Flexible dissolved oxygen sensor and preparation method thereof
By integrating dissolved oxygen and temperature sensors on a flexible substrate and preparing using magnetron sputtering and dispensing inkjet processes, the existing dissolved oxygen sensors have been solved, and high-performance and low-cost dissolution are achieved Oxygen measurement and temperature compensation are suitable for a variety of scenarios.
Patent Information
- Application Number
- CN202411048898.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-01
- Publication Date
- 2024-11-19
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The existing dissolved oxygen sensors are costly, large in size, and have limited application scenarios. They need to be used in combination with temperature sensors for compensation and correction, which is cumbersome in operation.
The integrated dissolved oxygen sensor and temperature sensor are on a flexible substrate and prepared by magnetron sputtering and dispensing inkjet processes, achieving a flexible, low-cost dissolved oxygen sensor with temperature compensation capabilities and is suitable for a variety of application scenarios.
It provides a flexible dissolved oxygen intelligent sensor that is high-performance, low-cost, suitable for quantitative production, overcomes the problems of large size and limited application scenarios of traditional sensors, and simplifies operation, realizing the simultaneous measurement and regulation of dissolved oxygen and temperature.
Smart Images

Figure CN118980728A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of sensors, and in particular to a flexible dissolved oxygen sensor and a preparation method thereof. Background Art
[0002] Dissolved oxygen level is one of the key indicators for evaluating water quality. Real-time monitoring and effective regulation of dissolved oxygen are of vital importance to ensuring the economy of aquaculture and the quality of aquatic products. Traditional dissolved oxygen sensors are expensive, have high maintenance costs, and have hard shells, large volumes, and single usage scenarios. The emergence of new application scenarios has put forward broader demands and higher requirements for dissolved oxygen measurement. For example, in aquaculture, accurate research on the habits of farmed fish requires dissolved oxygen sensors with better fit to reflect the tendency of fish activities to dissolved oxygen concentration. At the same time, according to the range of fish activities, the distribution of dissolved oxygen in the breeding environment can be understood in order to carry out targeted oxygenation, as well as to monitor the dissolved oxygen on the inner wall of the pipes of the breeding facilities to better guide scientific fertilization and fit underwater soft robots for water quality monitoring. These scenarios put forward requirements for dissolved oxygen sensors such as small size, light weight, and bendability.
[0003] Although the prior art has disclosed a variety of micro sensors, the research on flexible dissolved oxygen sensors for dissolved oxygen measurement is still in the prototype development stage, and there are problems such as high manufacturing cost, complex process, and limited application scenarios (mostly used in the biomedical field).
[0004] In addition, when measuring dissolved oxygen in water, temperature is the main parameter that affects dissolved oxygen measurement. As the temperature rises, the saturated dissolved oxygen content in the water will decrease, and the electrochemical reaction will become more intense. At this time, only a dissolved oxygen sensor is used for measurement, and the parameters obtained are single. Therefore, when using a dissolved oxygen sensor for measurement, it is also necessary to use a temperature sensor for compensation and correction, which makes the test cumbersome and inconvenient to operate. Summary of the invention
[0005] In view of the deficiencies in the above-mentioned prior art, the present invention provides a flexible dissolved oxygen sensor and a preparation method thereof, aiming to provide a high-performance, low-cost, suitable for quantitative production, flexible micro-volume, with compensation capability, and application-proven flexible dissolved oxygen intelligent sensor, which has the characteristics of simple production process, low cost and temperature compensation, is suitable for a variety of application scenarios, has the advantages of flexibility and bendability, and overcomes the defects of traditional sensors with large volume and limited application scenarios, and at the same time overcomes the technical defect of needing to be used in conjunction with a temperature sensor for compensation and correction.
[0006] To achieve the above object, the technical solution of the present invention is as follows:
[0007] The present invention integrates a dissolved oxygen sensor and a temperature sensor on a flexible substrate to obtain a flexible dissolved oxygen sensor. While measuring dissolved oxygen, the temperature of aquaculture waters can be measured, thereby facilitating regulation of the water body according to the dissolved oxygen content and temperature.
