Low-power-consumption furnace bottom heat preservation structure and crystal pulling process thereof
By designing multi-layer coaxial insulation components and tightly attached furnace bottom insulation felt at the bottom of the single crystal furnace, combining the adjustment of the material ratio of the soft felt and the solid felt and the use of insulation cylinders and fillers, the single crystal furnace bottom is solved The problem of heat loss in the insulation structure achieves the effects of low power consumption and electricity bill saving.
Patent Information
- Application Number
- CN202411064947.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-05
- Publication Date
- 2024-11-15
AI Technical Summary
The existing single-crystal furnace bottom insulation structure has radial gaps that lead to heat loss, increasing power consumption and electricity costs.
Design a low-power furnace bottom insulation structure, adopting multi-layer coaxial structure insulation components and tightly attached furnace bottom insulation felt, adjusting the material ratio of soft felt and solid felt and setting insulation on the outside of the furnace bottom insulation felt The cylinder and insulation filler prevent heat loss and enhance the furnace bottom insulation capacity.
It effectively reduces heat loss at the furnace bottom insulation, reduces crystal induction and equal diameter power, saves power consumption costs, and closes the bottom heater of the single crystal furnace in advance, reducing production hours.
Smart Images

Figure CN118957732A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of single crystal furnace insulation, in particular to a low-power consumption furnace bottom insulation structure and a crystal pulling process thereof. Background Art
[0002] In the process of manufacturing single crystal silicon, it is necessary to add a heat field in the single crystal furnace to melt the polysilicon material, thereby realizing the crystal pulling process and finally obtaining a single crystal silicon rod. In this process, the heat in the heat field is mainly provided by the heater. Part of the heat provided is used to maintain crystal growth, while most of it is taken away by the heat dissipation system and airflow. In order to reduce the heat taken away by the heat dissipation system and airflow, a heat preservation structure needs to be designed.
[0003] With the massive expansion of the photovoltaic industry, non-silicon costs have risen sharply, and cost reduction and efficiency improvement have become the mainstream trend of the single crystal industry in the future. In addition to the cost of auxiliary materials, electricity costs account for an absolute proportion of non-silicon costs, so the purpose of reducing costs and increasing efficiency is achieved by enhancing the thermal insulation capacity of the single crystal furnace. The current furnace bottom insulation adopts the traditional flat soft felt or solid felt stacked in layers in the vertical direction. There are radial gaps between the soft felts of each layer of furnace bottom insulation felt. The heat emitted by the graphite electrode will be lost from the gap and taken away by the water cooling system of the single crystal furnace wall. This method causes the furnace bottom insulation to have leakage hot spots in the radial direction, resulting in high equal-diameter power and high electricity consumption. It is urgent to design a low-power furnace bottom insulation structure and its crystal pulling process. Summary of the invention
[0004] The technical problem to be solved by the present invention is to provide a low-power consumption furnace bottom insulation structure and a crystal pulling process thereof in view of the deficiencies of the above-mentioned prior art.
[0005] In order to solve the above technical problems, the technical solution adopted by the present invention is:
[0006] A low-power furnace bottom insulation structure is used to insulate the bottom of a single crystal furnace, comprising an insulation component and a first furnace bottom insulation felt, wherein the first furnace bottom insulation felt is in close contact with the outer wall of the bottom of the single crystal furnace, the insulation component is a multi-layer coaxial structure from the inside to the outside, and each layer of the insulation component is closely arranged in sequence from the inside to the outside, and the inner wall of the insulation component is in close contact with the outer wall of the first furnace bottom insulation felt.
[0007] The present invention designs a low-power consumption furnace bottom insulation structure, comprising an insulation component and a first furnace bottom insulation felt; and the insulation component is a multi-layer coaxial structure from inside to outside, which can increase the insulation performance of the furnace bottom, reduce heat loss at the furnace bottom insulation, reduce seeding and equal-diameter power, achieve the effect of reducing power consumption, and save electricity consumption costs.
