Alkali metal atom gas chamber with double-quadrangular frustum pyramid structure and manufacturing method of alkali metal atom gas chamber
By using an alkali metal gas cell with a double quadrangular frustum structure and employing etching and anodic bonding processes, the problems of low fabrication efficiency and triaxial optical path integration in existing alkali metal gas cell fabrication methods have been solved, achieving temperature uniformity and large-scale production of gas cells.
Patent Information
- Application Number
- CN202410988527.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-23
- Publication Date
- 2024-11-15
AI Technical Summary
Existing alkali metal gas chambers have low preparation efficiency, large size, and poor consistency, making it difficult to achieve large-scale industrial production. Furthermore, traditional gas chambers are difficult to integrate with triaxial optical paths and meet the requirements for temperature uniformity.
The alkali metal gas chamber with a double quadrangular frustum structure includes a P-type crystal double-sided polished silicon wafer and two glass cover plates. The working gas chamber and the auxiliary gas chamber are connected by a microchannel. The alkali metal releasing agent reacts in the auxiliary gas chamber to generate vapor and enters the working gas chamber through the microchannel. It is prepared by etching and anodic bonding processes.
A simplified fabrication process for the gas chamber was achieved, improving temperature uniformity and triaxial optical path integration, reducing processing costs and leakage risks, making it suitable for large-scale production.
Smart Images

Figure CN118971875A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the fields of quantum optics, atomic clock technology and atomic gyroscope, and in particular to an alkali metal atomic gas chamber with a double tetrahedral structure and a manufacturing method thereof. Background Art
[0002] The rapid development of quantum physics technology and atomic optics has enabled the development of atomic gyroscopes, atomic clocks, and atomic magnetometers based on the quantum principle of alkali metal energy level transitions. Alkali metal atomic gas chambers are the core components of these devices. At present, the existing gas chambers are mainly prepared using glass bubble blowing technology, but this method has low preparation efficiency and the gas chambers are large in size and poor in consistency, making it difficult to achieve large-scale industrial production. In recent years, as related instruments have become increasingly integrated and miniaturized, higher requirements have been placed on the performance and structure of alkali metal gas chambers.
[0003] Equipment such as atomic gyroscopes and atomic magnetometers have high requirements for temperature. When in use, the gas chamber temperature is required to reach 80-120°C and have high uniformity. Glass has poor thermal conductivity, and the gas chamber made of it puts higher heating power requirements and heat shielding requirements on the system, increases the volume and power consumption of the system, and is not convenient for miniaturization of the system. At the same time, miniaturization also requires the gas chamber to be able to cooperate with micro-optical components to achieve the integration of 3-axis optical paths, while traditional transmission-type gas chambers are difficult to further compress the volume of the optical path, and the materials used for manufacturing are limited due to the transparency requirements of the gas chamber. How to design an alkali metal gas chamber with simpler process, higher temperature uniformity, easy preparation and meeting the requirements of three-axis optical path integration has become a research issue at this stage. Summary of the invention
[0004] In order to solve the problems raised in the above background technology, simplify the manufacturing process, improve the temperature uniformity, and realize the three-axis optical path integration, the present invention proposes an alkali metal gas chamber with a double tetrahedral structure.
[0005] The alkali metal atomic gas chamber of the double tetrahedral structure of the present invention comprises a P-type crystal surface double-sided polished silicon wafer, an upper glass sheet cover bonded to the upper polished surface of the silicon wafer, and a lower glass sheet cover bonded to the lower polished surface of the silicon wafer;
[0006] A working gas chamber, a microchannel and an auxiliary gas chamber are etched in the P-type crystal surface double-sided polished silicon wafer, the working gas chamber and the auxiliary gas chamber are connected through the microchannel, the working gas chamber passes through the P-type crystal surface double-sided polished silicon wafer along the connecting direction of the two glass cover plates, and the working gas chamber is composed of two identical regular tetrahedral pyramids vertically spliced, and the bottom surfaces of the two regular tetrahedral pyramids with smaller areas are spliced with each other and completely overlap;
[0007] An alkali metal release agent is arranged in the auxiliary gas chamber, and the alkali metal release agent is used for releasing alkali metal vapor;
[0008] The working gas chamber is the gas chamber where the pumping and detection processes occur, the auxiliary gas chamber is the reaction space where the alkali metal releaser generates alkali metal vapor, and the microchannel is the channel for transmitting the alkali metal vapor.
