Method for testing combustion wave of solid propellant
By using minimally invasive pre-embedding and coating liquid treatment of thermocouple wire in solid propellant combustion wave test, the problems of test data fluctuations and propellant string fire are solved, and more stable temperature measurement results are achieved.
Patent Information
- Application Number
- CN202411022165.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-29
- Publication Date
- 2024-11-12
AI Technical Summary
The existing solid propellant combustion wave testing methods cannot guarantee the stability of temperature measurement, and the thermocouple temperature measuring head is easily affected by the flow of combustion flames, and the pre-embedding of the thermocouple on the section will cause damage to the propellant structure and strings. fire.
The thermocouple wire is used to insert it into the needle tube. The needle tube is inserted into the inside of the cut propellant strip. After removal, the thermocouple wire is retained. The surface and the cut joints are coated with a coating solution. The airflow disturbance and fire are avoided through minimally invasive embedding. .
It effectively stabilizes the thermocouple test data, avoids the propellant ignition during combustion, and improves the accuracy and reliability of temperature measurement.
Smart Images

Figure CN118936655A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of solid propellant combustion wave testing, and in particular to a solid propellant combustion wave testing method. Background Art
[0002] The solid propellant combustion wave is used to describe the temperature distribution of the flame during the combustion process of the solid propellant. As one of the important parameters for characterizing the energy performance of solid propellants, it is also a core parameter for studying the combustion mechanism of solid propellants. However, there are still many problems with the solid propellant combustion wave test. The accuracy of the propellant temperature distribution test cannot be guaranteed, which makes it impossible to verify the solid propellant combustion physical model and makes the understanding of the solid propellant combustion mechanism unclear. At present, the solid propellant temperature measurement methods are mainly divided into non-contact temperature measurement and contact temperature measurement.
[0003] Non-contact temperature measurement methods mainly include: radiation thermometer method, infrared thermal imaging method, spectroscopy method, laser scattering method. However, non-contact temperature measurement is greatly affected by the external environment, such as reflectivity, emissivity, ambient temperature, etc. The complexity and high cost of the equipment are also its disadvantages, and it is not easy to obtain accurate measurement results.
[0004] Contact temperature measurement mainly includes thermocouple method and thermistor method. The advantages of contact type are good stability and reliability, as well as real-time and reliability. For the thermocouple method, there are still the following disadvantages: First, the test results fluctuate greatly. Under high pressure, the thermocouple temperature measuring head swings due to the influence of the combustion flame flow during the combustion of the propellant, resulting in large fluctuations in the test results; second, the method of pre-embedded thermocouples in the cut surface causes damage to the propellant body structure. Due to the large area of the cut surface and the cut seam, the high temperature during the combustion process will cause cross-fire at the cut surface and the cut seam, resulting in increased thermocouple test errors or even test failures. Third, the current high-energy propellant cannot be bonded with the cut surface using acetone solution.
[0005] Therefore, there is an urgent need to improve the test method of solid propellant combustion waves, not only to ensure the stability of temperature measurement, but also to solve the problem of propellant cross-fire during the test.
[0006] In view of this, the present invention is proposed. Summary of the invention
[0007] The object of the present invention is to provide a method for testing the combustion wave of a solid propellant, aiming to ensure the stability of temperature measurement and avoid the problem of cross-fire of the propellant.
[0008] The present invention is achieved in that:
[0009] In a first aspect, the present invention provides a method for testing a solid propellant combustion wave, comprising: inserting a thermocouple wire into a needle tube, cutting a propellant strip, and inserting the needle tube with the thermocouple wire into the interior of the cut propellant strip;
[0010] Remove the needle tube, leaving only the thermocouple wire inside the propellant strip, apply the coating liquid to the cut surface and the cut seam, and dry;
[0011] Thermocouple wires are used to detect the temperature of the propellant rod during combustion.
