Method for manufacturing base plate ultra-fine circuit by adopting pre-embedded switching copper pad
Through the pre-embedded copper pad technology, the problem of difficult to achieve fine lines in integrated circuit packaging substrates is solved. High-quality sheets and fine processing methods are used to achieve fine lines of 35 microns wide, improving circuit quality and production efficiency .
Patent Information
- Application Number
- CN202311704574.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-12
- Publication Date
- 2024-11-08
AI Technical Summary
In the prior art, when making integrated circuit packaging substrates, it is difficult to achieve fine line specifications below 50 microns/50 microns, and the thickness of the electroplating copper layer on the entire plate is uneven, making it easy to have problems such as copper residue or excessive fine lines.
Using the pre-embedded copper pad method, using BT sheet or epoxy fiberglass cloth sheet as the core board, and using mechanical or laser drilling, electroless copper plating, dry film etching and other steps, a thin layer of about 35 microns wide is produced. The circuit avoids the residual problem of bottom copper caused by excessive copper thickness, and improves the conductivity of the circuit.
It achieves more detailed line specifications and higher conductivity, reduces the thickness of the surface copper, and improves the quality and production efficiency of integrated circuit packaging.
Smart Images

Figure CN118921886A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of integrated circuit design and manufacturing, and in particular to a method for manufacturing extremely fine and dense circuits of a pad by using a pre-buried transfer copper pad. Background Art
[0002] IC substrates and SLP substrates are both substrates used for packaging and transporting integrated circuits (ICs). IC substrates are substrates used to connect integrated circuits to external circuits, while SLP substrates are substrates used to connect multiple integrated circuits together.
[0003] Drilling a through hole means drilling a hole through the upper and lower layers on the substrate, while a buried via means drilling a partially penetrating hole on a certain layer of the substrate. Both types of holes are used to achieve connections between circuits. Electroplating copper on the hole wall of the substrate allows the copper to conduct, which is to enhance the conductivity of the circuit. Electroplating copper on the hole wall of the substrate allows the copper to conduct, which is to enhance the conductivity of the circuit; after copper plating, the hole is plugged and smoothed with resin, which is to protect the circuit from the influence of the external environment and make the surface of the substrate smoother.
[0004] The existing technology uses drilling technology to drill through holes on the substrate and plate copper on the hole wall to achieve conduction. Then the hole is plugged with resin and smoothed, and copper is electroplated on the resin surface for a second time to increase conductivity and strength. This method can make the entire surface of the substrate plated with copper, but the thick copper layer electroplated on the entire board may have uneven thickness. At the same time, since the bottom copper may remain or the line may be too thin when the line is corroded, it is difficult to achieve fine line specifications below the designed line width / spacing (50 microns / 50 microns). Summary of the invention
[0005] In order to overcome the above-mentioned shortcomings, the present invention aims to provide a technical solution that can solve the above-mentioned problems.
[0006] A method for making an extremely fine circuit of a pad using a pre-buried transfer copper pad, the specific steps comprising:
[0007] Step 1: Use BT sheet or epoxy fiberglass cloth sheet as the core board;
[0008] Step 2: Cut the sheet into appropriate size and shape;
[0009] Step 3: Use a mechanical drill or laser equipment to drill holes in the sheet;
[0010] Step 4: Remove the drilling glue residue remaining in the hole;
[0011] Step 5: Use chemical copper or graphite colloid to make the hole wall conductive and add copper plating thickness;
[0012] Step 6: After the resin plugging, grind the surface and thin the copper to about 10 microns;
[0013] Step 7: After chemical copper plating, the electroplated copper is thickened by about 15 microns;
[0014] Step 8: Use dry film to make a transfer copper pad pattern and etch out the transfer copper pad;
[0015] Step nine, pressing the prepreg and the thin copper foil to the core board;
[0016] Step 10: Use laser equipment to drill blind holes on the core board, place transfer copper pads and circuit patterns in the blind holes, and then make the hole walls of the blind holes conductive by chemical copper plating;
[0017] Step 11: Thin the surface copper to about 15 microns, use dry film to make circuit patterns, and etch out thin circuits about 35 microns wide.
[0018] As a further solution of the present invention: the method steps of making a transfer copper pad pattern with a dry film and then making a transfer copper pad by etching include:
[0019] Step S11, sticking the dry film on the surface where the transfer copper pad is to be made, ensuring that the dry film covers the entire copper pad area.
[0020] Step S12: placing the plate with the dry film attached thereto in an exposure machine, and transferring the pattern on the dry film to the surface of the plate by ultraviolet irradiation.
[0021] Step S13: Use appropriate chemical agents to wash away the dry film on the surface of the plate to expose the metal surface of the copper pad area.
