Method for improving etching uniformity
By using carbon tetrafluoride gas in dry etching technology to generate active ions and free radicals under glow discharge, combined with argon ionization and nitrogen purge, the etching uniformity problem is solved and more efficient polymerization is achieved Improved material removal and process uniformity.
Patent Information
- Application Number
- CN202410997386.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-24
- Publication Date
- 2024-11-12
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
In the existing dry etching technology, the proportional relationship between carbon tetrafluoride gas and hydrogen limits the etching uniformity, resulting in polymer adhesion affecting process uniformity and yield.
By introducing carbon tetrafluoride gas into the process cavity of the semiconductor etching equipment, carbon trifluoride ions and free radicals are generated under glow discharge conditions for etching, and then the carbon tetrafluoride gas is stopped and ionization is used for ionization of argon gas. and magnetic field bombardment, combined with nitrogen purge to remove fluorocarbon polymer.
The etching uniformity is improved, the complexity of proportional formulation of multiple gases is avoided, the polymer removal efficiency is enhanced, and the process uniformity and efficiency are improved.
Smart Images

Figure CN118943013A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of semiconductor etching, and in particular relates to a method for improving etching uniformity. Background Art
[0002] Dry etching is closely related to the rapid development of the semiconductor industry and the continuous progress of microelectronics manufacturing processes. As the feature size of semiconductor devices continues to shrink, the requirements for manufacturing processes are becoming increasingly higher. The uniformity of dry etching technology has gradually become one of the key parameters that cannot be ignored in semiconductor manufacturing. In the silicon oxide film etching process, carbon tetrafluoride has become the mainstream etching gas, but it is inevitable that a series of polymers will be attached to the surface of the film, preventing further etching of the local area, seriously affecting the uniformity and yield of the film etching process, so it is necessary to remove the polymers from the film surface in a timely manner.
[0003] In the related art, in order to remove fluorocarbon polymers during the etching process, hydrogen or other gases are introduced into the process chamber, and etching is performed in the process chamber together with carbon tetrafluoride gas, and hydrogen radicals extract fluoride ions in fluorocarbon compounds to form gaseous compounds and discharge. Since the etching and polymer removal effect is limited by the ratio of hydrogen to carbon tetrafluoride and other factors, there is a problem of relatively poor etching uniformity. Summary of the invention
[0004] The present invention overcomes the deficiencies of the prior art and provides a method for improving etching uniformity to solve the problems existing in the prior art.
[0005] To achieve the above object, the technical solution adopted by the present invention is: a method for improving etching uniformity, comprising the following steps:
[0006] S1. Introducing carbon tetrafluoride gas into a process chamber of a semiconductor etching device, wherein the carbon tetrafluoride gas dissociates into carbon trifluoride ions, carbon trifluoride free radicals and fluorine free radicals in the process chamber;
[0007] S2, the generated carbon trifluoride free radicals and fluorine free radicals etch the film to be etched in the etching process chamber to generate target gas and carbon fluorine polymer, and exhaust the target gas;
[0008] S3, stop introducing carbon tetrafluoride gas, introduce argon gas to bombard the surface to be etched to remove the fluorocarbon polymer, introduce nitrogen gas to purge the particles, and exhaust the gas.
[0009] In a preferred embodiment of the present invention, in step S1, the carbon tetrafluoride gas can generate free radicals with strong chemical reaction activity under the action of glow discharge.
[0010] In a preferred embodiment of the present invention, in step S2, the target gas is carbon dioxide.
[0011] In a preferred embodiment of the present invention, in step S3, argon gas is introduced into the etching process chamber and ionized to form argon ions. The argon ions bombard the fluorocarbon polymer remaining on the surface of the film to be etched under the action of the magnetic field, causing it to separate from the surface of the film to be etched.
[0012] In a preferred embodiment of the present invention, after the fluorocarbon polymer is separated from the surface of the film to be etched, the surface of the film to be etched and the cavity are purged and evacuated with nitrogen to discharge the fluorocarbon polymer that affects the etching uniformity out of the equipment process chamber.
