Millimeter wave radar PCB of antenna area Hoz and preparation method thereof

By employing local micro-etching and multiple pattern transfer etching steps, the issues of copper thickness uniformity and pattern mating accuracy in the Hoz millimeter-wave PCB of the antenna area were resolved, achieving a high-quality millimeter-wave radar PCB design.

CN118973123AActive Publication Date: 2024-11-15ZHUHAI MUTAILAI CIRCUIT CO LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202411094495.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-10
Publication Date
2024-11-15
Estimated Expiration
2044-08-10

AI Technical Summary

Technical Problem

Existing millimeter-wave PCBs with antenna area Hoz have several drawbacks during manufacturing, including the inability to achieve local thin copper Hoz design on the same plane, insufficient precision in pattern alignment for areas with different copper thicknesses, difficulty in controlling copper thickness uniformity, and issues related to processing compensation for patterns with different copper thicknesses on the same plane.

Method used

Copper thickness monitoring and control are achieved through local micro-etching. By performing multiple pattern transfer and etching steps, the design of local Hoz patterns on the same plane is realized. The combination of wet film and dry film ensures copper thickness uniformity and pattern alignment accuracy.

Benefits of technology

The design of local Hoz on the same plane was achieved, which ensured the uniformity of copper thickness and the accuracy of pattern docking in areas with different copper thicknesses, thereby improving the performance and appearance quality of the product.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118973123A_ABST
    Figure CN118973123A_ABST
Patent Text Reader

Abstract

The invention discloses a millimeter wave radar PCB of an antenna area Hoz and a preparation method thereof, and belongs to the technical field of PCB preparation. The method comprises the following steps of cutting, first pattern transfer, first etching and film removal, first browning, lamination, target hole drilling, frame milling, first browning removal, second browning, laser drilling, drilling, degumming, first copper deposition and thickening, hole blocking, baking, polishing, second pattern transfer, first micro-etching copper reduction, copper deposition and thickening and third pattern transfer. The method comprises the following steps: first-time micro-etching copper reduction, second-time micro-etching copper reduction, fourth-time pattern transfer, second-time etching film removal, solder mask manufacturing, surface treatment, character silk-screen printing, shape processing, testing and finished product inspection. The method has the beneficial effects that the method provided by the invention is adopted for production, the design and manufacturing of the millimeter wave radar PCB of the Hoz antenna area are realized, and the product performance and appearance can completely meet the design requirements of such products.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application belongs to the technical field of PCB preparation, and specifically relates to a millimeter wave radar PCB with an antenna area Hoz and a preparation method thereof. Background Art

[0002] Millimeter wave radar refers to radar working in the millimeter wave frequency band. It can be used as a non-contact sensing technology to detect objects and provide distance, speed and angle information of objects. It is widely used in multiple fields of detection, detection and other sensing technologies. The main frequencies used by millimeter wave products are 24GHz, 60GHz, 77-79GHz, etc. The upstream and downstream industrial chains of the 24GHz frequency band are mature and the cost is relatively low. It is mainly used in the consumer market and industrial fields. The bandwidth of the 60GHz frequency band is 4GHz. At present, chip manufacturers mainly develop CMOS process millimeter wave radar chips, which are widely used in the industrial and Internet of Things fields. In the "Interim Provisions on the Management of Automotive Radar Radio" issued by the Ministry of Industry and Information Technology in 2021, the 76-79GHz frequency band is planned for automotive radars, and the use of this frequency band by other ground radars is restricted. Automotive-grade millimeter wave radar products have become the mainstream sensor devices in the automotive field, and subsequent industrial-grade radar 60GHz millimeter wave radar products will become mainstream. Millimeter wave radar was produced abroad in the 1940s. After decades of development, it entered China in 2013 and then entered a rapid development stage in my country.

[0003] However, the existing millimeter-wave PCB with antenna area Hoz has the following technical problems during production: 1. It is impossible to design a local thin copper Hoz on the same plane; 2. The pattern docking accuracy of areas with different copper thicknesses is insufficient; 3. The control of copper thickness uniformity and the compensation problem of pattern processing with different copper thicknesses on the same plane; 4. The pattern coating quality problem caused by the step difference of different copper thicknesses on the same plane. Summary of the invention

[0004] The purpose of an embodiment of the present application is to provide a millimeter-wave radar PCB with an antenna area Hoz, which realizes the design of local Hoz on the same plane by local micro-etching, and the uniformity of the micro-etching area is controlled by copper thickness monitoring, thereby solving at least one technical problem involved in the background technology.

