Active interlayer flexible protective screen and preparation method, preparation device and application of active material of active interlayer flexible protective screen

Through the new active material preparation method and device, the problems of preparation and application of THV-based active material are solved, and the flexible active interlayer flexible protective screen with small volume and weight is realized, which improves the protection performance of space debris and micrometeors, and through Self-healing materials extend the service life of the spacecraft.

CN118978776APending Publication Date: 2024-11-19ZHONGBEI UNIV
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410950111.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-16
Publication Date
2024-11-19

AI Technical Summary

Technical Problem

The traditional Whipple rigid protective structure has a large volume and a fixed installation position, and the inert material protection mechanism is single, making it difficult to effectively resist the impact of large-sized space debris. The THV-based active material preparation process is not suitable for use in aerospace pressure cabin protective screens.

Method used

Using new active material preparation methods and devices, the THV pellets are uniformly mixed with metal powder through the dissolution and distillation process of ethyl acetate to form an active material with zero oxygen balance ratio, and applied it to the flexible protective screen of the active interlayer. High temperature, high pressure and high speed explosion products are used to generate reverse impulse to reduce the axial kinetic energy of space debris.

Benefits of technology

It realizes a small volume and flexible protective screen, improves the protection performance of space debris and micrometeors, meets the protection needs of large space structures, and reduces maintenance costs through self-healing materials and extends the service life of the spacecraft.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118978776A_ABST
    Figure CN118978776A_ABST
Patent Text Reader

Abstract

The invention provides an active interlayer flexible protective screen as well as a preparation method, a preparation device and application of an active material of the active interlayer flexible protective screen, the preparation of a THV-based active material is improved, and the THV-based active material is applied to a spaceflight pressure cabin protective screen. The active interlayer flexible protective screen prepared from the active material occupies small volume and weight of a spaceflight pressure chamber, and can be matched with the working process of the chamber body to realize a protection function, meanwhile, the THV-based active material is applied to the protective screen, high-temperature, high-pressure and high-speed moving detonation products at the moment of explosion can generate reverse impulse on projectiles, and the projectiles are prevented from being exploded by the THV-based active material. The axial kinetic energy of the space debris is further reduced, the protection performance is improved, meanwhile, activation and flexibility of the protection structure are achieved, and the application requirement for space debris and micrometeor protection is met.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to an active sandwich flexible protective screen and a method, a device and application of its active material preparation, and belongs to the field of aerospace vehicle protection and safety. Background Art

[0002] Improving the safety and survivability of spacecraft is crucial to the aerospace field. Collision protection is a key aspect of this, which requires effective protection against the impact of space debris and micrometeorites. Traditional collision protection technology mainly uses Whipple rigid protection structure, which consists of two layers of aluminum alloy protection screens, which can absorb and disperse collision energy to a certain extent and provide protection for the space pressure cabin wall. However, this rigid protection structure has disadvantages such as large size and weight and fixed installation position, which limits its application in large space structures such as space pressure cabins.

[0003] Although the materials of space debris protection structures in aerospace pressure cabins are diverse, they are all inert materials. Due to the single protection mechanism, the protection ability of the protection structure against large-sized space debris is largely restricted. Replacing the traditional aluminum protective screen with active materials and utilizing the characteristics of active materials releasing chemical energy during high-speed impact can further increase the expansion speed of the debris cloud and effectively reduce the damage effect of space debris on the cabin wall. Active materials have potential application prospects in Whipple protective screens. However, due to their low melting point, they are difficult to cope with the complexity of the space environment, so their application in protective screens has certain challenges.

[0004] Therefore, how to apply active materials to the protective shields of large space structures such as aerospace pressure cabins has become the key technical problem to be solved in this program.

