Lens pipe cap and manufacturing method thereof

By plating solder in the non-lens area of ​​the lens and hot melt connection, the existing lens cap production methods are solved, and efficient and environmentally friendly lens installation is achieved, ensuring the long-term stability and reliability of the optical module. .

CN118930073APending Publication Date: 2024-11-12XIAMEN YEYING ELECTRONIC TECH CO LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202410986977.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-23
Publication Date
2024-11-12

AI Technical Summary

Technical Problem

The existing lens caps are cumbersome and unstable. The adhesive aging under high temperature environments, resulting in the lens position shift or fall off, and the production cycle is long and not environmentally friendly.

Method used

The lens is fixed by solder, and solder is plated on the non-lens area of ​​the lens through evaporation, sputtering, plating or electroplating processes. Combined with welding technology, the solder and the tube cap are ensured to hot melt connection between the solder and the tube cap to form a stable lens tube cap.

Benefits of technology

It improves the reliability and stability of lens installation, avoids the aging of adhesives, shortens the production cycle, and ensures the long-term stability and environmental protection of the optical module.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118930073A_ABST
    Figure CN118930073A_ABST
Patent Text Reader

Abstract

The invention provides a lens tube cap and a manufacturing method thereof, and the manufacturing method comprises the steps: providing a welding flux with the thickness corresponding to the flatness information according to the flatness information of a tube cap opening of the tube cap; fixing the solder on a lens to form an integral structure; determining the crimping position of the opening of the pipe cap according to the alignment condition; the welding flux of the overall structure is in compression joint with the compression joint position, the lens tube cap is manufactured, the welding flux replaces an adhesive in the prior art, the structure is stable and reliable, accurate control over the amount and the position of the welding flux during welding is guaranteed, and the manufacturing efficiency is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of tube caps, and in particular to a lens tube cap and a manufacturing method thereof. Background Art

[0002] Lens caps, as an optical component, are usually used in combination with specific packaging forms (such as TO packaging), especially in applications such as photoelectric sensors, infrared thermometers, and thermal imaging systems. Lens caps, as the name implies, are cap structures that combine lens functions. They are usually installed on the packaging tube of sensors or optical devices, and use built-in lenses to achieve focusing, refraction, or projection of optical fibers, thereby enhancing or improving optical performance.

[0003] For example, the lens cap manufacturing method disclosed in publication number CN1080027168 first places the lens in the through hole of the cap, and then seals the joint between the lens and the cap with adhesive. However, it has the following defects:

[0004] (1) Placing the lens on the tube cap and then sealing it by dispensing glue not only has complicated manufacturing steps and a long time, but also has large manufacturing errors;

[0005] (2) The use of adhesives requires extremely strict control of the amount of glue dispensed. If there is too little glue, gaps will be created, resulting in unstable installation. If there is too much glue, it is easy to cause glue overflow during the process of pressing the lens down to the tube cap, thereby contaminating the lens itself.

[0006] (3) Adhesives may become unreliable when used at high temperatures or for long periods of time, causing the lens to shift or fall off. This is because the adhesive is prone to aging in high temperature environments and loses its adhesion, which causes the lens to loosen.

[0007] (4) Adhesives exhibit different stabilities under different environmental conditions, and are particularly prone to failure under high temperature and high humidity conditions. High temperature and high humidity accelerate the chemical degradation of adhesives, leading to a decrease in their mechanical and adhesion properties.

[0008] (5) The mechanical strength of the adhesive is relatively low. When subjected to mechanical shock or vibration, it is easy to cause the lens to shift or fall off, affecting the performance and reliability of the optical module;

[0009] (6) Adhesives usually require a certain curing time, whether it is thermal curing or light curing, which will extend the overall production cycle and reduce production efficiency;

[0010] (7) Certain adhesives will release volatile organic compounds (VOCs) during long-term use, causing pollution to the internal environment of the optical module and affecting the stability and service life of the components. Summary of the invention

[0011] The object of the present invention is to provide a lens cap and a manufacturing method thereof which can improve assembly efficiency, reduce assembly error, and have a stable and reliable structure in view of the deficiencies in the prior art.

[0012] In order to achieve the above object, the present invention provides the following technical solutions:

[0013] A method for manufacturing a lens tube cap comprises the following steps:

[0014] b. providing solder having a thickness corresponding to the flatness information according to the flatness information of the tube cap opening of the tube cap;

[0015] c. fixing the solder to the lens to form an integral structure;

[0016] d. determining the crimping position of the pipe cap opening according to the alignment condition;

[0017] e. Crimping the solder of the overall structure with the crimping position to make a lens cap.