[0005] In order to solve the above technical problems, this application is implemented as follows:

[0006] The embodiment of the present application provides a method for preparing a millimeter wave radar PCB of an antenna area Hoz, comprising the following steps:

[0007] Step S1, cutting the material according to the designed size;

[0008] Step S2, the first pattern transfer, coating the board with a photosensitive material, using film exposure, and removing the required non-circuit photosensitive material with a weak alkaline chemical solution;

[0009] Step S3, etching the film for the first time, using a strong oxidizing chemical solution to remove the exposed copper layer, and then using a strong alkaline chemical solution to remove all the photosensitive materials;

[0010] Step S4, first browning, removing grease and dirt from the board surface, roughening the copper surface and increasing the area for the copper surface to bond with the prepreg;

[0011] Step S5, lamination, using a traditional press core board at constant temperature and pressure, bonding them together through prepreg, and placing release films on the upper and lower surfaces of the boards;

[0012] Step S6, drilling target holes, using an xray target drilling machine to drill required positioning holes;

[0013] Step S7, milling the frame, and removing the excess copper foil and the overflow glue on the edge of the board after lamination by a CNC milling machine;

[0014] Step S8, first de-browning, using mechanical brushing to remove the brown film and resin spots on the outer core board;

[0015] Step S9, second browning, removing grease and dirt from the board surface, applying a browning film on the surface copper surface and reducing copper to meet the needs of laser drilling;

[0016] Step S10, laser drilling, using laser to drill the required blind holes;

[0017] Step S11, drilling, using mechanical drilling to drill the required through holes;

[0018] Step S12, removing the glue, using a strong oxidizing chemical solution to remove the resin and drill stains remaining in the drilling hole;

[0019] Step S13, first copper plating and thickening, metallizing the resin and glass fiber of the non-conductive part of the hole wall;

[0020] Step S14, plugging the blind holes and the holes in the disk with resin;

[0021] Step S15, baking to dry and solidify the semi-cured resin;

[0022] Step S16, grinding, grinding the pore resin clean;

[0023] Step S17, second pattern transfer, coating the board with photosensitive material, using film selective exposure, removing the required non-circuit photosensitive material with weak alkaline chemical solution, and making dry film masking holes for through holes and device holes;

[0024] Step S18, first micro-etching to reduce copper, using a strong oxidizing chemical solution to reduce copper on the entire outer layer of the board;

[0025] Step S19, copper plating and thickening, and making POFV caps for blind holes and vias in disks;

[0026] Step S20, the third pattern transfer, coating the plate with a photosensitive material, using film selective exposure, removing the required non-circuit photosensitive material with a weak alkaline chemical solution, exposing the required Hoz area of ​​the antenna;

[0027] Step S21, a second micro-etching process to reduce copper, using a strong oxidizing chemical solution to reduce copper in the exposed antenna local area where the required Hoz is required;

[0028] Step S22, the fourth pattern transfer, coating the board with photosensitive material, using the outer layer circuit data and exposing, and removing the required non-circuit photosensitive material by weak alkaline chemical solution;

[0029] Step S23, etching the film for the second time, using a strong oxidizing chemical solution to remove the exposed copper layer, and then using a strong alkaline chemical solution to remove all the photosensitive materials;

[0030] Step S24, solder mask production, screen printing the photosensitive solder mask material on the board by screen printing, using film selective exposure, removing the photosensitive material on the required pads by weak alkaline chemical solution and curing the green oil;

[0031] Step S25, surface treatment, performing surface treatment on the welding area;

[0032] Step S26, screen printing characters, using a screen to screen print a layer of thermosetting ink on the surface of the product;

[0033] Step S27, shape processing, cutting into the required shape;

[0034] Step S28, testing, using a testing machine to test the electrical performance of each network;

[0035] Step S29, finished product inspection, visual inspection of the panel appearance, and storage after no defects.