[0012] In an optional embodiment, the coating liquid contains polyvinyl butyral and a solvent, the mass fraction of polyvinyl butyral is 7%-10%, and the drying temperature is 30° C.-40° C.;
[0013] More preferably, the solvent is anhydrous ethanol.
[0014] In an optional embodiment, the embedded depth of the thermocouple wire is 2 mm-6 mm, preferably 3 mm-5 mm.
[0015] In an optional embodiment, the propellant strip has a length direction, and the propellant strip is cut along the length direction from one end of the length direction;
[0016] Preferably, when cutting, the cutting surface is controlled to be parallel to the side surface.
[0017] In an optional embodiment, the thermocouple wire includes a first thermocouple wire as a positive electrode and a second thermocouple wire as a negative electrode, and the preparation process of the thermocouple wire includes: welding the ends of the first thermocouple wire and the second thermocouple wire, controlling the welding size to be 0.05 mm-0.08 mm, and the diameter of the needle tube to be 0.1 mm-0.2 mm;
[0018] Preferably, the first thermocouple wire and the second thermocouple wire are both tungsten-rhenium alloy wires, the mass fraction of rhenium in the first thermocouple wire is 3%, and the mass fraction of rhenium in the second thermocouple wire is 25%.
[0019] In an optional embodiment, the first thermocouple wire and the second thermocouple wire each have a welding end and a mounting end opposite to the welding end, and the mounting ends of the first thermocouple wire and the second thermocouple wire are moved away from each other to form a cross; the welding ends of the first thermocouple wire and the second thermocouple wire are welded.
[0020] In an optional embodiment, the length of the first thermocouple wire and the second thermocouple wire are both 15cm-20cm, and the first thermocouple wire and the second thermocouple wire are reinforced near the welding end by winding the first thermocouple wire and the second thermocouple wire, with a winding length of 3mm-7mm, and welding is performed after winding is completed.
[0021] In an optional embodiment, the preparation process of the thermocouple wire further includes: after the first thermocouple wire and the second thermocouple wire are welded, rolling is performed so that the diameter of the winding part is less than 0.1 mm.
[0022] In an optional embodiment, after the thermocouple wires are pre-embedded in the propellant strip, the mounting ends of the first thermocouple wire and the second thermocouple wire are extended from the end surface of the propellant strip and are respectively wound around the test signal input end of the test bracket, with the first thermocouple wire as the positive electrode and the second thermocouple wire as the negative electrode.
[0023] In an optional embodiment, the method further comprises: after fixing the medicine strip sample with the thermocouple wire inside, inserting an ignition wire into the medicine strip sample;
[0024] Preferably, the ignition wire is a nickel-chromium alloy ignition wire.
[0025] The present invention has the following beneficial effects: the present invention inserts the thermocouple wire into the needle tube, and inserts it into the cut propellant strip. After the needle tube is removed, only the thermocouple wire can be retained inside the propellant strip, and the cut surface and the cut seam are coated with a coating liquid. The present invention adopts a pinhole "minimally invasive" thermocouple pre-embedding method, which can effectively solve the problem of fluctuations in the thermocouple test due to airflow disturbance during the combustion wave test, ensure the validity of the thermocouple test data, and solve the problem of easy cross-fire of the propellant in the case of a single cut seam. BRIEF DESCRIPTION OF THE DRAWINGS
[0026] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the drawings required for use in the embodiments are briefly introduced below. It should be understood that the following drawings only show certain embodiments of the present invention and therefore should not be regarded as limiting the scope. For ordinary technicians in this field, other related drawings can be obtained based on these drawings without creative work.
[0027] Figure 1 Schematic diagram of winding and welding of thermocouple wires provided in an embodiment of the present invention; (a) is a schematic diagram of welding after winding; (b) is a schematic diagram of testing the firmness of welding;
[0028] Figure 2 Schematic diagram of cutting the propellant strip and embedding the thermocouple wire inside;
[0029] Figure 3 It is the combustion wave curve of composite solid propellant during combustion;
[0030] Figure 4 It is the combustion wave curve of double-base solid propellant during combustion;
[0031] Figure 5 is the combustion wave curve of the propellant in comparative example 1 during combustion;
[0032] Figure 6 is the combustion wave curve of the propellant in comparative example 2 during combustion;
[0033] Figure 7 This is the combustion wave curve of the propellant in comparative example 3 during combustion.