[0009] Furthermore, the auxiliary gas chamber has a cubic structure and does not penetrate the P-type crystal double-sided polished silicon wafer; the auxiliary gas chamber is sealed by an on-chip heating film, and the on-chip heating film heats the alkali metal releaser to cause the alkali metal releaser to undergo a chemical reaction to generate alkali metal vapor, and the alkali metal vapor enters the working gas chamber through the microchannel.
[0010] The present invention also provides a method for preparing the alkali metal atom gas chamber, comprising the following steps:
[0011] 1) cleaning the surface of the P-type crystal surface double-sided polished silicon wafer, and baking and preheating the P-type crystal surface double-sided polished silicon wafer;
[0012] The cleaning of the surface of the P-type crystal double-sided polished silicon wafer comprises sequentially cleaning the surface of the silicon wafer with deionized water and acetone to remove impurities and water vapor on the surface of the silicon wafer;
[0013] The baking preheating temperature is 100° C. The purpose of the baking preheating is to remove the deionized water and acetone on the surface of the silicon wafer and to preheat the P-type double-sided polished silicon wafer to enhance the adhesion effect of the adhesion promoter;
[0014] 2) applying an adhesion promoter to the two polished surfaces of the P-type crystal surface double-sided polished silicon wafer, and performing a pre-baking treatment; cooling the P-type crystal surface double-sided polished silicon wafer after the pre-baking treatment to room temperature, and applying photoresist to the two polished surfaces of the P-type crystal surface double-sided polished silicon wafer for multiple times and baking for multiple times;
[0015] 3) The upper polished surface of the double-sided polished silicon wafer of the P-type crystal surface is subjected to photolithography processing to form the upper half of the working gas chamber, the auxiliary gas chamber and the microchannel; the lower polished surface of the double-sided polished silicon wafer of the P-type crystal surface is subjected to photolithography processing to form the lower half of the working gas chamber, and the upper half and the lower half of the working gas chamber are connected;
[0016] 4) cleaning the silicon wafer processed in step 3), and bonding a lower glass cover plate to the lower polished surface of the P-type crystal double-sided polished silicon wafer;
[0017] 5) adding an alkali metal release agent to the auxiliary gas chamber, and sealing the auxiliary gas chamber with an on-chip heating film; bonding an upper glass cover plate to the upper polished surface of the P-type crystal double-sided polished silicon wafer; and the auxiliary gas chamber after bonding needs to be reserved with a wire channel, and the wire channel is used to pass the wire for energizing the on-chip heating film;
[0018] 6) applying alternating current to the on-chip heating film, causing the alkali metal releaser to undergo a chemical reaction to generate alkali metal vapor, which then enters the working gas chamber through the microchannel, and then the wire channel is sealed, and the double tetrahedral alkali metal atomic gas chamber is completed.
[0019] Furthermore, in step 2), the adhesion promoter is hexamethyldisilazane adhesion promoter (10), the temperature of the pre-baking treatment is 90° C.-110° C., and the thickness of the applied adhesion promoter is 14 nm-16 nm.
[0020] Furthermore, in step 3), the photolithography process is specifically as follows: firstly, the polished surface of the P-type crystal double-sided polished silicon wafer (1) is exposed and etched; the etching adopts a deep silicon etching process, during the etching, C4F8 plasma is first used to cover the polished surface of the P-type crystal double-sided polished silicon wafer (1), and then SF6 plasma is injected for etching; and the roughness of the inner surface of the working gas chamber (4) obtained by etching is less than 50nm.
