Method of manufacturing turbine blade
By setting a cavity layer with periodic patterns in the manufacturing of turbine blades, the deformation problems caused by part shrinkage and thermal changes are solved, precise control of asymmetric and slender parts and efficient manufacturing of complex geometric shapes are achieved, and production efficiency is improved and creep resistance.
Patent Information
- Application Number
- CN202380028295.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2022-03-18
- Filing Date
- 2023-03-13
- Publication Date
- 2024-11-08
AI Technical Summary
In the manufacturing of turbine blades, existing metal powder injection molding technology leads to deformation and crack problems caused by shrinkage and thermal changes in parts, making it difficult to achieve precise control and manufacturing of complex geometric shapes.
By providing a cavity layer with periodic patterns during the manufacturing process of turbine blades, cracks are prevented and deformation in sintering and machining steps are avoided, the cavity structure provides support during the sintering process, reducing material consumption and manufacturing costs.
Accurate control of asymmetric and slender parts and efficient manufacturing of complex geometric shapes, reducing the risk of deformation and cracks, improving production efficiency and product creep resistance.
Smart Images

Figure CN118922262A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the manufacture of turbine blades. Background Art
[0002] The technology of injecting metal powder (metal injection molding or MIM) for manufacturing metal products is known. This technology makes it possible to respond to the needs of high production rates while still having good repeatability and good reproducibility.
[0003] This involves injection molding starting with a mixture of metal powder and polymer binder. This mixture (forming an aggregate known as "feedstock") is extruded and then cut into flakes or pellets for the injection press.
[0004] After injection, a so-called "green" part is obtained, which is held together by an adhesive. This adhesive is then removed in a so-called debonding phase, which can be carried out in different ways (by wet, thermal or chemical methods), resulting in a so-called "brown" part.
[0005] The part, with almost all of the binder removed, is very fragile because the part is composed of nearly 40% air and is held together only by the remainder of the binder. The brown part is finally sintered, a process in which the brown part is subjected to temperatures close to the melting point of the powder. This temperature enables the grains to weld together to form a solid.
[0006] After this step a "grey" part is obtained, which consists only of powder material and which has shrunk relative to the molded volume due to the spaces left by the binder. Depending on the method, for different applications, parts with a density of 95% to 99.5% can be obtained. The part is then finished.
[0007] This technology enables the creation of complex shapes with excellent surface conditions and fine tolerances. Injection molding of metal powders is more economical for complex shapes, enabling the manufacture of small parts for a broad market in medium and large production runs. By duplicating the parts that form part of a technology family, raw materials (for the powder part) are very economical. This does not generate waste and does not use oil.
[0008] However, the shrinkage of the parts mentioned above makes it difficult to apply this technology to the manufacture of turbine blades. In fact, the observed shrinkage can reach 15% of the blade size. However, it is important to accurately control the dimensions of such parts. In addition, the thermal changes to which the blades are subjected during the manufacturing process can cause deformation or cracks. This is especially important because blades are often asymmetrical and are 3.5 times thicker in some locations than in another location in the blade.
[0009] It is therefore an object of the present invention to make the manufacture of turbine blades, in particular by injection of metal powder, easier and more reliable. Summary of the invention
[0010] To this end, a method for manufacturing a turbine blade is provided according to the present invention, wherein:
[0011] - manufacturing a part comprising an air flow path region and a layer covering the region,
[0012] The layer has cavities, the cavities forming a periodic pattern,
[0013] Manufactured by injecting a mixture comprising a binder and a powder;
[0014] -Remove most of the adhesive from the part;
[0015] - sintering the parts; and
[0016] -Remove layers from the part to obtain the blade.
[0017] This layer thus makes it possible to prevent the appearance of cracks associated with the injection step, and also avoids the appearance of deformation phenomena associated with the steps of sintering and machining, such as collapse, torsion, bending, buckling and mechanical stresses. The invention thus makes it possible to manufacture elongated and in particular asymmetrical parts with complex geometries and to control the dimensions of the parts. The invention makes it possible to produce with high efficiency. Providing cavities in the layer has the advantage of saving material and therefore reducing manufacturing costs. Finally, the cavities reduce the risk of pulling out during removal from the mould.
