal region and the active region, the transition region is configured with a first injection region 11a, and the active region is configured with a second injection region 11b. In other words, the semiconductor substrate 11 includes the active region, the transition region, and the terminal region in sequence from the inside to the outside.
[0038] The field oxide layer 13 is disposed on the semiconductor substrate 11 and forms a contact hole CH (refer to Figure 7 ) to expose the active area.
[0039] The contact metal layer 15 is disposed on the active region to form an electrical contact, such as a Schottky contact, with the semiconductor substrate 11, and extends from the active region toward the peripheral region. More specifically, the contact metal layer 15 is, for example, located in the contact hole CH and extends toward the peripheral region to a side of the field oxide layer 13 away from the semiconductor substrate 11 to partially overlap with the field oxide layer 13 to form a field plate structure. For example, the overlapping length of the contact metal layer 15 and the field oxide layer 13 is, for example, greater than 0 μm and less than or equal to 50 μm.
[0040] The front metal layer 17 is arranged on a side of the contact metal layer 15 away from the semiconductor substrate 11 and extends from the active area toward the peripheral area. The front metal layer 17 has an end face 17e (or side wall) facing the terminal area of the peripheral area, and the contact metal layer 15 has an end face 15e (or side wall) facing the terminal area, and the end face 17e is retracted relative to the end face 15e, that is, it has a non-zero distance D1 (D1>0μm).
[0041] The passivation layer 18 is disposed on the semiconductor substrate 11, and covers the contact metal layer 15 and the front metal layer 17 and exposes at least a portion of the surface 17T of the front metal layer 17 (for example, the upper surface away from the semiconductor substrate 11), and specifically may expose the entire surface 17T, or the central portion of the surface 17T. The material of the passivation layer 18 is typically an inorganic material. More specifically, the passivation layer 18 may extend from the surface 13T of the field oxide layer 13 (for example, the upper surface away from the semiconductor substrate 11) toward the active area to the surface 17T of the front metal layer 17. As an example, the thickness of the passivation layer 18 ranges from 0.8 μm to 1.5 μm, and the lateral width of the passivation layer 18 covering the surface 17T of the front metal layer 17 ranges from 2 μm to 100 μm.
[0042] The protective layer 19 is disposed on the semiconductor substrate 11, wherein the protective layer 19 covers the passivation layer 18 and exposes at least a portion of the surface 17T of the front metal layer 17. For example, the material of the protective layer 19 is an organic material, such as polyimide, but the embodiment of the present invention is not limited thereto. For example, the thickness of the protective layer 19 ranges from 3.5 μm to 12 μm.
[0043] The embodiment of the present invention adopts structural design so that the contact metal layer 15 that does not react with water vapor extends outward by a certain distance compared with the end face 17e of the front metal layer 17, that is, the end face 17e of the front metal layer 17 is retracted relative to the end face 15e of the contact metal layer 15. The contact metal layer 15 here plays the function of a water vapor barrier layer, which can prevent water vapor from penetrating into the surface of the semiconductor substrate 11 even if the corner of the passivation layer 18 (such as the passivation layer corresponding to the connection between the end face 17e and the end face 15e) is broken due to excessive stress, thereby improving the H3TRB and other moisture resistance reliability capabilities of the power device 10. It is worth mentioning that the contact metal layer 15 of this embodiment can also serve as a Schottky contact layer and a water vapor barrier layer, and thus has multiple functions.
[0044] In some embodiments, see Figure 1, the contact metal layer 15 extends from the active region toward the peripheral region to cover the first injection region 11a. For example, the first injection region 11a has an outer side surface 11e facing the terminal region of the peripheral region and an inner side surface 11f facing the active region. In the lateral direction from the active region to the terminal region, the end surface 15e of the contact metal layer 15 is located between the end surface 17e of the front metal layer 17 and the outer side surface 11e of the first injection region 11a. Typically, the end surface 15e of the contact metal layer 15 is located directly above the first injection region 11a and is retracted relative to the outer side surface 11e of the first injection region 11a, that is, it has a non-zero distance D2 (D2>0μm).
[0045] In some embodiments, see Figure 1 In the lateral direction from the active area to the terminal area, the distance D1 between the end surface 17e of the front metal layer 17 and the end surface 15e of the contact metal layer 15 is, for example, greater than 1 μm (micrometer), so as to ensure that the contact metal layer 15 extends outwardly by a sufficiently large distance relative to the end surface 17e of the front metal layer 17, thereby more effectively ensuring the water vapor barrier effect of the contact metal layer 15 as a water vapor barrier layer.
