Reaction cavity structure and deposition equipment

By designing a structure that is deposited and cured in the same reaction cavity in semiconductor manufacturing, the problem of insufficient filling efficiency and reliability of high-deep aspect ratio structures in FCVD technology is solved, and efficient and reliable preparation of target material layer is achieved.

CN118957546AActive Publication Date: 2024-11-15JIANGSU SHOUXIN SEMICON TECH CO LTD
View PDF 11 Cites 0 Cited by

Patent Information

Application Number
CN202411362113.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-27
Publication Date
2024-11-15
Estimated Expiration
2044-09-27

AI Technical Summary

Technical Problem

In the existing semiconductor manufacturing, the efficiency and reliability of FCVD technology to prepare the target material layer need to be improved, especially when filling the high-deep aspect ratio structure, the efficiency and reliability of the deposition equipment are insufficient, resulting in low efficiency in the preparation process and prone to defects.

Method used

A reaction cavity structure is designed in which the deposited film layer and the cured film layer are carried out in the same reaction cavity, the curing mechanism moves in the vertical direction, is located in the receiving cavity during the deposited film layer, and moves to the reaction after the film layer is deposited. In the cavity, the film layer is provided with curing energy to convert it into a target material layer, avoiding the step of moving the wafer to other chambers, saving time and improving reliability.

Benefits of technology

The preparation efficiency and reliability of the target material layer are improved, defects caused by wafer movement are reduced, preparation time is saved, and the curing effect of the upper and lower parts of the target material layer is consistent.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118957546A_ABST
    Figure CN118957546A_ABST
Patent Text Reader

Abstract

The embodiment of the invention relates to the field of semiconductor manufacturing, and provides a reaction cavity structure and deposition equipment, the reaction cavity structure comprises a reaction cavity body, the reaction cavity body internally comprises a reaction cavity and a containing cavity communicated with the reaction cavity in the vertical direction, and the reaction cavity is located above the containing cavity; the reaction cavity structure further comprises an air inlet mechanism, an extraction opening, a carrying table, a curing mechanism and a controller, the curing mechanism is arranged in the containing cavity and can move up and down in the reaction cavity in the vertical direction, and the curing mechanism is used for providing curing energy for the film layer so as to convert the film layer into a target material layer; the controller is used for controlling the curing mechanism to move in the vertical direction so that the curing mechanism can be located in the containing cavity during film layer deposition, controlling the curing mechanism to move into the reaction cavity in the vertical direction after film layer deposition and controlling the curing mechanism to provide curing energy for the film layer. The embodiment of the invention at least can improve the efficiency and reliability of preparing the target material layer.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The embodiments of the present disclosure relate to the field of semiconductor manufacturing, and in particular to a reaction chamber structure and deposition equipment. Background Art

[0002] In the semiconductor industry, as the integration requirements of devices become higher and higher, the size of devices is continuously reduced to improve the integration density of various electronic components (for example, transistors, diodes, resistors, capacitors, etc.). Therefore, semiconductor devices need to have a high aspect ratio structure, and insulating materials can be used to fill the gaps between high aspect ratio structures. Among them, flowable chemical vapor deposition (FCVD) is a preparation method for materials suitable for filling high aspect ratio structures. It can form a film layer with relatively good fluidity on the wafer, and then use a curing mechanism to provide curing energy to convert the film layer on the wafer into a target material layer. Since the target material layer prepared by FCVD exhibits good conformality, step coverage and the ability to fully fill high aspect ratio spaces, FCVD can be used to fill high aspect ratio gaps in semiconductor devices.

[0003] However, the efficiency and reliability of deposition equipment currently used in FCVD for preparing target material layers need to be improved. Summary of the invention

[0004] The embodiments of the present disclosure provide a reaction chamber structure and a deposition device, which can at least improve the efficiency and reliability of preparing a target material layer.

[0005] According to some embodiments of the present disclosure, on the one hand, the embodiments of the present disclosure provide a reaction chamber structure, including: a reaction chamber body, wherein the reaction chamber body includes a reaction chamber and a accommodating chamber connected to the reaction chamber in a vertical direction, and the reaction chamber is located above the accommodating chamber; an air intake mechanism, wherein the air intake mechanism is arranged at the top of the reaction chamber, the air intake mechanism has an air intake hole and an air intake channel connected to the air intake hole, the air intake channel is connected to the reaction chamber, and the air intake hole is used to connect to an air intake pipe for providing gas; an air suction port, wherein the air suction port is connected to the reaction chamber; a carrier, wherein the carrier is used to carry a wafer, and the carrier is used to carry a wafer. The carrier is located in the reaction chamber; the curing mechanism is arranged in the receiving chamber and can move up and down along the vertical direction in the reaction chamber, and the curing mechanism is used to provide curing energy for the film layer to convert the film layer into a target material layer; the controller is connected to the curing mechanism and is used to control the curing mechanism to move in the vertical direction so that the curing mechanism is located in the receiving chamber during the deposition of the film layer, and after the deposition of the film layer, the curing mechanism is controlled to move in the vertical direction to the reaction chamber, and the curing mechanism is controlled to provide the curing energy for the film layer.

[0006] In some embodiments, the controller controls the solidification mechanism to move alternately in the receiving chamber and the reaction chamber.

[0007] In some embodiments, a cross-sectional area of ​​the accommodating chamber perpendicular to the vertical direction is smaller than a cross-sectional area of ​​the reaction chamber perpendicular to the vertical direction.

[0008] In some embodiments, the accommodating chamber is an annular chamber connected to the bottom of the reaction chamber; the solidification mechanism is circumferentially arranged in the accommodating chamber, or the solidification mechanism includes a plurality of solidifiers, and the solidifiers are circumferentially arranged in the accommodating chamber.

[0009] In some embodiments, the accommodating chamber includes a plurality of circumferentially arranged sub-accommodating chambers, each of which is connected to the bottom of the reaction chamber, and the curing mechanism includes a plurality of curing devices, which are disposed in the sub-accommodating chambers.

[0010] In some embodiments, the reaction chamber structure also includes: a baffle, which is located in the receiving chamber, and is retractable in the horizontal direction. The baffle is connected to the controller. During the deposition of the film layer, the controller controls the baffle to stretch so that the baffle blocks the passage between the reaction chamber and the receiving chamber. After the deposition of the film layer, the controller controls the baffle to shrink so that the baffle does not block the movement of the curing mechanism in the vertical direction.

[0011] In some embodiments, the curing mechanism is a light source curing mechanism, which is used to provide a light beam to provide the curing energy for the film layer; the reaction chamber structure also includes: a reflector, which is located at the top of the curing mechanism, and the side of the reflector facing away from the air intake mechanism is a reflective surface, which is used to reflect the light beam, and the reflector is retractable in the horizontal direction. The reflector is connected to the controller, and during the curing of the film layer, the controller is used to control the stretching of the reflector so that at least part of the reflective surface faces the wafer. After curing the film layer, the controller is used to control the contraction of the reflector so that the reflector does not block the movement of the curing mechanism in the vertical direction.

[0012] In some embodiments, the curing mechanism includes at least one movable curing device; the reaction chamber structure also includes: a first telescopic mechanism, the first telescopic mechanism is arranged in the accommodating chamber, the first telescopic mechanism is telescopic in the vertical direction, the first telescopic mechanism is connected to the curing mechanism, the first telescopic mechanism is connected to the controller, after depositing the film layer, the controller controls the first telescopic mechanism to stretch in the vertical direction to drive the curing mechanism to move into the reaction chamber to provide the curing energy for the film layer, after curing the film layer, the controller controls the first telescopic mechanism to shrink in the vertical direction to drive the curing mechanism to move into the accommodating chamber; a second telescopic mechanism, the first telescopic mechanism is connected to the curing mechanism, the first telescopic mechanism is connected to the controller, after depositing the film layer, the controller controls the first telescopic mechanism to stretch in the vertical direction to drive the curing mechanism to move into the reaction chamber to provide the curing energy for the film layer, after curing the film layer, the controller controls the first telescopic mechanism to shrink in the vertical direction to drive the curing mechanism to move into the accommodating chamber; The mechanism is connected to the second telescopic mechanism, the second telescopic mechanism is telescopic in the horizontal direction, the second telescopic mechanism is connected to the movable solidifier, and the second telescopic mechanism is connected to the controller. When the movable solidifier is located in the reaction chamber, the controller controls the second telescopic mechanism to stretch and drive the movable solidifier to move so that the movable solidifier is located directly above the wafer, and the controller controls the movable solidifier to provide the curing energy. After curing the film layer, the controller controls the movable solidifier to stop providing the curing energy, and the controller controls the second telescopic mechanism to contract so that the movable solidifier does not block the first telescopic mechanism from moving in the vertical direction.

[0013] In some embodiments, the curing mechanism includes at least one rotatable curing device; the reaction chamber structure also includes: a first telescopic mechanism, the first telescopic mechanism is arranged in the reaction chamber, the first telescopic mechanism is telescopic in the vertical direction, the first telescopic mechanism is connected to the curing mechanism, the first telescopic mechanism is connected to the controller, after depositing the film layer, the controller controls the first telescopic mechanism to stretch in the vertical direction to drive the curing mechanism to move into the reaction chamber to provide the curing energy for the film layer, after curing the film layer, the controller controls the first telescopic mechanism to shrink in the vertical direction to drive the curing mechanism to move into the accommodating chamber; a rotating fixing member, the rotating fixing member The fixed part is connected to the first telescopic mechanism, and the rotating fixed part is rotatably connected to the rotatable curing device; the controller is connected to the rotatable curing device, and when the curing mechanism is located in the reaction chamber, the controller controls the rotatable curing device to rotate around the rotating fixed part to be parallel to the horizontal direction, so that at least a part of the rotatable curing device is located directly above the wafer, and the controller controls the rotatable curing device to provide the curing energy. After curing the film layer, the controller controls the rotatable curing device to stop providing the curing energy, and the controller controls the rotatable curing device to rotate around the rotating fixed part to be parallel to the vertical direction, so that the rotatable curing device fits the first telescopic mechanism.

