Stabilizer manufacturing method and base material

By forming a recess in the base material end of the vehicle stabilizer and perforating it therein, the problem of insufficient durability of the perforated parts is solved, and the effect of reducing load and extending the number of uses is achieved.

CN118973734APending Publication Date: 2024-11-15NHK SPRING CO LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202380029725.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2022-03-31
Filing Date
2023-03-17
Publication Date
2024-11-15

AI Technical Summary

Technical Problem

Perforated components are prone to wear during installation of vehicle stabilizers, resulting in reduced usage and insufficient durability.

Method used

By forging the base material, a recess is formed at the end of the stabilizer, and perforated is performed in the recess to form a through hole, thereby reducing the load of the perforated member.

Benefits of technology

Improves durability of perforated parts, reduces wear on the parts by load, and extends the number of uses.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118973734A_ABST
    Figure CN118973734A_ABST
Patent Text Reader

Abstract

The present invention is a method for manufacturing a stabilizer for manufacturing a stabilizer in which a through-hole is formed at both ends by performing a forging process on a base material, the method comprising: a recess forming step for forming a recess at a through-hole forming position corresponding to the through-hole in the stabilizer at the end of the base material; and a through-hole forming step of forming a through-hole by perforating the through-hole forming position including the recess.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a manufacturing method and a base material of a stabilizer. Background Art

[0002] A stabilizer for a vehicle or the like is mounted on the vehicle to stabilize the posture of the vehicle. The stabilizer is formed, for example, by deforming a solid or hollow rod-shaped member (see, for example, Patent Document 1). Both ends of the stabilizer are connected to the vehicle, and the connecting portion is flat. At the ends of the stabilizer, the rod-shaped member is flattened to form a flat plate, and a through hole is formed for inserting a fastening member such as a bolt.

[0003] Patent Document 1: Japanese Patent Application Laid-Open No. 63-273541 Summary of the invention

[0004] On the other hand, the through hole at the end of the stabilizer is formed by punching the end with a punching member. At this time, the load applied from the base material to the punching member during punching causes the punching member to wear. In order to increase the number of times the punching member can be used, it is necessary to improve the durability of the punching member.

[0005] The present invention has been made in view of the above circumstances, and an object of the present invention is to provide a method for manufacturing a stabilizer and a base material capable of improving the durability of a perforated member for forming a through hole by perforating.

[0006] In order to solve the above-mentioned problems and achieve the purpose, the manufacturing method of the stabilizer of the present invention is a method for manufacturing a stabilizer, which is a method for manufacturing a stabilizer in which a base material is subjected to forging treatment to produce a stabilizer having through holes formed at both ends, comprising: a recessed portion forming a recessed portion at a through hole forming position corresponding to the through hole in the stabilizer at the end of the base material; and a through hole forming step of punching the through hole forming position including the recessed portion to form a through hole.

[0007] Furthermore, in the method for manufacturing a stabilizer of the present invention according to the above invention, in the recessed portion forming step, the recessed portion is formed while the end portion of the base material is made into a flat plate shape.

[0008] Furthermore, the method for manufacturing a stabilizer of the present invention further comprises a heating step of heating an end portion of the base material according to the above invention, and in the recess forming step, the convex portion is formed on the end portion heated in the heating step.

[0009] Furthermore, the manufacturing method of the stabilizer of the present invention further includes a burr removal step of removing burrs from a region including the through hole formed in the through hole forming step according to the above invention.

[0010] In addition, the base material of the present invention is a base material for manufacturing a stabilizer having through holes formed at both ends by forging, and has a recessed portion formed at the end of the base material at a through hole forming position corresponding to the through holes in the stabilizer.

[0011] According to the present invention, it is possible to improve the durability of a punching member for forming a through hole by punching. BRIEF DESCRIPTION OF THE DRAWINGS

[0012] Figure 1 This is a side view showing an example of the structure of a stabilizer manufactured in one embodiment of the present invention.