[0018] The manufacturing method according to the present invention may also have at least one of the following features:
[0019] -The cavities are arranged in a staggered manner;
[0020] - the cavities form at least one row of identical cavities, the row being parallel to the length of the air flow path area;
[0021] - the cavities form at least one first row and one second row, the cavities of the first row being identical to one another, the cavities of the second row being identical to one another and, finally, the cavities of the first row being different from the cavities of the second row;
[0022] - the contours of the cavities of the first row have a different orientation than the cavities of the second row;
[0023] - Each cavity has a closed contour;
[0024] - Each cavity has a profile having at least one axis of symmetry;
[0025] - Each cavity has a hexagonal profile;
[0026] - Each cavity is constructed such that the cavity can be described by a parametric surface that does not include any singular points;
[0027] Each cavity has a lateral face having an area of connection with the cavity bottom and the external face of the layer, the connection area having a groove having a radius between 0.2 mm and 1 mm;
[0028] the cavities are arranged such that the distance between two adjacent cavities is greater than or equal to 3 mm, for example greater than or equal to 6 mm; and
[0029] - The cavity extends over a large part of the layer.
[0030] It can be provided that the cavity extends over the entire thickness of the layer.
[0031] It can be provided that the layer extends over the entire air flow path area.
[0032] According to one embodiment, the layer covers the lower surface of the air flow path area.
[0033] It can be set that the thickness of the layer is uniform.
[0034] This facilitates uniform debonding of the parts.
[0035] According to one embodiment, the layer is supported directly on the support, in particular during the sintering step.
[0036] Here, the layer serves as an overall support for the component in order to prevent the component from deforming, and in particular collapsing, during the sintering process.
[0037] It may be provided that the part comprises a root, and that the layer forms a plane merging with an edge of the root.
[0038] According to one embodiment, at least one machining operation is performed in order to make the thickness of the layer uniform.
[0039] Here, therefore, the layer plays a reinforcing role during machining by making it possible to harden the blade, which is faced with large deformations during roughing operations involving high cutting forces.
[0040] According to one embodiment, the layer and the upper face are machined a number of times, each machining having a depth between 0.2 mm and 1 mm and / or a step width between 0.1 mm and 10 mm.
[0041] These machining parameters make it possible to meet the geometric specifications of the aeronautical field and the complexity of the contour shape of the air flow path area during the finishing operation.
[0042] According to the present invention, there is also provided a part, comprising:
[0043] - a turbine blade including an air flow path region, and
[0044] - A layer distinct from the blades, the layer extending over the air flow path area and the layer having cavities forming a periodic pattern.
[0045] This part constitutes an intermediate product obtained during the implementation of the method according to the invention before the layer is removed.
[0046] According to one embodiment of the component, the material used is an alloy of titanium and aluminum.
[0047] According to the invention, there is also provided a turbine blade, in particular a blade for an aircraft turbine engine, the blade comprising an air flow path region, the blade being produced by carrying out the method according to the invention.
[0048] Such a blade may have the same shape and size in a macroscopic plane as a blade manufactured by a prior art method. However, such a blade differs from a blade manufactured by a prior art method in microstructure. Thus, such a blade has a larger average grain size than that of a blade obtained by a prior art method, and such a blade provides better creep resistance.
[0049] Furthermore, according to the invention, a turbomachine is provided, which comprises at least one blade according to the invention. BRIEF DESCRIPTION OF THE DRAWINGS
[0050] Embodiments of the invention will now be presented by way of non-limiting examples with the aid of the accompanying drawings, in which:
[0051] Figure 1 and Figure 2 is a perspective view from the underside of an intermediate part obtained in an embodiment of the method of the invention;
[0052] Figure 3 yes Figure 1 and Figure 2 an enlarged view of the underside of the part;
[0053] Figure 4 and Figure 5 is the upper side view of the same part;
[0054] Figure 6 and Figure 7 The positioning and position retention of the intermediate part in its workpiece holder is shown during a first machining stage;
[0055] Figure 8 and Fig. 9shows the trajectory followed by the milling cutter during the first machining phase;
[0056] Fig.10 and Fig.11 shows the positioning and position retention of the intermediate part in its workpiece holder during the second machining stage;
[0057] Fig.12 and Fig.13 shows the trajectory followed by the milling cutter during the second machining phase;
[0058] Fig.14 is similar to Figure 4 and Figure 5 showing a blade obtained starting from this intermediate part; and
[0059] Fig.15 is a half-section view of an aircraft turbojet engine incorporating this type of blade. DETAILED DESCRIPTION
[0060] An embodiment of a manufacturing method according to the invention for producing a turbine blade will be presented.