[0005] In addition, as the basic formula of fluoropolymer-based active materials, active materials prepared by mechanical mixing-molding-sintering of aluminum powder and polytetrafluoroethylene powder (Al / PTFE) have been widely studied by scholars at home and abroad, and certain application results have been achieved. However, the finished product of tetrafluoroethylene-hexafluoropropylene-vinylidene fluoride terpolymer (THV) is generally in the form of large particles rather than ultrafine powders, so it is impossible to obtain a uniform mixture of metal powder and THV particles through traditional mechanical mixing methods. The traditional preparation process is obviously not suitable for THV-based active materials. Therefore, before the active materials are applied to the protective shields of large space structures such as aerospace pressure cabins, it is necessary to improve the preparation method and device of THV-based active materials. Summary of the invention

[0006] The purpose of the present invention is to overcome the above-mentioned defects, provide an active material preparation method and preparation device, solve the preparation of THV-based active materials, and apply them to the protective screens of large space structures such as aerospace pressure cabins. The active sandwich flexible protective screen made of this active material occupies a small volume and weight of the aircraft, and can cooperate with the working process of the cabin to realize the deployment of the protective function. At the same time, the THV-based active material is applied to the protective screen, and the high-temperature, high-pressure, and high-speed movement of the detonation products at the moment of explosion will produce a reverse impulse to the projectile, further reducing the axial kinetic energy of space debris and improving the protective performance. In this way, the activation and flexibility of the protective structure are realized at the same time, meeting the application requirements for the protection of space debris and micrometeorites.

[0007] In order to achieve the above-mentioned object of the invention, the present invention provides the following technical solutions: A method for preparing an active material comprises the following steps: Step 1: dissolving THV particles; specifically, adding ethyl acetate and THV particles into a reaction kettle, controlling the concentration of THV solution at 0.1 g / ml, heating in a water bath to 70-90° C., stirring continuously during the process, until the THV particles are completely dissolved; Step 2: Add metal powder; specifically, add metal powder according to the mass of THV monomer in a zero oxygen balance ratio, and stir to mix evenly, the stirring time is 30-60 minutes; Step 3: Solvent evaporation; Specifically, the water bath temperature is raised to 82°C, and a distillation device is installed for distillation. In order to keep the metal powder uniformly dispersed at all times, it is necessary to stir continuously during the distillation until the solvent is completely evaporated; Step 4: Extraction and drying; specifically, after complete evaporation, a large solid mixture is obtained, and the solid mixture is cut into small pieces of 1-2 mm and placed in a drying oven for vacuum drying for 12 h; Step 5: hot pressing; specifically, the dried active material is loaded into a forming mold, the forming mold is placed in a drying oven, the temperature of the drying oven is heated to 160°C and kept warm for 30 minutes, and then the forming mold is taken out; or the dried material is loaded into a heating mold, the heating mold is heated to 120-160°C and kept warm for 30 minutes; finally, the forming mold or the heating mold is placed on a universal testing machine and pressurized to 15MPa at a pressurization speed of 0.05MPa / s, and the pressure is maintained for 30 minutes. After the pressurization is completed, the mold is removed after cooling to obtain the active material. Furthermore, the metal includes any one of aluminum, tungsten, tantalum, nickel, hafnium and zirconium, or a combination of two or more thereof.

[0008] A preparation device for active materials, used to perform steps 1 to 4 of the above-mentioned preparation method, comprising a reactor, a water bath sleeved outside the reactor, a piston plate slidably arranged in the reactor, a vertical column with a top fixedly connected to the bottom of the piston plate, a lifting cylinder fixedly connected to the bottom of the vertical column, and a stirring and dividing structure arranged above the piston plate, wherein the stirring and dividing structure and the water bath are fixed on a bracket; the reactor is vertically cylindrical and connected at both ends.

[0009] The stirring and dividing structure includes a plurality of dividing plates connected to each other and arranged in a circular array, a rotating cylinder fixedly connected to the top ends of the plurality of dividing plates, a vertical gear rod connected to the rotating cylinder at the bottom end, gear 2 and gear 3 respectively arranged on both sides of the upper end of the gear rod, gear 1 meshingly connected to the outer side of gear 2, a transmission belt coaxially connected to gear 1 and gear 3 at both ends respectively, and a driving motor coaxially connected to gear 3.

