Formation method of semiconductor structure
By first removing the first side wall layer of the side wall of the gate structure in the process process of the semiconductor structure and forming the second side wall layer, the process difficulty and material residue problems caused by the small space of adjacent gate structures in the semiconductor structure are solved. Improved performance.
Patent Information
- Application Number
- CN202310540981.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-05-12
- Publication Date
- 2024-11-12
AI Technical Summary
In the process process of semiconductor structures, as the device size decreases, the spatial area between adjacent gate structures becomes smaller, resulting in a process window for removing the material of the second side wall of the first groove and the bottom of the second side wall layer at the bottom becomes smaller. , increases the process difficulty and the probability of residual materials, affecting the performance of semiconductor structures.
Before forming the second side wall layer, the first side wall layer of the side wall of the gate structure is removed, the spatial area between adjacent gate structures is increased, and the second side wall layer is formed through an atomic layer deposition process to cover the gate The side walls and groove areas of the electrode structure expand the process window and reduce the probability of material residue.
By expanding the spatial region between adjacent gate structures, the process difficulty of removing the second side wall layer material of the first groove bottom and side wall is reduced, and the probability of material residue is reduced, thereby improving the performance of the semiconductor structure.
Smart Images

Figure CN118943017A_ABST
Abstract
Description
Technical Field
[0001] The embodiments of the present invention relate to the field of semiconductor manufacturing, and in particular to a method for forming a semiconductor structure. Background Art
[0002] With the rapid development of semiconductor manufacturing technology, semiconductor transistors are moving towards higher component density and higher integration, and semiconductor process nodes are continuously decreasing in accordance with Moore's Law. Transistors, as the most basic semiconductor transistors, are currently being widely used. Therefore, with the increase in component density and integration of semiconductor transistors, in order to adapt to the reduction of process nodes, the channel length of transistors must be continuously shortened.
[0003] In order to better adapt to the requirement of proportional reduction of transistor size, semiconductor processes have gradually begun to transition from planar transistors to three-dimensional transistors with higher efficiency, such as fin field effect transistors (FinFETs) and gate-all-around (GAA) transistors. Among them, gate-all-around transistors include vertical gate-all-around transistors and horizontal gate-all-around transistors. In a gate-all-around transistor, the gate surrounds the area where the channel is located from all sides. Compared with planar transistors, the gate of a gate-all-around transistor has a stronger control ability over the channel and can better suppress the short channel effect.
[0004] As device size continues to shrink, improving the performance of all-around gate structure devices becomes increasingly difficult and challenging. Summary of the invention
[0005] The problem solved by the embodiments of the present invention is to provide a method for forming a semiconductor structure, which is beneficial to further improve the performance of the semiconductor structure.
[0006] To solve the above problems, an embodiment of the present invention provides a method for forming a semiconductor structure, comprising: providing a substrate, on which a channel stack structure is formed, the channel stack structure comprising one or more channel stacks stacked in sequence in a longitudinal direction, the channel stack comprising a sacrificial layer and a channel layer located on the sacrificial layer, a gate structure spanning the channel stack structure is formed on the substrate, the gate structure covers a portion of the top and a portion of the sidewall of the channel stack structure, and a first sidewall layer is formed on the sidewall of the gate structure; forming a first groove in the channel stack structure on both sides of the gate structure, the sidewall of the first groove exposing the channel stack structure; in a direction parallel to the substrate and perpendicular to the extension direction of the gate structure, laterally etching a portion of the sacrificial layer exposed by the sidewall of the first groove to form a second groove, the second groove being surrounded by an adjacent channel layer and the remaining sacrificial layer, or the second groove being surrounded by the substrate, the channel layer adjacent to the substrate, and the remaining sacrificial layer; after forming the first groove, removing the first sidewall layer; after removing the first sidewall layer, forming a second sidewall layer in the second groove and on the sidewall of the gate structure.
[0007] Optionally, the step of forming a first groove in the channel stack structure on both sides of the gate structure includes: forming a photoresist layer on the top of the gate structure and the first sidewall layer, the photoresist layer exposing the channel stack structure on both sides of the gate structure; using the photoresist layer as a mask, performing patterning on the channel stack structure on both sides of the gate structure, and forming a first groove in the channel stack structure on both sides of the gate structure.
[0008] Optionally, the process of forming the first groove includes a dry etching process.
[0009] Optionally, the process of laterally etching the portion of the sacrificial layer exposed by the sidewall of the first groove includes a wet etching process.
[0010] Optionally, after the second groove is formed, the first spacer layer is removed; or, after the first spacer layer is removed, the second groove is formed.