[0034] Icon: 1-propellant stick; 2-thermocouple. DETAILED DESCRIPTION
[0035] In order to make the purpose, technical scheme and advantages of the embodiments of the present invention clearer, the technical scheme in the embodiments of the present invention will be described clearly and completely below. If the specific conditions are not specified in the embodiments, they are carried out according to conventional conditions or conditions recommended by the manufacturer. If the manufacturer of the reagents or instruments used is not specified, they are all conventional products that can be purchased commercially.
[0036] An embodiment of the present invention provides a method for testing a solid propellant combustion wave, comprising the following steps:
[0037] S1. Preparation of thermocouple wire
[0038] like Figure 1 As shown, the thermocouple wire includes a first thermocouple wire as a positive electrode and a second thermocouple wire as a negative electrode. The preparation process of the thermocouple wire includes: welding the ends of the first thermocouple wire and the second thermocouple wire, and controlling the welding size to be 0.05mm-0.08mm, such as 0.05mm, 0.06mm, 0.07mm, 0.08mm, etc.
[0039] That is to say, Figure 1 The diameter of the welding head at the top of (a) is 0.05mm-0.08mm, which needs to be smaller than the inner diameter of the needle tube.
[0040] In actual operation, use the welding tongs to clamp the Wre-3 wire and Wre-25 wire to the welding head of the welding machine. Adjust the positions of the two thermocouple wires so that the two wires can cross at one point, and control the angle of the two wires to about 45°. Turn on the welding machine power, adjust the transformer to about 10V, turn on the argon gas purge system immediately before welding, and use the welding tongs to quickly tap the intersection on the welding head to weld the tungsten-rhenium wires together. After welding, gently pull them hard. If they can be pulled apart, cut off the welding point and weld again until they can be pulled together. Figure 1 After welding, the soldering is completed until the shape is obtained as in (b). Then, the soldering is completed and stored in a plexiglass box.
[0041] In some embodiments, the first thermocouple wire and the second thermocouple wire are both tungsten-rhenium alloy wires, the mass fraction of rhenium in the first thermocouple wire is 3% (i.e., W / Re is 97 / 3, also known as Wre-3 wire), and the mass fraction of rhenium in the second thermocouple wire is 25% (i.e., W / Re is 75 / 25, also known as Wre-25 wire). Both Wre-3 wire and Wre-25 wire are commercially available materials.
[0042] In some embodiments, Figure 1 As shown, the first thermocouple wire and the second thermocouple wire each have a welding end and a mounting end opposite to the welding end. The mounting ends of the first thermocouple wire and the second thermocouple wire are separated from each other to form a cross, and the cross angle can be about 45°. The mounting end is used to connect the test signal input end of the detection bracket. The welding ends of a thermocouple wire and a second thermocouple wire are welded. After the thermocouple wire is pre-embedded in the propellant strip, the mounting ends of the first thermocouple wire and the second thermocouple wire extend out of the end surface, which is used to connect the test signal input end of the test bracket to form a complete thermocouple temperature measurement structure.
[0043] Further, the length of the first thermocouple wire and the second thermocouple wire are both 15cm-20cm, which are obtained by cutting a whole roll of tungsten-rhenium wire that has been uniformly stripped in advance, and the length can be 15cm, 16cm, 17cm, 18cm, 19cm, 20cm, etc. The first thermocouple wire and the second thermocouple wire are reinforced by winding near the welding end, and the winding length is 3mm-7mm (such as 3mm, 4mm, 5mm, 6mm, 7mm, etc.), and welding is performed after the winding is completed.