[0018] As a preferred embodiment, the surface of the tube cap is plated with a metal layer, and before step b, the manufacturing method further includes the following steps:

[0019] a. Select a metal with the same composition as the metal layer as the solder.

[0020] As a preferred embodiment, the lens has a front lens and a back lens facing each other, the front lens has a spherical region and a non-lens region surrounding the spherical region, and step c comprises the following steps:

[0021] The solder is fixed on the non-lens area by means of an evaporation process, a sputtering process, a chemical plating process or an electroplating process.

[0022] As a preferred embodiment, the tube cap includes an end cap having a relative end cap upper surface and an end cap lower surface, the tube cap opening passes through the end cap upper surface and the end cap lower surface, and the alignment condition includes the front face of the lens being relative to the end cap lower surface, and the spherical area of ​​the lens being relative to the tube cap opening.

[0023] As a preferred embodiment, the step d comprises the following steps:

[0024] The area on the lower surface of the end cap and surrounding the pipe cap opening is selected as the crimping position.

[0025] As a preferred embodiment, the step e comprises the following steps:

[0026] e1. Preheating the tube cap;

[0027] e2. Crimping the solder of the overall structure with the crimping position of the tube cap, so that the solder is thermally melted and connected with the tube cap under the action of the preheated tube cap.

[0028] As a preferred embodiment, the step e2 comprises the following steps:

[0029] e21. Place the preheated pipe cap on the welding table;

[0030] e22, grabbing the back side of the lens in the overall structure so that the solder on the front side of the lens is opposite to the crimping position of the tube cap;

[0031] e23. The overall structure and the tube cap are crimped together, and the solder is thermally melted to the tube cap under the action of the preheated tube cap.

[0032] As a preferred embodiment, the following steps are further included after step e2:

[0033] e3. Cool the whole structure and the tube cap after crimping.

[0034] The present invention also provides a lens cap, comprising:

[0035] An integral structure, the integral structure comprising a lens and solder, the solder being fixedly connected to the lens;

[0036] A pipe cap, wherein the pipe cap is provided with a pipe cap opening, and the pipe cap opening has a crimping position;

[0037] The solder of the integral structure is crimped to the crimping position of the tube cap.

[0038] As a preferred embodiment, the tube cap comprises an end cap, the end cap has an end cap upper surface and an end cap lower surface opposite to each other, and the tube cap opening passes through the end cap upper surface and the end cap lower surface;

[0039] The lens has a front lens and a back lens facing each other, the front lens has a spherical region and a non-lens region surrounding the spherical region, and the solder is fixed on the non-lens region;

[0040] The solder is connected between the non-lens area and the lower surface of the end cap of the end cap, and the spherical area of ​​the front side of the lens is located in the tube cap opening.

[0041] Compared with the prior art, this technical solution has the following advantages:

[0042] By pre-preparing solder on the lens surface, the amount and position of solder can be precisely controlled during welding. The non-lens area of ​​the lens is plated with solder of appropriate thickness by evaporation, sputtering, chemical plating or electroplating. This method avoids the difficulty of controlling the amount of glue during the dispensing process, avoids the problem of overflow and gap, and improves the consistency and reliability of lens installation;

[0043] During the high temperature welding process at 320-350℃, the solder can ensure the stable fixation of the lens, and will not age or lose adhesion at high temperature like adhesives. This greatly improves the reliability of the package, avoids the phenomenon of lens deviation or falling off during high temperature or long-term use, and is suitable for applications in high temperature environments;

[0044] The pre-soldered lens package shows excellent stability under different environmental conditions, especially in high temperature and high humidity environments, and will not fail as easily as adhesives. The problem of chemical degradation in high temperature and high humidity environments is effectively solved, ensuring the long-term stability of the mechanical properties and adhesion properties of the package;

[0045] Solder has higher mechanical strength than adhesives, and can effectively prevent the lens from shifting or falling off when subjected to mechanical shock or vibration, ensuring the performance and reliability of the optical module under various working conditions;

[0046] The production cycle is shortened, and welding can be completed in only 3 to 5 seconds, without waiting for the curing time of the adhesive (whether it is heat curing or light curing), which greatly shortens the overall production cycle and improves production efficiency. Through machine recognition and grabbing, the process of pipe cap preheating and high-temperature welding can be completed quickly, improving the degree of automation and speed of production;

[0047] The use of solder avoids the risk of adhesives releasing volatile organic compounds (VOCs) during long-term use, ensuring the cleanliness and stability of the internal environment of the optical module, thereby extending the service life of the components.

