Chromium-aluminum-titanium-yttrium-based nitride composite coating for metal processing tool matrix

By depositing a composite coating of chromium, aluminum, titanium yttrium-based nitride on the metal processing tool matrix, the problem of insufficient hardness and high-temperature macrotoughness of high-steel tools in the prior art is solved, and high hardness suitable for cemented carbide and high-steel tools is achieved and low friction characteristics improve tool service life and machining efficiency.

CN118957494APending Publication Date: 2024-11-15POLESTAR PLASMA TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410988371.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-23
Publication Date
2024-11-15

AI Technical Summary

Technical Problem

The existing metal processing tool coatings are not suitable for high-steel tools and cannot meet the needs of high-steel tools in terms of hardness and high-temperature macro-toughness.

Method used

Using chromium aluminum titanium yttrium-based nitride composite coating, Ti, TiN, CrAlTiYN and CrAl layers are deposited successively on the surface of the metal processing tool substrate to form a composite coating with thickness and structure specificity, ensuring high hardness, low friction coefficient and high temperature macro toughness.

Benefits of technology

This coating is not only suitable for cemented carbide, but also for high-steel tools, which improves the hardness and high-temperature macro toughness of the tool, reduces friction, and extends the service life and processing efficiency of the tool.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

A base layer, a transition layer, a supporting layer and a protective layer are sequentially deposited on the surface of a metal processing hard alloy matrix, the base layer is a Ti layer with the thickness of 0.1-0.3 micron, the transition layer is a TiN layer with the thickness of 0.5-1.2 micron, the supporting layer is a CrAlTiYN layer with the thickness of 2-3 microns, and the protective layer is a chromium-aluminum-titanium-yttrium nitride layer with the thickness of 1-3 microns. And the protective layer is a CrAl layer with the thickness of 0.8-1.2 [mu] m. The high-hardness and high-impact-resistance aluminum alloy material has the advantages of high hardness, high binding force, high impact resistance and extremely low friction coefficient.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to a PVD vacuum ion plating structure, and in particular relates to a chromium-aluminum-titanium-yttrium-based nitride composite coating for a metal processing tool substrate. Background Art

[0002] Metal processing tool coatings have been widely used in existing mechanical processing applications. Coated tools are coated with a thin layer of refractory metal or non-metallic compound with good wear resistance on the surface of cemented carbide or high-speed steel (HSS) substrate with good strength and toughness by vapor deposition method. They can also be coated on superhard material blades such as ceramics, diamond and cubic boron nitride. The coating acts as a chemical barrier and thermal barrier, reducing the diffusion and chemical reaction between the tool and the workpiece, thereby reducing the wear of the substrate. Coated tools have the characteristics of high surface hardness, good wear resistance, stable chemical properties, heat and oxidation resistance, low friction coefficient and low thermal conductivity. When cutting, the life of uncoated tools can be increased by more than 3 to 5 times, the cutting speed can be increased by 20% to 70%, the processing accuracy can be increased by 0.5 to 1 level, and the tool consumption cost can be reduced by 20% to 50%.

[0003] Because the surface coating material has high hardness and wear resistance, and is resistant to high temperatures. Therefore, compared with uncoated tools (blades), coated tools allow for higher cutting speeds, thereby improving cutting efficiency; or can increase tool life at the same cutting speed. Since the friction coefficient between the coating material and the material being processed is small, the cutting force of the coated tool is less than that of the uncoated tool. The surface quality of the parts processed with the coated tool is better. Due to the good comprehensive performance of the coated tool, the coated carbide blade has good versatility, but it is not suitable for high-steel tools. Summary of the invention

[0004] The purpose of the present invention is to provide a chromium-aluminum-titanium-yttrium-based nitride composite coating for metal processing tool substrates. The coating is not only suitable for cemented carbide, but also for high-steel tools, and has the characteristics of high hardness, high-temperature macro-toughness, low friction coefficient, etc.

[0005] To achieve the above object, the present invention adopts the following technical solution:

[0006] A chromium-aluminum-titanium-yttrium-based nitride composite coating for a metal processing tool substrate, wherein a base layer, a transition layer, a support layer and a protective layer are sequentially deposited on the surface of the metal processing cemented carbide substrate, wherein the base layer is a Ti layer with a thickness of 0.1 to 0.3 μm, the transition layer is a TiN layer with a thickness of 0.5 to 1.2 μm, the support layer is a CrAlTiYN layer with a thickness of 2 to 3 μm, and the protective layer is a CrAl with a thickness of 0.8 to 1.2 μm.

[0007] Further, the composite coating is prepared by the following steps:

[0008] (1) Glow cleaning: Ar gas is introduced, the vacuum degree of the furnace chamber is 0.01-0.5 Pa, a negative bias voltage of 400-1000 V is applied to the substrate, and the glow cleaning is performed for 10-35 min;

[0009] (2) adjusting the substrate negative bias voltage to 400-600 V, introducing Ar gas with a gas flow rate of 50-100 sccm, turning on two Ti targets, adjusting the target current to 100-250 A, and bombarding the substrate with high energy Ti ions for 1-10 min to form a Ti base layer;

[0010] (3) N gas is introduced at a gas flow rate of 800 sccm to 1000 sccm, the gas pressure in the furnace is controlled at 2 to 3 Pa, the pulse bias voltage is 80 to 150 V, the duty cycle is 40% to 60%, two Ti targets are turned on, the target current is 125 to 130 A, and the TiN transition layer is deposited for 30 minutes;

[0011] (4) N gas was introduced at a gas flow rate of 800 sccm to 1000 sccm, and the gas pressure in the furnace was controlled at 2 to 3 Pa, the pulse bias voltage was 80 to 150 V, the duty cycle was 40% to 60%, two CrAlTiY targets were turned on, the target current was 125 to 130 A, and the CrAlTiYN support layer was formed by deposition for 90 min;

[0012] (5) N gas is introduced at a gas flow rate of 800 sccm to 1000 sccm, the gas pressure in the furnace is controlled at 2 to 3 Pa, the pulse bias is 80 to 150 V, the duty cycle is 40% to 60%, two CrAl targets are turned on, the target current is 125 to 130 A, and the CrAl protective layer is formed after deposition for 30 minutes.