[0011] Optionally, in the process of laterally etching the portion of the sacrificial layer exposed by the sidewall of the first groove, an etching selectivity ratio between the sacrificial layer and the channel layer is greater than 10:1.
[0012] Optionally, the process of removing the first spacer layer includes a wet etching process.
[0013] Optionally, the etching solution used in the wet etching process includes a phosphoric acid solution.
[0014] Optionally, the material of the second spacer layer includes one or more of silicon nitride, silicon oxide and silicon oxynitride.
[0015] Optionally, the step of forming a second spacer layer in the second groove and on the sidewall of the gate structure includes: forming a second spacer material layer on the sidewall and top of the gate structure, the sidewall and bottom of the first groove, and in the second groove; removing the second spacer material layer on the top of the gate structure, the second spacer material layer on the sidewall and bottom of the first groove, and the remaining second spacer material layer located in the second groove and the second spacer material layer located on the sidewall of the gate structure serve as the second spacer layer.
[0016] Optionally, the process of forming the second spacer material layer includes an atomic layer deposition process.
[0017] Optionally, the process of removing the second spacer material layer on the sidewall of the first groove includes an anisotropic dry etching process.
[0018] Optionally, in the step of providing a substrate, an insulating layer is also formed on the top of the substrate, and the channel stack structure covers the insulating layer; in the process of removing the second sidewall material layer on the sidewall and bottom of the first groove, the etching selectivity ratio between the second sidewall material layer and the insulating layer is greater than 20:1.
[0019] Optionally, the material of the insulating layer includes silicon oxide.
[0020] Compared with the prior art, the technical solution of the embodiment of the present invention has the following advantages:
[0021] An embodiment of the present invention provides a method for forming a semiconductor structure, wherein a first groove is formed in a channel stack structure on both sides of a gate structure, the sidewall of the first groove exposes the channel stack structure, and a portion of the sacrificial layer exposed by the sidewall of the first groove is laterally etched in a direction parallel to the substrate and perpendicular to the extension direction of the gate structure to form a second groove, wherein the second groove is surrounded by an adjacent channel layer and the remaining sacrificial layer, or the second groove is surrounded by the substrate, the channel layer adjacent to the substrate, and the remaining sacrificial layer. After the first groove is formed, the first sidewall layer is removed, and a second sidewall layer is formed in the second groove and on the sidewall of the gate structure, that is, in the embodiment of the present invention, when the second groove is formed, Before forming the sidewall layer, the first sidewall layer of the gate structure is removed first, thereby increasing the spatial area between adjacent gate structures. Accordingly, in the process of forming the second sidewall layer, the material forming the second sidewall layer will cover the sidewall of the gate structure, the bottom and sidewall of the first groove, and the second groove. Since the spatial area between adjacent gate structures becomes larger, the process window for removing the material of the second sidewall layer at the bottom and sidewall of the first groove becomes larger, thereby reducing the process difficulty of removing the material of the second sidewall layer at the bottom and sidewall of the first groove, and reducing the probability of the material of the second sidewall layer remaining at the bottom and sidewall of the first groove, thereby improving the performance of the semiconductor structure. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] Figures 1 to 3is a structural schematic diagram corresponding to a method for forming a semiconductor structure;
[0023] Figures 4 to 16 It is a schematic structural diagram corresponding to each step in an embodiment of a method for forming a semiconductor structure of the present invention. DETAILED DESCRIPTION
[0024] The performance of the current semiconductor structure needs to be improved. The reasons why the performance needs to be improved are analyzed in combination with a structural schematic diagram corresponding to a method for forming a semiconductor structure.
[0025] Figures 1 to 3 The present invention is a structural schematic diagram corresponding to a method for forming a semiconductor structure.
[0026] refer to Figure 1 A substrate 10 is provided, on which a channel stack structure (not marked) is formed, the channel stack structure comprising one or more channel stacks 13 stacked in sequence in the longitudinal direction, the channel stack 13 comprising a sacrificial layer 12 and a channel layer 11 located on the sacrificial layer 12, the sidewalls of the sacrificial layer 12 are indented inward relative to the sidewalls of the channel layer 11, and the adjacent channel layers 11 and the sacrificial layer 12 form a second groove 18, and the substrate 10, the channel layers 11 adjacent to the substrate 10 and the sacrificial layer 12 form the second groove 18, a gate structure 15 spanning the channel stack structure is formed on the substrate 10, the gate structure 15 covers a portion of the top and a portion of the sidewalls of the channel stack structure, a sidewall layer 14 is formed on the sidewalls of the gate structure 15, and a first groove 17 is formed in the channel stack structure on both sides of the gate structure 104, and the sidewalls of the first groove 17 expose the channel stack structure.