[0008] A flexible dissolved oxygen sensor comprises a dissolved oxygen sensor and a temperature sensor, which are respectively arranged on both sides or on the same side of a flexible substrate. The temperature sensor is used to assist the dissolved oxygen sensor in measuring the dissolved oxygen concentration in water.
[0009] Preferably, the dissolved oxygen sensor comprises an electrode assembly and an electrolyte, the electrode assembly comprises a working electrode, a reference electrode and an auxiliary electrode, the working electrode is located between the reference electrode and the auxiliary electrode, the electrode assembly is also covered with an oxygen permeable membrane, the electrolyte is located between the oxygen permeable membrane and the electrode assembly, oxygen permeates through the oxygen permeable membrane, and the dissolved oxygen is measured;
[0010] The working electrode, the reference electrode and the auxiliary electrode are electrically connected to electrode pins I respectively.
[0011] Preferably, the working electrode and the auxiliary electrode are both noble metal electrodes, and the reference electrode is an Ag / AgCl electrode.
[0012] Preferably, the noble metal electrode is an Au electrode or a Pt electrode.
[0013] Preferably, the working electrode is a circular electrode, and the auxiliary electrode surrounds the working electrode in a concentric arc manner.
[0014] Preferably, the ratio of the diameter of the working electrode, the arc width of the auxiliary electrode, and the distance between the working electrode and the auxiliary electrode is 4:2:1, ensuring that the areas of the auxiliary electrode and the working electrode are large enough and the distance between the auxiliary electrode and the working electrode is close.
[0015] Preferably, the temperature sensor comprises a temperature sensitive layer electrode and an electrode pin II, the two electrode pins II are electrically connected to the head end and the tail end of the temperature sensitive layer electrode respectively, and the temperature sensitive layer electrode is a temperature sensitive conductive electrode.
[0016] Preferably, the electrode material of the temperature-sensitive conductive electrode is selected from conductive polymers, carbon-based materials or conductive metal nano-inks.
[0017] Preferably, the temperature sensitive layer electrode is composed of a plurality of sensing lines arranged in a zigzag grid structure, two adjacent sensing lines do not abut, the width of the sensing line is 0.25 mm, and the spacing between the sensing lines is 3-6 mm, ensuring that the lines do not overlap and the spacing is not too large.
[0018] The present invention also protects a method for preparing the above-mentioned flexible dissolved oxygen sensor, comprising the following steps:
[0019] The flexible substrate is cleaned to obtain a treated substrate;
[0020] After depositing two electrode pins II on one side of the processing substrate by magnetron sputtering, the temperature sensitive layer electrode is deposited on the processing substrate, and the head end and the tail end of the temperature sensitive layer electrode are respectively connected to the electrode pin II;
[0021] Depositing a working electrode and an auxiliary electrode on the other side of the treated substrate by magnetron sputtering, and then dispensing a Ag electrode so that the working electrode is located between the auxiliary electrode and the Ag electrode, and then chlorinating the Ag electrode in an HCl electrolyte using a three-electrode system to obtain an AgCl electrode;
[0022] The chlorination method is as follows: a commercial Ag / AgCl electrode is used as a reference electrode, an Ag electrode is used as a working electrode, and a platinum electrode is used as an auxiliary electrode to form a three-electrode system, which are placed together in a 0.1 mol / L HCl solution, and a constant potential scan is performed using an electrochemical workstation, and the Ag electrode is chlorinated to form an Ag / AgCl electrode;
[0023] The electrode assembly is covered with an oxygen permeable membrane, and the electrolyte is filled between the electrode assembly and the oxygen permeable membrane.
[0024] Preferably, when the dissolved oxygen sensor and the temperature sensor are disposed on the same side of the flexible substrate, the temperature sensitive layer electrode is electrically connected to the electrode pin I.
