Stable ore filling control method for concealed goaf of strip mine
Through geological exploration and drilling, the location of the goaf is determined, combined with cemented materials and layered filling method of multiple grouting, the problem of poor filling effect of hidden goafs in open-pit mines is solved, and safety and slope stability are improved , reducing the risk of groundwater gushing out.
Patent Information
- Application Number
- CN202411113119.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-14
- Publication Date
- 2024-11-12
AI Technical Summary
The existing technology has poor filling effect in hidden goafs in open-pit mines, resulting in equipment and personnel safety threats, slope instability and groundwater resources. The filling effect is caused by poor ventilation and high water content in single or secondary grouting methods. Not ideal.
Geological exploration is used to determine the goaf location, drilling construction and cementing materials are mixed, and layered filling of feed pipes and multiple grouting reinforcement, combined with dry filling and cementing filling, the volume is gradually compensated and the filling strength is enhanced.
It effectively improves the stability and safety of goaf filling, reduces the risk of equipment damage and casualties, enhances slope stability, reduces the possibility of groundwater gushing out, and improves the filling effect.
Smart Images

Figure CN118934011A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a field, and in particular to a method for controlling the stability of ore filling in a concealed goaf area of an open-pit mine. Background Art
[0002] Concealed goaf in open-pit mines refers to the undiscovered or incompletely processed hollow areas formed under or around the ore body during open-pit mining due to historical mining activities or other geological reasons. These goafs may be difficult to detect directly due to thick overburden and complex geological conditions, so they are called "concealed" goafs.
[0003] "Hidden" goaf areas are more harmful:
[0004] Hazards to operating equipment and personnel: When operating equipment such as drilling rigs, electric shovels, portable crushing stations, bulldozers, and dump trucks are operating or staying above the goaf, if the overlying rock strata in the goaf suddenly collapse, the equipment may overturn or fall into the collapsed area, causing casualties to the operators and damage to the equipment; at the same time, harmful gases such as hydrogen sulfide and carbon monoxide may escape during the collapse process, seriously threatening the personal safety of the operators.
[0005] Impact on the stability of open-pit mine slopes: The existence of goafs will destroy the stress balance of the rock strata, causing the rock strata and the ground surface to move. When goafs are located near the slopes of open-pit mines, it is likely to cause landslides on the slopes, thus affecting the normal production of the open-pit mine.
[0006] Impact on groundwater resources and ecological environment: A large amount of groundwater may accumulate in the goaf, forming old goaf water. This old goaf water may suddenly gush out due to geological activities or human factors, which will not only increase the burden of underground drainage, but also cause water seepage accidents and damage the ecological environment.
[0007] However, in the prior art, single or double grouting is used to fill the goaf. Since the ventilation of the goaf is poor and the grouting water content is high, this method will reduce the volume of the entire filling area after grouting, resulting in poor filling effect.
[0008] To this end, the present invention proposes a method for controlling the stability of ore filling in concealed goaf areas of open-pit mines Summary of the invention
[0009] The purpose of the present invention is to solve the shortcomings of the prior art and to propose a method for controlling the stability of ore filling in concealed goaf areas of open-pit mines.
[0010] In order to achieve the above object, the present invention adopts the following technical solutions:
[0011] The method for controlling the stability of ore filling in concealed goaf of open-pit mines comprises the following steps:
[0012] S1: Geological exploration, using geophysical exploration methods to determine the location, shape and scale of hidden goaf areas;
[0013] S2: Drilling construction, determine the drilling location and drill, and verify the location of the goaf while drilling;
[0014] S3: Filler preparation, ore processing and selection of cementing materials for mixing;
[0015] S4: Installation of feeding pipe: insert a feeding pipe with a hemoplate into each borehole, and extend the lower pipe opening of the feeding pipe into the roof of the goaf;
[0016] S5: Layered filling and grouting reinforcement, followed by grouting filling along the feeding pipe;
[0017] S6: Maintenance: perform maintenance on the filled area.
