Particle bioelectrode based on metal-loaded sodium alginate carbon aerogel and preparation method and application thereof

Through the granular bioelectrode based on metal-loaded sodium alginate carbon aerogel, the problem of low efficiency and high cost of treating phenol-containing wastewater in traditional technology is solved, and efficient and economical removal of phenolic pollutants is achieved, and good application is achieved. prospect.

CN118929854AActive Publication Date: 2024-11-12QINGDAO UNIV OF TECH
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN202411351519.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-26
Publication Date
2024-11-12
Estimated Expiration
2044-09-26

AI Technical Summary

Technical Problem

The prior art is difficult to effectively treat phenol-containing wastewater, and the preparation cost of traditional particulate bioelectrodes is high and the source of materials is limited, which affects the economic and sustainable nature of water pollution control.

Method used

Using a granular bioelectrode based on metal-supported sodium alginate carbon aerogel, a metal salt solution is mixed with sodium alginate solution, freeze-dried, carbonized, combined with garden soil and starch, a granular bioelectrode was prepared. The particle electrode is used for the three-dimensional electrocatalytic biological filter to treat phenol-containing wastewater.

Benefits of technology

It has achieved efficient removal of phenolic pollutants, has good adsorption capacity and environmental safety performance, is low cost, is simple in preparation process, is suitable for a variety of bioelectrochemical systems, and has a wide range of application prospects.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118929854A_ABST
    Figure CN118929854A_ABST
Patent Text Reader

Abstract

The invention provides a particle biological electrode based on metal-loaded sodium alginate carbon aerogel and a preparation method and application thereof, and belongs to the technical field of particle electrode preparation, the particle biological electrode comprises the raw materials of metal-loaded sodium alginate carbon aerogel, garden soil and starch; the mass ratio of the three components is (6-8): (1-3): 1. The metal-loaded sodium alginate carbon aerogel is used as a substrate, and is functionally modified through starch and garden soil, so that the electrochemical performance and stability of the particle biological electrode are improved; the method can be used for various bioelectrochemical systems, and has a wide application prospect.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of particle electrode preparation, and in particular relates to a particle bioelectrode based on metal-loaded sodium alginate carbon aerogel, and a preparation method and application thereof. Background Art

[0002] Phenol-containing wastewater comes from a wide range of sources, mainly from the production processes of coal processing, petrochemicals, pharmaceutical industry, wood processing, plastic and rubber production, paint manufacturing, papermaking and food processing. Phenol is highly toxic and has the potential to cause cancer, teratogenesis and mutagenesis. It is one of the key hazardous wastewaters to be addressed in current water pollution control. The effective treatment of phenol-containing wastewater is of great significance for saving water resources, protecting the environment, improving people's living standards and achieving sustainable economic development.

[0003] The three-dimensional electrocatalytic aerated biofilter provides an effective way to deeply degrade phenolic pollutants in wastewater. The core of this method is the selection of granular bioelectrodes. Using sodium alginate carbon aerogel, which is widely available and low-cost, as raw material to prepare granular bioelectrodes is an economical and sustainable method. Summary of the invention

[0004] In order to solve the above technical problems, the present invention proposes a particle bioelectrode based on metal-loaded sodium alginate carbon aerogel and a preparation method and application thereof.

[0005] To achieve the above object, the present invention provides the following technical solutions:

[0006] One of the technical solutions of the present invention:

[0007] A particle bioelectrode based on metal-loaded sodium alginate carbon aerogel, the raw materials of which include metal-loaded sodium alginate carbon aerogel, garden soil and starch; the mass ratio of the three is (6-8):(1-3):1.

[0008] Beneficial effects: The present invention uses metal-loaded sodium alginate carbon aerogel as the main material, selects garden soil as the adhesive, and selects soluble starch as the pore-forming agent to finally prepare a particle bioelectrode based on metal-loaded sodium alginate carbon aerogel. The particle bioelectrode has high electrocatalytic activity, high specific surface area and good conductivity, and can be applied to three-dimensional electrocatalytic biofilters to treat phenol-containing wastewater. The particle electrode has a typical multi-level pore structure on its surface, has good adsorption capacity for phenolic substances, and has environmental safety performance. Its preparation raw materials are widely available, the cost is low, and the promotion potential is huge.

[0009] Preferably, the mass ratio of the metal-supported sodium alginate carbon aerogel, garden soil and starch is 8:1:1 or 7:2:1 or 6:3:1.

