Kiln for extracting phosphorus steam from phosphate ore
By designing the preheating section, heating section and cooling section of the kiln, combined with gas-cooled pipes and automated control, the high energy consumption and environmental pollution problems of the existing phosphorus ore extraction process are solved, and the recycling and drying of high-purity phosphorus vapor is achieved. Reduces operating costs and improves production safety and environmental protection.
Patent Information
- Application Number
- CN202411252091.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-06
- Publication Date
- 2024-11-12
AI Technical Summary
The existing electric furnace process for extracting phosphorus vapor from phosphate ores has high energy consumption, environmental pollution, complex refining processes and high investment costs, and the waste residue generated contains harmful components, affecting the environment and human health.
A kiln is designed, including a preheating section, a heating section and a cooling section, equipped with phosphorus discharge ports, a temperature measurement unit and an air-cooling pipe. Through automated control, high-purity phosphorus vapor is recovered and dried, reducing smoke and impurities, and reducing operating costs. .
It improves the purity and recycling efficiency of phosphorus vapor, reduces operating costs, realizes a safe and environmentally friendly production process, and reduces the generation of waste slag.
Smart Images

Figure CN118936033A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of extracting phosphorus vapor from phosphate ore, and particularly relates to a kiln used for extracting phosphorus vapor from phosphate ore. Background Art
[0002] Phosphoric acid production technology has developed to date, and there are two main processes: (1) Wet method: using sulfuric acid to decompose medium- and high-grade phosphate ore to produce phosphoric acid. This method requires a large amount of high-quality phosphate ore and sulfuric acid, and also produces a large amount of phosphogypsum waste that is difficult to utilize. Wet phosphoric acid has a high impurity content, a complex purification process, and high costs. In addition, the current domestic sulfur price remains high, resulting in a substantial increase in the cost of wet phosphoric acid. (2) Thermal method: using an electric furnace to reduce phosphate ore to produce elemental yellow phosphorus, which is then burned and absorbed in a combustion tower to produce phosphoric acid. This method requires a large amount of electricity (15,000-16,000 kWh per ton of yellow phosphorus produced) and medium- and high-grade phosphate ore blocks, and causes serious environmental pollution. This is almost the only method for producing yellow phosphorus in the world, but many developed countries restrict the use of thermal methods to produce yellow phosphorus.
[0003] Kiln-process phosphoric acid is the third method that is different from the wet method and the thermal method. Its reaction principle is similar to that of thermal phosphoric acid. The mixed material is subjected to a solid-phase reaction, and the reduction and oxidation processes of elemental phosphorus are placed in one device. In this way, the heat released by the combustion of elemental phosphorus and by-product carbon monoxide can be used to provide the heat required for the reduction of elemental phosphorus, greatly saving energy consumption. At the same time, medium and low-grade phosphate ore can be used, greatly broadening the grade range of direct utilization of phosphate ore.
[0004] The existing production method of extracting phosphorus vapor from phosphate ore is to use a carbon thermal reduction method in an electric furnace, and the raw materials are phosphate ore, silica and coke. Under the high temperature of the electric furnace, the phosphate ore undergoes a carbon thermal reduction reaction to generate phosphorus vapor, which is cooled to a suitable temperature together with the furnace dust to produce yellow phosphorus, and then the yellow phosphorus product is obtained after rinsing and refining. The high-temperature slag is directly discharged from the electric furnace. If other products such as red phosphorus need to be produced, it needs to be converted through the yellow phosphorus product.
[0005] At present, the phosphorus vapor preparation electric furnace in China directly introduces the phosphorus vapor generated by the reaction into the subsequent cooling and spraying system. This method has a large dust content in the phosphorus vapor and produces a large amount of waste slag, which contains a large amount of harmful components such as fluoride, arsenide and heavy metals, which will cause serious harm to the environment and human body.