[0014] According to some embodiments of the present disclosure, another aspect of the present disclosure further provides a deposition device, comprising the reaction chamber structure described in any of the above embodiments.

[0015] The technical solution provided by the embodiments of the present disclosure has at least the following advantages:

[0016] The technical solution of the reaction chamber structure provided in the embodiment of the present disclosure includes: a reaction chamber body, an air intake mechanism, an air suction port, a carrier, a curing mechanism and a controller. The reaction chamber body includes a reaction chamber and a accommodating chamber connected to the reaction chamber in the vertical direction, and the reaction chamber is located above the accommodating chamber. The air intake mechanism is arranged at the top of the reaction chamber, and the air intake mechanism has an air intake hole and an air intake channel connected to the air intake hole, the air intake channel is connected to the reaction chamber, and the air intake hole is used to connect to the air intake pipe for providing gas; the air suction port, the air suction port is connected to the reaction chamber. The carrier is used to carry the wafer, and the carrier is located in the reaction chamber so that a film layer is deposited on the surface of the wafer. The curing mechanism is arranged in the accommodating chamber, and can move up and down in the vertical direction in the reaction chamber. The curing mechanism is used to provide curing energy for the film layer to convert the film layer into a target material layer. The controller is connected to the curing mechanism, and is used to control the curing mechanism to move in the vertical direction, so that the curing mechanism is located in the accommodating chamber during the deposition of the film layer, and the curing mechanism is controlled to move in the vertical direction into the reaction chamber after the deposition of the film layer, and the curing mechanism is controlled to provide curing energy for the film layer. In the reaction chamber structure, the deposition of the film layer and the curing of the film layer are carried out in the same reaction chamber. During the deposition of the film layer, the curing mechanism is located in the accommodating chamber. After the film layer is deposited, the curing mechanism moves in the vertical direction into the reaction chamber to provide curing energy for the film layer to convert it into a target material layer. In this process, there is no need to add steps such as moving the wafer to other chambers in the related technology. On the one hand, a lot of time can be saved, thereby improving the preparation efficiency of the target material layer. On the other hand, it can also avoid the increase of defects due to the movement of the wafer between different chambers, thereby improving the reliability of preparing the target material layer. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] One or more embodiments are exemplarily illustrated by pictures in the corresponding drawings, and these exemplified descriptions do not constitute a limitation on the embodiments. Unless otherwise specified, the pictures in the drawings do not constitute a scale limitation. In order to more clearly illustrate the embodiments of the present disclosure or the technical solutions in the traditional technology, the drawings required for use in the embodiments are briefly introduced below. Obviously, the drawings described below are only some embodiments of the present disclosure. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0018] Figure 1 A schematic diagram of a deposition chamber structure in the related art;

[0019] Figure 2 A structural schematic diagram of a curing cavity structure in the related art;

[0020] Figure 3 A schematic diagram of a reaction chamber structure in the related art;

[0021] Figure 4 A schematic cross-sectional structure diagram of a first reaction chamber structure provided in some embodiments of the present disclosure in which a curing mechanism is located in a containing chamber;

[0022] Figure 5 A schematic cross-sectional structure diagram of a first reaction chamber structure provided in some embodiments of the present disclosure in which a curing mechanism is located in a reaction chamber;

[0023] Figure 6 A schematic cross-sectional structure diagram of a second reaction chamber structure provided in some embodiments of the present disclosure in which a curing mechanism is located in a containing chamber;

[0024] Figure 7 A schematic cross-sectional structure diagram of an air intake mechanism provided in some embodiments of the present disclosure;

[0025] Figure 8 A schematic diagram of a top view of the structure of the accommodating cavity and the curing mechanism provided in some embodiments of the present disclosure;

[0026] Fig. 9 Another schematic diagram of a top view of the accommodating cavity and the curing mechanism provided in some embodiments of the present disclosure;

[0027] Fig.10 A schematic diagram of another top view of the accommodating cavity and the curing mechanism provided in some embodiments of the present disclosure;

[0028] Fig.11 A schematic cross-sectional structure diagram of a baffle in a retracted state in a third reaction chamber structure provided in some embodiments of the present disclosure;

[0029] Fig.12 A schematic cross-sectional structure diagram of a baffle in a stretched state in a third reaction chamber structure provided in some embodiments of the present disclosure;

[0030] Fig.13 A schematic cross-sectional structure diagram of a telescopic member in a contracted state in a fourth reaction chamber structure provided in some embodiments of the present disclosure;

[0031] Fig.14 A schematic cross-sectional structure diagram of a telescopic member in a stretched state in a fourth reaction chamber structure provided in some embodiments of the present disclosure;

[0032] Fig.15 A schematic cross-sectional structure diagram of a reflector in a retracted state in a fifth reaction chamber structure provided in some embodiments of the present disclosure;

[0033] Fig.16 A schematic cross-sectional structure diagram of a reflector in a stretched state in a fifth reaction chamber structure provided in some embodiments of the present disclosure;

[0034] Fig.17A schematic cross-sectional structure diagram of a second telescopic mechanism in a reaction chamber structure in another embodiment of the present disclosure in a contracted state;

[0035] Fig.18 A schematic cross-sectional structure diagram of a second telescopic mechanism in a reaction chamber structure in a stretched state provided by other embodiments of the present disclosure;

[0036] Fig.19 A schematic diagram of a cross-sectional structure of a rotatable solidifier parallel to the vertical direction in a reaction chamber structure provided by some other embodiments of the present disclosure;

[0037] Fig. 20 A schematic diagram of a cross-sectional structure in which a rotatable solidifier is parallel to the horizontal direction in a reaction chamber structure provided in some other embodiments of the present disclosure;

[0038] Fig.21 A schematic cross-sectional structure diagram of a retractable solidifier in a reaction chamber structure in some further embodiments of the present disclosure in a retracted state;

[0039] Fig. 22 A schematic diagram of the cross-sectional structure of a retractable solidifier in a stretched state in a reaction chamber structure provided in some further embodiments of the present disclosure. DETAILED DESCRIPTION

[0040] Figure 1 is a structural schematic diagram of a deposition chamber structure in the related art, Figure 2 It is a structural schematic diagram of a curing cavity structure in the related technology.

[0041] Combined with reference Figure 1 and Figure 2 The reaction chamber structure in the related art includes a deposition chamber structure 100 and a curing chamber structure 101. The deposition chamber structure 100 includes a deposition chamber 110, a first vacuum transmission chamber 120, a first loading chamber 130, and a first wafer boat 140 for placing the wafer 11; the curing chamber structure 101 includes a curing chamber 111, a second vacuum transmission chamber 121, a second loading chamber 131, and a second wafer boat 141 for placing the wafer 11. After the film layer of the wafer 11 is deposited in the deposition chamber 110, the wafer 11 needs to pass through the first vacuum transmission chamber 120, the first loading chamber 130, the first wafer boat 140, the second wafer boat 141, the second loading chamber 131, and the second vacuum transmission chamber 121 in sequence and then move to the curing chamber 111, so that the film layer on the surface of the wafer 11 can receive curing energy in the curing chamber 111 and be converted into a target material layer.

[0042] In this reaction chamber structure, the deposition chamber 110 for depositing the film layer and the curing chamber 111 for curing the film layer are located on two platforms. After the wafer 11 is deposited in the deposition chamber 110, it takes a lot of time to move through other chambers to the curing chamber 111, which makes the efficiency of preparing the target material layer on the surface of the wafer 11 low.

[0043] Figure 3 It is a structural schematic diagram of a reaction chamber structure in the related technology.

[0044] refer to Figure 3 The reaction chamber structure in the related art includes a deposition chamber 200, a vacuum transfer chamber 201, a curing chamber 202, a loading chamber 203, and a wafer boat 204 for placing the wafer 11. After the wafer 11 is deposited in the deposition chamber 200 to deposit a film layer on the surface of the wafer 11, the wafer 11 needs to pass through the vacuum transfer chamber 201 and move to the curing chamber 202, so that the film layer on the surface of the wafer 11 can receive curing energy in the curing chamber 202 and be converted into a target material layer.

[0045] In this reaction chamber structure, although the deposition chamber 200 for depositing the film layer and the curing chamber 202 for curing the film layer are located on the same platform, after the film layer is deposited in the deposition chamber 200, the wafer 11 still needs to be moved to the curing chamber 202. A lot of time will be consumed during the movement, resulting in low efficiency in preparing the target material layer on the surface of the wafer 11.

[0046] In summary, in the reaction chamber structure in the current related art, the deposition chamber and the curing chamber are two independent chambers. After the film layer is deposited in the deposition chamber, the wafer needs to be moved to another chamber so that the film layer receives the curing energy and is converted into the target material layer. A lot of time will be consumed during the movement, making the efficiency of preparing the target material layer on the wafer surface low. In addition, the movement of the wafer in different chambers may increase defects in the wafer and / or the target material layer, making the reliability of preparing the target material layer low.

