Heat sublimation soft label coating with high heat resistance and color density at high speed and preparation method of heat sublimation soft label coating

By using specific components in the thermal sublimation soft label coating, the melt bonding, color density reduction and anti-adhesive ribbon problems during high-speed printing are solved, and the thermal sublimation soft label coating with high heat resistance and color density is achieved. layer to ensure print quality and print head security.

CN118931332AInactive Publication Date: 2024-11-12HUNAN DINGYIYUAN TECH DEV CO LTD +1

Patent Information

Application Number
CN202411003509.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-25
Publication Date
2024-11-12
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The existing thermal sublimation printing technology has problems with melt bonding of the substrate, reduced color density and anti-adhesive ribbon during high-speed printing, resulting in damage to the print head and difficulty in maintaining high heat resistance and color density.

Method used

A thermal sublimation soft standard coating consisting of a base, a base coat and a printing layer. The base coat consists of a bonding resin, a reinforced bonding resin, a fluorescent whitening agent and a hollow thermal insulation material. The printing layer is made of dye-receiving resin and liquid. Sliding agents, solid fillers, crosslinking curing agents and antistatic agents are composed of which improve adhesion, dye acceptance and heat resistance.

Benefits of technology

It realizes no anti-stick phenomenon under high-speed printing (10m/min), maintains high color density and heat resistance, and the color density of the printing pattern is comparable to that of the traditional 2m/min thermal sublimation printer, avoiding damage to the print head.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118931332A_ABST
    Figure CN118931332A_ABST
Patent Text Reader

Abstract

The invention relates to a thermal dye sublimation soft label coating with high heat resistance and color density at high speed and a preparation method thereof, and relates to the technical field of thermal dye sublimation printing, the thermal dye sublimation soft label coating comprises a base body, a bottom coating and a printing layer, one side of the base body is provided with the bottom coating, and the other side of the base body is provided with the printing layer; the bottom coating is prepared from the following components in parts by weight: 8 to 24 parts of bonding resin, 5 to 15 parts of reinforced bonding resin, 0.1 to 0.3 part of fluorescent whitening agent and 1.25 to 3.75 parts of hollow heat insulation material; the printing layer is prepared from the following components in parts by weight: 20 parts of dye receiving resin, 0.25 to 0.75 part of liquid lubricant, 1.5 to 4.5 parts of solid filler, 0.2 to 2 parts of cross-linking curing agent, 0.5 to 4 parts of curing aid and 0.1 to 0.3 part of antistatic agent. The printing speed of the heat sublimation soft label coating can reach 6-10 m / min, meanwhile, high heat resistance and color density are kept during continuous printing, and the phenomenon of reverse adhesion of the coating is avoided.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of thermal sublimation printing, and in particular to a thermal sublimation soft label coating with high heat resistance and color density at high speed and a preparation method thereof. Background Art

[0002] Thermal sublimation soft label coating can realize continuous printing of patterns and can be used to replace the substrates of traditional photo printing. Generally speaking, there are several problems when the substrates without surface treatment are directly applied to thermal sublimation printing of packaging materials: (1) The substrates used for packaging printing require high-speed continuous printing. Traditional thermal sublimation photo paper is mainly used for photo printing. If it is directly applied to continuous printing, there will be a problem of melting and bonding between the thermal sublimation carbon ribbon and the substrate layer, which will fall off and stick to the print head, and even cause the print head to burn out in severe cases; (2) When the printing speed exceeds 2m / min, the dye acceptance capacity of the thermal sublimation printed substrate, that is, the color density, will be significantly reduced; (3) When the printing concentration is too high and the print head is pressed down at a low position, the substrate coating will have anti-sticky ribbons or carbon ribbons will fade, which will cause the print head to burn out in severe cases. In view of this, the present invention provides a thermal sublimation soft label coating with high heat resistance and color density at high speed and a preparation method thereof. Summary of the invention

[0003] The technical problem to be solved by the present invention is to provide a thermal sublimation soft label coating with high heat resistance and color density at high speed and a preparation method thereof. The purpose is to ensure that the thermal sublimation soft label coating does not stick back during high-speed printing (the continuous printing speed is increased to 10m / min), maintain the high color density and heat resistance of the printing, make the printed pattern exquisite, and have good applicability.

