Thin film type ultrasonic coupling patch and preparation method thereof

By adopting a thin-film ultrasonic coupled patch with a laminated structure, the problem of waste and cleaning of traditional ultrasonic coupling agents is solved, efficient and uniform ultrasonic conduction and good biocompatibility are achieved, and ultrasonic imaging quality and convenience of use are improved. sex.

CN118924333APending Publication Date: 2024-11-12SHANGHAI SOUNDWISE TECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411109355.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-13
Publication Date
2024-11-12

AI Technical Summary

Technical Problem

Traditional liquid or gel-like ultrasonic coupling agents have problems such as waste of use, complex operation, difficulty in cleaning, uneven coating, bacterial growth and low comfort, which affects the ultrasonic conduction effect and imaging quality.

Method used

Thin film-type ultrasonic coupled patches with laminated structures, including polyurethane or polyvinyl alcohol films and hydroxypropyl methylcellulose or polyethylene glycol films, form a firm laminated body by hot pressing, for contact with ultrasonic probes and skin. , reduce waste and operation complexity, and improve cleaning convenience and uniformity.

Benefits of technology

It realizes efficient use of thin-film ultrasonic coupled patches, reduces waste and operational complexity, ensures uniform coating and good biocompatibility, improves ultrasonic conduction effect and imaging quality, and is easy to clean and store.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118924333A_ABST
    Figure CN118924333A_ABST
Patent Text Reader

Abstract

The invention provides a thin film type ultrasonic coupling patch. The thin film type ultrasonic coupling patch comprises a first thin film and a second thin film which are stacked, the first film is a polyurethane film or a polyvinyl alcohol film; the second film is a hydroxypropyl methyl cellulose film or a polyethylene glycol film; wherein the first film is used for being in contact with an ultrasonic probe, and the second film is used for being in contact with skin. The composite material can be directly attached to the skin or the surface of an object, the usage amount and waste are reduced, and the composite material is easy to tear off after being used, free of residues, easy to clean and not prone to pollution and has good biocompatibility, sound transmission, wettability and use comfort.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of ultrasonic medical materials, and in particular to a thin-film ultrasonic coupling patch and a preparation method thereof. Background Art

[0002] Ultrasonic coupling agent plays a vital role in medical imaging and treatment. It can eliminate the air between the ultrasound probe and the skin or surface of the object and improve the efficiency of ultrasound transmission. However, traditional liquid or gel-like ultrasonic coupling agents have the following problems:

[0003] (1) Wasteful use: Liquid or gel coupling agents are easily lost during use, resulting in waste.

[0004] (2) Complex operation: Traditional coupling agents need to be frequently replenished, which increases the complexity and inconvenience of operation.

[0005] (3) Difficult to clean: After use, the coupling agent remains on the skin or the surface of the device, which can easily contaminate the patient's clothing and ultrasound equipment, increasing cleaning costs and time.

[0006] (4) Uneven coating: It is difficult to ensure the thickness and uniformity of liquid or gel coupling agent during the coating process, which affects the ultrasonic transmission effect.

[0007] (5) Bacterial growth: The gel is exposed to the air during use and is prone to breeding bacteria, posing a health hazard.

[0008] (6) Low comfort: The gel spreads easily on the skin, resulting in a poor user experience.

[0009] Patent 1 (CN201611182252.6) mixes polyurethane, polyethylene glycol and other materials to form a finished liquid, and forms an ultrasonic coupling patch after mold curing and demolding. The characteristics of each material such as polyurethane and polyethylene glycol cannot be fully utilized. It is difficult to control the thickness and uniformity of the film of the coupling patch formed by mold curing.