[0021] Furthermore, the bonding in step 4) and step 5) adopts a glass-silicon-glass three-layer anodic bonding method, and the upper glass cover plate (2) and the lower glass cover plate (3) are both BF33 glass;
[0022] The bonding of the lower glass cover plate (3) occurs at a depth of less than 1.5×10 -5 Under a vacuum condition of 1000 mbar, a pressure of 900-1100 N is applied to the lower glass sheet cover plate (3) to make it closely fit the silicon wafer and heat it to 290-310° C., and a pulse voltage with a peak value of 590-610 V and a gradually decreasing peak duration is applied between the P-type crystal surface double-sided polished silicon wafer (1) and the lower glass sheet cover plate (3) to complete bonding;
[0023] The bonding of the upper glass sheet cover plate (2) is carried out in a buffer gas atmosphere, wherein the buffer gas comprises N2, 131 Xe and 129 Xe, applying a pressure of 900-1100N to the upper glass sheet cover plate (2) to make it closely fit the silicon wafer and heating it to 290-310°C, and applying a pulse voltage with a peak value of 590-610V and a gradually decreasing peak duration between the P-type crystal surface double-sided polished silicon wafer (1) and the upper glass sheet cover plate (2) to complete bonding.
[0024] Compared with the prior art, the present invention has the following advantages:
[0025] The double tetrahedral alkali metal gas chamber of the present invention adopts a double gas chamber structure with an auxiliary gas chamber and a working gas chamber separated, and the gas chambers are connected by microchannels. The reaction position of the alkali metal atom releaser is separated from the working position of the alkali metal vapor to avoid the high temperature required for the excitation reaction from destroying the working gas chamber structure, and at the same time avoid residual reactants from affecting the transparency and relaxation performance of the gas chamber. Compared with the traditional gas injection method, the preparation process of first closing the gas chamber and then chemically reacting to generate alkali metal vapor reduces the operating environment requirements, reduces the processing cost, and also avoids the damage to the gas chamber structure by the reserved injection channel, while avoiding the risk of leakage. The traditional transmission type gas chamber for realizing the three-axis optical path is mostly a glass gas chamber due to the transparency requirement of the substrate. The shape of the gas chamber of the present invention is a double tetrahedral prism, and the corresponding optical path is a refractive optical path. The opaque single crystal silicon material can be used as the substrate to realize the three-axis optical path. The thermal conductivity of single crystal silicon is much greater than that of glass, which can achieve higher uniformity of gas chamber temperature. Compared with a glass gas chamber, the gas chamber of the present invention adopts an etching process and an anodic bonding process, has a simple structure, high process maturity, good repeatability, and is more convenient for large-scale production. BRIEF DESCRIPTION OF THE DRAWINGS
[0026] Figure 1 The overall structural schematic diagram of the alkali metal atom gas chamber of the double tetrahedral structure of the present invention;
[0027] Figure 2 A three-dimensional diagram of the alkali metal atom gas chamber of the double tetrahedral structure of the present invention;
[0028] Figure 3 It is a cross-sectional view of the alkali metal atom gas cell of the double tetrahedral structure of the present invention;
[0029] Figure 4 It is a schematic diagram of the preparation process of the alkali metal atom gas cell with a double tetrahedral structure of the present invention;
[0030] In the figure, 1-P-type crystal double-sided polished silicon wafer, 2-upper glass cover plate, 3-lower glass cover plate, 4-working gas chamber, 5-microchannel, 6-on-chip heating film, 7-auxiliary gas chamber, 8-alkali metal release agent, 9-photoresist, 10-hexamethyldisilazane adhesion promoter, 11-AC power supply. DETAILED DESCRIPTION
[0031] The present invention is further described and illustrated below in conjunction with specific embodiments. The embodiments are merely exemplary of the present disclosure and do not define the scope of limitation. The technical features of each embodiment of the present invention may be combined accordingly without conflicting with each other.
