Pipe piece steel reinforcement framework top-speed welding integrated forming technology
Through automated welding devices and carbon dioxide gas protective welding technology, the problems of low manual welding efficiency and unstable quality are solved, and efficient automated welding of pipe sheet reinforcement frames is achieved, which improves welding speed and quality and reduces costs.
Patent Information
- Application Number
- CN202411318996.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-21
- Publication Date
- 2024-11-19
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
In the prior art, welding of pipe sheet reinforcement frames relies on manual operations, resulting in low production efficiency, slow welding speed, and easy to miss welding and de-welding, which makes it difficult to control the welding strength, affecting the welding quality.
The automated welding device is adopted, including a control module, a detection module and a welding module. The detection module identifies the marks on the prefabricated parts and feedback signals to the control module to control the welding module for welding, combining carbon dioxide gas protective welding and specific types of welding wires. Achieve automated welding.
Automatic welding of pipe sheet reinforcement frames has been realized, which significantly accelerates the welding speed, improves welding quality, reduces costs, and avoids the problems of missing welding and desoldering in manual welding.
Smart Images

Figure CN118977070A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of steel bar welding, and in particular to a technology for extremely fast welding and integrally forming a steel bar skeleton of a pipe segment. Background Art
[0002] With the rapid development of the construction industry and the introduction of the concepts of green building and building industrialization, prefabricated structures for construction have gradually become an important part of prefabricated buildings. In order to produce prefabricated components more efficiently and with higher quality, the automatically formed steel skeleton is an important supporting part of the components. The quality assurance of its production directly affects the overall quality of the construction project. However, in the prior art, manual welding is often used when welding the steel bar skeleton of the pipe segment. A person holds a welding gun and welds each intersection of the main reinforcement and the ring reinforcement. In actual production, the production efficiency is relatively low, the welding speed is slow, and during the welding process, manual welding is prone to welding leaks and de-welding. The welding strength is difficult to control, and the welding quality cannot be guaranteed. Summary of the invention
[0003] In view of the shortcomings of the prior art, the present invention solves the technical problems by adopting a technical solution: a rapid welding integrated forming technology for a pipe segment steel frame, comprising the following steps: Step 1: Steel bar processing: Process the inner and outer steel bar rings and other components required for the steel bar skeleton and assemble them into prefabricated parts; Step 2: Cleaning the steel bars: Clean the prefabricated parts processed in step 1, and clean the debris and rust marks on the surface of the steel bars; Step 3: Welding marking: Place the cleaned prefabricated parts on the welding workbench, determine the welding position and weld layout on the prefabricated parts cleaned in step 2 according to the required steel skeleton size and welding requirements, and mark them on the prefabricated parts; Step 4, welding operation: move the prefabricated part marked in step 3 to the welding area, the welding device tracks and determines the position to be welded, and performs welding. The welding equipment automatically welds the prefabricated part marked in step 3; Step 5. Welding inspection: After welding is completed, visually inspect the welding parts to ensure that the welds are firm and free of obvious cracks and defects, thus completing the welding of the steel frame of the pipe segment.
[0004] The present invention is further configured as follows: the welding device in step 4 includes a control module, a detection module and a welding module, the welding module and the detection module are separately connected to the control module, the control module is used to control the operation of the detection module and the welding module, the detection module is used to identify the marking area of the prefabricated part, and feed back to the control module to control the movement of the welding module, and the welding module is used to weld the marking area. During welding, the mark on the prefabricated part is identified by the detection module, and when the welding mark is detected, the signal is fed back to the control module, and the control module controls the welding module to approach the mark on the prefabricated part and perform welding.
[0005] The present invention is further configured as follows: the welding module includes a gas supply unit, a wire filling unit and a welding transfer unit. The gas supply unit is used to deliver protective gas, the wire filling unit quickly fills the starting weld with welding wire under arc heating conditions, and the welding transfer unit keeps the processed part moving at a constant speed relative to the welding wire in the forward direction.
[0006] The present invention is further configured as follows: the protective gas of the gas supply unit is selected from carbon dioxide gas, and the gas flow rate is 20-25 L / min. Carbon dioxide gas shielded welding does not require cleaning after welding, and is not limited by the welding position, which not only ensures the welding quality, but also effectively speeds up the welding speed.
