Manufacturing method of AOP three-dimensional assembled microwave rigid-flex board-level assembly

The manufacturing of microwave rigid-flex bonding plates and metal structural parts through the semi-addition process solves the problems of large assembly space and large weight in traditional AOPs, and realizes high-integration RF front-end components, significantly reduces size and weight, and improves performance and reliability.

CN118973148APending Publication Date: 2024-11-15CHINA ELECTRONIC TECH GRP CORP NO 38 RES INST
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411030756.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-30
Publication Date
2024-11-15

AI Technical Summary

Technical Problem

Traditional AOP assembly in highly integrated devices takes up a large space, has a large weight and is difficult to make microwave rigid-flexibly combined plates, which limits its application in the front end of the RF of millimeter wave active passive imaging radar.

Method used

The semi-addition process is used to manufacture flexible inner plates and microwave inner plates with patterns, and microwave rigid-flex bonding plates are made through adhesive materials, and AOP device assembly is performed on the top and bottom layers, using the bend of flexible inner plates. Folding into three-dimensional assembly, combining metal structural parts to achieve high integration of RF front-end board-level components.

Benefits of technology

Achieve high integration of the RF front-end, with a size reduction of more than 65%, a weight reduction of more than 50%, a cost reduction of more than 30%, and a better performance in the high frequency band, meeting the thermal cycle of -45℃~+60℃ Environmental testing requires good reliability and environmental adaptability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118973148A_ABST
    Figure CN118973148A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of manufacturing of radar electronic functional parts, in particular to a manufacturing method of an AOP three-dimensional assembled microwave rigid-flex board-level assembly, which comprises the following steps of: (1) manufacturing a flexible inner-layer board with a pattern; (2) manufacturing a microwave inner-layer plate with an inner-layer pattern; (3) manufacturing the microwave rigid-flex printed circuit board through the bonding material; (4) carrying out AOP and other device assembly on the top layer and the bottom layer of the microwave rigid-flex printed circuit board; and (5) mounting the rigid part on the metal structural member, and bending the flexible inner layer plate to form three-dimensional assembly. The method effectively solves the problems that in traditional AOP plane assembly, cable interconnection needs to be carried out among multiple boards, high-integration-level devices needed by a power supply system and the like occupy AOP assembly space, traditional multi-board AOP assembly integration is large in weight and space, and microwave rigid-flexible combined boards are difficult to manufacture.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of manufacturing radar electronic functional components, and in particular to a method for manufacturing an AOP three-dimensionally assembled microwave rigid-flexible board-level component. Background Art

[0002] Combining active imaging that can obtain a three-dimensional image of the target with passive imaging that can obtain the geometric shape, material, temperature and other characteristics of the target all day and all weather, active and passive imaging can obtain more comprehensive and detailed target information, providing a priori conditions for target detection and identification. Therefore, millimeter wave short-range imaging technology in the Ka band and above has been widely studied as the next generation technology in military radar, satellite navigation, traffic control and public safety.

[0003] Synthetic aperture phased array radar is an important research direction for active and passive imaging millimeter wave radar, and the RF front end composed of the transceiver system and array antenna is the core component of the phased array radar. With the development trend of miniaturization and high integration, traditional metal waveguide antennas, metal array antennas, microstrip antenna patches, etc. cannot meet the requirements. Brick-type TR components are also gradually shifting to packaged antennas due to weight, profile thickness and interconnection density. AOP (packaged antenna) is a new design that integrates the RF chip and antenna into one package. It only needs to connect the DC power supply, control signal and baseband signal to the package pins to achieve the integrated transceiver effect. It is the latest technical route for system-level packaged RF front end.

[0004] However, limited by existing materials and technical routes, the current AOP gain and efficiency are lower than traditional antennas. When the combination with PCB is not good and involves multiple interconnection paths between boards, the efficiency of AOP will be greatly reduced to ≤6%, which limits its integrated application. In addition, AOP has high integration and multi-functionality. It is mostly installed on PCB in the form of CBGA package. It requires PCB to have multiple functions such as multi-stage amplification, power division, synthesis, control, power supply, etc., and it cannot affect the dense installation space of AOP. Therefore, the complex structure of AOP+multiple PCBs+multiple groups of connectors+low-frequency / RF cables+mounting boards is often used, which cannot give full play to the advantages of AOP in terms of lightness and small size. The rigid-flex boards currently used are all a combination of digital copper clad boards (FR4) and PI flexible inner layers. Due to the large differences in the material properties of copper clad boards and the high lamination temperature of the adhesive materials used, there are few rigid-flex boards of microwave copper clad boards (PTFE, etc.) that have been developed and produced.