[0046] In some embodiments, see Figure 1 In the lateral direction from the active area to the terminal area, the distance between the end face 15e of the contact metal layer 15 and the outer side face 11e of the first injection area 11a is, for example, greater than 1 μm, so as to more effectively ensure that the end face 15e of the contact metal layer 15 is located directly above the first injection area 11a and has a sufficiently large distance from the outer side face 11e of the first injection area 11a, thereby more effectively ensuring that the position design of the end face 15e of the contact metal layer 15 will not significantly affect the electric field of the terminal structure.
[0047] In some embodiments, see Figure 1 In the direction from the semiconductor substrate 11 to the contact metal layer 15, the thickness of the contact metal layer 15 is, for example, greater than 0.1 μm and less than 3 μm, so as to more effectively prevent the contact metal layer 15 from breaking, thereby forming a more stable barrier layer that does not react with water vapor in the path of water vapor intrusion.
[0048] In some embodiments, see Figure 1The thickness of the front metal layer 17 is, for example, greater than 2 μm, and the thickness of the front metal layer 17 is greater than the thickness of the contact metal layer 15, so as to serve as a thickened metal layer of the front electrode (including the contact metal layer 15 and the front metal layer 17) of the power device 10. The front metal layer 17 herein may also be referred to as an anode metal layer. As an example, the front metal layer 17 includes but is not limited to any one or a combination of multiple metals such as aluminum (Al), silver (Ag), copper (Cu), and a metal solid solution formed by any one or more metals such as Al, Ag, Cu, and elements such as nitrogen (N) and silicon (Si).
[0049] In some embodiments, see Figure 1 The contact metal layer 15 is, for example, a single-layer metal layer, which forms a Schottky contact with the semiconductor substrate 11 and also serves as a water vapor barrier layer. For example, the material of the single-layer metal layer can be one or more of titanium (Ti), titanium nitride (TiN), titanium tungsten alloy (TiW), W, tantalum (Ta), nickel (Ni), etc., which can serve as both a Schottky contact layer and a water vapor barrier layer. In this embodiment, by designing the contact metal layer 15 as a single-layer metal layer, it can simplify the process and reduce the cost.
[0050] In some embodiments, see Figure 2 , the contact metal layer 15 is a multi-layer metal layer, for example, including a bottom metal layer 152 adjacent to the semiconductor substrate 11 and a top metal layer 154 away from the semiconductor substrate 11. The bottom metal layer 152 forms a Schottky contact with the semiconductor substrate 11, and the top metal layer 154 serves as a water vapor barrier. As an example, the material of the bottom metal layer is a Schottky metal such as molybdenum (Mo) and Al, which can be one or more of Mo and Al; the top metal layer includes but is not limited to iridium (Ir), Ta, ruthenium (Ru), rhodium (Rh), niobium (Nb), osmium (Os), platinum (Pt), gold (Au), Ti, W, etc., which can be one or more of Ir, Ta, Ru, Rh, Nb, Os, Pt, Au, Ti and W. In this embodiment, by designing the contact metal layer 15 into a multi-layer metal structure, it allows different layers to fully play their respective functions, such as the bottom metal layer as a Schottky contact layer and the top metal layer as a water vapor barrier, and the material selection range of the contact metal layer 15 is wider.
[0051] In some embodiments, see Figure 1The semiconductor substrate 11 is, for example, a SiC substrate, which includes a silicon carbide substrate 110 and a silicon carbide epitaxial layer 112 disposed on the silicon carbide substrate 110. The doping concentration of the silicon carbide epitaxial layer 112 is lower than the doping concentration of the silicon carbide substrate 110. For example, the doping concentration of the silicon carbide substrate 110 is 1E19-5E20 / cm 3 , the corresponding silicon carbide substrate 110 is n + SiC substrate; the doping concentration of the silicon carbide epitaxial layer 112 is 5E15-5E16 / cm 3 , the corresponding silicon carbide epitaxial layer 112 is n - The first implantation region 11a and the second implantation region 11b extend from the surface of the silicon carbide epitaxial layer 112 to the silicon carbide substrate 110, respectively. The conductivity type of the silicon carbide epitaxial layer 112 (for example, n - ), which is different from the conductivity type of the silicon carbide substrate 110 (for example, n + ) and has the same conductivity type as the first implantation region 11a and the second implantation region 11b (for example, p + ) are different.