[0007] The present invention is further configured as follows: the wire-filling unit adopts H08MnA type welding wire, the wire-filling speed of the wire-filling unit is 5-10 mm / s, and the moving speed of the moving welding unit is 1-8 mm / s. The conventional welding wire reacts with carbon dioxide gas, and part of the carbon monoxide gas generated by the reaction is dispersed into the air by boiling, and the other part is blocked in the weld to cause pores because it cannot volatilize in time. The H08MnA type special welding wire containing manganese and silicon elements for welding low-carbon steel is adopted. When welding with this welding wire, the iron oxide in the molten pool will be reduced by manganese and silicon elements, and the generated silicon dioxide and manganese oxide will further react to generate iron oxide and manganese silicates on the slag surface to protect the weld.
[0008] The present invention is further configured as follows: the welding current of the transfer welding unit is 180A to 200A, the welding voltage is 25 to 27V, and the control unit controls the moving speed of the transfer welding unit to be Q, wherein Q=I²RT, wherein: I-welding current, R-arc and dry extension equivalent resistance, T-welding time. When the welding speed is too high, the protective effect of the gas will be reduced, and at the same time, the cooling speed of the weld will be accelerated. Therefore, the plasticity of the weld will be reduced, making it difficult to form the weld. On the contrary, when the welding speed is too low, the width of the weld will be significantly widened, and welding defects such as burn-through are likely to occur due to the heat concentration of the molten pool.
[0009] The beneficial effects of the present invention are as follows: 1. The present invention sets a control module, a detection module and a welding module. The detection module identifies the mark on the prefabricated part. When the welding mark is detected, the signal is fed back to the control module. The control module controls the welding module to approach the mark on the prefabricated part and perform welding. It can realize automated operation, effectively replace manual welding, and speed up the welding speed of the steel frame of the pipe segment.
[0010] 2. The present invention adopts carbon dioxide gas for shielded welding, so there is no need to clean up after welding, and it is not limited by the welding position, which ensures the welding quality. Compared with manual arc welding, the cost of the entire welding process is very low, which can be reduced by about half. The carbon dioxide gas shielded welding process is not limited by the welding position, and the open arc welding form of carbon dioxide gas shielded welding is also conducive to the control of the welding process. The welding speed is effectively accelerated.
[0011] 3. The present invention matches the welding speed by controlling the welding current, welding resistance and welding time combination to prevent the welding speed from being too high, thereby reducing the protective effect of the gas and causing the weld to cool faster, or the welding speed from being too low, in which case the width of the weld will become significantly wider. Due to the heat concentration in the molten pool, welding defects such as burn-through are likely to occur. BRIEF DESCRIPTION OF THE DRAWINGS
[0012] Figure 1 is a flow chart of the present invention; Figure 2 It is a performance test comparison table of the present invention. DETAILED DESCRIPTION
[0013] The present invention is further described in detail below in conjunction with the accompanying drawings and specific embodiments. The embodiments of the present invention are provided for the purpose of illustration and description, and are not intended to be exhaustive or to limit the present invention to the disclosed forms. Many modifications and variations will be apparent to those of ordinary skill in the art. The embodiments are selected and described in order to better illustrate the principles and practical applications of the present invention, and to enable those of ordinary skill in the art to understand the present invention and thereby design various embodiments with various modifications suitable for specific uses.
[0014] Embodiment 1: See also Figure 1 - Figure 2 The present invention provides a technical solution: a technology for rapid welding and integrally forming a pipe segment reinforcement frame, comprising the following steps: Step 1: Steel bar processing: Process the inner and outer steel bar rings and other components required for the steel bar skeleton and assemble them into prefabricated parts; Step 2: Cleaning the steel bars: Clean the prefabricated parts processed in step 1, and clean the debris and rust marks on the surface of the steel bars; Step 3: Welding marking: Place the cleaned prefabricated parts on the welding workbench, determine the welding position and weld layout on the prefabricated parts cleaned in step 2 according to the required steel skeleton size and welding requirements, and mark them on the prefabricated parts; Step 4, welding operation: move the prefabricated part marked in step 3 to the welding area, the welding device tracks and determines the position to be welded, and performs welding. The welding equipment automatically welds the prefabricated part marked in step 3; Step 5. Welding inspection: After welding is completed, visually inspect the welding parts to ensure that the welds are firm and free of obvious cracks and defects, thus completing the welding of the steel skeleton of the pipe segment.
[0015] In step four, the welding device includes a control module, a detection module and a welding module. The welding module and the detection module are separately connected to the control module. The control module is used to control the operation of the detection module and the welding module. The detection module is used to identify the marking area of the prefabricated part and provide feedback to the control module to control the movement of the welding module. The welding module is used to weld the marking area.