[0013] Figure 2 It is used to illustrate the production Figure 1 A diagram showing a method of manufacturing a stabilizer.

[0014] Figure 3 It is used to make Figure 1 The base material of the stabilizer shown is a diagram of the base material before forging.

[0015] Figure 4 It is a figure which shows the structure of the end part of a base material before forging process.

[0016] Figure 5 yes Figure 4 AA line cross-sectional view shown in .

[0017] Figure 6 This is a diagram for explaining the change in the load on the punching member due to the presence or absence of a recessed portion when forming a through hole.

[0018] Figure 7 This is a diagram for explaining changes in the load on the punching component due to the presence or absence of a recessed portion when forming a through hole using a solid base material. DETAILED DESCRIPTION

[0019] Hereinafter, a method for implementing the present invention (hereinafter referred to as "implementation method") will be described with reference to the accompanying drawings. In addition, the accompanying drawings are schematic diagrams, and the relationship between the thickness and width of each part, the ratio of the thickness of each part, etc. may be different from the actual object, and the drawings may sometimes include parts with different size relationships or ratios.

[0020] Implementation

[0021] Figure 1 This is a side view showing an example of the structure of a stabilizer manufactured in one embodiment of the present invention. Figure 1The stabilizer 1 shown is formed of metal or various fiber-reinforced resins (e.g., GFRP (Glass Fiber Reinforced Plastic)). The stabilizer 1 has a main body 2, a first end 3, and a second end 4. The main body 2 is bent at both ends and extends in a straight line in the middle. The first end 3 is arranged at one end of the main body 2, and the second end 4 is arranged at the other end of the main body 2.

[0022] The main body 2 is in a columnar shape, for example, extending in a cylindrical shape. Although an example in which the main body 2 is hollow is described, the main body 2 may also be solid.

[0023] The first end portion 3 is in the shape of a flat plate and is provided with a through hole 31 penetrating the first end portion 3 in the plate thickness direction.

[0024] The second end portion 4 is in the shape of a flat plate. A through hole 41 penetrating the second end portion 4 in the plate thickness direction is formed.

[0025] For example, when the stabilizer 1 is installed in a car, the first end 3 is connected to one of the left and right suspensions, and the second end 4 is connected to the other suspension. At this time, fastening members such as bolts are inserted into the through holes to fix each end to the suspension.

[0026] Next, refer to Figure 2 to Figure 5 A method for manufacturing the stabilizer 1 will be described. Figure 2 It is used to illustrate the production Figure 1 The stabilizer 1 is manufactured by forging a base material.

[0027] The base material 10 is formed by bending both ends of a cylindrical member, and has a main body 11, a first end 12, and a second end 13. First, the first end 12 and the second end 13 of the base material 10 are heated (see Figure 2 (a): Heating step). In the heating process, each end portion is heated using, for example, a heating coil 110 .

[0028] After heating both ends of the base material 10, each end is pressed (see Figure 2 (b): plating step). For example, Figure 2 As shown in (b), the end of the base material 10 ( Figure 2 The first end portion 12 in the embodiment is held on the holding member 120a, and the end portion placed on the holding member 120a is pressed by the pressing member 120b, thereby flattening the end portion into a flat plate shape (see Figure 2(c)). At this time, a convex portion 120c is formed at a position of the pressing member 120b corresponding to the position where the through hole of the base material 10 is formed. Therefore, by flattening, a concave portion 12a corresponding to the shape of the convex portion 120c is formed at the end of the base material 10 (concave portion forming step). In this embodiment, the flattening step and the concave portion forming step are performed simultaneously.

[0029] After the first end portion 12 and the second end portion 13 are formed, a cutting process is performed (see Figure 2 (d)). In the cutting process, the first end portion 12 and the second end portion 13 are subjected to a through hole forming process (through hole forming step) and a trimming process (trimming process step). Figure 2 (d) shows an example of processing the first end portion 12 , and the second end portion 13 is processed in the same manner.