[0052] In some embodiments, see Figure 1 The crystal form of the silicon carbide substrate is, for example, 4H SiC, and the thickness of the silicon carbide substrate 110 is greater than the thickness of the silicon carbide epitaxial layer 112. For example, the thickness of the silicon carbide substrate 110 is in the range of 250 μm to 350 μm, and the thickness of the silicon carbide epitaxial layer 112 is in the range of 5 μm to 40 μm.
[0053] In some embodiments, see Figure 1 The terminal region of the semiconductor substrate 11 is provided with a third implantation region 11c, the third implantation region 11c extends from the surface of the silicon carbide epitaxial layer 112 to the silicon carbide substrate 110, and the third implantation region 11c, the first implantation region 11a and the second implantation region 11b have the same conductivity type, for example, all are p + In this embodiment, the third injection region 11c is added to play the role of a voltage divider and helps to reduce the curvature of the main junction depletion region. Figure 1 As shown in the figure, the number of the third injection region 11c is multiple and the shape is ring-shaped, the number of the first injection region 11a is one and the shape is ring-shaped, the number of the second injection region 11b is three and the shape includes but is not limited to strip, square, hexagon or other combination structures. It should be noted that the third injection region 11c, the first injection region 11a and the second injection region 11b can be formed simultaneously by ion implantation, for example, the implantation concentration range is 1E17 ~ 5E18 / cm 3; It can also be formed by using different ion implantation concentrations; Therefore, the depth, width, and implantation concentration of the third implantation region 11c, the first implantation region 11a, and the second implantation region 11b can be designed using existing mature technologies and are not specifically limited here. In addition, it is worth mentioning that the size of the transition region can be determined by Figure 1 The outer side surface 11e and the inner side surface 11f of the continuous first injection region 11a are jointly defined, and accordingly, the size of the active region can be defined by the inner side surface 11f of the first injection region 11a; in other embodiments, when the first injection region 11a in the transition region includes multiple discontinuous sub-regions, the transition region can be jointly defined by the inner side surface of the innermost sub-region and the outer side surface of the outermost sub-region, and accordingly, the size of the active region can be defined by the inner side surface of the innermost sub-region.
[0054] In some embodiments, see Figure 1 and Figure 3 The passivation layer 18 extends from the surface 13T of the field oxide layer 13 toward the active area to the surface 17T of the front metal layer 17. For example, it is a multilayer stacked structure composed of multiple different inorganic material layers, and includes a first stacked transverse section 181, a first stacked longitudinal section 182, a second stacked transverse section 183, a second stacked longitudinal section 184, and a third stacked transverse section 185 in sequence. The first stacked transverse section 181 contacts and covers the surface 13T of the field oxide layer 13. The first stacked longitudinal section 182 connects the first stacked transverse section 181 and the second stacked transverse section 183 and contacts and covers the end surface 15e of the contact metal layer 15. The second stacked transverse section 183 contacts and covers the surface 15T of the contact metal layer 15. The second stacked longitudinal section 184 connects the second stacked transverse section 183 and the third stacked transverse section 185 and contacts and covers the end surface 17e of the front metal layer 17. The third stacked transverse section 185 contacts and covers the surface 17T of the front metal layer 17. For example, the passivation layer 18 with a multi-layer stacking structure can be a layer stacking structure of silicon oxide and silicon nitride or silicon oxynitride. It is understandable that in some practical applications, the passivation layer 18 can also be a single inorganic material layer, such as a silicon oxide layer, a silicon nitride layer, or a silicon oxynitride layer. However, the passivation layer 18 with a multi-layer stacking structure has better structural performance and water vapor resistance.
[0055] See also Figure 4 Another embodiment of the present invention provides a power device, which Figure 1 The structures of the power devices 10 shown are basically the same, and the main differences are: Figure 4The power device shown is not provided with a field oxide layer. Accordingly, the passivation layer extends from the surface of the terminal region of the semiconductor substrate 11 toward the active region to the surface 17T of the front metal layer 17 and exposes at least a portion of the surface 17T of the front metal layer 17 .
[0056] Another embodiment of the present invention provides a method for manufacturing a power device, which is, for example, a method for manufacturing a Schottky diode device. Figures 5 to 10 The method for manufacturing the power device of this embodiment includes, for example, the following steps.