[0004] The present invention solves the above technical problems. The first purpose is to provide a thermal sublimation soft label coating with high heat resistance and color density at high speed, comprising a substrate, a primer layer and a printing layer, wherein one side of the substrate is provided with the primer layer, and the other side of the substrate is provided with the printing layer;

[0005] The primer layer comprises the following components in parts by weight: 8-24 parts of a bonding resin, 5-15 parts of a reinforcing bonding resin, 0.1-0.3 parts of a fluorescent brightener, and 1.25-3.75 parts of a hollow heat insulating material;

[0006] The printing layer comprises the following components in parts by weight: 20 parts of dye receiving resin, 0.25-0.75 parts of liquid lubricant, 1.5-4.5 parts of solid filler, 0.2-2 parts of cross-linking curing agent, 0.5-4 parts of curing auxiliary agent, and 0.1-0.3 parts of antistatic agent.

[0007] The beneficial effects of the present invention are:

[0008] (1) In the primer layer of the present invention, the bonding resin and the reinforcing bonding resin improve the adhesion between the substrate and the printing layer, making the printed material difficult to peel off; the fluorescent brightener improves the brightness of the dye receiving layer. The main characteristics of the fluorescent brightener are to absorb invisible ultraviolet rays and emit blue-violet light visible to the naked eye, thereby increasing the total amount of reflection, thereby making the thermal sublimation soft label coating look more vivid and bright; by adding a certain amount of hollow heat-insulating material to the primer layer, the dye receiving capacity of the printing layer can be improved, so that the printing layer is heated more evenly, the heat is not easily lost, and more dyes are sublimated to the coating surface, thereby obtaining a higher color density;

[0009] (2) In the printing layer of the present invention, the function of the dye receiving layer is to have a strong acceptance and coloring ability for the dye when the thermal sublimation ribbon image is printed, and to have better adhesion to the base layer and is not easy to peel off; because during the thermal sublimation printing process, the dye receiving layer is in close contact with the ribbon, and the substrate at the same position has to contact the ribbon three times, the risk of the dye receiving layer and the ribbon being bonded increases step by step. In order to prevent the problem of the dye receiving layer and the ribbon being bonded due to the melting of the resin caused by heating during the printing process, a certain amount of liquid lubricant needs to be added. The liquid lubricant will gradually Gradually migrate to the surface of the ribbon, so that the risk of the dye receiving layer ribbon bonding is reduced; the amount of liquid lubricant added should not be too high, and too much addition will affect the flatness of the film surface and affect the color density; in order to further improve the coating from sticking to the ribbon under high-speed printing, a certain amount of solid filler is added to increase the anti-stickiness and heat resistance; in order to further adapt to the high heat resistance required for thermal sublimation high-speed printing, the coating is cross-linked and cured to a certain extent by a cross-linking curing agent and a curing aid; in order to improve the resistance of the coating, a certain amount of antistatic agent is added;

[0010] (3) The printing speed of the thermal sublimation soft label coating of the present invention can reach 6-10m / min, while maintaining high heat resistance during continuous printing, without anti-sticking coating phenomenon, and the color density of the printed pattern is comparable to that of a traditional 2m / min thermal sublimation printer.

[0011] Based on the above technical solution, the present invention can also be improved as follows.

[0012] Further, the primer layer comprises the following components in parts by weight: 12-20 parts of a bonding resin, 7-13 parts of a reinforcing bonding resin, 0.15-0.25 parts of a fluorescent brightener, and 2-3 parts of a hollow heat insulating material;

[0013] The printing layer comprises the following components in parts by weight: 20 parts of dye receiving resin, 0.3-0.7 parts of liquid lubricant, 2-4 parts of solid filler, 0.3-1.5 parts of cross-linking curing agent, 0.5-3 parts of curing auxiliary agent, and 0.15-0.25 parts of antistatic agent.

[0014] Furthermore, the primer layer further comprises the following components in parts by weight: 0.1-0.3 parts of titanium dioxide.

[0015] The beneficial effect of adopting the above further scheme is that the above titanium dioxide can improve the reflectivity of light, make the color look fuller and brighter, and make the color density value higher.

[0016] Furthermore, the bonding resin includes any one of polyester resin, polyurethane resin (Po l yurethane), polycarbonate resin (PC for short), polyvinyl pyrrolidone resin (PVP for short), polyvinyl butyral resin, or a combination of at least two of them; the reinforcing bonding resin includes any one of CPP resin (chlorinated polypropylene resin), thermoplastic acrylic resin, EVA resin (ethylene-vinyl acetate copolymer), or a combination of at least two of them; the hollow insulation material includes any one of silicone resin particles, gas silicon, hollow particles (styrene acrylic or other acrylic hollow particles), and metal inorganic oxides (such as aluminum oxide, zinc oxide, titanium oxide), or a combination of at least two of them.