[0013] The present invention solves the defects existing in the background technology and has the following beneficial effects:
[0014] The method for improving etching uniformity of the present invention introduces carbon tetrafluoride gas into the process chamber, so that the carbon tetrafluoride gas can be ionized into carbon trifluoride ions, carbon trifluoride free radicals and fluorine free radicals required for the etching process under the condition of glow discharge, and then the carbon trifluoride ions, carbon trifluoride free radicals and fluorine free radicals have the characteristics of strong chemical reaction activity, so that the fluorine-containing free radicals etch the silicon oxide film, and the carbon trifluoride ions, carbon trifluoride free radicals and fluorine free radicals react chemically with the silicon oxide film to generate target gas and carbon fluoride polymer, so that the target gas is discharged. The argon gas is introduced into the process chamber to form argon ions, and the fluorocarbon polymer on the surface of the silicon oxide to be etched is bombarded under the action of the magnetic field to form particles, and nitrogen gas is introduced for purging. The particles are discharged from the process chamber after evacuation, so as to achieve the purpose of removing the polymer that affects the uniformity of the etching process formed during the etching process of the wafer surface, thereby improving the uniformity of the etching process on the wafer surface. In addition, the present invention does not require the introduction of multiple gases at the same time, thereby avoiding the complex problem of accurately adjusting the gas ratio and a series of other factors that affect the etching uniformity and efficiency. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] The present invention is further described below in conjunction with the accompanying drawings and embodiments;
[0016] Figure 1 A flowchart of a preferred embodiment of the present invention;
[0017] Figure 2 A schematic diagram of a timeline of a preferred embodiment of the present invention; DETAILED DESCRIPTION
[0018] The present invention is further described below in conjunction with the accompanying drawings and specific embodiments so that those skilled in the art can better understand the present invention and implement it, but the embodiments are not intended to limit the present invention.
[0019] This embodiment provides a method for improving etching uniformity, which achieves the purpose of removing polymers formed during the etching process on the wafer surface that affect the uniformity of the etching process, thereby improving the uniformity of the etching process on the wafer surface.
[0020] like Figure 1 As shown, the method for improving etching uniformity in this embodiment includes the following steps:
[0021] S1. Introducing carbon tetrafluoride gas into a process chamber of a semiconductor etching device, wherein the carbon tetrafluoride gas dissociates into carbon trifluoride ions, carbon trifluoride free radicals and fluorine free radicals in the process chamber. Under the action of glow discharge, the carbon tetrafluoride gas dissociates into carbon trifluoride ions, carbon trifluoride free radicals and fluorine free radicals, wherein the carbon trifluoride free radicals and fluorine free radicals have strong chemical reaction activity;
[0022] S2, the generated carbon trifluoride free radicals and fluorine free radicals etch the film to be etched in the etching process chamber to generate a target gas and a fluorocarbon polymer, and the target gas is discharged. The target gas generated in this step is carbon dioxide. After the carbon dioxide is discharged, the fluorocarbon polymer can be processed;
[0023] S3. Stop introducing carbon tetrafluoride gas, introduce argon gas to bombard the surface to be etched to remove the fluorocarbon polymer, introduce nitrogen gas to purge the particles, and exhaust them by vacuum. In this step, argon gas is introduced into the etching process chamber and ionized to form argon ions. Under the action of the magnetic field, the argon ions bombard the fluorocarbon polymer remaining on the surface of the film to be etched to separate it from the surface of the film to be etched. After the fluorocarbon polymer is separated from the surface of the film to be etched, nitrogen gas is used to purge and exhaust the surface of the film to be etched and the cavity to discharge the fluorocarbon polymer that affects the etching uniformity from the equipment process chamber.
[0024] like Figure 2 As shown, A represents the carbon tetrafluoride gas introduced into the process chamber at a first flow rate, B represents the argon gas introduced into the process chamber at a second flow rate, C represents the nitrogen gas introduced into the process chamber, and D represents the etching gas carbon tetrafluoride introduced in the next etching cycle, wherein the t axis represents the time axis. The etching method comprises the following steps:
[0025] Step E1: introducing carbon tetrafluoride gas into the process chamber for a first time period;
[0026] Step E2: After the carbon tetrafluoride gas is introduced into the process chamber for a first time period, the introduction of the carbon tetrafluoride gas is stopped, and argon gas is introduced into the process chamber for a second time period;
[0027] Step E3: stopping the introduction of argon gas into the process chamber, and continuing to stop the introduction of carbon tetrafluoride gas, and starting to introduce nitrogen gas into the process chamber for a third period of time;
[0028] Step E4: Stop introducing argon and nitrogen into the process chamber, and only introduce the carbon tetrafluoride etching gas for the first time into the process chamber to enter the next etching process cycle.