[0010] An active material is prepared by the preparation method.

[0011] Application of active materials in protective shields of aerospace pressure chambers.

[0012] An active sandwich flexible protective screen, made of the active material, comprising a front screen, a rear screen and an inflatable tube; The front screen includes a plurality of unit bodies connected in sequence, and an MLI (Multi-Layer Insulation, MLI) heat insulation layer attached to the outside of the plurality of unit bodies; the unit body includes the active material, and Kevlar fiber coated on the outside of the active material; Furthermore, there are multiple inflation tubes; the inflation tubes penetrate and connect the rear screen, the outer ends of the inflation tubes are connected to the front screen, the inner ends are connected to the cabin and are provided with inflation ports; the inflation ports are connected to the inflation device; The inflation tube is provided with an air outlet between the front screen and the rear screen, and between the rear screen and the cabin body.

[0013] Furthermore, two adjacent unit bodies are flexibly connected, and a woven structure is formed by interweaving the Kevlar fibers.

[0014] Furthermore, the metal material includes any one of aluminum, tungsten, tantalum, nickel, hafnium and zirconium, or a combination of at least two of them.

[0015] Furthermore, the MLI heat insulation layer is made of a composite of polyimide and aluminum; and the rear screen is made of Kevlar fiber.

[0016] Furthermore, the inflation tube is made of a laminated polyimide film and an aluminum film, and is formed by an epoxy resin bonding process.

[0017] Furthermore, the cabin body is made of self-repairing material, which is composed of two-component microcapsules of resin and curing agent embedded in an epoxy resin matrix.

[0018] Furthermore, after the active interlayer flexible protective screen is inflated and unfolded, the distance between the front screen and the rear screen is not less than 5 cm, and the distance between the rear screen and the cabin is not less than 5 cm.

[0019] The present invention achieves the following significant effects: (1) The present invention proposes a new method for preparing active materials, which solves the problem that traditional mechanical mixing methods cannot prepare THV-based active materials, simplifies the process, and improves production efficiency. The uniformity of the prepared materials is improved by heating and dissolving ethyl acetate in the reactor and heating in a water bath during the distillation process. At the same time, the active materials prepared by zero oxygen balance ratio can release chemical energy to the maximum extent, thereby improving energy density and reaction efficiency; (2) The stirring and dividing structure designed in the active material preparation device of the present invention has the following technical effects: first, under the cooperation of the rotating cylinder, a plurality of dividing plates are rotated to achieve a stirring effect; second, a plurality of dividing plates are placed together, which themselves have a dividing effect. Before hot pressing, there is no need to deliberately cut the solid mixture, which saves time and labor; (3) The present invention applies active materials to inflatable active sandwich flexible protective shields. The active materials release chemical energy during high-speed impacts, which further improves the protective capability of the shield. The explosion products generate reverse impulses on space debris, reducing the axial kinetic energy of space debris, and can block space debris or micro-meteorites of a certain size and speed. (4) The present invention uses self-repairing materials as the bulkhead material. This material can repair itself when slightly damaged, reducing maintenance and replacement costs and extending the service life of the spacecraft; (5) Compared with the traditional rigid protection structure, the flexible protection screen of the present invention occupies less volume and weight of the aircraft. At the same time, it is made of lightweight materials such as Kevlar fiber, active materials and MLI insulation layer. The whole system reduces the load of the aircraft while ensuring the protection effectiveness, which is conducive to improving the performance and flexibility of the aerospace pressure cabin; (6) The active interlayer flexible protective shield of the present invention has a flexible structure and can adapt to aerospace pressure chambers of different shapes and sizes. It can work in an environment of -100℃-150℃ and has strong environmental adaptability. BRIEF DESCRIPTION OF THE DRAWINGS

[0020] Figure 1 Schematic diagram of the structure of the active material preparation device.

