Multilayer composite

By using multi-layer composites of polymer materials and metal oxide coatings in furniture manufacturing, the complex and expensive multi-layer composite manufacturing problems in the prior art are solved, and cost-effective high-quality surface effect and color stability are achieved. sex.

CN118922306APending Publication Date: 2024-11-08REHAU IND SE & CO KG
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202380027716.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2022-03-15
Filing Date
2023-03-02
Publication Date
2024-11-08

Smart Images

  • Figure CN118922306A_ABST
    Figure CN118922306A_ABST
Patent Text Reader

Abstract

The invention relates to a multi-layer composite comprising: a first layer made of at least one polymeric material wherein the first layer has a transmission of at least 80% for visible light over its thickness according to DIN EN ISO 13468-2: 2006-07; a second layer made of at least one polymer material comprising pigments and / or dyes, optionally further comprising a photoprotective agent, the material of the second layer comprising at least 0.1 to 8 wt%, preferably 0.1 to 5 wt%, relative to the total weight of a layered silicate, in particular a pearlescent pigment, and optionally comprising at least one polymer material comprising pigments and / or dyes. The invention relates to a pigment composition comprising muscovite, mica, aluminum oxide, silicon oxide, calcium-aluminum-borosilicate, bismuth oxychloride and mixtures thereof, having a pigment size according to ISO 13320: 2020-01 of about 1 [mu] m to 300 [mu] m, preferably 5 [mu] m to 200 [mu] m, the second layer has at least one coating made of at least one metal oxide, preferably titanium oxide and / or iron (III) oxide and / or tin oxide and / or zirconium oxide and their mixed oxides, the total thickness of the multilayer composite being about 0.3 to 8 mm, preferably 0.5 to 5 mm, and the thickness of the multilayer composite being about 1 to 5 mm. The surface has a [Delta] L * value of at least-30, preferably at least-50, particularly preferably at least-70, measured by multi-angle measurement between-15 degrees and 110 degrees according to DIN 5033-7: 20 14-10. The invention also relates to a furniture panel and to a laminate comprising at least one multilayer composite.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a multilayer composite comprising a first layer and a second layer. The invention also relates to a furniture panel and a laminate comprising at least one multilayer composite. Background Art

[0002] Such multilayer composites are known from the prior art.

[0003] For example, DE 2 730 899 describes a multilayer composite consisting of a transparent cover layer preferably 50 to 100 μm thick and a support layer, wherein the cover layer is made of polycarbonate, a low-melting thermoplastic polyester, a transparent ABS polymer or PMMA, the support layer preferably has a thickness of more than about 500 μm and is made of polyvinyl chloride or a styrene polymer, preferably an impact-modified polystyrene, and the cover layer and the support layer are firmly connected together if necessary by one or more connecting layers, wherein the layer adjacent to the cover layer is decoratively printed or embossed or colored and embossed on its side facing the cover layer. Polycarbonate is a known commercial material, and as a thermoplastic polyester, polybutylene terephthalate and / or a modified polybutylene terephthalate are preferably used. As an ABS polymer, a styrene-acrylonitrile copolymer should be used. PMMA is transparent and can be impact-modified.

[0004] Such multilayer composites are used, for example, in the sanitary ware sector for producing shower trays, sinks etc., where hardness, scratch resistance and gloss of the surface are considered to be particularly important and there should be the possibility of repairing surface damage by polishing.

[0005] Furthermore, the multilayer composite should be designed, for example by deep drawing, in such a way that the mechanical and optical properties of a bathtub insert, shower tray or the like produced therefrom remain essentially unchanged after forming.

[0006] A disadvantage of such a multilayer composite is that its production is very complicated and, owing to the materials chosen, very expensive.

[0007] Another disadvantage is that such multilayer composites can only be used to a limited extent, in particular in the furniture industry, to produce furniture parts with high-quality, flat surfaces. This is due in particular to the complex layer structure of such multilayer composites and the selected material combinations. High-gloss and / or matte surfaces cannot be produced using the multilayer composites of the prior art.

[0008] Another multilayer composite is described in DE 202010013841 U1. This multilayer composite is a furniture panel in which the upper side of a support element made of wood or artificial wood is bonded to a transparent or satin plastic sheet, which is provided with a colored paint on its lower side, which is provided with a scratch-resistant varnish on its upper side, and the edges of the cut-to-size furniture panel are covered with a plastic edge with a glass appearance. The plastic sheet should be made of acrylic or polycarbonate and have a material thickness of about 2 to 4 mm.