[0027] refer to Figure 2 An inner wall spacer material layer 20 is formed on the bottom and sidewalls of the first groove 17 , the top and sidewalls of the gate structure 15 , and the second groove 18 .
[0028] refer to Figure 3 , the inner wall spacer material layer 20 on the sidewall and bottom of the first groove 17 and the top and sidewall of the gate structure 15 is removed, and the remaining inner wall spacer material layer 20 located in the second groove 18 is used as the inner wall spacer layer 21.
[0029] Through research, it is found that, when the process technology of semiconductor structure is continuously reduced, the space area between adjacent gate structures 15 is getting smaller and smaller. Accordingly, in the process of removing the sidewall and bottom of the first groove 17, and the inner wall sidewall material layer 20 of the top and sidewall of the gate structure 15, since the space area between adjacent gate structures 15 is getting smaller and smaller, the process window for removing the sidewall and bottom of the first groove 17, and the inner wall sidewall material layer 20 of the top and sidewall of the gate structure 15 is also getting smaller and smaller, thereby increasing the difficulty of completely removing the sidewall and bottom of the first groove 17, and the inner wall sidewall material layer 20 of the top and sidewall of the gate structure 15, and especially increasing the probability of residual inner wall sidewall material layer 20 on the sidewall and bottom of the first groove 17, thereby affecting the performance of the semiconductor structure.
[0030] In order to solve the technical problem, an embodiment of the present invention provides a method for forming a semiconductor structure, comprising: providing a substrate, on which a channel stack structure is formed, the channel stack structure comprising one or more channel stacks stacked in sequence in a longitudinal direction, the channel stack comprising a sacrificial layer and a channel layer located on the sacrificial layer, a gate structure spanning the channel stack structure is formed on the substrate, the gate structure covers a portion of the top and a portion of the sidewall of the channel stack structure, and a first sidewall layer is formed on the sidewall of the gate structure; forming a first groove in the channel stack structure on both sides of the gate structure, the sidewall of the first groove exposing the channel stack structure; in a direction parallel to the substrate and perpendicular to the extension direction of the gate structure, laterally etching a portion of the sacrificial layer exposed by the sidewall of the first groove to form a second groove, the second groove being surrounded by an adjacent channel layer and the remaining sacrificial layer, or the second groove being surrounded by the substrate, the channel layer adjacent to the substrate, and the remaining sacrificial layer; after forming the first groove, removing the first sidewall layer; after removing the first sidewall layer, forming a second sidewall layer in the second groove and on the sidewall of the gate structure.
[0031] An embodiment of the present invention provides a method for forming a semiconductor structure. Before forming a second sidewall layer, the first sidewall layer of the sidewall of the gate structure is first removed, thereby increasing the spatial area between adjacent gate structures. Accordingly, in the process of forming the second sidewall layer, the material forming the second sidewall layer will cover the sidewall of the gate structure, the bottom and sidewall of the first groove, and the second groove. Since the spatial area between the adjacent gate structures becomes larger, the process window for removing the material of the second sidewall layer at the bottom and sidewall of the first groove becomes larger, thereby reducing the process difficulty of removing the material of the second sidewall layer at the bottom and sidewall of the first groove, and reducing the probability of the material of the second sidewall layer remaining at the bottom and sidewall of the first groove, thereby improving the performance of the semiconductor structure.
[0032] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and easy to understand, specific embodiments of the present invention are described in detail below with reference to the accompanying drawings.
[0033] Figures 4 to 16 It is a schematic structural diagram corresponding to each step in an embodiment of a method for forming a semiconductor structure of the present invention.
[0034] refer to Figures 4 to 6 , providing a substrate (not marked), having a channel stack structure 190 formed on the substrate, the channel stack structure 190 including one or more channel stacks 102 stacked in sequence in the vertical direction, the channel stack 102 including a sacrificial layer 1021 and a channel layer 1022 located on the sacrificial layer 1021, a gate structure 104 spanning the channel stack structure 190 is formed on the substrate, the gate structure 104 covers a portion of the top and a portion of the sidewalls of the channel stack structure 190, and a first spacer layer 103 is formed on the sidewalls of the gate structure 104.
[0035] The substrate is used to provide a process platform for forming a gate-all-around (GAA) transistor.
[0036] In this embodiment, the substrate is a three-dimensional substrate, and the substrate includes a substrate 100 and a protruding portion 101 protruding from the substrate 100 .
[0037] In this embodiment, the substrate 100 is a silicon substrate. In other embodiments, the substrate material may also be other materials such as germanium, silicon germanium, silicon carbide, gallium arsenide or indium gallium, and the substrate may also be other types of substrates such as a silicon on insulator substrate or a germanium on insulator substrate.