[0025] The present invention also protects a method for preparing the above-mentioned flexible dissolved oxygen sensor, comprising the following steps:
[0026] The flexible substrate is cleaned to obtain a treated substrate;
[0027] After depositing the electrode pin I on one side of the processing substrate by magnetron sputtering, depositing the temperature sensitive layer electrode on the processing substrate between any two of the electrode pins I, and connecting the head end and the tail end of the temperature sensitive layer electrode to the electrode pin I respectively, to obtain a temperature sensor;
[0028] A working electrode and an auxiliary electrode are deposited on the temperature sensor by magnetron sputtering, and then a Ag electrode is prepared by dispensing glue, and the working electrode is located between the auxiliary electrode and the Ag electrode, and then the Ag electrode is chlorinated in a HCl electrolyte using a three-electrode system to obtain an AgCl electrode;
[0029] The electrode assembly is covered with an oxygen permeable membrane, and the electrolyte is filled between the electrode assembly and the oxygen permeable membrane.
[0030] Compared with the prior art, the present invention has the following beneficial effects:
[0031] 1. In the preparation process of the flexible sensor, the present invention adopts a magnetron sputtering process and a dispensing inkjet process. The magnetron sputtering process has the advantages of fast deposition rate, low deposition temperature, large coating area, good uniformity, and strong film-base bonding. In addition, the process is environmentally friendly and pollution-free, easy to control, and has low requirements for the substrate, and can be used for industrial-scale production. The dispensing inkjet process has the advantages of precise control, material saving, and improved production efficiency and accuracy. Both processes have good comprehensive performance. The most important thing is that both methods are suitable for flexible substrates, which can not only obtain dissolved oxygen sensors and temperature sensors on flexible substrates, but also ensure the structural integrity of the flexible substrate.
[0032] 2. The dissolved oxygen sensor of the present invention adopts a polarographic three-electrode structure. The reaction principle of the dissolved oxygen sensor is as follows: Figure 1 As shown, the dissolved oxygen sensor uses precious metals as working electrodes and auxiliary electrodes, Ag / AgCl electrodes as reference electrodes, and uses an oxygen-permeable membrane to encapsulate KCl electrolyte and electrode components. The advantages of the three-electrode structure over the two-electrode structure are: after adding the reference electrode, the reference electrode is used to maintain a constant polarization voltage on the one hand, improving the accuracy and stability of the measurement; on the other hand, it changes the reaction principle in dissolved oxygen detection, making up for the problem of auxiliary electrode and electrolyte consumption, and enhancing the life of the flexible dissolved oxygen sensor. In addition, the reaction no longer consumes oxygen in the solution to be tested, making the measurement result more accurate. The reaction principle is as follows:
[0033] Working electrode: O2+2H + +2e - →H2O2 (1)
[0034] H2O2+2H + +2e - →2H2O (2)
[0035] Auxiliary electrode: 2H2O→O2+4H + +4e - (3)
[0036] In the process of polarographic dissolved oxygen detection, it is necessary to apply polarization voltage to the flexible dissolved oxygen sensor electrode to induce oxygen reduction reaction of dissolved oxygen on the electrode surface, and detect the dissolved oxygen concentration by the magnitude of the reaction current. Specifically, the applied voltage will form a potential difference on the surface of the flexible dissolved oxygen sensor electrode, which will reduce the electron energy level on the electrode surface. When oxygen molecules approach the electrode surface, they will capture electrons on the electrode surface and undergo a reduction reaction. The flow of electrons during the reaction forms a current, and the concentration of dissolved oxygen is determined by measuring the magnitude of the current signal.