[0009] A disadvantage of such multilayer composites is that they must be made absolutely flat and planar in order to form a material connection with a supporting element made of wood or artificial wood, which greatly increases their complexity. Another disadvantage of such multilayer composites is that when the plastic sheet provided with a colored paint on the back is glued to the supporting element, the paint layer can be damaged or destroyed, so that the furniture panel produced in this way is no longer usable.

[0010] A further disadvantage is that long-term color stability is not guaranteed and such composites can fail prematurely, in particular under stress at different temperatures. Summary of the invention

[0011] The object of the present invention is to overcome the disadvantages of the prior art and to provide a multilayer composite which is easy to manufacture and economically manufactured and which can be used in furniture manufacturing, in particular with various decorative elements and various attractive appearances. Another object of the present invention is to provide a furniture panel and a laminate having at least one multilayer composite.

[0012] According to the invention, the object of providing a multilayer composite is solved by the features of claim 1. Further preferred embodiments are described in the dependent claims.

[0013] Surprisingly, a multilayer composite has been found, comprising: a first layer made of at least one polymer material, wherein the first layer has a transmittance of at least 80% for visible light measured over its thickness according to DIN EN ISO 13468-2:2006-07; a second layer made of at least one polymer material containing pigments and / or dyes and, if necessary, light protection agents, wherein the material of the second layer contains at least 0.1 to 8 wt. %, preferably 0.1 to 5 wt. %, based on the total weight, of sheet silicates, in particular pearlescent pigments, including muscovite, mica, aluminum oxide, silicon oxide, calcium-aluminum-borosilicate, bismuth oxychloride and mixtures thereof, according to ISO 13320:2020-01 whose pigment size is about 1 μm to 300 μm, preferably 5 μm to 200 μm, the second layer has at least one coating made of at least one metal oxide, preferably titanium oxide and / or iron (III) oxide and / or tin oxide and / or zirconium oxide and mixed oxides thereof, wherein the total thickness of the multilayer composite is about 0.3 to 8 mm, preferably 0.5 to 5 mm, and whose surface has a ΔL* value of at least -30, preferably at least -50, particularly preferably at least -70, measured by multi-angle measurement between -15° and 110° according to DIN 5033-7:2014-10. It has been found that, in particular, by means of the type, amount and size of the pigments, a multilayer composite can be provided which has an upper side with a very visually appealing, high-quality appearance, which has the appearance of a differently colored anodized, matte metal surface. Surprisingly, this visually appealing surface can also be well demonstrated by multi-angle measurement using the L*a*b* color space.

[0014] In the sense of the present invention, the L*a*b* color space (also known as: CIELAB, CIEL*a*b*, Lab color) describes all perceptible colors. It uses a three-dimensional color space in which the lightness values ​​L* are perpendicular to the color planes (a*, b*). The a-coordinate represents the hue and chromaticity between green and red, and the b-coordinate represents the hue and chromaticity between blue and yellow. The larger the positive a and positive b values, and the smaller the negative a and negative b values, the more intense the hue. If a=0 and b=0, there are non-color hues on the lightness axis. In a typical software implementation, L (lightness) can take values ​​between 0 and 100, and a and b can vary between -128 and 127. In the usual model of 8 bits per color channel, 16.7 million possible Lab coordinates can be realized in this way. The actual L*a*b* color space (our color perception) exceeds the mentioned a / b limits in some areas and does not reach the mentioned a / b limits in most areas. The most important properties of the L*a*b* color model include device independence and perception-dependence, i.e.: the color is defined independently of its generation or reproduction technology, as perceived by a standard observer under standard lighting conditions. Surprisingly, ΔL* values ​​of at least -30, preferably at least -50, particularly preferably at least -70, measured between -15° and 110° according to DIN 5033-7:2014-10, can be determined on the surface of the multilayer composite. With regard to the pigments that can be used, the resulting high-quality appearance of the multilayer composite surface can also be achieved in different color combinations.

[0015] It has proven to be advantageous if the surface of the multilayer composite has a ΔE* value of at least -30, preferably at least -50, particularly preferably at least -70, measured by multi-angle measurement between -15° and 110° according to DIN 5033-7:2014-10. Thus, a multilayer composite can be provided which, on the one hand, has a certain three-dimensional effect due to the first layer made of polymer material and, in addition, also emits a visually appealing metallic effect, the so-called iridescent effect.

[0016] Another advantage of the multilayer composite is that the first layer has at least one covering layer with a thickness of about 2 to 60 μm, preferably 5 to 30 μm, which protects the first layer and also enhances the metallic effect produced by the pigment contained in the second layer.