[0036] Optionally, in step S16, a ceramic brush and a non-woven brush are used to grind the orifice resin clean.

[0037] Optionally, in step S26, the surface treatment includes immersion silver, immersion gold, and OSP.

[0038] Optionally, in step S27, a CNC milling machine is used to cut out a desired shape.

[0039] Optionally, in step S28, the electrical performance includes open circuit, short circuit, resistance, and inductance.

[0040] The present invention also provides a millimeter wave radar PCB with an antenna area Hoz, which is prepared by adopting the preparation method.

[0041] Compared with the prior art, this application has the following beneficial effects:

[0042] 1. The design of local Hoz on the same plane is realized by local micro-etching. The uniformity of the micro-etching area is controlled by copper thickness monitoring, which ensures the uniformity of copper thickness and solves the problem of compensation in the processing of graphics with different copper thicknesses on the same plane;

[0043] 2. Graphic transfer is performed simultaneously in the thin copper Hoz and 1OZ areas, ensuring the accuracy of graphic docking in areas with different copper thicknesses;

[0044] 3. The coating is made by wet film + dry film. The wet film filling ensures the flatness of the board surface and prevents the post-process etching solution from attacking the step positions of different copper thicknesses;

[0045] 4. The thin copper Hoz and 1OZ areas are compensated in the same way and etched at the same time. A 45° triangle design is added to the EA position outside the antenna, and 25um is added to the outside. A 45° triangle is designed at the EA position inside, and 25um is cut inside to ensure the accuracy of the feeder, pad, and EA.

[0046] 5. The method provided by the invention is adopted for production, and the design and production of the millimeter-wave radar PCB of the antenna area Hoz is realized. The product performance and appearance can fully meet the design requirements of such products. BRIEF DESCRIPTION OF THE DRAWINGS

[0047] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the following briefly introduces the drawings required for describing the embodiments. Obviously, the drawings described below are only some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on these drawings without creative work, among which:

[0048] Figure 1 The present invention provides a flow chart of a method for preparing a millimeter wave radar PCB in the antenna area Hoz. DETAILED DESCRIPTION

[0049] The following will be combined with the drawings in the embodiments of the present application to clearly and completely describe the technical solutions in the embodiments of the present application. Obviously, the described embodiments are part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of this application.

[0050] The terms "first", "second", etc. in the specification and claims of the present application are used to distinguish similar objects, and are not used to describe a specific order or sequence. It should be understood that the data used in this way can be interchangeable under appropriate circumstances, so that the embodiments of the present application can be implemented in an order other than those illustrated or described here, and the objects distinguished by "first", "second", etc. are generally of one type, and the number of objects is not limited. For example, the first object can be one or more. In addition, "and / or" in the specification and claims represents at least one of the connected objects, and the character " / " generally indicates that the objects associated with each other are in an "or" relationship.

[0051] See also Figure 1 As shown, the embodiment of the present application provides a method for preparing a millimeter wave radar PCB of an antenna area Hoz, comprising the following steps:

[0052] Step S1, cutting the material according to the designed size;

[0053] Step S2, the first pattern transfer, coating the board with a photosensitive material, using film exposure, and removing the required non-circuit photosensitive material with a weak alkaline chemical solution;

[0054] Step S3, etching the film for the first time, using a strong oxidizing chemical solution to remove the exposed copper layer, and then using a strong alkaline chemical solution to remove all the photosensitive materials;

[0055] Step S4, first browning, removing grease and dirt from the board surface, roughening the copper surface and increasing the area for the copper surface to bond with the prepreg;

[0056] Step S5, lamination, using a traditional press core board with constant temperature and pressure, bonding them together through prepreg, and placing release films on the upper and lower surfaces of the boards to ensure that the board surface is flat;

[0057] Step S6, drilling target holes, using an xray target drilling machine to drill required positioning holes;

[0058] Step S7, milling the frame, using a CNC milling machine to remove excess copper foil and overflow glue from the edge of the board after lamination to ensure that the edge of the board is neat;

[0059] Step S8, first de-browning, using mechanical brushing to remove the brown film and resin spots on the outer core board;

[0060] Step S9, second browning, removing grease and dirt from the board surface, applying a browning film on the surface copper surface and reducing copper to meet the needs of laser drilling;