[0038] The protrusion 101 exposes a portion of the substrate 100 , thereby providing a process basis for subsequently forming an isolation layer.
[0039] In this embodiment, the material of the protrusion 101 is the same as that of the substrate 100, and the material of the protrusion 101 is silicon. In other embodiments, the material of the protrusion may also be a semiconductor material suitable for forming a fin, such as germanium, silicon germanium, silicon carbide, gallium arsenide, or indium gallium, and the material of the protrusion may also be different from that of the substrate.
[0040] In this embodiment, the channel stack structure 190 is located on the top of the protrusion 101 , and the extending direction of the channel stack structure 190 is the same as the extending direction of the protrusion 101 .
[0041] In this embodiment, the channel stack structure 190 includes one or more channel stacks 102 stacked in sequence in the vertical direction.
[0042] Each channel stack 102 includes a sacrificial layer 1021 and a channel layer 1022 located on the sacrificial layer 1021. The channel stack 102 provides a process basis for the subsequent formation of the suspended and spaced channel layer 1022. Specifically, the sacrificial layer 1021 supports the channel layer 1022, thereby providing a process basis for the subsequent realization of the spaced and suspended arrangement of the channel layer 1022, and also occupies a spatial position for the subsequent formation of the device gate structure. The channel layer 1022 is used to provide a conductive channel that fully surrounds the gate transistor.
[0043] Correspondingly, when there are multiple channel stacks 102 , there are also multiple channel layers 1022 , and the multiple channel layers 1022 are arranged at intervals.
[0044] In this embodiment, the material of the channel layer 1022 is Si, and the material of the sacrificial layer 1021 is SiGe. In the subsequent process of removing the sacrificial layer 1021, the etching selectivity of SiGe and Si is relatively high, so by setting the material of the sacrificial layer 1021 to SiGe and the material of the channel layer 1022 to Si, in the subsequent process of forming the second groove, the effect of the removal process of the sacrificial layer 1021 on the channel layer 1022 can be effectively reduced, thereby improving the quality of the channel layer 1022, and further facilitating the improvement of device performance. In other embodiments, when forming a PMOS transistor, in order to improve the performance of the PMOS transistor, SiGe channel technology can be used, the material of the fin and the channel layer is SiGe, and the material of the sacrificial layer is Si.
[0045] In this embodiment, the gate structure 104 is a dummy gate structure, and the gate structure 104 occupies a space position for a gate structure of a device to be formed subsequently.
[0046] In this embodiment, the gate structure 104 includes a dummy gate layer.
[0047] The material of the dummy gate layer includes polysilicon.
[0048] In this embodiment, in the step of providing a substrate, an insulating layer (not shown) is further formed on the top of the substrate, and the channel stack structure covers the insulating layer.
[0049] The insulating layer is used to protect the channel stack structure 190. The insulating layer can also be used as an etching stop layer in the subsequent step of removing the gate structure 104, which is beneficial to reduce the probability of damage to the channel layer 1022 caused by the process of removing the gate structure 104. At the same time, by forming the insulating layer, after the device gate structure is subsequently formed, the risk of leakage between adjacent device gate structures through the substrate can be reduced, thereby improving the performance of the semiconductor structure.
[0050] In this embodiment, the material of the insulating layer includes silicon oxide.
[0051] It should be noted that silicon oxide is an insulating material, which can reduce the risk of leakage through the substrate between adjacent device gate structures formed subsequently. At the same time, there is a large etching selectivity ratio between the silicon oxide material and the material selected for the gate structure 104. In the subsequent process of removing the gate structure 104, the insulating layer can play a role in etching stop, reducing the probability of damage to the channel layer 1022 caused by the process of removing the gate structure 104.
[0052] In this embodiment, a first spacer layer 103 is further formed on the sidewall of the gate structure 104 .
[0053] The first spacer layer 103 is used as an etching mask in a subsequent etching process to define a formation region of a source / drain doped layer to be formed subsequently. The first spacer layer 103 is also used to protect a sidewall of the gate structure 104 .
[0054] In this embodiment, the first spacer layer 103 is a single-layer structure, and the material of the spacer layer 103 is silicon nitride.
[0055] refer to Figure 7 , a first groove 107 is formed in the channel stack structure 190 on both sides of the gate structure 104 , and the sidewall of the first groove 107 exposes the channel stack structure 190 .
[0056] The first groove 107 provides a spatial position for the subsequent formation of a source-drain doping layer, and also provides a process window for the subsequent formation of a second groove.
[0057] In this embodiment, the step of forming the first groove 107 in the channel stack structure 190 on both sides of the gate structure 104 includes: patterning the channel stack structure 190 on both sides of the gate structure 104 to form the first groove 107 in the channel stack structure 190 on both sides of the gate structure 104 .