[0017] Another advantage of the multilayer composite is that the cover layer contains at least one acrylic polymer and has a maximum transmittance of about 80% for visible light measured over its thickness according to DIN EN ISO 13468-2:2006-07. Such a cover layer achieves an optimal surface gloss and a certain 3D effect over the entire surface in the multilayer composite.

[0018] The multilayer composite is also advantageously characterized in that the first layer comprises at least one (meth)acrylate copolymer having a haze of less than 0.5, measured according to ASTM D 1003:2021, and having a refractive index of about 1.49, measured according to DIN EN ISO 489:1999-08. However, it is also possible within the scope of the invention that the first layer comprises at least one polycarbonate (PC) having a refractive index of about 1.585; polystyrene (PS) having a refractive index of about 1.58; styrene-acrylonitrile (SAN) having a refractive index of about 1.56; polypropylene (PP) having a refractive index of about 1.50; and polyethylene terephthalate (PET) having a refractive index of about 1.57, or a mixture thereof, the refractive index being measured according to DIN EN ISO 489:1999-08. As a result, the surface of the multilayer composite not only has a certain 3D effect, but also the metallic effect is different in intensity or color intensity for the observer in its cross section.

[0019] It has been found to be advantageous to provide at least one third layer on the side of the second layer opposite to the first layer. This leads to better rigidity of the multilayer composite on the one hand and good adhesion on the other hand. Another advantage of the multilayer composite is that the third layer contains at least one styrene polymer, in particular a styrene copolymer, preferably styrene-acrylonitrile (SAN). Another advantage is that the third layer contains at least one acrylonitrile-butadiene-styrene copolymer (ABS). Another advantage of the multilayer composite is that the third layer contains at least one (meth)acrylate copolymer. Thus, a multilayer composite can be provided that is economically and cost-effectively producible and has a visually attractive surface that corresponds to the appearance of a matte metal surface with different colored anodized surfaces. Another advantage of the multilayer composite is that the third layer contains a mixture of acrylonitrile-butadiene-styrene copolymer (ABS) and styrene-acrylonitrile (SAN), the proportion of which is about 10 to 90% by weight, preferably 20 to 80% by weight, relative to the total weight. Therefore, such a multilayer composite is very easy to produce economically and cost-effectively.

[0020] Another advantage of the multilayer composite is that the processing shrinkage of the material of the composite is about 0.3 to 0.7%, measured in accordance with DIN EN ISO 294-4:2019-04. Thus, multilayer composites can also be produced in an economical and cost-effective manner, which also have an absolutely flat surface without warping and similar defects.

[0021] The problem of providing a furniture panel with at least one multilayer composite is solved by the features of claims 11 and 12. The furniture panel with the multilayer composite is characterized in that at least one supporting element is arranged on the side of the second layer opposite to the first layer. Thus, for the first time, a multilayer composite with supporting elements can be provided, for example for use as furniture doors, side panels, furniture bodies, etc. in furniture manufacturing.

[0022] Another surprising advantage of a furniture panel having at least one multilayer composite is that at least one supporting element is arranged on the side of the second layer opposite the first layer, on which at least one further multilayer composite is arranged. Thus, furniture components can be provided which achieve a visually appealing, metallic-effect surface on both the front and back sides, which are economically and cost-effectively producible and which can be used for high-quality components, in particular for furniture manufacturing.

[0023] The problem of the invention of providing a laminate having at least one multilayer composite is solved by the features of claims 13 to 15 .

[0024] In a laminate with at least one multilayer composite, it has proven to be advantageous to arrange at least one further multilayer composite on the side of the second layer opposite to the first layer. Similarly, in another embodiment of a laminate with at least one multilayer composite, it has proven to be advantageous to arrange at least one further multilayer composite on the side of the third layer opposite to the first layer. In another preferred embodiment of a laminate with at least one multilayer composite, it is also characterized in that it contains at least two multilayer composites according to the aforementioned embodiments arranged close to each other. In particular, by varying the individual multilayer composites, it is thus possible to provide economically and cost-effectively manufacturable laminates, components, etc., which meet all optical and static requirements, in particular in the field of furniture manufacturing.