[0048] The present invention is further described below with reference to the accompanying drawings and embodiments. BRIEF DESCRIPTION OF THE DRAWINGS

[0049] Figure 1 is a flow chart of a method for manufacturing a lens tube cap according to the present invention;

[0050] Figure 2 is a schematic structural diagram of the lens cap of the present invention;

[0051] Figure 3 It is a structural schematic diagram of the overall structure of the present invention.

[0052] In the figure: 100 lens tube cap, 110 overall structure, 111 lens, 111a lens front, 111a1 spherical area, 111a2 non-lens area, 111b lens back, 112 solder, 120 tube cap, 121 end cap, 121a end cap upper surface, 121b end cap lower surface, 121c tube cap opening, 121c1 crimping position, 122 end side. DETAILED DESCRIPTION

[0053] The following description is used to disclose the present invention so that those skilled in the art can implement the present invention. The preferred embodiments described below are only examples, and those skilled in the art can think of other obvious variations. The basic principles of the present invention defined in the following description can be applied to other embodiments, variations, improvements, equivalents, and other technical solutions that do not deviate from the spirit and scope of the present invention.

[0054] First embodiment

[0055] Figure 1 A flowchart of a method for manufacturing a lens cap provided by an embodiment of the invention, the method comprising:

[0056] According to the flatness information of the tube cap opening 121c of the tube cap 120, providing the solder 112 with a thickness corresponding to the flatness information;

[0057] The solder 112 is fixed to the lens 111 to form an integral structure 110;

[0058] Determine the crimping position 121c1 of the cap opening 121c according to the alignment condition;

[0059] The solder 112 of the integral structure 110 is crimped to the crimping position 121 c 1 to manufacture the lens cap 100 .

[0060] By replacing the adhesive in the prior art with the solder 112, no gas volatilization will be generated during the soldering process of the solder 112, thereby ensuring the internal environment and stability of the optical module, thereby extending the service life of the component; the solder 112 exhibits excellent stability under different environments and will not fail as easily as adhesives; the solder 112 has higher mechanical strength and can effectively prevent the lens 111 from shifting or falling off when subjected to mechanical shock or vibration. Secondly, the solder 112 and the lens 111 are fixed to form an overall structure 110, and then the solder 112 on the overall structure 110 is crimped with the tube cap 120 having the tube cap opening 121c, thereby manufacturing the lens tube cap 100. Compared with the prior art method of first connecting the lens and the tube cap and then connecting the connection between the two with an adhesive, the manufacturing is convenient and the manufacturing efficiency is effectively improved. In addition, the thickness of the solder 112 is selected based on the flatness information of the cap opening 121c, which avoids the difficulty of controlling the amount of glue during the dispensing process, avoids the problem of overflow and gap, and improves the consistency and reliability of lens installation. Furthermore, the crimping position 121c1 of the cap opening 121c is determined, and then the overall structure 110 and the lens 111 are crimped to ensure accurate control of the crimping position.

[0061] Specifically, the manufacturing method of the lens cap 100 includes the following steps:

[0062] a. Select a metal with the same composition as the metal layer as the solder 112.

[0063] The surface of the tube cap 120 is plated with a metal layer as a protective layer to prevent oxidation of the tube cap 120. Therefore, a solder 112 with the same metal composition is selected and deposited on the lens 111 to form the overall structure 110. In this way, when the solder 112 is subsequently connected to the tube cap by hot melting, the metal layer on the surface of the solder 112 and the tube cap 120 has the same composition, which improves the stability of the connection between the tube cap 120 and the overall structure 110.

[0064] The solder 112 and the metal layer may contain the same metal component, which may be tin, but is not limited thereto.

[0065] It should be noted that conventional lenses do not have metal, so in the prior art, the lens and the tube cap 120 are connected by gluing. However, this embodiment utilizes the convenience of the metal layer on the surface of the tube cap 120 to prevent oxidation, and deposits solder 112 with the same metal composition as the metal layer on the lens 111 to form the overall structure 110.

[0066] b. According to the flatness information of the tube cap opening 121 c of the tube cap 120 , provide the solder 112 having a thickness corresponding to the flatness information.