[0032] Combination Figure 1 , Figure 2 , Figure 3As shown, the double tetrahedral alkali metal gas chamber of the present invention comprises a P-type crystal surface double-sided polished silicon wafer 1 and two glass cover plates. The P-type crystal surface double-sided polished silicon wafer 1 also has a working gas chamber 4 and an auxiliary gas chamber 7 and a microchannel 5 connecting the working gas chamber 4 and the auxiliary gas chamber 7. The two glass cover plates are bonded to the polished upper and lower surfaces of the P-type crystal surface double-sided polished silicon wafer 1, respectively, and cover the working gas chamber 4, the auxiliary gas chamber 7 and the microchannel 5. The working gas chamber 4 is the gas chamber where the pumping and detection processes are located when the instrument is working, the auxiliary gas chamber 7 is the alkali metal release agent 8 placement and reaction space, and the microchannel 5 is the release gas channel. The alkali metal release agent 8 can be an Rb release agent; the crystal phase of the P-type crystal surface double-sided polished silicon wafer is 100.
[0033] The working gas chamber 4 is separated from the auxiliary gas chamber 7 and connected by a microchannel 5. The alkali metal vapor is generated by a chemical reaction in the auxiliary gas chamber 7 by heating the alkali metal releaser 8 through the on-chip heating film 6. The alkali metal vapor enters the working gas chamber 4 through the microchannel 5. The reaction position of the alkali metal releaser 8 is separated from the working position of the alkali metal vapor, so as to avoid the high temperature required for the excitation reaction from damaging the working gas chamber structure and at the same time avoid the residual reactants from affecting the transparency and relaxation performance of the gas chamber, thereby improving the sensitivity of the sensor. There are multiple microchannels 5.
[0034] The working gas chamber penetrates the silicon wafer in the direction perpendicular to the polished surface of the P-type (crystal phase 100) crystal face silicon wafer, while the auxiliary gas chamber and the microchannel do not penetrate the silicon wafer in the direction perpendicular to the polished surface of the P-type (100) crystal face silicon wafer. The working gas chamber is a double quadrangular pyramid structure, the bottom surfaces of the two pyramids are square, respectively located on the upper and lower polished surfaces of the P-type (100) crystal face double-sided polished silicon wafer and aligned perpendicular to the polished surface of the silicon wafer; the top surface of the pyramid is square, located in the middle of the gas chamber parallel to the polished surface of the P-type (100) crystal face double-sided polished silicon wafer, the center of the square is aligned with the center of the bottom surface of the pyramid perpendicular to the polished surface of the silicon wafer, and is shared by the upper and lower pyramids.
[0035] The auxiliary gas chamber 7 is in a cubic structure, one side of which is located on the front polished surface of the P-type (100) crystal plane double-sided polished silicon wafer.
[0036] When using an alkali metal atom gas cell, the detection light or pump light emitted by an external light source is incident on the inclined surface of the working gas cell perpendicular to the z direction. The light is reflected by the side surface of the tetrahedron (the inclined surface of the working gas cell) to become parallel light in the x direction or y direction. After passing through the side surface opposite to the side surface, the reflected x direction or y direction is reflected again and then emitted from the working gas cell. If the detection light or pump light emitted by the external light source does not pass through the side surface of the tetrahedron (the inclined surface of the working gas cell), the incident light is reflected by the glass cover plate and directly passes through the working gas cell to become parallel light in the z direction. The upper and lower tetrahedral sides are the working areas for generating parallel light in the x and y directions, respectively.
[0037] In a specific embodiment of the present invention, Figure 2 As shown, there are two microchannels in a rectangular structure, with long sides arranged parallel to each other on the polished surface of a P-type (100) crystal double-sided polished silicon wafer, connecting the working gas chamber and the auxiliary gas chamber.
[0038] As one of the preferred embodiments of the present invention, the main structural dimensions of the alkali metal atom gas cell of the double tetrahedral structure of the present invention are as follows:
[0039] The overall dimensions of the double tetrahedral alkali metal gas chamber are: length × width × height = 8 mm × 5 mm × 2 mm;
[0040] The bottom surface size of the working air chamber 4 is: length × width = 3mm × 3mm;
[0041] The height of the working air chamber 4 is: height = 1 mm;
[0042] The angle between the bottom and the side of the working air chamber 4 is: angle = 54.7°;
[0043] The dimensions of the auxiliary air chamber 7 are: length×width×height=1mm×1mm×1mm;
[0044] The dimensions of the microchannel 5 are: number × length × width × height = 2 × 1 mm × 0.1 mm × 0.1 mm;
[0045] The size of the glass cover plate 2 is: length×width×height=8mm×5mm×0.3mm.
