Novel method for circularly producing potassium nitrate and ammonium chloride
Through the recycling production process of dilute nitric acid, limestone and potassium chloride, the safety hazards of ammonium nitrate storage and the problems of treatment of by-product magnesium chloride are solved, and the production of high-purity potassium nitrate and the recycling of ammonium chloride are realized, reducing production costs and resources waste.
Patent Information
- Application Number
- CN202411089961.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-09
- Publication Date
- 2024-11-12
AI Technical Summary
In the existing potassium nitrate production process, there are great storage safety risks of ammonium nitrate, and it is difficult to deal with by-product magnesium chloride aqueous solution, resulting in high production costs and waste of resources.
Dilute nitric acid, limestone and potassium chloride are used as raw materials, and potassium nitrate and ammonium chloride are prepared through neutralization reaction, filtration, cooling and evaporation, so as to realize the recycling of raw materials and the reuse of by-products.
It solves the safety hazards of ammonium nitrate storage, reduces production costs, improves the purity and output of potassium nitrate, realizes the recycling of resources, and adapts to the needs of industrial production.
Smart Images

Figure BDA0004986252050000051
Abstract
Description
Technical field:
[0001] The invention relates to the field of inorganic chemical raw material product production, mainly to a new process method for cyclically producing potassium nitrate, and in particular to a new method for cyclically producing potassium nitrate and ammonium chloride. Background technology:
[0002] Potassium nitrate, commonly known as saltpeter, is a colorless, transparent orthorhombic crystal or rhombic crystal or white powder. It is odorless, non-toxic, salty, refreshing, low in hygroscopicity, not easy to agglomerate, and easily soluble in water. Potassium nitrate is an inorganic chemical product with a wide range of uses. It is a chlorine-free, high-quality fertilizer in agriculture. It is widely used in gunpowder, fireworks, metal welding aids, synthetic ammonia catalysts, ceramics, etc. in industry. It is used as a colorant and preservative for meat products in food. It is used as a diuretic, a coolant, and a raw material for the production of penicillin potassium salt, rifampicin, etc. in medicine. In optical glass products, it is a raw material for the production of high-end chemically strengthened glass such as mobile phone screens and tablet computer displays. With the further expansion of the scope of use of potassium nitrate, people have higher and higher requirements for the output and purity of potassium nitrate. And with its wide application, people are constantly exploring and researching the production of potassium nitrate.
[0003] As disclosed in the Chinese patent announcement CN103771464B, "Method for preparing potassium nitrate by double decomposition", the present invention is a method for preparing potassium nitrate by double decomposition using ammonium nitrate and potassium chloride as raw materials, and relates to the field of inorganic chemical technology. The mother liquor of this process is recycled. Since the raw material potassium chloride brings in impurities, the mother liquor has the problem of accumulation and treatment of impurities in long-term circulation, which has not been solved. The present invention is characterized in that a shunt impurity removal production line is set up next to the production device, wherein a sodium and magnesium removal unit is set up, and 1 to 30% of the total circulation amount of the mother liquor is introduced into the production line for impurity removal treatment. The main components of the impurities are water-soluble sodium salts and magnesium salts. Magnesium chloride is used as a salting-out agent to remove sodium salts, and ammonium bicarbonate is used as a precipitant to remove magnesium salts. The solution temperature is 10°C to 90°C, and the mother liquor after impurity removal is returned to the mother liquor circulation system.
[0004] Application publication number CN 112142075 A, invention name "A method for preparing potassium nitrate and potassium nitrate thereof"; the present invention discloses a method for preparing potassium nitrate and potassium nitrate thereof. The preparation method comprises the following steps: step S1, reaction: adding raw potassium hydroxide into water to form a solution, then adding nitric acid into the solution, stirring and reacting in an ice-water mixture for 10-30 minutes; then heating the reacted solution to 50-60°C, then cooling to 4-8°C for cooling crystallization, then putting it into a centrifuge and adding elution water for separation to obtain mother liquor M1 of potassium nitrate and potassium hydroxide; drying to obtain potassium nitrate product. The preparation method has short process flow, low energy consumption, small equipment corrosiveness and circulation load, green production process, high production efficiency, and is suitable for large-scale production. The prepared potassium nitrate product has high purity and easy-to-obtain raw materials.
[0005] Application publication number CN 108423693 A, disclosed invention name "High-yield preparation method of potassium nitrate", the present invention discloses a high-yield preparation method of potassium nitrate. It includes raw material configuration, the raw material configuration includes mixing and dissolving raw materials ammonium nitrate and potassium chloride with water in a certain ratio to form a mixed solution, and the raw material configuration also includes adding potassium chloride emulsion to the mixed solution formed by the mixed dissolution of raw materials at a certain temperature when the potassium chloride dissolution reaches a saturated state. This method makes the potassium ions and nitrate ions in the ingredient solution reach a balanced match to the maximum extent in a way of making up for the shortcomings, and the output rate of potassium nitrate is high, which relatively reduces energy consumption and production costs, and improves production efficiency.
[0006] There is also a new process for producing potassium nitrate by sodium nitrate conversion (Zhang Gang. Chemical Engineering Design, 2009, 19 (5)), which discloses a method for producing potassium nitrate. In the process of producing potassium nitrate by double decomposition of sodium nitrate and potassium chloride, it is noted that impurities in the mother liquor should be accumulated and treated, and it is proposed that the mother liquor should be treated regularly to remove impurities to ensure qualified product quality and normal production operation. It is proposed that the main impurities in the mother liquor are sodium nitrite, sodium sulfate and magnesium chloride. The solution is to add ammonium nitrate to remove sodium nitrite, add barium chloride to remove sodium sulfate, and add potassium carbonate to remove magnesium chloride. The disadvantage is that there is no technology for removing impurities from the circulating mother liquor of the potassium nitrate production device disclosed in the present invention.