[0021] Figure 2 This is a schematic diagram of the structure of the stirring and dividing structure of the active material preparation device.

[0022] Figure 3 Schematic diagram of the connection structure between the reactor and the water bath of the active material preparation device.

[0023] Figure 4 Schematic diagram of the deployment of the active interlayer flexible protective screen.

[0024] Figure 5 Schematic diagram of the composition of the front screen of the active interlayer flexible protective screen.

[0025] Figure 6 Schematic diagram of the active interlayer flexible protective screen in the folded state.

[0026] Figure 7 Schematic diagram of the protection effect of traditional inert shield against 10mm, 6km / s space debris.

[0027] Figure 8 Schematic diagram of the protective effect of the active interlayer flexible shield against 10mm, 6km / s space debris.

[0028] Fig. 9 This is a numerical simulation of the debris cloud resulting from a projectile impacting a traditional inert protective screen.

[0029] Fig.10 This is a numerical simulation diagram of the debris cloud obtained when a projectile hits an active interlayer flexible protective shield.

[0030] Among them, the figure markings are: 10, bracket; 20, lifting cylinder; 30, vertical column; 40, reactor; 50, water bath; 60, partition plate; 70, rotating cylinder; 80, vertical gear rod; 90, gear one; 100, gear two; 110, drive motor; 120, gear three; 130, transmission belt; 1, inflation port; 2, front screen; 3, rear screen; 4, inflation tube; 5, cabin; 51, piston plate; 6, active material; 7, Kevlar fiber; 8, MLI insulation layer. DETAILED DESCRIPTION

[0031] In order to more clearly illustrate the technical features of this solution, this solution is described below through specific implementation methods.

[0032] The present invention provides a method for preparing an active material, which specifically comprises the following steps: Step 1: dissolving THV particles; specifically, adding ethyl acetate and THV particles to the reaction kettle 40, the concentration of the THV solution is controlled at 0.1 g / ml, and the water bath is heated to 70-90° C., and the mixture is stirred continuously until the THV particles are completely dissolved; Step 2: Add metal powder; specifically, add metal powder according to the mass of THV monomer in a zero oxygen balance ratio, and stir to mix evenly, the stirring time is 30-60 minutes; The metal includes any one of aluminum, tungsten, tantalum, nickel, hafnium and zirconium or a combination of two or more thereof; The metal powder can be micron or nanometer in size; the preferred particle size range is 10-100nm; Zero oxygen balance means that the oxidant and the reductant are completely consumed in a chemical reaction and the reaction reaches a state of equilibrium. The main purpose of selecting the "zero oxygen balance ratio" is to ensure that the oxidant and the reductant react completely during the reaction, improve the reaction efficiency, and release chemical energy to the maximum extent, thereby increasing the energy density. In addition, it can reduce or eliminate by-products in the reaction. The above metals have better reducibility and can play a more important role in redox reactions, ensuring the maximum energy release during the reaction.

[0033] The zero oxygen balance ratio calculation method in the above preparation method is based on the chemical reaction equation of the reactants. Take the American 3M THV 220A model granules and metal aluminum as an example to illustrate the calculation process. The chemical reaction equation of aluminum and each THV monomer is: Tetrafluoroethylene (TFE): ; Hexafluoropropylene (HFP): ; Vinylidene fluoride (VDF): ; The American 3M THV 220A model granules, the THV monomer ratio is 45.8wt% TFE, 18.5wt% HFP, 35.7wt% VDF. Assuming that the total mass of THV220 is 100g, the masses of the three monomers are 45.8g, 18.5g, and 35.7g respectively. The masses of the three monomers are divided by their molar masses of 100g / mol, 150g / mol, and 64g / mol respectively, and the amounts of substances obtained are 0.458mol, 0.123mol, and 0.558mol respectively. The corresponding zero oxygen balance reaction equations are multiplied by the proportional coefficients 4 / 3, 2, and 2 / 3 to obtain the corresponding aluminum amount of substance, and then multiplied by the aluminum molar mass of 27g / mol, and the required aluminum masses are 16.49g, 19.98g, and 10.04g respectively, and the total mass is 46.51g. Thus, the mass ratio of aluminum and THV220 zero oxygen balance reaction is obtained to be 32%:68%. The same conclusion is: The mass ratio of zirconium and THV220 in the zero oxygen equilibrium reaction is 46%:54%; The mass ratio of nickel and THV220 in the zero oxygen equilibrium reaction is 52%:48%; The mass ratio of tantalum and THV220 in the zero oxygen equilibrium reaction is 57%:43%; The mass ratio of hafnium and THV220 in the zero oxygen equilibrium reaction is 62%:38%; The mass ratio of tungsten and THV220 in the zero oxygen equilibrium reaction is 69%:31%.

