Preparation method of composite layer heterogeneous ozone catalyst
Through the preparation method of composite layer heterogeneous ozone catalyst, the structure of the catalyst core and shell is controlled, and the problems of high catalyst density and cost in the prior art are solved, thereby achieving efficient catalytic effects and cost savings.
Patent Information
- Application Number
- CN202411072436.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-06
- Publication Date
- 2024-11-12
AI Technical Summary
The complete mixing of existing heterogeneous ozone catalysts on the support and the active ingredients leads to high metal support density, low catalyst efficiency and high cost.
The preparation method of composite layer heterogeneous ozone catalyst is adopted to prepare the catalyst core and shell through the granulation mechanism to control the distribution of transition metals and rare earth metals, so that the catalytic activity is more reflected in the outer layer, increase the contact area between the catalyst and wastewater, and through the construction of Pore agent optimizes structure and reduces density.
The efficiency of the catalyst is improved and the cost is reduced, while the effective contact area between the catalyst and wastewater is increased, thereby improving the catalytic efficiency.
Smart Images

Figure CN118929891A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of deep wastewater treatment and catalysts, and in particular to a method for preparing a composite layer heterogeneous ozone catalyst. Background Art
[0002] Ozone catalytic oxidation technology belongs to advanced oxidation technology. It uses catalysts to produce free hydroxyl groups to enhance the degradation of difficult-to-degrade organic matter in water. Its carbon reduction and decolorization ability is significantly higher than that of simple ozone oxidation. It has the characteristics of high degradation efficiency and environmental friendliness. Its cost is also lower than that of simple ozone oxidation. Therefore, it has gradually attracted attention and become one of the research hotspots. It has good application prospects in the field of deep treatment of industrial wastewater. Catalytic ozone oxidation technology can be divided into homogeneous ozone catalytic oxidation using metal ions and hydrogen peroxide as catalysts and heterogeneous ozone catalytic oxidation using solid metals, metal oxides or metals or metal oxides loaded on carriers as catalysts according to the different phases of the catalysts used. Homogeneous ozone catalysts are evenly distributed and have high catalytic activity, but they are not easy to recycle and are prone to secondary pollution; therefore, most researchers pay more attention to heterogeneous ozone catalysts that can be recycled and reused, economical and environmentally friendly.
[0003] In heterogeneous ozone catalytic oxidation, the catalyst exists in a solid state and is obtained by loading the active component with catalytic ability on a catalyst carrier. The active component has a catalytic effect, and the catalyst carrier has an adsorption effect. The active components are mainly divided into three categories: precious metal elements, cheap transition metal elements (Mn, Fe, Cu, etc.) and abundant rare earth elements (Ce, La, etc.). The application of precious metals is limited due to their high prices. Currently, cheap transition metals and their oxides are mainly used. Among them, manganese dioxide is the most studied and mature metal oxide in catalytic ozone oxidation.
[0004] The methods for preparing heterogeneous ozone catalysts currently used to treat refractory wastewater generally use mechanical mixing, impregnation, precipitation, and hot melt methods. Among them, the mechanical mixing method using solid metal oxides has the advantages of being easy to operate and suitable for large-scale batch production. Since heterogeneous ozone catalysts generally load transition metals and rare earth metals on carriers as catalytically active components, the content of catalytically active components and the number of active sites are the key to determining their catalytic efficiency. Conventional mechanical mixing methods completely mix the carrier with activators such as transition metals and rare earth metals, resulting in a high density of the metal carrier, difficulty in exerting the efficiency of the active components in the inner layer of the catalyst, and high costs, so the existing technology has limitations. Summary of the invention
[0005] The present invention is made to solve the above-mentioned problem, and its purpose is to provide a method for preparing a composite layer heterogeneous ozone catalyst.
[0006] The present invention provides a method for preparing a composite layer heterogeneous ozone catalyst, which has the following characteristics and comprises the following steps:
[0007] Step 1: uniformly mix the carrier, the active agent and the pore-forming agent to form a first mixed powder and a second mixed powder;
[0008] Step 2: placing the first mixed powder and water into a granulator to prepare a spherical catalyst core, and stopping the preparation when the catalyst core particle size is 2 to 5 mm;
[0009] Step 3, placing the second mixed powder and water into a granulator, preparing a catalyst shell outside the catalyst core to form a spherical catalyst crude product, and stopping the preparation when the particle size of the catalyst crude product is 3 to 8 mm;
[0010] Step 4: Place the crude catalyst in a drying oven at a temperature of 75 to 110° C. under air atmosphere and dry for 1 to 6 hours;
[0011] Step 5: calcine the crude catalyst in a muffle furnace or kiln at a maximum temperature of 1200° C. for 1 to 6 hours, and heat it at a rate of 3 to 20° C. / min, and finally cool it to room temperature to obtain a composite layer heterogeneous ozone catalyst.