[0007] The invention titled "A method for strengthening the separation of by-product ammonium chloride in the production of potassium nitrate by double decomposition" disclosed in Chinese application number 201510483618.2 discloses a method for strengthening the separation of by-product ammonium chloride in the production of potassium nitrate by double decomposition. The method of the present invention is based on the traditional double decomposition process for producing potassium nitrate, and adds C12-C20 high-grade straight-chain fatty amines and other flotation reagents to the reaction system. Under certain pH conditions, after reaction and crystallization, the by-product ammonium chloride is effectively separated from potassium nitrate by foam entrainment of ammonium chloride under stirring or pumping. Compared with the washing and hot dissolution processes in traditional production, this method has the advantages of simple operation, low dosage of reagents and good separation effect. On the one hand, the grade of crude potassium nitrate is improved, and the content of impurities such as NH4+ and Cl is significantly reduced; on the other hand, the energy-saving and consumption-reducing effect is significant, and the water consumption in the washing process is reduced. It is applied to the large-scale continuous production of potassium nitrate by double decomposition of potassium chloride and ammonium nitrate, with obvious economic and social benefits. And so on.
[0008] From the above-mentioned disclosed method for producing potassium nitrate, at present, there are mainly two kinds of potassium nitrate production process methods, namely, ammonia method and magnesium nitrate method. Ammonia method is a double decomposition production process of ammonium nitrate and potassium chloride. The disadvantages of this process technology are: high cost, and another main reason is that due to the severe state of the current safety production situation, the storage requirements for ammonium nitrate as an explosive are very strict, and ordinary chemical industrial production enterprises are generally not allowed to store a large amount of storage, and it is necessary to report to the corresponding management departments such as public security and other administrative management agencies, which greatly affects the industrial production of enterprises and causes production inconvenience for industrial enterprises. Therefore, many enterprises adopt the magnesium nitrate method to produce potassium nitrate.
[0009] The continuous advancement of the process technology of producing potassium nitrate by magnesium nitrate method has the disadvantage that the byproduct of a large amount of magnesium chloride aqueous solution is difficult to handle, thus affecting the factory production. Magnesium chloride aqueous solution generally contains 4.0-5.0% potassium nitrate (calculated as potassium oxide), which cannot be reused to participate in the production cycle and is lost in vain, which not only wastes precious potassium resources, but also greatly increases the production cost of potassium nitrate. Finding other raw material substitutes and different process routes has become inevitable for the industrial production of potassium nitrate products.
[0010] Therefore, how to provide a production process of potassium nitrate and its byproducts with easy-to-obtain raw materials and simple production process, that is, to provide a new method for cyclic production of potassium nitrate and ammonium chloride. Common limestone, dilute nitric acid and potassium chloride can be used as main raw materials to produce potassium nitrate products and ammonium chloride byproducts, so that the raw materials can be fully recycled, and the prepared potassium nitrate product has a high purity and meets the quality requirements for optical glass. At the same time, the byproduct ammonium chloride can be continuously recycled to achieve the recycling of resources, which is a need of current practical production. It has good economic and social benefits. Summary of the invention:
[0011] The present invention provides a new method for cyclically producing potassium nitrate and ammonium chloride, which is prepared by using dilute nitric acid, limestone, potassium chloride and ammonium bicarbonate as raw materials, including potassium nitrate and by-product ammonium chloride. The method of the present invention is adopted to prepare potassium nitrate products, which is in line with the times to adapt to the market environment safety and can meet the requirements of industrialized economy and market, and better solves the safety hazard requirements of raw material ammonium nitrate during storage during the current potassium nitrate production. The raw materials are easy to obtain, and the by-product ammonium chloride produced can be applied to agricultural production requirements.
[0012] The present invention aims to provide a new method for cyclically producing potassium nitrate and ammonium chloride, which uses dilute nitric acid, limestone, potassium chloride and ammonium bicarbonate as raw materials, including potassium nitrate and by-product ammonium chloride; the method is characterized in that the steps of preparing potassium nitrate are as follows:
[0013] (1) raw material configuration reaction, limestone is placed in a reaction tank device, and then dilute nitric acid is slowly added to react with the limestone in the reaction tank device to neutralize and discharge carbon dioxide; after the reaction is completed, a neutralization reaction solution is obtained;
[0014] (2) Filtration; The neutralization reaction solution is filtered using a plate and frame filter to obtain a filtrate as a mother liquor 1 and a filter residue,
[0015] (3) a secondary batching reaction, wherein potassium chloride is added to the mother solution 1 of step (2) in portions, and a dissolution reaction is carried out under continuous stirring and heating conditions to obtain a dissolution reaction solution, which is the mother solution 2;
[0016] (4) Filtration and cooling crystallization: The mother liquor 2 in the previous step is filtered using a plate and frame filter device, and subjected to cooling crystallization treatment to precipitate potassium nitrate crystals and a potassium nitrate solid-liquid mixture.