[0018] Preferably, in step S1, the geophysical exploration method adopts any one or more combinations of seismic exploration, electrical exploration, and radar exploration.
[0019] Preferably: the step S2 specifically includes the following steps:
[0020] S21: Drilling a first hole at the middle position above the goaf determined in step S1. If the first hole is not actually located in the goaf, return to S1 for re-exploration. If the first hole is located in the goaf, proceed to the next step.
[0021] S22: According to the plum blossom pattern, with the first hole as the center of the plum blossom pattern, determine the location of subsequent holes, and drill holes one by one. If the drilling position is not located in the goaf, determine that the hole is the edge of the goaf. Otherwise, use the corner holes of the plum blossom pattern as a reference and drill the remaining holes again according to the plum blossom pattern until the locations of the new holes are no longer located in the goaf.
[0022] Preferably: the step S3 includes the following steps:
[0023] S31: crushing the mined ore using a crusher, and then screening the crushed ore;
[0024] S32: mixing the screened fine material with cement to form a cementitious material;
[0025] S33: The cementing material is allowed to stand to separate water, and the separated water is removed.
[0026] Preferably: in the step S31, the diameter of the sieve hole is 30-50 mm.
[0027] Preferably: in the step S4, the diameter of the feeding pipe is 20-30 mm smaller than the diameter of the drill hole.
[0028] Preferably: the step S5 comprises the following steps:
[0029] S51: dry filling stage, the screened coarse material is put into the goaf through the feeding pipe;
[0030] S52: cementing and filling stage, injecting the cementing material after removing the water into the feeding pipe, so that it falls into the goaf;
[0031] S53: multiple grouting, after the last grouting is completed, if the grouting height decreases over time, continue to grout.
[0032] Preferably: in the step S51, the coarse material occupies 40%-60% of the volume of the goaf.
[0033] Preferably: in the step S52, the grouting pressure is greater than 2.5 MPa.
[0034] Preferably: in the step S6, after the filler solidifies, water spray maintenance is carried out, the water spraying is maintained at a moderate level greater than 95%, and the maintenance period is 25-30 days.
[0035] The beneficial effects of the present invention are:
[0036] 1. The present invention performs water separation treatment on the grouting slurry to reduce the water content, and then performs grouting in multiple times, so as to compensate for the volume and ensure the filling effect. At the same time, the filler is first filled with screened coarse materials and then poured, so as to increase the filling strength. BRIEF DESCRIPTION OF THE DRAWINGS
[0037] Figure 1 The present invention is a flow chart of the method for controlling the stability of ore filling in concealed goaf areas in open-pit mines. DETAILED DESCRIPTION
[0038] The technical solution of the present invention is further described in detail below in conjunction with specific implementation methods.
[0039] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", and "set" should be understood in a broad sense, for example, they can be fixedly connected or set, or detachably connected or set, or integrally connected or set. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0040] Embodiment 1:
[0041] The method for controlling the stability of ore filling in concealed goaf of open-pit mines comprises the following steps:
[0042] S1: Geological exploration, using geophysical exploration methods to determine the location, shape and scale of hidden goaf areas;
[0043] S2: Drilling construction, determine the drilling location and drill, and verify the location of the goaf while drilling;
[0044] S3: Filler preparation, ore processing and selection of cementing materials for mixing;
[0045] S4: Installation of feeding pipe: insert a feeding pipe with a hemoplate into each borehole, and extend the lower pipe opening of the feeding pipe into the roof of the goaf;
[0046] S5: Layered filling and grouting reinforcement, followed by grouting filling along the feeding pipe;
[0047] S6: Maintenance: perform maintenance on the filled area.
[0048] Embodiment 2:
[0049] The method for controlling the stability of ore filling in concealed goaf of open-pit mines comprises the following steps:
[0050] S1: Geological exploration, using geophysical exploration methods to determine the location, shape and scale of hidden goaf areas;
[0051] S2: Drilling construction, determine the drilling location and drill, and verify the location of the goaf while drilling;
[0052] S3: Filler preparation, ore processing and selection of cementing materials for mixing;
[0053] S4: Installation of feeding pipe: insert a feeding pipe with a hemoplate into each borehole, and extend the lower pipe opening of the feeding pipe into the roof of the goaf;
[0054] S5: Layered filling and grouting reinforcement, followed by grouting filling along the feeding pipe;
[0055] S6: Maintenance: perform maintenance on the filled area.
