Ultra-slender flexible temperature sensor and manufacturing method thereof
Through high-temperature thermosetting adhesive pressing and multi-process processing, the ultra-fine flexible temperature sensor is formed, which solves the problem of low bonding force of the temperature sensor and material in minimally invasive equipment, and achieves efficient and accurate temperature monitoring and low-cost large-scale batches Production.
Patent Information
- Application Number
- CN202411161606.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-22
- Publication Date
- 2024-11-08
AI Technical Summary
When used in minimally invasive equipment, existing temperature sensors are difficult to adapt to narrow spaces and efficient production due to the coarse product and low material bonding force, and the processing cost is high, which affects the temperature monitoring accuracy and production efficiency of minimally invasive equipment.
The high-temperature thermosetting adhesive press bonding process is used to bond non-pure copper metal and flexible substrate into different metal layers on both sides. The ultra-fine flexible temperature sensor is formed through drilling, chemical copper deposition, electroplating, film removal and etching processes. Combining the PI insulating film and protective film, conduction connection and insulation protection are achieved.
It realizes the production of ultra-slim temperature sensors, suitable for installation in narrow spaces, fast reaction speed, high detection accuracy, and low production process cost, making it suitable for large-scale production.
Smart Images

Figure CN118921879A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the application field of flexible circuit boards, and in particular to an ultra-slender flexible temperature sensor and a manufacturing method thereof. Background Art
[0002] Some surgical medical devices, such as minimally invasive ones, may generate heat when they come into contact with tissues. Once the temperature approaches or exceeds the threshold that the tissue can withstand, it can alert the doctor to adjust the operation to prevent tissue damage. Therefore, temperature sensors are needed for real-time monitoring.
[0003] Conventional temperature sensors:
[0004] 1. The product is thick when two kinds of metal wires are welded, which is not conducive to the application of minimally invasive devices in small spaces.
[0005] 2. The two metal conductors are deposited on the flexible substrate using a sputtering process or an inkjet process. The material bonding force is low, and the processing cost is high and the efficiency is low, which is not conducive to mass production. Summary of the invention
[0006] In order to solve the application problem of temperature sensors in minimally invasive devices, the present invention provides an ultra-slender flexible temperature sensor and a manufacturing method thereof. The specific technical solution is as follows:
[0007] Based on the first aspect of the present invention, a method for manufacturing an ultra-slender flexible temperature sensor is provided, comprising:
[0008] Step S1: using a high-temperature thermosetting adhesive, through a lamination process, the impure copper metal, the flexible substrate, and the pure copper are bonded together to form an elongated substrate with different metal layers on both sides;
[0009] Step S2: forming a via hole at one end of the composite board after step S1 by using a drilling process;
[0010] Step S3: using a chemical copper deposition process to deposit a layer of chemical copper on the surface of the composite board and the hole wall after step S2 to form a copper deposition layer, connecting the two sides of the substrate; and using an oven to quickly dry the product;
[0011] Step S4: applying anti-plating photosensitive dry film to the front and back of the composite board after step S3, and forming dry film openings in the conductive hole area and the pad area where the via hole is located through exposure and development; the via hole and the pad area are located at two ends of the elongated substrate;
[0012] Step S5: copper plating is added to the exposed metal area of the composite board after step S4 through a copper electroplating process, so that a copper plating layer is formed on the via hole area and the pad area, and the front and back metal layers form a conductive connection;
[0013] Step S6: using a film removal process to remove the dry film on the surface of the composite board after step S5, and then using a micro-etching process to remove the copper layer exposed on the surface, exposing the impure copper metal, forming a pure copper layer on one side and an impure copper metal layer on the other side, and the two sides are conductive;
[0014] Step S7: attaching a photosensitive dry film to the front and back surfaces of the composite board after step S6, and forming front and back circuits through exposure, development, and etching;
[0015] Step S8: After step S7, protective films are attached to the front and back sides of the composite board to insulate the circuits, and windows are opened in the pad areas and temperature collection areas on the front and back sides; the temperature collection area is the conductive hole area on the back side.
[0016] Furthermore, the non-pure copper metal is constantan.
[0017] Furthermore, the nickel-copper ratio of the constantan is 45:55 or 40:60.
[0018] Furthermore, the pressing parameters of step S1 are: temperature 180 degrees, time 180 seconds, and pressure 50kg / cm2.
[0019] Furthermore, the flexible substrate in step S1 is PI material.
[0020] Furthermore, the drilling process in step S2 is CNC mechanical drilling or laser drilling.
[0021] Furthermore, in step S4 and step S7, the anti-plating photosensitive dry film is exposed and developed by laser direct imaging technology or mask.
[0022] Furthermore, the protective film in step S8 is a PI protective film.
[0023] Furthermore, after step S8, the process further includes performing an anti-oxidation surface treatment on the pads in the window area of the protective film.
[0024] Based on the second aspect of the present invention, an ultra-slender flexible temperature sensor is provided, which is manufactured by using the manufacturing method of the ultra-slender flexible temperature sensor as described in any one of the above items.