[0022] Etching: Place the plate into an etching machine and etch away the metal surface of the copper pad area through chemical corrosion to form the pattern of the transfer copper pad.
[0023] Step S14: using a chemical method to remove the dry film remaining on the surface of the plate, thereby completing the production of the transfer copper pad.
[0024] Beneficial effects of the present invention: Based on the prior art, the present invention firstly etches out only the thick copper pad for transfer by using dry film and acid etching process, then presses the semi-cured sheet and the thin copper foil, and then lasers the blind hole and plates the flat blind hole to make the hole wall conduct the pre-buried transfer copper pad. In this way, the surface copper can be thinned to about 15 microns, and the dry film and etching can be used to make the fine line specification of about 35 microns wide, avoiding the problem of bottom copper residue caused by too thick surface copper, which is beneficial to improving the fine line capacity and specification.
[0025] Additional aspects and advantages of the present invention will be given in part in the following description and in part will be obvious from the following description, or will be learned through practice of the present invention. BRIEF DESCRIPTION OF THE DRAWINGS
[0026] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative labor.
[0027] Figure 1 It is a schematic flow chart of the method of the present invention. DETAILED DESCRIPTION
[0028] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0029] See also Figure 1 In an embodiment of the present invention, a method for making a pad extremely fine circuit using a pre-buried transfer copper pad comprises the following steps:
[0030] Step 1: Use BT sheet or epoxy glass fiber cloth sheet as the core board. BT sheet refers to a sheet made of bisphenol A epoxy resin and polycarbonate resin, which has high heat resistance and dimensional stability. Epoxy glass fiber cloth sheet is a composite material made of epoxy resin and glass fiber cloth, which has excellent mechanical and electrical properties.
[0031] Step 2: Cutting: Cut the sheet into appropriate size and shape for subsequent processing.
[0032] Step 3: Mechanical or laser drilling: Use a mechanical drill or laser equipment to drill holes in the sheet material so that the transfer copper pads and circuit patterns can be placed in the holes.
[0033] Step 4: Remove the drilling slag remaining in the hole: During the drilling process, some drilling slag may be left, which needs to be removed by chemical or physical methods to ensure the quality of subsequent processing.
[0034] Step 5: Use chemical copper or graphite colloid to make the hole wall conductive and increase the copper plating thickness: Use chemical copper plating or graphite colloid to make the hole wall conductive and increase the copper thickness so as to form the transfer copper pad and circuit pattern in the subsequent processing;
[0035] Chemical copper plating is a process that forms a layer of metal or alloy on the surface of an object through a chemical reaction. When making IC substrates and SLP-type substrates, chemical copper plating is used to increase the conductivity of the hole wall and increase the thickness of the copper. The following are the basic steps of chemical copper plating:
[0036] Pretreatment: First, the sheet is cleaned to remove dirt, grease and other impurities on the surface. This can improve the adhesion and quality of chemical copper plating.
[0037] Sensitization treatment: A layer of sensitizer is applied to the surface of the sheet to form a chemical bond with the surface of the sheet. The sensitizer is usually a solution containing heavy metal ions, such as stannous chloride.
[0038] Activation treatment: A layer of catalyst is coated on the surface of the sensitizer, usually a salt solution of palladium or platinum. The role of the catalyst is to promote the chemical copper plating reaction.
[0039] Chemical copper plating is to immerse the board in a solution containing copper salt. Under the action of the catalyst, the copper ions are reduced to metallic copper and deposited on the surface of the board.
[0040] Post-processing: clean and remove excess copper on the surface, and adjust the thickness and conductivity of the copper layer.
[0041] The process of making the hole wall conductive and increasing the copper thickness by using graphite colloid involves applying graphite colloid to the hole wall of the sheet material, and then forming a conductive layer between the graphite colloid and the hole wall surface by chemical or electrochemical methods. Subsequently, copper plating can be further performed on this conductive layer to increase the copper thickness.
[0042] These steps may be adjusted and optimized according to actual needs and process conditions. The use of chemical copper plating and graphite colloid can provide reliable conductive connections and enhance the electrical performance of IC substrates and SLP-type substrates.
[0043] Step 6. After plugging the holes with resin, grind the surface and thin the copper layer to about 10 microns: Plug the holes with resin, then grind the surface and thin the copper layer to about 10 microns, so that more sophisticated circuit patterns can be produced in subsequent processing.
[0044] Step 7. After chemical copper plating, electroplated copper is thickened by about 15 microns: Through chemical copper plating and electroplating, the copper layer is thickened to about 15 microns to improve conductivity and reliability.