[0025] Alternatively, the multilayer composite, in particular its components, can be manufactured using an additive manufacturing process, in particular single-layer manufacturing, for example by a 3D printing process. For manufacturing the multilayer composite, in particular its components, a data-processed, machine-readable three-dimensional model can advantageously be used. The present invention also includes a method for generating a data-processed, machine-readable three-dimensional model, which is used in a method for manufacturing a multilayer composite, in particular its components. In this case, the method also includes, in particular, inputting data representing the multilayer composite, in particular its components, into a data processing machine, and using this data to represent the multilayer composite, in particular its components, as a three-dimensional model, wherein the three-dimensional model is suitable for use when manufacturing the multilayer composite, in particular its components. The multilayer composite, in particular its components, can be manufactured in whole or in part using a manufacturing process that is built up line by line or layer by layer. In this case, it is very advantageous to use a 3D data set during the construction or manufacturing. The method also includes a technique in which data is input using one or more 3D scanners, which can be contact or non-contact, wherein in the latter case energy is emitted onto the multilayer composite, in particular its components, and the reflected energy is received, and wherein a virtual three-dimensional model of the multilayer composite, in particular its components, is generated using computer-aided design software. The manufacturing process can include an additive powder bed process, in particular selective laser melting (SLM), selective laser sintering (SLS), selective hot sintering (SHS), selective electron beam melting (EBM / electron beam additive manufacturing-EBAM) or solidification of powdered materials by a binder (binder jetting). The manufacturing process can include an additive free form manufacturing process, in particular directed energy deposition (DED), wax filament deposition modeling (WDM), contour crafting (Contour Crafting), metal powder directed energy deposition (MPA), plastic powder directed energy deposition, cold spraying, electron beam welding (EBW) or a fused deposition process, such as fused deposition modeling (FDM) or fused filament fabrication (FFF). The manufacturing process may include an additive material jetting process, in particular stereolithography (SLA), digital light processing (DLP), multi-nozzle modeling (MJM), polymer jet modeling or liquid composite molding (LCM). In addition, the manufacturing process may include other additive layer-by-layer building processes, in particular layered object manufacturing (LOM), 3D screen printing or light-induced electrophoretic deposition. BRIEF DESCRIPTION OF THE DRAWINGS

[0026] The present invention will be described in more detail below by way of non-limiting examples.

[0027] As shown in the figure:

[0028] Figure 1 : Perspective view of the multi-layer composite;

[0029] Figure 2: A cross-sectional view of a furniture panel having at least one multilayer composite;

[0030] Figure 3 : A perspective view of a laminate having at least two multilayer composites;

[0031] Figure 4 : A cross-sectional view of another laminate having at least two multilayer composites. DETAILED DESCRIPTION

[0032] Figure 1 The invention shows a perspective view of a multilayer composite 10, comprising: a first layer 1 made of at least one polymer material, wherein the first layer 1 has a transmittance of at least 80% for visible light measured over its thickness according to DIN EN ISO 13468-2:2006-07; a second layer 2 made of at least one polymer material, containing pigments and / or dyes and, if necessary, light protection agents, wherein the material of the second layer 2 contains at least 0.1 to 8% by weight, preferably 0.1 to 5% by weight (relative to the total weight) of sheet silicates, in particular pearlescent pigments, including muscovite, mica, aluminum oxide, silicon oxide, calcium-aluminum-borosilicate, bismuth oxychloride and mixtures thereof according to ISO 13320:2020-01 whose pigment size is about 1 μm to 300 μm, preferably 5 μm to 200 μm, the second layer has at least one coating made of at least one metal oxide, preferably titanium oxide and / or iron (III) oxide and / or tin oxide and / or zirconium oxide and their mixed oxides, wherein the total thickness of the multilayer composite 10 is about 0.3 to 8 mm, preferably 0.5 to 5 mm, and its surface has a ΔL* value of at least -30, preferably at least -50, and particularly preferably at least -70 measured by multi-angle measurement between -15° and 110° according to DIN 5033-7:2014-10.

[0033] In this embodiment, the multilayer composite 10 is designed so that the material of the second layer 2 contains about 3% by weight (relative to the total weight) of a layered silicate, in particular a pearlescent pigment containing muscovite, whose pigment size according to ISO 13320:1020-01 is about 200 μm, and the second layer has at least one coating made of at least one metal oxide, titanium oxide.

[0034] The total thickness of the multilayer composite 10 is about 3.5 mm. The surface of the multilayer composite 10 has a ΔL* value of about -50 measured by multi-angle measurement between -15° and 110° according to DIN 5033-7:2014-10. In addition, in this embodiment, the multilayer composite 10 is designed so that its surface has a ΔE* value of about -55 measured by multi-angle measurement between -15° and 110° according to DIN 5033-7:2014-10.