[0017] Among them, EVA resin (ethylene-vinyl acetate copolymer), English abbreviation: EVA, molecular formula: (C2H4) x· (C4H6O2) y .

[0018] Furthermore, the melting point of the hollow heat-insulating material is higher than 300° C., and the average particle size is 1-5 μm. Preferably, the average particle size is lower than 3 μm.

[0019] The beneficial effect of adopting the above further scheme is: if the particle size of the hollow thermal insulation material is too large, it will affect the smoothness of the coating surface. Similarly, if the amount added is too large, it will also affect the smoothness of the coating surface. If it is too little, it will not work. The advantage of adding hollow thermal insulation material to the base coating is to ensure that heat is not easily dissipated during printing. The size of the hollow thermal insulation material particle size will affect the roughness of the film surface, heat transfer efficiency and adhesion of the base coating. Therefore, the selection of the particle size of the hollow thermal insulation material is based on a balance between these three.

[0020] Furthermore, the dye receiving resin includes any one of chloroacetic acid resin (P(VC-VAc)), acrylonitrile-styrene copolymer (AS for short), polyethanol butyral resin, and chloroether resin (vinyl chloride-vinyl isobutyl ether resin) or a combination of at least two of them; the liquid lubricant includes aromatic modified polysiloxane, the solid filler includes any one of gas silica, wax powder, silicone resin, and metal inorganic oxides (such as aluminum oxide, zinc oxide) or a combination of at least two of them; the cross-linking curing agent includes polyisocyanate, and the curing aid includes any one of polyethylene glycol, polypropylene glycol, hydroxy acrylic resin, and ternary chloroacetic acid or a combination of at least two of them.

[0021] The chlorovinyl acetate resin is a vinyl chloride-vinyl acetate copolymer, such as dichlorovinyl acetate and terchlorovinyl acetate.

[0022] The aromatic modified polysiloxane can provide good slipperiness at high temperature (about 200° C.), so that the coating can maintain excellent slipperiness, and at the same time can help the coating film to level and improve the flatness of the coating film, thereby avoiding the problem of color fading caused by the adhesion of the color ribbon and the dye receiving layer during printing.

[0023] The aromatic polyisocyanate, for example, 2,4-toluene diisocyanate, 2,6-toluene diisocyanate, or a mixture of 2,4-toluene diisocyanate and 2,6-toluene diisocyanate, 1,5-naphthalene diisocyanate, toluidine diisocyanate, p-phenylene diisocyanate, trans-cyclohexane-1,4-diisocyanate, xylylene diisocyanate, triphenylmethane triisocyanate, tris(isocyanate phenyl)thiophosphate, particularly preferably 2,4-toluene diisocyanate, 2,6-toluene diisocyanate, a mixture of 2,4-toluene diisocyanate and 2,6-toluene diisocyanate. The addition amount is 1-10 phr, preferably 3-5 phr. In order to accelerate the curing of the coating, a certain amount of polar group-containing curing aids such as polyethylene glycol 200, polyethylene glycol 400, polyethylene glycol 600, polyethylene glycol 800, polyethylene glycol 2000, polyethylene glycol 8000, polyethylene glycol 20000 and polypropylene glycol 2000, hydroxylated acrylic resin, terchloroacetic acid, etc. are also required, preferably polyethylene glycol 600 and polypropylene glycol 2000. The NCO:OH ratio is 0.1-1.2, preferably 0.3-0.7.

[0024] Furthermore, the substrate includes any one of polyphenylene sulfide (PPS) film, polystyrene (PS) film, polyethylene (PE) film, polypropylene (PP) film, polyimide (PI) film, engineering plastic polyethylene terephthalate (PET) film, and coated paper.

[0025] Furthermore, the thickness of the substrate is 40-80 μm; the thickness of the primer layer is 0.3-1 μm; and the thickness of the printing layer is 3-10 μm.

[0026] The beneficial effects of adopting the above further scheme are: although the average particle size of the hollow insulation material is larger than the thickness of the base coating, the amount of hollow insulation material added is small. Although it will affect the roughness of the base coating film surface, it will not affect the printing quality at all when the thickness of the printing layer is thicker than the base coating; the thickness of the base coating affects the adhesion and print quality during printing; if it is too thick, the base coating resin will float to the printing layer due to the printing temperature during printing and stick to the ribbon; if it is too thin, the adhesion is insufficient during printing and the coating will peel off from the substrate.

[0027] Furthermore, the thickness of the substrate is 70 μm; the thickness of the primer layer is 0.4-0.6 μm; and the thickness of the printing layer is 5-7 μm.