[0017] (5) separation and rinsing, separating the solid-liquid mixture of potassium nitrate from step (4) to obtain a semi-finished potassium nitrate product, rinsing and purifying the semi-finished potassium nitrate product with clean water, and drying and packaging the semi-finished potassium nitrate product, the separation solution and the rinsing solution;
[0018] (6) freezing crystallization, placing the separated solution rinse liquid of step (5) in a freezing device for freezing crystallization treatment, controlling the temperature during freezing crystallization treatment to be -10 to -20°C, freezing the solid-liquid separation again to obtain a calcium chloride solution and a frozen crystallized solid, the frozen crystallized solid is a potassium nitrate semi-finished product, and repeating the rinsing, purification, and drying steps of step (5) to package the potassium nitrate finished product;
[0019] (7) recycling, converting the frozen liquid separated in step (6) into a calcium chloride solution, and then using it in the ammonium chloride preparation process for recycling production;
[0020] The steps of the ammonium chloride preparation method are as follows:
[0021] A) preparing an ammonium chloride raw material preparation reaction, fully mixing the calcium chloride frozen solution and the ammonium bicarbonate solution in step (7), reacting to generate a calcium carbonate solution, and releasing carbon dioxide gas;
[0022] B) flocculation solidification precipitation, adding a calcium agent flocculant to the calcium carbonate solution in step A) to promote the precipitation of potassium nitrate wrapped in the calcium carbonate reaction solution; obtaining potassium nitrate precipitation and feed solution;
[0023] C) solid-liquid separation, the feed liquid of step B) is subjected to plate-and-frame filtration to obtain solid calcium carbonate and ammonium chloride solution; the solidified calcium carbonate is returned to step (1) as raw material;
[0024] D) evaporation, the ammonium chloride solution in step C) is evaporated, and then cooled to room temperature to crystallize a large amount of ammonium chloride, which is filtered and dried to obtain the ammonium chloride product.
[0025] Preferably, the new method for cyclically producing potassium nitrate and ammonium chloride is to control the mass concentration of the raw material dilute nitric acid to 50-62Wt%, and to control the volume and mass ratio of dilute nitric acid, calcium carbonate, potassium chloride and ammonium bicarbonate to 65-90L:60-85Kg:58-80Kg:60-85Kg.
[0026] The novel method for cyclically producing potassium nitrate and ammonium chloride comprises the following steps (1): adding process flushing water during the reaction process so that the limestone in the reaction tank device can fully undergo a neutralization reaction; after the reaction is completed; adjusting the pH value of the neutralization reaction solution to 4.2-6.5 with slaked lime, and controlling the concentration of the neutralization reaction solution to 35-40 Be.
[0027] The novel method for cyclically producing potassium nitrate and ammonium chloride, step (3), after all the potassium chloride is added and fully reacted, the heating reaction temperature is controlled to be 90-105°C, the reaction is carried out for 30-50 minutes, and the concentration of the mother liquor 2 is controlled to be 39-45Be.
[0028] In the novel method for cyclic production of potassium nitrate and ammonium chloride, step (4) cooling crystallization treatment is to add 0-10°C carbon dioxide into the mother liquor 2 for cooling crystallization, and the temperature of the solution during the cooling crystallization treatment is controlled at 25-35°C.
[0029] The novel method for cyclically producing potassium nitrate and ammonium chloride comprises the following steps: step A) the calcium agent flocculant is calcium hypochlorite or a mixture of calcium hypochlorite, polyacrylamide and calcium hydroxide in equal mass ratio, and the amount of the calcium agent flocculant added is controlled to be 0.1-0.2% of the mass of the calcium carbonate solution.
[0030] The main chemical equations involved in the method of the present invention are:
[0031] 1. Limestone (calcium carbonate) reacts with dilute nitric acid to produce calcium nitrate.
[0032] CaCO3+2HNO3→Ca(NO3)2+CO2+H2O,
[0033] 2. Calcium nitrate undergoes double decomposition reaction with potassium chloride to generate potassium nitrate.
[0034] Ca(NO3)2+2KCL→2KNO3+CaCL2,
[0035] 3. Calcium chloride aqueous solution reacts with ammonium bicarbonate to produce calcium carbonate and ammonium chloride.
[0036] CaCL2+2NH4HCO3→CaCO3+2NH4CL+CO2+H2O.
[0037] By controlling the addition and progress of various components in each chemical reaction process in the above reaction, a potassium nitrate product with higher purity can be prepared.
[0038] The invention discloses a new method for cyclic production of potassium nitrate and ammonium chloride. The above technical scheme is used to prepare potassium nitrate, which has the following beneficial effects. First, potassium nitrate is produced using dilute nitric acid, limestone and potassium chloride as raw materials. The raw materials are easy to obtain and store, and there is no safety hazard in the storage of raw materials. The by-product calcium chloride aqueous solution is treated with ammonium bicarbonate, and the precipitated calcium carbonate is re-invested in the cyclic production of potassium nitrate; and the separated ammonium chloride solution evaporates and crystallizes the by-product ammonium chloride product, which can be used for agricultural production fertilizer. Second, the new process of the invention does not use ammonium nitrate, eliminating the hidden danger of raw material storage; because with the necessity of safe production, the country pays more and more attention to safe production, and the existing general chemical production enterprises are not allowed to store ammonium nitrate raw materials in the company's ordinary warehouses, and need to be stored in special warehouses with higher safety conditions. The current company produces and uses the raw materials of ammonium nitrate. After reporting to the safety management agency for approval, it can only purchase a small amount for storage and use, which seriously affects the production and operation of the enterprise and greatly increases the production cost of the enterprise. Therefore, it is inevitable to explore other production process paths and raw material replacement for the production of potassium nitrate; third, the new process of the present invention is cyclically produced continuously, and there are no difficult-to-handle by-products. The by-product ammonium chloride is one of the main raw materials for the production of fertilizers, with large market demand, cost-effectiveness, and no production bottleneck in the factory. Fourth, the present invention adds a special calcium agent flocculant when treating calcium chloride aqueous solution with ammonium bicarbonate. It has been proven through practical use that it can cause about 40% of potassium nitrate in the calcium carbonate solution generated by the reaction to settle down and enter the production cycle for reuse, which greatly increases the yield of potassium nitrate by 1.5-2.0%. At the same time, in order to increase the yield of potassium nitrate, the present invention adopts a two-step cooling and freezing potassium nitrate crystallization method, thereby greatly increasing the yield and purity of potassium nitrate products, and its product content reaches more than 99.65%. The above-mentioned new process method for potassium nitrate disclosed by the present invention has easy-to-obtain raw materials, no safety hazards in storage, simple process, and low production cost. It has good economic and social benefits.