[0037] 3. In the embodiment of the present invention, poly(3,4-ethylenedioxythiophene)-polystyrene sulfonic acid is used as the electrode material of the temperature-sensitive conductive electrode. Poly(3,4-ethylenedioxythiophene)-polystyrene sulfonic acid is a conductive polymer with unique electrical properties, good flexibility and wear resistance, and stronger fatigue resistance than similar metal products. In addition, due to its special electronic structure and molecular orbital characteristics, it also exhibits high conductivity like metal. The temperature sensor in the present invention adopts the resistive principle, that is, the resistance of the temperature sensor changes linearly with temperature. BRIEF DESCRIPTION OF THE DRAWINGS
[0038] Figure 1 This is the reaction principle diagram of the dissolved oxygen sensor;
[0039] Figure 2 The figure is a flow chart of the preparation of the flexible dissolved oxygen sensor;
[0040] Figure 3 In the figure, the left picture is a top view of the electrode assembly of the dissolved oxygen sensor, and the right picture is a top view of the electrode of the temperature sensor;
[0041] Figure 4 is a relationship diagram between the dissolved oxygen concentration obtained by using the flexible dissolved oxygen sensor of Example 1 of the present invention and the current collected by the flexible dissolved oxygen sensor at different temperatures;
[0042] Figure 5 This is a fitting curve diagram showing the change of the response slope with temperature obtained by using the flexible dissolved oxygen sensor of Example 1 of the present invention.
[0043] Description of reference numerals:
[0044] 1. Flexible substrate; 2. Working electrode; 3. Reference electrode; 4. Auxiliary electrode; 5. Oxygen permeable membrane; 6. Temperature sensitive layer electrode. DETAILED DESCRIPTION
[0045] The specific embodiments of the present invention are described in detail below, but it should be understood that the protection scope of the present invention is not limited by the specific embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work belong to the protection scope of the present invention. The experimental methods described in the embodiments of the present invention are conventional methods unless otherwise specified.
[0046] The flexible dissolved oxygen sensor of the present invention adopts a planar electrode structure. On this basis, in order to ensure that a good circuit is formed between the working electrode and the auxiliary electrode and the sensor exhibits better sensitivity, the dissolved oxygen sensor adopts a planar layout design in which the working electrode is located between the reference electrode and the auxiliary electrode, and the auxiliary electrode surrounds the working electrode. The layout design of the planar electrode is vertically encapsulated by an oxygen permeable membrane, and the electrolyte is encapsulated between the planar electrode and the oxygen permeable membrane.
[0047] The edges of the broken lines may cause the edge effect of charge tip discharge due to the electric field concentration effect and the large change of local current density. Therefore, the edges of the dissolved oxygen electrode reaction area are designed with arcs to reduce the change and unevenness of local current density. Based on the layout design, the shape of the working electrode is circular (with a diameter of 1.5 mm), and the auxiliary electrode surrounds the working electrode in a concentric arc manner.
[0048] In addition, in order to increase the contact area between the electrode sensing structure and the measurement environment under limited electrode area and accurately reflect the actual temperature of the environment, the temperature sensor electrode adopts a zigzag grid structure.
[0049] The technical solution of the present invention is further explained by using embodiments below, which are specifically as follows:
[0050] Example 1
[0051] A method for preparing a flexible dissolved oxygen sensor comprises the following steps:
[0052] S1. Material pretreatment: tear off the protective film on one side of the polyimide film, repeatedly soak the polyimide film with ethanol to remove the oily organic molecules attached thereto, then place it in an ultrasonic cleaner and perform ultrasonic treatment at 80W power for 10 minutes to remove small water-soluble impurities, then rinse it with deionized water, blow dry the surface with nitrogen, and finally place it in a UV light cleaner for cleaning for 5 minutes to obtain a treated flexible substrate 1;
[0053] S2, magnetron sputtering: a gold electrode pin II7 of the temperature sensor is manufactured on the flexible substrate 1 by using a magnetron sputtering instrument, the current of the magnetron sputtering instrument is set to 40 mA, the time is set to 120 s, and the dispensing function of the microelectronic printer is used to dispense poly(3,4-ethylenedioxythiophene)-polystyrene sulfonic acid temperature-sensitive ink according to the designed pattern to prepare a temperature-sensitive layer electrode, and the excess organic solvent is removed by sintering at 120°C for 30 min to form a dense conductive layer. At this time, the head and the end of the poly(3,4-ethylenedioxythiophene)-polystyrene sulfonic acid are respectively connected to the gold electrode pin II7, and finally the PDMS mixed solution with bubbles removed is evenly scraped on the conductive area, the mass ratio of the PDMS main agent to the PDMS curing agent in the PDMS mixed solution is 10:1, and after the scraping is completed, it is heated at 60°C for 40 min to complete the preparation of the temperature sensor. The temperature sensor electrode adopts a zigzag grid structure, the width of the sensing line is 0.25 mm, and the electrode grid spacing is 4 mm;
[0054] S3. According to the designed electrode pattern, a mask is engraved by a laser engraving machine and is closely attached to the other side of the flexible substrate 1. Then, the mask is placed in a magnetron sputtering apparatus and a working electrode 2 and an auxiliary electrode 4 are deposited by magnetron sputtering. Both the working electrode 2 and the auxiliary electrode 4 are gold electrodes, and both the working electrode 2 and the auxiliary electrode 4 are connected to the gold electrode pin 18.