[0013] The present invention uses Ti as the base, and the Ti layer has an excellent bonding material, which ensures that the ultra-high hardness surface layer structure has good bonding with the mold / punch base material, and the vertical impact force and shear force in metal machining can be well absorbed, avoiding the delamination of the base material and the surface ultra-high hardness composite structure. Then TiN is covered as a transition layer, CrAlTiYN is used as a supporting layer, and the outermost surface is CrAlN. This surface coating has the characteristics of high hardness, high-temperature macro-toughness, and low friction coefficient. DETAILED DESCRIPTION

[0014] The present embodiment provides a chromium-aluminum-titanium-yttrium-based nitride composite coating for a metal processing tool substrate, comprising the following steps:

[0015] (1) When performing glow cleaning, the gas introduced is Ar gas, the vacuum degree of the furnace chamber is 0.01-0.5 Pa, the substrate is subjected to a negative bias voltage of 400-1000 V, and the glow cleaning is performed for 10-35 minutes;

[0016] (2) Adjust the negative bias voltage of the substrate to 400-600 V, introduce Ar gas with a gas flow rate of 50-100 sccm, turn on two Ti targets, adjust the target current to 100-250 A, bombard the substrate with high energy Ti ions for 1-10 min to activate the substrate surface, and simultaneously grow a surface activation layer within 0.1-0.3 μm.

[0017] (3) The amount of N2 gas introduced is 800 sccm to 1000 sccm, the gas pressure in the furnace is controlled at 2 to 3 Pa, the pulse bias is 80 to 150 V, the duty cycle is 40% to 60%, two Ti targets are turned on, the current is 125 to 130 A, and a TiN transition layer is obtained. The deposition time is adjusted according to the thickness and the impact strength requirements. The greater the impact strength, the appropriate increase in thickness. The thickness is usually 0.5-1.2 μm, and the deposition time is about 30 minutes.

[0018] (4) N gas is introduced at a gas volume of 800 sccm to 1000 sccm; the gas pressure in the furnace is controlled at 2 to 3 Pa, the pulse bias is 80 to 150 V, the duty cycle is 40% to 60%, two CrAlTiY targets are turned on, the current is 125 to 130 A, and a CrAlTiYN support layer is obtained, which is usually 2 to 3 μm thick and the deposition time is about 90 minutes.

[0019] (5) N gas is introduced at a gas volume of 800 sccm to 1000 sccm; the gas pressure in the furnace is controlled at 2 to 3 Pa, the pulse bias is 80 to 150 V, the duty cycle is 40% to 60%, two CrAl targets are turned on, the current is 125 to 130 A, and a surface layer is obtained, which is usually 0.8 to 1.2 μm thick and the deposition time is about 30 minutes.

[0020] The above description is only a preferred implementation manner of the present invention, but the protection scope of the present invention is not limited thereto, and any modification and replacement based on the technical solution and inventive concept provided by the present invention should be included in the protection scope of the present invention.

Claims

1. A chromium-aluminum-titanium-yttrium-based nitride composite coating for a metalworking tool substrate, characterized in that: A base layer, a transition layer, a support layer and a protective layer are sequentially deposited on the surface of the metal processing cemented carbide substrate, wherein the base layer is a Ti layer with a thickness of 0.1 to 0.3 μm, the transition layer is a TiN layer with a thickness of 0.5 to 1.2 μm, the support layer is a CrAlTiYN layer with a thickness of 2 to 3 μm, and the protective layer is a CrAl layer with a thickness of 0.8 to 1.2 μm.

2. The chromium-aluminum-titanium-yttrium-based nitride composite coating for a metalworking tool substrate according to claim 1, characterized in that: The composite coating was prepared by the following steps: (1) Glow cleaning: Ar gas is introduced, the vacuum degree of the furnace chamber is 0.01-0.5 Pa, a negative bias voltage of 400-1000 V is applied to the substrate, and the glow cleaning is performed for 10-35 min; (2) adjusting the substrate negative bias voltage to 400-600 V, introducing Ar gas with a gas flow rate of 50-100 sccm, turning on two Ti targets, adjusting the target current to 100-250 A, and bombarding the substrate with high energy Ti ions for 1-10 min to form a Ti base layer; (3) N gas is introduced at a gas flow rate of 800 sccm to 1000 sccm, the gas pressure in the furnace is controlled at 2 to 3 Pa, the pulse bias voltage is 80 to 150 V, the duty cycle is 40% to 60%, two Ti targets are turned on, the target current is 125 to 130 A, and the TiN transition layer is deposited for 30 minutes; (4) N gas was introduced at a gas flow rate of 800 sccm to 1000 sccm, and the gas pressure in the furnace was controlled at 2 to 3 Pa, the pulse bias voltage was 80 to 150 V, the duty cycle was 40% to 60%, two CrAlTiY targets were turned on, the target current was 125 to 130 A, and the CrAlTiYN support layer was formed by deposition for 90 min; (5) N gas is introduced at a gas flow rate of 800 sccm to 1000 sccm, the gas pressure in the furnace is controlled at 2 to 3 Pa, the pulse bias is 80 to 150 V, the duty cycle is 40% to 60%, two CrAl targets are turned on, the target current is 125 to 130 A, and the CrAl protective layer is formed after deposition for 30 minutes.