[0046] like Figure 4 As shown, as one of the preferred embodiments of the present invention, the main steps of preparing the alkali metal atom gas cell with a double tetrahedral structure of the present invention are as follows:
[0047] 1) Use 200 mL of deionized water and 50 mL of acetone to clean the surface of the silicon wafer, repeat twice to remove debris and water vapor on the surface of the silicon wafer, and bake the silicon wafer to 100° C. to remove the deionized water and acetone on the surface of the silicon wafer and preheat the silicon wafer.
[0048] 2) After baking, hexamethyldisilazane adhesion promoter is applied on the front and back sides of the double-sided polished silicon wafer with a P-type (100) crystal surface by spin coating, and pre-baked in an oven at 100° C. to obtain a 15 nm thick adhesion promoter film; cooled to room temperature, photoresist is applied on the front and back sides of the silicon wafer by spin coating, and after a layer of photoresist is applied, it is baked at 60° C., and applied again after cooling, and the above process is repeated for multiple applications; the following is obtained: Figure 4 As a preferred embodiment of the present invention, the total number of coating times may be three times.
[0049] 3) using a photolithography machine to align with the front side of the P-type (100) crystal surface double-sided polished silicon wafer, and exposing the front side of the P-type (100) crystal surface double-sided polished silicon wafer; Figure 4 As shown in (b); C4F8 plasma is used to cover the front of the silicon wafer, and SF6 plasma is introduced for etching. After a period of time, the SF6 plasma is stopped, and C4F8 plasma is used to cover the front of the silicon wafer again. Passivation and etching are repeated until the front half of the working gas chamber and the auxiliary gas chamber are formed, as shown in FIG. Figure 4 As shown in (c);
[0050] Then, back-side photolithography is performed, and the photolithography machine is aligned with the front pattern and then exposed, and the atomic gas chamber structure is transferred to the back side of the unetched P-type (100) crystal surface double-sided polished silicon wafer, such as Figure 4 As shown in (d), the back of the silicon wafer is covered with C4F8 plasma, and SF6 plasma is introduced for etching. After a period of time, the introduction of SF6 plasma is stopped, and C4F8 plasma is used to cover the back of the silicon wafer again. Passivation and etching are repeated until the back half of the working gas chamber is formed, as shown in FIG. Figure 4 As shown in (e);
[0051] Finally, SF6 plasma etching is used to form microchannels, such as Figure 4 As shown in (f) in .
[0052] 4) Clean the structure obtained after etching, and -5 Under vacuum conditions of 1000 mbar, the back of the silicon cavity structure is bonded to the second glass cover plate, and a pressure of 1000N is applied to make them fit tightly and heated to 300°C. Then, a pulse voltage with a peak value of 600V and a gradually decreasing peak duration is applied between the P-type (100) crystal surface double-sided polished silicon wafer and the glass cover plate to complete the first anodic bonding. Figure 4 As shown in (g) in .
[0053] 5) Use a dropper to drop an alkali metal releaser (e.g., a rubidium atom releaser) into the auxiliary gas chamber, and use an on-chip heating film to seal the auxiliary gas chamber, such as Figure 4 As shown in (h); in the buffer gas N2 and two isotopes of Xe 131 Xe, 129 Under the condition of Xe atmosphere, the front side of the silicon cavity structure is bonded to the first glass cover plate, and a pressure of 1000N is applied to make them bond tightly and heated to 300℃. Then, a pulse voltage with a peak value of 600V and a gradually decreasing peak duration is applied between the P-type (100) crystal surface double-sided polished silicon wafer and the glass cover plate to complete the second anodic bonding. Figure 4 As shown in (i); and the auxiliary air chamber 7 after bonding needs to have a wire channel reserved, and the wire channel is used to pass the wire that energizes the on-chip heating film 6.