[0005] Therefore, it is urgent to develop a method for manufacturing RF front-end board-level components that fully utilizes the high integration advantages of AOP, realizes three-dimensional assembly through rigid-flexible boards, integrates multi-stage amplification of transceiver antennas and feeders on a single board, and performs phase shifting, attenuation, power division, synthesis, control, and power supply for four beam channels, so as to break through the key technical bottleneck for the high-integration application of AOP in the RF front-end of millimeter-wave active and passive imaging radars.

[0006] In view of the above-mentioned defects, the inventors of the present invention finally obtained the present invention after a long period of research and practice. Summary of the invention

[0007] The purpose of the present invention is to solve the problems that the traditional AOP plane assembly requires cable interconnection between multiple boards, the high-integration devices required for power supply and other systems occupy the AOP assembly space, the traditional multi-board AOP assembly has large weight and space, and the microwave rigid-flexible board is difficult to manufacture. A method for manufacturing an AOP three-dimensional assembly microwave rigid-flexible board-level component is provided.

[0008] In order to achieve the above object, the present invention discloses a method for manufacturing an AOP stereoscopically assembled microwave rigid-flexible board-level component, comprising the following steps:

[0009] S1, manufacturing a flexible inner layer board with patterns through a semi-additive process;

[0010] S2, manufacturing a microwave inner layer board with inner layer patterns through a semi-additive process;

[0011] S3, manufacturing a microwave rigid-flexible board by bonding materials, wherein the microwave rigid-flexible board comprises a first rigid outer layer, a first flexible inner layer, a rigid inner layer, a second flexible inner layer, and a second rigid outer layer, wherein the first rigid outer layer, the rigid inner layer, and the second rigid outer layer are all microwave inner layer boards, and the first flexible inner layer and the second flexible inner layer are flexible inner layer boards;

[0012] S4, assembling AOP devices on the top and bottom layers of the microwave rigid-flex board;

[0013] S5, the rigid part is mounted on the metal structure and a three-dimensional assembly is formed by bending the flexible inner layer plate.

[0014] In step S1, the production process of the flexible inner layer board is: cutting, film lamination, LDI exposure, etching and developing, AOI inspection, browning, plasma treatment, cover film lamination, cover film pressing, laser milling shape;

[0015] The graphics of the flexible inner layer board include signal lines and grid lines. The minimum line width of the signal line is 0.25mm, and the minimum line width of the grid line is 0.1mm.

[0016] The grid lines of the flexible inner layer board are not coplanar with the signal lines, but are located on the ground of the signal lines. The shielding effect and the strength of the flexible inner layer board are enhanced by the mesh copper foil. The grid lines are encrypted within 1 to 10 mm of the overlapped edge with the rigid board to increase the fit between the flexible inner layer board and the structural support.

[0017] Use dry film for graphic production process, the film pressure is 2~10Kg / cm 2 , the roller speed is 1-5m / s, the flexible inner layer board is patterned by LDI, the LDI spot diameter is 28μm, the depth of field is ±300μm, the resolution is 35μm, the exposure energy is 30-100mJ, the pH value of the flexible inner layer board development is set to 3.5-5, and the temperature is 30-45℃;

[0018] The browning of the flexible inner layer board uses a mixture of H2SO4, H2O2 and organic compounds to oxidize Cu into Cu2O, and an organic copper oxide layer is formed through the chemical bonding of Cu2O and the organic compound;

[0019] The thickness of the flexible inner layer is 0.1mm, and the thickness of the copper foil is 18um;

[0020] The flexible inner layer board can be any one of Panasonic's R-8700, Ube Exsymo's Upisel-N, Shinyang Technology's W-Type, Shengyi Technology's SF280, SF202, and SF230;

[0021] The covering film is modified by plasma treatment, with CF4:O2 of 0.05-0.2, power of 10-15 kW, time of 5-15 min, and flow rate of 1200-1800 mL / min;

[0022] The pressing temperature of the covering film is 180-200°C, the pressure is 300-400psi, the vacuum degree is 25-35Bar, and the pressing time is 45-70min.