[0025] The present invention achieves the following technical effects:
[0026] 1. It can realize ultra-slender temperature sensors, and the products can be installed and applied in narrow spaces, which is conducive to improving the capabilities of minimally invasive medical equipment;
[0027] 2. The temperature sampling point can be closely attached to the heating area, with fast response speed and high detection accuracy;
[0028] 3. The surface adopts PI insulation film, which has high insulation withstand voltage strength and can adapt to various complex environmental requirements;
[0029] 4. The product production process has low cost and high degree of automation, which is suitable for mass production. BRIEF DESCRIPTION OF THE DRAWINGS
[0030] Figure 1 This is the production process flow chart of the ultra-slender flexible temperature sensor;
[0031] Figure 2 is a schematic diagram of the stacking of the product after step S1;
[0032] Figure 3 is a schematic diagram of the stacking of the product after step S2;
[0033] Figure 4 is a schematic diagram of the stacking of the product after step S3;
[0034] Figure 5 is a schematic diagram of the stacking of the product after step S4;
[0035] Figure 6 is a schematic diagram of the stacking of the product after step S5;
[0036] Figure 7 is a schematic diagram of the stacking of the product after step S6;
[0037] Figure 8 is a schematic diagram of the front and back surfaces of the product after step S7;
[0038] Fig. 9 It is a schematic diagram of the front and back surfaces of the product after step S8. DETAILED DESCRIPTION
[0039] To further illustrate the various embodiments, the present invention provides drawings. These drawings are part of the disclosure of the present invention, which are mainly used to illustrate the embodiments and can be used in conjunction with the relevant descriptions in the specification to explain the operating principles of the embodiments. With reference to these contents, a person of ordinary skill in the art should be able to understand other possible implementations and advantages of the present invention. The components in the figures are not drawn to scale, and similar component symbols are generally used to represent similar components.
[0040] The present invention will now be further described with reference to the accompanying drawings and specific implementation methods.
[0041] The present invention provides a method for manufacturing an ultra-slender flexible temperature sensor, such as Figures 1 to 9 As shown, it includes lamination, drilling, copper deposition, dry film windowing, electroplating, film stripping, circuit etching and protective film application. The specific description of each processing technology is as follows:
[0042] Step S1: using high temperature thermosetting adhesives 2 and 4, through a hot press lamination process, the impure copper metal 1, the flexible substrate 3, and the pure copper 5 are bonded together to form a double-sided different metal layer substrate, such as Figure 2 As shown. The flexible substrate 3 is preferably made of PI (polyimide) material; the non-pure copper metal 1 is preferably constantan; the nickel-copper ratio of the constantan is preferably 45:55 or 40:60; the non-pure copper metal 1 can also be replaced by nickel or other non-copper metals. In this process, the preferred pressing parameters are: temperature 180°C, time 180 seconds, and pressure 50kg / cm2.
[0043] Step S2: Use CNC mechanical drilling or laser drilling to form a via hole 6 at one end of the product. Figure 3 shown.
[0044] Step S3: A thin layer of chemical copper is deposited on the surface of the product and the wall of the via hole 6 by using a chemical copper deposition process to form a copper deposition layer 7, and an oven is used to quickly dry the product. Figure 4 The preferred baking parameters are: temperature 80°C, time 30 minutes, to prevent the deposited thin copper from being oxidized due to the residual moisture left for too long.
[0045] Step S4: A photosensitive dry film 8 is applied to the front and back of the product, and is exposed and developed by LDI (laser direct imaging technology) or mask, so as to form dry film openings at the via hole areas 11, 12 where the via hole 6 is located and the set pad areas 9, 10, such as Figure 5 shown.
[0046] Step S5: electroplating. Through the copper electroplating process, copper plating is added to the exposed metal areas of the product (the via areas 11, 12 and the pad areas 9, 10), so that a copper plating layer 13 is formed on the via areas 11, 12 and the pad areas 9, 10, and the front and back metal layers form a conductive connection, such as Figure 6 shown.
[0047] Step S6: Use a film removal process to remove the surface dry film, and then use a micro-etching process to remove the copper layer 7 exposed on the surface, exposing the impure copper metal 1, forming a pure copper layer on one side and an impure copper metal layer on the other side, and the two sides are conductive, such as Figure 7 shown.
[0048] Step S7: attaching photosensitive dry film to the front and back sides, exposing through LDI or mask, developing, and then etching to form front and back circuits, such as Figure 8As shown. In order to make the product thinner, the front and back lines are arranged in an overlapping manner. According to the product structure, the line width is preferably 0.1mm~0.3mm, and the outer width can be 0.2mm~0.5mm. Since the metal materials of the front and back lines are different, a thermocouple node is formed at the via area 12. When the temperature of the via areas 11 and 12 is different from the temperature of the pad areas 9 and 10, a potential difference will be formed between the front and back lines of the product. The temperature difference can be confirmed by monitoring the voltage change between the two pad areas 9 and 10, thereby realizing temperature monitoring.