[0047] Therefore, the efficiency and reliability of the target material layer prepared by the reaction chamber structure in the related art need to be improved.

[0048] In the reaction chamber structure provided in the embodiment of the present disclosure, the deposition of the film layer and the curing of the film layer are carried out in the same reaction chamber. During the deposition of the film layer, the curing mechanism is located in the accommodating chamber. After the film layer is deposited, the curing mechanism moves into the reaction chamber in a vertical direction to provide curing energy for the film layer to convert it into a target material layer. In this process, there is no need to add steps such as moving the wafer to other chambers in the related technology. On the one hand, a lot of time can be saved, thereby improving the preparation efficiency of the target material layer. On the other hand, it can also avoid the increase of defects due to the movement of the wafer between different chambers, thereby improving the reliability of preparing the target material layer.

[0049] The following will describe the various embodiments of the present disclosure in detail with reference to the accompanying drawings. However, it will be appreciated by those skilled in the art that in the various embodiments of the present disclosure, many technical details are provided in order to enable the reader to better understand the present disclosure. However, even without these technical details and various changes and modifications based on the following embodiments, the technical solutions claimed in the present disclosure can be implemented.

[0050] Figure 4 A schematic cross-sectional structure diagram of a first reaction chamber structure provided in some embodiments of the present disclosure in which a curing mechanism is located in a containing chamber, Figure 5 A schematic cross-sectional structure diagram of a first reaction chamber structure in which a solidifying mechanism is located within a reaction chamber in some embodiments of the present disclosure.

[0051] Combined with reference Figure 4 and Figure 5 The reaction chamber structure includes a reaction chamber body 300, an air intake mechanism 301, an air extraction port 302, a stage 303, a curing mechanism 304, and a controller (not shown). The reaction chamber body 300 includes a reaction chamber 310 and a receiving chamber 320 connected to the reaction chamber 310 in the vertical direction Y, and the reaction chamber 310 is located above the receiving chamber 320. The air intake mechanism 301 is arranged at the top of the reaction chamber 310, and the air intake mechanism 301 has an air intake hole 311 and an air intake channel 321 connected to the air intake hole 311, and the air intake channel 321 is connected to the reaction chamber 310, and the air intake hole 311 is used to connect the air intake pipe for providing gas. The air extraction port 302 is connected to the reaction chamber 310. The stage 303 is used to carry the wafer 11, and the stage 303 is located in the reaction chamber 310. The curing mechanism 304 is disposed in the containing chamber 320 and can move up and down in the reaction chamber 310 along the vertical direction Y. The curing mechanism 304 is used to provide curing energy for the film layer to convert the film layer into a target material layer. The controller is connected to the curing mechanism 304 and is used to control the curing mechanism 304 to move in the vertical direction Y so that the curing mechanism 304 is located in the containing chamber 320 during the deposition of the film layer, and controls the curing mechanism 304 to move in the vertical direction Y to the reaction chamber 310 after the deposition of the film layer, and controls the curing mechanism 304 to provide curing energy for the film layer.

[0052] The reaction chamber structure is used to generate a target material layer on the surface of the wafer 11 . Specifically, the reaction chamber body 300 is used to generate a target material layer on the surface of the wafer 11 .

[0053] The wafer 11 may be a silicon wafer, a germanium wafer, or a silicon-germanium wafer, etc. The wafer 11 may have a high aspect ratio (aspect ratio greater than 8:1) groove, and the opening of the groove is narrower than 20nm; or, the wafer 11 may have a groove with an aspect ratio less than or equal to 8:1, and the opening of the groove is greater than or equal to 20nm; or, the wafer 11 may have a smooth surface (i.e., no groove).

[0054] The film layer is a thin film with good fluidity. After the film layer is deposited, it needs to be solidified to make it densified and transformed into the target material layer.

[0055] For example, when generating a fluid silicon oxide film, the precursors for generating the film layer may be TSA (Trisilylamine) and NH 3 (ammonia), solidified gas is O 3 , O 2 For example, when forming a positive stress silicon nitride film, the reaction gas may include SiH 4 、N 2 NH 3 The solidifying gas may be an inert gas such as He or Ar.

[0056] The target material layer may be silicon oxide, or materials with a dielectric constant greater than 3.9 such as silicon nitride and silicon oxynitride, or materials with a dielectric constant less than 3.9 such as fluorine-doped silicon dioxide, carbon-doped silicon dioxide, and fluorocarbon compounds.

[0057] The reaction chamber 310 is used to provide a reaction space for generating a target material layer on the surface of the wafer 11, and the accommodating chamber 320 is used to place the curing mechanism 304. Specifically, when the curing mechanism 304 is located in the accommodating chamber 320, the reaction gas enters the reaction chamber 310 through the air intake mechanism 301, and deposits a film layer on the surface of the wafer 11. When the film layer deposition is completed, the controller controls the curing mechanism 304 to move into the reaction chamber 310 in the vertical direction, and controls the curing mechanism 304 to provide curing energy for the film layer, so that the film layer is converted into a target material layer.

[0058] Figure 6 A schematic cross-sectional structure diagram of a second reaction chamber structure provided in some embodiments of the present disclosure in which a curing mechanism is located within a containing chamber.

[0059] refer to Figure 6 In some embodiments, the cross-sectional area of ​​the accommodating chamber 320 perpendicular to the vertical direction Y may be smaller than the cross-sectional area of ​​the reaction chamber 310 perpendicular to the vertical direction Y. Since the accommodating chamber 320 is mainly used to place the curing mechanism 304, the cross-sectional area of ​​the accommodating chamber 320 perpendicular to the vertical direction Y may be smaller than the cross-sectional area of ​​the reaction chamber 310 perpendicular to the vertical direction Y, so that the overall volume of the reaction chamber structure can be smaller, which is conducive to saving the manufacturing cost of the reaction chamber structure.

[0060] In other embodiments, the cross-sectional area of ​​the accommodating chamber 320 perpendicular to the vertical direction Y may also be greater than or equal to the cross-sectional area of ​​the reaction chamber 310 perpendicular to the vertical direction Y.

[0061] The gas inlet mechanism 301 is used to provide gas to the reaction chamber 310 .

[0062] The gas may be one or more of a reaction gas, a cleaning gas or a curing gas. The reaction gas reacts on the surface of the wafer 11 to form a film layer, the curing gas is the gas required for the film layer to receive curing energy and transform into a target material layer, and the cleaning gas is used to clean the byproducts on the sidewall of the reaction chamber structure.

[0063] In one example, the reactant gas may include H 2 N(SiH 3 )、HN(SiH 3 ) 2 、N(SiH 3 ) 3 、HMDSO(C 6 H 18 Si 2 O, hexamethyldisiloxane) or other materials containing SiH 3 The reaction gas may also include NH 3 、N 2 H 4 、N 2 , H 2 At least one of the above, the reaction gas may also include other 2 -group gas, the solidifying gas may include O 3 , O 2 , H 2 O、N 2 O、NO 2 The solidifying gas may also be an inert gas such as He or Ar.

[0064] It is understandable that the parameters such as the composition and content of the reaction gas, cleaning gas and curing gas can be adjusted according to actual conditions, and the embodiments of the present disclosure do not limit the parameters such as the composition and content of the reaction gas, cleaning gas and curing gas.

[0065] Figure 7 A schematic cross-sectional structure diagram of an air intake mechanism provided in some embodiments of the present disclosure.

[0066] Combined with reference Figure 4 and Figure 7In some embodiments, the air inlet mechanism 301 includes a guide plate 331, a first air outlet plate 341, and a second air outlet plate 351. The guide plate 331 has an air inlet hole 311 and a guide channel 3211 connected to the air inlet hole 311; the first air outlet plate 341 has a plurality of first air outlet holes 3212 that penetrate the first air outlet plate, and the first air outlet holes 3212 are connected to the guide channel 3211; the second air outlet plate 351 and the guide plate 331 are respectively located on the first air outlet plate 341. On both sides, the second air outlet plate 351 has a plurality of second air outlet holes 3213 penetrating the second air outlet plate 351, the second air outlet holes 3213 are connected to the first air outlet holes 3212, the distribution density of the second air outlet holes 3213 is greater than the distribution density of the first air outlet holes 3212, and the aperture of the second air outlet holes 3213 is smaller than the aperture of the first air outlet holes 3212; the air inlet channel 321 is composed of the guide channel 3211, the first air outlet hole 3212 and the second air outlet hole 3213.

[0067] The guide plate 331 is used to connect to the air inlet pipe for providing gas. Specifically, the air inlet hole 311 of the guide plate 331 is used to connect to the air inlet pipe for providing gas and guide the gas so that the gas is distributed not only near the air inlet hole 311 but also in the part far away from the air inlet hole 311.

[0068] The first outlet plate 341 is used to communicate with the guide channel 3211, and is used to transfer the gas in the guide channel 3211 to the second outlet plate 351. Specifically, the first outlet hole 3212 of the first outlet plate 341 is used to communicate with the guide channel 3211, and is used to transfer the gas in the gas guide channel 3211 to the second outlet plate 351.

[0069] The second gas outlet plate 351 and the guide plate 331 are respectively located on two opposite sides of the first gas outlet plate 341. The second gas outlet plate 351 is used to transport the gas in the first gas outlet plate 341 to the reaction chamber 310. Specifically, the second gas outlet hole 3213 of the second gas outlet plate 351 is connected to the first gas outlet hole 3212 to transport the gas in the first gas outlet plate 341 to the reaction chamber 310.