[0035] The multilayer composite 10 is designed such that the first layer 1 has at least one cover layer 5 having a thickness of approximately 2 to 60 μm, preferably 5 to 30 μm. In this exemplary embodiment, the multilayer composite 10 is designed such that the thickness of the cover layer 5 is approximately 10 μm. Furthermore, the multilayer composite 10 is designed such that the cover layer 5 contains at least one acrylic polymer and has a maximum transmittance of approximately 80% for visible light measured over its thickness according to DIN EN ISO 13468-2: 2006-07. In this exemplary embodiment, the multilayer composite 10 is designed such that the transmittance of the cover layer 5 measured over its thickness according to DIN EN ISO 13468-2: 2006-07 for visible light is approximately 75%.

[0036] The first layer 1 of the multilayer composite 10 comprises at least one (meth)acrylate copolymer having a haze of less than 0.5 measured according to ASTM D1003:2021 and a refractive index of about 1.49 measured according to DIN EN ISO 489:1999-08.

[0037] In this embodiment, the multilayer composite 10 is designed such that the first layer 1 comprises polymethyl methacrylate (PMMA) having a haze of about 0.2 measured according to AST D 1003: 2021. Furthermore, in this embodiment, the multilayer composite 10 is designed such that the refractive index of the first layer 1 is about 1.49 measured according to DIN EN ISO 489: 1999-08.

[0038] Figure 2 A sectional view of a furniture panel having at least one multilayer composite 10 is shown.

[0039] The furniture panel with at least one multilayer composite 10 comprises: a first layer 1 made of at least one polymer material, wherein the first layer 1 has a transmittance of at least 80% for visible light measured over its thickness according to DIN EN ISO 13468-2:2006-07; a second layer 2 made of at least one polymer material, which contains pigments and / or dyes and, if necessary, light protection agents, wherein the material of the second layer 2 contains at least 0.1 to 8 wt. %, preferably 0.1 to 5 wt. %, based on the total weight, of sheet silicates, in particular pearlescent pigments, including muscovite, mica, aluminum oxide, silicon oxide, calcium-aluminum-borosilicate, bismuth oxychloride and mixtures thereof, according to ISO 13320:2020-01 whose pigment size is about 1 μm to 300 μm, preferably 5 μm to 200 μm, the second layer has at least one coating made of at least one metal oxide, preferably titanium oxide and / or iron (III) oxide and / or tin oxide and / or zirconium oxide and their mixed oxides, wherein the total thickness of the multilayer composite 10 is about 0.3 to 8 mm, preferably 0.5 to 5 mm, and its surface has a ΔL* value of at least -30, preferably at least -50, and particularly preferably at least -70 measured by multi-angle measurement between -15° and 110° according to DIN 5033-7:2014-10, wherein at least one supporting element 4 is arranged on the side of the second layer 2 opposite to the first layer 1.

[0040] The supporting element 4 is arranged here at a distance from the second layer 2 of the multilayer composite 10 by means of the connecting layer 6 .

[0041] The total thickness of the multilayer composite 10 of the furniture panel is about 3.0 mm. The surface of the multilayer composite 10 of the furniture panel has a ΔL* value of about -55 measured by multi-angle measurement between -15° and 110° according to DIN 5033-7:2014-10.

[0042] Furthermore, the multilayer composite 10 of the furniture panel is designed such that the first layer 1 has at least one cover layer 5 having a thickness of approximately 2 to 60 μm, preferably 5 to 30 μm. In this exemplary embodiment, the thickness of the cover layer 5 is 25 μm.

[0043] The multilayer composite 10 of the furniture panel is characterized in that the surface of the multilayer composite 10 has a ΔE* value of at least -30, preferably at least -50, particularly preferably at least -70, measured by multi-angle measurement between -15° and 110° according to DIN 5033-7:2014-10.

[0044] The processing shrinkage of the material of the multilayer composite 10 of the furniture panel measured according to DIN EN ISO 294-4:2019-04 is about 0.3% to 0.7%. In this embodiment, the processing shrinkage of the material of the multilayer composite 10 of the furniture panel measured according to DIN EN ISO 294-4:2019-04 is about 0.35%.

[0045] The supporting element 4 is arranged spaced apart from the second layer 2 of the multilayer composite 10 of the furniture panel by means of the connecting layer 6 .

[0046] The connecting layer 6 is designed as an adhesive layer and contains at least one reactive adhesive based on polyurethane (PUR). Single-component and multi-component adhesives based on polyurethane (PUR) can be used here.

[0047] In this embodiment, the support element 4 of the furniture board is designed as a so-called MDF board. However, within the scope of the invention, it is also possible for the support element 4 of the furniture board to be made of wood, wood material, artificial wood, polymer material, metal material, ceramic material, glass, paper, composite support material, etc.