[0058] In this embodiment, the process of forming the first groove 107 includes a dry etching process.
[0059] Specifically, the dry etching process is an anisotropic dry etching process, which has good cross-sectional controllability and is beneficial to improving the cross-sectional morphology quality of the first groove 107 .
[0060] refer to Figure 8 , along a direction parallel to the substrate and perpendicular to the extension direction of the gate structure 104, the portion of the sacrificial layer 1021 exposed on the sidewall of the first groove 107 is laterally etched to form a second groove 108, and the second groove 108 is surrounded by the adjacent channel layer 1022 and the remaining sacrificial layer 1021, or the second groove 108 is surrounded by the substrate, the channel layer 1022 adjacent to the substrate, and the remaining sacrificial layer 1021.
[0061] It should be noted that the second groove 108 provides a spatial position for the subsequent formation of a second sidewall layer, so that the second sidewall layer is located between the subsequently formed source-drain doped layer and the device gate structure. The second sidewall layer can isolate the source-drain doped layer and the device gate structure, which is beneficial to reducing the parasitic capacitance between the source-drain doped layer and the device gate structure.
[0062] In this embodiment, the process of laterally etching the portion of the sacrificial layer 1021 exposed by the sidewall of the first groove 107 includes a wet etching process.
[0063] The wet etching process is an isotropic etching process, so that the sacrificial layer 1021 can be etched in a direction parallel to the substrate and perpendicular to the extension direction of the gate structure 104, and the wet etching process can easily achieve a larger etching selectivity ratio, which is beneficial to reduce the difficulty of etching the sacrificial layer 1021 and reduce the probability of damage to other film layer structures.
[0064] In this embodiment, the material of the sacrificial layer 1021 is SiGe, the material of the channel layer 1022 is Si, and the exposed sacrificial layer 1021 is wet-etched by HCl vapor. The etching rate of HCl vapor on SiGe material is much higher than that on Si material, so the use of HCl vapor to etch part of the sacrificial layer 1021 on the side of the groove 107 can effectively reduce the probability of damage to the channel layer 1022.
[0065] In other embodiments, when the material of the channel layer is SiGe and the material of the sacrificial layer 1021 is Si, the etching solution used in the wet etching process is a tetramethylammonium hydroxide (TMAH) solution. The difference between the etching rate of the tetramethylammonium hydroxide solution on the Si material and the etching rate on the SiGe material is large, so the use of the tetramethylammonium hydroxide solution to etch the sacrificial layer can also effectively reduce the probability of the channel layer being damaged.
[0066] It should be noted that, in the process of laterally etching the portion of the sacrificial layer 1021 exposed by the sidewall of the first groove 107, the etching selectivity ratio between the sacrificial layer 1021 and the channel layer 1022 should not be too small. If the etching selectivity ratio between the sacrificial layer 1021 and the channel layer 1022 is too small, in the process of laterally etching the sacrificial layer 1021, the probability of the channel layer 1022 being mistakenly etched is increased, and the probability of the channel layer 1022 being damaged is increased, thereby affecting the performance of the semiconductor structure. For this reason, in the present embodiment, in the process of laterally etching the portion of the sacrificial layer 1021 exposed by the sidewall of the first groove 107, the etching selectivity ratio between the sacrificial layer 1021 and the channel layer 1022 is greater than 10:1.
[0067] Specifically, along the direction parallel to the substrate and perpendicular to the extension direction of the gate structure 104, the lateral dimension of the second groove 108 should not be too large or too small. If the lateral dimension of the second groove 108 is too small, in the process of removing the sacrificial layer 1021, the protective effect of the inner wall sidewall layer formed in the second groove 108 on the source and drain doping layer formed subsequently is reduced, increasing the probability of damage to the source and drain doping layer, thereby affecting the performance of the semiconductor structure; if the lateral dimension of the second groove 108 is too large, the distance between the device gate structure formed subsequently and the source and drain doping layer becomes larger, thereby affecting the performance of the semiconductor structure. For this reason, in the present embodiment, along the direction parallel to the substrate and perpendicular to the extension direction of the gate structure 104, the lateral dimension of the second groove 108 is 4 nanometers to 6 nanometers.
[0068] refer to Fig. 9 After forming the first groove 107 , the first spacer layer 103 is removed.
[0069] It should be noted that by removing the first spacer layer 103 on the side wall of the gate structure 104, the spatial area between adjacent gate structures 104 is increased. Accordingly, in the subsequent process of forming the second spacer layer, the material forming the second spacer layer will cover the side wall and top of the gate structure 104, the bottom and side wall of the first groove 107, and the second groove 108. Since the spatial area between adjacent gate structures 104 becomes larger, the process window for removing the material of the second spacer layer at the bottom and side wall of the first groove 107 becomes larger, which reduces the process difficulty of removing the material of the second spacer layer at the bottom and side wall of the first groove 107, and reduces the probability of the material of the second spacer layer remaining at the bottom and side wall of the first groove 107, thereby improving the performance of the semiconductor structure.