[0044] It should be noted that if the test sample burns more violently and the thermocouple fluctuates during the test, it can be reinforced by winding. That is, before welding, the tungsten-rhenium thermocouples are wound around each other at a distance of about 3mm-7mm from the welding point, with a winding length of 3mm-7mm, to increase its firmness.
[0045] Furthermore, the preparation process of the thermocouple wire also includes: after the first thermocouple wire and the second thermocouple wire are welded, calendering is performed so that the diameter of the winding part is less than 0.1 mm, and the damage to the propellant strip is reduced by reducing the diameter of the winding part. In the actual operation process, after the thermocouple is welded, the welded thermocouple needs to be calendered, and the gap of the calender is adjusted to 0.1 mm. In order to see the pressed wire clearly, a piece of white paper can be placed under the roller. Gently feed the end with the weld point into the calender, push forward with your left hand, and turn the handle evenly in the counterclockwise direction with your right hand, press about 10 mm, and then withdraw the wire in the opposite direction and let it fall on the white paper.
[0046] S2, Minimally Invasive Pre-embedded
[0047] like Figure 2 As shown, the thermocouple wire is inserted into the needle tube, the propellant strip is cut, and the needle tube with the thermocouple wire is inserted into the cut propellant strip; the needle tube is removed, and only the thermocouple wire is left inside the propellant strip. This "minimally invasive" thermocouple pre-embedding method can ensure that the thermocouple does not swing during the test process, and the propellant will not ignite in the test area.
[0048] In some embodiments, the embedded depth of the thermocouple wire is 2 mm-6 mm, such as 2 mm, 3 mm, 4 mm, 5 mm, 6 mm, etc., preferably 3 mm-5 mm. The embedded depth refers to the distance that continues to go deeper on the basis of the incision surface.
[0049] Furthermore, the diameter of the needle tube is 0.1mm-0.2mm, such as 0.10mm, 0.15mm, 0.20mm, etc. The diameter of the needle tube is preferably within the above range. If the diameter is too small, the thermocouple wire cannot be inserted, and if the diameter is too large, the damage to the propellant strip will increase.
[0050] In some embodiments, Figure 2 As shown, the propellant strip has a length direction, and the propellant strip is cut along the length direction from one end of the length direction, and the cut surface can be controlled to be parallel to the side surface during cutting. Then, the needle tube with the thermocouple wire is inserted vertically into the previously cut propellant strip 1 along the center of the cut surface, and the thermocouple insertion depth is ensured to be 4-5mm. The two sides of the propellant strip 1 without the cut seam are clamped with the thumb and index finger of the left hand, and the needle tube is pulled out with the right hand, leaving only the rolled thermocouple 2 pre-buried in the propellant strip 1.
[0051] S3, coating liquid
[0052] After taking out the needle tube, apply the coating liquid to the cut surface and the cut seam and dry it. By introducing the coating liquid, it can play a flame retardant role to a certain extent and solve the problem of propellant fire during the combustion wave test.
[0053] In some embodiments, the coating liquid contains polyvinyl butyral and a solvent, and the mass fraction of polyvinyl butyral is 1%-3%, such as 1%, 2%, 3%, etc. The drying temperature is 30°C-40°C, such as 30°C, 35°C, 40°C, etc. It is preferable to control the coating temperature within the above range to form a uniform coating.
[0054] Furthermore, the solvent is anhydrous ethanol.
[0055] S4. Assembly inspection
[0056] An ignition wire is inserted into the propellant strip sample with thermocouple wires, and the first thermocouple wire and the second thermocouple wire are wound and connected to the test signal input end of the test bracket, and then the thermocouple wires can be used to detect the temperature of the propellant strip during combustion.
