Concrete pole with high crack resistance and preparation method thereof

By using a combined structure of main steel bar frame, stirrup, hollow spiral tube and crack-resistant net in concrete poles, and using sand or water to adjust the temperature, the crack problem caused by temperature changes in traditional poles at low and high temperatures is solved. Significantly improves crack resistance and service life.

CN118952441AInactive Publication Date: 2024-11-15GUANGDONG CHENYUAN BUILDING MATERIALS TECH CO LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202411168757.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-23
Publication Date
2024-11-15
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Traditional concrete poles are prone to cracking due to temperature changes in low and high temperature environments, and have low crack resistance and are unable to effectively deal with the influence of ambient temperature.

Method used

Using a structural design including main reinforcement frame, stirrups, hollow spiral tubes and anti-crack nets, the temperature of the pole is adjusted by adding sand or water to the hollow spiral tubes, slowing heat loss or reducing temperature, and preventing temperature caused by temperature changes. crack.

Benefits of technology

It effectively improves the crack resistance of concrete poles, extends service life, prevents dryness and damage, and enhances the overall structural strength and stability of the poles.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118952441A_ABST
    Figure CN118952441A_ABST
Patent Text Reader

Abstract

The invention discloses a high-crack-resistance concrete pole and a preparation method thereof, and the high-crack-resistance concrete pole comprises a pouring mold which is used for limiting the shape and appearance of the concrete pole; the electric pole comprises an electric pole body, a main steel bar frame is arranged in the electric pole body, the main steel bar frame is formed by sequentially and annularly arranging a plurality of steel bars, and a plurality of stirrups which are vertically arranged are arranged outside the main steel bar frame. The heat capacity of the electric pole is increased by adding sand into the hollow spiral pipe at the low temperature, loss of heat in the electric pole is relieved, the temperature of concrete can be kept, stress caused by temperature change can be relieved, and therefore the risk that the concrete electric pole cracks under temperature fluctuation is reduced; by means of evaporation and conduction characteristics of water, the overall temperature of the electric pole is reduced, material performance degradation caused by high temperature and thermal expansion and cold contraction of concrete and reinforcing steel bars are prevented, the service life of the electric pole is prolonged, the electric pole is prevented from being cracked and damaged, and the crack resistance of the electric pole is effectively improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of concrete poles, and in particular to a concrete pole with high crack resistance and a preparation method thereof. Background Art

[0002] Electric poles refer to a structure used to support power transmission and distribution lines. They are usually made of rod-shaped objects with strong materials and good insulation properties. They are used to fix conductors, support insulators and other power equipment to ensure the normal operation and safe and stable transmission of power lines. Electric poles generally include concrete poles, steel poles, wooden poles and composite poles. Concrete poles are power transmission line equipment made of concrete. They are usually used to support conductors in transmission lines and play the role of supporting and fixing conductors. Concrete poles are usually composed of concrete piles, cross arms and insulators, and are used for the construction and maintenance of transmission lines. Concrete poles have the following characteristics and advantages: strong durability, simple construction, environmental protection, strong plasticity and high safety.

[0003] After searching, a corrosion-resistant concrete pole and its manufacturing method with publication number CN115095212A are related to the field of power equipment, including a concrete layer and an anti-seepage layer arranged from the inside to the outside; a steel keel is arranged in the concrete layer; the anti-seepage layer is made of component A and component B with a mass ratio of (5.5-8): (1.5-3.5); based on the total amount of anti-seepage layer material, the component A contains the following raw materials in parts by weight: 35-40 parts of water, 55-65 parts of epoxy resin, 1-2 parts of solvent and 0.5-1.5 parts of additives; the component B includes water and curing agent in a mass ratio of 1: (1.2-1.75). This application can effectively enhance the corrosion resistance of the concrete pole and improve its practical life by setting an anti-seepage layer on the outside of the concrete pole.

