Method and structure for shielding semiconductor against ultraviolet rays

By forming a colored light shielding layer on the semiconductor layer, the stability and reliability problems caused by ultraviolet exposure in the photolithography process of oxide semiconductor materials are solved, effective protection of the semiconductor layer is achieved, and defects and oxygen vacancy are reduced. , improving the performance of semiconductor devices.

CN118969853APending Publication Date: 2024-11-15TAIWAN SEMICONDUCTOR MANUFACTURING CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410922671.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2023-07-27
Filing Date
2024-07-10
Publication Date
2024-11-15

AI Technical Summary

Technical Problem

When exposed to ultraviolet rays in the photolithography process, oxide semiconductor materials are easily damaged by high power, resulting in photo-induced holes and oxygen vacancy, resulting in reduced threshold voltage instability and reliability, and shorter semiconductor channel length Channel effect sensitive.

Method used

Using colored light shielding layers, including dielectric materials such as titanium dioxide, nickel oxide, etc., directly contacts the semiconductor layer to reduce the exposure of the semiconductor layer to wavelength radiation from 10 nanometers to 400 nanometers, reduces the damage caused by photolithography exposure, and passes ozone treatment. Enhance the quality of the shielding layer.

Benefits of technology

It effectively reduces the occurrence of defects in the semiconductor layer, improves the threshold voltage stability and reliability, reduces the oxygen vacancy state and the number of photo holes, and improves the reliability and carrier movement force of the semiconductor device.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118969853A_ABST
    Figure CN118969853A_ABST
Patent Text Reader

Abstract

The invention provides a method and a structure for shielding ultraviolet rays of a semiconductor. The transistor includes a colored light shielding layer over its semiconductor layer. The colored light shielding layer reduces exposure of the semiconductor layer to radiation having a wavelength of about 10 nm to about 400 nm. The colored light shielding layer may have white, black, red, yellow, or gray. The metal oxide film, the P-type oxide semiconductor or the perovskite can form a colored light shielding layer. The colored light shielding layer reduces defects which may be generated in the semiconductor layer due to ultraviolet exposure during the process, and improves performance and reliability of the device.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The embodiments of the present invention relate to a method and structure for shielding a semiconductor from ultraviolet rays. Background Art

[0002] Integrated circuits are made up of a large number of transistors. Field effect transistors are usually made up of a substrate, on which a conductive gate electrode controls the current between a source electrode and a drain electrode. An insulating gate dielectric layer separates the gate from the source and drain. A semiconductor layer bridges the source and drain and contacts the gate dielectric layer. Summary of the invention

[0003] In many embodiments, the transistor disclosed herein is a transistor including a colored light shielding layer above a semiconductor layer. The colored light shielding layer reduces exposure of the semiconductor layer to radiation having a wavelength of about 10 nanometers to about 400 nanometers. The colored light shielding layer has white, black, red, yellow, or gray.

[0004] In a plurality of embodiments, there are also disclosed transistors including a write line, a semiconductor layer, a source line, a bit line, and a colored light shielding layer. The source line and the bit line are in contact with the semiconductor layer. The colored light shielding layer includes a dielectric material and can be used as a gate dielectric layer. Examples of such materials include titanium dioxide (TiO2), nickel oxide (NiO), ferric oxide (Fe2O3), cobalt oxide (Co3O4), manganese oxide (Mn3O4), copper oxide (CuO), antimony oxide (Sb2O3), tin oxide (SnO), chromium oxide (Cr2O3), rare earth oxides, cerium dioxide (CeO2), yttrium oxide (Y2O3), neodymium oxide (Nd2O3), or perovskite including calcium (Ca), strontium (Sr), or bismuth (Bi). In some embodiments, the colored light shielding layer is in contact with the semiconductor layer and the write line, for example, located between the semiconductor layer and the write line. In some alternative embodiments, a separate gate dielectric layer contacts the write line and the semiconductor layer. In other embodiments, a channel cap layer may be located above the colored light shielding layer.

[0005] Also disclosed are a plurality of methods for manufacturing transistors, including forming a semiconductor layer on a substrate and forming a colored light shielding layer above the semiconductor layer. The colored light shielding layer reduces exposure of the semiconductor layer to radiation having a wavelength of about 10 nanometers to about 400 nanometers. BRIEF DESCRIPTION OF THE DRAWINGS

[0006] The various aspects of the present disclosure will be best understood by reading the following detailed description in conjunction with the accompanying drawings. It should be noted that, in accordance with standard practice in the industry, various features are not drawn to scale. In fact, the size of various features may be arbitrarily increased or reduced for clarity of discussion.

[0007] Figure 1 A flow chart of a first method for fabricating a transistor according to some embodiments is shown.

[0008] Figure 2 For Figure 1 A cross-sectional view showing the process steps for forming a transistor.

[0009] Figure 3 A cross-sectional view of the process steps for forming a transistor.

[0010] Figure 4 A cross-sectional view of the process steps for forming a transistor.

[0011] Figure 5 A cross-sectional view of the process steps for forming a transistor.

[0012] Figure 6 A cross-sectional view of the process steps for forming a transistor.