[0028] The second object of the present invention is to provide a method for preparing a thermal sublimation soft label coating with high heat resistance and color density at high speed, comprising the following steps:

[0029] (1) preparing a primer solution by mixing the components of the primer layer with a solvent; preparing a printing solution by mixing the components of the printing layer with a solvent;

[0030] (2) coating the primer liquid on one side of the substrate by a gravure coater, and drying to obtain a primer layer; coating the printing liquid on the other side of the substrate by a gravure coater, and drying to obtain a printing layer. BRIEF DESCRIPTION OF THE DRAWINGS

[0031] Figure 1 It is a schematic structural diagram of the thermal sublimation soft label coating of the present invention.

[0032] In the accompanying drawings, the components represented by the reference numerals are listed as follows:

[0033] 1-base coating, 2-substrate, 3-printing layer. DETAILED DESCRIPTION

[0034] The principles and features of the present invention are described below. The examples are only used to explain the present invention and are not used to limit the scope of the present invention. If no specific techniques or conditions are specified in the examples, the techniques or conditions described in the literature in this field or the product instructions are used. If the manufacturer of the reagents or instruments is not specified, they are all conventional products that can be purchased through regular channels.

[0035] Embodiment 1:

[0036] The present embodiment relates to a thermal sublimation soft label coating with high heat resistance and color density at high speed, comprising a substrate 2, a primer layer 1 and a printing layer 3. The primer layer 1 is arranged on one side of the substrate 2, and the printing layer 3 is arranged on the other side of the substrate 2.

[0037] The method for preparing a thermal sublimation soft label coating with high heat resistance and color density at high speed involved in this embodiment comprises the following steps:

[0038] (1) preparing a primer solution by mixing the components of the primer layer 1 with a solvent; preparing a printing solution by mixing the components of the printing layer 3 with a solvent;

[0039] (2) The primer liquid is coated on one side of the substrate 2 by a gravure coater, and dried to obtain a primer layer 1; the printing liquid is coated on the other side of the substrate 2 by a gravure coater, and dried to obtain a printing layer 3.

[0040] Among them, substrate 2 uses 70um PP film, and the manufacturer is Zhongshan Xinguan Adhesive Products.

[0041] <Base coat 1>:

[0042] Polyester resin (SG-20 Changhao Chemical) 16 parts;

[0043] Thermoplastic acrylic resin (CTR-6118 CNOOC Changzhou Institute) 8 parts;

[0044] 2.5 parts of gas silicon (OK607 Evonik Chemicals);

[0045] Fluorescent brightener (OB BASF, Germany) 0.2 parts;

[0046] 2-butanone 23.3 parts;

[0047] Toluene 50 parts;

[0048] Coating was done by gravure coater, with a coating thickness of 0.6 μm.

[0049] <Printing layer 3>:

[0050] 20 parts of vinyl chloride-vinyl acetate copolymer (H15-42 Wacker Chemical, Germany);

[0051] Aromatic modified polysiloxane (AFCONA-3252 Efcona Chemical) 0.5 parts;

[0052] 1 part of polyethylene glycol-600 (PEG-600);

[0053] Antistatic agent (Atmer 129V, Croda, UK) 0.2 parts;

[0054] 3 parts of gas silicon (OK607 Evonik Chemicals);

[0055] Polyisocyanate curing agent (TFD-90SB Asahi Chemical Co., Ltd., Japan) 0.5 parts;

[0056] 2-butanone 37.4 parts;

[0057] Toluene 37.4 parts;

[0058] Coating was done by gravure coater, with a coating thickness of 5 μm.

[0059] Embodiment 2:

[0060] The present embodiment relates to a thermal sublimation soft label coating with high heat resistance and color density at high speed, comprising a substrate 2, a primer layer 1 and a printing layer 3. The primer layer 1 is arranged on one side of the substrate 2, and the printing layer 3 is arranged on the other side of the substrate 2.

[0061] The method for preparing a thermal sublimation soft label coating with high heat resistance and color density at high speed involved in this embodiment comprises the following steps:

[0062] (1) preparing a primer solution by mixing the components of the primer layer 1 with a solvent; preparing a printing solution by mixing the components of the printing layer 3 with a solvent;

[0063] (2) The primer liquid is coated on one side of the substrate 2 by a gravure coater, and dried to obtain a primer layer 1; the printing liquid is coated on the other side of the substrate 2 by a gravure coater, and dried to obtain a printing layer 3.

[0064] Among them, substrate 2 uses 70um PP film, and the manufacturer is Zhongshan Xinguan Adhesive Products.

[0065] The scheme of <Undercoat Layer 1> is the same as that of Example 1.