[0067] like Figure 2 As shown, the tube cap 120 includes an end cap 121 and an end side 122, the edge of the end cap 121 extends downward to form the end side 122, the end cap 121 has opposite end cap upper surfaces 121a and end cap lower surfaces 121b, and the tube cap opening 121c passes through the end cap upper surface 121a and the end cap lower surface 121b.

[0068] Reference publication number CN109781659B discloses a method for preparing a photoelectric detector with a reference gas chamber, wherein the bottom surface of the end side 122 is connected to the pin, so the bottom surface of the end side 122 can be used as a reference surface, and the angle between the plane where the cap opening 121c is located and the reference surface is used as flatness information. Furthermore, in step b, a solder 112 of corresponding thickness is selected to ensure that the lens 111 is level, and the precise control of the amount of the solder 112 improves the consistency and reliability of the installation of the lens 111, wherein the thickness of the solder 112 can vary from 30 to 100 microns.

[0069] c. Fix the solder 112 to the lens 111 to form an integral structure 110 .

[0070] like Figure 2 and Figure 3 As shown, the lens 111 has a relative lens front side 111a and a lens back side 111b, the lens front side 111a has a spherical area 111a1 and a non-lens area 111a2 surrounding the spherical area 111a1, and the step c includes the following steps:

[0071] The solder 112 is fixed on the non-lens area 111 a 2 by means of an evaporation process, a sputtering process, a chemical plating process or an electroplating process.

[0072] The cap opening 121c is circular, the spherical area 111a1 is spherical, the edge of the lens 111 is square, and in the lens cap 100 structure, the spherical area 111a1 is located in the cap opening 121c, and the non-lens area 111a2 around the spherical area 111a1 is connected to the lower surface 121b of the end cap, that is, the solder 112 is connected between the lower surface 121b of the end cap and the non-lens area 111a2. Figure 3 , the solder 112 may be in a square frame structure, but is not limited thereto.

[0073] d. Determine the crimping position 121c1 of the tube cap opening 121c according to the alignment condition.

[0074] The alignment condition includes that the front face 111a of the lens is opposite to the lower surface 121b of the end cap, and the spherical region 111a1 of the lens 111 is opposite to the tube cap opening 121c. Thus, the spherical region 111a1 can be located in the tube cap opening 121c, and the non-lens region 111a2 around the spherical region 111a1 can be connected to the lower surface 121b of the end cap.

[0075] The step d comprises the following steps:

[0076] The area on the lower surface of the end cap 121 and surrounding the tube cap opening 121c is selected as the crimping position 121c1, that is, the solder 112 of the integral structure 110 is connected to the lower surface of the end cap 121 and surrounding the tube cap opening 121c.

[0077] e. Crimping the solder 112 of the overall structure 110 with the crimping position 121 c 1 to manufacture the lens cap 100 .

[0078] The step e comprises the following steps:

[0079] e1. Preheating the tube cap 120.

[0080] The tube cap 120 can be grabbed by the machine through recognition and brought to the preheating device, and the tube cap 120 can be preheated at 250° C. for 1S by the preheating device to provide a heat source for the subsequent hot-melt connection between the solder 112 and the tube cap 120. Automatic production can be achieved through machine recognition and grabbing.

[0081] e2. Crimping the solder 112 of the integral structure 110 with the crimping position 121c1 of the tube cap 120, so that the solder 112 is thermally melted to the tube cap 120 under the action of the preheated tube cap 120.

[0082] The step e2 comprises the following steps:

[0083] e21. Place the preheated pipe cap 120 on the welding table.

[0084] Similarly, the tube cap 120 can be grasped by the machine and placed on a high-temperature soldering table at 320-350° C., which not only keeps the heat of the tube cap 120 but also prepares for the subsequent solder 112 of the tube cap 120 and the overall structure 110 .

[0085] e22, grab the back side 111b of the lens 111 in the overall structure 110, so that the solder 112 on the front side 111a of the lens faces the crimping position 121c1 of the cap 120;

[0086] The grabbing of the overall structure 110 can also be performed through machine identification.

[0087] e23. The integral structure 110 and the tube cap 120 are crimped, and the solder 112 is thermally melted to the tube cap 120 under the action of the preheated tube cap 120.