[0008] As a further preferred embodiment of the present invention, the insulation assembly includes a furnace bottom insulation tube and a furnace bottom insulation tube felt; the furnace bottom insulation tube felt is tightly attached to the outside of the furnace bottom insulation tube by winding, and the furnace bottom insulation tube felt and the furnace bottom insulation tube have the same height, which is 1m-1.7m; the upper and lower edges of the furnace bottom insulation tube felt are ensured to be flush with the upper and lower edges of the furnace bottom insulation tube. The first furnace bottom insulation felt is installed from top to bottom in a layered manner, and the inner wall of the furnace bottom insulation tube is tightly attached to the outer wall of the first furnace bottom insulation felt without obvious gaps. And the furnace bottom insulation tube is made of carbon-carbon material.
[0009] Since the first furnace bottom insulation felt is stacked layer by layer in the vertical direction, there is a radial gap between each layer of the first furnace bottom insulation felt. The heat emitted by the graphite electrode will be lost from the gap and taken away by the water cooling system of the single crystal furnace wall. Therefore, a furnace bottom insulation tube is arranged on the outside of the furnace bottom insulation felt, and the furnace bottom insulation tube felt is rolled on the outside of the furnace bottom insulation tube. This structure can prevent heat loss at the radial gap, enhance the insulation capacity of the furnace bottom, and achieve the purpose of reducing power consumption.
[0010] As a further preferred embodiment of the present invention, the insulation assembly includes a second furnace bottom insulation felt and a third furnace bottom insulation felt; the first furnace bottom insulation felt, the second furnace bottom insulation felt and the third furnace bottom insulation felt are alternately arranged closely from the inside to the outside, the first furnace bottom insulation felt and the third furnace bottom insulation felt are soft felts, and the second furnace bottom insulation felt is solid felt. The first furnace bottom insulation felt, the second furnace bottom insulation felt and the third furnace bottom insulation felt are coaxially arranged. Since soft felts are superior to solid felts in terms of thermal insulation, the more soft felts are used, the better the thermal insulation.
[0011] The insulation structure of the furnace bottom is adjusted to soft felt + solid felt + soft felt, and the thickness of the solid felt is adjusted to 20-40mm. Example 1: the total insulation thickness of the furnace bottom is 220mm, the solid felt is 20-40mm, and the soft felt is 180mm-200mm; Example 2: the total insulation thickness of the furnace bottom is 200mm, the solid felt is 20-40mm, and the soft felt is 160mm-180mm.
[0012] This solution adjusts the material ratio of soft felt and solid felt for furnace bottom insulation. Increasing the proportion of soft felt can reduce heat loss at the furnace bottom insulation, enhance the furnace bottom insulation capacity, and achieve the purpose of reducing power consumption.
[0013] As a further preferred embodiment of the present invention, the insulation component is a third furnace bottom insulation felt, the inner wall of the third furnace bottom insulation felt is in close contact with the outer wall of the first insulation felt, and the first insulation felt and the third insulation felt are both soft felts.
[0014] If the furnace bottom insulation is all made of soft felt, the total thickness of the furnace bottom insulation = the total thickness of the soft felt = 220mm. This structure can prevent the heat loss at the furnace bottom insulation, enhance the furnace bottom insulation capacity, and achieve the purpose of reducing power consumption.
[0015] As a further preferred embodiment of the present invention, the thermal insulation assembly includes a cylindrical thermal insulation shell, a thermal insulation filler and a shell cover; the cylindrical thermal insulation shell is hollow inside, the thermal insulation filler is filled in the internal cavity of the cylindrical thermal insulation shell, the shell cover is connected to the top of the cylindrical thermal insulation shell through a first step and a second step, and the inner wall of the cylindrical thermal insulation shell is closely attached to the outer wall of the first furnace bottom thermal insulation felt without obvious gaps. The material of the cylindrical thermal insulation shell is carbon-carbon material.
[0016] Since the first furnace bottom insulation felt is stacked layer by layer in the vertical direction, there is a radial gap between each layer of the first furnace bottom insulation felt. The heat emitted by the graphite electrode will be lost from the gap and taken away by the water cooling system of the single crystal furnace wall. Therefore, a cylindrical insulation shell is arranged on the outside of the first furnace bottom insulation felt, and the inside of the cylindrical insulation shell is filled with insulation fillers, and the fillers are covered with a shell cover. The fillers leak out during use and cause sparks. This structure can prevent heat loss at the radial gaps, enhance the insulation capacity of the furnace bottom, and achieve the purpose of reducing power consumption.