[0066] <Printing layer 3>:

[0067] 20 parts of vinyl chloride-vinyl acetate copolymer (CP-450 Hanwha Chemical);

[0068] Aromatic modified silicone resin (KF-1005 Shin-Etsu silicone) 0.5 parts;

[0069] 1 part of polyethylene glycol-600 (PEG-600);

[0070] Antistatic agent (Atmer 129V, Croda, UK) 0.2 parts;

[0071] 3 parts of gas silicon (OK607 Evonik Chemicals);

[0072] Polyisocyanate curing agent (TFD-90SB Asahi Chemical Co., Ltd., Japan) 0.5 parts;

[0073] 2-butanone 37.4 parts;

[0074] Toluene 37.4 parts;

[0075] Coating was done by gravure coater, with a coating thickness of 5 μm.

[0076] Embodiment 3:

[0077] The present embodiment relates to a thermal sublimation soft label coating with high heat resistance and color density at high speed, comprising a substrate 2, a primer layer 1 and a printing layer 3. The primer layer 1 is arranged on one side of the substrate 2, and the printing layer 3 is arranged on the other side of the substrate 2.

[0078] The method for preparing a thermal sublimation soft label coating with high heat resistance and color density at high speed involved in this embodiment comprises the following steps:

[0079] (1) preparing a primer solution by mixing the components of the primer layer 1 with a solvent; preparing a printing solution by mixing the components of the printing layer 3 with a solvent;

[0080] (2) The primer liquid is coated on one side of the substrate 2 by a gravure coater, and dried to obtain a primer layer 1; the printing liquid is coated on the other side of the substrate 2 by a gravure coater, and dried to obtain a printing layer 3.

[0081] Among them, substrate 2 uses 70um PP film, and the manufacturer is Zhongshan Xinguan Adhesive Products.

[0082] The scheme of <Undercoat Layer 1> is the same as that of Example 1.

[0083] <Printing layer 3>:

[0084] Vinyl chloride-vinyl acetate copolymer (SOLBINC Nissin Chemical) 20 parts;

[0085] 0.5 parts of silicone resin (BYK-323, Germany)

[0086] 1 part of polyethylene glycol-600 (PEG-600);

[0087] Antistatic agent (Atmer 129V, Croda, UK) 0.2 parts;

[0088] 3 parts of gas silicon (OK607 Evonik Chemicals);

[0089] Polyisocyanate curing agent (TFD-90SB Asahi Chemical Co., Ltd., Japan) 0.5 parts;

[0090] 2-butanone 37.4 parts;

[0091] Toluene 37.4 parts;

[0092] Coating was done by gravure coater, with a coating thickness of 5 μm.

[0093] Embodiment 4:

[0094] The present embodiment relates to a thermal sublimation soft label coating with high heat resistance and color density at high speed, comprising a substrate 2, a primer layer 1 and a printing layer 3. The primer layer 1 is arranged on one side of the substrate 2, and the printing layer 3 is arranged on the other side of the substrate 2.

[0095] The method for preparing a thermal sublimation soft label coating with high heat resistance and color density at high speed involved in this embodiment comprises the following steps:

[0096] (1) preparing a primer solution by mixing the components of the primer layer 1 with a solvent; preparing a printing solution by mixing the components of the printing layer 3 with a solvent;

[0097] (2) The primer liquid is coated on one side of the substrate 2 by a gravure coater, and dried to obtain a primer layer 1; the printing liquid is coated on the other side of the substrate 2 by a gravure coater, and dried to obtain a printing layer 3.

[0098] Among them, substrate 2 uses 70um PP film, and the manufacturer is Zhongshan Xinguan Adhesive Products.

[0099] <Base coat 1>

[0100] Polyester resin (SG-20 Changhao Chemical) 16 parts;

[0101] Low chlorinated polypropylene (822S Nippon Paper Manufacturing Co., Ltd.) 10 parts;

[0102] 2.5 parts of gas silicon (OK607 Evonik Chemicals);

[0103] Fluorescent brightener (OB BASF, Germany) 0.2 parts;

[0104] 2-butanone 35.65 parts;

[0105] Toluene 35.65 parts;

[0106] Coating was done by gravure coater, with a coating thickness of 0.6 μm.

[0107] <Printing layer 3>: The scheme is consistent with Example 1.

[0108] Embodiment 5:

[0109] The present embodiment relates to a thermal sublimation soft label coating with high heat resistance and color density at high speed, comprising a substrate 2, a primer layer 1 and a printing layer 3. The primer layer 1 is arranged on one side of the substrate 2, and the printing layer 3 is arranged on the other side of the substrate 2.