[0010] Patent 2 (202021436135.X) includes an adhesive layer, a base film and an upper film. The edges of the base film and the upper film are sealed to form a coupling agent accommodating chamber, in which an ultrasonic coupling agent is filled. An anti-sticking layer is provided on the adhesive layer to prevent the adhesive layer from failing. When in use, the anti-sticking layer is torn off, and the adhesive layer is bonded to the skin of the human body part to be inspected, and then the film layer is squeezed with an ultrasonic probe for ultrasonic inspection. The method of sandwiching the coupling agent between the film layer in Patent 2 is relatively complex in structure, and the coupling agent and the film layer are not firmly bonded and easily uneven, which affects the imaging quality. In addition, the overall thickness of the film layer sandwich is relatively high, and the anti-sticking layer needs to be torn off when in use.

[0011] Therefore, it is of great practical significance to develop a new type of thin film ultrasonic coupling agent to solve these problems. Summary of the invention

[0012] Based on the above problems, the present invention provides a thin film type ultrasonic coupling patch and a preparation method thereof, which aims to solve the technical problems of the existing ultrasonic coupling agent such as waste in use and difficulty in cleaning.

[0013] A thin film type ultrasonic coupling patch comprises a first thin film and a second thin film stacked together;

[0014] The first film is a polyurethane film or a polyvinyl alcohol film;

[0015] The second film is a hydroxypropyl methylcellulose film or a polyethylene glycol film;

[0016] The first film is used for contacting with the ultrasonic probe, and the second film is used for contacting with the skin.

[0017] Furthermore, the thickness of the first film is 0.05-0.2 mm.

[0018] Furthermore, the thickness of the second film is 0.01-0.05 mm.

[0019] A method for preparing a thin film type ultrasonic coupling patch, used for preparing the aforementioned thin film type ultrasonic coupling patch, comprising:

[0020] Step A1, preparing a first thin film, and forming a second thin film on the first thin film;

[0021] Step A2, subjecting the laminated layer consisting of the first film and the second film to a heat pressing treatment, and then cooling the laminated layer to obtain a thin film type ultrasonic coupling agent;

[0022] Step A3, cutting the thin film type ultrasonic coupling agent into pieces to form ultrasonic coupling patches;

[0023] Step A4, sterile packaging each ultrasound coupling patch.

[0024] Furthermore, in step A1, the first film is prepared by a film blowing method or a solution casting method.

[0025] Furthermore, in step A1, the process of forming the second film on the first film includes:

[0026] Step A11, weighing a powder material of hydroxypropyl methylcellulose or polyethylene glycol;

[0027] Step A12, adding the powder material into the solvent and stirring to form a uniform solution;

[0028] Step A13, uniformly coating the solution on the surface of the first film and then drying it to form a stacked layer of the first film and the second film.

[0029] Furthermore, in step A1, after the first film is prepared by a film blowing method or a solution casting method, the first film is cut into a predetermined size, and the second film is formed on the first film cut into the predetermined size.

[0030] Furthermore, in step A4, the packaging material for packaging the ultrasonic coupling patch is an aluminum foil bag or a vacuum packaging bag.

[0031] The beneficial technical effect of the present invention is that: the present invention forms a coupling patch of a laminated body by forming a polyurethane film or a polyvinyl alcohol film with a hydroxypropyl methylcellulose film or a polyethylene glycol film, and when in use, the second film is attached to the skin, and the surface of the first film contacts the ultrasonic probe, making full use of the uniqueness of each material, the thickness and uniformity of the film are easy to control, and the bonding of the two layers of film is also stronger than the method of sandwiching a coupling agent. It is directly attached to the skin or the surface of an object, reducing the amount of use and waste, and is easy to tear off without residue after use, simple to clean, not easy to be contaminated, and has good biocompatibility, sound permeability, wettability and comfort in use. BRIEF DESCRIPTION OF THE DRAWINGS

[0032] Figure 1-2 The present invention is a flowchart of the steps of a method for preparing a thin film ultrasonic coupling patch. DETAILED DESCRIPTION

[0033] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0034] It should be noted that, in the absence of conflict, the embodiments of the present invention and the features in the embodiments may be combined with each other.

[0035] The present invention will be further described below in conjunction with the accompanying drawings and specific embodiments, but they are not intended to limit the present invention.