[0006] On the other hand, due to the limitation of the structure of the electric furnace, the temperature of phosphorus vapor passing through the phosphorus outlet is relatively low, and most of the phosphorus sprayed down is crude yellow phosphorus. Under the current process, the subsequent crude phosphorus refining process is very complicated and lengthy, and the refining equipment has a complex structure, occupies a large area, and has a high investment cost. Moreover, as the use time of the electric furnace increases, the dust and coke (coal) in the electric furnace are easily oxidized with phosphorus vapor to form metaphosphoric acid and condense around the electrode hole, which can easily cause poor insulation of the electrode, resulting in frequent arcing and furnace shutdown. The inner wall of the furnace cavity often retains a phosphorus-containing layer, which will increase the maintenance cost. Summary of the invention
[0007] In order to solve the above technical problems, the present invention adopts the following technical solutions:
[0008] A kiln for extracting phosphorus vapor from phosphate ore, comprising:
[0009] The kiln body has a preheating section, a heating section and a cooling section arranged in sequence along the length direction;
[0010] Tracks are symmetrically arranged in the kiln body and extend along the length direction of the kiln body;
[0011] At least one of the preheating section and the cooling section is provided with a phosphorus discharge port, and the phosphorus discharge port is connected to an external phosphorus vapor collection device;
[0012] The temperature measuring unit is arranged on the inner wall of the kiln body and acts on the material.
[0013] Furthermore, the kiln body is provided with an air cooling pipe for guiding the hot air in the cooling section to the external drying chamber.
[0014] Furthermore, the air cooling pipe includes a first connecting pipe that runs through the top of the cooling section, and both ends of the first connecting pipe are respectively connected to the second connecting pipe and the third connecting pipe, and the three form a U-shaped structure.
[0015] Furthermore, the end of the second connecting pipe is connected to a blowing device, and the end of the third connecting pipe is connected to an external drying chamber.
[0016] Furthermore, multiple groups of phosphorus discharge ports are provided in the preheating section and the cooling section.
[0017] Furthermore, isolation plates are installed at the top and bottom of the kiln body, and sealing plates are installed at the periphery of the kiln body.
[0018] Furthermore, the track is installed on the isolation plate, and the track runs through the entire kiln body.
[0019] Furthermore, the heating section area is provided with refractory material.
[0020] Furthermore, the temperature measuring unit is arranged in the heating section.
[0021] Furthermore, the temperature measuring unit includes a thermocouple and a pressure measuring element.
[0022] Compared with the prior art, the present invention has the following beneficial effects:
[0023] The present invention divides the kiln body into a preheating section, a heating section and a cooling section, and controls the temperature through a temperature measuring unit. When the material reaches the reaction temperature, a large amount of high-purity phosphorus vapor is generated. The phosphorus vapor at different temperature points can be evenly discharged to an external phosphorus collection device through the phosphorus discharge ports set in the preheating section and the cooling section as needed. Among them, the temperature measuring unit in the heating section has a pressure monitoring and control system that can better control the pressure in the furnace. Such a setting makes the phosphorus vapor recovery efficiency in the furnace higher;
[0024] The setting of the cooling section enables the heat brought out of the heating section by the material to be effectively recovered, thereby achieving the effect of drying the material;
[0025] During the entire preparation process, the materials are in a static state, the phosphorus vapor in the reaction process is of high purity, free of smoke and impurities, safe and environmentally friendly, and with low operating costs;
[0026] The automation level is high, and the whole process of trolley driving, temperature and pressure control can be automatically controlled by the computer in the central control room. BRIEF DESCRIPTION OF THE DRAWINGS
[0027] Figure 1 This is a schematic diagram of the overall structure of a kiln according to an embodiment of the present invention;
[0028] Figure 2 It is a schematic diagram of the cross-sectional structure of the preheating section of the kiln in an embodiment of the present invention;
[0029] Figure 3 This is a schematic diagram of the cross-sectional structure of the heating section of the kiln in an embodiment of the present invention;
[0030] Figure 4 It is a schematic diagram of the cross-sectional structure of the cooling section of the kiln in an embodiment of the present invention;
[0031] The reference numerals in the drawings of the specification include:
[0032] Kiln body 1, preheating section 10, heating section 11, refractory material 110, cooling section 12, track 2, phosphorus discharge port 3, temperature measuring unit 4, first connecting pipe 50, second connecting pipe 51, third connecting pipe 52, valve 53, isolation plate 60, sealing plate 61, blasting equipment 7, trolley 8. DETAILED DESCRIPTION
[0033] In order to enable those skilled in the art to better understand the present invention, the technical solution of the present invention is further described below in conjunction with the accompanying drawings and embodiments.
