Concrete filled steel tube void detection and operation method based on collision characteristic change
Through the detection method based on the change of collision characteristics, the contact time and impedance change characteristics are used to solve the problems of low air-removing detection efficiency and insufficient accuracy of steel pipe concrete in the prior art, and efficient and accurate detection results are achieved, in order to improve the steel pipe concrete The construction quality of the structure provides important inspection methods.
Patent Information
- Application Number
- CN202411020148.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-29
- Publication Date
- 2024-11-12
AI Technical Summary
The existing steel pipe concrete decanting detection method has low detection efficiency in high-altitude scenarios, and the accuracy of the calculation of the decanting index of the measurement point decanting index is questionable, resulting in uncertainty in the detection results.
The detection method based on the change of collision characteristics is adopted, and the steel pipe surface is hit by a tool, and the signal is transmitted to the signal equipment for analysis. The contact time and impedance change characteristics are used to establish a de-empty judgment reference, providing a more applicable and accurate detection method.
It improves the convenience and accuracy of inspection, realizes fast and simple air-removing inspection of steel pipe concrete, and improves the reliability of construction quality evaluation.
Smart Images

Figure CN118937480A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of engineering quality detection, and in particular to a steel tube concrete void detection and operation method based on collision characteristic changes. Background Art
[0002] According to the specification "Technical Specification for Detecting Concrete Defects by Impact Elastic Wave Method" (T / CECS 925-2021), steel tube concrete void detection should be carried out by vibration method. Combined with relevant information, this method requires fixing the probe on the surface of the steel tube and hitting it next to the probe. By picking up the vibration parameters of the steel tube after hitting, the void condition of the steel tube can be determined. However, when the steel tube concrete is located at high altitude, the detection efficiency is low due to the need to frequently move the measuring point and the hitting position, and its operability is low. Therefore, it is necessary to develop a more efficient and convenient detection method. On the other hand, the void index Si of the measuring point in the specification is different from the expected value. The calculated value of the distance Li has little to do with the reference value, so the accuracy of the test result is questionable.
[0003] Therefore, there is an urgent need in this field for a method with greater applicability and higher accuracy.
[0004] The information disclosed in this background technology section is only intended to enhance the understanding of the overall background of the invention and should not be regarded as an acknowledgment or any form of suggestion that the information constitutes the prior art already known to a person skilled in the art. Summary of the invention
[0005] The purpose of the present invention is to provide a method with stronger applicability and higher accuracy.
[0006] To achieve the above object, the present invention provides the following solutions:
[0007] A method for detecting voids in concrete-filled steel tubes based on changes in collision characteristics, comprising:
[0008] Hitting the surface of an object with a tool;
[0009] The signal generated by the impact passes through the signal probe;
[0010] The signal is transmitted to the signal device through the signal transmission line;
[0011] Signal equipment receives test data for storage and analysis;
[0012] The data of the test waveform is analyzed by the analysis software to obtain the contact time of the test waveform;
[0013] The test signal contact time is normalized and the correction formula is:
[0014]
[0015] Wherein, T1 is the waveform starting time, T2 is the waveform recovery time, xi(t) represents the acceleration signal collected by the probe, and A represents the maximum voltage of the signal;
[0016] Test the compacted and voided areas separately and establish a benchmark for void determination;
[0017] Whether the steel pipe is hollow is determined based on the hollow determination criteria.
[0018] Optionally, the tool includes a spherical hammer head and a cylindrical tool.
[0019] Optionally, the signal probe is fixed inside the striking tool.
[0020] Optionally, the signal device is used to amplify, convert and send the signal.
[0021] Optionally, the criteria for determining the air escape include:
[0022] When Tc≥0.5Tc0+0.5Tc1, the measuring point exists and there is a serious gap in the part;
[0023] When 0.75Tc0+0.25Tc1≤Tc<0.5Tc0+0.5Tc1, there is a slight gap at the measuring point;
[0024] When Tc<0.75Tc0+0.25Tc1, the measuring points are densely located.