[0034] When different types of THV granules or multiple metals are selected, the mass ratio is calculated using this method.

[0035] Step 3: Solvent evaporation; Specifically, the water bath temperature is raised to 82°C, and a distillation device is installed for distillation. In order to keep the metal powder uniformly dispersed at all times, it is necessary to stir continuously during the distillation until the solvent is completely evaporated; Step 4: Extraction and drying; Specifically, after complete evaporation, a large solid mixture can be obtained, and the solid mixture is cut into small pieces of about 1-2 mm and placed in a drying oven for vacuum drying for 12 h; Step 5: hot pressing; specifically, the dried active material is loaded into a molding mold, the molding mold is placed in a drying oven, the drying oven temperature is heated to 160°C and kept warm for 30 minutes, and then the molding mold is taken out; or the dried material is loaded into a heating mold, the heating mold is heated to 120-160°C and kept warm for 30 minutes; preferably, the heating mold is directly used, and the heating temperature of the mold is 140°C, which is based on the material becoming a molten state; Finally, the forming mold or the heating mold is placed on a universal testing machine and pressurized to 15 MPa at a pressurization speed of 0.05 MPa / s, and the pressure is maintained for 30 minutes. After the pressurization is completed, the mold is de-molded after cooling to obtain the active material.

[0036] The present invention provides an active material preparation device for performing steps 1 to 4 of the active material preparation method described above, see Figure 1-Figure 3 , including a reactor 40, a water bath 50 sleeved on the outside of the reactor 40, a piston plate 51 slidably arranged in the reactor 40, a vertical column 30 whose top end is fixedly connected to the bottom surface of the piston plate 51 at a vertical rule, a lifting cylinder 20 fixedly connected to the bottom end of the vertical column 30, and a stirring and dividing structure arranged above the piston plate 51. The stirring and dividing structure and the water bath 50 are fixed on the bracket 10; the reactor 40 is a vertical cylinder with upper and lower ends connected.

[0037] The stirring and dividing structure includes a plurality of dividing plates 60 connected to each other and arranged in a circular array, a rotating cylinder 70 fixedly connected to the top ends of the plurality of dividing plates 60, a vertical gear rod 80 connected to the rotating cylinder 70 at the bottom end, gear two 100 and gear three 120 respectively arranged on both sides of the upper end of the vertical gear rod 80, gear one 90 meshingly connected to the outer side of gear two 100, a transmission belt 130 coaxially connected to gear one 90 and gear three 120 at both ends respectively, and a drive motor 110 coaxially connected to gear three 120.

[0038] In actual operation, water is added to the water bath 50, and a heater is provided on the water bath 50. When executing steps 1 to 4, the water is heated to a suitable temperature according to the execution degree of the corresponding steps; materials are added to the reactor 40, and stirred by the stirring and dividing structure, that is, the rotating cylinder 70 drives the plurality of dividing plates 60 to rotate, and the materials are received above the piston plate 51; after the evaporation process is completed, the large solid mixture is naturally divided into multiple portions due to the provision of the dividing plates 60, so that the cutting process in the original step 4 is naturally omitted, saving manpower and cost; Under the action of the lifting cylinder 20 and the rotation of gear two 100 and gear three 120, the vertical gear rod 80 drives the rotating cylinder 70 and multiple dividing plates 60 below to rise synchronously, so that the piston plate 51 is pushed out of the reactor 40 by the lifting cylinder 20, and the subsequent vacuum drying process is carried out.