[0070] In this embodiment, after the second groove 108 is formed, the first spacer layer 103 is removed.
[0071] It should be noted that, during the formation of the second groove 108 , the first spacer layer 103 protects the sidewall of the gate structure 104 , reducing the probability of damage to the sidewall of the gate structure 104 . Therefore, after the second groove 108 is formed, the first spacer layer 103 is removed.
[0072] In this embodiment, the process of removing the first spacer layer 103 includes a wet etching process.
[0073] Specifically, the wet etching process is an isotropic etching process, so that the first sidewall layer 103 can be etched in a direction parallel to the substrate and perpendicular to the extension direction of the gate structure 104, and the wet etching process can easily achieve a larger etching selectivity ratio, which is beneficial to reduce the process difficulty of etching the first sidewall layer 103 and reduce the probability of damage to other film layer structures (such as gate structures).
[0074] In this embodiment, the etching solution used in the wet etching process includes a hot phosphoric acid solution.
[0075] As can be seen from the foregoing, as an example, the first spacer layer 103 is removed after the second groove 108 is formed. In other embodiments, the second groove may be formed after the first spacer layer is removed.
[0076] refer to Figure 10 to Figure 11 After removing the first spacer layer 103 , a second spacer layer 110 is formed in the second groove 108 and on the sidewall of the gate structure 104 .
[0077] It should be noted that the second sidewall layer 110 located in the second groove 108 is located between the subsequently formed source-drain doped layer and the device gate structure. The second sidewall layer 110 can isolate the source-drain doped layer and the device gate structure, which is beneficial to reducing the parasitic capacitance between the source-drain doped layer and the device gate structure.
[0078] In this embodiment, the step of forming a second spacer layer 110 in the second groove 108 and on the sidewall of the gate structure 104 includes: forming a second spacer material layer 109 on the sidewall and top of the gate structure 104, the sidewall and bottom of the first groove 107, and the second groove 108; removing the second spacer material layer 109 on the top of the gate structure 104, the second spacer material layer 109 on the sidewall and bottom of the first groove 107, and the remaining second spacer material layer 109 located in the second groove 108 and the second spacer material layer 109 located on the sidewall of the gate structure 104 serve as the second spacer layer 110.
[0079] It should be noted that in this embodiment, during the process of forming the second spacer layer 110 , the material layer forming the second spacer layer 110 is also formed on the sidewall of the gate structure 104 , and the material layer used to form the inner wall spacer layer 110 on the sidewall of the gate structure 104 is also used as the second spacer layer 110 .
[0080] The second spacer layer 110 located on the sidewall of the gate structure 107 protects the gate structure 107 and reduces the probability of the gate structure 107 being damaged.
[0081] In this embodiment, the process of forming the second spacer material layer 109 includes an atomic layer deposition process.
[0082] Taking the atomic layer deposition process as an example, the atomic layer deposition process has good film layer step coverage, which reduces the risk of voids in the inner wall spacer material layer 109, thereby improving the performance of the semiconductor structure.
[0083] In this embodiment, the process of removing the second spacer material layer 109 on the top of the gate structure 104 and the sidewall and bottom of the first groove 107 includes an anisotropic dry etching process.
[0084] It should be noted that the anisotropic dry etching process has better profile controllability, which is beneficial to improving the profile morphology quality of the side wall of the second sidewall layer 110. In addition, the selected anisotropic dry etching process is conducive to achieving a higher etching selectivity, thereby reducing the probability of mis-etching other film layers.
[0085] In this embodiment, the material of the second spacer layer 110 includes one or more of silicon nitride, silicon oxide and silicon oxynitride.
[0086] Specifically, silicon nitride, silicon oxide and silicon oxynitride are all dielectric materials that can electrically isolate the device gate structure and source-drain doping layers that are subsequently formed.
[0087] It should be noted that, in the process of removing the second spacer material layer 109 on the sidewall and bottom of the first groove 107, the etching selectivity between the second spacer material layer 109 and the insulating layer should not be too small. If the etching selectivity between the second spacer material layer 109 and the insulating layer is too small, the probability of the insulating layer being damaged is increased in the process of removing the second spacer material layer 109, that is, the protective effect of the insulating layer on the channel stack structure 190 is reduced, thereby increasing the probability of the channel stack structure 190 being mistakenly etched, thereby affecting the performance of the semiconductor structure. For this reason, in the present embodiment, in the process of removing the second spacer material layer 109 on the sidewall and bottom of the first groove 107, the etching selectivity between the second spacer material layer 109 and the insulating layer is greater than 20:1.