[0023] In step S2, the production process of the microwave inner layer board is: cutting, drilling, hole forming, plugging, film pasting, LDI exposure, etching and developing, AOI inspection, browning, lamination, drilling, hole forming, plugging, film pasting, LDI exposure, etching and developing, and browning.

[0024] The microwave inner layer board includes 5 layers of microwave rigid copper clad laminates, 2 layers of adhesive materials, 2 layers of flexible copper clad laminates, and 3 layers of adhesive materials. The adhesive material is a microwave adhesive sheet, which is any one of CFB278F of the 46th Institute of China Electronics Technology, RLP30 of Ruilong Company, SJ928B of Shengyi Technology, and GNC300BP of Guoneng Company.

[0025] Microwave rigid copper clad laminate is a PTFE-based system, and any one of PTFE / glass cloth, PTFE / micro-glass fiber, PTFE / glass cloth / ceramic powder, PTFE / micro-glass fiber / ceramic powder, PTFE / ceramic powder can be selected;

[0026] The copper foil on the top layer of the microwave rigid copper clad laminate is any one of rolled copper foil, electrolytic copper foil, reverse copper foil and low profile copper foil, and the thickness of the copper foil is 18μm or 35μm;

[0027] The dielectric thickness is 0.0127~1.016mm;

[0028] The plugging is done by a vacuum plugging machine using conductive paste. After plugging, the copper paste is cured at 130-160°C for 30-60 minutes to form a conductive path. The conductive paste is one of AE2217 from Tuozida and CB102 from DuPont.

[0029] The vacuum hot pressing temperature is 220℃-245℃.

[0030] In step S3, the first rigid outer layer integrates the functions of multi-stage amplification, power division and synthesis, and the second rigid outer layer integrates the functions of control and power supply.

[0031] In step S3, the rigid inner layer adopts a reverse depth control method to remove part of the material combined with the flexible inner layer board.

[0032] The microwave rigid copper clad laminate is a 2.94 PTFE / glass fiber cloth / ceramic filler or a PTFE / micro glass fiber system / ceramic filler.

[0033] In the step S3, the flexible inner layer board and the microwave inner layer board are compounded by lamination, and the production of the microwave rigid-flexible board includes: pressing, drilling, hole chemical plating and electroplating, including side metallization, plugging, film pasting, LDI exposure, etching and developing, AOI inspection, surface coating, solder mask production, character production, and appearance processing.

[0034] During the lamination, a gasket is placed on the flexible inner layer board to prevent the adhesive material from flowing onto the covering film; the non-welding areas of the rigid board are covered with solder resist to play a protective and welding auxiliary limit role; mechanical processing controlled depth milling is used to mill off the rigid parts above and below the flexible material to expose the flexible inner layer board part; the adhesive material used for the composite is a non-flow adhesive sheet, and the welding position of the microwave rigid-flexible composite board is surface-coated, and the coating material is gold-plated, chemical gold or nickel-gold-plated; the vacuum hot pressing temperature is 170°C-245°C, and the time is 1-6h; the nickel thickness of the chemical nickel-gold coating is 3-5um, and the gold thickness is 0.05-0.1um.

[0035] In the step S4, the rigid board area where the AOP device is installed is provided with stepped through grooves, the top-level large grooves are used for the nut installation of the pan head screws, and the bottom-level small grooves are used for the screws to pass through. The AOP devices on the rigid board are all provided with outer frame characters, position numbers, and mark points. The rigid board area where the connector is installed is provided with through grooves for installing screws. The inner walls of all the installation grooves are metallized on the sides, and the metallization production is the same process as the production of the metallized holes.

[0036] The installation of surface mount devices is completed through double-sided SMT, and the installation of plug-in devices and connectors is completed through manual soldering. The rigid board where the AOP is located has AOPs densely arranged on the entire surface, and there are no other devices. The rigid board where the AOP is located is secondary soldering. The peak temperature of SMT is 260-270℃. SnPb series low-temperature solder is selected, and the melting point temperature is not higher than 183℃.

[0037] In step S5, the rigid part of the AOP assembly is installed on the plane of the structural member, the flexible part is pressed against the structural member support frame, the bent PCBA is installed on another plane of the structural member, and the rigid plate is fastened by screws to obtain a three-dimensionally assembled AOP component.