[0061] In a first step, an intermediate part 4 is manufactured, which includes the blades. Figures 1 to 5 Shown in.
[0062] Thus, the part and blade comprises a root 6, a tip 8 and an airfoil or air flow path 10 extending between the root and the tip.
[0063] Air flow path area 10 (in Figure 2 and Figure 4 ) has two main faces, namely the lower surface 12 (in Figure 3 ) and the upper surface 14 (in Figure 4 , Figure 5 and Fig.14 The two faces are each delimited by a leading edge 16 and a trailing edge 18, which form the two longitudinal edges of the blade. Each main face 12, 14 extends from the root to the tip.
[0064] like Figure 2 As shown, the part 4 comprises a layer 20 which extends over the air flow path region, in this case over the lower surface face 12. In this example, the layer has a uniform thickness along the entire layer, with a minimum value of 2 mm at the top end.
[0065] About the cavity
[0066] This layer has a cavity 22 (at Figures 1 to 32 (see Figure 1), the cavities open on the side of the outer face 21 of the layer 20 opposite the air flow path area 10. Each cavity extends over the entire thickness of the layer. The cavities 22 extend over most of the layer 20, and the cavities extend over the entire air flow path area 10.
[0067] This layer is formed with the root 26 (at Figure 1 The planes where the edges are merged are visible in the figure.
[0068] In order to facilitate the manufacturing of the mold and the injection steps, each cavity 22 has a geometry that can be described by a parametric surface, which does not include any singular points, whose contour is closed and has at least one symmetry axis. Figure 3 In one embodiment shown, the cavity 22 has a hexagonal shape with rounded vertices. In another embodiment, it is conceivable that the cavity 22 has a cylindrical or elliptical profile.
[0069] Here, the cavities 22 form a periodic pattern. This means that the pattern reproduces identically along one or more lines in a plane parallel to the longitudinal direction of the layer and parallel to the width of the layer.
[0070] In this case, the cavities 22 form three identical rows of cavities 33, 34, 35 (in Figure 1 ), each row is parallel to the length of the air flow path area 28. More precisely, the cavities 22 form three rows, namely a first row, a second row and a third row. The cavities of the first row 33 are identical to each other. The cavities of the third row 35 are identical to each other and to the cavities of the first row 33. Furthermore, the cavities of both rows have the same orientation. In this case, one side of the hexagon is parallel to the leading edge 16 and the trailing edge 18. Therefore, the cavities of the two rows are mirror images of each other by translation.
[0071] The cavities of the second row 34 are identical to each other and are different from, in this case larger than, the cavities of the first and third rows. The cavities of the second row all have the same orientation. Therefore, the cavities of the second row are mirror images of each other by translation. However, the cavities of the second row do not have the same orientation as the cavities of the other two rows. In this case, the two edges of the hexagon are parallel to the leading and trailing edges. Therefore, by indirect similarity, they are images of the first and third rows.
[0072] These cavities are arranged in a staggered manner.
[0073] In order to limit the risk of pulling out and breaking of the intermediate part 4 during ejection from the mould, it is preferred that the minimum distance between two adjacent cavities 22 is 3 mm, this value being used for Figure 3 Example shown.
[0074] Each cavity 22 has six lateral faces with an area of connection with the bottom of the cavity and the external face 21 of the layer 20, with grooves 30 having a radius between 0.2 mm and 1 mm. The grooves are convex at the external faces and concave at the bottom.
[0075] About the steps of the method
[0076] Get the intermediate parts
[0077] In this case, the production is carried out by injection molding of metal powder.
[0078] Thus, in a first step, injection molding is performed starting from a mixture of metal powder and an organic binder. Here, the metal powder is an alloy of titanium and aluminum, such as Ti-48Al-2Cr-2Nb (in atomic %), commonly known as TiAl 48-2-2. Thus, a Figures 1 to 3 A blank of a part, i.e. a blade equipped with layers. This is the "green". In this blank, the powder is held in place by a binder.
[0079] This adhesive is then removed during a debonding operation, resulting in a "brown" part in which almost all of the adhesive has been removed, the part consisting of almost 40% air, and held together only by the remainder of the adhesive.
[0080] The part is then sintered, during which step it is subjected to temperatures close to the melting point of the powder, for example greater than 1200°C.