[0013] Figure 7 A cross-sectional view of the process steps for forming a transistor.

[0014] Figure 8 A cross-sectional view of the process steps for forming a transistor.

[0015] Fig. 9 A cross-sectional view of the process steps for forming a transistor.

[0016] Fig.10 A cross-sectional view of the process steps for forming a transistor.

[0017] Fig.11 A cross-sectional view of the final transistor is shown, which is a bottom-gate transistor.

[0018] Fig.12 A flow chart of a second method for fabricating a transistor according to some embodiments is shown.

[0019] Fig.13 A cross-sectional view of the process steps for forming a transistor.

[0020] Fig.14 A cross-sectional view of the process steps for forming a transistor.

[0021] Fig.15 A cross-sectional view of the process steps for forming a transistor.

[0022] Fig.16 A cross-sectional view of the process steps for forming a transistor.

[0023] Fig.17 A cross-sectional view of the process steps for forming a transistor.

[0024] Fig.18 A cross-sectional view of the process steps for forming a transistor.

[0025] Fig.19 A cross-sectional view of the process steps for forming a transistor.

[0026] Fig. 20 A cross-sectional view of the final transistor is shown, which is a top-gate transistor.

[0027] Fig.21 A flow chart of a second alternative method for fabricating a transistor is shown according to some embodiments. In this alternative method, a colored light shielding layer also serves as a gate dielectric layer.

[0028] Fig. 22 A cross-sectional view of the process steps for forming a transistor.

[0029] Fig.23 A cross-sectional view of the process steps for forming a transistor. DETAILED DESCRIPTION

[0030] The following disclosure provides many different embodiments or examples for implementing the different features of the present invention. Specific examples of components and configurations are described below to simplify the disclosure. Of course, these are only examples and are not intended to be restrictive. For example, in the following description, the formation of a first feature above or on a second feature may include an embodiment in which the first feature is formed in direct contact with the second feature, and may also include an embodiment in which an additional feature may be formed between the first feature and the second feature so that the first feature and the second feature may not be in direct contact. In addition, the disclosure may repeat the figure numbers and / or letters in various examples. This repetition is for the purpose of simplicity and clarity, and does not itself specify the relationship between the various embodiments and / or configurations discussed.

[0031] Additionally, for ease of description, spatially relative terms such as "below," "beneath," "lower," "above," "upper," and the like may be used herein to describe the relationship of one component or feature to another component or feature as illustrated in the figures. The spatially relative terms are intended to encompass different orientations of a component in use or operation in addition to the orientation depicted in the figures. The device may be otherwise oriented (rotated 90 degrees or at other orientations) and the spatially relative descriptors used herein should likewise be interpreted accordingly.

[0032] The scope of the application rights of this application and the numerical values ​​in the specification should be understood to include the same numerical values ​​when reduced to the same number of significant figures, and the experimental error value of the conventional measurement technology of the type used to determine the numerical value in this application. All ranges disclosed herein include the endpoints.

[0033] The term "about" can be used to include any value that can be varied without changing the basic function of the value. When used in the form of a range, "about" also discloses the range of absolute values ​​defining the two endpoints, for example, "about 2 to about 4" also discloses a range from 2 to 4. The term "about" can refer to plus or minus 10% of the specified value.

[0034] The present disclosure relates to multiple transistors and other structures composed of multiple different layers. When the words "on" or "upon" are used to refer to two different layers (including a substrate), these words only mean that one layer is on or above the other layers. These words do not require that the two layers are directly in contact with each other, and allow for multiple other layers to be located between the two layers. For example, all the layers of a transistor can be considered to be "on" a substrate, even if all of the layers are not directly in contact with the substrate. The word "directly" can be used to refer to two layers directly contacting each other without any layers between the two layers.

[0035] The present disclosure relates to methods of fabricating transistors with enhanced protection or resistance to ultraviolet light exposure. In such considerations, oxide semiconductor (OS) materials have high charge mobility, which allows for high-speed driving and low current for low power consumption. Therefore, oxide semiconductor materials are often used as semiconductor channel materials for metal-oxide-semiconductor (metal-oxide-semiconductor) field effect transistor (MOSFET) devices. However, exposure to ultraviolet light during photolithography processes has the potential to cause high-power damage, which may cause the creation / ionization of photogenerated holes and oxygen vacancy (Vo) states in the oxide semiconductor material body and its surface. Exposure to energies as low as 0.001 to 1 joule may cause heating issues at small feature sizes. In addition, photoionization generates free electrons, and the transition from neutral Vo to ionized Vo is accompanied by lattice relaxation, which increases the energy of the free oxygen vacancy. This may promote "defect generation" from atomic exchange with weakly bonded hydrogen, resulting in high instability of threshold voltage change (delta-Vt) during operation, threshold voltage shift, and reduced reliability. In addition, as the length of the semiconductor channel continues to shrink, transistors are increasingly sensitive to short channel effects. Therefore, in the present disclosure, a protective ultraviolet shielding layer is applied to the semiconductor layer. This reduces damage caused by photolithography light exposure.