[0038] Compared with the prior art, the beneficial effects of the present invention are:

[0039] 1. The AOP stereo assembly based on the microwave rigid-flexible board prepared in the present invention can be used in high frequency bands above Ku. When used in the Ku band, it can achieve an instantaneous bandwidth ≥ 200MHz, can complete 50° scanning, and the antenna unit gain ≥ 28dB, showing better performance than existing products;

[0040] 2. Compared with the traditional technical path, the RF front end based on the stereoscopic assembly of the microwave rigid-flexible board AOP prepared in the present invention improves the integration of the RF front end, reduces the size by more than 65%, reduces the weight by more than 50%, and reduces the cost by more than 30%, and has outstanding performance advantages and good process availability;

[0041] 3. The three-dimensional assembly of the microwave rigid-flex board AOP in the present invention has a processing yield rate of more than 80%, which can meet the typical environmental test requirements of -45℃~+60℃ thermal cycle, pass the typical ground vibration and impact environmental tests, and has good reliability and environmental adaptability. BRIEF DESCRIPTION OF THE DRAWINGS

[0042] Figure 1 This is a schematic diagram of the structure of the AOP three-dimensionally assembled microwave rigid-flex board-level component in Example 1;

[0043] Figure 2 This is a schematic diagram of the mounting surface structure of the rigid sub-board mounted on the AOP in Example 1;

[0044] Figure 3 This is a schematic diagram of the structure of the microwave rigid-flex board in Example 1;

[0045] Figure 4 This is a process flow chart of the rigid-flexible board in Example 1.

[0046] The numbers in the figure represent:

[0047] 1-Solder ball; 2-BGA package AOP; 3-Upper microwave rigid sub-board DETAILED DESCRIPTION

[0048] The above and other technical features and advantages of the present invention are described in more detail below in conjunction with the accompanying drawings.

[0049] Example 1

[0050] S101, AOP three-dimensional assembly microwave rigid-flex board-level components structure diagram Figure 1 The RF front end includes a BGA-packaged AOP2 (solder ball 1), an upper microwave rigid sub-board 3 for assembling the AOP, a lower microwave rigid sub-board 7 for installing other surface-mounted devices 8 and connectors 10, a double-layer embedded flexible inner board 11 and 12 connecting the two parts of the microwave rigid sub-board, a supporting U-shaped structural member 6 (including a through slot 4 for screw installation and a through slot 9 for exposing the device) and a pan head screw 5 for fixing. Among them, the top layer of the upper microwave rigid sub-board 3 only has the AOP solder pad 15, the outer frame 13, the fixed installation hole 15 and the mark point 14, as shown in FIG. Figure 2 shown.

[0051] S102. To demonstrate the flexible interconnection structure, the structure of the microwave rigid-flexible board is shown in the figure below. Figure 3 As shown. The rigid-flex board is divided into two parts, a rigid sub-board and two layers of flexible connecting boards. The rigid sub-board includes 5 layers of RS300B (thickness 0.127mm) rigid microwave copper clad board 34, 2 layers of GNC300BP adhesive material 35, 2 layers of flexible copper clad board AP 8515R 37, and 3 layers of RL-P8073 adhesive material 36. The rigid sub-board part where AOP is installed includes the top layer AOP pad pattern 17, the inner layer pattern 28, the bottom layer pattern 32, the metallized blind via 29 on the single-layer rigid microstrip board (including the plugging copper paste AE2217 30, and the subsequent plugging copper paste will not be additionally marked), the metallized blind via 38 that passes through the rigid microstrip board area, the metallized buried via 18 in the rigid microstrip board, the metallized through hole 31 that passes through the rigid-flex board, and the through groove for screw installation (including the step groove 20, 25, the installation groove frame 19, 27 and the metallized groove wall 26). The structure of the other rigid sub-board is basically similar, except that the through slot 24 for screw installation has no steps. The flexible inner layer board part includes a cover film 23, a transmission line pattern 21 and a grid reinforcement pattern 22 in addition to two layers of flexible copper clad laminates.