[0034] Among them, the drawings are only used for illustrative purposes, and they only show schematic diagrams rather than actual drawings, and cannot be understood as limitations on this patent; in order to better illustrate the embodiments of the present invention, some parts of the drawings may be omitted, enlarged or reduced, and do not represent the size of the actual product; for those skilled in the art, it is understandable that some well-known structures and their descriptions in the drawings may be omitted, and the same or similar reference numerals in the drawings of the embodiments of the present invention correspond to the same or similar parts; in the description of the present invention, it should be understood that if the terms "upper", "lower", "left", "right", "inner", "outer" and the like appear, the directions or positional relationships indicated are based on the directions or positional relationships shown in the drawings, which are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific direction, be constructed and operated in a specific direction, so the terms describing the positional relationship in the drawings are only used for illustrative purposes, and cannot be understood as limitations on this patent. For those of ordinary skill in the art, the specific meanings of the above terms can be understood according to specific circumstances.
[0035] like Figure 1 - Figure 4 As shown, a kiln for extracting phosphorus vapor from phosphate ore of the present invention comprises a kiln body 1, a temperature measuring unit 4 and an air cooling pipe;
[0036] The kiln body 1 is provided with a preheating section 10, a heating section 11 and a cooling section 12 in sequence along the length direction.
[0037] Tracks 2 are symmetrically arranged in the kiln body 1, and the tracks 2 extend along the length direction of the kiln body 1;
[0038] At least one of the preheating section 10 and the cooling section 12 is provided with a phosphorus discharge port 3, and the phosphorus discharge port 3 is connected to an external phosphorus vapor collection device;
[0039] The temperature measuring unit 4 is arranged on the inner wall of the kiln body 1 and acts on the material. Specifically, the temperature measuring unit 4 is arranged on the inner wall of the heating section 11. The temperature measuring unit 4 includes multiple sets of thermocouples and pressure measuring elements, and collects and outputs data signals to an external control room through sensors. The heating at the heating section 11 can be heated by microwave heating.
[0040] The kiln body 1 is provided with an air cooling pipe for guiding the hot air in the cooling section 12 to the external drying chamber.
[0041] The present invention divides the kiln body 1 into a preheating section 10, a heating section 11 and a cooling section 12. When the material reaches the reaction temperature, a large amount of high-purity phosphorus vapor is generated. The phosphorus vapor at different temperature points can be uniformly discharged to an external phosphorus collection device through the phosphorus discharge port 3 arranged in the preheating section 10 and the cooling section 12 as needed. Among them, the temperature measuring unit 4 of the heating section 11 has a pressure monitoring and control system, which can also better control the pressure in the furnace. Such a setting makes the phosphorus vapor recovery efficiency in the furnace higher.
[0042] During the entire preparation process, the materials are in a static state, the phosphorus vapor in the reaction process is of high purity, free of smoke and impurities, safe and environmentally friendly, and has low operating costs.
[0043] The automation level is high, and the whole process of trolley 8 driving, temperature and pressure control can be automatically controlled by the computer in the central control room.
[0044] The above-mentioned automatic control can use existing technology and is easy to implement. It does not belong to the protection scope of this application. Therefore, it at least has the beneficial effects brought by the technical solutions of the above-mentioned embodiments and will not be repeated here.
[0045] Specifically, the air cooling pipe includes a first connecting pipe 50 that passes through the top of the cooling section 12. Both ends of the first connecting pipe 50 are respectively connected to the second connecting pipe 51 and the third connecting pipe 52, and the three form a U-shaped structure.
[0046] The end of the second connecting pipe 51 is connected to the blowing device 7, and the end of the third connecting pipe 52 is connected to the external drying chamber.
[0047] The second connecting pipe 51 is also provided with a valve 53 , specifically a butterfly valve.
[0048] The arrangement of the cooling section 12 enables the heat brought out of the heating section 11 by the material to be effectively recovered, thereby achieving the effect of drying the material.
[0049] In this embodiment, multiple groups of phosphorus discharge ports 3 are provided in the preheating section 10 and the cooling section 12 .
[0050] In addition, isolation plates 60 are installed at the top and bottom of the kiln body 1 , a sealing plate 61 is installed at the periphery of the kiln body 1 , and the rail 2 is installed on the isolation plate 60 and passes through the entire kiln body 1 together with the sealing plate 61 .
[0051] The heating section 11 is provided with a refractory material 110. The special refractory material 110 used in conjunction with the heating section 11 not only has a good heat preservation effect, but also has good microwave penetration, so that the material is heated more quickly.