[0057] In some embodiments, a medicine strip sample with a thermocouple wire inside is fixed on a test stand, and an ignition wire is inserted parallel to the upper end surface of the medicine strip sample at a distance of about 3 mm, so that the ignition wire is in the middle of the surface. In other words, Figure 1 In the process, the thermocouple wire is inserted from one end in the length direction, and the ignition wire is inserted from the other end in the length direction. During the combustion process, the combustion starts from the ignition wire and gradually burns to the other end of the medicine strip sample. The ignition wire can be a nickel-chromium alloy ignition wire, but is not limited thereto.
[0058] In some embodiments, after the thermocouple wires are pre-buried in the propellant strip, the installation ends of the first thermocouple wire and the second thermocouple wire are extended from the end surface of the propellant strip and are respectively wound around the test signal input end of the test bracket, with the first thermocouple wire Wre-3 wire as the positive electrode and the second thermocouple wire Wre-25 wire as the negative electrode. The welded thermocouple wires are tested with the positive and negative poles of a multimeter to ensure that they are connected.
[0059] Specifically, the test signal input end of the test bracket has a positive input end and a negative input end. The test bracket is used to fix the sample to be tested, and is the other part of the thermocouple temperature detection device except the thermocouple wire. It is a commercially available device.
[0060] The features and performance of the present invention are further described in detail below in conjunction with the embodiments.
[0061] It should be noted that (1) the first thermocouple wire Wre-3 and the second thermocouple wire Wre-25 used in the following examples and comparative examples are commercially available materials with a length of 20 cm. (2) The shape of the propellant strip is a rectangular parallelepiped, with a length, width and height of 30 mm, 5 mm and 5 mm respectively. (3) The needle tube is made of stainless steel, with an inner diameter of 0.1 mm and a thickness of 0.01 mm. (4) The coating liquid is a mixture of polyvinyl butyral and anhydrous ethanol, and the mass ratio of polyvinyl butyral to anhydrous ethanol is 8:92.
[0062] Example 1
[0063] This embodiment provides a method for testing the combustion wave of a solid propellant, and this embodiment performs combustion wave tests on a composite solid propellant at different pressures. The raw material of the composite solid propellant is in powder form and is purchased from the Hubei Aerospace Chemical Technology Research Institute. The propellant pellets 1 are obtained by pressing and molding using a propellant mold.
[0064] The test method includes the following steps:
[0065] (1) Figure 1 As shown, the Wre-3 wire and the Wre-25 wire are reinforced by winding, that is, before welding, the tungsten-rhenium thermocouples are wound around each other at a distance of about 5mm from the welding point, and the winding length is 5mm, so as to increase its firmness. The Wre-3 wire and the Wre-25 wire are clamped to the welding head of the welding machine using the welding tongs of the welding machine, and the positions of the two thermocouple wires are adjusted so that the two wires can cross at one point, and the angle between the two wires is controlled at about 45°. Turn on the welding machine power supply, adjust the transformer to about 10V, turn on the argon gas blowing system instantly before welding, and use the welding tongs to quickly touch the intersection on the welding head to weld the two tungsten-rhenium wires together. The welding size is 0.08mm and stored in a plexiglass box.
[0066] (2) Roll the welded thermocouple wire, adjust the gap of the rolling machine to 0.1mm, and place a piece of white paper under the roller. Gently put the end with the weld point into the rolling machine, push forward with your left hand, and turn the handle evenly in the counterclockwise direction with your right hand, press about 10mm, and then withdraw the wire in the opposite direction and let it fall on the white paper.
[0067] (3) Figure 2 As shown, the propellant strip 1 is completely cut from a position 10 mm away from one end in a direction parallel to the side (i.e., the cutting depth is 10 mm), the welded thermocouple 2 is inserted into the pre-prepared needle tube, and then the needle tube with the thermocouple is vertically inserted into the pre-cut propellant strip 1 along the center of the cut surface, ensuring that the thermocouple insertion depth is 4-5 mm, the left thumb and index finger are used to clamp the two sides of the propellant strip 1 without the cut seam, and the needle tube is pulled out with the right hand, leaving only the rolled thermocouple 2 pre-buried in the propellant strip 1. Then apply the coating liquid to the cut surface and the cut seam for 3 times, each time with an interval of 30 minutes, the coating thickness is 1-2 mm, and it is dried at 35°C for 1.5 hours.