[0036] Figure 1 A flow chart of a first method 100 for fabricating a transistor is shown in accordance with some disclosed embodiments. Figures 2 to 11The steps of the first method are shown and discussed together. The figures are shown with reference to a bottom-gate transistor.

[0037] First, please refer to Figure 2 , receiving or providing a substrate. This figure shows the substrate starting stage before manufacturing transistors. The substrate is typically a chip composed of semiconductor materials. Such materials may include silicon, for example in the form of single crystal silicon (crystalline Si) or polycrystalline silicon (polycrystalline Si). The substrate may also be formed from other elementary semiconductors, such as germanium or aluminum oxide (Al2O3 (sapphire)); or may include compound semiconductors, such as silicon carbide (SiC), gallium nitride (GaN), gallium arsenide (GaAs), indium arsenide (InAs) and indium phosphide (InP). In a specific embodiment, the chip substrate is silicon.

[0038] Now, in Figure 1 In step 105, and Figure 3 The gate electrode 210 is shown as being formed. This can be accomplished by forming an insulating (or dielectric) layer, applying and patterning a photoresist layer to place the gate in the desired location, etching the insulating layer, depositing a conductive material to form the gate, and removing the photoresist layer. Note that the insulating layer is not shown in FIG. Figure 3 middle.

[0039] The insulating layer is usually formed by thermal oxidation of the silicon substrate. However, other processes may be used, such as thermal oxidation, atomic layer deposition (ALD), or chemical vapor deposition (CVD), including plasma-enhanced atomic layer deposition (PEALD) or plasma-enhanced chemical vapor deposition (PECVD). The insulating layer can be formed of silicon dioxide (SiO2), but can also be formed of a high-k dielectric material (which has a dielectric constant greater than 3.9). For example, suitable high dielectric materials include silicon nitride (Si3N4), silicon carbide (SiC), hafnium dioxide (HfO2), zirconium dioxide (ZrO2), aluminum oxide (Al2O3), silicon oxynitride (SiO x N y ), hafnium oxynitride (HfO x N y ), zirconium oxynitride (ZrO x N y ), hafnium silicates (HfSi x O y ), zirconium silicates (ZrSi x O y )、Silicon carboxynitride (SiC x O y N z) or hexagonal boron nitride (hBN). Other dielectric materials may include tantalum oxide (Ta2O5), nitrides such as silicon nitride, polysilicon, phosphosilicate glass (PSG), fluorosilicate glass (FSG), undoped silicate glass (USG), high-stress undoped silicate glass (HSUSG), and borosilicate glass (BSG).

[0040] For example, the photoresist layer can be applied by spin coating, spraying, roller coating, dip coating, or extrusion coating. Generally, during the spin coating process, the substrate is placed on a rotating platen, which may include a vacuum chuck to hold the substrate in place. Next, the photoresist composition is applied to the center of the substrate. The speed of the rotating platen is then increased so that the photoresist is spread evenly from the center of the substrate to the edge of the substrate. Finally, the rotation speed of the platen is fixed so that the thickness of the final photoresist layer can be controlled.

[0041] Next, the photoresist layer can be baked or cured to remove the solvent and cure the photoresist layer. In some specific embodiments, the baking temperature is about 90° C. to about 110° C. The baking can be performed using a hot plate or an oven or similar equipment.

[0042] Next, the photoresist layer is patterned by exposure to radiation. The radiation can be any wavelength of light that carries the desired shielding pattern, even though ultraviolet radiation is currently commonly used. Ultraviolet radiation has a wavelength in the range of about 10 nanometers (nm) to about 400 nanometers, such as from KrF lasers (248nm) or ArF lasers (193nm). In a specific embodiment, extreme ultraviolet (EUV) with a wavelength of about 13.5 nanometers is used for patterning because it allows smaller pattern sizes to be obtained. This causes some parts of the photoresist layer to be exposed to radiation, while some parts of the photoresist layer are not exposed to radiation. This exposure causes some parts of the photoresist layer to become soluble in the developer, and other parts of the photoresist remain insoluble in the developer.

[0043] An additional photoresist bake step may be performed after the radiation exposure, for example to help release acid leaving groups (ALGs) or other molecules important in chemical amplification photoresists.

[0044] Next, a developer is used to develop the photoresist layer. The developer can be an aqueous solution or an organic solution. During the development step, the soluble portion of the photoresist layer is dissolved or washed away, leaving the photoresist pattern. An example of a common developer is aqueous tetramethylammonium hydroxide (TMAH). Other developing agents may include 2-heptanone, n-butyl acetate, isoamyl acetate, cyclohexanone, 5-methyl-2-hexanone, methyl-2-hydroxyisobutyrate, ethyl lactate, propylene glycol monomethyl ether acetate, n-pentyl acetate, n-butyl propionate, n-hexyl acetate, n-butyl butyrate, isobutyl butyrate, 2,5-dimethyl-4-hexanone, 2,6-dimethyl-4-heptanone, propyl isobutyrate, or isobutyl isobutyrate. In general, any suitable developer may be used. Sometimes, in order to optimize performance in subsequent steps, a post-develop bake or "hard bake" may be performed to stabilize the developed photoresist pattern.