[0036] The present invention provides a thin film type ultrasonic coupling patch, comprising a first thin film and a second thin film stacked;

[0037] The first film is a polyurethane film or a polyvinyl alcohol film;

[0038] The second film is a hydroxypropyl methylcellulose film or a polyethylene glycol film;

[0039] The first film is used for contacting with the ultrasonic probe, and the second film is used for contacting with the skin.

[0040] The first film is used to contact the ultrasound probe, and the surface of the second film is used to stick to the skin. Therefore, the first film is selected from a film material with good biocompatibility, sound permeability and mechanical strength. Polyurethane (PU) has good elasticity and mechanical strength and good biocompatibility. Polyvinyl alcohol (PVA) has excellent biocompatibility and sound permeability and is easy to process. The first film ensures the effective transmission of ultrasound and the durability of the patch.

[0041] The second film is a water-soluble polymer material with good wettability and appropriate viscosity. Hydroxypropyl methylcellulose (HPMC) has good wettability and biocompatibility. Polyethylene glycol (PEG) has good wettability and adjustable viscosity. The second film ensures good contact between the ultrasound probe and the skin, improving the imaging quality.

[0042] Furthermore, the thickness of the first film is 0.05-0.2 mm.

[0043] Furthermore, the thickness of the second film is 0.01-0.05 mm.

[0044] The thickness of the first film and the second film is controlled to be relatively thin, so that the coupling patch is relatively thin as a whole, to ensure that the sound waves can effectively pass through without being absorbed or scattered. If the coupling patch is too thick, it may cause the sound waves to attenuate and affect the image quality.

[0045] See also Figure 1 The present invention also provides a method for preparing a thin film type ultrasonic coupling patch, which is used to prepare the aforementioned thin film type ultrasonic coupling patch, comprising:

[0046] Step A1, preparing a first thin film, and forming a second thin film on the first thin film;

[0047] Step A2, subjecting the laminated layer consisting of the first film and the second film to a heat pressing treatment, and then cooling the laminated layer to obtain a thin film type ultrasonic coupling agent;

[0048] Step A3, cutting the thin film type ultrasonic coupling agent into pieces to form ultrasonic coupling patches;

[0049] Step A4, sterile packaging each ultrasound coupling patch.

[0050] Furthermore, in step A1, the first film is prepared by a film blowing method or a solution casting method.

[0051] Furthermore, in step A1, after the first film is prepared by a film blowing method or a solution casting method, the first film is cut into a predetermined size, and the second film is formed on the first film cut into the predetermined size.

[0052] The process of preparing the first film by solution casting includes:

[0053] In the first step, a certain amount of polyurethane (PU) or polyvinyl alcohol (PVA) powder is weighed;

[0054] In the second step, PU or PVA powder is slowly added into a suitable solvent, and slowly added under stirring to avoid agglomeration; PU powder uses dimethylformamide as solvent, and PVA uses water as solvent.

[0055] The third step is to use a magnetic stirrer or mechanical stirrer to continuously stir the solution to ensure that the U or PVA powder material is completely dissolved to form a uniform solution. The stirring time is generally 2-4 hours until the solution is clear and transparent.

[0056] Step 4: Select a flat glass plate or stainless steel plate as the substrate, clean and dry it, and evenly cast the prepared solution on the substrate;

[0057] The fifth step is to use a scraper to spread the solution into a uniform thin layer, and control the film thickness to preferably between 0.05-0.2 mm. The angle and speed of the scraper should be uniform to avoid bubbles and unevenness.

[0058] The sixth step is drying. The cast film is dried naturally at room temperature for 12-24 hours, or the cast film is placed in an oven at a temperature of 50-60° C. for 4-6 hours until the solvent is completely evaporated to form a first film.

[0059] Step 7: Peeling and cutting: After drying, carefully peel off the formed first film from the substrate. Use a cutting tool to cut it into a predetermined size, ensuring that the edges are neat.