[0017] A crystal pulling process with a low-power consumption furnace bottom insulation structure comprises the following steps:
[0018] S1, feeding stage; after the last barrel of material is added to the single crystal furnace, the heater at the bottom of the single crystal furnace is turned off 20-40 minutes; in the prior art, it takes 30-50 minutes to turn off the heater at the bottom of the single crystal furnace after the last barrel of material is added to the single crystal furnace, while the present method can advance the time of turning off the bottom heater by 10 minutes, thereby avoiding slow cooling during the temperature adjustment stage and also reducing production hours.
[0019] S2, welding-seeding stage; the crucible is rotated to 4rpm to prevent the liquid temperature from being too high due to the enhancement of thermal insulation performance. The seeding power is reduced by 2.5KW compared with the conventional furnace.
[0020] S3, shoulder release stage; for every 20mm increase in the length of the shoulder growth crystal, the crucible speed is reduced by 0.2rpm: when the length of the shoulder growth crystal is 85mm, the crucible speed is 3.8rpm, when the length of the shoulder growth crystal is 105mm, the crucible speed is 3.6rpm, when the length of the shoulder growth crystal is 125mm, the crucible speed is 3.4rpm, when the length of the shoulder growth crystal is 145mm, the crucible is changed to 3.2rpm, and when the length of the shoulder growth crystal is 165mm, the crucible speed is maintained at 3.0rpm.
[0021] S4, equal-diameter growth stage; the equal-diameter power is reduced by 10kw based on the seeding power.
[0022] After using the device of the present invention, 2.5kw of electricity and 10 minutes of work time can be saved in the process of pulling single crystals, and the effect is remarkable.
[0023] A crystal pulling process with a low-power consumption furnace bottom insulation structure comprises the following steps:
[0024] S1, feeding stage; after the last barrel of material is added to the single crystal furnace, the heater at the bottom of the single crystal furnace is turned off 25-45 minutes; in the prior art, it takes 30-50 minutes to turn off the heater at the bottom of the single crystal furnace after the last barrel of material is added to the single crystal furnace, while the present method can advance the time of turning off the bottom heater by 5 minutes, thereby avoiding slow cooling in the temperature adjustment stage and also reducing production hours.
[0025] S2, welding-seeding stage; the crucible rotates to 4rpm to prevent the liquid temperature from being too high due to the enhancement of thermal insulation performance; the seeding power is reduced by 1.5KW compared with the conventional furnace.
[0026] S3, shoulder release stage; for every 20mm increase in the length of the shoulder growth crystal, the crucible speed is reduced by 0.2rpm; when the length of the shoulder growth crystal is 85mm, the crucible speed is 3.8rpm, when the length of the shoulder growth crystal is 105mm, the crucible speed is 3.6rpm, when the length of the shoulder growth crystal is 125mm, the crucible speed is 3.4rpm, when the length of the shoulder growth crystal is 145mm, the crucible is changed to 3.2rpm, and when the length of the shoulder growth crystal is 165mm, the crucible speed is maintained at 3.0rpm;
[0027] S4, equal-diameter growth stage; the equal-diameter power is reduced by 10kw based on the seeding power.
[0028] After using the device of the present invention, 1.5kw of electricity and 5 minutes of work time can be saved in the process of pulling single crystals, and the effect is remarkable.
[0029] A crystal pulling process with a low-power consumption furnace bottom insulation structure comprises the following steps:
[0030] S1, feeding stage; after the last barrel of material is added to the single crystal furnace, the heater at the bottom of the single crystal furnace is turned off 15-35 minutes; in the prior art, it takes 30-50 minutes to turn off the heater at the bottom of the single crystal furnace after the last barrel of material is added to the single crystal furnace, while the present method can advance the time of turning off the bottom heater by 15 minutes, thereby avoiding slow cooling during the temperature adjustment stage and also reducing production hours.
[0031] S2, welding-seeding stage; the crucible is rotated to 4rpm to prevent the liquid temperature from being too high due to the enhancement of thermal insulation performance; the seeding power is reduced by 3.5KW compared with the conventional furnace.