[0025] A method for detecting the voiding of concrete-filled steel tubes based on the change of collision characteristics, characterized by comprising determining the object to be detected and the detection position;
[0026] At the target position of the steel pipe, the measuring points are arranged at certain intervals;
[0027] Use a signal cable to connect the excitation tool and the detection host, turn on the host power, open the detection software and set the parameters.
[0028] The detection host collects and saves the test signal of the point, performs signal processing such as noise on the test signal, and analyzes and determines the characteristic parameters of the measuring point position;
[0029] The characteristic parameters obtained by analysis are corrected by introducing the maximum amplitude correction method;
[0030] Compare the corrected contact time at the detection position with the corrected contact time at the dense state or the empty state;
[0031] When the corrected contact time of the measuring point is greater than the corrected contact time of the dense state, there is a gap at this position;
[0032] Analyze and save the results;
[0033] The next position is tested.
[0034] Optionally, the characteristic parameter includes contact time.
[0035] Optionally, the collision-type steel tube concrete void detection device includes:
[0036] A vibration tool, a probe, a signal transmission line, a host, and a portable mobile detection host; the probe is located in the vibration tool, the probe is connected to the host via a transmission line, and the host is connected to the portable mobile detection host.
[0037] Compared with the prior art, the present invention has the following beneficial effects:
[0038] The present invention provides a steel tube concrete void detection and operation method based on collision characteristic changes, which solves the drawbacks of the existing method of separating striking and receiving (safety issues, low detection efficiency, etc.), and combines the changing characteristics of contact time and impedance change to provide a steel tube concrete void detection method based on collision characteristic changes; the present invention improves the convenience and stability of existing detection methods (vibration method, etc.), realizes fast, simple and accurate detection, and provides a detection system and detection method steps. The present invention provides a set of fast and accurate detection and evaluation means that are more suitable for engineering sites, and provides an important detection method for improving the construction quality of steel tube concrete structures. BRIEF DESCRIPTION OF THE DRAWINGS
[0039] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative labor.
[0040] Figure 1 A schematic diagram of a method for detecting voids in concrete-filled steel tubes based on changes in collision characteristics provided by an embodiment of the present invention.
[0041] Figure 2 A schematic diagram of a method for detecting a void in a concrete-filled steel tube based on changes in collision characteristics provided by an embodiment of the present invention.
[0042] Figure 3 A schematic diagram of a collision-type steel tube concrete void detection device provided in an embodiment of the present invention.
[0043] Figure 4 A schematic diagram of a detection rectangular coordinate system provided by an embodiment of the present invention.
[0044] Figure 5 A schematic diagram of the detection method flow provided by an embodiment of the present invention.
[0045] Figure 6 A schematic diagram of the appearance of a steel pipe column under test provided in an embodiment of the present invention.
[0046] Figure 7 A schematic diagram of a test waveform of an empty state provided by an embodiment of the present invention.
[0047] Figure 8 A schematic diagram of a test waveform of a dense state provided by an embodiment of the present invention.
[0048] Fig. 9 A schematic diagram of the analysis results of the dense part and the hollow part provided in an embodiment of the present invention.
[0049] Fig.10 This is a diagram of the measurement point arrangement provided in an embodiment of the present invention.
[0050] Fig.11 A schematic diagram of the detection and determination results provided by an embodiment of the present invention. DETAILED DESCRIPTION
[0051] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0052] The purpose of the present invention is to provide a method with stronger applicability and higher accuracy.
[0053] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and easy to understand, the present invention is further described in detail below with reference to the accompanying drawings and specific embodiments.