[0052] The top and side walls of the external sealing plate 61 of the heating section 11 are filled with microwave refractory materials 110 , and the external microwave equipment is connected to the top of the external sealing plate 61 .
[0053] When the kiln is in use, firstly, the trolley 8 loaded with materials is connected to the track 2 of the kiln body 1 from the external drying chamber through the return line, and the trolley 8 is sent to the inside of the kiln body 1 by a hydraulic stepper, and then the blast device 7 is turned on, and the trolley 8 passes through the preheating section 10, the heating section 11 and the cooling section 12 of the kiln body 1 in sequence. When the trolley 8 with materials travels to the heating section 11, the phosphorus vapor collection device is started, and the phosphorus vapor generated by the reaction is collected through different phosphorus discharge ports 3 according to product requirements;
[0054] During the reaction process in the heating section 11, the temperature and pressure of the kiln body 1 are read in real time through thermocouples and pressure measuring elements, and the temperature is controlled not to exceed 1200° C. and the pressure is slightly positive through an external control room.
[0055] Then, the external air blowing device 7 is started. After the trolley 8 enters the cooling section 12, the heat taken out of the trolley 8 from the heating section 11 is transported to the drying chamber through the first connecting pipe 50 and the third connecting pipe 52 through the air cooling pipe for material drying.
[0056] The above are only embodiments of the present invention. The common sense such as the known specific structures and characteristics in the scheme is not described in detail here. The ordinary technicians in the relevant field are aware of all the common technical knowledge in the technical field to which the invention belongs before the application date or priority date, can obtain all the existing technologies in the field, and have the ability to apply the conventional experimental means before that date. The ordinary technicians in the relevant field can improve and implement the scheme in combination with their own abilities under the enlightenment given by this application. Some typical known structures or known methods should not become obstacles for the ordinary technicians in the relevant field to implement this application. It should be pointed out that for the technicians in this field, without departing from the structure of the present invention, several deformations and improvements can be made, which should also be regarded as the protection scope of the present invention, and these will not affect the effect of the implementation of the present invention and the practicality of the patent.
Claims
1. A kiln for extracting phosphorus vapor from phosphate ore, characterized in that: include: The kiln body has a preheating section, a heating section and a cooling section arranged in sequence along the length direction; Tracks are symmetrically arranged in the kiln body and extend along the length direction of the kiln body; At least one of the preheating section and the cooling section is provided with a phosphorus discharge port, and the phosphorus discharge port is connected to an external phosphorus vapor collection device; The temperature measuring unit is arranged on the inner wall of the kiln body and acts on the material.
2. A kiln for extracting phosphorus vapor from phosphate ore as claimed in claim 1, characterized in that: The kiln body is provided with an air cooling pipe for guiding the hot air in the cooling section to the external drying chamber.
3. A kiln for extracting phosphorus vapor from phosphate ore as claimed in claim 2, characterized in that: The air cooling pipe includes a first connecting pipe that runs through the top of the cooling section. Both ends of the first connecting pipe are respectively connected to the second connecting pipe and the third connecting pipe, and the three form a U-shaped structure.
4. A kiln for extracting phosphorus vapor from phosphate ore as claimed in claim 3, characterized in that: The end of the second connecting pipe is connected to a blowing device, and the end of the third connecting pipe is communicated with an external drying chamber.
5. A kiln for extracting phosphorus vapor from phosphate ore as claimed in claim 1, 2, 3 or 4, characterized in that: A plurality of groups of phosphorus discharge ports are arranged in the preheating section and the cooling section.
6. A kiln for extracting phosphorus vapor from phosphate ore as claimed in claim 1, 2, 3 or 4, characterized in that: The top and bottom of the kiln body are provided with isolation plates, and the periphery of the kiln body is provided with sealing plates.
7. A kiln for extracting phosphorus vapor from phosphate ore as claimed in claim 6, characterized in that: The rail is installed on the isolation plate, and the rail runs through the entire kiln body.
8. A kiln for extracting phosphorus vapor from phosphate ore as claimed in claim 1, 2, 3, 4 or 7, characterized in that: The heating section area is provided with refractory material.
9. A kiln for extracting phosphorus vapor from phosphate ore as claimed in claim 8, characterized in that: The temperature measuring unit is arranged in the heating section.
10. A kiln for extracting phosphorus vapor from phosphate ore as claimed in claim 9, characterized in that: The temperature measuring unit includes a thermocouple and a pressure measuring element.