[0060] The process of preparing the first film by the blown film method includes:

[0061] The first step is melt extrusion, where PU or PVA particles are put into the hopper of the extruder, and the extruder is heated to an appropriate temperature (about 180-200°C for PU and about 160-180°C for PVA) to melt the material.

[0062] The second step is film blowing, which involves extruding the molten material through an extruder, and using a film blowing machine to blow the molten material into a first film by controlling the airflow. The temperature, pressure and speed of the film blowing machine are adjusted to obtain a uniform film thickness (0.05-0.2mm).

[0063] The third step is cooling and winding. The first film formed by blowing is cooled by a cooling roller to ensure that the film is fixed. The cooled first film is wound by a winder to form a coil. Use a cutting tool to cut it into a predetermined size to ensure that the edges are neat.

[0064] See also Figure 2 Further, in step A1, the process of forming the second film on the first film includes:

[0065] Step A11, weighing a powder material of hydroxypropyl methylcellulose or polyethylene glycol;

[0066] Step A12, adding the powder material into the solvent and stirring to form a uniform solution;

[0067] Step A13, uniformly coating the solution on the surface of the first film and then drying it to form a stacked layer of the first film and the second film.

[0068] In step A11, a certain amount of hydroxypropyl methylcellulose (HPMC) or polyethylene glycol (PEG) powder is weighed.

[0069] In step A12, HPMC or PEG powder is slowly added to a suitable solvent (such as water or ethanol) and slowly added under stirring to avoid lumps. The solution is continuously stirred using a magnetic stirrer or a mechanical stirrer to ensure that the HPMC or PEG powder material is completely dissolved to form a uniform solution. The stirring time is generally 2-4 hours until the solution is clear and transparent.

[0070] In step A13, a flat first film is selected as a substrate, cleaned and dried. The prepared HPMC or PEG solution is evenly coated on the surface of the first film. A scraper or coater is used to control the coating thickness. The angle and speed of the scraper should be uniform to avoid bubbles and unevenness. The first film coated with HPMC or PEG is naturally dried at room temperature for 12-24 hours. Alternatively, the first film coated with HPMC or PEG is placed in an oven, the temperature is controlled at 50-60°C, and the drying time is 4-6 hours until the solvent is completely evaporated. Alternatively, the film coated with HPMC or PEG is placed in an oven, the temperature is controlled at 50-60°C, and the drying time is 4-6 hours until the solvent is completely evaporated, thereby forming a second film on the first film to form a laminate of the first film and the second film.

[0071] In step A2, preheat the heat press to an appropriate temperature (e.g., 60-80°C), and then preheat the laminate of the first film and the second film to an appropriate temperature (e.g., 60-80°C). Place the preheated laminate in the heat press and perform heat pressing at an appropriate temperature and pressure (e.g., 80°C, 0.1-0.5MPa). Control the heat pressing time (e.g., 30-60 seconds) to ensure that the first film and the second film are tightly bonded. Cool naturally after heat pressing or cool quickly through a cooling system. Check to ensure that the second film is uniform and free of bubbles.

[0072] Furthermore, in step A4, the packaging material for packaging the ultrasonic coupling patch is an aluminum foil bag or a vacuum packaging bag.

[0073] Cut the prepared thin-film ultrasonic coupling patch into a suitable size (e.g., 10 cm × 10 cm), ensure that the edges are neat, and perform packaging operations in a sterile environment to avoid bacterial contamination. Use aluminum foil bags or vacuum packaging bags for packaging to ensure that the product is not contaminated during storage. In step A4, use a sealing machine to seal the packaging bag to ensure good sealing.

[0074] Before use, clean the skin of the area to be inspected or treated to ensure that there is no grease and dirt. Apply the second film surface of the thin-film type ultrasound coupling patch to the skin, press gently to make it fit tightly, and ensure that there are no bubbles between the coating and the skin. Use an ultrasound probe to inspect or treat on the second film surface. The thin-film coupling patch can effectively transmit ultrasound to ensure imaging quality. After the inspection or treatment is completed, gently peel off the thin-film type ultrasound coupling patch. There will be no residue on the skin surface and it is easy to clean. The thin-film type ultrasound coupling patch of the present invention can achieve excellent sound permeability, wettability and viscosity, ensuring the use effect and convenience of cleaning.