[0045] Generally speaking, any etching step used herein may be performed using a wet or dry etching (plasma etching) process, such as reactive ion etching (RIE), inductively coupled plasma (ICP), or a combination thereof, as appropriate. The etching may be anisotropic. Depending on the material, the etchant may include carbon tetrafluoride (CF4), hexafluoroethane (C2F6), octafluoropropane (C3F8), fluoroform (CHF3), difluoromethane (CH2F2), fluoromethane (CH3F), trifluoromethane (CHF3), carbon fluorides, nitrogen (N2), hydrogen (H2), oxygen (O2), argon (Ar), xenon (Xe), xenon difluoride (XeF2), helium (He), carbon monoxide (CO), carbondioxide (CO2), fluorine (F2), chlorine (Cl2), oxygen (O2), hydrogen bromide (HBr), etc. bromide (HBr), hydrofluoric acid (HF), nitrogen trifluoride (NF3), sulfur hexafluoride (SF6), boron trichloride (BCl3), ammonia (NH3), bromine (Br2) or the like, or a combination of these substances in various ratios. For example, hydrofluoric acid and ammonium fluoride are used to wet etch silicon dioxide; or trifluoromethane (CHF3), oxygen (O2), carbon tetrafluoride (CF4) and / or hydrogen (H2) are used to dry etch silicon dioxide.

[0046] The gate and any other conductive components may be formed by deposition of any suitable conductive material. Examples of the material may include polysilicon, metals (e.g., aluminum (Al), zirconium (Zr), tungsten (W), ruthenium (Ru), cobalt (Co), nickel (Ni), platinum (Pt), gold (Au), cobalt (Co), rhodium (Rh), palladium (Pd), bismuth (Bi), titanium (Ti), tantalum (Ta), and the like), compounds (e.g., titanium nitride (TiN), tungsten nitride (WN), or tantalum nitride (TaN); or alloys thereof). For example, the material may be deposited by evaporation or sputtering, plating, atomic layer deposition (ALD), chemical vapor deposition (CVD), or other suitable methods. Chemical-mechanical planarization (CMP) may be used to remove excess deposited material. The gate may have a thickness 215 of about 10 nanometers to about 100 nanometers.

[0047] Then, in Figure 1 Step 110 and is shown in Figure 4 In the present invention, a gate dielectric layer 220 is formed above the substrate, more specifically, on the gate 210. This can be formed in the same manner as described above. In a specific embodiment, the gate dielectric layer 220 is formed of a high dielectric material. In some embodiments of the present disclosure, the high dielectric material has a dielectric constant greater than 5 or greater than 7 or greater than 10. Examples of high dielectric materials include the materials previously described. Other suitable high dielectric materials may include aluminum oxide (Al2O3), hafnium dioxide (HfO2), hafnium lanthanum oxide (HfLaO), and hafnium silicon oxide (HfSiO). Other suitable dielectric materials may include ferroelectric materials (whose dielectric constant may vary with temperature) and oxide-nitride-oxide (ONO) films. The gate dielectric layer may have a thickness 225 of about 1 nanometer to about 10 nanometers.

[0048] Then, in Figure 1 Step 115 and is shown in Figure 5 In the embodiment of the present invention, a semiconductor layer 230 is formed on a substrate, more specifically, on a gate dielectric layer 220. The semiconductor layer can be formed using processes such as physical vapor deposition, chemical vapor deposition, or atomic layer deposition. The semiconductor layer 230 can have a thickness 235 of about 1 nanometer to about 50 nanometers.

[0049] In a particular embodiment, the semiconductor layer 230 is formed of an oxide semiconductor. Examples of oxide semiconductors can include zinc oxide (ZnO), magnesium oxide (MgO), gadolinium oxide (GdO), gallium trioxide (Ga2O3), tin oxide (SnO x ), indium oxide (InO x ), and binary, ternary, or quaternary compounds composed of these elements. In a more specific embodiment, the oxide semiconductor is indium gallium zinc oxide (InGaZnO, IGZO), which has the general formula In x Ga y Zn z O, where 0 < x < 1, 0 ≤ y ≤ 1, and 0 ≤ z ≤ 1. Indium gallium zinc oxide can be selectively doped with a metal and has the formula In x Ga y Zn z O:M, where M is titanium (Ti), aluminum (Al), silver (Ag), tungsten (W), cerium (Ce), tin (Sn), vanadium (V), or scandium (Sc).

[0050] Next, in Figure 1 step 120 and illustrated in Figure 6 , a colored lightshielding layer 240 is formed over the substrate, and more specifically, on the semiconductor layer 230. In a particular embodiment as shown, the colored lightshielding layer 240 directly contacts the semiconductor layer 230. The colored lightshielding layer 240 reduces exposure of the semiconductor layer to radiation in the wavelength range of about 10 nanometers to about 400 nanometers. The colored lightshielding layer 240 is not transparent and is deliberately made to have a very low light transmittance, especially for ultraviolet light.