[0052] S103, the processing process of the flexible area is as follows:

[0053] (1) Cutting;

[0054] (2) At a pressure of 5 kg / cm 2 , the process parameter of film lamination is 3m / s with roller speed;

[0055] (3) Graphics are produced by LDI with an exposure energy of 50 mJ;

[0056] (4) The pH value of the development is set to 4 and the temperature is set to 40°C;

[0057] (5) Plasma treatment modification of the covering film, CF4:O2 is 0.1, power is 10 kW, time is 15 min, flow rate is 1800 ml / min;

[0058] (6) Browning;

[0059] (7) The cover film is attached to the flexible circuit. The cover film and the flexible inner layer are pressed together at a temperature of 180-200°C, a pressure of 300-400 psi, and a vacuum of 25-35 Bar for 45-70 minutes. After pressing, the area for attaching the cover film is laser milled out

[23] .

[0060] S104, the processing process of the rigid area is:

[0061] (1) Cutting;

[0062] (2) Drilling and hole plating (chemical plating and electroplating);

[0063] (3) AE2217 plugging is completed by vacuum plugging machine, cured in oven at 130°C for 60 min, and then polished with automatic grinding machine to remove the protruding resin from the hole;

[0064] (4) After film pasting, LDI exposure, etching and development, and AOI inspection are used;

[0065] (5) After browning, the GNC300BP and the prepared RS300B core board are stacked and positioned by pins, and then loaded with steel board, cushioning material, and kraft paper, and laminated at 220°C for 4 hours;

[0066] (6) Repeat the above steps to obtain a multi-layer microstrip core board that has been laminated multiple times.

[0067] S105, the processing process of rigid-flex PCB is as follows:

[0068] (1) After RL-P8073 and the prepared rigid core board and flexible core board are stacked, they are positioned by pins, loaded with rigid board, cushioning material, and kraft paper, and laminated at 200°C for 3 hours;

[0069] (2) Drilling (including milling), hole plating (chemical plating and electroplating) and plugging;

[0070] (3) After film pasting, LDI exposure, etching and development, and AOI inspection are used;

[0071] (4) Chemical nickel-gold plating, solder mask production, character production;

[0072] (5) The flexible inner layer is exposed by mechanical depth control, and the finished board is obtained by external processing.

[0073] S106. Complete double-sided soldering of AOP components using Sn36Pb62Ag2 solder paste, and install J30J low-frequency connector by manual soldering.

[0074] S107, install the rigid part of the AOP assembly on the plane of the structural component, attach the flexible part to the structural component support frame, bend the PCBA and install it on another plane of the structural component, fasten the rigid board with screws to obtain a three-dimensional assembled AOP component.

[0075] S108, the AOP stereo assembly microwave rigid-flex board-level component can be used in the Ka band, can achieve an instantaneous bandwidth ≥ 250MHz, can complete a 50° scan, and the antenna unit gain ≥ 30dB. The size of the component is reduced by 70%, the weight is reduced by 55%, and the cost is reduced by 30%. The processing yield is 82.5%, which can meet the typical environmental test requirements of -45℃~+60℃ thermal cycle, and has passed the typical ground vibration and impact environmental tests, with good reliability and environmental adaptability.

[0076] Example 2

[0077] The structure of Example 2 is the same as that of Example 1, except that the materials used for the rigid-flex board are different, as follows:

[0078] The rigid sub-board contains 5 layers of RS300B rigid microwave copper clad laminate, 2 layers of CFB278F adhesive material, 2 layers of SF202 flexible copper clad laminate, and 3 layers of SP168GN adhesive material. The copper paste for plugging all the metallized blind holes in the board is CB102.

[0079] The process flow is basically the same, and some of the different processing parameters are:

[0080] (1) CB102 plugging is completed by vacuum plugging machine, and cured in an oven at 150°C for 60 min, and then the protruding resin of the hole is polished by an automatic plate grinding machine;

[0081] (2) After browning, CFB278F and the prepared RS300B core board were stacked and positioned by pins, and then loaded with steel board, cushioning material, and kraft paper, and laminated at 220°C for 4 hours;

[0082] (3) After stacking SP168GN and the prepared rigid core board and flexible core board, they are positioned by pins, loaded with rigid boards, cushioning materials, and kraft paper, and laminated at 180°C for 4 hours.

[0083] S109, the AOP stereo assembly microwave rigid-flex board-level component can be used in the Ka band, can achieve an instantaneous bandwidth ≥ 244MHz, can complete a 50° scan, and the antenna unit gain is ≥ 27.5dB. The size of the component is reduced by 70%, the weight is reduced by 55%, and the cost is reduced by 45%. The processing yield is 80%, which can meet the typical environmental test requirements of -45℃~+60℃ thermal cycle, and has passed the typical ground vibration and impact environmental tests, with good reliability and environmental adaptability.