[0048] Figure 3 A perspective view of a laminate having at least two multilayer composites 10 , 10 ′ is shown.

[0049] The multilayer composite 10, 10' of a laminate comprises: a first layer 1, 1', which is made of at least one polymer material, wherein the first layer 1, 1' has a transmittance of at least 80% for visible light measured over its thickness according to DIN EN ISO 13468-2:2006-07; a second layer 2, 2', which is made of at least one polymer material, contains pigments and / or dyes and, if necessary, light protection agents, wherein the material of the second layer 2, 2' contains at least 0.1 to 8 wt. %, preferably 0.1 to 5 wt. %, based on the total weight, of sheet silicates, in particular pearlescent pigments, including muscovite, mica, aluminum oxide, silicon oxide, calcium-aluminum-borosilicate, bismuth oxychloride and mixtures thereof according to ISO 13320:2020-01 whose pigment size is about 1 μm to 300 μm, preferably 5 μm to 200 μm, the second layer has at least one coating made of at least one metal oxide, preferably titanium oxide and / or iron (III) oxide and / or tin oxide and / or zirconium oxide and their mixed oxides, wherein the total thickness of the multilayer composite 10, 10' is about 0.3 to 8 mm, preferably 0.5 to 5 mm, and its surface has a ΔL* value of at least -30, preferably at least -50, and particularly preferably at least -70 measured by multi-angle measurement between -15° and 110° according to DIN 5033-7:2014-10, wherein the multilayer composite 10 is arranged separated from the multilayer composite 10' by at least one connecting layer 6.

[0050] In this embodiment, the multilayer composite 10 of the laminate is designed so that the material of the second layer 2 contains about 2.5% by weight (relative to the total weight) of a layered silicate, in particular a pearlescent pigment containing an aluminum-borosilicate, whose pigment size according to ISO 13320:2020-01 is about 200 μm, and the pigment has at least one coating made of a metal oxide, zirconium oxide, wherein the total thickness of the multilayer composite 10 is about 6.5 mm and its surface has a ΔL* value of about -78 measured between -15° and 110° by multi-angle measurement according to DIN 5033-7:2014-10.

[0051] In this embodiment, the multilayer composite 10' of the laminate is designed such that the material of the second layer 2' contains about 4% by weight (relative to the total weight) of a layered silicate, in particular a pearlescent pigment containing bismuth oxychloride, whose pigment size according to ISO 13320:2020-01 is about 180 μm, and the second layer has at least one coating made of a metal oxide, iron (III) oxide, wherein the total thickness of the multilayer composite 10' is about 4 mm and its surface has a ΔL* value of about -65 measured by multi-angle measurement between -15° and 110° according to DIN 5033-7:2014-10.

[0052] The multilayer composite 10 of the laminate is designed such that the first layer 1 has at least one cover layer 5 with a thickness of approximately 2 μm to 60 μm, preferably 5 μm to 30 μm. In this embodiment, the thickness of the cover layer 5 is approximately 15 μm. The cover layer 5 of the multilayer composite 10 of the laminate is designed such that it contains at least one acrylic polymer and has a transmittance of approximately 72 for visible light measured over its thickness according to DIN EN ISO 13468-2:2006-07.

[0053] The connecting layer 6 between the multilayer composite 10 and the multilayer composite 10' of the laminate is designed as an adhesive layer and fixes the multilayer composites 10, 10' to form a laminate. The connecting layer 6 contains at least one reactive hot melt adhesive based on polyurethane (PUR) with a coating amount of about 30 to 150 g / m 2 , preferably 40 to 80 g / m 2 In this embodiment, the coating amount is about 50g / m 2 .

[0054] Figure 4 A cross-sectional view of another laminate having at least two multilayer composites 10 , 10 ′ is shown.

[0055] The multilayer composite 10, 10' comprises a first layer 1, 1' made of at least one polymer material, wherein the first layer 1, 1' has a transmittance of at least 80% for visible light measured over its thickness according to DIN EN ISO 13468-2:2006-07; a second layer 2, 2' made of at least one polymer material, containing pigments and / or dyes and, if necessary, light protection agents, wherein the material of the second layer 2, 2' contains at least 0.1 to 8% by weight, preferably 0.1 to 5% by weight (relative to the total weight) of sheet silicates, in particular pearlescent pigments, including muscovite, mica, aluminum oxide, silicon oxide, calcium-aluminum-borosilicate, bismuth oxychloride and mixtures thereof according to ISO 13320:2020-01 whose pigment size is about 1 μm to 300 μm, preferably 5 μm to 200 μm, the second layer has at least one coating made of at least one metal oxide, preferably titanium oxide and / or iron (III) oxide and / or tin oxide and / or zirconium oxide and their mixed oxides, wherein the total thickness of the multilayer composite 10, 10' is about 0.3 to 8 mm, preferably 0.5 to 5 mm, and its surface has a ΔL* value of at least -30, preferably at least -50, and particularly preferably at least -70 measured by multi-angle measurement between -15° and 110° according to DIN 5033-7:2014-10, wherein the multilayer composite 10 is arranged separated from the multilayer composite 10' by at least one connecting layer 6.