[0068] (4) Fix the prepared medicine strip sample fixture on the test bracket, and insert the nickel-chromium alloy ignition wire parallel to the upper end of the sample at a distance of 3 mm, so that the ignition wire is in the center of the surface. Wrap the extended ends of the pre-embedded thermocouple wires in the sample around the test signal input end of the test bracket, with Wre-3 as the positive pole and Wre-25 wire as the negative pole. Use a multimeter to test the positive and negative poles of the welded thermocouple wires to ensure that they are connected.
[0069] (5) The solid propellant coated as required is loaded into the high-pressure combustion chamber, the ignition circuit is connected, the pressure and combustion wave acquisition system is connected, the ignition button is started, and the electromotive force change during the entire combustion process of the solid propellant is obtained. Then, the entire electromotive force curve data is calculated using the temperature-electromotive force fitting formula to obtain the combustion wave curve during the propellant combustion process.
[0070] The working conditions tested in this embodiment are shown in Table 1, and the combustion wave curve is shown in Figure 3 .
[0071] Table 1 Test conditions of Example 1
[0072] Test conditions Propellant type pressure Working condition 1 Composite propellant 7MPa Working condition 2 Composite propellant 10MPa
[0073] The two working conditions only differ in pressure. The test pressure of working condition 1 is 7MPa, and the test pressure of working condition 2 is 10MPa. It can be seen from the combustion wave curve that the higher the initial pressure of the propellant combustion, the higher the maximum temperature of the combustion wave curve and the higher the temperature rise rate during the combustion process. There was no data fluctuation during the entire data collection process, which is in line with the combustion law of composite propellants.
[0074] Example 2
[0075] This embodiment provides a method for testing the combustion wave of a solid propellant, and this embodiment performs a combustion wave test on a double-base solid propellant at different pressures. The raw material of the double-base solid propellant is in powder form and is purchased from the Hubei Aerospace Chemical Technology Research Institute. The propellant pellets 1 are obtained by pressing and molding using a propellant mold.
[0076] The test method is shown in steps (1)-(5) of Example 1.
[0077] The test conditions are shown in Table 2, and the combustion wave curve is shown in Figure 4 .
[0078] Table 2 Test conditions of Example 2
[0079] Test conditions Propellant type pressure Working condition 1 Double base propellant 7MPa Working condition 2 Double base propellant 10MPa
[0080] The two working conditions only differ in pressure. The test pressure of working condition 1 is 7MPa, and the test pressure of working condition 2 is 10MPa. It can be found that the combustion wave curve has not fluctuated, indicating that the test environment is stable and no crossfire occurs. The maximum combustion temperature and temperature change gradient increase with increasing pressure, which is consistent with the combustion law of double-base propellant.
[0081] Comparative Example 1
[0082] This comparative example provides an existing test method for solid propellant combustion wave, which is as follows:
[0083] Cut one end of the propellant to be tested, bury the thermocouple directly in the middle of the propellant cut surface, repeatedly apply the coating liquid to the outer cut seam three times, dry it, and conduct the solid propellant combustion wave test.
[0084] The type and conditions of the solid propellant tested are the same as those in Example 1. The test results are as follows: Figure 5It can be seen that the data curve has a temperature fluctuation section during the heating process. This is because the thermocouple in the original test method fails to be fixed during the test, causing the thermocouple to swing and the test area to change, resulting in test errors.
[0085] Comparative Example 2
[0086] The only difference from Example 1 is that the coating liquid coating position is different, as follows:
[0087] Apply the coating liquid prepared in advance according to the proportion only to the outer cut of the propellant.