[0055] S4. Dispensing to make silver electrodes: The dispensing function of the microelectronic printer is used to prepare the silver electrodes. The dispensing needle is a 27G needle with a needle model of 210μm inner diameter, 200μm dispensing height, 80Kpa dispensing pressure, and 2mm / s dispensing speed. With this parameter, the dispensing line thickness is uniform, there is no redundant mixing at the start and end parts, the corners are clear, and the dispensing quality is high. After the silver paste is patterned, it needs to be sintered and solidified. At this time, the flexible substrate 1 is placed in a heating box and sintered at 150°C for 30 minutes to obtain a silver electrode;
[0056] S5. Fix the electrode shape: Use an electronic balance to weigh 10g of PDMS main agent and 1g of PDMS special curing agent, and mix them in a beaker. Use a glass rod to stir thoroughly until dense and uniform bubbles appear in the mixed liquid. Then place the beaker in a vacuum drying oven, set the vacuum degree to 0.9, and extract for 10 minutes. Extract until there are no obvious bubbles in the liquid. Take out the above PDMS mixed solution, scrape it on the conductive areas of the working electrode 2, the auxiliary electrode 4 and the silver electrode, and leave the reaction areas of the working electrode 2, the auxiliary electrode 4 and the silver electrode. Then place the flexible substrate 1 in a vacuum drying oven, set the extraction vacuum degree to 0.9, the heating temperature to 60°C, and the heating time to 40 minutes for curing and shaping.
[0057] S6, electrochemical deposition of AgCl: concentrated hydrochloric acid solution is prepared into a 0.1 mol / L HCl solution, the Ag electrode prepared in step S4 is used as the working electrode, the platinum electrode is used as the auxiliary electrode, and the commercial Ag / AgCl electrode is used as the reference electrode, and they are placed together in a 0.1 mol / L HCl solution, and the current time method (Amperometric it Curve, referred to as it) in the electrochemical workstation is used to perform a constant potential scan for 180 s at 200 mV, and the Ag electrode is chlorinated to form an Ag / AgCl electrode, at which time the working electrode 2, the auxiliary electrode 4 and the Ag / AgCl electrode form an electrode assembly of three electrodes, and the working electrode 2 is located between the Ag / AgCl electrode and the auxiliary electrode 4, and the Ag / AgCl electrode is designed to surround the working electrode 2 in a plane layout, and the ratio of the working electrode diameter, the auxiliary electrode arc width, and the distance between the working electrode and the auxiliary electrode is 4:2:1;
[0058] S7. Electrode packaging: Use a pipette to take 30 μL of 0.1 mol / L KCl solution and drop-cast it on the electrode assembly. Cut the oxygen permeable membrane and stick it to the surface of the KCl solution. After the solution is self-sticking under tension and there are no bubbles, use a micro-syringe to attach silicone to the contact edge of the oxygen permeable membrane and the flexible substrate. Finally, place the flexible substrate 1 in a vacuum drying oven and heat it at 45°C for 5 minutes to solidify the colloid and enhance the mechanical properties of the sensor. The sensor packaging is completed to obtain a flexible dissolved oxygen sensor.