[0088] refer to Fig.12 After forming the second spacer layer 110 , the method for forming the semiconductor structure further includes: forming a source-drain doping layer 160 in the first groove 107 .
[0089] Specifically, the source-drain doping layer 160 is used as a source region and a drain region of a transistor.
[0090] In this embodiment, the source-drain doped layer 160 is formed in the first groove 107 by using an epitaxial process.
[0091] Specifically, the epitaxial process has the characteristics of fast growth rate and good filling performance. By using the epitaxial process to form the source-drain doped layer 160, the risk of generating voids in the source-drain doped layer 160 is reduced, and the performance of the source-drain doped layer 160 itself is improved.
[0092] refer to Fig.13 After forming the source-drain doping layer 160 , the method for forming the semiconductor structure further includes: forming an interlayer dielectric layer 161 on the top of the source-drain doping layer 160 , wherein the interlayer dielectric layer 161 covers the sidewall of the gate structure 104 .
[0093] The interlayer dielectric layer 161 is used to achieve electrical isolation between adjacent devices.
[0094] In this embodiment, the material of the interlayer dielectric layer 161 is silicon oxide.
[0095] In this embodiment, the step of forming the interlayer dielectric layer 161 includes: forming a dielectric material layer (not shown) on the substrate of the side wall of the gate structure 104, and the dielectric material layer also covers the top of the gate structure 104; removing the dielectric material layer above the top of the gate structure 104, and the remaining dielectric material layer serves as the interlayer dielectric layer 161.
[0096] refer to Fig.14 , the gate structure 104 is removed, and a gate opening 163 is formed in the interlayer dielectric layer 161 .
[0097] Specifically, the gate opening 163 provides a process window for the subsequent removal of the sacrificial layer 1021 , and also provides a spatial position for the subsequent formation of a device gate structure.
[0098] In this embodiment, the process of removing the gate structure 104 includes a dry etching process.
[0099] refer to Fig.15 , the sacrificial layer 1021 exposed by the gate opening 163 is removed, and a through groove 193 communicating with the gate opening 163 is formed below the channel layer 1022 .
[0100] Specifically, the sacrificial layer 1021 is removed to form a through groove 193, which provides a spatial position for the subsequent formation of a device gate structure.
[0101] In this embodiment, the process of removing the sacrificial layer 1021 exposed by the gate opening 163 includes a wet etching process.
[0102] Specifically, the material of the channel layer 1022 is Si, and the material of the sacrificial layer 1021 is SiGe. Therefore, the sacrificial layer 1021 exposed by the gate opening 163 is removed by HCl vapor, and the etching rate of the sacrificial layer 1021 by the wet etching process is much greater than the etching rate of the channel layer 1022 and the protrusion 101.
[0103] The sacrificial layer 1021 is removed after the source-drain doped layer 160 is formed. Therefore, after removing the sacrificial layer 1021, along the extension direction of the protrusion 101, both ends of the channel layer 1022 are connected to the source-drain doped layer 160 and suspended in the gate opening 163, thereby providing a basis for the subsequent device gate structure to surround the channel layer 1022.
[0104] After the sacrificial layer 1021 is removed, the channel layers 1022 are arranged at intervals, and the remaining channel layers 1022 constitute a channel structure layer, which is located on the protrusion 101 and is arranged at intervals from the protrusion 101 .
[0105] refer to Fig.16 A device gate structure 166 is formed in the gate opening 163 and the through groove 193 , and the device gate structure 166 surrounds the channel layer 1022 .
[0106] The device gate structure 166 is used to control the opening and closing of the conductive channel when the device is working.
[0107] Specifically, the device gate structure 166 is a metal gate structure.
[0108] In this embodiment, the device gate structure 166 includes a gate dielectric layer (not shown) conformally covering a portion of the top, a portion of the sidewall and a portion of the bottom of the channel layer 1022 , and a gate electrode layer (not shown) covering the gate dielectric layer.
[0109] In this embodiment, the material of the gate dielectric layer includes one or more of HfO2, ZrO2, HfSiO, HfSiON, HfTaO, HfTiO, HfZrO, Al2O3, SiO2 and La2O3.
[0110] Specifically, the gate dielectric layer includes a gate oxide layer that conformally covers a portion of the top, a portion of the sidewall, and a portion of the bottom of the channel layer 1022, and a high-k gate dielectric layer that conformally covers the gate oxide layer. The material of the high-k gate dielectric layer is a high-k dielectric material, which refers to a dielectric material having a relative dielectric constant greater than the relative dielectric constant of silicon oxide.