[0088] The type and conditions of the solid propellant tested are the same as those in Example 1. The test results are as follows: Figure 6 It can be seen that the temperature curve has an obvious descending section in the rising process, and then rises. This is because the slit coating method used in the original test method has a poor flame retardant effect, causing the burning section of the embedded thermocouple to start burning, destroying the parallel layer combustion required by the test, resulting in test errors.
[0089] Comparative Example 3
[0090] The only difference from Example 1 is that the thermocouple pre-embedding method is different.
[0091] The type and conditions of the solid propellant tested are the same as those in Example 1. The test results are as follows: Figure 7 , it can be seen that a series of fire occurred during the process.
[0092] The above are only preferred embodiments of the present invention and are not intended to limit the present invention. For those skilled in the art, the present invention may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.
Claims
1. A method for testing solid propellant combustion waves. It is characterized in that include: Inserting the thermocouple wire into the needle tube, cutting the propellant strip, and inserting the needle tube with the thermocouple wire into the interior of the cut propellant strip; The needle tube is removed, and only the thermocouple wire is retained inside the propellant strip, and the coating liquid is applied to the cut surface and the cut seam, and dried; The thermocouple wire is used to detect the temperature of the propellant rod during its combustion.
2. The test method according to claim 1, It is characterized in that The coating liquid contains polyvinyl butyral and a solvent, the mass fraction of polyvinyl butyral is 7%-10%, and the drying temperature is 30°C-40°C; More preferably, the solvent is anhydrous ethanol.
3. The testing method according to claim 1, It is characterized in that The embedded depth of the thermocouple wire is 2 mm to 6 mm, preferably 3 mm to 5 mm.
4. The test method according to any one of claims 1 to 3, It is characterized in that The propellant strip has a length direction, and the propellant strip is cut along the length direction from one end of the length direction; Preferably, when cutting, the cutting surface is controlled to be parallel to the side surface.
5. The testing method according to claim 1, It is characterized in that The thermocouple wire includes a first thermocouple wire as a positive electrode and a second thermocouple wire as a negative electrode. The preparation process of the thermocouple wire includes: welding the ends of the first thermocouple wire and the second thermocouple wire, controlling the welding size to be 0.05 mm-0.08 mm, and the diameter of the needle tube to be 0.1 mm-0.2 mm; Preferably, both the first thermocouple wire and the second thermocouple wire are tungsten-rhenium alloy wires, the mass fraction of rhenium in the first thermocouple wire is 3%, and the mass fraction of rhenium in the second thermocouple wire is 25%.
6. The test method according to claim 5, It is characterized in that The first thermocouple wire and the second thermocouple wire each have a welding end and a mounting end opposite to the welding end. The mounting ends of the first thermocouple wire and the second thermocouple wire are separated from each other to form a cross; and the welding ends of the first thermocouple wire and the second thermocouple wire are welded.
7. The testing method according to claim 6, It is characterized in that The lengths of the first thermocouple wire and the second thermocouple wire are both 15cm-20cm. The first thermocouple wire and the second thermocouple wire are reinforced near the welding end by winding them, with a winding length of 3mm-7mm. Welding is performed after winding is completed.
8. The test method according to claim 7, It is characterized in that The preparation process of the thermocouple wire further includes: after the first thermocouple wire and the second thermocouple wire are welded, rolling is performed so that the diameter of the winding part is less than 0.1 mm.
9. The test method according to any one of claims 6 to 8, It is characterized in that After the thermocouple wire is pre-buried in the propellant strip, the installation ends of the first thermocouple wire and the second thermocouple wire are extended from the end surface of the propellant strip and are respectively wound around the test signal input end of the test bracket, with the first thermocouple wire as the positive electrode and the second thermocouple wire as the negative electrode.
10. The test method according to any one of claims 5 to 8, It is characterized in that Also includes: After fixing the medicine strip sample with the thermocouple wire inside, inserting an ignition wire into the medicine strip sample; Preferably, the ignition wire is a nickel-chromium alloy ignition wire.