[0059] Example 2
[0060] A method for preparing a flexible dissolved oxygen sensor comprises the following steps:
[0061] S1. Material pretreatment: tear off the protective film on one side of the polyimide film, repeatedly soak the polyimide film with ethanol to remove the oily organic molecules attached thereto, then place it in an ultrasonic cleaning machine, and ultrasonically treat it at a power of 100W for 5 minutes to remove small water-soluble impurities, then rinse it with deionized water, blow dry the surface with nitrogen, and finally place it in a UV light cleaning machine for 10 minutes to obtain a treated flexible substrate 1;
[0062] S2, magnetron sputtering: a gold electrode pin I8 is manufactured on the flexible substrate 1 by using a magnetron sputtering instrument, the current of the magnetron sputtering instrument is set to 30 mA, the time is set to 150 s, and the dispensing function of the microelectronic printer is used to dispense poly(3,4-ethylenedioxythiophene)-polystyrene sulfonic acid temperature-sensitive ink according to the designed pattern to prepare a temperature-sensitive layer electrode, and the excess organic solvent is removed by sintering at 100°C for 50 min to form a dense conductive layer. At this time, the head and the end of the poly(3,4-ethylenedioxythiophene)-polystyrene sulfonic acid are respectively connected to the gold electrode pin I8, and finally the PDMS mixed solution with bubbles removed is evenly scraped on the conductive area, the mass ratio of the PDMS main agent to the PDMS curing agent in the PDMS mixed solution is 10:1, and after the scraping is completed, it is heated at 80°C for 30 min to complete the preparation of the temperature sensor. The temperature sensor electrode adopts a zigzag grid structure, the width of the sensing line is 0.25 mm, and the electrode grid spacing is 3 mm;
[0063] S3. According to the designed electrode pattern, a mask is engraved by a laser engraving machine and is closely attached to the same surface of the flexible substrate 1. Then, the mask is placed in a magnetron sputtering apparatus and a working electrode 2 and an auxiliary electrode 4 are deposited by a magnetron sputtering method. Both the working electrode 2 and the auxiliary electrode 4 are platinum electrodes.
[0064] S4. Dispensing to make silver electrodes: The dispensing function of the microelectronic printer is used to prepare the silver electrodes. The dispensing needle is a 27G needle with a needle model of 210μm inner diameter, 200μm dispensing height, 100Kpa dispensing pressure, and 1.5mm / s dispensing speed. With this parameter, the dispensing line thickness is uniform, there is no redundant mixing at the beginning and end parts, the corners are clear, and the dispensing quality is high. After the silver paste is patterned, it needs to be sintered and solidified. At this time, the flexible substrate 1 is placed in a heating box and sintered at 120°C for 50min to obtain a silver electrode;
[0065] S5. Fix the electrode shape: Use an electronic balance to weigh 10g of PDMS main agent and 1g of PDMS special curing agent, and mix them in a beaker. Use a glass rod to stir thoroughly until dense and uniform bubbles appear in the mixed liquid. Then place the beaker in a vacuum drying oven, set the vacuum degree to 1.0, and extract for 8 minutes. Extract until there are no obvious bubbles in the liquid. Take out the above PDMS mixed solution, scrape it on the conductive areas of the working electrode 2, the auxiliary electrode 4 and the silver electrode, and leave the reaction areas of the working electrode 2, the auxiliary electrode 4 and the silver electrode. Then place the flexible substrate 1 in a vacuum drying oven, set the extraction vacuum degree to 1.0, the heating temperature to 80°C, and the heating time to 30 minutes for curing and shaping.