[0070] The second air outlet 3213 is connected to the first air outlet 3212, and the distribution density of the second air outlet 3213 is greater than the distribution density of the first air outlet, and the aperture of the second air outlet 3213 is smaller than the aperture of the first air outlet 3212, so that the gas is first roughly diverted through the first air outlet 3212 and then finely diverted through the second air outlet 3213, so that the gas entering the reaction chamber 310 through the air intake mechanism 301 is as uniform as possible in the horizontal direction X, which is beneficial to improving the uniformity of the target material layer prepared on the wafer 11.

[0071] Continue to refer Figure 4 The exhaust port 302 is used to remove byproducts and waste gas etc. of the film layer deposition in the reaction chamber 310 .

[0072] In some embodiments, a vacuum pump may be provided on the side of the vacuum port 302 away from the reaction chamber 310 to help the vacuum port 302 to quickly exhaust gas. The controller may be connected to the vacuum pump. After a film layer is deposited on the surface of the wafer 11, before the curing mechanism 304 moves in the vertical direction Y to the reaction chamber 310, the controller may control the vacuum pump to remove the byproducts and waste gas of the film layer deposition in the reaction chamber 310, so as to avoid the curing effect of the film layer being affected by the reaction gas remaining in the reaction chamber 310 when the curing gas needs to be introduced into the reaction chamber 310, which is beneficial to improving the reliability of the reaction chamber structure.

[0073] The carrier 303 is used to place the wafer 11 .

[0074] In some embodiments, a heater (not shown) may be provided in the carrier 303, and the heater is used to heat the wafer 11; the heater is also connected to the controller, and the controller is also used to control the heating temperature of the heater. In this way, the reaction chamber structure can provide the required temperature during the deposition of the film layer, and can also provide the required temperature during the curing of the film layer, which is conducive to improving the practicality of the reaction chamber structure. In addition, the controller can control the heating temperature of the heater. When the temperature required for the deposition of the film layer is different from the temperature required for the curing of the film layer, the heating temperature of the heater can be controlled by the controller, and the heating temperature of the heater is adjusted to the temperature required for the deposition of the film layer during the deposition of the film layer, and the heating temperature of the heater is adjusted to the temperature required for the curing of the film layer during the curing of the film layer, which can further improve the practicality of the reaction chamber structure.

[0075] The curing mechanism 304 is used to provide curing energy for the film layer so that the film layer can be transformed into a target material layer. The curing mechanism 304 can move up and down in the vertical direction Y. During the deposition of the film layer, the curing mechanism 304 is located in the accommodation chamber 320. After the deposition of the film layer, the curing mechanism 304 moves in the vertical direction Y to the reaction chamber 310 to provide the required curing energy for curing the film layer so that it can be transformed into a target material layer.

[0076] In some embodiments, the controller can control the curing mechanism 304 to move alternately between the receiving chamber 320 and the reaction chamber 310. Thus, the deposition and curing of the film layer by the reaction chamber structure can be performed alternately. During the deposition of the film layer, the controller can control the curing mechanism 304 to be located in the receiving chamber 320. After the film layer is deposited, the controller controls the curing mechanism 304 to move to the reaction chamber 310. After controlling the curing mechanism 304 to provide curing energy to convert the film layer into a target material layer, the controller controls the curing mechanism 304 to move to the receiving chamber 320, introduces the reaction gas again, and deposits another film layer on the surface of the target material layer. After that, the controller controls the curing mechanism 304 to move to the reaction chamber 310, and controls The curing mechanism 304 provides curing energy to convert the film layer on the surface of the target material layer into the target material layer. The above steps of depositing the film layer and curing the film layer can be performed alternately multiple times by moving the curing mechanism 304, so as to ensure that the curing effects of the upper and lower parts of the prepared target material layer are the same. This can avoid the situation where the curing effects of the upper and lower parts of the target material layer are different, resulting in the bending of other film layers and / or the target material layer when other film layers are subsequently prepared on the target material layer, thereby affecting the performance of the device containing the target material layer, thereby improving the reliability of the prepared target material layer.

[0077] In a specific example, when a 500 angstrom positive stress silicon nitride layer needs to be prepared, a first silicon nitride film layer with a thickness of 170 angstroms can be first deposited on the surface of the wafer 11, and then the first silicon nitride film layer is moved to the reaction chamber 310 through the curing mechanism 304 to provide curing energy, so that the first silicon nitride film layer receives the curing energy and is converted into a first positive stress silicon nitride layer, and then the first silicon nitride film layer is moved to the receiving chamber 320 through the curing mechanism 304, and a second silicon nitride film layer with a thickness of 170 angstroms is deposited on the surface of the ... second silicon nitride film layer is moved to the reaction chamber 310 through the curing mechanism 304. 04 is moved into the reaction chamber 310 to provide curing energy, so that the second silicon nitride film layer receives the curing energy and is converted into a second positive stress silicon nitride layer, and then moved into the receiving chamber 320 through the curing mechanism 304, and a third silicon nitride film layer with a thickness of 170 angstroms is deposited on the surface of the second positive stress silicon nitride layer, and then moved into the reaction chamber 310 through the curing mechanism 304, so that the third silicon nitride film layer receives the curing energy and is converted into a third positive stress silicon nitride layer, so as to obtain a positive stress silicon nitride layer with a required thickness of 500 angstroms. In other words, the curing mechanism 304 can be moved alternately in the reaction chamber 310 and the receiving chamber 320 to perform three deposition and curing processes, and a silicon nitride film layer with a thickness of 170 angstroms is deposited each time, and finally a 500 angstrom positive stress silicon nitride layer is obtained. Among them, the film layer in each curing process is a silicon nitride film layer with a thickness of 170 angstroms. The thickness of the silicon nitride film layer is small, so that the curing effect of the upper and lower parts of each layer of the silicon nitride film layer can be the same, so that the curing effect of the upper and lower parts of the final positive stress silicon nitride layer can be the same, so that the reliability of the positive stress silicon nitride layer prepared using the reaction chamber structure is high. It can be understood that curing the film layer is to densify it and transform it into a target material layer, so the thickness of the film layer after curing is slightly lower than the thickness of the film layer before curing. Therefore, when performing three deposition and curing processes to prepare a 500 angstrom positive stress silicon nitride layer, a silicon nitride film layer with a thickness of 170 angstroms needs to be deposited each time.

[0078] It is understandable that when the required thickness of the target material layer to be prepared is relatively thin, after the film layer is deposited, by moving the curing mechanism 304 and allowing the curing mechanism 304 to provide curing energy for the film layer, the film layer is converted into the target material layer, and the preparation of the target material layer with the required thickness and the same curing effect for the upper and lower parts can be completed. When the required thickness of the target material layer to be prepared is relatively thick, the curing mechanism 304 can be moved alternately in the accommodating chamber 320 and the reaction chamber 310 to complete the alternation of depositing the film layer and curing the film layer, so as to obtain the target material layer with the required thickness and the same curing effect for the upper and lower parts. That is, when the reaction chamber structure in the embodiment of the present disclosure prepares the target material layer, the preparation of the target material layer can be completed directly by first depositing and then curing, or by alternating deposition and curing multiple times to complete the preparation of the target material layer. The embodiment of the present disclosure does not limit the number of alternations of depositing the film layer and curing the film layer.

[0079] The curing mechanism 304 may be a light source curing mechanism such as an ultraviolet curing mechanism that provides light energy, and the wavelength of the light beam provided by the light source curing mechanism may be between 100 nm and 400 nm. The light beam provided by the light source curing mechanism may be a fixed wavelength, or a superposition of several wavelengths or a certain range of wavelengths. The curing mechanism 304 may also be a thermal energy curing mechanism that provides thermal energy, or a plasma curing mechanism that provides a plasma energy source.

[0080] Figure 8 A schematic top view of the structure of a receiving cavity and a curing mechanism provided in some embodiments of the present disclosure.

[0081] Combined with reference Figure 6 and Figure 8 In some embodiments, the accommodating chamber 320 may be an annular chamber connected to the bottom of the reaction chamber 310; the curing mechanism 304 is circumferentially arranged in the accommodating chamber 320. Compared with the structure in which the accommodating chamber is a cylindrical cavity, the accommodating chamber 320 is an annular cavity, which can save volume and help reduce the manufacturing cost of the reaction chamber structure. The circumferential arrangement of the curing mechanism can provide the required curing energy for the film layer in all directions, so that the film layer can receive the curing energy and convert it into the target material layer, which is conducive to improving the reliability of preparing the target material layer.

[0082] Fig. 9 Another schematic top view of the structure of the accommodating cavity and the curing mechanism provided in some embodiments of the present disclosure.

[0083] Combined with reference Figure 6 and Fig. 9 In some embodiments, the accommodating chamber 320 may be an annular chamber connected to the bottom of the reaction chamber 310; the curing mechanism 304 may include a plurality of curing devices 314, and the curing devices 314 are arranged circumferentially in the accommodating chamber 320. Compared with the structure in which the accommodating chamber is a cylindrical cavity, the accommodating chamber 320 is an annular cavity, which can save volume and help reduce the manufacturing cost of the reaction chamber structure. The curing mechanism 304 includes a plurality of curing devices 314, which can save the manufacturing cost of the curing mechanism 304 while satisfying the curing energy required for the film layer to be converted into the target material layer, which helps reduce the manufacturing cost of the reaction chamber structure.