[0088] When the solder 112 on the front side of the lens 111a is aligned with the crimping position 121c1 of the tube cap 120, the solder 112 on the front side of the lens 111a is crimped with the crimping position 121c1 of the tube cap 120 under a certain pressure of 10 to 15g. At this time, the solder 112 is connected to the tube cap 120 under the action of the tube cap 120 having thermal energy. At this time, welding can be completed in only 3 to 5 seconds without waiting for the curing time of the adhesive (whether it is thermal curing or light curing), which greatly shortens the overall production cycle, improves production efficiency, and is easy to manufacture.

[0089] e3. Cooling the crimped integral structure 110 and the tube cap 120.

[0090] The machine recognizes and grabs the whole structure 110 and the pipe cap 120 after crimping to the cooling zone, and nitrogen can be used to cool them down to room temperature to obtain the following Figure 2 The lens cap 100 is shown.

[0091] In summary, the solder 112 replaces the adhesive in the prior art, so that gas volatilization will not be generated during the soldering process of the solder 112, ensuring the internal environment and stability of the optical module, thereby extending the service life of the component; the solder 112 shows excellent stability under different environments and will not fail as easily as adhesives; the solder 112 has higher mechanical strength and can effectively prevent the lens 111 from being displaced or falling off when subjected to mechanical shock or vibration. Secondly, the solder 112 and the lens 111 are fixed to form an overall structure 110, and then the solder 112 on the overall structure 110 is used to crimp with the tube cap 120 having the tube cap opening 121c, thereby manufacturing the lens tube cap 100. Compared with the method of first connecting the lens and the tube cap in the prior art and then connecting the connection between the two with an adhesive, the manufacturing is convenient and the manufacturing efficiency is effectively improved. In addition, the thickness of the solder 112 is selected based on the flatness information of the cap opening 121c, which avoids the difficulty of controlling the amount of glue during the dispensing process, avoids the problem of overflow and gap, and improves the consistency and reliability of lens installation. Furthermore, the crimping position 121c1 of the cap opening 121c is determined, and then the overall structure 110 and the lens 111 are crimped to ensure accurate control of the crimping position.

[0092] It is further explained that in addition to tin metal, the solder 112 can also use glass solder. Compared with glass solder, the time required for soldering of gold-tin solder is shorter (3 to 5 seconds), and the thermal impact on the components during the soldering process is significantly reduced. At the same time, it has excellent thermal conductivity and mechanical strength, and can effectively conduct and dissipate heat to ensure the stability and reliability of the soldered joint. In addition, gold-tin solder has good solderability and oxidation resistance. The metal joint formed after welding is not easy to oxidize in a high temperature environment and is stable for a long time. These characteristics have a significant effect on improving performance and life.

[0093] Second embodiment

[0094] like Figure 2 and Figure 3 As shown, the lens cap 100 comprises:

[0095] An overall structure 110, wherein the overall structure 110 includes a lens 111 and a solder 112, wherein the solder 112 is fixedly connected to the lens 111;

[0096] A pipe cap 120, wherein the pipe cap 120 is provided with a pipe cap opening 121c, and the pipe cap opening 121c has a crimping position 121c1;

[0097] The solder 112 of the integral structure 110 is crimped to the crimping position 121 c 1 of the cap 120 .

[0098] The lens cap 100 of the second embodiment is manufactured by the manufacturing method of the first embodiment, so the lens cap 100 uses solder 112 to replace the adhesive in the prior art. The beneficial effects thereof can be referred to the first embodiment and will not be described in detail here.

[0099] refer to Figure 2 and Figure 3 The tube cap 120 includes an end cap 121, wherein the end cap 121 has an end cap upper surface 121a and an end cap lower surface 121b opposite to each other, and the tube cap opening 121c penetrates the end cap upper surface 121a and the end cap lower surface 121b;

[0100] The lens 111 has a front lens 111a and a back lens 111b opposite to each other, the front lens 111a has a spherical region 111a1 and a non-lens region 111a2 surrounding the spherical region 111a1, and the solder 112 is fixed on the non-lens region 111a2;

[0101] The solder 112 is connected between the non-lens area 111a2 and the end cap lower surface 121b of the end cap 121, and the spherical area 111a1 of the lens front surface 111a is located in the tube cap opening 121c.

[0102] The embodiments described above are only used to illustrate the technical ideas and features of the present invention, and their purpose is to enable technicians in this field to understand the contents of the present invention and implement them accordingly. The patent scope of the present invention cannot be limited only by this embodiment, that is, any equivalent changes or modifications made according to the spirit disclosed by the present invention still fall within the patent scope of the present invention.