[0045] Electroplated copper is the most widely used pre-plating layer in the electroplating industry. Copper grid lines are made by depositing metallic copper on the surface of base metals through electrolysis to collect carriers generated by the photovoltaic effect.
[0046] Step 8. Use dry film to make a transfer copper pad pattern and etch out the transfer copper pad (surface copper thickness is more than 25 microns): Use dry film to make a transfer copper pad pattern, and then make a transfer copper pad by etching to ensure that its thickness is greater than 25 microns.
[0047] The method steps of making a transfer copper pad pattern with a dry film and then making a transfer copper pad by etching include:
[0048] Step S11, sticking the dry film on the surface where the transfer copper pad is to be made, ensuring that the dry film covers the entire copper pad area.
[0049] Step S12: placing the plate with the dry film attached thereto in an exposure machine, and transferring the pattern on the dry film to the surface of the plate by ultraviolet irradiation.
[0050] Step S13: Use appropriate chemical agents to wash away the dry film on the surface of the plate to expose the metal surface of the copper pad area.
[0051] Etching: Place the plate into an etching machine and etch away the metal surface of the copper pad area through chemical corrosion to form the pattern of the transfer copper pad.
[0052] Step S14: using a chemical method to remove the dry film remaining on the surface of the plate, thereby completing the production of the transfer copper pad.
[0053] Step 9: Lamination (adding prepreg and thin copper foil): Lamination the prepreg and thin copper foil with the core board to form a more complex structure.
[0054] Step 10: Laser drill blind holes and plate the blind holes to make the hole walls conductive: Use laser equipment to drill blind holes on the core board, place transfer copper pads and circuit patterns in the blind holes, and then use chemical copper plating to make the hole walls conductive.
[0055] Step 11. Thin the surface copper to about 15 microns, use dry film to make a circuit pattern, and etch out a thin circuit about 35 microns wide: Thin the surface copper layer to about 15 microns, then use dry film to make a circuit pattern, and finally use etching to make a thin circuit about 35 microns wide.
[0056] In general, this method of using pre-embedded transfer copper pads to make extremely fine circuits on the pads achieves efficient and high-precision production of pad circuits by using high-quality sheet materials, fine processing steps and high-precision production methods. This production method can not only improve the quality and performance of the pads, but also reduce production costs and improve production efficiency.
[0057] It will be apparent to those skilled in the art that the invention is not limited to the details of the exemplary embodiments described above and that the invention can be implemented in other specific forms without departing from the spirit or essential features of the invention. Therefore, the embodiments should be considered exemplary and non-limiting in all respects, and the scope of the invention is defined by the appended claims rather than the foregoing description, and it is intended that all variations falling within the meaning and scope of the equivalent elements of the claims be included in the invention. Any reference numeral in a claim should not be considered as limiting the claim to which it relates.
Claims
1. A method for making extremely fine circuits on a pad using pre-buried transfer copper pads, characterized in that: The specific steps include: Step 1: Use BT sheet or epoxy fiberglass cloth sheet as the core board; Step 2: Cut the sheet into appropriate size and shape; Step 3: Use a mechanical drill or laser equipment to drill holes in the sheet; Step 4: Remove the drilling glue residue remaining in the hole; Step 5: Use chemical copper or graphite colloid to make the hole wall conductive and add copper plating thickness; Step 6: After the resin plugging, grind the surface and thin the copper to about 10 microns; Step 7: After chemical copper plating, the electroplated copper is thickened by about 15 microns; Step 8: Use dry film to make a transfer copper pad pattern and etch out the transfer copper pad; Step nine, pressing the prepreg and the thin copper foil to the core board; Step 10: Use laser equipment to drill blind holes on the core board, place transfer copper pads and circuit patterns in the blind holes, and then make the hole walls of the blind holes conductive by chemical copper plating; Step 11: Thin the surface copper to about 15 microns, use dry film to make circuit patterns, and etch out thin circuits about 35 microns wide.
2. The method for making a very fine circuit of a pad using a pre-buried transfer copper pad according to claim 1, characterized in that: The method steps of making a transfer copper pad pattern with a dry film and then making a transfer copper pad by etching include: Step S11, sticking the dry film on the surface where the transfer copper pad needs to be made; Step S12, placing the plate with the dry film attached in an exposure machine, and transferring the pattern on the dry film to the surface of the plate by ultraviolet irradiation; Step S13, using appropriate chemical agents to wash away the dry film on the surface of the plate to expose the metal surface of the copper pad area; Etching: Place the plate into an etching machine and etch away the metal surface of the copper pad area through chemical corrosion to form the pattern of the transfer copper pad; Step S14: using a chemical method to remove the dry film remaining on the surface of the plate, thereby completing the production of the transfer copper pad.