[0039] The potassium nitrate product prepared by the novel method of the present invention was tested by the National Inorganic Salt Product Quality Supervision and Inspection Center, and the test results are as follows, as shown in Table 1:
[0040] Product Name: Potassium Nitrate,
[0041] Inspection category: production license application inspection,
[0042] Sampling method: According to the implementation rules,
[0043] Sampling locations: Inventor's company, product warehouse,
[0044] Sampling base: 250g×2 bottles / 30 tons,
[0045] Sample state: white crystals.
[0046] Table 1
[0047]
[0048] Note: The data in the comparative example are without adding calcium agent flocculant, and the purity of the potassium nitrate product prepared therefrom is slightly lower than that of the example of the present invention, but still higher than the requirements of the national standard. Specific implementation method:
[0049] The present invention is further described below in conjunction with specific embodiments. The present invention is not limited to the embodiments. The limestone or calcium carbonate described in the embodiments of the present invention has the same meaning and the main components are the same;
[0050] The invention discloses a new method for cyclically producing potassium nitrate and ammonium chloride, which uses dilute nitric acid, limestone, potassium chloride and ammonium bicarbonate as raw materials, and comprises the preparation of potassium nitrate and by-product ammonium chloride; the steps of the potassium nitrate preparation method are as follows:
[0051] (1) Raw material configuration reaction, limestone is placed in a reaction tank device, and then dilute nitric acid is slowly added to neutralize the limestone in the reaction tank device to discharge carbon dioxide; process flushing water is added during the reaction process to allow the limestone in the reaction tank device to fully undergo neutralization reaction, and after the reaction is completed; slaked lime is used to adjust the pH value of the neutralization reaction solution to 4.2-6.5, and the concentration of the neutralization reaction solution is controlled to 35-40Be; the mass concentration of the raw material dilute nitric acid is controlled to 50-62Wt%, and the volume and mass ratio of dilute nitric acid, calcium carbonate, potassium chloride, and ammonium bicarbonate is controlled to 65-90L:60-85Kg:58-80Kg:60-85Kg; after the reaction is completed, a neutralization reaction solution is obtained;
[0052] (2) Filtration; The neutralization reaction solution is filtered using a plate and frame filter to obtain a filtrate as a mother liquor 1 and a filter residue,
[0053] (3) Secondary batching reaction, adding potassium chloride to the mother liquor 1 of step (2) in portions, dissolving and reacting under continuous stirring and heating conditions, and controlling the heating reaction temperature to 90-105° C. to react fully, and controlling the concentration of the mother liquor 2 to 39-45 Be to obtain a dissolving reaction solution, which is the mother liquor 2;
[0054] (4) Filtration and cooling crystallization: The mother liquor 2 in the previous step is filtered by a plate-and-frame filter device and subjected to cooling crystallization treatment, wherein 0-10° C. carbon dioxide is charged into the mother liquor 2 for cooling crystallization, and the temperature of the solution during the cooling crystallization treatment is controlled at 25-35° C. Potassium nitrate crystals and a potassium nitrate solid-liquid mixture are precipitated;
[0055] (5) separation and rinsing, separating the solid-liquid mixture of potassium nitrate from step (4) to obtain a semi-finished potassium nitrate product, rinsing and purifying the semi-finished potassium nitrate product with clean water, and drying and packaging the semi-finished potassium nitrate product, the separation solution and the rinsing solution;
[0056] (6) freezing crystallization, placing the separated solution rinse liquid of step (5) in a freezing device for freezing treatment, controlling the temperature during freezing treatment to be -10 to -20°C, freezing again for solid-liquid separation to obtain a frozen separated liquid and a frozen crystallized solid, the frozen crystallized solid is a potassium nitrate semi-finished product, and repeating the rinsing, purification, and drying steps of step (5) to obtain a finished potassium nitrate product by packaging;
[0057] (7) recycling, wherein the frozen liquid separated in step (6) is the calcium chloride solution, and then used in the ammonium chloride preparation process for recycling production;
[0058] The preparation of ammonium chloride: that is, the preparation method of by-product ammonium chloride comprises the following steps:
[0059] A) preparing an ammonium chloride raw material preparation reaction, fully mixing the calcium chloride solution and the ammonium bicarbonate solution of step (7), reacting to generate a mixed suspension solution of calcium carbonate and ammonium chloride, and releasing carbon dioxide gas;
[0060] B) Flocculation solidification precipitation, adding a calcium flocculant to the mixed suspension solution of calcium carbonate and ammonium chloride in step A), wherein the calcium flocculant is calcium hypochlorite or a mixture of calcium hypochlorite + polyacrylamide and calcium hydroxide in equal mass ratio, and the amount of calcium flocculant added is controlled to be 0.1-0.2% of the mass of calcium carbonate. This promotes the precipitation of potassium nitrate in the reaction solution wrapped by calcium carbonate, that is, promotes the separation and precipitation of a trace amount of potassium nitrate wrapped in the calcium carbonate suspension solution, thereby greatly improving the yield of potassium nitrate; potassium nitrate precipitation and feed solution are obtained;
[0061] C) solid-liquid separation, the feed liquid of step B) is subjected to plate-and-frame filtration to obtain solid calcium carbonate and ammonium chloride solution; the solid calcium carbonate is returned to step (1) as raw material;
[0062] D) evaporation, the ammonium chloride solution of step C) is evaporated, and then cooled to room temperature to crystallize a large amount of ammonium chloride, which is filtered and dried to obtain the ammonium chloride product.