[0084] It is understandable that in Fig. 9 In the embodiment, the number of curing devices is 4. In other embodiments, the number of curing devices in the curing mechanism may be other values ​​other than 4. The embodiment of the present disclosure does not limit the number of curing devices.

[0085] Fig.10 Another schematic top view of the structure of the accommodating cavity and the curing mechanism provided in some embodiments of the present disclosure.

[0086] Combined with reference Figure 6 and Fig.10 In some embodiments, the accommodating chamber 320 may include a plurality of circumferentially arranged sub-accommodating chambers 330 , each of which is connected to the bottom of the reaction chamber 310 , and the curing mechanism 304 includes a plurality of curing devices 314 , which are disposed in the sub-accommodating chambers 330 .

[0087] It is understandable that in Fig.10 In the embodiment, the number of sub-accommodating cavities is 4. In other embodiments, the number of sub-accommodating cavities in the curing mechanism can also be other values ​​other than 4. The embodiment of the present disclosure does not limit the number of sub-accommodating cavities. Fig.10 In the embodiment, the number of the solidifiers is the same as the number of the sub-accommodating cavities. In other embodiments, the number of the solidifiers may be different from the number of the sub-accommodating cavities.

[0088] Fig.11 A schematic cross-sectional structure diagram of a baffle in a retracted state in a third reaction chamber structure provided in some embodiments of the present disclosure, Fig.12 A schematic cross-sectional structure diagram of a baffle in a stretched state in a third reaction chamber structure provided in some embodiments of the present disclosure.

[0089] Combined with reference Fig.11 and Fig.12 In some embodiments, the reaction chamber structure may further include a baffle 305, which is located in the receiving chamber 320. The baffle 305 is retractable in the horizontal direction X. The baffle 305 is connected to a controller. During the deposition of the film layer, the controller controls the baffle 305 to be extended so that the baffle 305 blocks the passage between the reaction chamber 310 and the receiving chamber 320. After the deposition of the film layer, the controller controls the baffle 305 to be retracted so that the baffle 305 does not block the movement of the curing mechanism 304 in the vertical direction Y. During the deposition of the film layer, the controller controls the baffle 305 to be extended in the horizontal direction X so that the baffle 305 blocks the passage between the reaction chamber 310 and the receiving chamber 320 to prevent the reaction gas from entering the receiving chamber 320 and contaminating the curing mechanism 304. After the deposition of the film layer, the controller controls the baffle 305 to be retracted in the horizontal direction X so that the curing mechanism 304 can be moved in the vertical direction Y so that the curing mechanism 304 can be moved from the receiving chamber 320 to the reaction chamber 310 or from the reaction chamber 310 to the receiving chamber 320. The baffle 305 is provided to prevent the reaction gas from contaminating the curing mechanism 304 without affecting the movement of the curing mechanism 304, so as to ensure the curing effect of the curing mechanism 304, thereby improving the reliability of the reaction chamber structure.

[0090] Fig.13 A schematic cross-sectional structure diagram of a telescopic member in a contracted state in a fourth reaction chamber structure provided in some embodiments of the present disclosure, Fig.14A schematic cross-sectional structure diagram of a telescopic member in a stretched state in a fourth reaction chamber structure provided in some embodiments of the present disclosure.

[0091] Combined with reference Fig.13 and Fig.14 In some embodiments, the reaction chamber structure may further include: a baffle 305 and a telescopic member 315, and the baffle 305 and the telescopic member 315 are located at the top of the curing mechanism 304. The telescopic member 315 is telescopic in the horizontal direction X, and the telescopic member 315 is connected to the baffle 305 to drive the baffle 305 to move. The telescopic member 315 is connected to the controller. During the deposition of the film layer, the controller controls the telescopic member 315 to stretch, and the telescopic member 315 drives the baffle 305 to move. The baffle 305 is used to block the passage between the reaction chamber 310 and the receiving chamber 320. After the film layer is deposited, the controller controls the telescopic member 315 to shrink, and the telescopic member 315 drives the baffle 305 to move. The baffle 305 does not block the curing mechanism 304 from moving in the vertical direction Y. During the deposition of the film layer, the controller controls the telescopic member 315 to stretch in the horizontal direction X, so that the baffle 305 blocks the passage between the reaction chamber 310 and the receiving chamber 320 to prevent the reaction gas from entering the receiving chamber 320 and contaminating the curing mechanism 304. After the film layer is deposited, the controller controls the telescopic member 315 to contract in the horizontal direction X, so that the curing mechanism 304 can move in the vertical direction Y, so that the curing mechanism 304 can move from the accommodating chamber 320 to the reaction chamber 310 or from the reaction chamber 310 to the accommodating chamber 320. The baffle 305 is provided to prevent the reaction gas from contaminating the curing mechanism 304 without affecting the movement of the curing mechanism 304, so as to ensure the curing effect of the curing mechanism 304, thereby improving the reliability of the reaction chamber structure.

[0092] It is understandable that the reaction chamber structure may also not be provided with a baffle. After the target material layer is prepared on the surface of the wafer 11 and the wafer 11 is taken out, some by-products produced by the introduction of the reaction gas may be deposited on the surface of the curing mechanism 304. The clean gas can be introduced through the air intake mechanism 301 to clean the side walls of the reaction chamber body 300 while also cleaning the curing mechanism 304 to ensure that the curing mechanism 304 can work normally during the subsequent curing process, and the reliability of the reaction chamber structure can also be improved.

[0093] Fig.15 A schematic cross-sectional structure diagram of a reflector in a retracted state in a fifth reaction chamber structure provided in some embodiments of the present disclosure, Fig.16 A schematic diagram of the cross-sectional structure of a reflector in a stretched state in a fifth reaction chamber structure provided for some embodiments of the present disclosure.

[0094] Combined with reference Fig.15 and Fig.16In some embodiments, the curing mechanism 304 may be a light source curing mechanism, which is used to provide a light beam to provide curing energy for the film layer; the reaction chamber structure may also include a reflector 306, which is located at the top of the curing mechanism 304, and the side of the reflector 306 facing away from the air inlet mechanism 301 is a reflective surface 316, which is used to reflect the light beam, and the reflector 306 is retractable in the horizontal direction X. The reflector 306 is connected to a controller, and during the curing of the film layer, the controller is used to control the reflector 306 to stretch so that at least part of the reflective surface 316 of the reflector 306 faces the wafer 11, and after the curing of the film layer, the controller is used to control the reflector 306 to shrink so that the reflector 306 does not block the movement of the curing mechanism 304 in the vertical direction Y. The curing of the film layer refers to the period when the curing mechanism 304 provides the curing energy for the film layer; after the curing of the film layer refers to the period when the film layer receives the curing energy and is converted into the target material layer, and the curing mechanism 304 stops providing the curing energy. During the curing of the film layer, the controller controls the reflector 306 to stretch in the horizontal direction X so that at least part of the reflective surface 325 extends out of the top part of the curing mechanism 304, and the light source curing mechanism provides curing energy through a light beam. This arrangement can reflect part of the light emitted upward by the light source curing mechanism through the reflective surface 316 to the surface of the wafer 11, thereby increasing the light beam energy utilization rate of the light source curing mechanism, thereby improving the practicality of the reaction chamber structure.

[0095] In some embodiments, during the deposition of the film layer, the controller controls the reflector 306 to stretch in the horizontal direction X so that the reflector 306 blocks the passage between the reaction chamber 310 and the receiving chamber 320. After the deposition of the film layer, the controller controls the reflector 306 to shrink so that the reflector 306 does not block the movement of the curing mechanism 304 in the vertical direction Y. In this way, the reflector 306 can be used as a baffle to block the passage between the reaction chamber 310 and the receiving chamber 320 during the deposition of the film layer, so that the reflector 306 can not only increase the utilization rate of the light beam of the light source curing mechanism, but also protect the curing mechanism 304 from being contaminated during the deposition of the film layer, thereby facilitating the improvement of the reliability and practicality of the reaction chamber structure.

[0096] Continue to refer Figure 4 In some embodiments, the reaction chamber structure may include: a radio frequency (RF) power supply 307, and / or a remote plasma source (RPS) 317. The RF power supply 307 is used to provide an electric field required for forming plasma. The remote plasma source 317 is used to convert the gas into a plasma state.

[0097] The RF power source 307 may include at least one of a high frequency RF power source and a low frequency RF power source. The operating frequency of the high frequency power source is usually above 10 kHz, while the frequency of the low frequency power source is usually below 10 kHz.

[0098] The controller is connected to the RF power source 307 and can control the power of the RF power source 307 .

[0099] In a specific example, the target material layer is a positive stress silicon nitride layer, and the reaction gas is SiH 4 、N 2 and NH 3 , the flow rate of each gas can be 0sccm-20000sccm, and the RF power supply 307 uses a high-frequency power supply and a low-frequency power supply. Among them, the power of the high-frequency power supply is 1W-1500W, the power of the low-frequency power supply is 0W-1000W, the pressure in the reaction chamber 310 is 0.1torr-20torr, and the temperature is 100℃-600℃. The stress, thickness, uniformity and optical constant of the normal stress silicon nitride layer can be adjusted by adjusting the pressure in the reaction chamber 310, the gas flow rate and gas ratio of the reaction gas, and the size of the high-frequency power supply / low-frequency power supply.