[0032] S3, shoulder release stage; for every 20mm increase in the length of the shoulder growth crystal, the crucible speed is reduced by 0.2rpm; when the length of the shoulder growth crystal is 85mm, the crucible speed is 3.8rpm, when the length of the shoulder growth crystal is 105mm, the crucible speed is 3.6rpm, when the length of the shoulder growth crystal is 125mm, the crucible speed is 3.4rpm, when the length of the shoulder growth crystal is 145mm, the crucible is changed to 3.2rpm, and when the length of the shoulder growth crystal is 165mm, the crucible speed is maintained at 3.0rpm;
[0033] S4, equal-diameter growth stage; the equal-diameter power is reduced by 10kw based on the seeding power.
[0034] After using the device of the present invention, 3.5kw of electricity and 15 minutes of work time can be saved in the process of pulling single crystals, and the effect is remarkable.
[0035] The present invention has the following beneficial effects:
[0036] 1. The present invention designs a low-power furnace bottom insulation structure, including an insulation component and a first furnace bottom insulation felt; and the insulation component is a multi-layer coaxial structure from the inside to the outside, which can increase the insulation performance of the furnace bottom, reduce heat loss at the furnace bottom insulation, reduce seeding and equal-diameter power, achieve the effect of reducing power consumption, and save electricity consumption costs.
[0037] 2. The present invention adds a furnace bottom insulation tube and a furnace bottom insulation tube felt on the outside of the first furnace bottom insulation felt to prevent heat loss at the radial overlapping gaps of the first furnace bottom insulation felt, thereby enhancing the insulation capacity of the furnace bottom and achieving the purpose of reducing power consumption. After using the device of the present invention, 2.5kw of electricity and 10 minutes of work time can be saved in the process of pulling single crystals, with significant effects.
[0038] 3. By adjusting the material ratio of the soft felt and solid felt for furnace bottom insulation, increasing the proportion of soft felt can reduce the heat loss at the furnace bottom insulation, thereby enhancing the insulation capacity of the furnace bottom and achieving the purpose of reducing power consumption; after using the device of the present invention, 1.5kw of electricity can be saved in the process of pulling single crystals, and 5 minutes of work time can be saved, with significant effects.
[0039] 4. Adding a cylindrical insulation shell and insulation filler on the outside of the first furnace bottom insulation felt can prevent heat loss at the radial overlapping gaps of the furnace bottom insulation felt, thereby enhancing the insulation capacity of the furnace bottom and achieving the purpose of reducing power consumption; after using the device of the present invention, 3.5kw of electricity can be saved in the single crystal pulling process, and 15 minutes of work time can be saved, with significant effects. BRIEF DESCRIPTION OF THE DRAWINGS
[0040] Figure 1 is a top view of embodiment 1 of the present invention;
[0041] Figure 2is a side sectional view of embodiment 1 of the present invention;
[0042] Figure 3 is a top view of embodiment 2 of the present invention;
[0043] Figure 4 is a side sectional view of embodiment 2 of the present invention;
[0044] Figure 5 is a top view of embodiment 3 of the present invention;
[0045] Figure 6 is a side sectional view of embodiment 3 of the present invention;
[0046] The components include: 1. furnace bottom insulation tube; 2. first furnace bottom insulation felt; 3. furnace bottom insulation tube felt; 4. cylindrical insulation shell; 5. insulation filler; 6. shell cover; 7. first step platform; 8. second step platform. DETAILED DESCRIPTION
[0047] The present invention will be further described in detail below in conjunction with the accompanying drawings and specific preferred embodiments.
[0048] In the description of the present invention, it should be understood that the terms "left side", "right side", "upper part", "lower part" and the like indicate the orientation or positional relationship based on the orientation or positional relationship shown in the drawings, which is only for the convenience of describing the present invention and simplifying the description, and does not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation. "First", "second" and the like do not indicate the importance of the components, and therefore cannot be understood as limiting the present invention. The specific dimensions used in this embodiment are only for illustrating the technical solution, and do not limit the scope of protection of the present invention.