[0057] First, see Figure 5 , obtaining a semiconductor substrate 11, wherein the semiconductor substrate 11, for example, includes a silicon carbide substrate 110 and a silicon carbide epitaxial layer 112 formed on the silicon carbide substrate 110, the crystal form of the silicon carbide substrate 110, for example, is 4H SiC, the thickness of the silicon carbide substrate 110, for example, ranges from 250 μm to 350 μm, and the doping concentration ranges from 1E19 to 5E20 / cm 3 The thickness of the silicon carbide epitaxial layer 112 is, for example, in the range of 5 μm to 40 μm, and the doping concentration is, for example, in the range of 5E15 to 5E16 / cm 3 That is, the thickness of the silicon carbide substrate 110 is greater than the thickness of the silicon carbide epitaxial layer 112 , and the doping concentration of the silicon carbide substrate 110 is greater than the doping concentration of the silicon carbide epitaxial layer 112 .
[0058] Next, see Figure 6 , extending from the surface of the silicon carbide epitaxial layer 112 to the silicon carbide substrate 110 by ion implantation, so as to configure a first implantation region 11a in the transition region of the SiC epitaxial layer 112 of the semiconductor substrate 11, a second implantation region 11b in the active region, and a third implantation region 11c in the terminal region; wherein the first implantation region 11a, the second implantation region 11b and the third implantation region 11c have the same conductivity type (for example, p-type, which can be p + ), and the conductivity type of the silicon carbide substrate and the silicon carbide epitaxial layer (for example, n-type, which can be n + 、n - ) are different; the first injection region 11a, the second injection region 11b and the third injection region 11c have, for example, the same injection depth and injection concentration (e.g., 1E17-5E18 / cm 3 ); As for the process parameters of ion implantation, it can adopt the existing mature technology, so it will not be described here. In addition, for example, Figure 6As shown in the example, the number of the third injection area 11c is multiple and the shape is ring-shaped, the number of the first injection area 11a is one and the shape is ring-shaped, and the number of the second injection area 11b is three, and the shape includes but is not limited to strip, square, hexagon or other combination structures. It should be noted that the third injection area 11c, the first injection area 11a and the second injection area 11b can be formed simultaneously by ion implantation, or can be formed separately by using different ion implantation concentrations; therefore, the depth, width and implantation concentration of the third injection area 11c, the first injection area 11a and the second injection area 11b can be flexibly designed according to the specific situation, and no specific restrictions are made here.
[0059] Then, see Figure 7 , a field oxide layer 13 having a contact hole CH is formed on the silicon carbide epitaxial layer 112, wherein the contact hole CH exposes the active area. Specifically, a material layer (such as a silicon dioxide layer) with a thickness in the range of 0.6 μm to 1.2 μm can be deposited on the upper surface of the silicon carbide epitaxial layer 112 by chemical vapor deposition (CVD), and then the field oxide layer 13 is formed by a wet etching process, but the embodiment of the present invention is not limited thereto, for example, the field oxide layer 13 can also be a multilayer stacked structure of a thermal oxide layer and a CVD deposited oxide layer.
[0060] Next, see FIG. 8A to FIG. 8C A contact metal layer 15 is formed in the active region to form an electrical contact, such as a Schottky contact, with the semiconductor substrate 11, and the contact metal layer 15 extends from the active region toward the transition region. Typically, the contact metal layer 15 is, for example, located in the contact hole CH and extends toward the transition region to a side of the field oxide layer 13 away from the silicon carbide epitaxial layer 112 to partially overlap with the field oxide layer 13 to form a field plate structure.
[0061] Specifically, a metal material layer 150 (eg, Fig. 8A As shown in FIG. 1 , the metal material layer 150 may be composed of one or two layers. A single layer may be one or more of Ti, TiN, TiW, W, Ta, and Ni, which may serve as both a Schottky contact layer and a water vapor barrier layer; two layers of metal may be a bottom layer of a Schottky metal such as Mo or Al plus a water vapor barrier layer of metal including but not limited to Ir, Ta, Ru, Rh, Nb, Os, Pt, Au, Ti, W, and the like.
[0062] Then, a photoresist material is coated on the metal material layer 150. The thickness of the formed photoresist material layer is, for example, in the range of 2 μm to 6 μm. By adjusting the exposure range, a photoresist layer PR1 (eg, Figure 8B shown).