[0066] S6, electrochemical deposition of AgCl: concentrated hydrochloric acid solution is prepared into a 0.1 mol / L HCl solution, the Ag electrode prepared in step S4 is used as the working electrode, the platinum electrode is used as the auxiliary electrode, and the commercial Ag / AgCl electrode is used as the reference electrode, and they are placed together in a 0.1 mol / L HCl solution, and the current time method (Amperometric it Curve, referred to as it) in the electrochemical workstation is used to perform a constant potential scan for 180 s at 200 mV, and the Ag electrode is chlorinated to form an Ag / AgCl electrode, at which time the working electrode 2, the auxiliary electrode 4 and the Ag / AgCl electrode form an electrode assembly of three electrodes, and the working electrode 2 is located between the Ag / AgCl electrode and the auxiliary electrode 4, and the Ag / AgCl electrode is designed to surround the working electrode 2 in a plane layout, and the ratio of the working electrode diameter, the auxiliary electrode arc width, and the distance between the working electrode and the auxiliary electrode is 4:2:1;
[0067] S7. Electrode packaging: Use a pipette to take 40 μL of 0.1 mol / L KCl solution and drop-cast it on the electrode assembly. Cut the oxygen permeable membrane and fit it on the surface of the KCl solution. After the solution is self-fitted under tension and there are no bubbles, use a micro-syringe to attach silicone to the contact edge of the oxygen permeable membrane and the flexible substrate. Finally, place the flexible substrate 1 in a vacuum drying oven and heat it at 40°C for 10 minutes to solidify the colloid and enhance the mechanical properties of the sensor. The sensor packaging is completed to obtain a flexible dissolved oxygen sensor.
[0068] S8. Making an adhesion layer: Use the scraping function of a microelectronic printer to scrape an adsorbent PDMS mixture (made as in S5) on the other side of the base material and heat it to set it. This side of the sensor is used to adsorb on the surface of a robot dolphin, underwater robot, etc. to measure dissolved oxygen.
[0069] The following temperature compensation experiment is conducted using the flexible dissolved oxygen sensor of Example 1 of the present invention. The experimental method and results are as follows:
[0070] Method of temperature compensation experiment: Temperature is the main parameter that affects dissolved oxygen measurement. As the temperature rises, the saturated dissolved oxygen content in the water will decrease, and the electrochemical reaction will become more intense, so compensation testing is required through experiments. The dissolved oxygen sensor is used to measure the output values of oxygen-saturated environment and oxygen-free environment at different temperatures. The two ends of each straight line in the figure are the values of oxygen-free environment and oxygen-saturated environment at that temperature. The methods of manufacturing oxygen-saturated environment and oxygen-free environment are to pass oxygen and nitrogen into the water respectively. The relationship between dissolved oxygen concentration and the current collected by the flexible dissolved oxygen sensor at different temperatures is obtained by using the two-point straight line fitting method. The results are as follows: Figure 4 As shown;
[0071] The key to temperature compensation is to find the relationship between the slope K of the dissolved oxygen sensor response curve and temperature at different temperatures. Figure 5 The fitting curve of slope K and temperature was obtained, and the curve equation is: y = -0.0676x 2 -4.7784x+88.59, R 2 =0.9995, and after matching this curve with the temperature of the flexible dissolved oxygen sensor, the K value of the dissolved oxygen sensor response curve at this temperature is obtained, corresponding to Figure 4 The response curve of the dissolved oxygen sensor at different temperatures is combined with the response current measured by the sensor to obtain the dissolved oxygen content value.
[0072] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or replace some or all of the technical features therein by equivalents. However, these modifications or replacements do not make the essence of the corresponding technical solutions deviate from the scope of the technical solutions of the embodiments of the present invention.
Claims
1. A flexible dissolved oxygen sensor, characterized in that: It comprises a dissolved oxygen sensor and a temperature sensor, wherein the dissolved oxygen sensor and the temperature sensor are arranged together on the same side or both sides of a flexible substrate (1), and the temperature sensor is used to assist the dissolved oxygen sensor in measuring the dissolved oxygen concentration in the water body.
2. A flexible dissolved oxygen sensor according to claim 1, characterized in that: The dissolved oxygen sensor comprises an electrode assembly and an electrolyte, wherein the electrode assembly comprises a working electrode (2), a reference electrode (3) and an auxiliary electrode (4), wherein the working electrode (2) is located between the reference electrode (3) and the auxiliary electrode (4), and the electrode assembly is also covered with an oxygen permeable membrane (5), and the electrolyte is located between the oxygen permeable membrane (5) and the electrode assembly; The working electrode (2), the reference electrode (3) and the auxiliary electrode (4) are electrically connected to the electrode pin I (8) respectively.