[0049] A low-power furnace bottom insulation structure is used to insulate the bottom of a single crystal furnace, including an insulation component and a first furnace bottom insulation felt 2, the first furnace bottom insulation felt 2 is in close contact with the outer wall of the bottom of the single crystal furnace, the insulation component is a multi-layer coaxial structure from the inside to the outside, and each layer of the insulation component is closely arranged in sequence from the inside to the outside, and the inner wall of the insulation component is in close contact with the outer wall of the first furnace bottom insulation felt 2.
[0050] The present invention designs a low-power consumption furnace bottom insulation structure, including an insulation component and a first furnace bottom insulation felt 2; and the insulation component is a multi-layer coaxial structure from the inside to the outside, which can increase the insulation performance of the furnace bottom, reduce heat loss at the furnace bottom insulation, reduce seeding and equal-diameter power, achieve the effect of reducing power consumption, and save electricity consumption costs.
[0051] Based on the above structure, the present invention includes the following three embodiments, which are further described in detail below in conjunction with the accompanying drawings and specific preferred implementations:
[0052] Embodiment 1:
[0053] like Figure 1-2 As shown, the insulation assembly includes a furnace bottom insulation tube 1 and a furnace bottom insulation tube felt 3; the furnace bottom insulation tube felt 3 is tightly attached to the outside of the furnace bottom insulation tube 1 by winding, and the furnace bottom insulation tube felt 3 and the furnace bottom insulation tube 1 have the same height, which is 1m-1.7m; the upper and lower edges of the furnace bottom insulation tube felt 3 are ensured to be flush with the upper and lower edges of the furnace bottom insulation tube 1. The first furnace bottom insulation felt 2 is installed from top to bottom in a layered manner, and the inner wall of the furnace bottom insulation tube 1 is tightly attached to the outer wall of the first furnace bottom insulation felt 2 without obvious gaps. And the furnace bottom insulation tube 1 is made of carbon-carbon material.
[0054] Since the first furnace bottom insulation felt 2 is stacked layer by layer in the vertical direction, there is a radial gap between each layer of the first furnace bottom insulation felt 2, and the heat emitted by the graphite electrode will be lost from the gap and taken away by the water cooling system of the single crystal furnace wall. Therefore, a furnace bottom insulation tube 1 is arranged on the outside of the furnace bottom insulation felt, and a furnace bottom insulation tube felt 3 is rolled on the outside of the furnace bottom insulation tube 1. This structure can prevent heat loss at the radial gap, play the effect of enhancing the insulation capacity of the furnace bottom, and achieve the purpose of reducing power consumption.
[0055] After using the device of this embodiment, a crystal pulling process with a low-power furnace bottom insulation structure is adopted, including the following steps: S1, feeding stage; after the last barrel of material is added to the single crystal furnace, the heater at the bottom of the single crystal furnace is turned off 20-40 minutes; in the prior art, it takes 30-50 minutes to turn off the heater at the bottom of the single crystal furnace after the last barrel of material is added to the single crystal furnace, while this method can advance the time of turning off the bottom heater by 10 minutes, avoiding slow cooling in the temperature adjustment stage, and also reducing production hours.
[0056] S2, welding-seeding stage; the crucible is rotated to 4rpm to prevent the liquid temperature from being too high due to the enhancement of thermal insulation performance. The seeding power is reduced by 2.5KW compared with the conventional furnace.
[0057] S3, shoulder release stage; for every 20mm increase in the length of the shoulder growth crystal, the crucible speed is reduced by 0.2rpm: when the length of the shoulder growth crystal is 85mm, the crucible speed is 3.8rpm, when the length of the shoulder growth crystal is 105mm, the crucible speed is 3.6rpm, when the length of the shoulder growth crystal is 125mm, the crucible speed is 3.4rpm, when the length of the shoulder growth crystal is 145mm, the crucible is changed to 3.2rpm, and when the length of the shoulder growth crystal is 165mm, the crucible speed is maintained at 3.0rpm.
[0058] S4, equal-diameter growth stage; the equal-diameter power is reduced by 10kw based on the seeding power.
[0059] After using the device of the present invention, 2.5kw of electricity and 10 minutes of work time can be saved in the process of pulling single crystals, and the effect is remarkable.