[0030] The through hole is formed by punching the first end portion 12 using the punching member 130a. At this time, the first end portion 12 is placed on the support member 130b and pressed against the support member 130b by the punching template 130c. The support member 130b and the punching template 130c have a hollow portion through which the front end of the punching member 130a can be inserted. The punching member 130a is passed through the punching template 130c to punch a hole at the through hole forming position of the first end portion 12 including the recess 12a, thereby forming a through hole ( Figure 2 The through hole 12b shown in (e).

[0031] Figure 3 It is used to make Figure 1 The base material of the stabilizer shown is a diagram of the base material before forging. Figure 4 It is a diagram showing the structure of the end portion of a base material before forging. Figure 5 yes Figure 4 AA line cross-sectional view shown in . Figure 3 and Figure 4 The base material 10 shown has a main body 11 with both ends bent, a first end 12 provided at one end of the main body 11, and a second end 13 provided at the other end of the main body 11. In addition, recesses 12a and 13a are formed in the first end 12 and the second end 13, respectively.

[0032] For example, the recess 12a is in the shape of a hole forming a conical internal space. The recess 12a is set in an area including the position where the through hole is formed. The formation range of the recess 12a, for example, the area with the width W1 of the opening as the diameter on the surface of the first end 12, is set in the first end 12 (first end 3) according to the area where the fastening member is arranged. At this time, the recess 12a is preferably formed at a position where the central axis of the perforated member 130a passes through the apex of the cone. In addition, the width W1 is set to be within a range of 70% or more and less than 100% relative to the diameter R1 of the perforated member 130a (that is, the diameter of the through hole 12b). In addition, the depth D1 of the recess is set to be within a range of 10% or more and 80% or less relative to the thickness H1 of the first end 12. By setting the width W1 and the diameter R1 to the above range, the load on the perforated member 130a can be effectively reduced. In the present embodiment, the case where the recessed portion 12a forms a conical space is described, but the recessed portion may be a recessed portion in another concave shape, for example, a truncated cone-shaped space.

[0033] The same applies to the recessed portion 13a.

[0034] Return to Figure 2 During the trimming process, a trimming knife 130d is used to form the outer shape of the first end portion 12 (see Figure 2 In the trimming process, a trimming knife 130d is used, for example, Figure 4 As shown, along the processing line L of the first end portion 12 C The cutout is performed, thereby forming the outer shape of the first end portion 3 .

[0035] In addition, the construction order of the through hole formation and the trimming process may be either one of them is performed first.

[0036] After the cutting process, a burr removal process is performed to remove burrs using the formed part 140a (see Figure 2 (e): burr removal step). At this time, the first end portion 12 is placed on the support member 140b. By clamping the first end portion 12 with the forming member 140a and the support member 140b, the burrs formed around the through hole 12b are flattened, thereby removing the burrs. Figure 1 The stabilizer 1 is shown.

[0037] Here, refer to Figure 6 The difference in load applied to the punching member 130 a depending on whether or not there is a recessed portion in the base material will be described. Figure 6 This is a diagram for explaining changes in the load on the punching member depending on the presence or absence of a recessed portion when forming a through hole. Figure 6The following is an example of analyzing the load change in the punching component when forming a through hole when the diameter R1 of the punching component 130a is set to 14.4mm and the thickness H1 of the end of the base material 10 is set to 7.3mm. The stroke is equivalent to the length of the punching component 130a entering from the surface of the base material. Curve L1 represents the load change when the width W1 of the recess 12a is set to 12.96mm and the depth D1 is set to 5.00mm. Curve L2 represents the load change when the width W1 of the recess 12a is set to 12.96mm and the depth D1 is set to 3.00mm. Curve L3 represents the load change when there is no recess 12a. According to Figure 6 The analysis results show that the presence of the recessed portion 12a can reduce the load.