[0051] In a particular embodiment, the colored lightshielding layer 240 appears white, black, red, yellow, or gray when viewed. White is generally considered the color that appears when all visible light wavelengths are reflected and / or scattered. Conversely, black is the color that appears when all visible light wavelengths are absorbed and not reflected / scattered. Red is the color that appears when light wavelengths in the range of 620 nanometers to 750 nanometers are reflected. Yellow is the color that appears when light wavelengths in the range of 570 nanometers to 590 nanometers are reflected. Gray is between black and white. In a more specific embodiment, the colored lightshielding layer appears black.

[0052] According to some disclosed embodiments, the colored light shielding layer 240 may be formed of materials such as metal oxide film, p-type oxide semiconductor or perovskite. Suitable examples of metal oxides may include titanium dioxide (TiO2, white), nickel oxide (NiO, black), ferric oxide (Fe2O3, red), cobalt (II, III) tetroxide (Co3O4, black), manganese (Mn3O4, black), copper oxide (CuO, black), antimony trioxide (Sb2O3, white / grey), tin oxide (SnO, black / red) and chromium trioxide (Cr2O3, brown / green). Other metal oxides may include rare earth oxides, i.e., oxides of cobalt (Sc), europium (Y), lanthanum (La), cerium (Ce), samarium (Pr), neodymium (Nd), promethium (Pm), vanadium (Sm), europium (Eu), gadolinium (Gd), terbium (Tb), dysprosium (Dy), holmium (Ho), erbium (Er), thulium (Tm), ytterbium (Yb) or lutetium (Lu). Specific rare earth oxide examples include cerium dioxide (CeO2, white / yellow), cerium trioxide (Y2O3, white) and neodymium trioxide (Nd2O3, blue / grey). Rare earth oxides may provide chemical / physical resistance to colored light shielding layers. P-type oxide semiconductors may include copper oxide (CuO), nickel oxide (NiO), cobalt tetraoxide (Co3O4) and chromium trioxide (Cr2O3). The perovskite referred to herein refers to a compound having the same crystalline structure as calcium titanate (CaTiO3). Perovskite may have a structure of the general formula ABO3, wherein A is an alkaline earth or rare-earth element, and B is a 3d, 4d or 5d transition element. There are also metal halide-derived perovskites, such as bismuth (Bi)-based perovskites. In specific embodiments, the perovskite includes calcium (Ca), strontium (Sr) or bismuth (Bi). In other specific embodiments, highvalence element oxides, such as those containing tetravalent titanium ions (Ti 4+ ), pentavalent tantalum ion (Ta 5+ ), tetravalent chromium ion (Cr 4+ ) etc., are used to suppress the generation of oxygen vacancies. It should be noted that the material of the colored light shielding layer 240 is different from that of the semiconductor layer 230.

[0053] The material forming the colored shielding layer 240 can be provided in the form of thin films, nanoparticles or nanocomposites, which can be appropriately selected according to the situation. The diameter of the nanoparticles is between 1 and 100 nanometers. The nanocomposite is a solid composed of multiple materials (or phases) and has at least one dimension of 100 nanometers or less.

[0054] The colored light shielding layer 240 can be formed by physical vapor deposition (PVD), chemical vapor deposition (CVD), atomic layer deposition (ALD), sputtering or other appropriate processes. In some specific embodiments, during the manufacture of the colored light shielding layer 240 or after its deposition, the layer can also be treated with ozone. This can be done by exposure to ozone or an ozone precursor. The oxygen atoms / radicals produced by ozone decomposition can make up for any defects that may exist in the colored light shielding layer 240. The ozone treatment method ideally fills any oxygen vacancies and can enhance the quality of the dense oxide film.

[0055] Please refer to Figure 6 The colored light shielding layer 240 has a thickness 245. In a specific embodiment, the thickness 245 of the colored light shielding layer 240 is about 1 angstrom (A) to about 100 angstroms. In more specific embodiments, the thickness 245 is about 10 angstroms to about 100 angstroms.

[0056] Then, in Figure 1 Step 125 and shown in Figure 7 In the embodiment of the present invention, a channel cover layer 250 is formed over the substrate, more specifically, over the colored light shielding layer 240. The channel cover layer 250 can reduce the exposure of the semiconductor layer to hydrogen atoms, which are known to damage oxide semiconductors. The channel cover layer 250 can be formed by physical vapor deposition (PVD), chemical vapor deposition (CVD) or atomic layer deposition (ALD) or other suitable processes. Suitable materials may include oxides such as silicon oxide, nitrides such as silicon nitride, or other dielectric materials. Please note that the presence of the channel cover layer 250 is optional, and an operable transistor can still be manufactured without the presence of this layer.

[0057] Then, in Figure 1 Step 130 and is shown in Figure 8In the process, the semiconductor layer 230 is patterned. This can be accomplished by providing and patterning a photoresist layer, etching to transfer the pattern to the semiconductor layer, and then removing the photoresist layer. As shown, the colored light shielding layer 240 and the channel cover layer 250 are also patterned. Please note that in this process step, the colored light shielding layer 240 has reduced the exposure of the semiconductor layer 230 to ultraviolet radiation.