[0012] In the preparation method of the composite layer heterogeneous ozone catalyst provided by the present invention, it can also have the following characteristics: the weight ratio of the carrier, the active agent and the pore-forming agent in the first mixed powder is 82-99%: 0-10%: 0.2-15%, and the weight ratio of the carrier, the active agent and the pore-forming agent in the second mixed powder is 60-95%: 5-40%: 0-2%.
[0013] In the preparation method of the composite layer heterogeneous ozone catalyst provided by the present invention, it can also have the following characteristics: the carrier is one or more combinations of activated alumina, clay, kaolin, diatomaceous earth, molecular sieve, and activated carbon.
[0014] In the preparation method of the composite layer heterogeneous ozone catalyst provided by the present invention, it can also have the following characteristics: the activator includes transition metals and rare earth metals, the transition metal is one or more combinations of iron oxide, manganese oxide, copper oxide, titanium oxide, cobalt oxide, zirconium oxide, magnesium oxide, zinc oxide, silver oxide, vanadium oxide, molybdenum oxide, ruthenium oxide, rhodium oxide, and palladium oxide, and the rare earth metal is one or more combinations of cerium oxide, lanthanum oxide, samarium oxide, yttrium oxide, neodymium oxide, and europium oxide.
[0015] In the preparation method of the composite layer heterogeneous ozone catalyst provided by the present invention, it can also have the following characteristics: the pore-forming agent is one or more combinations of polyethylene glycol, polyvinyl alcohol, hydroxypropyl cellulose, magnesium peroxide, and magnesium bicarbonate.
[0016] Functions and Effects of the Invention
[0017] According to the preparation method of a composite layer heterogeneous ozone catalyst involved in the present invention, the first mixed powder and the second mixed powder, which are uniformly mixed in proportion by a carrier, an active agent and a pore-forming agent, and water are sequentially added into a granulator to prepare a catalyst core and a catalyst shell. Among them, the catalyst core and the catalyst shell contain different active agents such as transition metals and rare earth metals. The catalyst core has less or no active agents such as transition metals and rare earth metals, and more pore-forming agents; the catalyst outer layer has more active agents such as transition metals and rare earth metals, and less or no pore-forming agents, so that the catalytic activity of the composite layer heterogeneous ozone catalyst is more reflected in the catalyst outer layer, and the effective contact area between the catalyst and the wastewater is increased, thereby increasing the catalytic efficiency, reducing the catalyst density, and effectively saving costs. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] Figure 1 is a flow chart of the present invention;
[0019] Figure 2 It is a schematic diagram of the structure of the composite layer heterogeneous ozone catalyst in the present invention.
[0020] Description of reference numerals:
[0021] 1. Catalyst core; 2. Catalyst shell. DETAILED DESCRIPTION
[0022] In order to make the technical means, creative features, objectives and effects achieved by the present invention easy to understand, the present invention is specifically described in the following embodiments in conjunction with the accompanying drawings.
[0023] Example
[0024] This embodiment provides a method for preparing a composite layer heterogeneous ozone catalyst, comprising the following steps:
[0025] Step 1: uniformly mix the carrier, the active agent and the pore-forming agent to form a first mixed powder and a second mixed powder;
[0026] Step 2: placing the first mixed powder and water into a granulator to prepare a spherical catalyst core, and stopping the preparation when the catalyst core particle size is 2 to 5 mm;
[0027] Step 3, placing the second mixed powder and water into a granulator, preparing a catalyst shell outside the catalyst core to form a spherical catalyst crude product, and stopping the preparation when the particle size of the catalyst crude product is 3 to 8 mm;
[0028] Step 4: Place the crude catalyst in a drying oven at a temperature of 75 to 110° C. under air atmosphere and dry for 1 to 6 hours;
[0029] Step 5: calcine the crude catalyst in a muffle furnace or kiln at a maximum temperature of 1200° C. for 1 to 6 hours, and heat it at a rate of 3 to 20° C. / min, and finally cool it to room temperature to obtain a composite layer heterogeneous ozone catalyst.
[0030] In this embodiment, the weight ratio of the carrier, the active agent and the pore-forming agent in the first mixed powder is 82-99%: 0-10%: 0.2-15%, and the weight ratio of the carrier, the active agent and the pore-forming agent in the second mixed powder is 60-95%: 5-40%: 0-2%.
[0031] In this embodiment, the carrier is one or more combinations of activated alumina, clay, kaolin, diatomaceous earth, molecular sieve, and activated carbon.
[0032] In this embodiment, the active agent includes transition metals and rare earth metals, the transition metal is one or more combinations of iron oxide, manganese oxide, copper oxide, titanium oxide, cobalt oxide, zirconium oxide, magnesium oxide, zinc oxide, silver oxide, vanadium oxide, molybdenum oxide, ruthenium oxide, rhodium oxide, and palladium oxide, and the rare earth metal is one or more combinations of cerium oxide, lanthanum oxide, samarium oxide, yttrium oxide, neodymium oxide, and europium oxide.