[0063] Then, for example, by dry etching, the metal material layer 150 is etched and the photoresist layer PR1 is removed; Figure 8C As shown, the end surface 15e of the contact metal layer 15 formed after etching overlaps the plane of the field oxide layer 13, for example, the overlapping length of the contact metal layer 15 and the field oxide layer 13 is greater than 0 μm and less than or equal to 50 μm. Figure 8C It can be known that the end surface 15e of the contact metal layer 15 is located directly above the first injection region 11a and is retracted relative to the outer side surface 11e of the first injection region 11a to form a non-zero distance D2 therebetween.
[0064] Afterwards, see 9A to 9C A front metal layer 17 is formed on the side of the contact metal layer 15 away from the silicon carbide epitaxial layer 112, and the front metal layer 17 extends from the active area toward the transition area; wherein the end surface 17e of the front metal layer 17 is retracted relative to the end surface 15e of the contact metal layer 15.
[0065] Specifically, a metal material layer 170 (eg, Fig. 9A As shown), the metal material layer 170 includes but is not limited to any one or a combination of multiple metals such as Al, Ag, Cu, and a metal solid solution formed by any one or multiple metals such as Al, Ag, Cu, and elements such as N and Si.
[0066] Then, a photoresist material is coated on the metal material layer 170. The thickness of the formed photoresist material layer is, for example, in the range of 2 μm to 6 μm. By adjusting the exposure range, a photoresist layer PR2 (eg, Fig. 9B shown).
[0067] Then, for example, by dry etching, the metal material layer 170 is etched and the photoresist layer PR2 is removed; Fig. 9C As shown, the end surface 17e of the front metal layer 17 formed after etching is retracted relative to the end surface 15e of the contact metal layer 15 to form a non-zero distance D1 between the two.
[0068] Next, see Fig.10, a passivation layer 18 is formed on the silicon carbide epitaxial layer 112, wherein the passivation layer 18 extends from the surface of the field oxide layer 13 toward the active area to the surface 17T of the front metal layer 17 to cover the end face 15e of the contact metal layer 15 and the end face 17e of the front metal layer 17 and expose at least a portion of the surface 17T of the front metal layer 17. Specifically, the passivation layer 18 can be formed by CVD deposition combined with a photolithography process, and can be deposited using any one or more dielectric stacks such as silicon oxide, silicon nitride, and silicon oxynitride, with a thickness ranging from 0.8 μm to 1.5 μm, for example, and the lateral width of the passivation layer 18 covering the surface 17T of the front metal layer 17 is, for example, between 2 μm and 100 μm.
[0069] Then, a protective layer 19 is formed on the silicon carbide epitaxial layer 112, wherein the protective layer 19 covers the passivation layer 18 and exposes at least a portion of the surface 17T of the front metal layer 17. Figure 1 The power device 10 shown is shown. Specifically, polyimide can be spin-coated on the passivation layer 18, and the protection layer 19 can be formed after exposure and baking. The thickness of the protection layer 19 is, for example, in the range of 3.5 μm to 12 μm.
[0070] In addition, for Figure 4 The manufacturing method of the power device shown without a field oxide layer can refer to the aforementioned manufacturing method, except that the step of forming the field oxide layer is omitted, so it will not be repeated here.
[0071] In addition, it is worth mentioning that when the power device 10 is a Schottky diode device, those skilled in the art will understand that a back electrode is usually formed on the back side of the semiconductor substrate 11 (for example, the side of the silicon carbide substrate 110 away from the silicon carbide epitaxial layer 112), and the back electrode here includes, for example, a cathode metal layer and an ohmic contact layer located between the semiconductor substrate 11 and the cathode metal layer, and the ohmic contact layer is formed, for example, by electron beam evaporation or sputtering deposition of nickel metal and then annealing, and the cathode metal layer is, for example, a TiNiAg metal layer formed by deposition, but the embodiments of the present invention are not limited thereto.
[0072] The above description is only a preferred embodiment of the present invention and does not limit the present invention in any form. Although the present invention has been disclosed as a preferred embodiment as above, it is not used to limit the present invention. Any technician familiar with this profession can make some changes or modifications to equivalent embodiments of equivalent changes using the technical contents disclosed above without departing from the scope of the technical solution of the present invention. However, any simple modification, equivalent change and modification made to the above embodiments based on the technical essence of the present invention without departing from the content of the technical solution of the present invention still fall within the scope of the technical solution of the present invention.