[0058] Continue, in Figure 1 Step 135 and is shown in Fig. 9 In the process, an interlayer dielectric (ILD) layer 260 is provided above the semiconductor layer 230. Suitable methods and materials for forming the dielectric layer have been previously described and are also suitable for use in this process step. As shown, the semiconductor layer 230 is encapsulated by the interlayer dielectric layer.

[0059] Then, in Figure 1 Step 140 and shown in Fig.10 In the embodiment of the present invention, a source / drain region 268 in contact with the semiconductor layer 230 is formed by etching. A photoresist layer is provided on the interlayer dielectric layer and patterned, and each layer is etched using a different etching recipe. As shown in the figure, the source / drain region 268 is an empty volume extending through the interlayer dielectric layer 260, the channel cover layer 250 and the colored light shielding layer 240.

[0060] Next, in Figure 1 Step 145 and is shown in Fig.11 In the process, conductive material is deposited into the source / drain region to form source / drain 270. The same methods and materials used to form gate 210 described previously are also suitable for use in this process step. This figure also shows an example of a final bottom gate transistor 202. The semiconductor channel length 235 between the source / drain 270 can be about 1 nanometer to about 100 nanometers.

[0061] The gate dielectric layer 220 generally separates the gate 210 from the source / drain 270. The semiconductor layer 230 bridges the source / drain 270 and is in contact with the gate dielectric layer 220. The semiconductor layer 230 can also be considered to separate the gate 210 from the source / drain 270. In other words, the source / drain 270 and the gate 210 are located on opposite sides of the semiconductor layer 230 / gate dielectric layer 220.

[0062] Fig.12 A flow chart of a second method 300 for fabricating a transistor according to some disclosed embodiments is shown. Figures 13 to 20The steps of the second method are shown and discussed together. The drawings are shown with reference to a top-gate transistor.

[0063] Fig.13 Again, the substrate is shown at the initial stage before transistors are fabricated. Next, Fig.12 Step 305 and is shown in Fig.14 In the embodiment, source / drain 270 is formed on or in substrate 205. As shown in the figure, relative to Figures 2 to 11 In the process described, the source / drain 270 is shown in the substrate 205. For example, this can be accomplished by ion implantation. In simple terms, an ion implanter is used to implant atoms into a silicon crystal lattice to adjust the lattice conductivity at the implantation location. An ion implanter generally includes an ion source, an ion beam line, and a process chamber. The ion source generates the desired ions (here, for example, cobalt (Co), titanium (Ti), nickel (Ni), platinum (Pt), or lead (Pb), depending on the desired N-type or P-type electrode); the ion beam organizes the ions into a beam, which has high purity ion mass, energy, and species; then, the ion beam is irradiated to the chip substrate in the process chamber, the ion beam bombards the exposed area on the chip substrate, and the ions as dopants can be implanted into the substrate at a desired depth. Alternatively, the substrate may be partially etched, followed by blanket metal deposition, followed by annealing, where the metal reacts with the exposed silicon beneath it. The unreacted metal may then be removed, for example using a selective etch process.

[0064] Next, in Fig.12 Step 310 and is shown in Fig.15 In the embodiment, a semiconductor layer 230 is formed on the substrate, more specifically, on the source / drain 270. Then, Fig.12 Step 315 and is shown in Fig.16In the embodiment, the colored light shielding layer 240 is formed above the semiconductor layer 230. Furthermore, in a specific embodiment, the colored light shielding layer 240 is directly in contact with the semiconductor layer 230. During the manufacturing of the colored light shielding layer 240 or after its deposition, the layer can also be treated with ozone. Please note that the source / drain 270 should be fully covered by the semiconductor layer 230 and / or the colored light shielding layer 240, because exposure to oxygen may cause adhesion problems of the source / drain 270 due to oxidation, especially when the source / drain 270 is composed of metal.

[0065] If necessary, Fig.12 In the optional step 320 , the channel cover layer 250 is formed on the semiconductor layer 230 and may also be located on the colored light shielding layer 240 .

[0066] Then, in Fig.12 Step 325 and is shown in Fig.17 In the process, the semiconductor layer 230 is patterned. The semiconductor layer 230 is patterned to contact the source and drain electrodes 270 at the same time. Fig.12 Step 330 and is shown in Fig.18 In the embodiment of the present invention, a gate dielectric layer 220 is formed in contact with the semiconductor layer 230. As shown in the figure, the colored light shielding layer 240 must be etched before forming the gate dielectric layer 220. However, because the gate dielectric layer 220 is shorter than the semiconductor layer 230, part of the colored light shielding layer 240 still exists.

[0067] Then, in Fig.12 Step 335 and is shown in Fig.19 In the embodiment, gate 210 is formed on gate dielectric layer 220. Finally, in Fig.12 Step 340 and is shown in Fig. 20 In the figure, an interlayer dielectric layer 260 is formed above the semiconductor layer 230. As shown, the interlayer dielectric layer 260 is also etched to form a gap 262 that allows electrical contact with the gate 210. This figure also shows the final top-gate transistor 204. Please note that the semiconductor layer 230 does not need to fully cover the source / drain 270.