[0033] In this embodiment, the pore-forming agent is one or more combinations of polyethylene glycol, polyvinyl alcohol, hydroxypropyl cellulose, magnesium peroxide, and magnesium bicarbonate.
[0034] In this embodiment, the preparation steps of the composite layer heterogeneous ozone catalyst can be cyclic or partially cyclic, so that composite layer heterogeneous ozone catalysts with different structures can be produced. For example, the composite layer heterogeneous ozone catalyst can be a three-layer structure with an inner layer, a middle layer, and an outer layer, or a multi-layer structure with an inner layer, multiple middle layers, and an outer layer, thereby meeting different usage requirements.
[0035] Functions and Effects of the Embodiments
[0036] According to the preparation method of a composite layer heterogeneous ozone catalyst involved in the present invention, the first mixed powder and the second mixed powder, which are uniformly mixed in proportion by a carrier, an active agent and a pore-forming agent, and water are sequentially added into a granulator to prepare a catalyst core and a catalyst shell. Among them, the catalyst core and the catalyst shell contain different active agents such as transition metals and rare earth metals. The catalyst core has less or no active agents such as transition metals and rare earth metals, and more pore-forming agents; the catalyst outer layer has more active agents such as transition metals and rare earth metals, and less or no pore-forming agents, so that the catalytic activity of the composite layer heterogeneous ozone catalyst is more reflected in the catalyst outer layer, and the effective contact area between the catalyst and the wastewater is increased, thereby increasing the catalytic efficiency, reducing the catalyst density, and effectively saving costs.
[0037] The above-mentioned embodiments are preferred examples of the present invention and are not intended to limit the protection scope of the present invention.
Claims
1. A method for preparing a composite layer heterogeneous ozone catalyst, characterized in that: The following steps are involved: Step 1: uniformly mix the carrier, the active agent and the pore-forming agent to form a first mixed powder and a second mixed powder; Step 2: placing the first mixed powder and water into a granulator to prepare a spherical catalyst core, and stopping the preparation when the catalyst core particle size is 2 to 5 mm; Step 3, placing the second mixed powder and water into a granulator, preparing a catalyst shell outside the catalyst core to form a spherical catalyst crude product, and stopping the preparation when the particle size of the catalyst crude product is 3 to 8 mm; Step 4: placing the crude catalyst in a drying oven at a temperature of 75 to 110° C. under air atmosphere and drying for 1 to 6 hours; Step 5: calcine the crude catalyst in a muffle furnace or kiln at a maximum temperature of 1200° C. for 1 to 6 hours, and heat the mixture at a rate of 3 to 20° C. / min, and finally cool the mixture to room temperature to obtain a composite heterogeneous ozone catalyst.
2. The method for preparing a composite layer heterogeneous ozone catalyst according to claim 1, characterized in that: in, The weight ratio of the carrier, the active agent and the pore-forming agent in the first mixed powder is 82-99%: 0-10%: 0.2-15%, and the weight ratio of the carrier, the active agent and the pore-forming agent in the second mixed powder is 60-95%: 5-40%: 0-2%.
3. The method for preparing a composite layer heterogeneous ozone catalyst according to claim 1, characterized in that: in, The carrier is one or more combinations of activated alumina, clay, kaolin, diatomaceous earth, molecular sieve and activated carbon.
4. The method for preparing a composite layer heterogeneous ozone catalyst according to claim 1, characterized in that: in, The active agent includes transition metals and rare earth metals, wherein the transition metal is one or more combinations of iron oxide, manganese oxide, copper oxide, titanium oxide, cobalt oxide, zirconium oxide, magnesium oxide, zinc oxide, silver oxide, vanadium oxide, molybdenum oxide, ruthenium oxide, rhodium oxide, and palladium oxide, and the rare earth metal is one or more combinations of cerium oxide, lanthanum oxide, samarium oxide, yttrium oxide, neodymium oxide, and europium oxide.
5. The method for preparing a composite layer heterogeneous ozone catalyst according to claim 1, characterized in that: in, The pore-forming agent is one or more combinations of polyethylene glycol, polyvinyl alcohol, hydroxypropyl cellulose, magnesium peroxide, and magnesium bicarbonate.
Citation Information
Patent Citations
Method for preparing ceramsite catalyst for ozone catalytic oxidation
CN101185898A
Ozone catalyst preparation method
CN104759286A
Multi-layer-structure catalyst for catalytic ozonation of nbsCOD as well as preparation method and application thereof
CN111468105A
High-strength catalyst composite carrier and preparation method thereof
CN116688970A
Method for preparing supported catalyst for heterogeneous catalytic ozonation
US20180264457A1