[0039] It should be noted that there is no limitation on the arrangement of the plurality of partition plates 60 , and the topological structure of the plurality of partition plates 60 can be adjusted according to the required material shape.

[0040] The present invention provides an active material, which is prepared by the above preparation method, and the components and mass fractions of the active material are determined by the selected THV monomer mass and the metal material in a zero oxygen balance ratio.

[0041] The present invention provides the application of active materials in aerospace pressure cabin protection screens. The active sandwich flexible protection screen made of the active material occupies a small volume and weight of the aerospace pressure cabin, and can cooperate with the working process of the cabin to realize the deployment protection function. At the same time, the THV-based active material is applied to the protection screen, and the high-temperature, high-pressure, and high-speed movement of the detonation products at the moment of explosion will generate a reverse impulse to the projectile, further reducing the axial kinetic energy of space debris and improving the protection performance. In this way, the activation and flexibility of the protection structure are realized at the same time, meeting the application requirements for the protection of space debris and micrometeorites.

[0042] The present invention provides an active sandwich flexible protective screen, such as Figure 4-6 As shown, it includes a front screen 2, a rear screen 3 and an inflation tube 4.

[0043] The front screen 2 plays the role of differentiating energy distribution and causing recoil to debris and micro-meteorites. The front screen 2 includes a plurality of unit bodies connected in sequence, and an MLI heat insulation layer 8 is added outside the plurality of unit bodies, and the MLI heat insulation layer is the outermost layer; the unit body is made of Kevlar fiber 7 coated with active material 6; two adjacent unit bodies are flexibly connected, and a woven structure is formed by interweaving Kevlar fiber 7. The MLI heat insulation layer 8 is made of a composite of polyimide and aluminum.

[0044] The rear screen 3 provides a blocking protection function and is made of Kevlar fiber 7 .

[0045] Preferably, the front screen 2 is composed of Kevlar fiber 7 covering active material 6 and MLI thermal insulation layer 8, the thickness of Kevlar fiber 7 is 0.05mm, the thickness of active material 6 interlayer is 2.2mm, and the thickness of MLI thermal insulation layer 8 is 0.2mm. The rear screen 3 is composed of Kevlar fiber 7, and its thickness is 2mm.

[0046] The inflation tube 4 penetrates and connects the rear screen 3, the outer end is connected to the front screen 2, the inner end is connected to the cabin 5 and is provided with an inflation port 1; the inflation tube 4 is provided with an air outlet between the front screen 2 and the rear screen 3, and between the rear screen 3 and the cabin 5. After inflation, the inflation tube 4 causes both the front screen 2 and the rear screen 3 to unfold.

[0047] Preferably, there are six inflation tubes 4, which are arranged symmetrically according to the center line of the cabin 5; the inflation tubes 4 fix the spatial positions of the front screen 2 and the rear screen 3, and are fixedly connected to the cabin 5 to ensure the distance between the front screen 2 and the rear screen 3 and the positional relationship with the cabin 5; the two inflation tubes 4 arranged on the transverse center line are provided with air outlets between the front screen 2 and the rear screen 3, and between the rear screen 3 and the cabin 5.

[0048] The inflatable tube 4 is made of a laminated structure of polyimide and aluminum film, with polyimide film on both sides and aluminum film in the middle, and is formed by epoxy resin bonding process; it has the functions of folding, unfolding and rigidification. When the yield point of the aluminum film is reached under the action of external force, the polyimide film and the aluminum film will be strengthened, and the rigidity will be enhanced to a certain extent. At the same time, this material has good environmental adaptability and is suitable for use in space environments. The inflatable tube 4 has its own creases to facilitate folding before unfolding.