[0054] Embodiment 1:
[0055] This embodiment provides a method for detecting the voids in concrete-filled steel tubes based on collision characteristics. Figure 1 As shown, including:
[0056] Hitting the surface of an object with a tool;
[0057] The signal generated by the impact passes through the signal probe;
[0058] The signal is transmitted to the signal device through the signal transmission line;
[0059] Signal equipment receives test data for storage and analysis;
[0060] The data of the test waveform is analyzed by the analysis software to obtain the contact time of the test waveform;
[0061] The test signal contact time is normalized and the correction formula is:
[0062]
[0063] Among them, T1 is the waveform start time, T2 is the waveform recovery time, x i (t) represents the acceleration signal collected by the probe, and A represents the maximum voltage of the signal;
[0064] Test the compacted and voided areas separately and establish a benchmark for void determination;
[0065] Whether the steel pipe is hollow is determined based on the hollow determination criteria.
[0066] Furthermore, the tool includes a spherical hammer head and a cylindrical tool.
[0067] Furthermore, the signal probe is fixed inside the striking tool.
[0068] Furthermore, the signal device is used to amplify, convert and send the signal.
[0069] Furthermore, the criteria for determining the air escape include:
[0070] When Tc≥0.5Tc0+0.5Tc1, the measuring point exists and there is a serious gap in the part;
[0071] When 0.75Tc0+0.25Tc1≤Tc<0.5Tc0+0.5Tc1, there is a slight gap at the measuring point;
[0072] When Tc<0.75Tc0+0.25Tc1, the measuring points are densely located.
[0073] Embodiment 2:
[0074] This embodiment provides a method for detecting the void of concrete-filled steel tubes based on the change of collision characteristics. Figure 2 As shown, including:
[0075] Determine the object to be tested and the testing location;
[0076] At the target position of the steel pipe, the measuring points are arranged at certain intervals;
[0077] Use the signal cable to connect the vibration tool and the detection host, turn on the host power, open the detection software and set the parameters;
[0078] The detection host collects and saves the test signal of the point, performs signal processing such as noise on the test signal, and analyzes and determines the characteristic parameters of the measuring point position;
[0079] The characteristic parameters obtained by analysis are corrected by introducing the maximum amplitude correction method;
[0080] Compare the corrected contact time at the detection position with the corrected contact time at the dense state or the empty state;
[0081] When the corrected contact time of the measuring point is greater than the corrected contact time of the dense state, there is a gap at this position;
[0082] Analyze and save the results;
[0083] The next position is tested.
[0084] like Figure 3 As shown, the collision type steel tube concrete void detection equipment includes:
[0085] A vibration tool, a probe, a signal transmission line, a host, and a portable mobile detection host; the probe is located in the vibration tool, the probe is connected to the host via a transmission line, and the host is connected to the portable mobile detection host.
[0086] The present invention was used to detect the hollowing of steel tube concrete in the main line bridge column of an airport casing. According to the information provided, the wall thickness of the tested steel tube is 16mm, the diameter of the steel tube is 2.2m, the strength grade of the internal concrete is C30, and the concrete age is greater than 7 days. Figure 6 , the lower part of the measured area is about 1.5m from the ground.
[0087] Before testing, the compactness and empty positions of the steel pipe after construction are calibrated and tested, and the pressure is hit 10 times respectively. Please refer to the calibration test waveform Figure 7 and Figure 8 For the analysis results of the compacted and depleted areas, please refer to Fig. 9 .
[0088] According to the calibration results, the standard deviation of each test result after correction is smaller than the standard deviation before correction. According to the results, the correction values Tc0 and Tc1 of the dense part and the empty part are 0.196ms and 0.245ms respectively. Therefore, the calculation results of the judgment benchmark of the structure are as follows:
[0089] 1) Severely out of the market: [0.221, ﹢∞)
[0090] 2) Slightly out of range: [0.208, 0.221)
[0091] 3)Dense (0,0.208)
[0092] Use this benchmark to test the nearby area. During the test, the measuring points are arranged in a grid with 100mm intervals, and 6 measuring points are arranged in each column. For the arrangement of measuring points, please refer to Fig.10 For test results, please refer to Fig.11 .
[0093] In order to verify the reliability of the test results, holes were opened in the dense and hollow parts respectively. The verification results showed that the hole opening results were consistent with the test results.