[0056] In this embodiment, the multilayer composite 10 of the laminate is designed such that the material of the second layer 2 contains about 4% by weight (relative to the total weight) of a layered silicate, in particular a pearlescent pigment containing mica, whose pigment size according to ISO 13320:2020-01 is about 120 μm, and the second layer has at least one coating made of a metal oxide, tin oxide, wherein the total thickness of the multilayer composite 10 is about 5 mm and its surface has a ΔL* value of about -75 measured by multi-angle measurement between -15° and 110° according to DIN 5033-7:2014-10.

[0057] In this embodiment, the multilayer composite 10' of the laminate is designed such that the material of the second layer 2' contains about 4% by weight (relative to the total weight) of a layered silicate, in particular a pearlescent pigment containing bismuth oxychloride, whose pigment size according to ISO 13320:2020-01 is about 180 μm, and the second layer has at least one coating made of a metal oxide, iron (III) oxide, wherein the total thickness of the multilayer composite 10' is about 4 mm and its surface has a ΔL* value of at least -65 measured by multi-angle measurement between -15° and 110° according to DIN 5033-7:2014-10.

[0058] The multilayer composite 10 of the laminate is designed such that the first layer 1 has at least one cover layer 5 having a thickness of about 2 μm to 60 μm, preferably 5 μm to 30 μm. In this embodiment, the thickness of the cover layer 5 of the multilayer composite 10 of the laminate is about 15 μm. The cover layer 5 of the multilayer composite 10 of the laminate is designed such that it contains at least one acrylic polymer and has a transmittance of about 72 for visible light measured over its thickness according to DIN EN ISO 13468-2:2006-07.

[0059] The multilayer composite 10, 10' of the laminate is also designed such that at least one third layer 3, 3' is arranged on the side of the second layer 2, 2' opposite to the first layer 1, 1'. The layer 3 of the multilayer composite 10 of the laminate contains at least one styrene polymer, in particular a styrene copolymer, preferably styrene-acrylonitrile (SAN). In an advantageous embodiment, the third layer 3 of the multilayer composite 10 of the laminate is designed such that it contains at least one acrylonitrile-butadiene-styrene copolymer (ABS).

[0060] The layer 3' of the multilayer composite 10' of the laminate comprises a mixture of acrylonitrile-butadiene-styrene copolymer (ABS) and styrene-acrylonitrile (SAN), wherein the proportion of styrene-acrylonitrile (SAN) is about 10 to 90% by weight, preferably 20 to 80% by weight. In this embodiment, the proportion of styrene-acrylonitrile in the third layer 3' of the multilayer composite 10' of the laminate is about 45% by weight.

[0061] The processing shrinkage of the material of each composite body 10, 10' of the laminate measured according to DIN EN ISO 294-4: 2019-04 is about 0.3% to 0.7%. In this embodiment, the processing shrinkage of the material of the composite body 10 of the laminate is about 0.38%, and the processing shrinkage of the material of the composite body 10' of the laminate is about 0.41%, and the processing shrinkage is measured according to DIN EN ISO 294-4: 2019-04.

[0062] The connecting layer 6 between the multilayer composite 10 and the multilayer composite 10' is designed as an adhesive layer and fixes the multilayer composites 10, 10' to form a laminate. The connecting layer 6 contains at least one reactive hot melt adhesive based on polyurethane (PUR) with a coating amount of about 30 g / m 2 Up to 150g / m 2 , preferably 40g / m 2 Up to 80g / m 2 In this embodiment, the coating amount of the connecting layer 6 designed as a reactive hot melt adhesive based on polyurethane (PUR) is about 45 g / m 2 .