[0068] In some embodiments of the second method 300 of manufacturing a transistor, when manufacturing a top gate transistor, the colored light shielding layer 240 can be composed of a material that also serves as a dielectric layer. As previously described, such dielectric materials can include metal oxide films, P-type oxide semiconductors, or perovskites. In these embodiments, the colored light shielding layer 240 can also serve as a gate dielectric layer, and there is no need to form a separate gate dielectric layer.

[0069] Fig.21 According to some disclosed embodiments, a flow chart of a second method 300 for manufacturing a transistor is shown. Initially, steps 305, 310, 315, 320 (optional), and 325 are performed with Fig.12 As well as Figures 13 to 17 The steps shown are identical. Note that in these embodiments, the material used in the semiconductor layer 230 is different from the material used in the colored light shielding layer 240.

[0070] Then, in Fig.21 Step 337 and is shown in Fig. 22 In the embodiment, the gate 210 is formed on the colored light shielding layer 240. Then, Fig.21 Step 340 and is shown in Fig.23 In the embodiment of the present invention, an interlayer dielectric layer 260 is formed over the semiconductor layer 230. Furthermore, the interlayer dielectric layer 260 includes a gap 262 that allows electrical contact with the gate 210.

[0071] Note that in some applications, gate 210 is referred to as a write line, one of source / drain 270 is referred to as a source line, and the other source / drain 270 is referred to as a bit line. These terms are used interchangeably and should be considered to apply equally to the previous discussion of transistors. Also note that although Figures 1 to 23 A single transistor is shown formed on a chip substrate, but during chip production, a large number of transistors are simultaneously formed on a chip substrate. Please understand the present disclosure accordingly.

[0072] The transistors formed can be used in a variety of different applications and systems. Transistors can be used in charge coupled devices (CCDs), complementary metal-oxide semiconductor (CMOS) image sensors, contact image sensors (CIS), and ambient light sensors (ALS). Such sensors can be used in systems such as mobile phones, facial recognition systems, or as motion sensors for automotive applications, security applications, and energy applications. Random access memory uses transistors to read and write bit values ​​to memory cells (nonvolatile or volatile). Transistors can be integrated with Micro-Electro-Mechanical Systems (MEMS) devices on a single chip. MEMS devices can include multiple components formed from metals, polysilicon, dielectrics, and / or other materials. MEMS devices can include mechanical structures, electronic structures, or fluid structures.

[0073] The addition of a colored light shielding layer provides many advantages. First, the presence of a colored light shielding layer reduces defects in the semiconductor layer that may be caused by exposure to ultraviolet light, especially when using oxide semiconductors. For example, processes that use ultraviolet light, such as curing some photoresists or forming an intermetallic dielectric (IMD) layer in a back-end process. Ultraviolet curing is also widely used in some applications, such as adhesive bonding and assembly, component marking, gasketing and sealing, potting, masking, encapsulating and conformal coating, wafer masking, wafer contamination inspection, and wafer polishing inspection. Secondly, the surface of oxide semiconductors is generally hydrophilic, and the presence of a colored light shielding layer reduces the absorption of hydrogen and water that may occur in the semiconductor layer due to exposure during various process steps. Third, the highly chemically and physically resistant stabilizing layer can reduce chemical or physical damage to the semiconductor layer that may occur during the various process steps of the chip substrate during chip production. Finally, the use of a colored light shielding layer will also reduce the number of oxygen vacancies and photoinduced holes that may be generated in the semiconductor layer. This in turn reduces the change in charge carrier concentration that may be generated in the semiconductor layer. Charge carrier concentration is an important indicator for maintaining high carrier mobility and high-speed driving, thereby improving the reliability of the entire semiconductor device.

[0074] The colored light shielding layer shown is used in a two-dimensional field effect transistor. However, the colored light shielding layer can also be provided for use in three-dimensional transistors, such as fin field effect transistors (FinFETs) and gate-all-around (GAA) transistors.

[0075] In many embodiments, the transistor disclosed herein is a transistor including a colored light shielding layer above a semiconductor layer. The colored light shielding layer reduces exposure of the semiconductor layer to radiation having a wavelength of about 10 nanometers to about 400 nanometers. The colored light shielding layer has white, black, red, yellow, or gray.

[0076] In a plurality of embodiments, there are also disclosed transistors including a write line, a semiconductor layer, a source line, a bit line, and a colored light shielding layer. The source line and the bit line are in contact with the semiconductor layer. The colored light shielding layer includes a dielectric material and can be used as a gate dielectric layer. Examples of such materials include titanium dioxide (TiO2), nickel oxide (NiO), ferric oxide (Fe2O3), cobalt oxide (Co3O4), manganese oxide (Mn3O4), copper oxide (CuO), antimony oxide (Sb2O3), tin oxide (SnO), chromium oxide (Cr2O3), rare earth oxides, cerium dioxide (CeO2), yttrium oxide (Y2O3), neodymium oxide (Nd2O3), or perovskite including calcium (Ca), strontium (Sr), or bismuth (Bi). In some embodiments, the colored light shielding layer is in contact with the semiconductor layer and the write line, for example, located between the semiconductor layer and the write line. In some alternative embodiments, a separate gate dielectric layer contacts the write line and the semiconductor layer. In other embodiments, a channel cap layer may be located above the colored light shielding layer.