[0063] The present invention adopts the above method to prepare potassium nitrate, and its raw materials are easy to obtain, mainly using dilute nitric acid, limestone, potassium chloride and ammonium bicarbonate as raw materials. The limestone, i.e., calcium carbonate raw material, has low requirements and is easy to obtain. At the same time, its by-product ammonium chloride can be used as an agricultural production fertilizer. Therefore, in the process of producing potassium nitrate products, the by-products can be recycled, will not cause impact on the social environment, and has good economic and social benefits.
[0064] Example 1
[0065] The invention discloses a new method for cyclically producing potassium nitrate and ammonium chloride, which uses dilute nitric acid, limestone, potassium chloride and ammonium bicarbonate as raw materials, and comprises the preparation of potassium nitrate and by-product ammonium chloride; the steps of the potassium nitrate preparation method are as follows:
[0066] (1) Raw material configuration reaction, limestone is placed in a reaction tank device, and then dilute nitric acid is slowly added to neutralize the limestone in the reaction tank device to discharge carbon dioxide; process flushing water is added during the reaction process to allow the limestone in the reaction tank device to fully undergo neutralization reaction, and after the reaction is completed; slaked lime is used to adjust the pH value of the neutralization reaction solution to 5.5-6.0, and the concentration of the neutralization reaction solution is controlled to 35-40Be; the mass concentration of the raw material dilute nitric acid is controlled to 60Wt%, and the volume and mass ratio of dilute nitric acid, calcium carbonate, potassium chloride, and ammonium bicarbonate is controlled to 65-90L:60-85Kg:58-80Kg:60-85Kg; after the reaction is completed, a neutralization reaction solution is obtained;
[0067] (2) Filtration; The neutralization reaction solution is filtered using a plate and frame filter to obtain a filtrate as a mother liquor 1 and a filter residue, and the content of calcium and chloride ions in the mother liquor 1 is detected. The amount of potassium chloride added is obtained according to the above calculation data, and the step (3) is entered to slowly add potassium chloride to the reaction device in steps.
[0068] (3) Secondary batching reaction, potassium chloride is added to the mother solution 1 of step (2) in batches and steps, and the dissolution reaction is carried out under continuous stirring and heating conditions. After all the potassium chloride is added and fully reacted, the heating reaction temperature is controlled to be 90-105°C, and the reaction is carried out for 30-50 minutes, and the concentration of the mother solution 2 is controlled to be 39-45Be. The amount of potassium chloride added is controlled by the mother solution 2 obtained by the above reaction, and the addition is stopped when the solution concentration reaches the above 39Be; the dissolution reaction solution is obtained, which is the mother solution 2;
[0069] (4) Filtration and cooling crystallization: The mother liquor 2 in the previous step is filtered by a plate-and-frame filter device and subjected to cooling crystallization treatment. The cooling crystallization treatment is to fill the mother liquor 2 with 0-5°C carbon dioxide gas, so that the mother liquor 2 can be continuously tumbled and stirred under the above low temperature conditions, so that the solution is fully cooled and mixed, thereby achieving efficient cooling crystallization, that is, gas cooling is used for cooling, and the temperature of the solution during the cooling crystallization treatment is controlled to be between 30°C. The precipitated potassium nitrate crystals and potassium nitrate solid-liquid mixture are obtained by filtration;
[0070] (5) separation and rinsing, separating the solid-liquid mixture of potassium nitrate from step (4) to obtain a semi-finished potassium nitrate product, rinsing and purifying the semi-finished potassium nitrate product with clean water, and drying and packaging the semi-finished potassium nitrate product, the separation solution and the rinsing solution;
[0071] (6) freezing crystallization, placing the separation solution and the washing liquid in step (5) in a freezing device for freezing treatment, controlling the temperature during the freezing treatment to be -10 to -20°C, freezing again for solid-liquid separation to obtain a frozen separation liquid and a frozen crystallized solid, the frozen crystallized solid is a potassium nitrate semi-finished product, and repeating the washing, purification and drying steps of step (5) to package the potassium nitrate product;
[0072] (7) recycling, wherein the frozen liquid separated in step (6) is the calcium chloride solution, and then used in the ammonium chloride preparation process for recycling production;
[0073] The preparation of ammonium chloride: that is, the preparation method of by-product ammonium chloride comprises the following steps:
[0074] A) preparing an ammonium chloride raw material preparation reaction, fully mixing the calcium chloride solution and the ammonium bicarbonate solution of step (7), reacting to generate a mixed suspension solution of calcium carbonate and ammonium chloride, and releasing carbon dioxide gas to be recovered for use as a cooling medium during cooling crystallization;
[0075] B) Flocculation solidification precipitation: add calcium flocculant to the mixed suspension solution of calcium carbonate and ammonium chloride in step A), wherein the calcium flocculant is calcium hypochlorite, and the amount of calcium flocculant added is controlled to be 0.15% of the mass of calcium carbonate. The calcium carbonate is used to encapsulate the potassium nitrate in the reaction solution and precipitate it; thus obtaining potassium nitrate precipitate and feed solution;
[0076] C) solid-liquid separation, the feed liquid of step B) is subjected to plate-and-frame filtration to obtain solid calcium carbonate and ammonium chloride solution; the solidified calcium carbonate is returned to step (1) as raw material;
[0077] D) evaporation, the ammonium chloride solution in step C) is evaporated, and then cooled to room temperature to crystallize a large amount of ammonium chloride, which is filtered and dried to obtain the ammonium chloride product.