Claims

1. A multilayer composite (10, 10') comprising: include: a first layer (1, 1') made of at least one polymer material, wherein the first layer (1, 1') has a transmission for visible light of at least 80% measured over its thickness according to DIN EN ISO 13468-2:2006-07, a second layer (2, 2') made of at least one polymer material containing pigments and / or dyes and, if necessary, light protection agents, ° wherein the material of the second layer (2, 2') comprises at least 0.1 to 8 wt. % relative to the total weight, Preferably 0.1 to 5% by weight of phyllosilicates, especially pearlescent pigments, include muscovite, Mica, aluminum oxide, silicon oxide, calcium-aluminum-borosilicate, bismuth oxychloride and mixtures thereof, ° according to ISO 13320:2020-01, the pigment size is about 1 μm to 300 μm, preferably 5 μm to 200 μm, ° the second layer (2, 2') has at least one coating made of at least one metal oxide, preferably titanium oxide and / or iron(III) oxide and / or tin oxide and / or zirconium oxide and mixed oxides thereof, wherein the multilayer composite (10, 10') having a total thickness of about 0.3 to 8 mm, preferably 0.5 to 5 mm, Its surface has a ΔL* value of at least −30, preferably at least −50, particularly preferably at least −70, measured by multi-angle measurement between −15° and 110° in accordance with DIN 5033-7:2014-10.

2. The multilayer composite (10, 10') according to claim 1, It is characterized in that The surface thereof has a ΔE* value of at least −30, preferably at least −50, particularly preferably at least −70, measured by multi-angle measurement between −15° and 110° in accordance with DIN 5033-7:2014-10.

3. The multilayer composite (10, 10') according to any one of the preceding claims, It is characterized in that The first layer (1, 1') has at least one cover layer (5) having a thickness of approximately 2 μm to 60 μm, preferably 5 μm to 30 μm.

4. The multilayer composite (10, 10') according to any one of the preceding claims, It is characterized in that The cover layer (5) comprises at least one acrylic polymer and has a maximum transmission of approximately 80% for visible light, measured over its thickness in accordance with DIN EN ISO 13468-2:2006-07.

5. The multilayer composite (10, 10') according to any one of the preceding claims, It is characterized in that The first layer (1, 1') comprises at least one (meth)acrylate copolymer having a haze of less than 0.5 measured in accordance with ASTM D1003 and a refractive index of about 1.49 measured in accordance with DIN EN ISO 489:1999-08.

6. The multilayer composite (10, 10') according to any one of claims 1 to 5, It is characterized in that At least one third layer (3, 3') is arranged on a side of the second layer (2, 2') opposite to the first layer (1, 1').

7. The multilayer composite (10, 10') according to claim 6, It is characterized in that The third layer (3, 3') comprises at least one styrene polymer, in particular a styrene copolymer, preferably styrene-acrylonitrile (SAN).

8. The multilayer composite (10, 10') according to claim 6, It is characterized in that The third layer (3, 3') comprises at least one acrylonitrile-butadiene-styrene copolymer (ABS).

9. The multilayer composite (10, 10') according to claim 6, It is characterized in that The third layer (3, 3') comprises a mixture of acrylonitrile-butadiene-styrene copolymer (ABS) and styrene-acrylonitrile (SAN), wherein the proportion of styrene-acrylonitrile (SAN) is about 10 to 90% by weight, preferably 20 to 80% by weight, relative to the total weight.

10. The multilayer composite (10, 10') according to claim 6, It is characterized in that The processing shrinkage of the material of the composite (10, 10'), measured according to DIN EN ISO 294-4:2019-04, is about 0.3 to 0.7%.

11. A furniture panel comprising at least one multilayer composite (10, 10') according to any one of claims 1 to 10, It is characterized in that At least one supporting element (4) is arranged on a side of the second layer (2, 2') opposite to the first layer (1, 1').

12. A furniture panel comprising at least one multilayer composite (10, 10') according to any one of claims 1 to 10, It is characterized in that At least one supporting element (4) is arranged on the side of the second layer (2, 2') opposite the first layer (1, 1'), on which at least one further multilayer composite (10') is arranged.

13. A laminate comprising at least one multilayer composite (10, 10') according to any one of claims 1 to 10, It is characterized in that At least one further multilayer composite (10') is arranged on the side of the second layer (2, 2') opposite the first layer (1, 1').

14. A laminate comprising at least one multilayer composite (10, 10') according to any one of claims 1 to 10, It is characterized in that At least one further multilayer composite (10') is arranged on the side of the third layer (3, 3') opposite the first layer (1, 1').

15. A laminate comprising at least two multilayer composites (10, 10') according to any one of claims 1 to 10 arranged next to one another.

Citation Information

Patent Citations

  • Multilayer composites having improved physical properties

    CN103547448A

  • Green phase golden pearl pigment based on synthetic mica as well as preparation method and application of green phase golden pearl pigment

    CN108752978A

  • Blow molded multilayer article with color gradient

    US20210206141A1