[0049] Step S8: Fig. 9 As shown, a protective film 14 is attached to the front and back sides to insulate the circuit, and windows are opened in the temperature sampling area where the pad area 9, 10 and the via area 11 are located. The window in the temperature sampling area is conducive to contact with the temperature sampling point for rapid heat conduction, improving the timeliness of temperature response, and the window in the pad area is used as a signal output end. At the same time, the pad in the window area can be surface treated, preferably chemical nickel gold, to avoid pad oxidation, to ensure temperature sensing accuracy and reliable welding. The material of the protective film 14 is preferably PI (polyimide) material. PI material has the characteristics of high temperature resistance, electrical insulation and high mechanical strength.
[0050] The present invention also provides an ultra-slender flexible temperature sensor, which is manufactured based on the processing flow of the above-mentioned manufacturing method.
[0051] Advantages of this product:
[0052] 1. It can realize ultra-slender temperature sensors, and the products can be installed and applied in narrow spaces, which is conducive to improving the capabilities of minimally invasive medical equipment;
[0053] 2. The temperature sampling point can be closely attached to the heating area, with fast response speed and high detection accuracy;
[0054] 3. The surface adopts PI insulation film, which has high insulation withstand voltage strength and can adapt to various complex environmental requirements;
[0055] 4. The product production process has low cost and high degree of automation, which is suitable for mass production
[0056] Although the present invention has been specifically shown and described in conjunction with the preferred embodiments, it should be understood by those skilled in the art that various changes may be made to the present invention in form and details without departing from the spirit and scope of the present invention as defined by the appended claims, all of which are within the scope of protection of the present invention.
Claims
1. A method for manufacturing an ultra-slender flexible temperature sensor, characterized in that: include: Step S1: using a high-temperature thermosetting adhesive, through a lamination process, the impure copper metal, the flexible substrate, and the pure copper are bonded together to form an elongated substrate with different metal layers on both sides; Step S2: forming a via hole at one end of the composite board after step S1 by using a drilling process; Step S3: using a chemical copper deposition process to deposit a layer of chemical copper on the surface of the composite board and the hole wall after step S2 to form a copper deposition layer, connecting the two sides of the substrate; and using an oven to quickly dry the product; Step S4: applying anti-plating photosensitive dry film to the front and back of the composite board after step S3, and forming dry film openings in the conductive hole area and the pad area where the via hole is located through exposure and development; the via hole and the pad area are located at two ends of the elongated substrate; Step S5: copper plating is added to the exposed metal area of the composite board after step S4 through a copper electroplating process, so that a copper plating layer is formed on the via hole area and the pad area, and the front and back metal layers form a conductive connection; Step S6: using a film removal process to remove the dry film on the surface of the composite board after step S5, and then using a micro-etching process to remove the copper layer exposed on the surface, exposing the impure copper metal, forming a pure copper layer on one side and an impure copper metal layer on the other side, and the two sides are conductive; Step S7: attaching a photosensitive dry film to the front and back surfaces of the composite board after step S6, and forming front and back circuits through exposure, development, and etching; Step S8: After step S7, protective films are attached to the front and back sides of the composite board to insulate the circuits, and windows are opened in the pad areas and temperature collection areas on the front and back sides; the temperature collection area is the conductive hole area on the back side.
2. The method for manufacturing the ultra-slender flexible temperature sensor according to claim 1, characterized in that: The impure copper metal is constantan.
3. The method for manufacturing the ultra-slender flexible temperature sensor according to claim 2, characterized in that: The nickel-copper ratio of the constantan is 45:55 or 40:
60.
4. The method for manufacturing the ultra-slender flexible temperature sensor according to claim 1, characterized in that: The pressing parameters of step S1 are: temperature 180 degrees, time 180 seconds, and pressure 50 kg / cm2.
5. The method for manufacturing the ultra-slender flexible temperature sensor according to claim 1, characterized in that: The flexible substrate in step S1 is PI material.
6. The method for manufacturing the ultra-slender flexible temperature sensor according to claim 1, characterized in that: The drilling process in step S2 is CNC mechanical drilling or laser drilling.
7. The method for manufacturing the ultra-slender flexible temperature sensor according to claim 1, characterized in that: In step S4 and step S7, the anti-plating photosensitive dry film is exposed and developed by laser direct imaging technology or mask.
8. The method for manufacturing the ultra-slender flexible temperature sensor according to claim 1, characterized in that: The protective film in step S8 is a PI protective film.
9. The method for manufacturing the ultra-slender flexible temperature sensor according to claim 1, characterized in that: After step S8, the method further includes performing anti-oxidation surface treatment on the pads in the window area of the protective film.
10. An ultra-slender flexible temperature sensor, characterized in that: The ultra-slender flexible temperature sensor is manufactured by the manufacturing method according to any one of claims 1 to 9.
Citation Information
Patent Citations
Flexible temperature-strain integrated sensor array and preparation method thereof
CN109855687A
Manufacturing method of circuit board taking boss as bonding pad
CN110536564A
Flexible film temperature sensor and manufacturing method thereof
CN117906772A
Manufacture of printed wiring board
JP2000151100A