[0056] In step S1, the geophysical exploration method adopts any one or more combinations of seismic exploration, electrical exploration, and radar exploration.
[0057] The step S3 includes the following steps:
[0058] S31: crushing the mined ore using a crusher, and then screening the crushed ore;
[0059] S32: mixing the screened fine material with cement to form a cementitious material;
[0060] S33: The cementing material is allowed to stand to separate water, and the separated water is removed.
[0061] In the step S4, the diameter of the feeding pipe is 20-30 mm smaller than the diameter of the drilled hole.
[0062] The step S5 comprises the following steps:
[0063] S51: dry filling stage, the screened coarse material is put into the goaf through the feeding pipe;
[0064] S52: cementing and filling stage, injecting the cementing material after removing the water into the feeding pipe, so that it falls into the goaf;
[0065] S53: multiple grouting, after the last grouting is completed, if the grouting height decreases over time, continue to grout.
[0066] In the step S52, the grouting pressure is greater than 2.5 MPa.
[0067] In the step S6, after the filler solidifies, water spraying maintenance is performed.
[0068] In the step S6, water is sprayed to maintain the humidity greater than 95%, and the maintenance period is 25-30 days.
[0069] Embodiment 3:
[0070] The method for controlling the stability of ore filling in concealed goaf of open-pit mines comprises the following steps:
[0071] S1: Geological exploration, using geophysical exploration methods to determine the location, shape and scale of hidden goaf areas;
[0072] S2: Drilling construction, determine the drilling location and drill, and verify the location of the goaf while drilling;
[0073] S3: Filler preparation, ore processing and selection of cementing materials for mixing;
[0074] S4: Installation of feeding pipe: insert a feeding pipe with a hemoplate into each borehole, and extend the lower pipe opening of the feeding pipe into the roof of the goaf;
[0075] S5: Layered filling and grouting reinforcement, followed by grouting filling along the feeding pipe;
[0076] S6: Maintenance: perform maintenance on the filled area.
[0077] In step S1, the geophysical exploration method adopts any one or more combinations of seismic exploration, electrical exploration, and radar exploration.
[0078] The S2 step specifically includes the following steps:
[0079] S21: Drilling a first hole at the middle position above the goaf determined in step S1. If the first hole is not actually located in the goaf, return to S1 for re-exploration. If the first hole is located in the goaf, proceed to the next step.
[0080] S22: According to the plum blossom pattern, with the first hole as the center of the plum blossom pattern, determine the location of subsequent holes, and drill holes one by one. If the drilling position is not located in the goaf, determine that the hole is the edge of the goaf. Otherwise, take the corner holes of the plum blossom pattern as a reference, and drill the remaining holes again according to the plum blossom pattern until the locations of the new holes are not located in the goaf.
[0081] The step S3 includes the following steps:
[0082] S31: crushing the mined ore using a crusher, and then screening the crushed ore;
[0083] S32: mixing the screened fine material with cement to form a cementitious material;
[0084] S33: The cementing material is allowed to stand to separate water, and the separated water is removed.
[0085] In the step S31, the diameter of the sieve hole is 30-50 mm.
[0086] In the step S4, the diameter of the feeding pipe is 20-30 mm smaller than the diameter of the drilled hole.
[0087] The step S5 comprises the following steps:
[0088] S51: dry filling stage, the screened coarse material is put into the goaf through the feeding pipe;
[0089] S52: cementing and filling stage, injecting the cementing material after removing the water into the feeding pipe, so that it falls into the goaf;
[0090] S53: multiple grouting, after the last grouting is completed, if the grouting height decreases over time, continue to grout.