[0081] After this operation, a “grey” part is obtained, which consists only of powdered material and which has shrunk relative to the moulding volume due to the spaces left by the binder.
[0082] The part 4 is manufactured in a single block. During the debinding and sintering operations, the part is arranged to be supported directly on a flat support, with the outer face 21 of the layer 20 at the lower part and the upper surface face 14 turned upwards. The layer is thus in contact with the flat support. The flat support provides local support for the air flow path area 10.
[0083] This layer forms a support and also a reinforcement, which makes it possible to maintain the shape of the part and its integrity during these operations, in particular during sintering and then cooling.
[0084] At the end of this first manufacturing stage, a part 4 is thus obtained which forms an intermediate product composed of a blade 34 and a layer 20, such as Figures 1 to 5 shown.
[0085] Machining
[0086] This layer is then removed from the air flow path area by two machining stages 200 and 300 .
[0087] To this end, during the machining phase 200 , the positioning and position holding of the parts is accomplished in the workpiece holder 202 . Figure 6 A front view showing a section of the intermediate part taken in its workpiece holder 202, Figure 7 A top view of the parts in the same configuration is shown. The outer face 21 of the layer 20 is supported directly on the workbench 208. Therefore, the outer face of the layer is selected as a reference for positioning, covering 80% of the intermediate part, so that the dispersion associated with the possible shape errors generated by the method can be avoided, and the robustness of the clamping is contributed to. Three point contacts 204 are arranged (the three point contacts can be embodied by pins or other support members), that is, one point contact against the root 6 in the longitudinal direction and two point contacts against the leading edge 16 in the width direction. In other embodiments, the first stopper can be arranged at the top 8, the lower surface 14 or the upper surface 16, and the other two stops against the trailing edge 18. The two flanges 206 arranged at the upper surface 14 complete the rigid maintenance of the position of the intermediate part on the workbench through the width and through the top against the upper surface. The number of direct contacts of the flange with the upper surface can be singular, or greater than or equal to twice. The workbench, the stopper and the flange form a workpiece holder. Furthermore, the workpiece holder will be disengaged on one side of the root 6 and the tip 8 in order to allow access to all these areas by the milling tool.
[0088] In this configuration, machining is performed of the root 6 and the tip 8 which will serve as a reference for the tooling and clamping areas for the second machining stage.
[0089] The machining trajectory of stage 200 is Figure 8 In the top view of the middle part in Fig. 9 The front view of the cross section of the middle part of the two parts is shown. The machine tool used includes five or six axes and the machining program corresponds to the following operations:
[0090] 1a. The surface milling cutter 210 establishes a first plane on one side of the upper surface 14 at the root 6 and then at the tip 8,
[0091] 1b. The workpiece holder 202 rotates, and
[0092] 1c. A second plane is established at the tip 8 and then at the root 6 on the lower surface 12 profile side.
[0093] In another embodiment, the machine tool comprises only three axes, which does not allow the workpiece holder 202 to rotate. Therefore, in order to be able to machine both sides, it is necessary to remove the part and turn it over. Therefore, an additional machining stage is provided, separating operations (1a) and (1c).
[0094] Next, in a second machining stage 300, the positioning and holding of the part in another workpiece holder 302 is completed, such as Fig.10 and Fig.11 As shown, Fig.10 A front view showing a section of the intermediate part taken in its workpiece holder 302, Fig.11 A top view of the part is shown, taken in its workpiece holder 302. The root 6 and the top 8 are supported directly on the table 308, forming a sufficiently precise contact area to meet the geometric tolerances during adjustment and clamping and the compatibility of the cutting forces required for the second machining stage 300. Three point contacts 304 are arranged (the three point contacts can be embodied by pins or other supports), namely two point contacts against the root 6 and one point contact against the top 8. Two flanges 306 arranged at the root 6 and the top 8 ensure that the intermediate part is rigidly held in place. At this point, rigid holding occurs only through the root and the top, making the air flow path area 10 available for machining, and the workpiece holder is disengaged in this area.