[0100] It can be understood that when the reaction gas is introduced through the air intake mechanism 301, the reaction gas first passes through the RF power supply 307 or the remote control plasma controller 317 to convert the reaction gas into a plasma state, and then enters the reaction chamber 310 through the air intake mechanism 301. When the air intake mechanism 301 introduces the curing gas required for film curing and there is no need for the curing gas to be converted into a plasma state, the curing gas can directly enter the reaction chamber 310 through the air intake mechanism 302. At this time, the curing gas does not need to pass through the RF power supply 307 and the remote control plasma controller 317.

[0101] In some embodiments, the reaction chamber structure may include a ceramic sleeve 327 , which is located on a side wall of the reaction chamber 310 to protect the reaction chamber 310 .

[0102] In the reaction chamber structure of the above embodiment, the deposition of the film layer and the curing of the film layer are carried out in the same reaction chamber 310. After the film layer is deposited, the curing mechanism 304 can be moved in the vertical direction Y so that the curing mechanism 304 is in the reaction chamber 310 to provide curing energy for the film layer to convert it into a target material layer. In this process, there is no need to add steps such as moving the wafer to other chambers in the related technology, which can save a lot of time and thus improve the preparation efficiency of the target material layer.

[0103] Some other embodiments of the present disclosure also provide a reaction chamber structure, the reaction chamber mechanism is substantially the same as the reaction chamber mechanism provided in the aforementioned embodiment, the main difference being that the curing mechanism in the reaction chamber mechanism provided in the following embodiment includes at least one movable curing device. The reaction chamber mechanism will be described in detail below in conjunction with the accompanying drawings. It should be noted that the features that are the same or corresponding to the aforementioned embodiment will not be described in detail below to avoid redundancy. In the absence of contradiction, the corresponding description of the aforementioned embodiment is also applicable to the corresponding features of the following embodiment.

[0104] Fig.17 Schematic diagram of the cross-sectional structure of the second telescopic mechanism in the reaction chamber structure provided in other embodiments of the present disclosure in a contracted state, Fig.18 A schematic cross-sectional structure diagram of a second telescopic mechanism in a stretched state in a reaction chamber structure provided in some other embodiments of the present disclosure.

[0105] It should be noted that Fig.17 and Fig.18 The figure shows the case where the curing mechanism includes two movable curing devices. In fact, the number of movable curing devices in the curing mechanism can also be other values. The embodiment of the present disclosure does not limit the number of movable curing devices.

[0106] Combined with reference Fig.17 and Fig.18 , the reaction chamber structure includes a reaction chamber body 400, an air intake mechanism 401, an air extraction port 402, a stage 403, a curing mechanism 404 and a controller (not shown). The reaction chamber body 400 includes a reaction chamber 410 and a receiving chamber 420 connected to the reaction chamber 410 in the vertical direction Y, and the reaction chamber 410 is located above the receiving chamber 420. The air intake mechanism 401 is arranged at the top of the reaction chamber 410, and the air intake mechanism 401 has an air intake hole 411 and an air intake channel 421 connected to the air intake hole 411, and the air intake channel 421 is connected to the reaction chamber 410, and the air intake hole 411 is used to connect the air intake pipe for providing gas. The air extraction port 402 is connected to the reaction chamber 410. The stage 403 is used to carry the wafer 11, and the stage 403 is located in the reaction chamber 410. The curing mechanism 404 is disposed in the containing chamber 420 and can move up and down in the reaction chamber 410 along the vertical direction Y. The curing mechanism 404 is used to provide curing energy for the film layer to convert the film layer into a target material layer. The controller is connected to the curing mechanism 404 and is used to control the curing mechanism 404 to move in the vertical direction Y so that the curing mechanism 404 is located in the containing chamber 420 during the deposition of the film layer, and controls the curing mechanism 404 to move in the vertical direction Y to the reaction chamber 410 after the deposition of the film layer, and controls the curing mechanism 404 to provide curing energy for the film layer.

[0107] It should be noted that the reaction chamber body 400, the air inlet mechanism 401, the exhaust port 402, the carrier 403, the RF power supply 407, the remote control plasma controller 417 and the ceramic kit 427 of the embodiment of the present disclosure can refer to the reaction chamber body 300, the air inlet mechanism 301, the exhaust port 302, the movable carrier 303, the RF power supply 307, the remote control plasma controller 317 and the ceramic kit 327 in the previous embodiment, and will not be repeated here.

[0108] In some embodiments, the curing mechanism 404 may include at least one movable curing device 424; the reaction chamber structure includes: a first telescopic mechanism 408 and a second telescopic mechanism 418, the first telescopic mechanism 408 is arranged in the accommodating chamber 420, the first telescopic mechanism 408 is telescopic in the vertical direction Y, the first telescopic mechanism 408 is connected to the curing mechanism 404, and the first telescopic mechanism 408 is connected to the controller. After the film layer is deposited on the wafer 11, the controller controls the first telescopic mechanism 408 to stretch in the vertical direction Y to drive the curing mechanism 404 to move into the reaction chamber to provide curing energy for the film layer. When the film layer is converted into the target material layer, the controller controls the first telescopic mechanism 408 to shrink in the vertical direction Y to drive the curing mechanism 404 to move into the accommodating chamber 420. The first telescopic mechanism 408 is connected to the second telescopic mechanism 418, and the second telescopic mechanism 418 is telescopic in the horizontal direction X. The second telescopic mechanism 418 is connected to the movable curing device 424, and the second telescopic mechanism 418 is connected to the controller. When the movable curing device 424 is located in the reaction chamber 410, the controller controls the second telescopic mechanism 418 to stretch, and drives the movable curing device 424 to move, so that the movable curing device 424 is located directly above the wafer 11, and the controller controls the movable curing device 424 to provide curing energy. After the film layer is cured, the controller controls the movable curing device 424 to stop providing curing energy, and the controller controls the second telescopic mechanism 418 to contract, so that the movable curing device 424 does not block the curing mechanism 404 from moving in the vertical direction Y.

[0109] After the film layer is deposited, the first telescopic mechanism 408 moves in the vertical direction Y, driving the movable curing device 424 to move into the reaction chamber 410, and the second telescopic mechanism 418 stretches in the horizontal direction X, driving the movable curing device 424 to move, so that the movable curing device 424 is located directly above the wafer 11, so that the movable curing device 424 provides curing energy to the film layer on the surface of the wafer 11, and because the movable curing device 424 is located directly above the wafer 11, the curing energy received by the central area of ​​the film layer on the surface of the wafer 11 and the edge area surrounding the central area can be made consistent, thereby improving the reliability of the cured film layer, and further improving the reliability of the reaction chamber structure in preparing the target material layer. When the cured film layer is converted into the target material layer, the movable curing device 424 stops providing the curing energy, the second telescopic mechanism 418 shrinks in the horizontal direction X, and the first telescopic mechanism 408 shrinks in the vertical direction Y, so that the movable curing device 424 returns to the accommodating chamber 420. In addition, the deposition of the film layer and the curing of the film layer are carried out in the same reaction chamber 410. After the film layer is deposited, the curing mechanism can be moved along the vertical direction Y so that the curing mechanism 404 is in the reaction chamber 410 to provide curing energy for the film layer to convert it into a target material layer. In this process, there is no need to add steps such as moving the wafer to other chambers in the related technology, which can save a lot of time and thus improve the preparation efficiency of the target material layer.

[0110] The first telescopic mechanism 408 is used to drive the curing mechanism 404 to move in the vertical direction Y. During the deposition of the film layer, the first telescopic mechanism 408 contracts to place the curing mechanism 404 in the accommodating chamber 420. After the deposition of the film layer, the first telescopic mechanism 408 stretches to place the curing mechanism 408 in the reaction chamber 410 to provide curing energy for the film layer.

[0111] The second telescopic mechanism 418 is used to drive the movable curing device 424 to move in the horizontal direction X.

[0112] Some other embodiments of the present disclosure also provide a reaction chamber structure, the reaction chamber mechanism is substantially the same as the reaction chamber mechanism provided in the aforementioned embodiment, the main difference being that the curing mechanism in the reaction chamber mechanism provided in the following embodiment includes at least one rotatable curing device. The reaction chamber mechanism will be described in detail below in conjunction with the accompanying drawings. It should be noted that the features that are the same or corresponding to the aforementioned embodiment will not be described in detail below to avoid redundancy. In the absence of contradiction, the corresponding description of the aforementioned embodiment is also applicable to the corresponding features of the following embodiment.

[0113] Fig.19 A schematic diagram of a cross-sectional structure of a rotatable solidifier parallel to the vertical direction in a reaction chamber structure provided by some embodiments of the present disclosure, Fig. 20A schematic diagram of a cross-sectional structure in which a rotatable solidifier is parallel to the horizontal direction in a reaction chamber structure provided in some other embodiments of the present disclosure.

[0114] It should be noted that Fig.19 and Fig. 20 The figure shows the case where the curing mechanism includes two rotatable curing devices. In fact, the number of rotatable curing devices in the curing mechanism can also be other values. The embodiment of the present disclosure does not limit the number of rotatable curing devices.