[0078] Example 2
[0079] The invention discloses a new method for cyclically producing potassium nitrate and ammonium chloride, which uses dilute nitric acid, limestone, potassium chloride and ammonium bicarbonate as raw materials, and comprises the preparation of potassium nitrate and by-product ammonium chloride; the steps of the potassium nitrate preparation method are as follows:
[0080] (1) Raw material configuration reaction, limestone is placed in a reaction tank device, and then dilute nitric acid is slowly added to neutralize the limestone in the reaction tank device to discharge carbon dioxide; process flushing water is added during the reaction process to allow the limestone in the reaction tank device to fully undergo a neutralization reaction, and after the reaction is completed; slaked lime is used to adjust the pH value of the neutralization reaction solution to 4.2, and the concentration of the neutralization reaction solution is controlled to be 35-40Be; the mass concentration of the raw material dilute nitric acid is controlled to be 61Wt%, and the volume and mass ratio of dilute nitric acid, calcium carbonate, potassium chloride, and ammonium bicarbonate is controlled to be 65-90L:60-85Kg:58-80Kg:60-85Kg; after the reaction is completed, a neutralization reaction solution is obtained;
[0081] (2) Filtration; The neutralization reaction solution is filtered using a plate and frame filter to obtain a filtrate as a mother liquor 1 and a filter residue,
[0082] (3) Secondary batching reaction, adding potassium chloride to the mother solution 1 of step (2) in batches and steps, dissolving and reacting under continuous stirring and heating conditions, and controlling the heating reaction temperature to 95-105° C. for 30-50 minutes after all the potassium chloride is added and fully reacted, and controlling the concentration of the mother solution 2 to 39-45 Be. Obtaining a dissolving reaction solution, which is the mother solution 2;
[0083] (4) Filtration and cooling crystallization: The mother liquor 2 in the previous step is filtered by a plate-and-frame filter device and subjected to cooling crystallization treatment. The cooling crystallization treatment is to fill the mother liquor 2 with 0-5°C carbon dioxide gas, so that the mother liquor 2 can be continuously tumbled and stirred under the above-mentioned low temperature conditions, so that the solution is fully cooled and mixed, thereby achieving efficient cooling crystallization, that is, gas cooling is used for cooling, and the temperature of the solution during the cooling crystallization treatment is controlled to be between 25 and 35°C. The precipitated potassium nitrate crystals and potassium nitrate solid-liquid mixture are obtained by filtration;
[0084] (5) separation and rinsing, separating the solid-liquid mixture of potassium nitrate from step (4) to obtain a semi-finished potassium nitrate product, rinsing and purifying the semi-finished potassium nitrate product with clean water, and drying and packaging the semi-finished potassium nitrate product, the separation solution and the rinsing solution;
[0085] (6) freezing crystallization, placing the separated solution rinse liquid of step (5) in a freezing device for freezing treatment, controlling the temperature during freezing treatment to be -10 to -20°C, freezing the solid-liquid separation again to obtain a frozen separated liquid and a frozen crystallized solid, and in order to improve the extraction yield of potassium nitrate, adding an appropriate amount of saturated potassium nitrate solution to the above-mentioned separated liquid so that potassium nitrate can be rapidly crystallized and precipitated, while improving the yield and purity of potassium nitrate; the frozen crystallized solid is a potassium nitrate semi-finished product, and the rinsing, purification and drying steps of step (5) are repeated to obtain a finished potassium nitrate product by packaging;
[0086] (7) recycling, wherein the frozen liquid separated in step (6) is the calcium chloride solution, and then used in the ammonium chloride preparation process for recycling production;
[0087] The preparation of ammonium chloride: that is, the preparation method of by-product ammonium chloride comprises the following steps:
[0088] A) preparing an ammonium chloride raw material preparation reaction, fully mixing the calcium chloride solution and the ammonium bicarbonate solution of step (7), reacting to generate a mixed suspension solution of calcium carbonate and ammonium chloride, and releasing carbon dioxide gas;
[0089] B) Flocculation solidification precipitation: add a calcium flocculant to the mixed suspension solution of calcium carbonate and ammonium chloride in step A), wherein the calcium flocculant is a mixture of calcium hypochlorite + polyacrylamide and calcium hydroxide in equal mass ratio, and the amount of calcium flocculant added is controlled to be 0.10% of the mass of calcium carbonate. The calcium carbonate is used to encapsulate the potassium nitrate in the reaction solution and precipitate it; thus obtaining potassium nitrate precipitate and feed solution;
[0090] C) solid-liquid separation, the feed liquid of step B) is subjected to plate-and-frame filtration to obtain solid calcium carbonate and ammonium chloride solution; the solidified calcium carbonate is returned to step (1) as raw material;
[0091] D) evaporation, evaporating the ammonium chloride solution in step C), cooling it to room temperature to crystallize a large amount of ammonium chloride, filtering and drying to obtain an ammonium chloride product. The quality indicators of the prepared potassium nitrate product are shown in Table 1 above. The potassium nitrate products prepared in the above embodiments all meet the national quality standards.
[0092] The matters not described in the following comparative examples are the same as those described in the above examples.