[0095] The machining trajectory of stage 300 is Fig.12 The middle part is shown in a top view and is Fig.13 The machine tool used includes five or six axes and the machining program corresponds to the following operations:
[0096] 2a. Two sizes of milling cutters 310 perform roughing operations on the layer 20 of the intermediate part to make the surface reach the same thickness as the thickness of the upper surface 14 side, which may be 2 mm,
[0097] 2b. The milling cutter performs a finishing operation on the same lower surface 16, advancing along the part by a spiral or helical sweeping motion until the final contour is formed or after 20 to 10 consecutive passes,
[0098] 2c. The workpiece holder 302 rotates, and
[0099] 2d. The milling cutter performs a finishing operation on the upper side 14, advancing along the part by a spiral or helical sweeping motion until the final contour is formed or 2 to 10 consecutive machining operations can be performed.
[0100] This operating sequence enables roughing operations to be carried out on a maximum amount of material, thereby sufficiently hardening the intermediate part which is subjected to the high cutting forces associated with the large amount of material of the layer 20 and its discontinuity due to the presence of the cavities 22 .
[0101] Depending on the roughness, the height of the desired peaks and the geometry of the milling tool, the passage preferably produces a material removal having a value between 0.2 mm and 1 mm, and the step width having a value between 0.1 mm and 10 mm.
[0102] In another embodiment, the machine tool comprises only three axes, which does not allow the workpiece holder 302 to rotate. Therefore, in order to be able to machine both sides, it is necessary to remove the part and turn it over. Therefore, an additional machining stage is provided, separating operations (2a), (2b) from operation (2c).
[0103] The cutting tool of the milling cutter 210, 310 used may have the following features:
[0104] - The material is a "micrograin" type of carbide in a single block or as an application wafer;
[0105] - depositing any type of coating; and
[0106] - Cutting angle between -5° and +10°.
[0107] It can be provided that the cutting speed is between 20 m / mm and 100 m / mm and the advance is between 0.01 mm and 1 mm.
[0108] Soluble oil or complete oil can be used at a pressure between 5 bar and 150 bar (one bar is equivalent to 10 5 Pa) is used at pressures between
[0109] Lubricants micro-sprayed with CO2 or nitrogen may also be used.
[0110] Then obtain only Fig.14 The blade 32 shown is composed of a part. The blade comprises a root 6, a tip 8 and an air flow path region 10. Both faces (lower surface 12 and upper surface 14) are smooth.
[0111] In blade 32, the thickness of air flow path region 10 is less than the thickness of root 6 and tip 8. In the absence of layer 20, this difference would have a large effect during the cooling and shrinkage of the part. As described above, the layers and cavities 22 of the layers are arranged and sized to reduce this ratio. Overall, taking into account the location of large areas of part 4 enables the material to be distributed during the design process to avoid excessive thickness differences throughout the part.
[0112] Furthermore, without the support of the layer 20, the air flow path area 10 would collapse during the manufacturing process. This is why the layer is made thicker in the air flow path area to support the air flow path area. The periodic pattern of cavities 22 makes it possible to reduce the risk of different types of deformations that the blade may face during the manufacturing process, while still minimizing costs.
[0113] Furthermore, it will preferably be ensured that injection stresses and segregation phenomena, core porosity phenomena and internal stresses generated and detected during sintering are taken into account.
[0114] In the present example, the blade 32 is intended to form part of an aircraft turbojet engine 100, forming a Fig.15 A double-flow, double-body turbine is shown. The turbine has a main axis XX which serves as the axis of rotation of the rotor relative to the stator.
[0115] The turbine runs from upstream to downstream (thus Fig.15 In the figure (from left to right) it comprises a fan 2, a low-pressure compressor 5, an intermediate-pressure compressor, a high-pressure compressor 7, a combustion chamber 9, a high-pressure turbine 11 and a low-pressure turbine 13. Apart from the fan, these elements form the central part of the turbojet engine. The part of these elements that can be moved rotatably around the axis XX forms the rotor.
[0116] The high pressure compressor 7, the combustion chamber 9 and the high pressure turbine 11 form a high pressure body which defines a primary air flow path together with the low pressure compressor 5 and the low pressure turbine 13. The nacelle surrounds the fan 2 and the core to form a fan compartment and define a secondary air flow path.
[0117] The turbine 11 , 13 comprises a blade 32 manufactured by means of the present invention.
[0118] The present invention is applicable to other manufacturing techniques, such as pressing of feedstock and compacting of feedstock.