[0115] Combined with reference Fig.19 and Fig. 20 , the reaction chamber structure includes a reaction chamber body 500, an air intake mechanism 501, an air suction port 502, a stage 503, a curing mechanism 504 and a controller (not shown). The reaction chamber body 500 includes a reaction chamber 510 and a receiving chamber 520 connected to the reaction chamber 510 in the vertical direction Y, and the reaction chamber 510 is located above the receiving chamber 520. The air intake mechanism 501 is arranged at the top of the reaction chamber 510, and the air intake mechanism 501 has an air intake hole 511 and an air intake channel 521 connected to the air intake hole 511, and the air intake channel 521 is connected to the reaction chamber 510, and the air intake hole 511 is used to connect the air intake pipe for providing gas. The air suction port 502 is connected to the reaction chamber 510. The stage 503 is used to carry the wafer 11, and the stage 503 is located in the reaction chamber 510. The curing mechanism 504 is disposed in the containing chamber 520 and can move up and down in the reaction chamber 510 along the vertical direction Y. The curing mechanism 504 is used to provide curing energy for the film layer to convert the film layer into a target material layer. The controller is connected to the curing mechanism 504 and is used to control the curing mechanism 504 to move in the vertical direction Y so that the curing mechanism 504 is located in the containing chamber 520 during the deposition of the film layer, and controls the curing mechanism 504 to move in the vertical direction Y to the reaction chamber 510 after the deposition of the film layer, and controls the curing mechanism 504 to provide curing energy for the film layer.

[0116] It should be noted that the reaction chamber body 500, the air inlet mechanism 501, the exhaust port 502, the carrier 503, the RF power supply 507, the remote control plasma controller 517 and the ceramic kit 527 of the embodiment of the present disclosure can refer to the reaction chamber body 300, the air inlet mechanism 301, the exhaust port 302, the movable carrier 303, the RF power supply 307, the remote control plasma controller 317 and the ceramic kit 327 in the above-mentioned embodiment, and will not be repeated here.

[0117] In some embodiments, the curing mechanism 504 may include at least one rotatable curing device 534. The reaction chamber structure includes: a first telescopic mechanism 508 and a rotating fixing member 509, the first telescopic mechanism 508 is disposed in the reaction chamber 510, the first telescopic mechanism 508 is telescopic in the vertical direction Y, the first telescopic mechanism 508 is connected to the curing mechanism 504, and the first telescopic mechanism 508 is connected to the controller. After the film layer is deposited, the controller controls the first telescopic mechanism 508 to stretch in the vertical direction Y to drive the curing mechanism 504 to move into the reaction chamber 510 to provide curing energy for the film layer. After the film layer is converted into the target material layer, the controller controls the first telescopic mechanism 508 to shrink in the vertical direction Y to drive the curing mechanism 504 to move into the accommodating chamber 520. The rotating fixed member 509 is connected to the first telescopic mechanism 508, and the rotating fixed member 509 is rotatably connected to the rotatable curing device 534; the controller is connected to the rotatable curing device 534. After the film layer is deposited and the curing mechanism 504 is located in the reaction chamber 510, the controller controls the rotatable curing device 534 to rotate around the rotating fixed member 509 to be parallel to the horizontal direction X, so that at least part of the rotatable curing device 534 is located directly above the wafer 11, and the controller controls the rotatable curing device 534 to provide curing energy. After the film layer is cured, the controller controls the rotatable curing device 534 to stop providing curing energy, and the controller controls the rotatable curing device 534 to rotate around the rotating fixed member 509 to be parallel to the vertical direction Y, so that the rotatable curing device 534 fits the first telescopic mechanism 508.

[0118] After the film layer is deposited, the first telescopic mechanism 508 moves in the vertical direction Y, driving the rotatable curing device 534 to move into the reaction chamber 510. The controller controls the rotatable controller 534 to rotate to be parallel to the horizontal direction X, so that the rotatable curing device 534 is located directly above the wafer 11, so that the rotatable curing device 534 provides curing energy to the film layer on the surface of the wafer 11. Since the rotatable curing device 534 is located directly above the wafer 11, the curing energy received by the central area of ​​the film layer on the surface of the wafer 11 and the edge area surrounding the central area can be made consistent, thereby improving the reliability of the cured film layer, and further improving the reliability of the reaction chamber structure in preparing the target material layer. After the cured film layer is converted into the target material layer, the rotatable curing device 534 stops providing the curing energy, and the rotatable curing device 534 rotates to be parallel to the vertical direction Y. The first telescopic mechanism 508 contracts in the vertical direction Y, so that the curing mechanism 504 returns to the accommodating chamber 520. In addition, the deposition of the film layer and the curing of the film layer are carried out in the same reaction chamber 510. After the film layer is deposited, the curing mechanism can be moved along the vertical direction Y so that the curing mechanism 504 is in the reaction chamber 510 to provide curing energy for the film layer to convert it into a target material layer. In this process, there is no need to add steps such as moving the wafer to other chambers in the related technology, which can save a lot of time and thus improve the preparation efficiency of the target material layer.

[0119] The rotating fixing member 509 may be a rotating bearing or a slewing bearing or other components.

[0120] Some other embodiments of the present disclosure also provide a reaction chamber structure, the reaction chamber mechanism is substantially the same as the reaction chamber mechanism provided in the aforementioned embodiment, the main difference being that the curing mechanism in the reaction chamber mechanism provided in the following embodiment includes at least one movable curing device. The reaction chamber mechanism will be described in detail below in conjunction with the accompanying drawings. It should be noted that the features that are the same or corresponding to the aforementioned embodiment will not be described in detail below to avoid redundancy. In the absence of contradiction, the corresponding description of the aforementioned embodiment is also applicable to the corresponding features of the following embodiment.

[0121] Fig.21 A schematic cross-sectional structure diagram of a retractable solidifier in a reaction chamber structure in some further embodiments of the present disclosure in a retracted state, Fig. 22 A schematic diagram of the cross-sectional structure of a retractable solidifier in a stretched state in a reaction chamber structure provided in some further embodiments of the present disclosure.

[0122] It should be noted that Fig.21 and Fig. 22 The figure shows the case where the curing mechanism includes two retractable curing devices. In fact, the number of retractable curing devices in the curing mechanism can also be other values. The embodiment of the present disclosure does not limit the number of retractable curing devices.

[0123] Combined with reference Fig.21 and Fig. 22, the reaction chamber structure includes a reaction chamber body 600, an air intake mechanism 601, an air suction port 602, a carrier 603, a curing mechanism 604 and a controller (not shown). The reaction chamber body includes a reaction chamber 610 and a receiving chamber 620 connected to the reaction chamber 610 in the vertical direction Y, and the reaction chamber 610 is located above the receiving chamber 620. The air intake mechanism 601 is arranged at the top of the reaction chamber 610, and the air intake mechanism 601 has an air intake hole 611 and an air intake channel 621 connected to the air intake hole 611, and the air intake channel 621 is connected to the reaction chamber 610, and the air intake hole 611 is used to connect the air intake pipe for providing gas. The air suction port 602 is connected to the reaction chamber 610. The carrier 603 is used to carry the wafer 11, and the carrier 603 is located in the reaction chamber 610. The curing mechanism 604 is disposed in the containing chamber 620 and can move up and down in the reaction chamber 610 along the vertical direction Y. The curing mechanism 604 is used to provide curing energy for the film layer to convert the film layer into a target material layer. The controller is connected to the curing mechanism 604 and is used to control the curing mechanism 604 to move in the vertical direction Y so that the curing mechanism 604 is located in the containing chamber 620 during the deposition of the film layer, and controls the curing mechanism 604 to move in the vertical direction Y to the reaction chamber 610 after the deposition of the film layer, and controls the curing mechanism 604 to provide curing energy for the film layer.

[0124] It should be noted that the reaction chamber body 600, the air inlet mechanism 601, the exhaust port 602, the carrier 603, the RF power supply 607, the remote control plasma controller 617 and the ceramic kit 627 of the embodiment of the present disclosure can refer to the reaction chamber body 300, the air inlet mechanism 301, the exhaust port 302, the movable carrier 303, the RF power supply 307, the remote control plasma controller 317 and the ceramic kit 327 in the above-mentioned embodiment, and will not be repeated here.

[0125] In some embodiments, the curing mechanism 604 may include at least one retractable curing device 644, which is retractable in the horizontal direction X. The retractable curing device 644 is connected to a controller. After the film layer is deposited and the curing mechanism 604 is located in the reaction chamber 610, the controller controls the retractable curing device 644 to stretch so that at least part of the retractable curing device 644 is located directly above the wafer 11, and the controller controls the retractable curing device 644 to provide curing energy. When the film layer is converted into a target material layer, the controller controls the retractable curing device 644 to stop providing curing energy, and the controller controls the retractable curing device 644 to contract so that the retractable curing device 644 does not block the movement of the fixing mechanism 604 in the vertical direction Y. The reaction chamber structure also includes: a first telescopic mechanism 608, which is arranged in the accommodating chamber 620, and the first telescopic mechanism 608 is telescopic in the vertical direction Y. The first telescopic mechanism 608 is connected to the curing mechanism 604, and the first telescopic mechanism 608 is connected to the controller. After the film layer is deposited, the controller controls the first telescopic mechanism 608 to stretch in the vertical direction Y to drive the curing mechanism 604 to move into the reaction chamber 610 to provide curing energy for the film layer. After the film layer is cured, the controller controls the first telescopic mechanism 608 to shrink in the vertical direction Y to drive the curing mechanism 604 to move into the accommodating chamber 620.