[0093] Comparative Example
[0094] The invention discloses a new method for cyclically producing potassium nitrate and ammonium chloride, which uses dilute nitric acid, limestone, potassium chloride and ammonium bicarbonate as raw materials, and comprises the preparation of potassium nitrate and by-product ammonium chloride; the steps of the potassium nitrate preparation method are as follows:
[0095] (1) Raw material configuration reaction, limestone is placed in a reaction tank device, and then dilute nitric acid is slowly added to neutralize the limestone in the reaction tank device to discharge carbon dioxide; at the same time, process flushing water is added during the reaction process to allow the limestone in the reaction tank device to fully undergo a neutralization reaction, and after the reaction is completed; slaked lime is used to adjust the pH value of the neutralization reaction solution to 4.2-6.5, and the concentration of the neutralization reaction solution is controlled to 35-40Be; the mass concentration of the raw material dilute nitric acid is controlled to 50-60Wt%, and the volume and mass ratio of dilute nitric acid, calcium carbonate, potassium chloride, and ammonium bicarbonate is controlled to 65-90L:60-85Kg:58-80Kg:60-85Kg; after the reaction is completed, a neutralization reaction solution is obtained;
[0096] (2) Filtration; The neutralization reaction solution is filtered using a plate and frame filter to obtain a filtrate as a mother liquor 1 and a filter residue,
[0097] (3) Secondary batching reaction, adding potassium chloride to the mother solution 1 of step (2) in batches and steps, dissolving and reacting under continuous stirring and heating conditions, and controlling the heating reaction temperature to 90-105° C. for 30-50 minutes after all the potassium chloride is added and fully reacted, and controlling the concentration of the mother solution 2 to 39-45 Be. Obtaining a dissolving reaction solution, which is the mother solution 2;
[0098] (4) Filtration and cooling crystallization: The mother liquor 2 in the previous step is filtered by a plate-and-frame filter device and subjected to cooling crystallization treatment. The cooling crystallization treatment is to fill the mother liquor 2 with 0-5°C carbon dioxide gas, so that the mother liquor 2 can be continuously tumbled and stirred under the above-mentioned low temperature conditions, so that the solution is fully cooled and mixed, thereby achieving efficient cooling crystallization, that is, gas cooling is used for cooling, and the temperature of the solution during the cooling crystallization treatment is controlled to be between 25 and 35°C. The precipitated potassium nitrate crystals and potassium nitrate solid-liquid mixture are obtained by filtration;
[0099] (5) separation and rinsing, separating the solid-liquid mixture of potassium nitrate from step (4) to obtain a semi-finished potassium nitrate product, rinsing and purifying the semi-finished potassium nitrate product with clean water, and drying and packaging the semi-finished potassium nitrate product, the separation solution and the rinsing solution;
[0100] (6) freezing crystallization, placing the separated solution rinse liquid of step (5) in a freezing device for freezing treatment, controlling the temperature during freezing treatment to be -10 to -20°C, freezing again for solid-liquid separation to obtain a frozen separated liquid and a frozen crystallized solid, the frozen crystallized solid is a potassium nitrate semi-finished product, and repeating the rinsing, purification, and drying steps of step (5) to obtain a finished potassium nitrate product by packaging;
[0101] (7) recycling, wherein the frozen liquid separated in step (6) is the calcium chloride solution, and then used in the ammonium chloride preparation process for recycling production;
[0102] The preparation of ammonium chloride: that is, the preparation method of by-product ammonium chloride comprises the following steps:
[0103] A) preparing an ammonium chloride raw material preparation reaction, fully mixing the calcium chloride solution and the ammonium bicarbonate solution of step (7), reacting to generate a mixed suspension solution of calcium carbonate and ammonium chloride, and releasing carbon dioxide gas;
[0104] B) flocculation solidification precipitation: in this embodiment, filtering and precipitation are directly performed in this step, that is, no calcium flocculant is added to the mixed suspension solution of calcium carbonate and ammonium chloride in step A), so as to obtain calcium carbonate precipitate and feed solution;
[0105] C) solid-liquid separation, the feed liquid of step B) is subjected to plate-and-frame filtration to obtain solid calcium carbonate and ammonium chloride solution; the solidified calcium carbonate is returned to step (1) as raw material;
[0106] D) evaporation, the ammonium chloride solution of step C) is evaporated, and then cooled to room temperature to crystallize a large amount of ammonium chloride, which is filtered and dried to obtain the ammonium chloride product.
[0107] The new method for cyclically producing potassium nitrate and ammonium chloride disclosed in the present invention uses nitric acid, limestone and potassium chloride as raw materials to produce potassium nitrate, and the by-product calcium chloride aqueous solution is treated with ammonium bicarbonate, and the precipitated calcium carbonate is re-introduced into the potassium nitrate production cycle; the separated ammonium chloride solution is evaporated and crystallized to obtain an ammonium chloride product. The by-product ammonium chloride is one of the main raw materials for producing fertilizers, has a large market demand, good benefits, and the factory has no production bottleneck.
[0108] Table 2 below is an explanation of the effects of adding and not adding flocculants in the above-mentioned Examples 1 and 2 and the comparative example with different process parameters. At the same time, in the actual production process, the process parameters require that the K2O content in the calcium chloride solution and the ammonium chloride solution is less than 2.5%. Examples 1 and 2 of the present invention both meet the above requirements, while the parameters of the calcium chloride solution in the comparative example exceed the above range.