[0004] Concrete poles may crack due to the influence of the surrounding environmental factors during use. For example, the temperature changes around the concrete poles, the large temperature difference between day and night or the drastic seasonal changes will cause cracks in the concrete due to thermal expansion and contraction, thus causing the poles to crack. The concrete poles in this patent cannot cope with the surrounding temperature in the low temperature winter and the high temperature summer, and are easily affected by the surrounding temperature and crack, and have low crack resistance. Summary of the invention

[0005] The purpose of the present invention is to provide a concrete pole with high crack resistance and a preparation method thereof, so as to solve the problem that traditional concrete poles cannot cope with the ambient temperature in low temperature winter and high temperature summer, are easily affected by the ambient temperature and crack, and have low crack resistance.

[0006] The present invention solves the above technical problems through the following technical solutions, which include: A casting mold, which is used to define the shape and appearance of the concrete pole; An electric pole body, wherein a main steel bar frame is arranged inside the electric pole body, wherein the main steel bar frame is formed by a plurality of steel bars arranged in a ring shape in sequence, wherein a plurality of vertically arranged stirrups are arranged outside the main steel bar frame, wherein a hollow spiral tube is arranged outside the main steel bar frame, wherein the hollow spiral tube is fixed to the outside of the plurality of stirrups by a plurality of steel wire ropes, wherein both ends of the hollow spiral tube extend to the outside of the electric pole body, and both ends of the hollow spiral tube are threadedly connected with sealing plugs.

[0007] Preferably, both ends of the main steel frame are welded with retaining steel rings, and an anti-cracking net is fixed between the two retaining steel rings via a plurality of steel wires.

[0008] Preferably, a plurality of U-shaped steel bars are arranged on one side of the main steel bar frame, and the plurality of U-shaped steel bars are arranged vertically in sequence.

[0009] Preferably, a vertical straight groove is provided on one side of the anti-cracking net, and the plurality of U-shaped steel bars are all located on the inner side of the vertical straight groove.

[0010] Preferably, the casting mold includes a first template, a first slot is formed on one side of the first template, a second template is provided on one side of the first template, a clip is fixed on one side of the second template, and the clip is clamped inside the first slot.

[0011] Preferably, a second slot is provided on the other side of the first template and the second template, an arc-shaped template is clamped between the two second slots, and a plurality of vertically arranged U-shaped hollow templates are fixed to the outer side of the arc-shaped template.

[0012] Preferably, the first card slot and the two second card slots are provided with trapezoidal slots, the card strip and the arc-shaped template are provided with plug-in slots, the three trapezoidal slots are provided with limit strips, and a pull-out handle is fixed to the outside of the limit strip.

[0013] A method for preparing a concrete pole with high crack resistance comprises the following steps: Step 1: Arrange multiple steel bars in a ring shape and insert them into the inner side of a stirrup and weld them to the stirrup to form a main steel frame. Then arrange multiple stirrups vertically in sequence and insert them into the outside of the main steel frame and weld them to fix them. Wrap the hollow spiral tube around the outer ring of the welded main steel bars and stirrups, and use steel wire rope to fix it and the stirrups together for support. Weld fixed steel rings at both ends of the main steel frame, and use multiple steel wires to fix the upper and lower ends of the anti-cracking net on the two fixed steel rings. Then, arrange multiple U-shaped steel frames vertically and weld them to the main steel frame. The internal support structure of the pole can be completed. Step 2: fit the first template and the second template together, and splice them together using a limit strip. Then put the completed internal support structure of the pole into the first template and the second template, and use the limit rings at the bottom of the first template and the second template to limit the support structure of the pole, so as to ensure that there is a certain gap between the support structure of the pole and the inner wall of the spliced ​​template. Then, clamp the arc template in the corresponding position and complete the splicing using two limit strips, and then pour the fully mixed concrete into the casting mold. Step 3: Use a vibrator to vibrate the concrete in the casting mold to ensure that it is evenly distributed and remove bubbles, enhance compactness, avoid gaps, maintain appropriate humidity and temperature for a few days, and then remove the casting mold when the concrete reaches the designed strength.