[0060] Embodiment 2:
[0061] like Figure 3-4 As shown, the insulation assembly includes a second furnace bottom insulation felt and a third furnace bottom insulation felt; the first furnace bottom insulation felt 2, the second furnace bottom insulation felt and the third furnace bottom insulation felt are alternately arranged closely from the inside to the outside, the first furnace bottom insulation felt 2 and the third furnace bottom insulation felt are soft felts, and the second furnace bottom insulation felt is solid felt. The first furnace bottom insulation felt 2, the second furnace bottom insulation felt and the third furnace bottom insulation felt are coaxially arranged. Since soft felts are superior to solid felts in terms of thermal insulation, the more soft felts are used, the better the thermal insulation.
[0062] The insulation structure of the furnace bottom is adjusted to soft felt + solid felt + soft felt, and the thickness of the solid felt is adjusted to 20-40mm. Example 1: the total insulation thickness of the furnace bottom is 220mm, the solid felt is 20-40mm, and the soft felt is 180mm-200mm; Example 2: the total insulation thickness of the furnace bottom is 200mm, the solid felt is 20-40mm, and the soft felt is 160mm-180mm.
[0063] This solution adjusts the material ratio of soft felt and solid felt for furnace bottom insulation. Increasing the proportion of soft felt can reduce heat loss at the furnace bottom insulation, enhance the furnace bottom insulation capacity, and achieve the purpose of reducing power consumption.
[0064] The insulation component may also be only the third furnace bottom insulation felt, the inner wall of the third furnace bottom insulation felt is in close contact with the outer wall of the first insulation felt, and both the first insulation felt and the third insulation felt are soft felts.
[0065] If the furnace bottom insulation is all made of soft felt, the total thickness of the furnace bottom insulation = the total thickness of the soft felt = 220mm. This structure can prevent the heat loss at the furnace bottom insulation, enhance the furnace bottom insulation capacity, and achieve the purpose of reducing power consumption.
[0066] After using the device of this embodiment, a crystal pulling process with a low-power furnace bottom insulation structure is adopted, including the following steps: S1, feeding stage; after the last barrel of material is added to the single crystal furnace, the heater at the bottom of the single crystal furnace is turned off 25-45 minutes; in the prior art, it takes 30-50 minutes to turn off the heater at the bottom of the single crystal furnace after the last barrel of material is added to the single crystal furnace, while this method can advance the time of turning off the bottom heater by 5 minutes, avoiding slow cooling in the temperature adjustment stage, and also reducing production hours.
[0067] S2, welding-seeding stage; the crucible rotates to 4rpm to prevent the liquid temperature from being too high due to the enhancement of thermal insulation performance; the seeding power is reduced by 1.5KW compared with the conventional furnace.
[0068] S3, shoulder release stage; for every 20mm increase in the length of the shoulder growth crystal, the crucible speed is reduced by 0.2rpm; when the length of the shoulder growth crystal is 85mm, the crucible speed is 3.8rpm, when the length of the shoulder growth crystal is 105mm, the crucible speed is 3.6rpm, when the length of the shoulder growth crystal is 125mm, the crucible speed is 3.4rpm, when the length of the shoulder growth crystal is 145mm, the crucible is changed to 3.2rpm, and when the length of the shoulder growth crystal is 165mm, the crucible speed is maintained at 3.0rpm;
[0069] S4, equal-diameter growth stage; the equal-diameter power is reduced by 10kw based on the seeding power.
[0070] After using the device of the present invention, 1.5kw of electricity and 5 minutes of work time can be saved in the process of pulling single crystals, and the effect is remarkable.
[0071] Embodiment 3:
[0072] like Figure 5-6 As shown, the insulation assembly includes a cylindrical insulation shell 4, an insulation filler 5 and a shell cover 6; the cylindrical insulation shell 4 is hollow inside, and the insulation filler 5 is filled in the inner cavity of the cylindrical insulation shell 4. The shell cover 6 is connected to the top of the cylindrical insulation shell 4 through a first step 7 and a second step 8, and the inner wall of the cylindrical insulation shell 4 is close to the outer wall of the first furnace bottom insulation felt 2 without obvious gaps. The material of the cylindrical insulation shell 4 is carbon-carbon material.