[0016] The welding module includes a gas supply unit, a wire filling unit and a welding transfer unit. The gas supply unit is used to deliver shielding gas, the wire filling unit quickly fills the starting weld with welding wire under arc heating conditions, and the welding transfer unit keeps the processed parts moving at a constant speed relative to the welding wire in the forward direction. During welding, the detection module identifies the mark on the prefabricated part, and when the welding mark is detected, the signal is fed back to the control module, which controls the welding module to approach the mark on the prefabricated part and perform welding.
[0017] The shielding gas of the gas supply unit is selected from carbon dioxide gas, and the gas flow rate is 20-25L / min. Carbon dioxide gas shielded welding does not require cleaning after welding, and is not limited by the welding position, which not only ensures the welding quality, but also effectively speeds up the welding speed. When welding with this welding wire, the iron oxide in the molten pool will be reduced by manganese and silicon elements, and the generated silicon dioxide and manganese oxide will further react to form iron oxide and manganese silicates on the slag surface to protect the weld.
[0018] The wire filling unit adopts H08MnA type welding wire, the wire filling speed of the wire filling unit is 5-10 mm / s, and the moving speed of the welding transfer unit is 1-8 mm / s.
[0019] The welding current of the transfer welding unit is 180A~200A, the welding voltage is 25~27V, and the control unit controls the moving speed of the transfer welding unit to be Q, Q=I²RT, where: I-welding current, R-arc and dry extension equivalent resistance, T-welding time.
[0020] Embodiment 2: Based on Example 1, please refer to Figure 1 The present invention provides a technical solution: a technology for rapid welding and forming a steel frame of a pipe segment, comprising the following steps: Step 1: Steel bar processing: Process the inner and outer steel bar rings and other components required for the steel bar skeleton and assemble them into prefabricated parts; Step 2: Cleaning the steel bars: Clean the prefabricated parts processed in step 1, and clean the debris and rust marks on the surface of the steel bars; Step 3: Welding marking: Place the cleaned prefabricated parts on the welding workbench, determine the welding position and weld layout on the prefabricated parts cleaned in step 2 according to the required steel skeleton size and welding requirements, and mark them on the prefabricated parts; Step 4, welding operation: move the prefabricated part marked in step 3 to the welding area, the welding device tracks and determines the position to be welded, and performs welding. The welding equipment automatically welds the prefabricated part marked in step 3; Step 5. Welding inspection: After welding is completed, visually inspect the welding parts to ensure that the welds are firm and free of obvious cracks and defects, thus completing the welding of the steel frame of the pipe segment.
[0021] In step four, the welding device includes a control module, a detection module and a welding module. The welding module and the detection module are separately connected to the control module. The control module is used to control the operation of the detection module and the welding module. The detection module is used to identify the marking area of the prefabricated part and provide feedback to the control module to control the movement of the welding module. The welding module is used to weld the marking area.
[0022] The welding module includes a gas supply unit, a wire filling unit and a welding transfer unit.
[0023] The protective gas of the gas supply unit is selected from argon, and the gas flow rate is 15L / min.
[0024] The wire filling speed of the wire filling unit is 5 to 10 mm / s, and the moving speed of the welding transfer unit is 1 to 8 mm / s.
[0025] The welding current of the transfer welding unit is 180AA, the welding voltage is 27V, and the control unit controls the moving speed of the transfer welding unit to be Q, Q=I²RT, where: I-welding current, R-arc and dry extension equivalent resistance, T-welding time.
[0026] Embodiment three: Based on Example 1, please refer to Figure 1 The present invention provides a technical solution: a technology for rapid welding and forming a steel frame of a pipe segment, comprising the following steps: Step 1: Steel bar processing: Process the inner and outer steel bar rings and other components required for the steel bar skeleton and assemble them into prefabricated parts; Step 2: Cleaning the steel bars: Clean the prefabricated parts processed in step 1, and clean the debris and rust marks on the surface of the steel bars; Step 3: Welding marking: Place the cleaned prefabricated parts on the welding workbench, determine the welding position and weld layout on the prefabricated parts cleaned in step 2 according to the required steel skeleton size and welding requirements, and mark them on the prefabricated parts; Step 4, welding operation: move the prefabricated part marked in step 3 to the welding area, the welding device tracks and determines the position to be welded, and performs welding. The welding equipment automatically welds the prefabricated part marked in step 3; Step 5. Welding inspection: After welding is completed, visually inspect the welding parts to ensure that the welds are firm and free of obvious cracks and defects, thus completing the welding of the steel skeleton of the pipe segment.
[0027] In step four, the welding device includes a control module, a detection module and a welding module. The welding module and the detection module are separately connected to the control module. The control module is used to control the operation of the detection module and the welding module. The detection module is used to identify the marking area of the prefabricated part and provide feedback to the control module to control the movement of the welding module. The welding module is used to weld the marking area.