[0091] In the step S51, the coarse material occupies 40%-60% of the volume of the goaf.
[0092] In the step S52, the grouting pressure is greater than 2.5 MPa.
[0093] In the step S6, after the filler solidifies, water spraying maintenance is performed.
[0094] In the step S6, water is sprayed to maintain the humidity greater than 95%, and the maintenance period is 25-30 days.
[0095] The above description is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes according to the technical scheme and inventive concept of the present invention within the technical scope disclosed by the present invention, which should be covered by the protection scope of the present invention.
Claims
1. A method for controlling the stability of ore filling in concealed goaf areas of open-pit mines, characterized in that: The following steps are involved: S1: Geological exploration, using geophysical exploration methods to determine the location, shape and scale of hidden goaf areas; S2: Drilling construction, determine the drilling location and drill, and verify the location of the goaf while drilling; S3: Filler preparation, ore processing and selection of cementing materials for mixing; S4: Installation of feeding pipe: insert a feeding pipe with a hemoplate into each borehole, and extend the lower pipe opening of the feeding pipe into the roof of the goaf; S5: Layered filling and grouting reinforcement, followed by grouting filling along the feeding pipe; S6: Maintenance: perform maintenance on the filled area.
2. The method for controlling the stability of ore filling in concealed goaf areas in open-pit mines according to claim 1, characterized in that: In step S1, the geophysical exploration method adopts any one or more combinations of seismic exploration, electrical exploration, and radar exploration.
3. The method for controlling the stability of ore filling in concealed goaf areas in open-pit mines according to claim 1, characterized in that: The S2 step specifically includes the following steps: S21: Drilling a first hole at the middle position above the goaf determined in step S1. If the first hole is not actually located in the goaf, return to S1 for re-exploration. If the first hole is located in the goaf, proceed to the next step. S22: According to the plum blossom pattern, with the first hole as the center of the plum blossom pattern, determine the location of subsequent holes, and drill holes one by one. If the drilling position is not located in the goaf, determine that the hole is the edge of the goaf. Otherwise, use the corner holes of the plum blossom pattern as a reference and drill the remaining holes again according to the plum blossom pattern until the locations of the new holes are no longer located in the goaf.
4. The method for controlling the stability of ore filling in concealed goaf areas in open-pit mines according to claim 1, characterized in that: The step S3 includes the following steps: S31: crushing the mined ore using a crusher, and then screening the crushed ore; S32: mixing the screened fine material with cement to form a cementitious material; S33: The cementing material is allowed to stand to separate water, and the separated water is removed.
5. The method for controlling the stability of ore filling in concealed goaf areas in open-pit mines according to claim 4 is characterized in that: In the step S31, the diameter of the sieve hole is 30-50 mm.
6. The method for controlling the stability of ore filling in concealed goaf areas in open-pit mines according to claim 1, characterized in that: In the step S4, the diameter of the feeding pipe is 20-30 mm smaller than the diameter of the drilled hole.
7. The method for controlling the stability of ore filling in concealed goaf areas in open-pit mines according to claim 1, characterized in that: The step S5 comprises the following steps: S51: dry filling stage, the screened coarse material is put into the goaf through the feeding pipe; S52: cementing and filling stage, injecting the cementing material after removing the water into the feeding pipe, so that it falls into the goaf; S53: multiple grouting, after the last grouting is completed, if the grouting height decreases over time, continue to grout.
8. The method for controlling the stability of ore filling in concealed goaf areas in open-pit mines according to claim 7, characterized in that: In the step S51, the coarse material occupies 40%-60% of the volume of the goaf.
9. The method for controlling the stability of ore filling in concealed goaf areas in open-pit mines according to claim 1, characterized in that: In the step S52, the grouting pressure is greater than 2.5 MPa.
10. The method for controlling the stability of ore filling in concealed goaf areas in open-pit mines according to claim 1, characterized in that: In the step S6, after the filler solidifies, water spraying maintenance is carried out to keep the humidity greater than 95%, and the maintenance period is 25-30 days.