[0073] Since the first furnace bottom insulation felt 2 is stacked layer by layer in the vertical direction, there is a radial gap between each layer of the first furnace bottom insulation felt 2. The heat emitted by the graphite electrode will be lost from the gap and taken away by the water cooling system of the single crystal furnace wall. Therefore, a cylindrical insulation shell 4 is arranged on the outside of the first furnace bottom insulation felt 2, and the inside of the cylindrical insulation shell 4 is filled with insulation filler 5, and the shell cover 6 is used to cover the filler. The filler leaks out during use and causes sparks. This structure can prevent heat loss at the radial gap, thereby enhancing the insulation capacity of the furnace bottom and achieving the purpose of reducing power consumption.
[0074] After using the device of this embodiment, a crystal pulling process with a low-power furnace bottom insulation structure is adopted, including the following steps: S1, feeding stage; after the last barrel of material is added to the single crystal furnace, the heater at the bottom of the single crystal furnace is turned off 15-35 minutes; in the prior art, it takes 30-50 minutes to turn off the heater at the bottom of the single crystal furnace after the last barrel of material is added to the single crystal furnace, while this method can advance the time of turning off the bottom heater by 15 minutes, avoiding slow cooling in the temperature adjustment stage, and also reducing production hours.
[0075] S2, welding-seeding stage; the crucible is rotated to 4rpm to prevent the liquid temperature from being too high due to the enhancement of thermal insulation performance; the seeding power is reduced by 3.5KW compared with the conventional furnace.
[0076] S3, shoulder release stage; for every 20mm increase in the length of the shoulder growth crystal, the crucible speed is reduced by 0.2rpm; when the length of the shoulder growth crystal is 85mm, the crucible speed is 3.8rpm, when the length of the shoulder growth crystal is 105mm, the crucible speed is 3.6rpm, when the length of the shoulder growth crystal is 125mm, the crucible speed is 3.4rpm, when the length of the shoulder growth crystal is 145mm, the crucible is changed to 3.2rpm, and when the length of the shoulder growth crystal is 165mm, the crucible speed is maintained at 3.0rpm;
[0077] S4, equal-diameter growth stage; the equal-diameter power is reduced by 10kw based on the seeding power.
[0078] After using the device of the present invention, 3.5kw of electricity and 15 minutes of work time can be saved in the process of pulling single crystals, and the effect is remarkable.
[0079] The preferred embodiments of the present invention are described in detail above; however, the present invention is not limited to the specific details in the above embodiments. Within the technical concept of the present invention, various equivalent transformations can be made to the technical solutions of the present invention, and these equivalent transformations all belong to the protection scope of the present invention.
Claims
1. A low-power furnace bottom insulation structure, used to insulate the bottom of a single crystal furnace. Features: It comprises a thermal insulation component and a first furnace bottom thermal insulation felt (2), wherein the first furnace bottom thermal insulation felt (2) is in close contact with the outer wall of the bottom of the single crystal furnace, the thermal insulation component is a multi-layer coaxial structure from the inside to the outside, and each layer of the thermal insulation component is arranged in close contact in sequence from the inside to the outside, and the inner wall of the thermal insulation component is in close contact with the outer wall of the first furnace bottom thermal insulation felt (2).
2. A low-power consumption furnace bottom insulation structure according to claim 1, Features: The insulation component comprises a furnace bottom insulation tube (1) and a furnace bottom insulation tube felt (3); the furnace bottom insulation tube felt (3) is tightly attached to the outside of the furnace bottom insulation tube (1) by winding, and the furnace bottom insulation tube felt (3) and the furnace bottom insulation tube (1) have the same height, which is 1m-1.7m; the first furnace bottom insulation felt (2) is a layered structure from top to bottom, and the inner wall of the furnace bottom insulation tube (1) is tightly attached to the outer wall of the first furnace bottom insulation felt (2).
3. A low-power consumption furnace bottom insulation structure according to claim 1, Features: The insulation component comprises a second furnace bottom insulation felt and a third furnace bottom insulation felt; the first furnace bottom insulation felt (2), the second furnace bottom insulation felt and the third furnace bottom insulation felt are arranged closely from the inside to the outside, the first furnace bottom insulation felt (2) and the third furnace bottom insulation felt are soft felts, and the second furnace bottom insulation felt is a solid felt.