[0084] The above description is only a preferred embodiment of the present invention, which is only illustrative and not restrictive of the present invention. Those skilled in the art understand that many changes, modifications, and even equivalences may be made to the present invention within the spirit and scope defined by the claims of the present invention, but all of them will fall within the scope of protection of the present invention.

Claims

1. A method for manufacturing an AOP stereoscopically assembled microwave rigid-flexible board-level component, characterized in that: The following steps are involved: S1, manufacturing a flexible inner layer board with patterns through a semi-additive process; S2, manufacturing a microwave inner layer board with inner layer patterns through a semi-additive process; S3, manufacturing a microwave rigid-flexible board by bonding materials, wherein the microwave rigid-flexible board comprises a first rigid outer layer, a first flexible inner layer, a rigid inner layer, a second flexible inner layer, and a second rigid outer layer, wherein the first rigid outer layer, the rigid inner layer, and the second rigid outer layer are all microwave inner layer boards, and the first flexible inner layer and the second flexible inner layer are flexible inner layer boards; S4, assembling AOP devices on the top and bottom layers of the microwave rigid-flex board; S5, the rigid part is mounted on the metal structure and a three-dimensional assembly is formed by bending the flexible inner layer plate.

2. The method for manufacturing an AOP stereoscopically assembled microwave rigid-flexible board-level component according to claim 1, characterized in that: In step S1, the production process of the flexible inner layer board is: cutting, film lamination, LDI exposure, etching and developing, AOI inspection, browning, plasma treatment, cover film lamination, cover film pressing, laser milling shape; The graphics of the flexible inner layer board include signal lines and grid lines. The minimum line width of the signal line is 0.25mm, and the minimum line width of the grid line is 0.1mm. The grid lines of the flexible inner layer board are not coplanar with the signal lines, but are located on the ground of the signal lines. The shielding effect and the strength of the flexible inner layer board are enhanced by the mesh copper foil. The grid lines are encrypted within 1 to 10 mm of the overlapped edge with the rigid board to increase the fit between the flexible inner layer board and the structural support. Use dry film for graphic production process, the film pressure is 2~10Kg / cm 2 , the roller speed is 1-5m / s, the flexible inner layer board is patterned by LDI, the LDI spot diameter is 28μm, the depth of field is ±300μm, the resolution is 35μm, the exposure energy is 30-100mJ, the pH value of the flexible inner layer board development is set to 3.5-5, and the temperature is 30-45℃; The browning of the flexible inner layer board uses a mixture of H2SO4, H2O2 and organic compounds to oxidize Cu into Cu2O, and an organic copper oxide layer is formed through the chemical bonding of Cu2O and the organic compound; The thickness of the flexible inner layer is 0.1mm, and the thickness of the copper foil is 18um; The flexible inner layer board can be any one of Panasonic's R-8700, Ube Exsymo's Upisel-N, Shinyang Technology's W-Type, Shengyi Technology's SF280, SF202, and SF230; The covering film is modified by plasma treatment, with CF4:O2 of 0.05-0.2, power of 10-15 kW, time of 5-15 min, and flow rate of 1200-1800 mL / min; The pressing temperature of the covering film is 180-200°C, the pressure is 300-400psi, the vacuum degree is 25-35Bar, and the pressing time is 45-70min.