Claims

1. A method for manufacturing a lens cap (100), characterized in that: The following steps are involved: b. providing solder (112) having a thickness corresponding to the flatness information of a tube cap opening (121c) of a tube cap (120); c. fixing the solder (112) to the lens (111) to form an integral structure (110); d. determining the crimping position (121c1) of the tube cap opening (121c) according to the alignment condition; e. crimping the solder (112) of the overall structure (110) and the crimping position (121c1) to produce a lens tube cap (100).

2. The method for manufacturing the lens cap (100) according to claim 1, characterized in that: The surface of the tube cap (120) is plated with a metal layer, and before step b, the manufacturing method further comprises the following steps: a. Select a metal with the same composition as the metal layer as the solder (112).

3. The method for manufacturing the lens cap (100) according to claim 1, characterized in that: The lens (111) has a front lens face (111a) and a back lens face (111b) opposite to each other, the front lens face (111a) has a spherical region (111a1) and a non-lens region (111a2) surrounding the spherical region (111a1), and step c comprises the following steps: The solder (112) is fixed on the non-lens area (111a2) by means of an evaporation process, a sputtering process, a chemical plating process or an electroplating process.

4. The method for manufacturing the lens cap (100) according to claim 3, characterized in that: The tube cap (120) includes an end cap (121), the end cap (121) has an end cap upper surface (121a) and an end cap lower surface (121b) opposite to each other, the tube cap opening (121c) passes through the end cap upper surface (121a) and the end cap lower surface (121b), and the alignment condition includes the front face of the lens (111a) being opposite to the end cap lower surface (121b), and the spherical area (111a1) of the lens (111) being opposite to the tube cap opening (121c).

5. The method for manufacturing the lens cap (100) according to claim 4, characterized in that: The step d comprises the following steps: The area on the lower surface of the end cap (121) and surrounding the pipe cap opening (121c) is selected as the crimping position (121c1).

6. The method for manufacturing the lens cap (100) according to claim 1, characterized in that: The step e comprises the following steps: e1, preheating the tube cap (120); e2. The solder (112) of the integral structure (110) is crimped onto the crimping position (121c1) of the tube cap (120), so that the solder (112) is thermally melted to the tube cap (120) under the action of the preheated tube cap (120).

7. The method for manufacturing the lens cap (100) according to claim 6, characterized in that: The step e2 comprises the following steps: e21, placing the preheated pipe cap (120) on a welding table; e22. Grab the back side (111b) of the lens (111) in the overall structure (110) so that the solder (112) on the front side (111a) of the lens is opposite to the crimping position (121c1) of the tube cap (120); e23. The overall structure (110) and the tube cap (120) are crimped together, and the solder (112) is thermally melted to the tube cap (120) under the action of the preheated tube cap (120).

8. The method for manufacturing the lens cap (100) according to claim 7, characterized in that: After step e2, the method further includes the following steps: e3. Cooling the crimped integral structure (110) and the tube cap (120).

9. A lens cap (100), characterized in that: include: An integral structure (110), the integral structure (110) comprising a lens (111) and solder (112), the solder (112) being fixedly connected to the lens (111); A pipe cap (120), wherein the pipe cap (120) is provided with a pipe cap opening (121c), and the pipe cap opening (121c) has a crimping position (121c1); The solder (112) of the integral structure (110) is crimped to the crimping position (121c1) of the tube cap (120).

10. The lens cap (100) according to claim 9, characterized in that: The tube cap (120) comprises an end cap (121), wherein the end cap (121) has an end cap upper surface (121a) and an end cap lower surface (121b) opposite to each other, and the tube cap opening (121c) penetrates the end cap upper surface (121a) and the end cap lower surface (121b); The lens (111) has a front lens face (111a) and a back lens face (111b) opposite to each other, the front lens face (111a) has a spherical region (111a1) and a non-lens region (111a2) surrounding the spherical region (111a1), and the solder (112) is fixed on the non-lens region (111a2); The solder (112) is connected between the non-lens area (111a2) and the lower surface (121b) of the end cap (121), and the spherical area (111a1) of the lens front (111a) is located in the tube cap opening (121c).

Citation Information

Patent Citations

  • Gold tin ring sealing technology method of semi-conductor device

    CN109514018A

  • Fixing method and fixing structure of optical lens in laser system

    CN110676674A

  • Method for making pipe caps by welding with glass solder

    CN111360434A

  • Lens tube cap and preparation method thereof

    CN111807721A

  • Pipe cap with novel optical lens

    CN220271639U