[0054] 6) The on-chip heating film is connected to a power source through a wire to generate high temperature, and the rubidium atom release agent undergoes a chemical reaction to generate rubidium vapor, which enters the working gas chamber through a microchannel. Subsequently, a high-temperature glue is used to seal the circuit interface, and the alkali metal atom gas chamber is prepared. Figure 4 As shown in (j) in .
[0055] In step 2), the effective ingredient of the adhesion promoter is hexamethyldisilazane; and step 2) adopts a thick photoresist manufacturing process, and the photoresist is thickened by multiple coatings.
[0056] In step 3), a deep silicon etching process is adopted, SF6 plasma is used as the corrosive gas, C4F8 plasma is used as the protective gas, etching and passivation protection are alternated multiple times, and the angle between the side and bottom of the chamber formed by etching is 54.7°; and the etching process is carried out in a low temperature environment to reduce the reactivity of the etching gas and the silicon structure, and reduce the roughness caused by defects on the surface of the MEMS air chamber. The surface roughness of the air chamber is less than 50nm.
[0057] The above-mentioned embodiments only express several implementation modes of the present invention, and the description is relatively specific and detailed, but it cannot be understood as limiting the scope of the present invention. For those skilled in the art, several modifications and improvements can be made without departing from the concept of the present invention, which all belong to the protection scope of the present invention.
Claims
1. An alkali metal atom gas cell with a double tetrahedral structure, characterized in that: It comprises a P-type crystal double-sided polished silicon wafer (1), an upper glass sheet cover plate (2) bonded to the upper polished surface of the silicon wafer, and a lower glass sheet cover plate (3) bonded to the lower polished surface of the silicon wafer; A working air chamber (4), a microchannel (5) and an auxiliary air chamber (6) are etched inside a P-type crystal surface double-sided polished silicon wafer (1); the working air chamber (4) and the auxiliary air chamber (6) are connected via the microchannel (5); the working air chamber (4) penetrates the P-type crystal surface double-sided polished silicon wafer (1) along the direction of the line connecting the two glass cover plates; the working air chamber (4) is composed of two identical regular tetrahedral pyramids that are vertically spliced together; the bottom surfaces of the two regular tetrahedral pyramids with smaller areas are spliced together and completely overlap; An alkali metal release agent (8) is arranged in the auxiliary gas chamber (7), and the alkali metal release agent (8) is used to release alkali metal vapor; The working gas chamber (4) is the gas chamber where the pumping and detection processes occur, the auxiliary gas chamber (7) is the reaction space where the alkali metal releaser (8) generates alkali metal vapor, and the microchannel is the channel for transmitting the alkali metal vapor.
2. The alkali metal atom gas cell with a double tetrahedral structure according to claim 1, characterized in that: The crystal phase of the P-type crystal surface double-sided polished silicon wafer (1) is 100.
3. The alkali metal atom gas cell of the double tetrahedral structure according to claim 1, characterized in that: The auxiliary gas chamber (7) has a cubic structure and does not penetrate the P-type crystal surface double-sided polished silicon wafer (1); the auxiliary gas chamber (7) is sealed by an on-chip heating film (6), and the on-chip heating film (6) heats the alkali metal release agent (8) to cause the alkali metal release agent (8) to undergo a chemical reaction to generate alkali metal vapor, and the alkali metal vapor enters the working gas chamber (4) through a microchannel (5).
4. The alkali metal atom gas cell with a double tetrahedral structure according to claim 1, characterized in that: The alkali metal releasing agent (8) is a Rb releasing agent.
5. The alkali metal atom gas cell with a double tetrahedral structure according to claim 1, characterized in that: There are multiple microchannels (5).