[0010] Preferably, the preparation process of the metal-supported sodium alginate carbon aerogel is:

[0011] The metal salt solution and the sodium alginate solution are mixed and stirred to obtain a hydrogel;

[0012] The hydrogel is sequentially frozen and vacuum freeze-dried to obtain an aerogel;

[0013] The aerogel is carbonized under a nitrogen atmosphere to obtain a metal-loaded sodium alginate carbon aerogel.

[0014] Preferably, the metal ions in the metal salt solution include Co 2+ , Cu 2+ 、Zn 2+ 、Al 3+ or Fe 3+ One or more of .

[0015] Preferably, the concentration of the sodium alginate solution is 1 wt %.

[0016] Preferably, the vacuum freeze-drying conditions are: temperature of -40°C and pressure of 10Pa.

[0017] Preferably, the conditions during the carbonization process are: carbonization at 500-700° C. for 4 hours.

[0018] The second technical solution of the present invention:

[0019] The method for preparing the above-mentioned metal-loaded sodium alginate carbon aerogel particle bioelectrode comprises the following steps:

[0020] The metal-loaded sodium alginate carbon aerogel, garden soil and starch are mixed, sprayed with water and shaken into spherical particles, calcined and cooled to obtain a particle bioelectrode based on the metal-loaded sodium alginate carbon aerogel.

[0021] Preferably, the conditions during the calcination process are: calcination at a temperature of 1200° C. for 6 hours.

[0022] The third technical solution of the present invention:

[0023] As mentioned above, the granular bioelectrode based on metal-loaded sodium alginate carbon aerogel is used in the treatment of phenol-containing wastewater.

[0024] Compared with the prior art, the present invention has the following advantages and technical effects:

[0025] The preparation process of the metal-loaded sodium alginate carbon aerogel-based granular bioelectrode disclosed in the present invention is simple and low in cost; the carbon aerogel obtained in the preparation process has good biocompatibility and conductivity as a substrate; the granular bioelectrode is functionally modified by starch and garden soil, thereby improving the electrochemical performance and stability of the granular bioelectrode; the granular bioelectrode can be used in a variety of bioelectrochemical systems, and has broad application prospects. BRIEF DESCRIPTION OF THE DRAWINGS

[0026] The drawings constituting a part of the present application are used to provide a further understanding of the present application. The illustrative embodiments and descriptions of the present application are used to explain the present application and do not constitute an improper limitation on the present application. In the drawings:

[0027] Figure 1 This is a flow chart of the preparation of a particle bioelectrode based on metal-loaded sodium alginate carbon aerogel according to the present invention;

[0028] Figure 2 This is a diagram showing the removal effect of phenol removal using the metal-loaded sodium alginate carbon aerogel-based particle bioelectrode prepared in Example 1-3 of the present invention;

[0029] Figure 3 These are SEM images of the metal-loaded sodium alginate carbon aerogel-based particle bioelectrodes prepared in Example 1 of the present invention (20, 5, 2, and 1 nm, respectively). DETAILED DESCRIPTION

[0030] Various exemplary embodiments of the present invention will now be described in detail. This detailed description should not be considered as limiting the present invention, but should be understood as a more detailed description of certain aspects, features, and embodiments of the present invention.

[0031] It should be understood that the terms described in the present invention are only for describing special embodiments and are not intended to limit the present invention. In addition, for the numerical range in the present invention, it should be understood that each intermediate value between the upper and lower limits of the scope is also specifically disclosed. Each smaller range between the intermediate value in any stated value or stated range and any other stated value or intermediate value in the described range is also included in the present invention. The upper and lower limits of these smaller ranges can be independently included or excluded in the scope.

[0032] Unless otherwise indicated, all technical and scientific terms used herein have the same meanings as those generally understood by those skilled in the art. Although the present invention describes only preferred methods and materials, any methods and materials similar or equivalent to those described herein may also be used in the implementation or testing of the present invention. All documents mentioned in this specification are incorporated by reference to disclose and describe the methods and / or materials associated with the documents. In the event of a conflict with any incorporated document, the content of this specification shall prevail.

[0033] It will be apparent to those skilled in the art that various modifications and variations may be made to the specific embodiments of the present invention description without departing from the scope or spirit of the present invention. Other embodiments derived from the present invention description will be apparent to those skilled in the art. The present invention description and examples are exemplary only.

[0034] The words “include,” “including,” “have,” “contain,” etc. used in this document are open-ended terms, meaning including but not limited to.