[0014] Compared with the prior art, the beneficial effects of the present invention are: When the temperature is low, adding sand into the hollow spiral tube increases the heat capacity of the pole and slows down the heat loss inside the pole, which helps maintain the temperature of the concrete and relieves the stress caused by temperature changes, thereby reducing the risk of cracks in the concrete pole under temperature fluctuations. When the temperature is high, adding water into the hollow spiral tube and utilizing the evaporation and conduction characteristics of water can reduce the overall temperature of the pole, prevent the degradation of material properties caused by high temperature, the thermal expansion and contraction of concrete and steel bars, extend the service life of the pole, prevent the pole from drying out and damage, and effectively improve the crack resistance of the pole. BRIEF DESCRIPTION OF THE DRAWINGS

[0015] Figure 1 It is a schematic diagram of the disassembly of the pole body and the casting mold in the present invention; Figure 2 It is a schematic diagram of the overall structure of the internal structure of the pole body in the present invention; Figure 3 for Figure 2 The local split diagram of ; Figure 4 for Figure 3 The enlarged schematic diagram of the middle A part; Figure 5 It is a schematic diagram of the overall structure of the pole body and the casting mold in the present invention; Figure 6 for Figure 5 Enlarged schematic diagram of part B in the middle.

[0016] 1. Casting mold; 11. First template; 12. First slot; 13. Second template; 14. Clip strip; 15. Second slot; 16. Arc template; 17. U-shaped hollow template; 18. Trapezoidal slot; 19. Plug slot; 110. Limit strip; 111. Pull-out handle; 2. The main body of the pole; 21. The main steel bar frame; 22. The stirrups; 23. The hollow spiral tube; 24. The steel wire rope; 25. The sealing plug; 26. The retaining steel bar ring; 27. The anti-cracking net; 28. The U-shaped steel bar frame; 29. ​​The vertical straight groove. DETAILED DESCRIPTION

[0017] The above and other technical features and advantages of the present invention are described in more detail below in conjunction with the accompanying drawings.

[0018] The present invention provides a technical solution: a concrete pole with high crack resistance, such as Figure 1 , Figure 5 and Figure 6 As shown, it includes a casting mold 1 and a pole body 2. The casting mold 1 is used to limit the shape and appearance of the concrete pole. The casting mold 1 includes a first template 11. A second template 13 is arranged on one side of the first template 11. The first template 11 and the second template 13 have the same shape and size. A raised limiting ring is arranged at the bottom of the inner side of both. The limiting ring plays a role in positioning the internal supporting structure of the pole body 2. A first slot 12 is opened on one side of the first template 11. A clamping strip 14 is fixed on one side of the second template 13, and the clamping strip 14 is clamped inside the first slot 12. The clamping of the two can align the first template 11 and the second template 13.

[0019] like Figure 1 , Figure 2 , Figure 5 and Figure 6 As shown, the other side of the first template 11 and the second template 13 are both provided with a second card slot 15, an arc-shaped template 16 is clamped between the insides of the two second card slots 15, a trapezoidal groove 18 is opened inside the first card slot 12 and the two second card slots 15, and a plug-in groove 19 is opened inside the card strip 14 and the arc-shaped template 16. When the card strip 14 is clamped in the first card slot 12 and the two sides of the arc-shaped template 16 are respectively clamped in the inner sides of the two second card slots 15, the opening of the trapezoidal groove 18 corresponds to and communicates with the plug-in groove 19. A limiting strip 110 is inserted into the inside of each of the three trapezoidal grooves 18. The shape of the limiting strip 110 is consistent with the shape of the groove body formed by splicing the trapezoidal groove 18 and the plug-in groove 19, and the size is adapted. A pull-out handle 111 is fixed to the outside of the limiting strip 110. A plurality of vertically arranged U-shaped hollow templates 17 are fixed to the outside of the arc template 16. The position arrangement of the U-shaped hollow template 17 corresponds to the U-shaped steel bar frame 28, and the U-shaped steel bar frame 28 is wrapped so that the concrete can wrap the U-shaped steel bar frame 28 to form it.