[0029] In actual operation, the method for improving etching uniformity in this embodiment is to introduce carbon tetrafluoride gas into the process chamber so that the carbon tetrafluoride gas can be ionized into carbon trifluoride ions, carbon trifluoride free radicals and fluorine free radicals required for the etching process under the condition of glow discharge, and then utilize the characteristics of carbon trifluoride ions, carbon trifluoride free radicals and fluorine free radicals with strong chemical reactivity to make fluorine-containing free radicals etch the silicon oxide film, and the carbon trifluoride ions, carbon trifluoride free radicals and fluorine free radicals chemically react with the silicon oxide film to generate target gas and carbon fluoride polymer, thereby making the silicon oxide film The target gas is discharged from the process chamber, and argon gas is introduced to ionize it to form argon ions. Under the action of the magnetic field, the fluorocarbon polymer on the surface of the silicon oxide to be etched is bombarded to form particles. Nitrogen gas is introduced for purging, and the particles are discharged from the process chamber after evacuation, so as to achieve the purpose of removing the polymer that affects the uniformity of the etching process formed during the etching process of the wafer surface, thereby improving the uniformity of the etching process on the wafer surface. In addition, the present invention does not require the introduction of multiple gases at the same time, thereby avoiding the complex problem of accurately adjusting the gas ratio and a series of other factors that affect the etching uniformity and efficiency.
[0030] Obviously, the above embodiments are merely examples for clear explanation and are not intended to limit the implementation methods. For those skilled in the art, other different forms of changes or modifications can be made based on the above description. It is not necessary and impossible to list all the implementation methods here. The obvious changes or modifications derived from these are still within the protection scope of the invention.
Claims
1. A method for improving etching uniformity, characterized in that: The following steps are involved: S1. Introducing carbon tetrafluoride gas into a process chamber of a semiconductor etching device, wherein the carbon tetrafluoride gas dissociates into carbon trifluoride ions, carbon trifluoride free radicals and fluorine free radicals in the process chamber; S2, the generated carbon trifluoride free radicals and fluorine free radicals etch the film to be etched in the etching process chamber to generate target gas and carbon fluorine polymer, and exhaust the target gas; S3, stop introducing carbon tetrafluoride gas, introduce argon gas to bombard the surface to be etched to remove the fluorocarbon polymer, introduce nitrogen gas to purge the particles, and exhaust the gas.
2. A method for improving etching uniformity according to claim 1, characterized in that: In step S1, the carbon tetrafluoride gas can generate free radicals with strong chemical reaction activity under the action of glow discharge.
3. The method for improving etching uniformity according to claim 1, characterized in that: In step S2, the target gas is carbon dioxide.
4. The method for improving etching uniformity according to claim 1, characterized in that: In step S3, argon gas is introduced into the etching process chamber and ionized to form argon ions. Under the action of the magnetic field, the argon ions bombard the fluorocarbon polymer remaining on the surface of the film to be etched, so that the fluorocarbon polymer is separated from the surface of the film to be etched.
5. A method for improving etching uniformity according to claim 4, characterized in that: After the fluorocarbon polymer is separated from the surface of the film to be etched, the surface of the film to be etched and the cavity are purged and evacuated with nitrogen gas to discharge the fluorocarbon polymer that affects the etching uniformity out of the equipment process cavity.
Citation Information
Patent Citations
Cleaning method for substrate processing chamber, storage medium, and substrate processing chamber
CN101022693A
Silicon slice etching method
CN101197269A
Multilayered medium etching method
CN103050396A
Cited By
Method for etching polysilicon gate of MOS device with SGT structure
CN121038344A