[0110] The method for preparing a thermal sublimation soft label coating with high heat resistance and color density at high speed involved in this embodiment comprises the following steps:

[0111] (1) preparing a primer solution by mixing the components of the primer layer 1 with a solvent; preparing a printing solution by mixing the components of the printing layer 3 with a solvent;

[0112] (2) The primer liquid is coated on one side of the substrate 2 by a gravure coater, and dried to obtain a primer layer 1; the printing liquid is coated on the other side of the substrate 2 by a gravure coater, and dried to obtain a printing layer 3.

[0113] Among them, substrate 2 uses 70um PP film, and the manufacturer is Zhongshan Xinguan Adhesive Products.

[0114] The scheme of <Undercoat Layer 1> is the same as that of Example 4.

[0115] <Printing layer 3>: The scheme is consistent with Example 2.

[0116] Coating was done by gravure coater, with a coating thickness of 5 μm.

[0117] Embodiment 6:

[0118] The present embodiment relates to a thermal sublimation soft label coating with high heat resistance and color density at high speed, comprising a substrate 2, a primer layer 1 and a printing layer 3. The primer layer 1 is arranged on one side of the substrate 2, and the printing layer 3 is arranged on the other side of the substrate 2.

[0119] The method for preparing a thermal sublimation soft label coating with high heat resistance and color density at high speed involved in this embodiment comprises the following steps:

[0120] (1) preparing a primer solution by mixing the components of the primer layer 1 with a solvent; preparing a printing solution by mixing the components of the printing layer 3 with a solvent;

[0121] (2) The primer liquid is coated on one side of the substrate 2 by a gravure coater, and dried to obtain a primer layer 1; the printing liquid is coated on the other side of the substrate 2 by a gravure coater, and dried to obtain a printing layer 3.

[0122] Among them, substrate 2 uses 70um PP film, and the manufacturer is Zhongshan Xinguan Adhesive Products.

[0123] The scheme of <Undercoat Layer 1> is the same as that of Example 4.

[0124] <Printing layer 3>: The scheme is consistent with Example 4.

[0125] Coating was done by gravure coater, with a coating thickness of 5 μm.

[0126] Comparative Example 1:

[0127] Compared with Example 1, the substrate 2 uses a 70um PP film, the manufacturer is Zhongshan Xinguan Adhesive Products. The bottom coating 1 is consistent with Example 1, without the printing layer 3. The rest is the same as Example 1.

[0128] Comparative Example 2:

[0129] Compared with Example 1, in this comparative example, the substrate 2 uses a 70um PP film produced by Zhongshan Xinguan Adhesive Products.

[0130] The scheme of <Undercoat Layer 1> is the same as that of Example 1.

[0131] <Printing layer 3>:

[0132] 20 parts of vinyl chloride-vinyl acetate copolymer (H15-42 Wacker Chemical, Germany);

[0133] 1 part of polyethylene glycol-600 (PEG-600);

[0134] Antistatic agent (Atmer 129V, Croda, UK) 0.2 parts;

[0135] 3 parts of gas silicon (OK607 Evonik Chemicals);

[0136] Polyisocyanate curing agent (TFD-90SB Asahi Chemical Co., Ltd., Japan) 0.5 parts;

[0137] 2-butanone 37.65 parts;

[0138] Toluene 37.65 parts;

[0139] Coating was done by gravure coater, with a coating thickness of 5 μm.

[0140] The rest is the same as Example 1.

[0141] Comparative Example 3:

[0142] Compared with Example 1, in this comparative example, the substrate 2 uses a 70um PP film produced by Zhongshan Xinguan Adhesive Products.

[0143] The scheme of <Undercoat Layer 1> is the same as that of Example 1.

[0144] <Printing layer 3>:

[0145] 20 parts of vinyl chloride-vinyl acetate copolymer (H15-42 Wacker Chemical, Germany);

[0146] Aromatic modified polysiloxane (AFCONA-3252 Efcona Chemical) 0.5 parts;

[0147] 1 part of polyethylene glycol-600 (PEG-600);

[0148] Antistatic agent (Atmer 129V, Croda, UK) 0.2 parts;

[0149] 3 parts of gas silicon (OK607 Evonik Chemicals);

[0150] 2-butanone 37.65 parts;

[0151] Toluene 37.65 parts;

[0152] Coating was done by gravure coater, with a coating thickness of 5 μm.

[0153] The rest is the same as Example 1.

[0154] Comparative Example 4:

[0155] Compared with Example 1, in this comparative example, the substrate 2 uses a 70um PP film produced by Zhongshan Xinguan Adhesive Products.