[0028] The welding module includes a gas supply unit, a wire filling unit and a welding transfer unit.
[0029] The protective gas of the gas supply unit is selected from carbon dioxide gas, and the gas flow rate is 20L / min.
[0030] The wire filling speed of the wire filling unit is 5 mm / s, and the moving speed of the welding transfer unit is 4 mm / s.
[0031] The welding current of the transfer welding unit is 180A, the welding voltage is 25V, and the control unit controls the moving speed of the transfer welding unit to be Q, Q=I²RT, where: I-welding current, R-arc and dry extension equivalent resistance, T-welding time.
[0032] Performance testing: Two sections of steel bars were selected for welding according to the methods of Example 1, Example 2 and Example 3, respectively as the first group, the second group and the third group, to obtain welded steel bars with different strengths, and their tensile strength, yield strength and yield stress were tested; In the comparison of three groups of experiments, the results of the three groups of welded steel bars in the tests of tensile strength, yield strength and yield stress are roughly the same, and the differences between the groups are not obvious. Therefore, after ensuring the welding strength, the present invention sets a control module, a detection module and a welding module. The detection module identifies the mark on the prefabricated part. When the welding mark is detected, the signal is fed back to the control module. The control module controls the welding module to approach the mark on the prefabricated part and perform welding. This can realize automated operation, effectively replace manual welding, and speed up the welding speed of the pipe segment steel skeleton.
[0033] Obviously, the described embodiments are only some embodiments of the present invention, not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field and related fields without creative work should fall within the scope of protection of the present invention. The structures, devices and operating methods not specifically described and explained in the present invention are implemented according to the conventional means in the field unless otherwise specified and limited.
Claims
1. The rapid welding and integrated forming technology of the segment steel frame is characterized by: The following steps are involved: Step 1: Steel bar processing: Process the inner and outer steel bar rings and other components required for the steel bar skeleton into shapes and assemble them into prefabricated parts; Step 2: Cleaning the steel bars: Clean the prefabricated parts processed in step 1, and remove debris and rust marks on the surface of the steel bars; Step 3: Welding Marking: Place the cleaned prefabricated part on the welding workbench. According to the required steel bar skeleton size and welding requirements, determine the welding position and weld layout on the prefabricated part cleaned in step 2, and mark it on the prefabricated part. Step 4, welding operation: move the prefabricated part marked in step 3 into the welding area, the welding device tracks and determines the position to be welded, and performs welding. The welding equipment automatically welds the prefabricated part marked in step 3; Step 5. Welding inspection: After welding is completed, conduct a visual inspection of the welding parts to ensure that the welds are firm and free of obvious cracks and defects, thus completing the welding of the steel frame of the pipe segment.
2. The rapid welding integrated forming technology for the segment reinforcement skeleton according to claim 1 is characterized in that: The welding device in step 4 includes a control module, a detection module and a welding module. The welding module and the detection module are separately connected to the control module. The control module is used to control the operation of the detection module and the welding module. The detection module is used to identify the marking area of the prefabricated part and provide feedback to the control module to control the movement of the welding module. The welding module is used to weld the marking area.
3. The rapid welding and integrated forming technology for the segment reinforcement skeleton according to claim 2 is characterized in that: The welding module includes an air supply unit, a wire filling unit and a welding transfer unit.
4. The rapid welding and integrated forming technology for the segment reinforcement skeleton according to claim 2 is characterized in that: The protective gas of the gas supply unit is selected from carbon dioxide gas, and the gas flow rate is 20 to 25 L / min.
5. The rapid welding and integrated forming technology for the segment reinforcement skeleton according to claim 2 is characterized in that: The wire filling unit adopts H08MnA type welding wire, the wire filling speed of the wire filling unit is 5-10 mm / s, and the moving speed of the welding transfer unit is 1-8 mm / s.
6. The rapid welding and integrated forming technology for the segment reinforcement skeleton according to claim 2 is characterized in that: The welding current of the transfer welding unit is 180A to 200A, the welding voltage is 25 to 27V, and the control unit controls the moving speed of the transfer welding unit to be Q, wherein Q=I²RT, wherein: I is welding current, R is arc and dry extension equivalent resistance, and T is welding time.
Citation Information
Patent Citations
Carbon dioxide gas shielded welding machine and method of controlling arc strike by adopting digital pulse
CN104096947A
Welding method of nuclear power station stainless steel container covering plate
CN114669842A
Steel structure profile welding method
CN116673569A
Reinforcing mesh welding method
CN117564415A
Performance testing device for reinforced concrete pipe piece
CN220251613U