3. The method for manufacturing an AOP stereoscopically assembled microwave rigid-flexible board-level component according to claim 1, characterized in that: In step S2, the production process of the microwave inner layer board is: cutting, drilling, hole forming, plugging, film pasting, LDI exposure, etching and developing, AOI inspection, browning, lamination, drilling, hole forming, plugging, film pasting, LDI exposure, etching and developing, and browning. The microwave inner layer board includes 5 layers of microwave rigid copper clad laminates, 2 layers of adhesive materials, 2 layers of flexible copper clad laminates, and 3 layers of adhesive materials. The adhesive material is a microwave adhesive sheet, which is any one of CFB278F of the 46th Institute of China Electronics Technology, RLP30 of Ruilong Company, SJ928B of Shengyi Technology, and GNC300BP of Guoneng Company. Microwave rigid copper clad laminate is a PTFE-based system, and any one of PTFE / glass cloth, PTFE / micro-glass fiber, PTFE / glass cloth / ceramic powder, PTFE / micro-glass fiber / ceramic powder, PTFE / ceramic powder can be selected; The copper foil on the top layer of the microwave rigid copper clad laminate is any one of rolled copper foil, electrolytic copper foil, reverse copper foil and low profile copper foil, and the thickness of the copper foil is 18μm or 35μm; The dielectric thickness is 0.0127~1.016mm; The plugging is done by a vacuum plugging machine using conductive paste. After plugging, the copper paste is cured at 130-160°C for 30-60 minutes to form a conductive path. The conductive paste is one of AE2217 from Tuozida and CB102 from DuPont. The vacuum hot pressing temperature is 220℃-245℃.

4. The method for manufacturing an AOP stereoscopically assembled microwave rigid-flexible board-level component according to claim 1, characterized in that: In step S3, the first rigid outer layer integrates the functions of multi-stage amplification, power division and synthesis, and the second rigid outer layer integrates the functions of control and power supply.

5. The method for manufacturing an AOP stereoscopically assembled microwave rigid-flexible board-level component according to claim 1, characterized in that: In step S3, the rigid inner layer adopts a reverse depth control method to remove part of the material combined with the flexible inner layer board.

6. The method for manufacturing an AOP stereoscopically assembled microwave rigid-flexible board-level component as claimed in claim 3, characterized in that: The microwave rigid copper clad laminate is a 2.94 PTFE / glass fiber cloth / ceramic filler or a PTFE / micro glass fiber system / ceramic filler.

7. The method for manufacturing an AOP stereoscopically assembled microwave rigid-flexible board-level component according to claim 1, characterized in that: In the step S3, the flexible inner layer board and the microwave inner layer board are compounded by lamination, and the production of the microwave rigid-flexible board includes: pressing, drilling, hole chemical plating and electroplating, including side metallization, plugging, film pasting, LDI exposure, etching and developing, AOI inspection, surface coating, solder mask production, character production, and appearance processing.

8. The method for manufacturing an AOP stereoscopically assembled microwave rigid-flexible board-level component as claimed in claim 7, characterized in that: During the lamination, a gasket is placed on the flexible inner layer board to prevent the adhesive material from flowing onto the covering film; the non-welding areas of the rigid board are covered with solder resist to play a protective and welding auxiliary limit role; mechanical processing controlled depth milling is used to mill off the rigid parts above and below the flexible material to expose the flexible inner layer board part; the adhesive material used for the composite is a non-flow adhesive sheet, and the welding position of the microwave rigid-flexible composite board is surface-coated, and the coating material is gold-plated, chemical gold or nickel-gold-plated; the vacuum hot pressing temperature is 170°C-245°C, and the time is 1-6h; the nickel thickness of the chemical nickel-gold coating is 3-5um, and the gold thickness is 0.05-0.1um.

9. The method for manufacturing an AOP stereoscopically assembled microwave rigid-flexible board-level component according to claim 1, characterized in that: In the step S4, the rigid board area where the AOP device is installed is provided with stepped through grooves, the top-level large grooves are used for the nut installation of the pan head screws, and the bottom-level small grooves are used for the screws to pass through. The AOP devices on the rigid board are all provided with outer frame characters, position numbers, and mark points. The rigid board area where the connector is installed is provided with through grooves for installing screws. The inner walls of all the installation grooves are metallized on the sides, and the metallization production is the same process as the production of the metallized holes. The installation of surface mount devices is completed through double-sided SMT, and the installation of plug-in devices and connectors is completed through manual soldering. The rigid board where the AOP is located has AOPs densely arranged on the entire surface, and there are no other devices. The rigid board where the AOP is located is secondary soldering. The peak temperature of SMT is 260-270℃. SnPb series low-temperature solder is selected, and the melting point temperature is not higher than 183℃.

10. The method for manufacturing an AOP stereoscopically assembled microwave rigid-flexible board-level component according to claim 1, characterized in that: In step S5, the rigid part of the AOP assembly is installed on the plane of the structural member, the flexible part is pressed against the structural member support frame, the bent PCBA is installed on another plane of the structural member, and the rigid plate is fastened by screws to obtain a three-dimensionally assembled AOP component.