[0109] Table 2
[0110] Test items Production internal control requirements Example 1 Example 2 Comparative Example Potassium nitrate finished product yield% ≥92.0 94.11 94.43 92.60 <![CDATA[Potassium oxide content in calcium chloride solution]]> ≤2.5 2.25 2.30 2.27 <![CDATA[K2O content of solid calcium carbonate]]> -- 1.87 1.90 0.53 <![CDATA[Potassium oxide content in ammonium chloride solution]]> ≤2.5 1.10 1.13 2.02 <![CDATA[Potassium oxide content in ammonium chloride]]> ≤3.5 2.48 2.39 3.41
[0111] Note: Example 1 adds calcium hypochlorite flocculant, Example 2 adds calcium hypochlorite, polyacrylamide + calcium hydroxide mixed flocculant, and the data in the comparative example are without adding calcium agent flocculant. From the data in Table 2, the finished product yield of Example 1 and Example 2 is 1.51-1.83 percentage points higher than that of the comparative example, the K2O content of solid calcium carbonate entering the production cycle of Example 1 and Example 2 is 1.34-1.3 percentage points higher than that of the comparative example, and the K2O brought out by the final ammonium chloride in Example 1 and Example 2 is 0.93-1.02 percentage points lower than that of the comparative example. The above data show that adding flocculants has the positive effect of reducing losses, that is, reducing the loss rate of conversion into potassium nitrate products, and improving the finished product yield.
Claims
1. A new method for cyclically producing potassium nitrate and ammonium chloride, using dilute nitric acid, limestone, potassium chloride and ammonium bicarbonate as raw materials, including potassium nitrate and by-product ammonium chloride; characterized in that: The steps of the potassium nitrate preparation method are as follows: (1) Raw material configuration reaction: limestone is placed in a reaction tank device, and then dilute nitric acid is slowly added to react with the limestone in the reaction tank device to neutralize and discharge carbon dioxide; after the reaction is completed, a neutralization reaction solution is obtained; (2) Filtration: The neutralization reaction solution is filtered using a plate and frame filter device to obtain a filtrate as the mother liquor 1 and a filter residue. (3) a secondary batching reaction, wherein potassium chloride is added to the mother solution 1 of step (2) in portions, and a dissolution reaction is carried out under continuous stirring and heating conditions to obtain a dissolution reaction solution, which is the mother solution 2; (4) Filtration and cooling crystallization: The mother liquor 2 in the previous step is filtered using a plate and frame filter device, and subjected to cooling crystallization treatment to precipitate potassium nitrate crystals and a potassium nitrate solid-liquid mixture. (5) separation and rinsing, separating the solid-liquid mixture of potassium nitrate from step (4) to obtain a semi-finished potassium nitrate product, rinsing and purifying the semi-finished potassium nitrate product with clean water, and drying and packaging the semi-finished potassium nitrate product, the separation solution and the rinsing solution; (6) freezing crystallization, placing the separated solution rinse liquid of step (5) in a freezing device for freezing crystallization treatment, controlling the temperature during freezing crystallization treatment to be -10 to -20°C, freezing the solid-liquid separation again to obtain a frozen separated liquid containing calcium chloride and a frozen crystallized solid, the frozen crystallized solid is a potassium nitrate semi-finished product, and repeating the rinsing, purification and drying steps of step (5) to package the potassium nitrate finished product; (7) recycling, wherein the frozen separated liquid containing calcium chloride separated in step (6) is reused in the ammonium chloride preparation process for recycling production; The steps of the ammonium chloride preparation method are as follows: A) preparing an ammonium chloride raw material preparation reaction, mixing the calcium chloride-containing frozen separation liquid of step (7) and the ammonium bicarbonate solution, reacting to generate a calcium carbonate solution and releasing carbon dioxide gas; B) Flocculation solidification precipitation: adding calcium flocculant to the calcium carbonate solution in step A) to promote the precipitation of potassium nitrate wrapped in the calcium carbonate reaction solution; potassium nitrate precipitation and feed solution are obtained; C) solid-liquid separation, the feed liquid of step B) is subjected to plate-and-frame filtration to obtain solid calcium carbonate and filtrate ammonium chloride solution; the solidified calcium carbonate is returned to step (1) as raw material; D) Evaporation: The ammonium chloride solution in step C) is evaporated, and then cooled to room temperature to crystallize a large amount of ammonium chloride, which is filtered and dried to obtain the ammonium chloride product.
2. A novel method for cyclically producing potassium nitrate and ammonium chloride according to claim 1, characterized in that: The mass concentration of the raw material dilute nitric acid is controlled to be 50-62Wt%, and the volume and mass ratio of dilute nitric acid, calcium carbonate, potassium chloride and ammonium bicarbonate is controlled to be 65-90L: 60-85Kg: 58-80Kg: 60-85Kg.
3. A novel method for cyclically producing potassium nitrate and ammonium chloride according to claim 1, characterized in that: Step (1), adding process flushing water during the reaction process to enable the limestone in the reaction tank device to fully undergo a neutralization reaction, and after the reaction is completed; adjusting the pH value of the neutralization reaction solution to 4.2-6.5 with slaked lime, and controlling the concentration of the neutralization reaction solution to 35-40Be.
4. A novel method for cyclically producing potassium nitrate and ammonium chloride according to claim 1, characterized in that: Step (3), after all potassium chloride is added and fully reacted, the heating reaction temperature is controlled to be 90-105°C, the reaction is carried out for 30-50 minutes, and the concentration of the mother solution 2 is controlled to be 39-45 Be.
5. A novel method for cyclically producing potassium nitrate and ammonium chloride according to claim 1, characterized in that: Step (4) cooling crystallization treatment is to charge 0-10°C carbon dioxide into the mother solution 2 for cooling crystallization, and control the temperature of the solution during the cooling crystallization treatment to be between 25 and 35°C.
6. A novel method for cyclically producing potassium nitrate and ammonium chloride according to claim 1, characterized in that: Step B) The calcium flocculant is calcium hypochlorite or a mixture of calcium hypochlorite + polyacrylamide and calcium hydroxide in equal weight ratio, and the amount of the calcium flocculant added is controlled to be 0.1-0.2% of the weight of the calcium carbonate solution.