6. A method for preparing the alkali metal atom gas cell according to claim 1, characterized in that: The steps include: 1) cleaning the surface of a P-type crystal surface double-sided polished silicon wafer (1), and preheating the P-type crystal surface double-sided polished silicon wafer (1); 2) applying an adhesion promoter to the two polished surfaces of the P-type double-sided polished silicon wafer (1), and performing a pre-baking treatment; The P-type crystal surface double-sided polished silicon wafer (1) after pre-baking is cooled to room temperature, and photoresist is applied to the two polished surfaces of the P-type crystal surface double-sided polished silicon wafer (1) for multiple times and baked for multiple times; 3) performing photolithography on the upper polished surface of the P-type crystal double-sided polished silicon wafer (1) to form the upper half of the working gas chamber (4), the auxiliary gas chamber (7) and the microchannel (5); then performing photolithography on the lower polished surface of the P-type crystal double-sided polished silicon wafer (1) to form the lower half of the working gas chamber (4), and the upper half and the lower half of the working gas chamber (4) are connected; 4) cleaning the silicon wafer processed in step 3), and bonding a lower glass cover plate (3) to the lower polished surface of the P-type crystal double-sided polished silicon wafer (4); 5) adding an alkali metal release agent (8) into the auxiliary gas chamber (7), and using an on-chip heating film (6) to seal the auxiliary gas chamber (7); and bonding an upper glass cover plate (2) to the upper polished surface of the P-type crystal double-sided polished silicon wafer (4); and the auxiliary gas chamber (7) after bonding needs to be reserved with a wire channel, and the wire channel is used to pass a wire for energizing the on-chip heating film (6); 6) applying alternating current to the on-chip heating film (6), causing the alkali metal release agent (8) to undergo a chemical reaction to generate alkali metal vapor, which then enters the working gas chamber (4) through the microchannel (5), and then the channel reserved with the wire is sealed, and the preparation of the double tetrahedral alkali metal atomic gas chamber is completed.
7. The method for preparing an alkali metal atom gas cell according to claim 6, characterized in that: In step 2), the adhesion promoter is hexamethyldisilazane adhesion promoter (10), the temperature of the pre-baking treatment is 90° C.-110° C., and the thickness of the applied adhesion promoter is 14 nm-16 nm.
8. The method for preparing an alkali metal atom gas cell according to claim 6, characterized in that: In step 3), the photolithography process is specifically as follows: firstly, the polished surface of the P-type crystal double-sided polished silicon wafer (1) is exposed and etched; the etching adopts a deep silicon etching process, during the etching, C4F8 plasma is first used to cover the polished surface of the P-type crystal double-sided polished silicon wafer (1), and then SF6 plasma is injected for etching; and the roughness of the inner surface of the working gas chamber (4) obtained by etching is less than 50nm.
9. The method for preparing an alkali metal atom gas cell according to claim 8, characterized in that: The bonding in step 4) and step 5) adopts a glass-silicon-glass three-layer anodic bonding method, and the upper glass cover plate (2) and the lower glass cover plate (3) are both BF33 glass; The bonding of the lower glass cover plate (3) occurs at a depth of less than 1.5×10 -5 Under a vacuum condition of 1000 mbar, a pressure of 900-1100 N is applied to the lower glass sheet cover plate (3) to make it closely fit the silicon wafer and heat it to 290-310° C., and a pulse voltage with a peak value of 590-610 V and a gradually decreasing peak duration is applied between the P-type crystal surface double-sided polished silicon wafer (1) and the lower glass sheet cover plate (3) to complete bonding; The bonding of the upper glass sheet cover plate (2) is carried out in a buffer gas atmosphere, wherein the buffer gas comprises N2, 131 Xe and 129 Xe, applying a pressure of 900-1100N to the upper glass sheet cover plate (2) to make it closely fit the silicon wafer and heating it to 290-310°C, and applying a pulse voltage with a peak value of 590-610V and a gradually decreasing peak duration between the P-type crystal surface double-sided polished silicon wafer (1) and the upper glass sheet cover plate (2) to complete bonding.
Citation Information
Cited By
Atomic beam tube device and atomic beam clock system
CN120669502A
Atomic gas chamber for realizing dynamic concentration adjustment and preparation method and application thereof
CN121165422A
An atomic gas chamber for dynamic concentration regulation, its preparation method and application
CN121165422B
Source of atom and / or molecule delivery and method of operation and production