[0020] like Figure 1 , Figure 5 and Figure 6As shown, when the casting mold 1 is spliced, the first template 11 and the second template 13 are first arranged relative to each other, the clamping strip 14 is clamped into the first clamping groove 12, and a limit strip 110 is inserted into the bottom of the groove body corresponding to the trapezoidal groove 18 and the plug-in groove 19 spliced ​​together at this time, the first template 11 and the second template 13 are spliced ​​together, and after the supporting structure of the electric pole is placed, the two sides of the arc template 16 are placed in the two second clamping grooves 15 respectively, and the arc template 16 is fixed on the first template 11 and the second template 13 by using the other two limit strips 110 to complete the splicing of the casting mold 1. When disassembling the mold, it is only necessary to pull the three limit strips 110 out of the trapezoidal groove 18 to release the limit of the first template 11, the second template 13 and the arc template 16, and the three can be separated to expose the concrete pole formed inside.

[0021] like Figure 1-4 As shown, a main steel bar frame 21 is arranged inside the pole body 2, and the main steel bar frame 21 is formed by a plurality of steel bars arranged in a ring shape in sequence. A plurality of vertically arranged stirrups 22 are arranged outside the main steel bar frame 21, and a hollow spiral tube 23 is arranged outside the main steel bar frame 21. The hollow spiral tube 23 is fixed to the outside of the plurality of stirrups 22 by a plurality of steel wire ropes 24, so that the hollow spiral tube 23 is firmly supported on the outside of the main steel bar frame 21. Both ends of the hollow spiral tube 23 extend to the outside of the pole body 2. When the concrete pole is poured, two through holes are provided on the first template 11 for the two ends of the hollow spiral tube 23 to pass through, so as to prevent the two ends of the hollow spiral tube 23 from being poured with concrete, and both ends of the hollow spiral tube 23 are threadedly connected with sealing plugs 25, and the two sealing plugs 25 are provided with sealing plugs 25. They are all marked with double arrows, and the directions of the double arrows are marked with the words "open" and "close" respectively, so that the staff can know clearly how to rotate when performing a certain work. Retaining steel rings 26 are welded at both ends of the main steel frame 21, and an anti-cracking net 27 is fixed between the two retaining steel rings 26 by multiple steel wires. The anti-cracking net 27 is mainly used to control and prevent concrete from cracking under shrinkage, temperature changes or loads. It is made of high-strength polymers, steel wires or glass fibers, and its structure has good ductility and toughness. A plurality of U-shaped steel frames 28 are arranged on one side of the main steel frame 21, and the plurality of U-shaped steel frames 28 are arranged vertically in sequence. A vertical straight groove 29 is opened on one side of the anti-cracking net 27, and the plurality of U-shaped steel frames 28 are all on the inner side of the vertical straight groove 29.

[0022] like Figure 1-4As shown, a plurality of steel bars are first arranged in a ring shape and inserted into the inner side of a stirrup 22 and welded to the stirrup 22, and the main steel frame 21 is fixed to shape by a stirrup 22, and then a plurality of stirrups 22 are arranged vertically in sequence and inserted into the outside of the main steel frame 21 and welded and fixed, the hollow spiral tube 23 is wrapped around the outer ring of the welded main steel frame 21, and it is fixed to the stirrup 22 by a steel wire rope 24, and a retaining steel ring 26 is welded at both ends of the main steel frame 21, and the anti-cracking net 27 is fixed to the outside of the main steel frame 21 and the hollow spiral tube 23 by two retaining steel rings 26, so that it can be fixed and hidden in the concrete during the later pouring of concrete, and a plurality of U-shaped steel frames 28 are arranged vertically and welded to the main steel frame 21, and concrete is poured outside the supporting structure by using a pouring mold 1 to obtain an electric pole.