[0035] The present invention provides a method for preparing a particle bioelectrode based on metal-loaded sodium alginate carbon aerogel, comprising the following steps:

[0036] Step 1: First, add the sodium alginate solution into the prepared metal salt solution through a separatory funnel and continue stirring for 12 hours to obtain a metal ion chelated hydrogel; rinse the hydrogel with deionized water 10 times, put it into a freeze dryer and freeze it for 24 hours, and then vacuum freeze-dry it to obtain an aerogel;

[0037] Step 2: placing the obtained aerogel in a tubular furnace and carbonizing it under 100% N2 atmosphere for 4 h to obtain metal oxide supported carbon aerogel (M-CA);

[0038] Step 3: Dry the obtained loaded carbon aerogel and garden soil in an oven at 100°C for 4 hours, sieve, mix the carbon aerogel, garden soil and starch in a mass ratio of 8:1:1, spray water and shake into spherical particles, calcine for 6 hours, and cool naturally to room temperature.

[0039] In some preferred embodiments, the concentration of the sodium alginate solution in step 1 is 1 wt %.

[0040] In some preferred embodiments, the metal salt solution in step 1 comprises Co 2+ , Cu 2+ 、Zn 2+ 、Al 3+ or Fe 3+ One or more of .

[0041] In some preferred embodiments, the vacuum freeze-drying conditions in step 1 are -40°C and 10Pa.

[0042] In some preferred embodiments, the carbonization temperature in step 2 is 500-700°C.

[0043] In some preferred embodiments, the sieving in step three is through a 200-mesh sieve.

[0044] In some preferred embodiments, the size of the spherical particles in step three is 5-8 mm.

[0045] In some preferred embodiments, the calcination temperature in step three is 1200°C.

[0046] In some preferred embodiments, the garden soil in step three is any loess in the garden of North China, which is sieved through a 200-mesh sieve.

[0047] In some preferred embodiments, the starch in step 3 (analytical grade) is purchased from Sinopharm Group.

[0048] In addition, the present invention also provides the use of the above-mentioned metal-loaded sodium alginate carbon aerogel-based particle bioelectrode in treating phenol-containing wastewater.

[0049] The specific implementation method is to place the prepared particle bioelectrode in a three-dimensional electrocatalytic biofilter to treat phenol-containing wastewater.

[0050] In some preferred embodiments, the phenol-containing wastewater is laboratory simulated phenol-containing wastewater.

[0051] In some preferred embodiments, ruthenium-iridium-titanium mesh is selected as the anode and cathode electrode plates.

[0052] All raw materials used in the examples of the present invention are commercially available.

[0053] The technical solution of the present invention is further illustrated by the following embodiments.

[0054] Example 1

[0055] like Figure 1 As shown, a method for preparing a particle bioelectrode based on metal-loaded sodium alginate carbon aerogel comprises the following steps:

[0056] 1000 mL of 1 wt% sodium alginate solution was added into 1000 mL of copper nitrate (concentration of 10 M) through a separatory funnel and stirred for 12 h to obtain a metal ion chelated hydrogel;

[0057] The obtained hydrogel was rinsed with deionized water for 10 times, placed in a freeze dryer and frozen for 24 hours, and then vacuum freeze-dried at -40°C and 10Pa to obtain an aerogel;

[0058] The obtained aerogel was placed in a tubular furnace and carbonized at 600°C for 4 h in a 100% N2 atmosphere to obtain a metal oxide-supported carbon aerogel (M-CA);

[0059] The obtained supported carbon aerogel and garden soil were dried in an oven at 100 °C for 4 h and sieved using a 200-mesh laboratory standard sieve;

[0060] The metal oxide-supported carbon aerogel, garden soil and starch were uniformly mixed in a mass ratio of 8:1:1, sprayed with water and shaken into 6 mm spherical particles, calcined at 1200° C. for 6 hours in a muffle furnace, and naturally cooled to room temperature.

[0061] Example 2

[0062] The difference from Example 1 is that the metal oxide-supported carbon aerogel, garden soil and starch are uniformly mixed in a ratio of 7:2:1, and the other conditions are consistent with Example 1.

[0063] Example 3

[0064] The difference from Example 1 is that the metal oxide-supported carbon aerogel, garden soil and starch are uniformly mixed in a ratio of 6:3:1, and the other conditions are consistent with Example 1.

[0065] Example 4

[0066] The difference from Example 1 is that the metal type in the metal oxide-supported carbon aerogel is Fe 3+ , other conditions are consistent with Example 1.

[0067] The characterization parameters of the metal-loaded sodium alginate carbon aerogel-based particle bioelectrodes prepared in Examples 1-4 are shown in Table 1 below.