[0049] The inflation port 1 of the inflation tube 4 is connected to the inflation device; the inflation device is composed of a gas cylinder, a valve and a pipeline, and is responsible for the inflation and expansion function, and provides the initial power required for the rigidification of the inflation tube 4. The inflation device adopts a drop pressure scheme, and controls the instantaneous flow of the gas through a small hole flow limiting method, and the working medium is nitrogen. The overall inflation device includes a gas cylinder, an electric explosion valve, an inflation valve, and a flow controller.

[0050] The cabin 5 is made of self-repairing material, which is composed of two-component microcapsules of resin and curing agent embedded in an epoxy resin matrix. When the cabin is slightly damaged, the capsules rupture, and the strong resin therein overflows and combines with the catalyst to solidify and harden.

[0051] Working process: The active interlayer flexible protective screen is wrapped around the outside of the cabin 5 and is in a packaged state during the launch phase. After entering orbit and reaching the predetermined point, the device is unlocked, and the inflation device inflates the flexible inflation tube 4, which unfolds and simultaneously unfolds and supports the front screen 2 and rear screen 3 of the protective screen to the predetermined position. The inflation tube 4 is then rigidified to keep the entire structure at a certain rigidity, thereby achieving a working protection state. After inflation and expansion, the distance between the front screen 2 and the rear screen 3 is not less than 5 cm, and the distance between the rear screen 3 and the cabin 5 is not less than 5 cm. The device is used to intercept and protect the cabin 5 from space debris and micrometeors, ensuring the structural safety of the cabin 5.

[0052] The active interlayer flexible protective screen can work in an environment of -100℃-150℃ and can block space debris or micrometeorites of a certain size and speed.

[0053] The protection effect of traditional inert shield against 10mm, 6km / s space debris is as follows: Figure 7 shown.

[0054] The protective effect of the active sandwich flexible shield against 10mm, 6km / s space debris is as follows Figure 8 shown.

[0055] Numerical simulation of the debris cloud generated by the projectile impacting the traditional inert protection screen is shown in the figure below. Fig. 9 shown.

[0056] Numerical simulation of the debris cloud resulting from the impact of the projectile on the active sandwich flexible protective screen Fig.10 shown.

[0057] By comparison, it can be seen that the traditional inert protection screen cannot effectively protect against space debris of 10mm and 6km / s, resulting in perforation of the cabin wall. The active interlayer flexible protection screen can effectively protect against space debris of 10mm and 6km / s without causing obvious damage. At the same time, the impact area of ​​the debris cloud generated by the active interlayer flexible protection screen is significantly larger than the impact area of ​​the debris cloud generated by the inert protection screen. When the energy of the debris cloud is constant, the larger the impact area, the more dispersed the kinetic energy of the debris cloud, the smaller the density of the collision energy flux acting on the cabin wall of the aerospace pressure cabin, and the damage and destructive effect on the cabin wall is reduced accordingly. As a result, the cabin wall under the protection of the inert protection screen has obvious perforation deformation, while the cabin wall under the protection of the active interlayer flexible protection screen has no obvious damage.

[0058] Technical features not described in the present invention can be achieved through or by adopting existing technologies and will not be described in detail here. Of course, the above description is not a limitation of the present invention, and the present invention is not limited to the above examples. Changes, modifications, additions or substitutions made by ordinary technicians in this technical field within the essential scope of the present invention should also fall within the scope of protection of the present invention.