3. A flexible dissolved oxygen sensor according to claim 2, characterized in that: The working electrode (2) and the auxiliary electrode (4) are both noble metal electrodes, and the reference electrode (3) is an Ag / AgCl electrode.
4. A flexible dissolved oxygen sensor according to claim 3, characterized in that: The noble metal electrode is an Au electrode or a Pt electrode.
5. A flexible dissolved oxygen sensor according to claim 4, characterized in that: The working electrode (2) is a circular electrode, and the auxiliary electrode (4) surrounds the working electrode (2) in a concentric arc manner.
6. A flexible dissolved oxygen sensor according to claim 5, characterized in that: The temperature sensor comprises a temperature sensitive layer electrode (6) and an electrode pin II (7), wherein the two electrode pins II (7) are electrically connected to the head end and the tail end of the temperature sensitive layer electrode (6) respectively, and the temperature sensitive layer electrode (6) is a temperature sensitive conductive electrode.
7. A flexible dissolved oxygen sensor according to claim 6, characterized in that: The electrode material of the temperature-sensitive conductive electrode is selected from conductive polymers, carbon-based materials or conductive metal nano-inks.
8. A method for preparing the flexible dissolved oxygen sensor according to claim 7, characterized in that: The steps include: The flexible substrate (1) is cleaned to obtain a treated substrate; After depositing the two electrode pins II (7) on one side of the processing substrate by magnetron sputtering, the temperature sensitive layer electrode (6) is deposited on the processing substrate between the two electrode pins II (7), and the head end and the tail end of the temperature sensitive layer electrode (6) are respectively connected to the electrode pin II (7); The working electrode (2) and the auxiliary electrode (4) are deposited on the other surface of the treated substrate by magnetron sputtering, and the Ag electrode is produced by dispensing, so that the working electrode (2) is located between the auxiliary electrode (4) and the Ag electrode, and the Ag electrode is chlorinated in HCl electrolyte using a three-electrode system to obtain the AgCl electrode; The electrode assembly is covered with the oxygen permeable membrane (5), and the electrolyte is filled between the electrode assembly and the oxygen permeable membrane (5).
9. A flexible dissolved oxygen sensor according to claim 8, characterized in that: When the dissolved oxygen sensor and the temperature sensor are arranged together on the same side of the flexible substrate (1), the temperature sensitive layer electrode (6) is electrically connected to any two of the electrode pins I (8).
10. A method for preparing the flexible dissolved oxygen sensor according to claim 9, characterized in that: The steps include: The flexible substrate (1) is cleaned to obtain a treated substrate; After depositing the electrode pins I (8) on one side of the processing substrate by magnetron sputtering, depositing the temperature sensitive layer electrode (6) on the processing substrate between any two of the electrode pins I (8), and connecting the head end and the tail end of the temperature sensitive layer electrode (6) to the electrode pins I (8) respectively, to obtain a temperature sensor; The working electrode (2) and the auxiliary electrode (4) are deposited on the temperature sensor by magnetron sputtering, and the Ag electrode is produced by dispensing, so that the working electrode (2) is located between the auxiliary electrode (4) and the Ag electrode, and the Ag electrode is chlorinated in an HCl electrolyte using a three-electrode system to obtain the AgCl electrode; The electrode assembly is covered with the oxygen permeable membrane (5), and the electrolyte is filled between the electrode assembly and the oxygen permeable membrane (5).
Citation Information
Patent Citations
All-solid state dissolved oxygen sensor and preparation method thereof
CN101881749A
Self-power flexible temperature pressure sensor system
CN109425381A
Thermohaline dissolved oxygen sensor and preparation method thereof
CN111121861A
Integrated array type multi-parameter flexible wearable sensor and preparation method thereof
CN117598670A
Cited By
Dissolved oxygen electrode assembly and method for measuring the amount of dissolved oxygen in liquid
TWI915096B