[0119] Manufacturing can also be carried out according to a printing technique by binder projection (or binder jetting). Binder projection is an additive manufacturing method that operates by projecting a binder onto a powder. An automated roller distributes a thin layer of powder onto a build tray. A printing head applies a liquid binder to the powder, which forms a layer of the object. The printing platform carrying the tray is then slightly lowered to enable a new layer of powder to be added. The method is repeated until the object is formed. The excess powder is then sucked out and the object is dusted by compressed air. The printed part is then placed in an oven for baking or sintering. Finally, a finishing treatment can improve the condition of the printed part. As previously mentioned, the intermediate product layer thus produced is removed to obtain the blade itself.
[0120] The present invention is applied to the manufacture of metal parts, in particular to the manufacture of metal parts by a method of injecting a mixture comprising a binder and powder, and the present invention can be used in all technical fields.
Claims
1. A method for manufacturing a turbine (100) blade (32), wherein: - manufacturing a part (4) comprising an air flow path region (10) and a layer (20) covering said region, The layer has cavities (22) forming a periodic pattern, The manufacturing is performed by injecting a mixture comprising a binder and a powder; - removing the majority of the adhesive from the part; - sintering the part; and - Removing said layer (20) from said part to obtain a blade (32).
2. The method according to the preceding claim, wherein: The cavity (22) opens on an outer face (21) of the layer (20) opposite the air flow path region (10).
3. The method according to at least one of the preceding claims, wherein: The cavities (22) are arranged in a staggered manner.
4. The method according to at least one of the preceding claims, wherein: The cavities (22) form at least one row of identical cavities, the row being parallel to the length of the air flow path region (10).
5. The method according to at least one of the preceding claims, wherein: The cavities (22) form at least one first row and one second row, The cavities of the first row are identical to each other, The cavities of the second row are identical to each other, The cavities of the first row are different from the cavities of the second row.
6. The method according to the preceding claim, wherein: The cavities (22) of the first row have a profile having a different orientation than the cavities of the second row.
7. The method according to at least one of the preceding claims, wherein: Each cavity (22) has a closed outline.
8. The method according to at least one of the preceding claims, wherein: The contour of each cavity (22) has at least one axis of symmetry.
9. The method according to at least one of the preceding claims, wherein: Each cavity (22) has a hexagonal outline.
10. The method according to at least one of the preceding claims, wherein: Each cavity (22) is constructed such that it can be described by a parametric surface that does not include any singular points.
11. The method according to at least one of the preceding claims, wherein: Each cavity (22) has a lateral face having an area of connection with the cavity bottom and the outer face of the layer, the connection area having a groove having a radius between 0.2 mm and 1 mm.
12. The method according to at least one of the preceding claims, wherein: The cavities (22) are arranged such that the distance between two adjacent cavities is greater than or equal to 3 mm, for example, greater than or equal to 6 mm.
13. The method according to at least one of the preceding claims, wherein: The cavity (22) extends across a majority of the layer (20).
14. The method according to at least one of the preceding claims, wherein: The cavity (22) extends over the entire thickness of the layer (20).
15. The method according to at least one of the preceding claims, wherein: The layer (20) extends over the entire air flow path area (10).
16. The method according to at least one of the preceding claims, wherein: The layer covers the lower surface of the air flow path region (12).
17. The method according to at least one of the preceding claims, wherein: The thickness of the layer (20) is uniform.
18. The method according to at least one of the preceding claims, wherein: The layer (20) is supported directly on the support, in particular during the sintering step.
19. Method according to any one of the preceding claims, the part comprising a root (6), the layer (20) forming a plane merging with the edge of the root (26).
20. The method according to at least one of the preceding claims, wherein: At least one machining operation is performed to make the thickness of the layer (20) uniform.
21. The method according to at least one of the preceding claims, wherein: The layer (20) and the upper surface (14) are machined multiple times, each machining having a depth between 0.2 mm and 1 mm.
22. The method according to at least one of the preceding claims, wherein: The layer (20) and the upper surface (14) are machined multiple times, each machining having a step width between 0.1 mm and 10 mm.
23. A component (4), comprising: - a turbine blade (32), said blade comprising an air flow path region (10), and - a layer (20) distinct from the blades, extending over the air flow path region (10) and having cavities (22) forming a periodic pattern.
24. A turbomachine blade (32), in particular a blade of an aircraft turbine engine (100), comprising an air flow path region (10) and produced by implementing the method according to at least one of claims 1 to 22.
25. A turbomachine (100) comprising at least one blade (32) according to the preceding claim.