[0023] When pouring concrete, the concrete will bury the anti-crack net 27, the main steel frame 21, the hollow spiral tube 23, the stirrups 22, the retaining steel ring 26 and the U-shaped steel frame 28 inside the concrete, and use the main steel frame 21 to provide strength for the concrete pole, effectively improve the tensile strength of the pole, and enhance the bearing capacity of the overall structure. In addition, it can also increase the anti-destruction ability and stability of the pole. The anti-crack net 27 will be attached to the inside of the concrete pole during concrete pouring, and reduce the possibility of cracks in the concrete during the curing process by dispersing stress. It can also effectively control the development of micro cracks in the concrete and prevent the formation of large-scale cracks, thereby improving the crack resistance of the concrete pole. In periods of low temperature (such as winter), sand can be added to the hollow spiral tube 23, and the sand can be sucked from the hollow spiral tube 23 above. Pour sand into the port at one end and fill it up along the pipe. The sand has a certain thermal insulation effect, which increases the thermal capacity of the pole, thereby slowing down the loss of heat inside the pole, helping to maintain the temperature of the concrete and preventing the concrete from failing to fully solidify due to low temperature during winter construction. The presence of sand can help alleviate the stress caused by temperature changes, thereby reducing the risk of cracks in the concrete pole under temperature fluctuations. When sand insulation is not needed, sand can be released from the lower end port of the hollow spiral tube 23. In hot weather, water can be added to the hollow spiral tube 23. The evaporation and conduction characteristics of water can be used to reduce the overall temperature of the pole and prevent the degradation of material properties caused by high temperature. High temperature will cause thermal expansion and contraction of concrete and steel bars. Proper water cooling can reduce thermal stress, extend the service life of the pole, and prevent the pole from drying out and damage.

[0024] A method for preparing a concrete pole with high crack resistance comprises the following steps: Step 1: insert multiple steel bars into the inner side of a stirrup 22 in a ring shape and weld them to the stirrup 22 to form a main steel frame 21, then arrange multiple stirrups 22 vertically in sequence and insert them into the outside of the main steel frame 21 and weld them, wrap the hollow spiral tube 23 around the welded main steel frame 21 and the outer ring of the stirrup 22, use the steel wire rope 24 to fix it and the stirrup 22 together to support it, weld the fixed steel ring 26 at both ends of the main steel frame 21, and use multiple steel wires to fix the upper and lower ends of the anti-cracking net 27 to the two fixed steel rings 26, then arrange multiple U-shaped steel frames 28 vertically and weld them to the main steel frame 21, and the internal support structure of the pole can be completed; Step 2: fit the first template 11 and the second template 13 together, and splice them together using a limit strip 110, then put the completed internal support structure of the pole into the first template 11 and the second template 13, and use the limit rings at the bottom of the first template 11 and the second template 13 to limit the support structure of the pole, ensuring that there is a certain gap between the support structure of the pole and the inner wall of the spliced ​​template, and then clamp the arc template 16 at the corresponding position and complete the splicing using two limit strips 110, and then pour the fully mixed concrete into the casting mold 1; Step 3: Use a vibrator to vibrate the concrete in the casting mold 1 to ensure that it is evenly distributed and remove bubbles, enhance compactness, avoid the existence of gaps, maintain appropriate humidity and temperature for several days, and then the casting mold 1 can be demolded when the concrete reaches the designed strength.

[0025] The above description is only a preferred embodiment of the present invention, which is only illustrative and not restrictive of the present invention. Those skilled in the art understand that many changes, modifications, and even equivalences may be made to the present invention within the spirit and scope defined by the claims of the present invention, but all of them will fall within the scope of protection of the present invention.

Claims

1. A concrete pole with high crack resistance, characterized in that: include: A casting mold (1), wherein the casting mold (1) is used to define the shape and appearance of a concrete pole; An electric pole body (2), wherein a main steel bar frame (21) is arranged inside the electric pole body (2), wherein the main steel bar frame (21) is formed by a plurality of steel bars arranged in sequence in a ring shape, wherein a plurality of stirrups (22) arranged vertically are arranged outside the main steel bar frame (21), wherein a hollow spiral tube (23) is arranged outside the main steel bar frame (21), wherein the hollow spiral tube (23) is fixed to the outside of the plurality of stirrups (22) via a plurality of steel wire ropes (24), wherein both ends of the hollow spiral tube (23) extend to the outside of the electric pole body (2), and both ends of the hollow spiral tube (23) are threadedly connected with sealing plugs (25).