[0094] The present invention is used to detect and verify the hollowing of steel tube concrete. The method can more accurately detect the hollowing of steel tube concrete, and provides a reliable detection method for improving engineering construction.
[0095] In this specification, each embodiment is described in a progressive manner, and each embodiment focuses on the differences from other embodiments. The same or similar parts between the embodiments can be referred to each other. For the system disclosed in the embodiment, since it corresponds to the method disclosed in the embodiment, the description is relatively simple, and the relevant parts can be referred to the method part.
[0096] The principles and implementation methods of the present invention are described in this article using specific examples. The description of the above embodiments is only used to help understand the method and core idea of the present invention. At the same time, for those skilled in the art, according to the idea of the present invention, there will be changes in the specific implementation methods and application scope. In summary, the content of this specification should not be understood as limiting the present invention.
Claims
1. A method for detecting the voiding of concrete-filled steel tubes based on the change of collision characteristics, characterized in that: include: Hitting the surface of an object with a tool; The signal generated by the impact passes through the signal probe; The signal is transmitted to the signal device through the signal transmission line; Signal equipment receives test data for storage and analysis; The data of the test waveform is analyzed by the analysis software to obtain the contact time of the test waveform; The test signal contact time is normalized and the correction formula is: Among them, T1 is the waveform start time, T2 is the waveform recovery time, x i (t) represents the acceleration signal collected by the probe, and A represents the maximum voltage of the signal; Test the compacted and voided areas separately and establish a benchmark for void determination; Whether the steel pipe is hollow is determined based on the hollow determination criteria.
2. The method for detecting voids in concrete-filled steel tubes based on changes in collision characteristics according to claim 1 is characterized in that: The tools include spherical hammer heads and cylindrical tools.
3. The method for detecting voids in concrete-filled steel tubes based on changes in collision characteristics according to claim 1 is characterized in that: The signal probe is fixed inside the striking tool.
4. The method for detecting voids in concrete-filled steel tubes based on changes in collision characteristics according to claim 1, characterized in that: The signal device is used to amplify, convert and send signals.
5. The method for detecting voids in concrete-filled steel tubes based on changes in collision characteristics according to claim 1, characterized in that: The criteria for determining the air escape include: When Tc≥0.5Tc0+0.5Tc1, the measuring point exists and there is a serious gap in the part; When 0.75Tc0+0.25Tc1≤Tc<0.5Tc0+0.5Tc1, there is a slight gap at the measuring point; When Tc<0.75Tc0+0.25Tc1, the measuring points are densely located.
6. A method for detecting the voiding of concrete-filled steel tubes based on the change of collision characteristics, characterized in that: include: Determine the object to be tested and the testing location; At the target position of the steel pipe, the measuring points are arranged at certain intervals; Use the signal cable to connect the vibration tool and the detection host, turn on the host power, open the detection software and set the parameters; The detection host collects and saves the test signal of the point, performs signal processing such as noise on the test signal, and analyzes and determines the characteristic parameters of the measuring point position; The characteristic parameters obtained by analysis are corrected by introducing the maximum amplitude correction method; Compare the corrected contact time at the detection position with the corrected contact time at the dense state or the empty state; When the corrected contact time of the measuring point is greater than the corrected contact time of the dense state, there is a gap at this position; Analyze and save the results; The next position is tested.
7. The method for detecting the void of concrete-filled steel tubes based on the change of collision characteristics according to claim 6 is characterized in that: The characteristic parameters include contact time.
8. The method for detecting the void of concrete-filled steel tube based on the change of collision characteristics according to any one of claims 6 to 7, characterized in that: Collision-type steel tube concrete void detection equipment includes: A vibration tool, a probe, a signal transmission line, a host, and a portable mobile detection host; the probe is located in the vibration tool, the probe is connected to the host via a transmission line, and the host is connected to the portable mobile detection host.
Citation Information
Cited By
Acoustic emission-based early warning method for void of concrete filled steel tube in construction process
CN119827636A