Claims

1. A method for preparing an active material, characterized in that: The steps include: Step 1: dissolving THV particles; specifically, adding ethyl acetate and THV particles into a reaction kettle, controlling the concentration of THV solution at 0.1 g / ml, heating in a water bath to 70-90° C., stirring continuously during the process, until the THV particles are completely dissolved; Step 2: Add metal powder; specifically, add metal powder according to the mass of THV monomer in a zero oxygen balance ratio, and stir to mix evenly, the stirring time is 30-60 minutes; Step 3: Solvent evaporation; Specifically, the water bath temperature is raised to 82°C, and a distillation device is installed for distillation. In order to keep the metal powder uniformly dispersed at all times, it is necessary to stir continuously during the distillation until the solvent is completely evaporated; Step 4: Extraction and drying; specifically, after complete evaporation, a large solid mixture is obtained, and the solid mixture is cut into small pieces of 1-2 mm and placed in a drying oven for vacuum drying for 12 h; Step 5: hot pressing; specifically, the dried material is loaded into a molding mold, the molding mold is placed in a drying oven, the drying oven temperature is heated to 160°C and kept warm for 30 minutes, and then the molding mold is taken out; or the dried material is loaded into a heating mold, the heating mold is heated to 120-160°C and kept warm for 30 minutes; finally, the molding mold or the heating mold is placed on a universal testing machine and pressurized to 15MPa at a pressurization speed of 0.05MPa / s, and the pressure is maintained for 30 minutes. After the pressurization is completed, the mold is removed after cooling to obtain the active material.

2. The method for preparing an active material according to claim 1, characterized in that: The metal includes any one of aluminum, tungsten, tantalum, nickel, hafnium and zirconium, or a combination of two or more thereof.

3. A device for preparing active materials, characterized in that: The preparation device is used to implement steps 1 to 4 of the preparation method according to claim 1 or 2, including a reactor, a water bath mounted on the outside of the reactor, a piston plate slidably arranged in the reactor, a vertical column with a top fixedly connected to the bottom of the piston plate, a lifting cylinder fixedly connected to the bottom of the vertical column, and a stirring and dividing structure arranged above the piston plate, wherein the stirring and dividing structure and the water bath are fixed on a bracket; the reactor is vertically cylindrical and connected at both ends.

4. The active material preparation device according to claim 3, characterized in that: The stirring and dividing structure includes a plurality of dividing plates connected to each other and arranged in a circular array, a rotating cylinder fixedly connected to the top ends of the plurality of dividing plates, a vertical gear rod connected to the rotating cylinder at the bottom end, gear 2 and gear 3 respectively arranged on both sides of the upper end of the gear rod, gear 1 meshingly connected to the outer side of gear 2, a transmission belt coaxially connected to gear 1 and gear 3 at both ends respectively, and a driving motor coaxially connected to gear 3.

5. An active material, characterized in that Prepared according to the preparation method of claim 1 or 2.

6. Use of the active material according to claim 5 in a protective shield for aerospace pressure chambers.

7. An active interlayer flexible protective screen, characterized in that: Made of the active material according to claim 5, the active sandwich flexible protective screen comprises a front screen, a rear screen and an inflatable tube; The front screen includes a plurality of unit bodies connected in sequence, and an MLI heat insulation layer attached to the outer sides of the plurality of unit bodies; the unit bodies include the active material, and Kevlar fibers coated on the outer sides of the active material.

8. The active sandwich flexible protective screen according to claim 7, characterized in that: There are multiple inflation tubes; the inflation tubes penetrate and connect the rear screen, the outer ends of the inflation tubes are connected to the front screen, the inner ends are connected to the cabin and are provided with inflation ports; the inflation ports are connected to the inflation device; The inflation tube is provided with an air outlet between the front screen and the rear screen, and between the rear screen and the cabin body.

9. The active sandwich flexible protective screen according to claim 7, characterized in that: Two adjacent unit bodies are flexibly connected, and a woven structure is formed by interweaving the Kevlar fibers.

10. The active sandwich flexible protective screen according to claim 7, characterized in that: The MLI heat insulation layer is made of a composite of polyimide and aluminum; the rear screen is made of Kevlar fiber; the inflatable tube is made of a laminated polyimide film and an aluminum film, and is formed by an epoxy resin bonding process.