Claims
1. A power device, characterized in that: include: A semiconductor substrate having an active region and a peripheral region surrounding the active region; a contact metal layer, disposed on the active area to form an electrical contact with the semiconductor substrate and extending from the active area toward the peripheral area; a front metal layer, arranged on a side of the contact metal layer away from the semiconductor substrate and extending from the active area toward the peripheral area, wherein an end surface of the front metal layer is indented relative to an end surface of the contact metal layer; A passivation layer is disposed on the semiconductor substrate, wherein the passivation layer covers the contact metal layer and the front metal layer and exposes at least a portion of the surface of the front metal layer, and the material of the passivation layer is an inorganic material; as well as A protection layer is disposed on the semiconductor substrate, wherein the protection layer covers the passivation layer and exposes at least a portion of the surface of the front metal layer.
2. The power device according to claim 1, characterized in that: The peripheral region includes a terminal region and a transition region between the terminal region and the active region, the transition region is configured with a first implant region, and the contact metal layer extends from the active region toward the peripheral region to cover the first implant region.
3. The power device according to claim 2, characterized in that: The first injection region has an outer side surface facing the terminal region, the end surface of the contact metal layer faces the terminal region, and the end surface of the front metal layer faces the terminal region, and in the lateral direction from the active region to the terminal region, the end surface of the contact metal layer is located between the end surface of the front metal layer and the outer side surface of the first injection region.
4. The power device according to claim 3, characterized in that: In the lateral direction, a distance between an end surface of the contact metal layer and an end surface of the front metal layer is greater than 1 micrometer.
5. The power device according to claim 3, characterized in that: In the lateral direction, a distance between an end surface of the contact metal layer and an outer side surface of the first injection region is greater than 1 micrometer.
6. The power device according to claim 1, characterized in that: In a direction from the semiconductor substrate to the contact metal layer, the thickness of the contact metal layer is greater than 0.1 micrometers and less than 3 micrometers.
7. The power device according to claim 6, characterized in that: The thickness of the front metal layer is greater than 2 micrometers, and the thickness of the front metal layer is greater than the thickness of the contact metal layer.
8. The power device according to claim 1, characterized in that: The contact metal layer is a single-layer metal layer, which forms a Schottky contact with the semiconductor substrate and also serves as a water vapor barrier layer.
9. The power device according to claim 1, characterized in that: The contact metal layer is a multi-layer metal layer, in which a bottom metal layer adjacent to the semiconductor substrate forms a Schottky contact with the semiconductor substrate, and a top metal layer away from the semiconductor substrate serves as a water vapor barrier layer.
10. The power device according to claim 2, characterized in that: The semiconductor substrate includes a silicon carbide substrate and a silicon carbide epitaxial layer arranged on the silicon carbide substrate, the doping concentration of the silicon carbide epitaxial layer is lower than the doping concentration of the silicon carbide substrate, the active area is configured with a second injection area, the second injection area extends from the surface of the silicon carbide epitaxial layer to the silicon carbide substrate, the terminal area is configured with a third injection area, the third injection area extends from the surface of the silicon carbide epitaxial layer to the silicon carbide substrate, and the conductivity type of the silicon carbide epitaxial layer is the same as the conductivity type of the silicon carbide substrate and different from the conductivity types of the first injection area, the second injection area and the third injection area.
11. The power device according to any one of claims 1 to 10, characterized in that: It also includes a field oxide layer, which is arranged on the semiconductor substrate and forms a contact hole to expose the active area, the contact metal layer is located in the contact hole and extends toward the peripheral area to the side of the field oxide layer away from the semiconductor substrate to partially overlap with the field oxide layer, and the passivation layer extends from the surface of the field oxide layer toward the active area to the surface of the front metal layer.
12. The power device according to claim 11, characterized in that: The passivation layer is a multilayer stacked structure composed of multiple different inorganic material layers, and includes a first stacked transverse segment, a first stacked longitudinal segment, a second stacked transverse segment, a second stacked longitudinal segment, and a third stacked transverse segment in sequence. The first stacked transverse segment contacts and covers the surface of the field oxide layer, the first stacked longitudinal segment connects the first stacked transverse segment and the second stacked transverse segment and contacts and covers the end surface of the contact metal layer, the second stacked transverse segment contacts and covers the surface of the contact metal layer away from the semiconductor substrate, the second stacked longitudinal segment connects the second stacked transverse segment and the third stacked transverse segment and contacts and covers the end surface of the front metal layer, and the third stacked transverse segment contacts and covers the surface of the front metal layer away from the semiconductor substrate.
Citation Information
Cited By
Semiconductor device and power device
WO2026143398A1