[0077] In a plurality of embodiments, there are also disclosed transistors including a write line, a gate dielectric layer, an oxide semiconductor layer, a source line, a bit line, a colored light shielding layer, and a channel cover layer. The gate dielectric layer contacts the write line. The oxide semiconductor layer contacts the gate dielectric layer. The source line and the bit line contact the oxide semiconductor layer. The colored light shielding layer contacts the oxide semiconductor layer. The colored light shielding layer includes titanium dioxide (TiO2), nickel oxide (NiO), iron oxide (Fe2O3), cobalt oxide (Co3O4), manganese oxide (Mn3O4), copper oxide (CuO), antimony oxide (Sb2O3), tin oxide (SnO), chromium oxide (Cr2O3), rare earth oxides, cerium oxide (CeO2), yttrium oxide (Y2O3), neodymium oxide (Nd2O3), or perovskite including calcium (Ca), strontium (Sr), or bismuth (Bi). The channel cover layer is located above the colored light shielding layer.

[0078] In a plurality of embodiments, there are also disclosed transistors including a write line, a semiconductor layer, a source line, a bit line, a colored light shielding layer, and a channel cover layer. The gate dielectric layer contacts the write line. The oxide semiconductor layer contacts the gate dielectric layer. The source line and the bit line contact the oxide semiconductor layer. The colored light shielding layer contacts the oxide semiconductor layer. The colored light shielding layer includes titanium dioxide (TiO2), nickel oxide (NiO), iron oxide (Fe2O3), cobalt oxide (Co3O4), manganese oxide (Mn3O4), copper oxide (CuO), antimony oxide (Sb2O3), tin oxide (SnO), chromium oxide (Cr2O3), rare earth oxides, cerium oxide (CeO2), yttrium oxide (Y2O3), neodymium oxide (Nd2O3), or perovskite including calcium (Ca), strontium (Sr), or bismuth (Bi). The channel cover layer is located above the colored light shielding layer.

[0079] Also disclosed are a plurality of methods for manufacturing transistors, including forming a semiconductor layer on a substrate and forming a colored light shielding layer above the semiconductor layer. The colored light shielding layer reduces exposure of the semiconductor layer to radiation having a wavelength of about 10 nanometers to about 400 nanometers.

[0080] The features of several embodiments are summarized above so that those skilled in the art can better understand the various aspects of the present disclosure. Those skilled in the art should understand that they can easily use the present disclosure as a basis for designing or modifying other processes and structures to implement the same purposes and / or achieve the same advantages as the embodiments described herein. Those skilled in the art should also recognize that various changes, substitutions and modifications can be made to such equivalent constructions without departing from the spirit and scope of the present disclosure.

Claims

1. A transistor, characterized in that: Includes a colored light shielding layer above the semiconductor layer, wherein the colored light shielding layer reduces exposure of the semiconductor layer to radiation with a wavelength of about 10 nanometers to about 400 nanometers; and wherein the colored light shielding layer has white, black, red, yellow or gray color.

2. The transistor according to claim 1, characterized in that The colored light shielding layer is formed of a metal oxide film, a P-type oxide semiconductor or a perovskite.

3. The transistor according to claim 1, characterized in that The colored light shielding layer includes titanium dioxide, nickel oxide, ferric oxide, cobalt oxide, manganese oxide, copper oxide, antimony oxide, tin oxide, chromium oxide, rare earth oxide, cerium dioxide, yttrium oxide, neodymium oxide or perovskite including calcium, strontium or bismuth.

4. The transistor according to claim 1, characterized in that The semiconductor layer is formed of an oxide semiconductor.

5. The transistor according to claim 4, characterized in that The oxide semiconductor is indium gallium zinc oxygen selectively doped with metal.

6. The transistor according to claim 5, characterized in that The oxide semiconductor is doped with the metal, and the metal is titanium, aluminum, silver, tungsten, cerium, tin, vanadium, or scandium.

7. The transistor according to claim 1, characterized in that A dielectric layer is further included.

8. The transistor according to claim 7, characterized in that The dielectric layer includes a high dielectric material, an oxide-nitride-oxide material or a ferroelectric material.

9. A transistor, characterized in that: include: Write line; Semiconductor layer; a source line and a bit line contacting the semiconductor layer; as well as A colored light shielding layer in contact with the semiconductor layer and located between the semiconductor layer and the writing line, wherein the colored light shielding layer includes titanium dioxide, nickel oxide, ferric oxide, cobalt oxide, manganese oxide, copper oxide, antimony oxide, tin oxide, chromium oxide, rare earth oxide, cerium dioxide, yttrium oxide, neodymium oxide or perovskite including calcium, strontium or bismuth.

10. A method for manufacturing a transistor, characterized in that: include: a semiconductor layer formed on a substrate; as well as A colored light shielding layer is formed over the semiconductor layer, wherein the colored light shielding layer reduces exposure of the semiconductor layer to radiation having a wavelength of about 10 nanometers to about 400 nanometers.