[0068] Table 1

[0069] sample <![CDATA[Specific surface area (m 2· g -1 )]]> <![CDATA[Total pore volume (cm 3· g -1 )]]> Average pore size (nm) Example 1 162.4 0.108 2.74 Example 2 145.6 0.092 2.58 Example 3 128.8 0.088 2.42 Example 4 178.8 0.164 2.98

[0070] Effect verification

[0071] The metal-loaded sodium alginate carbon aerogel-based particle bioelectrode prepared in Example 1-3 was used to prepare simulated phenolic wastewater with a phenol solution (the initial concentration of the phenolic wastewater was 10 mg / L), and a three-dimensional electrocatalytic pilot reactor was prepared. Ruthenium-coated iridium-titanium mesh was selected as the anode and cathode electrodes. The current density was 2.5 mA / cm 2 ) was used to test the performance of the reactor in degrading phenol.

[0072] Figure 2 This is a graph showing the phenol removal effect of the metal-loaded sodium alginate carbon aerogel-based particle bioelectrode prepared in Example 1-3 of the present invention. Figure 2 It can be seen that the removal rates of phenol by the three three-dimensional electrocatalytic pilot reactors mentioned above increase with the increase of electrolysis time (0-30min), and the final phenol removal rates are all higher than 85%, especially the phenol removal rate of the reactor using the metal-loaded sodium alginate carbon aerogel particle bioelectrode prepared in Example 1 as the bioelectrode is higher than 95%.

[0073] The above are only preferred specific implementations of the present application, but the protection scope of the present application is not limited thereto. Any changes or substitutions that can be easily thought of by a person skilled in the art within the technical scope disclosed in the present application should be included in the protection scope of the present application. Therefore, the protection scope of the present application should be based on the protection scope of the claims.

Claims

1. A particle bioelectrode based on metal-loaded sodium alginate carbon aerogel, characterized in that: The raw materials include metal-loaded sodium alginate carbon aerogel, garden soil and starch; the mass ratio of the three is (6-8):(1-3):

1.

2. The metal-supported sodium alginate carbon aerogel-based particle bioelectrode according to claim 1, characterized in that: The mass ratio of the metal-loaded sodium alginate carbon aerogel, garden soil and starch is 8:1:1 or 7:2:1 or 6:3:

1.

3. The metal-supported sodium alginate carbon aerogel-based particle bioelectrode according to claim 1, characterized in that: The preparation process of the metal-supported sodium alginate carbon aerogel is as follows: The metal salt solution and the sodium alginate solution are mixed and stirred to obtain a hydrogel; The hydrogel is sequentially frozen and vacuum freeze-dried to obtain an aerogel; The aerogel is carbonized under a nitrogen atmosphere to obtain a metal-loaded sodium alginate carbon aerogel.

4. The metal-loaded sodium alginate carbon aerogel-based particle bioelectrode according to claim 3, characterized in that: The metal ions in the metal salt solution include Co 2+ , Cu 2+ 、Zn 2+ 、Al 3+ or Fe 3+ One or more of .

5. The metal-supported sodium alginate carbon aerogel-based particle bioelectrode according to claim 3, characterized in that: The concentration of the sodium alginate solution is 1 wt %.

6. The metal-loaded sodium alginate carbon aerogel-based particle bioelectrode according to claim 3, characterized in that: The vacuum freeze-drying conditions are: temperature of -40°C and pressure of 10Pa.

7. The particle bioelectrode based on metal-loaded sodium alginate carbon aerogel according to claim 3, characterized in that: The conditions in the carbonization process are: carbonization at 500-700° C. for 4 hours.

8. A method for preparing a particle bioelectrode based on metal-loaded sodium alginate carbon aerogel according to any one of claims 1 to 7, characterized in that: The following steps are involved: The metal-loaded sodium alginate carbon aerogel, garden soil and starch are mixed, sprayed with water and shaken into spherical particles, calcined and cooled to obtain a particle bioelectrode based on the metal-loaded sodium alginate carbon aerogel.

9. The method for preparing a particle bioelectrode based on metal-loaded sodium alginate carbon aerogel according to claim 8, characterized in that: The conditions during the calcination process are: calcination at a temperature of 1200° C. for 6 hours.

10. Use of a particle bioelectrode based on metal-loaded sodium alginate carbon aerogel as claimed in any one of claims 1 to 7 in treating phenol-containing wastewater.

Citation Information

Patent Citations

  • Copper-loaded sodium alginate carbon aerogel and preparation method and application thereof

    CN109650373A

  • Preparation method and application of iron-loaded sodium alginate carbon aerogel

    CN109850865A

  • Electrocaloric refrigeration device and refrigeration method

    CN111238077A

  • Three-dimensional electro-catalysis in-situ adsorption water purification method

    CN113582431A

  • Novel metal-carbon aerogel composite electrodes, aerogel supercapacitors, process of the same and applications thereof