[0061] Step S10, laser drilling, using laser to drill the required blind holes;

[0062] Step S11, drilling, using mechanical drilling to drill the required through holes;

[0063] Step S12, removing the glue, using a strong oxidizing chemical solution to remove the resin and drill stains remaining in the drilling hole;

[0064] Step S13, first copper plating and thickening, metallizing the resin and glass fiber of the non-conductive part of the hole wall;

[0065] Step S14, plugging the blind holes and the holes in the disk with resin;

[0066] Step S15, baking to dry and solidify the semi-cured resin;

[0067] Step S16, grinding, grinding the orifice resin clean to ensure that the resin and the orifice are flat;

[0068] Step S17, second pattern transfer, coating the board with photosensitive material, using film selective exposure, removing the required non-circuit photosensitive material with weak alkaline chemical solution, and making dry film masking holes for through holes and device holes;

[0069] Step S18, first micro-etching to reduce copper, using a strong oxidizing chemical solution to reduce copper on the entire outer layer of the board;

[0070] Step S19, copper plating and thickening, and making POFV caps for blind holes and vias in disks;

[0071] Step S20, the third pattern transfer, coating the plate with a photosensitive material, using film selective exposure, removing the required non-circuit photosensitive material with a weak alkaline chemical solution, exposing the required Hoz area of ​​the antenna;

[0072] Step S21, a second micro-etching process to reduce copper, using a strong oxidizing chemical solution to reduce copper in the exposed antenna local area where the required Hoz is required;

[0073] Step S22, the fourth pattern transfer, coating the board with photosensitive material, using the outer layer circuit data and exposing, and removing the required non-circuit photosensitive material by weak alkaline chemical solution;

[0074] Step S23, etching the film for the second time, using a strong oxidizing chemical solution to remove the exposed copper layer, and then using a strong alkaline chemical solution to remove all the photosensitive materials;

[0075] Step S24, solder mask production, screen printing the photosensitive solder mask material on the board by screen printing, using film selective exposure, removing the photosensitive material on the required pads by weak alkaline chemical solution and curing the green oil;

[0076] Step S25, surface treatment, performing surface treatment on the welding area;

[0077] Step S26, screen printing characters, using a screen to screen print a layer of thermosetting ink on the surface of the product;

[0078] Step S27, shape processing, cutting into the required shape;

[0079] Step S28, testing, using a testing machine to test the electrical performance of each network;

[0080] Step S29, finished product inspection, visual inspection of the panel appearance, and storage after no defects.

[0081] Optionally, in step S16, a ceramic brush and a non-woven brush are used to grind the orifice resin clean.

[0082] Optionally, in step S26, the surface treatment includes immersion silver, immersion gold, and OSP.

[0083] Optionally, in step S27, a CNC milling machine is used to cut out a desired shape.

[0084] Optionally, in step S28, the electrical performance includes open circuit, short circuit, resistance, and inductance.

[0085] The present invention also provides a millimeter wave radar PCB with an antenna area Hoz, which is prepared by adopting the preparation method.

[0086] It should be noted that, in this article, the terms "include", "comprises" or any other variations thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device. In the absence of further restrictions, an element defined by the sentence "comprises a ..." does not exclude the existence of other identical elements in the process, method, article or device including the element.

[0087] In addition, it should be noted that the scope of the methods and systems in the embodiments of the present application is not limited to performing functions in the order shown or discussed, and may also include performing functions in a substantially simultaneous manner or in reverse order according to the functions involved. For example, the described methods may be performed in an order different from that described, and various steps may be added, omitted, or combined. In addition, features described with reference to certain examples may be combined in other examples.

[0088] The embodiments of the present application are described above in conjunction with the accompanying drawings, but the present application is not limited to the above-mentioned specific implementation methods. The above-mentioned specific implementation methods are merely illustrative and not restrictive. Under the guidance of the present application, ordinary technicians in this field can also make many forms without departing from the purpose of the present application and the scope of protection of the claims, all of which are within the protection of the present application.