[0156] <Base coat 1>:

[0157] Polyester resin (SG-20 Changhao Chemical) 16 parts;

[0158] 2-butanone 42 parts;

[0159] Toluene 42 parts;

[0160] Coating was done by gravure coater, with a coating thickness of 0.6 μm.

[0161] <Printing layer 3>: The scheme is consistent with Example 1.

[0162] Coating was done by gravure coater, with a coating thickness of 5 μm.

[0163] The rest is the same as Example 1.

[0164] Comparative Example 5:

[0165] Compared with Example 1, in this comparative example, the substrate 2 uses a 70um PP film produced by Zhongshan Xinguan Adhesive Products.

[0166] <Base coat 1>:

[0167] Polyester resin (SG-20 Changhao Chemical) 16 parts;

[0168] Thermoplastic acrylic resin (CTR-6118 CNOOC Changzhou Institute) 8 parts;

[0169] 2.5 parts of gas silicon (OK607 Evonik Chemicals);

[0170] 2-butanone 23.5 parts;

[0171] Toluene 50 parts;

[0172] Coating was done by gravure coater, with a coating thickness of 0.6 μm.

[0173] <Printing layer 3>: The scheme is consistent with Example 1.

[0174] Coating was done by gravure coater, with a coating thickness of 5 μm.

[0175] The rest is the same as Example 1.

[0176] Comparative Example 6:

[0177] Compared with Example 1, in this comparative example, the substrate 2 uses a 70um PP film produced by Zhongshan Xinguan Adhesive Products.

[0178] <Base coat 1>:

[0179] Polyester resin (SG-20 Changhao Chemical) 16 parts;

[0180] Thermoplastic acrylic resin (CTR-6118 CNOOC Changzhou Institute) 8 parts;

[0181] Fluorescent brightener (OB BASF, Germany) 0.2 parts;

[0182] 2-butanone 25.8 parts;

[0183] Toluene 50 parts;

[0184] Coating was done by gravure coater, with a coating thickness of 0.6 μm.

[0185] <Printing layer 3>: The scheme is consistent with Example 1.

[0186] Coating was done by gravure coater, with a coating thickness of 5 μm.

[0187] The rest is the same as Example 1.

[0188] Performance test plan:

[0189] The printing test was carried out using a DTP330 thermal sublimation soft label printer, the original ribbon was used, and the printing speed was 10m / min.

[0190] Color density test: Use X-Rite i1-PRO3 colorimeter for color density test, the printed pattern is 100% solid color block image, the sample size is 6×8 inches, and the OD value requirements are: K>1.8, C greater than 1.6, M>1.9, Y>1.5.

[0191] Heat resistance test: Use DTP330 to print, the printed pattern is 100% solid color block, the sample size is 6×8 inches, and the substrate coating is required to have no anti-sticking, and the ribbon is required to have no fading or breaking. The results are shown in Tables 1 and 2.

[0192] Table 1 Performance comparison results of the embodiments

[0193]

[0194] Table 2 Comparison results of comparative examples

[0195]

[0196] Tables 1 and 2 show that adding hollow insulation materials to the base coating can significantly improve the printing color density, and adding a lubricant to the printing layer can significantly improve the heat resistance of the coating.

[0197] In summary, the thermal sublimation soft label coating of the present invention can reach a printing speed of 6-10m / min, while maintaining high heat resistance during continuous printing, without anti-stick coating phenomenon, and the color density of the printed pattern is comparable to that of a traditional 2m / min thermal sublimation printer.

[0198] In the description of this specification, the description with reference to the terms "one embodiment", "some embodiments", "example", "specific example", or "some examples" etc. means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representations of the above terms do not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described may be combined in any one or more embodiments or examples in a suitable manner. In addition, those skilled in the art may combine and combine the different embodiments or examples described in this specification and the features of the different embodiments or examples, without contradiction.

[0199] Although the embodiments of the present invention have been shown and described above, it is to be understood that the above embodiments are exemplary and are not to be construed as limitations of the present invention. A person skilled in the art may change, modify, replace and vary the above embodiments within the scope of the present invention.

Claims

1. A thermal sublimation soft label coating with high heat resistance and color density at high speed, comprising a substrate, characterized in that: It also includes a primer layer and a printing layer, wherein one side of the substrate is provided with the primer layer, and the other side of the substrate is provided with the printing layer; The primer layer comprises the following components in parts by weight: 8-24 parts of a bonding resin, 5-15 parts of a reinforcing bonding resin, 0.1-0.3 parts of a fluorescent brightener, and 1.25-3.75 parts of a hollow heat insulating material; The printing layer comprises the following components in parts by weight: 20 parts of dye receiving resin, 0.25-0.75 parts of liquid lubricant, 1.5-4.5 parts of solid filler, 0.2-2 parts of cross-linking curing agent, 0.5-4 parts of curing auxiliary agent, and 0.1-0.3 parts of antistatic agent.