[0126] After the film layer is deposited, the first telescopic mechanism 608 moves in the vertical direction Y, driving the curing mechanism 604 to move into the reaction chamber 610, and the telescopic curing device 644 stretches in the horizontal direction X, so that the telescopic curing device 644 is located directly above the wafer 11, so that the telescopic curing device 644 provides curing energy to the film layer on the surface of the wafer 11, and because the telescopic curing device 644 is located directly above the wafer 11, the curing energy received by the central area of ​​the film layer on the surface of the wafer 11 and the edge area surrounding the central area can be made consistent, thereby improving the reliability of the cured film layer, and further improving the reliability of the reaction chamber structure in preparing the target material layer. After the cured film layer is converted into the target material layer, the telescopic curing device 644 stops providing the curing energy, and the telescopic curing device 644 shrinks in the horizontal direction X, and the first telescopic mechanism 608 shrinks in the vertical direction Y, so that the curing mechanism 604 returns to the accommodation chamber 620.

[0127] In the reaction chamber structure of the above-mentioned embodiment, the deposition of the film layer and the curing of the film layer are carried out in the same reaction chamber. After the film layer is deposited, the curing mechanism can be moved in the vertical direction so that the curing mechanism is in the reaction chamber to provide curing energy for the film layer to convert it into a target material layer. In this process, there is no need to add steps such as moving the wafer to other chambers in the related technology, which not only saves a lot of time, thereby improving the preparation efficiency of the target material layer, but also avoids the increase of defects due to the movement of the wafer between different chambers, thereby improving the reliability of preparing the target material layer.

[0128] Correspondingly, another embodiment of the present disclosure further provides a deposition device having a reaction chamber structure of any of the above embodiments. For the parts that are the same or corresponding to the previous embodiment, reference may be made to the corresponding description of the previous embodiment, and will not be described in detail below.

[0129] The deposition device includes the reaction chamber structure described in any one of the above embodiments.

[0130] The deposition equipment can be used to realize flowable chemical vapor deposition to obtain a target material layer. The deposition equipment can also be used to realize other vapor phase chemical deposition to obtain a target material layer, and other vapor phase chemical deposition can be atmospheric pressure chemical vapor deposition (APCVD, atmospheric pressure chemical vapor deposition), low pressure chemical vapor deposition (LPCVD, low pressure chemical vapor deposition), ultrahigh vacuum chemical vapor deposition (UHVCVD, Ultrahigh vacuumchemical vapor deposition), metal organic chemical vapor deposition (MOCVD, Metal-organic chemical vapor deposition) or plasma chemical vapor deposition (PECVD, Plasma-Enhanced chemical vapor deposition), etc.

[0131] Those skilled in the art can understand that the above-mentioned embodiments are specific examples for realizing the present disclosure, and in practical applications, various changes can be made to them in form and details without departing from the spirit and scope of the present disclosure. Any person skilled in the art can make various changes and modifications without departing from the spirit and scope of the present disclosure, so the protection scope of the present disclosure shall be based on the scope defined in the claims.

Claims

1. A reaction chamber structure, applied to a deposition device, It is characterized in that include: A reaction chamber body, wherein the reaction chamber body includes a reaction chamber and a receiving chamber vertically connected to the reaction chamber, and the reaction chamber is located above the receiving chamber; An air intake mechanism, the air intake mechanism is arranged at the top of the reaction chamber, the air intake mechanism has an air intake hole and an air intake channel connected to the air intake hole, the air intake channel is connected to the reaction chamber, and the air intake hole is used to connect to an air intake pipe for providing gas; A gas extraction port, the gas extraction port is connected to the reaction chamber; A carrier, the carrier is used to carry the wafer, and the carrier is located in the reaction chamber; A curing mechanism, which is disposed in the containing chamber and can move up and down along the vertical direction in the reaction chamber, and is used to provide curing energy for the film layer to convert the film layer into a target material layer; A controller is connected to the curing mechanism, and is used to control the curing mechanism to move in the vertical direction so that the curing mechanism is located in the accommodating chamber during the deposition of the film layer, and to control the curing mechanism to move in the vertical direction to the reaction chamber after the deposition of the film layer, and to control the curing mechanism to provide the curing energy for the film layer.

2. The reaction chamber structure according to claim 1, It is characterized in that The controller controls the curing mechanism to move alternately in the containing chamber and the reaction chamber.

3. The reaction chamber structure according to claim 1, It is characterized in that The cross-sectional area of ​​the accommodating chamber perpendicular to the vertical direction is smaller than the cross-sectional area of ​​the reaction chamber perpendicular to the vertical direction.

4. The reaction chamber structure according to claim 3, It is characterized in that The accommodating chamber is an annular chamber connected to the bottom of the reaction chamber; the solidification mechanism is circumferentially arranged in the accommodating chamber, or the solidification mechanism includes a plurality of solidifiers, and the solidifiers are circumferentially arranged in the accommodating chamber.

5. The reaction chamber structure according to claim 3, It is characterized in that The accommodating chamber includes a plurality of circumferentially arranged sub-accommodating chambers, each of which is communicated with the bottom of the reaction chamber. The curing mechanism includes a plurality of curing devices, and the curing devices are arranged in the sub-accommodating chambers.

6. The reaction chamber structure according to claim 1, It is characterized in that The reaction chamber structure also includes: A baffle, wherein the baffle is located in the accommodating chamber, the baffle is retractable in the horizontal direction, and the baffle is connected to the controller. During the deposition of the film layer, the controller controls the baffle to stretch so that the baffle blocks the passage between the reaction chamber and the accommodating chamber. After the deposition of the film layer, the controller controls the baffle to shrink so that the baffle does not block the movement of the curing mechanism in the vertical direction.

7. The reaction chamber structure according to claim 1, It is characterized in that The curing mechanism is a light source curing mechanism, and the light source curing mechanism is used to provide a light beam to provide the curing energy for the film layer; The reaction chamber structure also includes: A reflector, wherein the reflector is located at the top of the curing mechanism, a side of the reflector facing away from the air intake mechanism is a reflective surface, the reflective surface is used to reflect the light beam, the reflector is retractable in the horizontal direction, the reflector is connected to the controller, during the curing of the film layer, the controller is used to control the stretching of the reflector so that at least a portion of the reflective surface faces the wafer, and after the film layer is cured, the controller is used to control the contraction of the reflector so that the reflector does not block the movement of the curing mechanism in the vertical direction.

8. The reaction chamber structure according to claim 1, It is characterized in that The curing mechanism includes at least one movable curing device; The reaction chamber structure also includes: A first telescopic mechanism, the first telescopic mechanism is arranged in the accommodating chamber, the first telescopic mechanism is telescopic in the vertical direction, the first telescopic mechanism is connected to the curing mechanism, the first telescopic mechanism is connected to the controller, after the film layer is deposited, the controller controls the first telescopic mechanism to stretch in the vertical direction to drive the curing mechanism to move into the reaction chamber to provide the curing energy for the film layer, and after the film layer is cured, the controller controls the first telescopic mechanism to shrink in the vertical direction to drive the curing mechanism to move into the accommodating chamber; The second telescopic mechanism, the first telescopic mechanism is connected to the second telescopic mechanism, the second telescopic mechanism is telescopic in the horizontal direction, the second telescopic mechanism is connected to the movable solidifier, and the second telescopic mechanism is connected to the controller. When the movable solidifier is located in the reaction chamber, the controller controls the second telescopic mechanism to stretch and drive the movable solidifier to move so that the movable solidifier is located directly above the wafer, and the controller controls the movable solidifier to provide the curing energy. After curing the film layer, the controller controls the movable solidifier to stop providing the curing energy, and the controller controls the second telescopic mechanism to contract so that the movable solidifier does not block the first telescopic mechanism from moving in the vertical direction.

9. The reaction chamber structure according to claim 1, It is characterized in that The curing mechanism includes at least one rotatable curing device; The reaction chamber structure also includes: A first telescopic mechanism, the first telescopic mechanism is arranged in the reaction chamber, the first telescopic mechanism is telescopic in the vertical direction, the first telescopic mechanism is connected to the curing mechanism, the first telescopic mechanism is connected to the controller, after the film layer is deposited, the controller controls the first telescopic mechanism to stretch in the vertical direction to drive the curing mechanism to move into the reaction chamber to provide the curing energy for the film layer, and after the film layer is cured, the controller controls the first telescopic mechanism to shrink in the vertical direction to drive the curing mechanism to move into the accommodating chamber; A rotating fixture, wherein the rotating fixture is connected to the first telescopic mechanism, and the rotating fixture is rotatably connected to the rotatable solidifier; the controller is connected to the rotatable solidifier, and when the solidification mechanism is located in the reaction chamber, the controller controls the rotatable solidifier to rotate around the rotating fixture to be parallel to the horizontal direction, so that at least a portion of the rotatable solidifier is located directly above the wafer, and the controller controls the rotatable solidifier to provide the solidification energy. After solidifying the film layer, the controller controls the rotatable solidifier to stop providing the solidification energy, and the controller controls the rotatable solidifier to rotate around the rotating fixture to be parallel to the vertical direction, so that the rotatable solidifier fits the first telescopic mechanism.

10. A deposition device, It is characterized in that It comprises a reaction chamber structure as described in any one of claims 1 to 9.

Citation Information

Patent Citations

  • Metal chemical vapor deposition equipment and reaction chamber thereof

    CN103572255A

  • Atomic layer deposition equipment and cleaning method thereof

    CN109609930A

  • Thin film deposition cavity and air inlet mechanism thereof

    CN117512565A

  • Ventilation panel and thin film deposition cavity

    CN118127490A

  • Reaction cavity for plasma chemical vapor deposition

    CN217052390U