[0111] The gate electrode layer is used for subsequent electrical connection with external structures.
[0112] In this embodiment, the material of the gate electrode layer includes one or more of TiN, TaN, Ta, Ti, TiAl, W, Al, TiSiN and TiAlC.
[0113] Specifically, the gate electrode layer may include a work function layer and an electrode layer covering the work function layer, or the gate electrode layer may include only the work function layer.
[0114] Although the present invention is disclosed as above, the present invention is not limited thereto. Any person skilled in the art can make various changes and modifications without departing from the spirit and scope of the present invention. Therefore, the protection scope of the present invention shall be subject to the scope defined by the claims.
Claims
1. A method for forming a semiconductor structure, characterized in that: include: A substrate is provided, on which a channel stack structure is formed, the channel stack structure includes one or more channel stacks stacked in sequence in a longitudinal direction, the channel stack includes a sacrificial layer and a channel layer located on the sacrificial layer, a gate structure is formed on the substrate and spans the channel stack structure, the gate structure covers a portion of the top and a portion of the sidewall of the channel stack structure, and a first spacer layer is formed on the sidewall of the gate structure; forming a first groove in the channel stack structure on both sides of the gate structure, wherein the sidewall of the first groove exposes the channel stack structure; Laterally etching a portion of the sacrificial layer exposed by the sidewall of the first groove in a direction parallel to the substrate and perpendicular to the extension direction of the gate structure to form a second groove, wherein the second groove is surrounded by the adjacent channel layer and the remaining sacrificial layer, or the second groove is surrounded by the substrate, the channel layer adjacent to the substrate, and the remaining sacrificial layer; After forming the first groove, removing the first spacer layer; After removing the first spacer layer, a second spacer layer is formed in the second groove and on the sidewall of the gate structure.
2. The method for forming a semiconductor structure according to claim 1, wherein: The step of forming the first groove in the channel stack structure on both sides of the gate structure includes: forming a photoresist layer on the top of the gate structure and the first sidewall layer, the photoresist layer exposing the channel stack structure on both sides of the gate structure; using the photoresist layer as a mask, patterning the channel stack structure on both sides of the gate structure, and forming the first groove in the channel stack structure on both sides of the gate structure.
3. The method for forming a semiconductor structure according to claim 1, wherein: The process of forming the first groove includes a dry etching process.
4. The method for forming a semiconductor structure according to claim 1, wherein: The process of laterally etching the portion of the sacrificial layer exposed by the sidewall of the first groove comprises a wet etching process.
5. The method for forming a semiconductor structure according to claim 1, wherein: After forming the second groove, the first spacer layer is removed; or, after removing the first spacer layer, the second groove is formed.
6. The method for forming a semiconductor structure according to claim 1, wherein: In the process of laterally etching the portion of the sacrificial layer exposed by the sidewall of the first groove, an etching selectivity ratio between the sacrificial layer and the channel layer is greater than 10:
1.
7. The method for forming a semiconductor structure according to claim 1, wherein: The process of removing the first spacer layer includes a wet etching process.
8. The method for forming a semiconductor structure according to claim 7, wherein: The etching solution used in the wet etching process includes a phosphoric acid solution.
9. The method for forming a semiconductor structure according to claim 1, wherein: The material of the second spacer layer includes one or more of silicon nitride, silicon oxide and silicon oxynitride.
10. The method for forming a semiconductor structure according to claim 1, wherein: The step of forming a second spacer layer in the second groove and on the sidewall of the gate structure includes: forming a second spacer material layer on the sidewall and top of the gate structure, on the sidewall and bottom of the first groove, and in the second groove; removing the second spacer material layer on the top of the gate structure, the second spacer material layer on the sidewall and bottom of the first groove, and the remaining second spacer material layer located in the second groove and the second spacer material layer located on the sidewall of the gate structure serve as the second spacer layer.
11. The method for forming a semiconductor structure according to claim 10, wherein: The process of forming the second spacer material layer includes an atomic layer deposition process.
12. The method for forming a semiconductor structure according to claim 10, wherein: The process of removing the second spacer material layer on the sidewall of the first groove includes an anisotropic dry etching process.
13. The method for forming a semiconductor structure according to claim 10, wherein: In the step of providing a substrate, an insulating layer is also formed on the top of the substrate, and the channel stack structure covers the insulating layer; In the process of removing the second spacer material layer on the sidewall and the bottom of the first groove, the etching selectivity ratio between the second spacer material layer and the insulating layer is greater than 20:
1.
14. The method for forming a semiconductor structure according to claim 13, wherein: The material of the insulating layer includes silicon oxide.