2. The thermal sublimation soft label coating with high heat resistance and color density at high speed according to claim 1, characterized in that: The primer layer comprises the following components in parts by weight: 12-20 parts of a bonding resin, 7-13 parts of a reinforcing bonding resin, 0.15-0.25 parts of a fluorescent brightener, and 2-3 parts of a hollow heat insulating material; The printing layer comprises the following components in parts by weight: 20 parts of dye receiving resin, 0.3-0.7 parts of liquid lubricant, 2-4 parts of solid filler, 0.3-1.5 parts of cross-linking curing agent, 0.5-3 parts of curing auxiliary agent, and 0.15-0.25 parts of antistatic agent.

3. The thermal sublimation soft label coating with high heat resistance and color density at high speed according to claim 1 or 2, characterized in that: The primer layer further comprises the following components in parts by weight: 0.1-0.3 parts of titanium dioxide.

4. The thermal sublimation soft label coating with high heat resistance and color density at high speed according to claim 1 or 2, characterized in that: The bonding resin includes any one of polyester resin, polyurethane resin, polycarbonate resin, polyvinyl pyrrolidone resin, polyvinyl butyral resin, or a combination of at least two of them; the reinforcing bonding resin includes any one of CPP resin, thermoplastic acrylic resin, EVA resin, or a combination of at least two of them; the hollow insulation material includes any one of silicone resin particles, gas silicon, hollow particles, and metal inorganic oxides, or a combination of at least two of them.

5. The thermal sublimation soft label coating with high heat resistance and color density at high speed according to claim 4, characterized in that: The melting point of the hollow heat-insulating material is higher than 300° C., and the average particle size is 1-5 μm.

6. The thermal sublimation soft label coating with high heat resistance and color density at high speed according to claim 1 or 2, characterized in that: The dye receiving resin includes any one of chloroacetic acid resin, acrylonitrile-styrene copolymer, polyethanol butyral resin, chloroether resin or a combination of at least two thereof; the liquid lubricant includes aromatic modified polysiloxane; the solid filler includes any one of gas silicon, wax powder, silicone resin, and metal inorganic oxide or a combination of at least two thereof; the cross-linking curing agent includes polyisocyanate; the curing aid includes any one of polyethylene glycol, polypropylene glycol, hydroxy acrylic resin, and ternary chloroacetic acid or a combination of at least two thereof.

7. The thermal sublimation soft label coating with high heat resistance and color density at high speed according to claim 1, characterized in that: The substrate includes any one of polyphenylene sulfide film, polystyrene film, polyethylene film, polypropylene film, polyimide film, engineering plastic polyethylene terephthalate film, and coated paper.

8. The thermal sublimation soft label coating with high heat resistance and color density at high speed according to claim 1, characterized in that: The thickness of the substrate is 40-80 μm; the thickness of the primer layer is 0.3-1 μm; and the thickness of the printing layer is 3-10 μm.

9. The thermal sublimation soft label coating with high heat resistance and color density at high speed according to claim 1, characterized in that: The thickness of the substrate is 70 μm; the thickness of the primer layer is 0.4-0.6 μm; and the thickness of the printing layer is 5-7 μm.

10. The method for preparing a thermal sublimation soft label coating with high heat resistance and color density at high speed according to any one of claims 1 to 9, characterized in that: The steps include: (1) preparing a primer solution by mixing the components of the primer layer with a solvent; preparing a printing solution by mixing the components of the printing layer with a solvent; (2) coating the primer liquid on one side of the substrate by a gravure coater, and drying to obtain a primer layer; coating the printing liquid on the other side of the substrate by a gravure coater, and drying to obtain a printing layer.

Citation Information

Patent Citations

  • Thermal transfer receiving sheet

    CN101111391A

  • Thermal transfer receiving sheet

    CN101318423A

  • Holding paper for dye-sublimation thermal-transfer recording, and a production method therefor

    CN102089155A

  • Thermal sublimation ribbon capable of keeping high color density under high-speed printing and high-speed printing stock

    CN115635785A

  • Thermal transfer image receiving sheet and method for manufacturing the same

    JP2013071378A

Cited By

  • Thermal transfer printing receiving sheet and application thereof

    CN121043520A