Claims

1. A method for preparing a millimeter wave radar PCB with an antenna area Hoz, characterized in that: The steps include: Step S1, cutting the material according to the designed size; Step S2, the first pattern transfer, coating the board with a photosensitive material, using film exposure, and removing the required non-circuit photosensitive material with a weak alkaline chemical solution; Step S3, etching the film for the first time, using a strong oxidizing chemical solution to remove the exposed copper layer, and then using a strong alkaline chemical solution to remove all the photosensitive materials; Step S4, first browning, removing grease and dirt from the board surface, roughening the copper surface and increasing the area for the copper surface to bond with the prepreg; Step S5, lamination, using a traditional press core board at constant temperature and pressure, bonding them together through prepreg, and placing release films on the upper and lower surfaces of the boards; Step S6, drilling target holes, using an xray target drilling machine to drill required positioning holes; Step S7, milling the frame, and removing the excess copper foil and the overflow glue on the edge of the board after lamination by a CNC milling machine; Step S8, first de-browning, using mechanical brushing to remove the brown film and resin spots on the outer core board; Step S9, the second browning, to remove the grease and dirt on the board surface, to apply a browning film on the surface copper surface and to reduce the copper to meet the requirements of laser drilling; Step S10, laser drilling, using laser to drill the required blind holes; Step S11, drilling, using mechanical drilling to drill the required through holes; Step S12, removing the glue, using a strong oxidizing chemical solution to remove the resin and drill stains remaining in the drilling hole; Step S13, first copper plating and thickening, metallizing the resin and glass fiber of the non-conductive part of the hole wall; Step S14, plugging the blind holes and the holes in the disk with resin; Step S15, baking to dry and solidify the semi-cured resin; Step S16, grinding, grinding the pore resin clean; Step S17, second pattern transfer, coating the board with photosensitive material, using film selective exposure, removing the required non-circuit photosensitive material with weak alkaline chemical solution, and making dry film masking holes for through holes and device holes; Step S18, first micro-etching to reduce copper, using a strong oxidizing chemical solution to reduce copper on the entire outer layer of the board; Step S19, copper plating and thickening, and making POFV caps for blind holes and vias in disks; Step S20, the third pattern transfer, coating the plate with a photosensitive material, using film selective exposure, removing the required non-circuit photosensitive material with a weak alkaline chemical solution, exposing the required Hoz area of ​​the antenna; Step S21, a second micro-etching process to reduce copper, using a strong oxidizing chemical solution to reduce copper in the exposed antenna local area where the required Hoz is required; Step S22, the fourth pattern transfer, coating the board with photosensitive material, using the outer layer circuit data and exposing, and removing the required non-circuit photosensitive material by weak alkaline chemical solution; Step S23, etching the film for the second time, using a strong oxidizing chemical solution to remove the exposed copper layer, and then using a strong alkaline chemical solution to remove all the photosensitive materials; Step S24, solder mask production, screen printing the photosensitive solder mask material on the board by screen printing, using film selective exposure, removing the photosensitive material on the required pads by weak alkaline chemical solution and curing the green oil; Step S25, surface treatment, performing surface treatment on the welding area; Step S26, screen printing characters, using a screen to screen print a layer of thermosetting ink on the surface of the product; Step S27, shape processing, cutting into the required shape; Step S28, testing, using a testing machine to test the electrical performance of each network; Step S29, finished product inspection, visual inspection of the panel appearance, and storage after no defects.

2. The preparation method according to claim 1, characterized in that: In step S16, the orifice resin is ground clean using a ceramic brush and a non-woven brush.

3. The preparation method according to claim 1, characterized in that: In step S26, the surface treatment includes immersion silver, immersion gold, and OSP.

4. The preparation method according to claim 1, characterized in that: In step S27, a CNC milling machine is used to cut out the required shape.

5. The preparation method according to claim 1 or 4, characterized in that: In step S28, the electrical performance includes open circuit, short circuit, resistance, and inductance.

6. A millimeter wave radar PCB with an antenna area Hoz, characterized in that: The preparation method is described in any one of claims 1 to 5.

Citation Information

Patent Citations

  • Method for manufacturing local thin copper printed circuit board

    CN113939097A

  • Radar antenna PCB manufacturing process and antenna pattern manufacturing process and application thereof

    CN114423186A

  • Manufacturing method of high-reliability POFV hole and PCB

    CN116075060A

  • Millimeter wave radar PCB of antenna area Hoz

    CN223024684U