2. A concrete pole with high crack resistance as claimed in claim 1, characterized in that: Retaining steel bar rings (26) are welded to both ends of the main steel bar frame (21), and an anti-cracking net (27) is fixed between the two retaining steel bar rings (26) via a plurality of steel wires.

3. A concrete pole with high crack resistance as claimed in claim 2, characterized in that: A plurality of U-shaped steel bars (28) are arranged on one side of the main steel bar frame (21), and the plurality of U-shaped steel bar frames (28) are arranged vertically in sequence.

4. A concrete pole with high crack resistance as claimed in claim 3, characterized in that: A vertical straight groove (29) is provided on one side of the anti-cracking net (27), and the plurality of U-shaped steel bar frames (28) are all located inside the vertical straight groove (29).

5. A concrete pole with high crack resistance as claimed in claim 1, characterized in that: The casting mold (1) comprises a first template (11), a first slot (12) is provided on one side of the first template (11), a second template (13) is provided on one side of the first template (11), a clip (14) is fixed on one side of the second template (13), and the clip (14) is clipped inside the first slot (12).

6. A concrete pole with high crack resistance as claimed in claim 5, characterized in that: The first template (11) and the second template (13) are each provided with a second slot (15) on the other side, an arc-shaped template (16) is provided between the two second slots (15), and a plurality of vertically arranged U-shaped hollow templates (17) are fixed to the outside of the arc-shaped template (16).

7. A concrete pole with high crack resistance as claimed in claim 6, characterized in that: The first clamping slot (12) and the two second clamping slots (15) are each provided with a trapezoidal slot (18), the clamping strip (14) and the arc-shaped template (16) are each provided with a plug-in slot (19), and the three trapezoidal slots (18) are each provided with a limit strip (110) inserted therein, and a pull-out handle (111) is fixed to the outside of the limit strip (110).

8. A method for preparing a concrete pole with high crack resistance, characterized in that: The preparation method is applied to the concrete pole according to any one of claims 4 and 7, comprising the following steps: Step 1: insert multiple steel bars into the inner side of a stirrup (22) in a ring-like arrangement and weld them to the stirrup (22) to form a main steel bar frame (21), then arrange multiple stirrups (22) vertically in sequence and insert them into the outside of the main steel bar frame (21) and weld them to be fixed, wrap the hollow spiral tube (23) around the outer ring of the welded main steel bar (21) and stirrups (22), use a steel wire rope (24) to fix it and the stirrups (22) together to support it, weld fixed steel bar rings (26) at both ends of the main steel bar frame (21), and use multiple steel wires to fix the upper and lower ends of the anti-cracking net (27) to the two fixed steel bar rings (26), and then arrange multiple U-shaped steel bar frames (28) vertically and weld them to the main steel bar frame (21), and the internal support structure of the electric pole is completed; Step 2: fit the first template (11) and the second template (13) together, and splice the two using a limit strip (110), then place the completed internal support structure of the electric pole into the first template (11) and the second template (13), and use the limit rings at the bottom of the first template (11) and the second template (13) to limit the support structure of the electric pole, so as to ensure that there is a certain gap between the support structure of the electric pole and the inner wall of the spliced ​​templates, and then clamp the arc template (16) at the corresponding position and complete the splicing using two limit strips (110), and then pour the fully mixed concrete into the casting mold (1); Step 3: Use a vibrator to vibrate the concrete in the casting mold (1) to ensure that it is evenly distributed and remove bubbles, enhance compactness, avoid the existence of gaps, maintain appropriate humidity and temperature for several days, and then remove the casting mold (1) until the concrete reaches the designed strength.

Citation Information

Patent Citations

  • Concrete pole, production method, construction tool and construction method

    CN108131042A

  • Anti-freezing concrete pole with high collision resistance

    CN114000760A

  • Novel concurrent structure

    CN206616924U

  • Pouring mold for cement pole production

    CN214871533U

  • Curing of filament wound columns using a radiant heater

    WO1997022763A1