[0038] In addition, refer to Figure 7 The difference in load applied to the punching member 130a depending on whether or not there is a recessed portion in the solid base material will be described. Figure 7 This is a diagram for explaining changes in the load on the punching component due to the presence or absence of a recessed portion when forming a through hole using a solid base material. Figure 7 The following is an example of analyzing the load change in the punching member when forming a through hole when the diameter R1 of the punching member 130a is set to 14.4 mm and the thickness of the base material end is set to 7.3 mm. 11 The curve L shows the load change when the width W1 of the concave portion (equivalent to the concave portion 12a) is set to 12.96 mm and the depth D1 is set to 5.00 mm. 12 The load change when there is no concave portion is shown. Figure 7 The analysis results show that having a recessed portion can reduce the load.

[0039] In the embodiment of the present invention described above, a recess is formed at the through-hole forming position in the base material for manufacturing the stabilizer, and the through-hole is formed by punching the area including the recess. According to this embodiment, the load on the perforated component 130a is reduced by forming the recess, so that the durability of the perforated component can be improved.

[0040] Furthermore, according to the present embodiment, since the load on the recessed portion during the punching is reduced, it is possible to suppress the warping of the end portion due to the punching load and the reduction in the adhesion between the inner peripheral surfaces.

[0041] So far, the method for implementing the present invention has been described, but the present invention should not be limited to the above-mentioned embodiment. For example, the present invention can be applied to products in which through holes are formed by punching or trimming is performed. In addition, in the embodiment, an example of forming a concave portion while making the end of the base material 10 flat is described, but the flattening and the concave portion formation can also be performed at different points in time. That is, in the embodiment, although the flattening step and the concave portion formation step are performed at the same time, the flattening step and the concave portion formation step can also be performed at different points in time.

[0042] As described above, the present invention may include various embodiments and the like that are not described here, and various design changes and the like can be implemented within the scope of the technical concept defined in the claims.

[0043] As described above, the method for manufacturing a stabilizer and the base material of the present invention are suitable for improving the durability of a perforated member for forming a through hole by perforating.

[0044] Explanation of symbols

[0045] 1 Stabilizer

[0046] 2.11 Main body

[0047] 3.12 First end

[0048] 4.13 Second end

[0049] 10 Parent material

[0050] 12a, 13a concave parts

[0051] 31, 41 through hole

[0052] 120a Holding component

[0053] 120b Pressing part

[0054] 120c convex part

[0055] 130a Perforated parts

[0056] 130b, 140b support member

[0057] 130c Punching Template

[0058] 130d Trimming Knife

[0059] 140a Formed part.

Claims

1. A method for manufacturing a stabilizer, forging a base material to produce a stabilizer having through holes formed at both ends, characterized in that: include: A concave portion forming step of forming a concave portion at a through hole forming position corresponding to the through hole in the stabilizer at the end of the base material; as well as A through hole forming step of punching the through hole forming position including the recessed portion to form a through hole.

2. The method for manufacturing a stabilizer according to claim 1, characterized in that: In the recessed portion forming step, the recessed portion is formed while the end portion of the base material is changed into a flat plate shape.

3. The method for manufacturing a stabilizer according to claim 1 or 2, characterized in that: The method further comprises a heating step of heating the end of the base material. In the recess forming step, the recess is formed on the end portion heated in the heating step.

4. The method for manufacturing a stabilizer according to claim 1, characterized in that: The method further includes a burr removal step of removing burrs from a region including the through hole formed in the through hole forming step.

5. A base material used for manufacturing a stabilizer having through holes formed at both ends by forging, characterized in that: A recessed portion is formed at an end portion of the base material at a through-hole forming position corresponding to the through-hole in the stabilizer.

Citation Information

Patent Citations

  • Manufacturing process of hollow stabilizer rod of automobile

    CN102189910A

  • Hollow stabilizer for vehicle and manufacturing method thereof

    JP1995237428A

  • Metal processing apparatus and metal processing method

    JP2021142538A

  • Vehicle stabilizer, processing device for eye portion of stabilizer, and processing method for eye portion

    US20180229576A1

  • Method and device for producing stabilisers

    WO2006047990A1