4. A low-power consumption furnace bottom insulation structure according to claim 3, Features: The thickness of the second furnace bottom insulation felt is 20-40 mm.
5. A low-power consumption furnace bottom insulation structure according to claim 1, Features: The insulation component is a third furnace bottom insulation felt, the inner wall of the third furnace bottom insulation felt is in close contact with the outer wall of the first insulation felt, and both the first insulation felt and the third insulation felt are soft felts.
6. A low-power consumption furnace bottom insulation structure according to claim 1, Features: The thermal insulation component comprises a cylindrical thermal insulation shell (4), a thermal insulation filler (5) and a shell cover (6); the interior of the cylindrical thermal insulation shell (4) is hollow, the thermal insulation filler (5) is filled in the internal cavity of the cylindrical thermal insulation shell (4), the shell cover (6) covers the top of the cylindrical thermal insulation shell (4), and the inner wall of the cylindrical thermal insulation shell (4) is in close contact with the outer wall of the first furnace bottom thermal insulation felt (2).
7. A crystal pulling process using the low power consumption furnace bottom insulation structure of claim 2, Features: The following steps are involved: S1, charging stage: after the last barrel of material is added to the single crystal furnace, the heater at the bottom of the single crystal furnace is turned off for 20-40 minutes; S2, welding-seeding stage; the crucible is rotated to 4rpm, and the seeding power is reduced by 2.5KW; S3, shoulder release stage; for every 20mm increase in the length of the shoulder growth crystal, the crucible speed is reduced by 0.2rpm: when the length of the shoulder growth crystal is 85mm, the crucible speed is 3.8rpm, when the length of the shoulder growth crystal is 105mm, the crucible speed is 3.6rpm, when the length of the shoulder growth crystal is 125mm, the crucible speed is 3.4rpm, when the length of the shoulder growth crystal is 145mm, the crucible speed is changed to 3.2rpm, and when the length of the shoulder growth crystal is 165mm, the crucible speed is maintained at 3.0rpm; S4, equal-diameter growth stage; the equal-diameter power is reduced by 10kw based on the seeding power.
8. A crystal pulling process using the low-power consumption furnace bottom insulation structure according to claim 4 or 5, Features: The following steps are involved: S1, charging stage: after the last barrel of material is added to the single crystal furnace, the heater at the bottom of the single crystal furnace is turned off for 25-45 minutes; S2, welding-seeding stage; the crucible is rotated to 4rpm, and the seeding power is reduced by 1.5KW; S3, shoulder release stage; for every 20mm increase in the length of the shoulder growth crystal, the crucible speed is reduced by 0.2rpm; when the length of the shoulder growth crystal is 85mm, the crucible speed is 3.8rpm, when the length of the shoulder growth crystal is 105mm, the crucible speed is 3.6rpm, when the length of the shoulder growth crystal is 125mm, the crucible speed is 3.4rpm, when the length of the shoulder growth crystal is 145mm, the crucible is changed to 3.2rpm, and when the length of the shoulder growth crystal is 165mm, the crucible speed is maintained at 3.0rpm; S4, equal-diameter growth stage; the equal-diameter power is reduced by 10kw based on the seeding power.
9. A crystal pulling process using the low power consumption furnace bottom insulation structure of claim 6, Features: The following steps are involved: S1, charging stage: after the last barrel of material is added to the single crystal furnace, the heater at the bottom of the single crystal furnace is turned off for 15-35 minutes; S2, welding-seeding stage; the crucible is rotated to 4rpm, and the seeding power is reduced by 3.5KW; S3, shoulder release stage; for every 20mm increase in the length of the shoulder growth crystal, the crucible speed is reduced by 0.2rpm; when the length of the shoulder growth crystal is 85mm, the crucible speed is 3.8rpm, when the length of the shoulder growth crystal is 105mm, the crucible speed is 3.6rpm, when the length of the shoulder growth crystal is 125mm, the crucible speed is 3.4rpm, when the length of the shoulder growth crystal is 145mm, the crucible is changed to 3.2rpm, and when the length of the shoulder growth crystal is 165mm, the crucible speed is maintained at 3.0rpm; S4, equal-diameter growth stage; the equal-diameter power is reduced by 10kw based on the seeding power.