[0075] The present invention forms a coupling patch of a laminated body by forming a polyurethane film or a polyvinyl alcohol film and a hydroxypropyl methylcellulose film or a polyethylene glycol film. When in use, the second film is attached to the skin, and the surface of the first film contacts the ultrasonic probe, thereby making full use of the uniqueness of each material, making it easy to control the thickness and uniformity of the film, and the bonding of the two layers of film is stronger than that of the method of sandwiching a coupling agent, and also having the following technical effects:

[0076] (1) Reduce waste: The film-type coupling patch is directly attached to the skin or the surface of the object, and is not easily lost during use, thus reducing waste and usage.

[0077] (2) Easy to operate: No need for frequent refilling, easy to use and simple to operate.

[0078] (3) Easy to clean: The film can be easily torn off after use, leaving no residue and making cleaning simple.

[0079] (4) Uniform coating: The film thickness is uniform, ensuring stable ultrasonic transmission effect.

[0080] (5) Environmental protection and health: The selection of materials focuses on environmental protection and biocompatibility to reduce the impact on the human body and the environment.

[0081] The above are only preferred embodiments of the present invention, and are not intended to limit the implementation methods and protection scope of the present invention. Those skilled in the art should be aware that all solutions obtained by equivalent substitutions and obvious changes made using the description and illustrations of the present invention should be included in the protection scope of the present invention.

Claims

1. A thin film ultrasonic coupling patch, characterized in that: comprising a first film and a second film stacked; The first film is a polyurethane film or a polyvinyl alcohol film; The second film is a hydroxypropyl methylcellulose film or a polyethylene glycol film; The first film is used for contacting with the ultrasonic probe, and the second film is used for contacting with the skin.

2. A thin film type ultrasonic coupling patch as claimed in claim 1, characterized in that: The thickness of the first film is 0.05-0.2 mm.

3. A thin film type ultrasonic coupling patch as claimed in claim 1, characterized in that: The thickness of the second film is 0.01-0.05 mm.

4. A method for preparing a thin film ultrasonic coupling patch, characterized in that: A method for preparing a thin film ultrasonic coupling patch as claimed in any one of claims 1 to 3, comprising: Step A1, preparing a first thin film, and forming a second thin film on the first thin film; Step A2, subjecting the laminated layer composed of the first film and the second film to a heat pressing treatment, and then cooling the laminated layer to obtain the thin film type ultrasonic coupling agent; Step A3, cutting the thin film type ultrasonic coupling agent into pieces to form ultrasonic coupling patches; Step A4, sterile packaging each piece of the ultrasound coupling patch.

5. The method for preparing a thin film type ultrasonic coupling agent according to claim 4, characterized in that: In the step A1, the first film is prepared by a film blowing method or a solution casting method.

6. The method for preparing a thin film type ultrasonic coupling agent according to claim 4, characterized in that: In the step A1, the process of forming the second film on the first film includes: Step A11, weighing a powder material of hydroxypropyl methylcellulose or polyethylene glycol; Step A12, adding the powder material into a solvent and stirring to form a uniform solution; Step A13, uniformly coating the solution on the surface of the first film and then drying it to form a stacked layer of the first film and the second film.

7. The method for preparing a thin film type ultrasonic coupling agent according to claim 5, characterized in that: In the step A1, after the first film is prepared by a film blowing method or a solution casting method, the first film is cut into a predetermined size, and the second film is formed on the first film cut into the predetermined size.

8. The method for preparing a thin film type ultrasonic coupling agent according to claim 4, characterized in that: In step A4, the packaging material for packaging the ultrasonic coupling patch is an aluminum foil bag or a vacuum packaging bag.